Packaging structure for improving warping and heat dissipation and manufacturing method thereof
By designing silicon wafer grooves and through-holes in the semiconductor packaging structure, and connecting thin chips with dielectric layer and rewiring layer, the problems of insufficient warping and heat dissipation are solved, achieving higher integration and reliability simplifies process flow and reduces costs.
Patent Information
- Application Number
- CN202411070824.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-06
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-08-06
AI Technical Summary
The existing semiconductor packaging structure has shortcomings in warping and heat dissipation, which limits the improvement of chip integration and product reliability. It also has complex processes and high costs, making it difficult to meet the needs of miniaturization, high density and multifunctionality.
Design a packaging structure including silicon wafers, grooves, through holes and metal filling, connect thin chips through dielectric layer, passivation layer and rewiring layer, and form grooves and through holes on the back of the silicon wafer to fill the bottom glue To improve warpage and heat dissipation, simplify the process flow.
It effectively reduces warping in the vertical direction of die, improves product reliability and heat dissipation, simplifies production processes, reduces costs, and is suitable for industrial promotion.
Smart Images

Figure CN118983286A_ABST
Abstract
Description
Technical Field
[0001] The present invention belongs to the technical field of semiconductor packaging, and in particular relates to a packaging structure for improving warping and heat dissipation and a manufacturing method thereof. Background Art
[0002] As people's requirements for the performance of electronic products continue to increase, semiconductor packaging structures are developing in the direction of miniaturization, high density, multi-function and systematization. The current existing packaging structure directly connects the chips vertically through the adapter plate, which has a serious warping problem. It has great limitations on the diversification of chip integration and the improvement of integration. It is still difficult to deal with the integrated packaging of multiple chips or components, and the product reliability and heat dissipation need to be improved. In addition, the existing packaging process has a relatively complex process flow, high production cost, and the product yield needs to be improved. Summary of the invention
[0003] In order to solve the technical problems existing in the prior art, an object of the present invention is to provide a packaging structure with improved warping and heat dissipation and a manufacturing method thereof.
[0004] In order to achieve the above purpose and the above technical effect, the technical solution adopted by the present invention is:
[0005] A packaging structure for improving warping and heat dissipation comprises a silicon wafer, wherein a groove and a through hole are provided on the back of the silicon wafer, a chip I is arranged in the groove, the through hole is filled with metal, a chip II is arranged on the chip I and the metal, and a thin chip is arranged on the front of the silicon wafer.
[0006] Furthermore, a dielectric layer is disposed on the front side of the silicon wafer, a passivation layer and a redistribution layer are disposed on the dielectric layer, and a pad is formed on the outermost surface.
[0007] Furthermore, the front side of the silicon wafer is connected to the thin chip via a redistribution layer, the thickness of the thin chip is 50 to 150 microns, and the gap between the redistribution layer and the thin chip is filled with a filling material.
[0008] Furthermore, the chip I is fixed in the groove by means of an adhesive material, and the chip I is provided with one or a plurality of chips being stacked.
[0009] Furthermore, the gap between the chip I and the metal and the chip II is filled with primer to improve warping and increase heat dissipation.
[0010] The present invention also discloses a method for manufacturing a packaging structure with improved warping and heat dissipation, comprising the following steps:
[0011] Step 1: Deposit a dielectric layer on the surface of the silicon wafer to act as an insulator and a silicon etching stop layer;
[0012] Step 2: A passivation layer and a redistribution layer are sequentially arranged on the dielectric layer, a pad is formed on the surface, and then glass or ceramic material is bonded;
[0013] Step 3: Etching on the back of the silicon wafer to form a groove;
[0014] Step 4: Etching on the back of the silicon wafer to form a through hole;
[0015] Step 5: Paste chip I into the groove;
[0016] Step 6: Passivate the through-hole and the surface of the silicon wafer, fill the through-hole with metal through the electroplating process, remove the surface metal, and then form a rewiring structure;
[0017] Step 7: Solder chip II on the surface of the semi-finished product obtained in step 6, and fill the gap between the two with primer to improve warping and increase heat dissipation;
[0018] Step 8: Remove the glass or ceramic material, connect the thin chip to the redistribution layer, use filling material to fill the gap between the redistribution layer and the thin chip, and make solder joints on the pads.
