COB mirror surface copper package loading plate stack-up structure and process manufacturing method
Through COB mirror copper packaging load plate stacking technology, composite copper substrate, dielectric layer and high thermal conductivity colloids are used to solve the problems of high-temperature and electric field concentration in high-power lighting equipment, improve the stability and heat dissipation efficiency of the chip, and extend the use life.
Patent Information
- Application Number
- CN202411040211.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-19
AI Technical Summary
The high temperature of high-power lighting equipment leads to a reduced service life, the heat dissipation efficiency of traditional copper substrates is insufficient, and the high dielectric constant material causes electric field concentration to lead to a decrease in the chip's electrical performance.
The stacking method of COB mirror copper encapsulation plate is adopted, including composite copper substrate, dielectric layer, copper oxide particles and high thermal conductivity colloids. The dielectric constant is reduced through the dielectric layer, the copper oxide particles suppress thermal expansion rate, and high thermal conductivity colloids improve Heat dissipation efficiency.
It improves the electrical performance and stability of the chip, extends the service life, improves the heat dissipation efficiency, and reduces leakage current and thermal stress.
Smart Images

Figure CN118983389A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to LED packaging, and in particular to a COB mirror copper packaging carrier plate stacking structure and a process manufacturing method. Background Art
[0002] COB (Chip-on-Board) packaging technology is a technology that directly adheres the bare chip to the printed circuit board. This technology is mainly used to solve the heat dissipation problem of LEDs. It adheres the bare chip to the printed circuit board with conductive or non-conductive glue, and then achieves electrical connection through wire bonding. COB packaging technology has attracted widespread attention due to its excellent heat dissipation performance, cost-effectiveness and high reliability.
[0003] When packaged LED chips are used in actual applications, some of the heat will be dissipated in the form of thermal energy, causing the device temperature to rise, which can easily cause failures and affect device performance, work efficiency and service life. Currently commonly used high dielectric constant materials will enhance the local electric field strength, which not only poses a risk of material breakdown, but also causes local overheating problems, affecting the performance and service life of the device.
[0004] Therefore, the inventors of this application found that the above technology has at least the following technical problems in the process of implementing the technical solution of the invention in the embodiment of this application:
[0005] 1. As high-power lighting equipment generates a lot of heat, long-term high temperature will reduce the service life of the product, and the traditional copper substrate has insufficient heat dissipation efficiency and it is difficult to maintain a low temperature chip working environment;
[0006] 2. High dielectric constant materials will bring about a concentrated electric field environment, and the electrical performance and stability of the lighting chip packaged by the substrate will be reduced in an environment with a concentrated electric field. Summary of the invention
[0007] The embodiment of the present application provides a COB mirror copper packaging carrier stack and process manufacturing method, which solves the problems in the prior art that the high dielectric constant material brings about a concentrated electric field environment, resulting in the degradation of electrical performance and stability of the lighting chip packaged by the carrier in a concentrated electric field environment, and that high-power lighting equipment generates a lot of heat, and long-term high temperature will lead to a reduction in its lifespan, and the traditional copper plate has insufficient heat dissipation efficiency and is difficult to maintain a low temperature chip working environment, thereby achieving the technical effect of stable lighting of the lighting chip, increased service life, and improved heat dissipation efficiency.
[0008] The embodiment of the present application provides a COB mirror copper package carrier stack structure, including:
[0009] The composite copper substrate 1 is characterized in that the composite copper substrate 1 comprises:
[0010] A metal layer 7, wherein the metal layer 7 is included in the composite copper substrate 1;
[0011] A copper layer 8, wherein the copper layer 8 is included in the metal layer 7, and the thickness of the copper layer 8 is greater than 0.5 μm;
[0012] A copper matrix 9, wherein the copper matrix 9 is contained in the copper layer 8;
[0013] Cuprous oxide particles 10, wherein the cuprous oxide particles 10 are dispersed on the copper substrate 9;
[0014] The dielectric layer 11 is arranged on one side of the composite copper substrate 1 .
[0015] A first colloid 21, wherein the first colloid 21 covers the composite copper substrate 1;
[0016] Mirror aluminum 3, the mirror aluminum 3 covers the first colloid 21;
[0017] A second colloid 22, wherein the second colloid 22 covers the mirror aluminum 3;
[0018] A BT board 4, wherein the BT board 4 is located above the second colloid 22;
[0019] An ink layer 5, wherein the ink 5 is located above the BT board 4;
[0020] The circuit layer 6 is located above the BT board 4 and inside the ink layer 5 .
[0021] Furthermore, the colloid used for the first colloid 21 and the second colloid 22 is a high thermal conductive colloid.
[0022] Furthermore, the ink used in the ink layer 5 is white thermosetting ink.
[0023] Furthermore, the metal layer 7 is at least one metal selected from Ni, Sn, Ag, Au, Pt, Pd and Zn, and the thickness of the metal layer 7 is 0.4 to 100 μm.
[0024] Furthermore, the dielectric layer 11 is a dielectric powder-containing resin layer in which dielectric powder 12 is dispersed in a resin composition containing epoxy resin, active ester resin, polyvinyl acetal resin and a curing accelerator and semi-cured.
