Preparation method of tellurium-cadmium-mercury infrared detector chip
By forming a passivation layer and a dielectric layer during the preparation of infrared detection chips, avoiding contact between photoresist and metal, and using etching technology to form metal electrodes, the problems of photoresist residue and solvent corrosion in the prior art are solved, significantly improving the The conductivity and performance of the chip.
Patent Information
- Application Number
- CN202411471167.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-22
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2044-10-22
AI Technical Summary
During the preparation of existing infrared detection chips, the peeling process causes photoresist residues and solvents to corrode the metal layer, affecting the performance and conductivity of the substrate material.
The passivation layer and a dielectric layer are formed on the photoelectric material layer of the substrate. Through etching, the through holes are formed, the metal layer is covered and the dielectric layer is removed, so as to avoid direct contact between the photoresist and the metal, and the image is formed by wet or dry etching. Metal electrode.
有效避免了光刻胶残留和溶液腐蚀风险,提升了碲镉汞红外探测器芯片的导电性和性能。
Smart Images

Figure CN118983375A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the technical field of infrared detectors, and in particular to a method for preparing a mercury cadmium telluride infrared detector chip. Background Art
[0002] With the continuous promotion and development of infrared applications, advanced infrared detection technology requires detectors to have higher spatial resolution and better target recognition capabilities. Infrared detectors are photoelectric devices that convert infrared radiation into electronic signals. The photoelectric reaction only occurs on the photosensitive element, and the subsequent signal processing process only involves electronic technology. Therefore, infrared detection chips are the core components of infrared detectors.
[0003] In the production process of infrared detection chips, when etching the metal layer to form a metal electrode, the existing technology is to use a stripping process, using a mask layer such as a photoresist to protect the part that needs to be retained, and then use a specific chemical solution or physical method to strip the metal material on the photoresist to obtain the desired pattern. In this way, the solvent residue may cause certain damage to the base material, thereby affecting the product performance. Summary of the invention
[0004] In order to solve the problems existing in the prior art, the present invention provides a method for preparing a mercury cadmium telluride infrared detector chip.
[0005] The present invention provides a method for preparing a mercury cadmium telluride infrared detector chip, comprising the following steps: providing a substrate, which comprises a photoelectric material layer; sequentially forming a passivation layer and a dielectric layer on the photoelectric material layer; etching the dielectric layer to form a first through hole, exposing the passivation layer; etching the passivation layer in the first through hole to form a second through hole, exposing the photoelectric material layer; forming a metal layer on one side of the photoelectric material layer of the substrate, covering the dielectric layer, the passivation layer in the first through hole and the photoelectric material layer in the second through hole; etching the metal layer to form an imaged metal electrode; and removing the dielectric layer to form the mercury cadmium telluride infrared detector chip.
[0006] Optionally, the photoelectric material layer is a mercury cadmium telluride layer.
[0007] Optionally, the material of the passivation layer includes zinc sulfide.
[0008] Optionally, the material of the dielectric layer includes silicon dioxide.
[0009] Optionally, removing the dielectric layer includes: corroding the dielectric layer using a hydrofluoric acid solution.
[0010] Optionally, the metal layer includes a stacked structure of a first metal layer and a second metal layer, the material of the first metal layer is platinum, and the material of the second metal layer is chromium.
[0011] Optionally, the etching of the metal layer to form an imaged metal electrode comprises the steps of: covering the metal layer with a patterned positive photoresist; and wet-etching the metal layer to form a patterned metal electrode.
[0012] Optionally, the wet etching of the metal layer includes: etching the first metal layer and the second metal layer through a wet etching process; wherein, the etching solution for etching the first metal layer includes: a solution of hydrochloric acid and water mixed in a ratio of 1:3, and the etching solution for etching the second metal layer includes: a solution of iodine and potassium iodide and water mixed in a ratio of 1:2:20.