[0019] Furthermore, in step 1, the dielectric layer is made of silicon oxide or silicon nitride and has a thickness of 0.5 to 2 microns.
[0020] Furthermore, in step five, the chip I is attached to the groove by means of an adhesive material for fixation, and the chip I is provided with one or more chips stacked to improve the warping in the X and Y directions.
[0021] Furthermore, in step six, the through hole and the silicon wafer surface are first passivated by depositing a node layer, and then the through hole is filled with metal by an electroplating process. After removing the surface metal, a rewiring structure is formed, and the thickness of the node layer is 0.5 to 2 microns.
[0022] Furthermore, in step eight, the thickness of the thin chip is 50 to 150 microns.
[0023] Compared with the prior art, the present invention has the following beneficial effects:
[0024] The invention discloses a packaging structure for improving warpage and heat dissipation and a manufacturing method thereof. First, a dielectric layer is deposited on the front side of a silicon wafer, and then a passivation layer and a redistribution layer are sequentially arranged on the dielectric layer, and then glass or ceramic materials are bonded, which is beneficial to improving warpage, and grooves and through holes are formed on the back side of the silicon wafer, and then a chip I to be mounted is pasted into the groove, and then the hole is filled with electroplating, and then a chip II is welded on the surface and filled with primer to improve warpage and increase heat dissipation. Finally, the glass or ceramic material is removed, and a thin chip is connected to the redistribution layer, and a filling material is used to fill the gap between the redistribution layer and the thin chip. This design idea can reduce the warpage of stacked interconnection in the vertical direction of the die, and at the same time improve the reliability and heat dissipation of the product. The overall manufacturing process is simple and efficient, the product yield is high, the manufacturing cost is low, and it is suitable for industrial promotion and use. BRIEF DESCRIPTION OF THE DRAWINGS
[0025] Figure 1 It is a structural schematic diagram of step 1 of the present invention;
[0026] Figure 2 It is a structural schematic diagram of step 2 of the present invention;
[0027] Figure 3 It is a structural schematic diagram of step three of the present invention;
[0028] Figure 4 A top view of the groove in step three of the present invention;
[0029] Figure 5 The warping force direction diagram of step three of the present invention;
[0030] Figure 6 It is a structural schematic diagram of step 4 of the present invention;
[0031] Figure 7 A top view of the through hole in step 4 of the present invention;
[0032] Figure 8 It is a structural schematic diagram of step five of the present invention;
[0033] Fig. 9 It is a structural schematic diagram of step six of the present invention;
[0034] Fig.10 It is a structural schematic diagram of step seven of the present invention;
[0035] Fig.11 It is a structural schematic diagram of step eight of the present invention. DETAILED DESCRIPTION
[0036] The present invention is described in detail below so that the advantages and features of the present invention can be more easily understood by those skilled in the art, thereby making a clearer and more definite definition of the protection scope of the present invention.
[0037] A brief summary of one or more aspects is given below to provide a basic understanding of these aspects. This summary is not an exhaustive overview of all conceived aspects, and is neither intended to identify the key or critical elements of all aspects nor to define the scope of any or all aspects. Its only purpose is to give some concepts of one or more aspects in a simplified form as a prelude to a more detailed description that will be given later.
[0038] like Figure 1-11 As shown, the present invention discloses a packaging structure for improving warpage and heat dissipation, comprising a silicon wafer 2, a dielectric layer 1 is arranged on the front side of the silicon wafer 2, a passivation layer 3 and a redistribution layer 4 are arranged on the dielectric layer 1, a solder pad 5 is formed on the outermost surface, the front side of the silicon wafer 2 is connected to a thin chip 16 through the redistribution layer 4, the thickness of the thin chip 16 is 50 to 150 microns, a filling material 17 is filled in the gap between the redistribution layer 4 and the thin chip 16, a groove 7 and a through hole 8 are opened on the back side of the silicon wafer 2, a chip I9 is fixed in the groove 7 by an adhesive material 10, one or more chips I9 are arranged in a stacked manner, a metal 11 is filled in the through hole 8, a chip II 14 is arranged on the chip I9 and the metal 11, and a primer 15 is filled in the gap between the chip I9 and the metal 11 and the chip II 14, so as to improve the warpage and increase the heat dissipation.
[0039] Chip I 9, chip II 14, and thin chip 16 are selected according to the customer's needs and are of appropriate types, which will not be described in detail here.
[0040] The present invention also discloses a method for manufacturing a packaging structure with improved warping and heat dissipation, comprising the following steps:
[0041] Step 1: If Figure 1 As shown, a dielectric layer 1 is deposited on the surface of the silicon wafer 2 to play the role of insulation and silicon etching stop layer. The dielectric layer 1 can be made of silicon oxide, silicon nitride and other materials, with a thickness of 0.5 to 2 microns;
[0042] Step 2: If Figure 2 As shown, a passivation layer 3 and a redistribution layer 4 are sequentially arranged on the dielectric layer 1, a solder pad 5 is formed on the surface, and then glass 6 or ceramic material is bonded. In order to form a high-density package, the line width and line spacing of the redistribution layer 4 in this step can be 2 microns, 2 microns, or even 1.5 microns, 1.5 microns. The number of redistribution layers can be two or more layers. The redistribution is usually a copper line. The passivation layer 3 can be a solid dry film or a PI glue with a thickness of 10 to 20 microns. By bonding glass 6 or ceramic materials, the warping problem in step three can be controlled and the warping can be improved. If the chip is mounted in this step instead of bonding glass 6 or ceramic materials, there will be a smile-type warping. In step three, the groove angle will be subjected to expansion stress, causing the risk of hidden cracks;
[0043] Step 3: If Figure 3-5 As shown, the thickness of the silicon wafer 2 is reduced by grinding, and a groove 7 is formed on the back of the silicon wafer 2 by silicon oxide etching and silicon etching. The volume of the groove 7 is adapted to the volume of the chip Ⅰ9 to be mounted. The morphology of the groove 7 after etching is as shown in FIG. Figure 4 As shown. The etched groove shape and the cutting path (a 65-80 micron cutting path is made by exposure, development or etching, and the cutting path is between dies) are offset by 10° to 45°, which is achieved by yellow light etching. Figure 5 If the forces are superimposed in different directions, the warping will increase. By offsetting the angle, the superposition of forces in the vertical direction can be improved, thereby improving the warping.
[0044] Step 4: If Figure 6-7 As shown, a through hole 8 is formed by a silicon etching process, and the morphology after etching is as follows Figure 7 As shown, the through hole 8 penetrates the silicon wafer 2 but does not penetrate the dielectric layer 1, and the diameter of the through hole 8 is 10 to 80 microns;
[0045] Step 5: If Figure 8 As shown, the chip I9 is pasted into the groove 7 and fixed by the adhesive material 10. The embedded chip I9 can be a single chip or a multi-layer stacked chip. This chip pasting method can improve the warping in the X and Y directions;
[0046] Step 6: If Fig. 9 As shown, the through hole 8 and the silicon wafer surface are passivated by depositing a node layer 12. The node layer 12 can be made of silicon oxide, silicon nitride and other materials with a thickness of 0.5 to 2 microns. The through hole 8 is filled with metal 11 through an electroplating process, and the surface metal is removed by grinding, chemical mechanical polishing, etching and other methods. Then a rewiring structure 13 is formed, which can be a single layer or multiple layers;
[0047] Step 7: If Fig.10 As shown, the chip II 14 is welded on the surface of the semi-finished product obtained in step 6, and the gap between the two is filled with primer 15 to improve the warpage and increase the heat dissipation;
[0048] Step 8: If Fig.11 As shown, after removing the glass 6 or ceramic material, a thin chip 16 with a thickness of 50 to 150 microns is connected to the redistribution layer 4. Then, a filling material 17 is used to fill the gap between the redistribution layer 4 and the thin chip 16, and finally a solder joint 18 is made on the pad 5.