[0013] Optionally, etching the metal layer to form an imaged metal electrode includes: etching the first metal layer and the second metal layer through a dry etching process; wherein the dry etching includes ICP etching, the power range of the ICP etching is 200-600W, the radio frequency range used in the dry etching is 10-100W, and the pressure range used in the dry etching is 1-10Pa.
[0014] Optionally, the gas used for the dry etching includes: Cl2, BCl3, Ar, wherein the flow range of Cl2 is 5-10sccm, the flow range of BCl3 is 1-3sccm, and the flow range of Ar is 5-10sccm.
[0015] Compared with the prior art, the technical solution of the present invention has the following beneficial effects:
[0016] The present invention provides a method for preparing a mercury cadmium telluride infrared detector chip. By forming a dielectric layer on a passivation layer, a metal layer is prevented from directly contacting a photoresist on the passivation layer, and the photoresist film on the passivation layer is avoided from remaining on the metal surface and the reaction between the solution and the metal is avoided, so that the conductivity between the two metal layers of the mercury cadmium telluride infrared detector chip is greatly improved. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0018] Figure 1 A schematic diagram of the intermediate structure of the process of preparing an infrared detection chip in the prior art;
[0019] Figure 2 A schematic diagram of a process for preparing a mercury cadmium telluride infrared detector chip according to an embodiment of the present disclosure;
[0020] Figure 3 It is a schematic diagram of a first intermediate structure of a formation process of a mercury cadmium telluride infrared detector chip according to an embodiment of the present disclosure;
[0021] Figure 4 It is a schematic diagram of a second intermediate structure of a process for forming a mercury cadmium telluride infrared detector chip according to an embodiment of the present disclosure;
[0022] Figure 5 A schematic diagram of a third intermediate structure of a formation process of a mercury cadmium telluride infrared detector chip according to an embodiment of the present disclosure;
[0023] Figure 6 This is a schematic diagram of the fourth intermediate structure of a process for forming a mercury cadmium telluride infrared detector chip according to an embodiment of the present disclosure. DETAILED DESCRIPTION
[0024] The preferred embodiments of the present invention will be described in more detail below. Although the preferred embodiments of the present invention are described below, it should be understood that the present invention can be implemented in various forms and should not be limited to the embodiments set forth herein.
[0025] In the present invention, unless otherwise specified, the directional words used, such as "upper and lower", generally refer to the upper and lower parts of the device in normal use, and "inside and outside" refer to the outline of the device. In addition, the terms "first, second, third" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance or implicitly indicating the number of technical features indicated. Therefore, the features defined as "first, second, third" may explicitly or implicitly include one or more of the features. In the description of the present invention, "multiple" means two or more, unless otherwise clearly and specifically defined. In the present invention, it is an electrical device, so connection and interconnection both refer to conductive interconnection. Since the accompanying drawings are descriptions of the same device, the same numbers in the drawings represent the same components.
[0026] As described in the background technology, the prior art uses a stripping process to prepare infrared detection chips, using a mask layer such as a photoresist to protect the part that needs to be retained, and then using a specific chemical solution or physical method to strip the metal material on the photoresist. In this way, the chemical reagents and solvent residues may cause certain damage to the base material. Figure 1As shown, in the process of preparing infrared detection chips in the prior art, a through hole is formed on the passivation layer 120 using a photolithography process, and a patterned metal electrode 140 is formed in the through hole. During the etching process, the through hole of the passivation layer 120 is easily exposed to solvent contamination, and an oxide film is formed in the through hole. The oxide film in the through hole needs to be further processed later. When the oxide film in the through hole is corroded, the passivation layer 120 outside the through hole will be affected, increasing the risk of leakage. At the same time, in the process of forming the metal electrode, the metal layer is easily in contact with the photoresist 160 on the surface of the passivation layer 120, thereby corroding the metal layer 140.