[0049] Example 1
[0050] like Figure 1-11As shown, a packaging structure for improving warpage and heat dissipation includes a silicon wafer 2, a dielectric layer 1 is arranged on the front side of the silicon wafer 2, a passivation layer 3 and a redistribution layer 4 are arranged on the dielectric layer 1, a solder pad 5 is formed on the outermost surface, the front side of the silicon wafer 2 is connected to a thin chip 16 through the redistribution layer 4, the thickness of the thin chip 16 is 50 microns, and a filling material 17 is filled in the gap between the redistribution layer 4 and the thin chip 16, a groove 7 and a through hole 8 are opened on the back side of the silicon wafer 2, a chip I9 is fixed in the groove 7 by an adhesive material 10, a chip I9 is provided with a, a through hole 8 is filled with metal 11, a chip II 14 is arranged on the chip I9 and the metal 11, and a primer 15 is filled in the gap between the chip I9 and the metal 11 and the chip II 14, so as to improve the warpage and increase the heat dissipation.
[0051] A method for manufacturing a packaging structure with improved warpage and heat dissipation, comprising the following steps:
[0052] Step 1: If Figure 1 As shown, a dielectric layer 1 is deposited on the surface of the silicon wafer 2 to play the role of insulation and silicon etching stop layer. The dielectric layer 1 is made of silicon oxide material and has a thickness of 0.5 microns;
[0053] Step 2: If Figure 2 As shown, a passivation layer 3 and a redistribution layer 4 are sequentially arranged on the dielectric layer 1, a solder pad 5 is formed on the surface, and then bonding glass 6 is bonded. In order to form a high-density package, the line width and line spacing of the redistribution layer 4 in this step are 2 microns and 2 microns. There are two layers of redistribution. The redistribution is usually a copper line. The passivation layer 3 is a solid dry film with a thickness of 10 microns. The warping problem in step three can be controlled and improved by bonding glass 6. If the chip is mounted in this step instead of bonding glass 6, there will be a smile-type warping. In step three, the groove angle will be subjected to expansion stress, causing the risk of hidden cracks;
[0054] Step 3: If Figure 3-5 As shown, the thickness of the silicon wafer 2 is reduced by grinding, and a groove 7 is formed on the back of the silicon wafer 2 by silicon oxide etching and silicon etching. The volume of the groove 7 is adapted to the volume of the chip Ⅰ9 to be mounted. The morphology of the groove 7 after etching is as shown in FIG. Figure 4 As shown. The etched groove shape and the cutting path (a 65-micron cutting path is made by exposure, development or etching, and the cutting path is between dies) are offset by 10° and are achieved by yellow light etching. Figure 5 If the forces are superimposed in different directions, the warping will increase. By offsetting the angle, the superposition of forces in the vertical direction can be improved, thereby improving the warping.
[0055] Step 4: If Figure 6-7 As shown, a through hole 8 is formed by a silicon etching process, and the morphology after etching is as follows Figure 7As shown, the through hole 8 penetrates the silicon wafer 2 but does not penetrate the dielectric layer 1, and the diameter of the through hole 8 is 10 microns;
[0056] Step 5: If Figure 8 As shown, the chip I9 is pasted into the groove 7 and fixed by the adhesive material 10. The embedded chip I9 is a single chip, and this chip placement method can improve the warpage in the X and Y directions;
[0057] Step 6: If Fig. 9 As shown, the through hole 8 and the silicon wafer surface are passivated by depositing a node layer 12, the node layer 12 is a silicon oxide material with a thickness of 0.5 microns. The through hole 8 is filled with metal 11 through an electroplating process, and the surface metal is removed by grinding, chemical mechanical polishing, etching, etc. Then a rewiring structure 13 is formed, which can be a layer;
[0058] Step 7: If Fig.10 As shown, the chip II 14 is welded on the surface of the semi-finished product obtained in step 6, and the gap between the two is filled with primer 15 to improve the warpage and increase the heat dissipation;
[0059] Step 8: If Fig.11 As shown, after the glass 6 is removed, a thin chip 16 with a thickness of 50 microns is connected to the redistribution layer 4. Then, a filling material 17 is used to fill the gap between the redistribution layer 4 and the thin chip 16, and finally a solder joint 18 is made on the pad 5.
[0060] Parts or structures not specifically described in the present invention may adopt existing technologies or existing products and will not be described in detail here.
[0061] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.
Claims
1. A packaging structure for improving warpage and heat dissipation, comprising a silicon wafer, characterized in that: A groove and a through hole are provided on the back of the silicon wafer, a chip I is arranged in the groove, the through hole is filled with metal, a chip II is arranged on the chip I and the metal, and a thin chip is arranged on the front of the silicon wafer.
2. A packaging structure for improving warpage and heat dissipation according to claim 1, characterized in that: A dielectric layer is arranged on the front side of the silicon wafer, a passivation layer and a redistribution layer are arranged on the dielectric layer, and a pad is formed on the outermost surface.
3. A packaging structure for improving warpage and heat dissipation according to claim 2, characterized in that: The front side of the silicon wafer is connected to the thin chip through a redistribution layer. The thickness of the thin chip is 50 to 150 microns. The gap between the redistribution layer and the thin chip is filled with a filling material.
4. The packaging structure for improving warpage and heat dissipation according to claim 1, characterized in that: The chip I is fixed in the groove by means of adhesive material, and one or more chips I are stacked.
5. The packaging structure for improving warpage and heat dissipation according to claim 1, characterized in that: The gap between the chip I and the metal and the chip II is filled with primer to improve the warping and increase the heat dissipation.
6. A method for manufacturing a packaging structure with improved warpage and heat dissipation according to any one of claims 1 to 5, characterized in that: The following steps are involved: Step 1: Deposit a dielectric layer on the surface of the silicon wafer to act as an insulator and a silicon etching stop layer; Step 2: A passivation layer and a redistribution layer are sequentially arranged on the dielectric layer, a pad is formed on the surface, and then glass or ceramic material is bonded; Step 3: Etching on the back of the silicon wafer to form a groove; Step 4: Etching on the back of the silicon wafer to form a through hole; Step 5: Paste chip I into the groove; Step 6: Passivate the through-hole and the surface of the silicon wafer, fill the through-hole with metal through the electroplating process, remove the surface metal, and then form a rewiring structure; Step 7: Solder chip II on the surface of the semi-finished product obtained in step 6, and fill the gap between the two with primer to improve warping and increase heat dissipation; Step 8: Remove the glass or ceramic material, connect the thin chip to the redistribution layer, use filling material to fill the gap between the redistribution layer and the thin chip, and make solder joints on the pads.
7. The method for manufacturing a packaging structure with improved warpage and heat dissipation according to claim 6, characterized in that: In step 1, the dielectric layer is made of silicon oxide or silicon nitride and has a thickness of 0.5 to 2 microns.
8. The method for manufacturing a packaging structure with improved warpage and heat dissipation according to claim 6, characterized in that: In step five, chip I is attached to the groove by adhesive material for fixation, and the chip I is provided with one or more chips stacked to improve the warping in the X and Y directions.
9. The method for manufacturing a packaging structure with improved warpage and heat dissipation according to claim 6, characterized in that: In step six, the through hole and the silicon wafer surface are first passivated by depositing a node layer, and then the through hole is filled with metal through an electroplating process. After removing the surface metal, a rewiring structure is formed.
10. The method for manufacturing a packaging structure with improved warpage and heat dissipation according to claim 6, characterized in that: In step eight, the thickness of the thin chip is 50 to 150 microns.
Citation Information
Patent Citations
Deep trench manufacturing method for improving silicon wafer warping degree
CN103715130A
Silicon substrate fan-out packaging method and structure
CN110416091A
Silicon-based fan-out type 3D packaging structure and method for preferentially forming rewiring layer
CN116344463A
IC package structure
JP2007088049A
Overlay Mark Arrangement for Reducing Overlay Shift
US20070258637A1