[0027] Therefore, the embodiments of the present disclosure provide a method for preparing a mercury cadmium telluride infrared detector chip, which can effectively solve the above problems and greatly improve the performance of the mercury cadmium telluride infrared detector chip.
[0028] The disclosed embodiment provides a method for preparing a mercury cadmium telluride infrared detector chip, comprising the following steps: providing a substrate, which comprises a photoelectric material layer; sequentially forming a passivation layer and a dielectric layer on the photoelectric material layer; etching the dielectric layer to form a first through hole, exposing the passivation layer; etching the passivation layer in the first through hole to form a second through hole, exposing the photoelectric material layer; forming a metal layer on one side of the photoelectric material layer of the substrate, covering the dielectric layer, the passivation layer in the first through hole, and the photoelectric material layer in the second through hole; etching the metal layer to form an imaged metal electrode; and removing the dielectric layer to form the mercury cadmium telluride infrared detector chip.
[0029] The specific examples of the present invention are further described in detail below in conjunction with the accompanying drawings. Wherein, the substances not listed in detail in the embodiments can be selected from any substances on the market that can achieve corresponding functions.
[0030] This embodiment provides a method for preparing a mercury cadmium telluride infrared detector chip, the specific steps are as follows: Figure 2 As shown, Figures 3 to 6 The figure is a schematic diagram of the intermediate structure of the formation process of the mercury cadmium telluride infrared detector chip of the embodiment of the present disclosure. In combination with the accompanying drawings, the preparation method of the mercury cadmium telluride infrared detector chip includes the following steps:
[0031] S1: providing a substrate comprising a photoelectric material layer.
[0032] like Figure 3 As shown, a substrate 100 is provided, and the substrate 100 includes a photoelectric material layer 110. In the embodiment of the present disclosure, the substrate 100 is a cadmium zinc telluride substrate, and the photoelectric material layer 110 is a mercury cadmium telluride layer.
[0033] S2: forming a passivation layer and a dielectric layer in sequence on the photoelectric material layer.
[0034] like Figure 3As shown, first, a passivation layer 120 is formed on the surface of the photoelectric material layer 110. The passivation layer 120 can be formed by thermal evaporation as a protective layer for the refrigerated infrared detector device to prevent the device surface from being damaged in subsequent processes, which is conducive to better subsequent processes. For example, the surface of the device will not be contaminated or damaged in subsequent processes. In the embodiment of the present disclosure, the material of the passivation layer 120 is preferably zinc sulfide. Then, a dielectric layer 130 is formed on the surface of the passivation layer 120. In some embodiments, the dielectric layer 130 can be formed by plasma enhanced chemical vapor deposition. In the embodiment of the present disclosure, the material of the dielectric layer 130 is preferably silicon dioxide. In the subsequent process of corroding the metal, the silicon dioxide film as the dielectric layer 130 is in direct contact with the metal layer of the mercury cadmium telluride infrared detector chip, preventing the metal layer from contacting the photoresist on the passivation layer, and avoiding the photoresist layer on the passivation layer from corroding the metal layer.
[0035] S3: etching the dielectric layer to form a first through hole, exposing the passivation layer.
[0036] In the embodiments of the present disclosure, continue to refer to Figure 3 , a positive first photoresist is spin-coated on the surface of the dielectric layer 130, and then exposed and developed to form a patterned first photoresist layer; then, the dielectric layer 130 is etched by shielding the patterned first photoresist layer, and a first through hole is formed on the dielectric layer 130 using an etching process to expose the passivation layer 120; then, the patterned first photoresist layer is removed and dried with nitrogen, and the first through hole is a groove structure during the device preparation process, and the bottom of the groove is the exposed passivation layer 120.
[0037] S4: etching the passivation layer in the first through hole to form a second through hole, exposing the photoelectric material layer.
[0038] In the embodiment of the present disclosure, the passivation layer 120 in the first through hole is first etched by an overlay process. When etching the passivation layer 120 in the first through hole, only the passivation layer 120 in the center area of the first through hole is etched to form the second through hole, and the passivation layer 120 in the edge area of the first through hole is not etched. The second through hole exposes the optoelectronic material layer 110, such as Figure 3 As shown, the second through hole is presented as a groove and table structure during the device preparation process, the bottom of the groove is the exposed optoelectronic material layer 110, and the side of the groove and the table are the passivation layer 120. The use of the overlay process can improve the chip manufacturing accuracy, improve the chip performance and improve the process efficiency.
[0039] S5: forming a metal layer on one side of the optoelectronic material layer of the substrate, covering the dielectric layer, the passivation layer in the first through hole, and the optoelectronic material layer in the second through hole.
[0040] Specifically, Figure 4 As shown, a first metal layer 141 is formed on the surface of the dielectric layer 130, the passivation layer 120 in the first through hole, and the optoelectronic material layer 110 in the second through hole using a thermal evaporation device. Next, a second metal layer 142 is formed on the surface of the first metal layer 141 using a thermal evaporation device. The metal layer 140 composed of the first metal layer 141 and the second metal layer 142 is used to form a metal electrode later.
[0041] In some embodiments, the metal layer includes a stacked structure of a first metal layer and a second metal layer. In the embodiment of the present disclosure, the material of the first metal layer is preferably platinum, and the material of the second metal layer is preferably chromium.
[0042] S6: etching the metal layer to form a patterned metal electrode.
[0043] Specifically, refer to Figure 5 , first, spin-coat the second metal layer 142 with a second photoresist, which is a positive photoresist, and then perform exposure and development to form a patterned second photoresist layer 150. Next, the second metal layer 142 is covered with the patterned second photoresist, so that the second metal layer 142 and the first metal layer 141 are etched to form a patterned metal electrode 140. The patterned second photoresist 150 protects the patterned metal electrode area. In the process of etching the excess metal layer using the photolithography process, the photoelectric material layer 110 is not easily exposed to the photoresist developer solvent, thereby avoiding contamination of the prepared mercury cadmium telluride infrared detector chip. At the same time, the patterned second photoresist protects the patterned metal electrode area, so that an oxide film is not easily formed in the second through hole formed in the passivation layer, and there is no risk of leakage to the periphery of the through hole of the passivation layer.
[0044] In different embodiments, different etching methods may be used to form the metal electrode. For example, in the first embodiment of the present disclosure, a wet etching process is used to etch the first metal layer and the second metal layer. The etching solution for etching the first metal layer includes a solution of hydrochloric acid and water mixed in a ratio of 1:3, and the etching solution for etching the second metal layer includes a solution of iodine and potassium iodide mixed in a ratio of 1:2:20 with water.
[0045] In some other embodiments, the first metal layer and the second metal layer may also be etched by a dry etching process. Specifically, when the dry etching process is adopted, in the ICP etching process, the power range of the ICP etching is 200-600W, the radio frequency range used by the dry etching of the first metal layer and the second metal layer is 10-100W, and the pressure range used by the dry etching of the first metal layer and the second metal layer is 1-10Pa,
[0046] Preferably, in the second embodiment of the present disclosure, a dry etching process is used to form the metal electrode, the power of the ICP etching used is 400W, the radio frequency used is 60W, and the pressure used is 6Pa.
[0047] In some embodiments, the gas used for dry etching includes: Cl2, BCl3, Ar, wherein the flow rate of Cl2 is in the range of 5-10 sccm, the flow rate of BCl3 is in the range of 1-3 sccm, and the flow rate of Ar is in the range of 5-10 sccm. In the second embodiment of the present disclosure, the flow rate of Cl2 is preferably 8 sccm, the flow rate of BCl3 is preferably 2 sccm, and the flow rate of Ar is preferably 8 sccm.
[0048] S7: removing the dielectric layer to form the mercury cadmium telluride infrared detector chip.
[0049] In some embodiments, Figure 6 As shown, the dielectric layer 130 is corroded by a hydrofluoric acid solution to remove the dielectric layer 130 so as to form the mercury cadmium telluride infrared detector chip.
[0050] The preparation method of the mercury cadmium telluride infrared detector chip provided by the present invention can effectively avoid the photoresist film from remaining on the metal surface and the reaction between the solution and the metal, and also avoid the risk of leakage of the passivation layer in the subsequent preparation process, which can greatly improve the conductivity effect of the contact between the two metals.
[0051] The above descriptions are merely embodiments of the present application and are not intended to limit the patent scope of the present application. Any equivalent structural or equivalent process transformations made using the contents of the specification and drawings of the present application, such as the mutual combination of technical features between the embodiments, or direct or indirect application in other related technical fields, are also included in the patent protection scope of the present application.
Claims
1. A method for preparing a mercury cadmium telluride infrared detector chip, It is characterized in that Includes steps: providing a substrate comprising a layer of optoelectronic material; forming a passivation layer and a dielectric layer in sequence on the photoelectric material layer; Etching the dielectric layer to form a first through hole, exposing the passivation layer; Etching the passivation layer in the first through hole to form a second through hole, exposing the photoelectric material layer; Forming a metal layer on one side of the optoelectronic material layer of the substrate, covering the dielectric layer, the passivation layer in the first through hole, and the optoelectronic material layer in the second through hole; etching the metal layer to form a patterned metal electrode; The dielectric layer is removed to form the mercury cadmium telluride infrared detector chip.
2. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 1, It is characterized in that The photoelectric material layer is a mercury cadmium telluride layer.
3. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 1, It is characterized in that The material of the passivation layer includes zinc sulfide.
4. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 1, It is characterized in that The material of the dielectric layer includes silicon dioxide.
5. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 4, It is characterized in that The removing of the dielectric layer includes: corroding the dielectric layer with a hydrofluoric acid solution.
6. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 1, It is characterized in that The metal layer includes a stacked structure of a first metal layer and a second metal layer. The material of the first metal layer is platinum, and the material of the second metal layer is chromium.
7. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 1, It is characterized in that The etching of the metal layer to form an imaged metal electrode comprises the steps of: Covering the metal layer with a patterned positive photoresist; The metal layer is wet-etched to form a patterned metal electrode.
8. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 7, It is characterized in that The wet etching of the metal layer comprises: etching the first metal layer and the second metal layer by a wet etching process; wherein The etching solution for etching the first metal layer includes a solution of hydrochloric acid and water mixed in a ratio of 1:3, and the etching solution for etching the second metal layer includes a solution of iodine, potassium iodide and water mixed in a ratio of 1:2:
20.
9. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 6, It is characterized in that The etching of the metal layer to form an imaged metal electrode includes: etching the first metal layer and the second metal layer by a dry etching process; wherein the dry etching includes ICP etching, the power range of the ICP etching is 200-600W, the radio frequency range used in the dry etching is 10-100W, and the pressure range used in the dry etching is 1-10Pa.
10. The method for preparing the mercury cadmium telluride infrared detector chip according to claim 9, It is characterized in that The gas used in the dry etching includes: Cl 2 , BCl 3 , Ar, among which Cl 2 The flow rate range is 5-10sccm, BCl 3 The flow rate range of Ar is 1-3sccm, and the flow rate range of Ar is 5-10sccm.
Citation Information
Patent Citations
Method for detecting effective junction depth of PN junction of mercury cadmium telluride chip
CN114141645A
HgCdTe planar heterojunction detector and preparation method thereof
CN114141904A
Refrigeration infrared focal plane detector based on Schottky junction and preparation method thereof
CN118472106A
HgCdTe infrared detector and preparation method thereof
CN118676261A
Double inlaying method for barriering gas release and generating projective structure
CN1452234A
Cited By
Preparation method for mercury cadmium telluride infrared detector chip
WO2026086195A1