[0025] Furthermore, the dielectric powder is a powder composed of dielectric particles having a particle size of 0.02 μm to 2 μm and copper foil.
[0026] Furthermore, the thickness of the dielectric layer 11 is 0.5 μm to 25 μm.
[0027] In addition, a method for manufacturing a COB mirror copper package carrier is provided, comprising the following steps:
[0028] S1: remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding strength between the copper surface and the photosensitive dry film; S2: stick the photosensitive dry film on the board surface;
[0029] S3: Exposure and development to form a clear circuit pattern on the board to make a circuit layer;
[0030] S4: Remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding force between the copper surface and the ink;
[0031] S5: Scrape and print the ink evenly on the board surface and let it stand for 15 minutes;
[0032] S6: Push the ink into the oven for pre-baking to remove the organic solvent in the ink and partially harden the ink surface;
[0033] S7: Exposure, selectively forming unexposed areas and exposed areas on the ink surface to achieve solder mask phase transfer;
[0034] S8: Development, removing the ink coating on the unexposed area on the plate surface;
[0035] S9: Curing the ink in an oven;
[0036] S10: Paste a film on the back of the board to make it adhesive;
[0037] S11: Copper is plated with metal to prevent oxidation and enhance heat dissipation;
[0038] S12: bonding the copper plate and the mirror aluminum together by high temperature hot pressing;
[0039] S13: placing buffer auxiliary materials, and performing vacuum hot pressing on the pre-bonding to completely bond and solidify the BT and the mirror aluminum;
[0040] S14: Glue protective films on both sides of the laminated back plate to prevent the mirror surface from being scratched and contaminated.
[0041] Furthermore, a step may be added between S3 and S4: checking the circuit open and short circuits through electrical testing or AOI equipment to ensure electrical safety.
[0042] One or more technical solutions provided in the embodiments of the present application have at least the following technical effects or advantages:
[0043] 1. Since a dielectric layer 11 is arranged on the outside of the composite copper substrate 1, the adhesion between the inner circuit surface of the inner core material and the conductive layer is improved, forming a capacitor circuit layer with a low dielectric constant, solving the problem that the concentrated electric field environment caused by the relatively high dielectric constant of traditional materials has a negative impact on the electrical performance and stability of the lighting chip, reducing the leakage current of the circuit, reducing the heat generation of the chip, and improving the performance of the chip.
[0044] 2. Since cuprous oxide particles are added to the copper matrix in the composite copper substrate 1, the increase in the apparent thermal expansion coefficient of the composite material component is effectively suppressed, and the thermal stress or thermal strain generated by the traditional copper substrate material during production or operation is solved, thereby improving the heat dissipation efficiency, reducing the possibility of deformation, degradation and rupture of each component, thereby increasing the service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0045] Figure 1 This is the COB mirror copper package substrate stacking pattern for this application.
[0046] Figure 2 This is a schematic diagram of the appearance of the COB mirror copper package carrier board of this application.
[0047] Figure 3 This is a structural diagram of the composite copper substrate in the COB mirror copper package carrier of this application.
[0048] Figure 4 This is a schematic diagram of the dielectric layer of the composite copper substrate in the COB mirror copper package carrier of this application.
[0049] Figure 5 This is a flow chart of the manufacturing method of the COB mirror copper package carrier of this application.
[0050] Figure 6 This is a flow chart of the manufacturing method of the COB mirror copper package carrier after circuit testing in this application.
[0051] Figure 7 The relationship between the composition and thermal conductivity of the composite copper substrate 1 in the COB mirror copper package carrier of this application
[0052] Figure 8 This is a graph showing the relationship between the composition and thermal expansion coefficient of the composite copper substrate in the COB mirror copper package carrier of this application. DETAILED DESCRIPTION
[0053] In order to make the purpose, technical solution and advantages of the COB mirror copper package carrier stacking structure and process manufacturing method of the present application clearer, the present invention is further described in detail below in conjunction with the accompanying drawings and embodiments. It should be understood that the specific embodiments described here are only used to explain the present invention and are not used to limit the present invention.
[0054] Embodiment 1
[0055] like Figure 1 As shown in the figure, a COB mirror copper package carrier 1 of this embodiment is characterized in that the composite copper substrate 1 includes: a metal layer 7, the metal layer 7 is included in the composite copper substrate 1; a copper layer 8, the copper layer 8 is included in the metal layer 7, and the thickness of the copper layer 8 is greater than 0.5 μm; a copper matrix 9, the copper matrix 9 is included in the copper layer 8; cuprous oxide particles 10, the cuprous oxide particles 10 are dispersed on the copper matrix 9; a dielectric layer 11, the dielectric layer 11 is arranged on one side of the composite copper substrate 1. A first colloid 21, the first colloid 21 covers the composite copper substrate 1; a mirror aluminum 3, the mirror aluminum 3 covers the first colloid 21; a second colloid 22, the second colloid 22 covers the mirror aluminum 3; a BT board 4, the BT board 4 is located above the second colloid 22; an ink layer 5, the ink 5 is located above the BT board 4; a circuit layer 6, the circuit layer 6 is located above the BT board 4 and is located inside the ink layer 5. In this embodiment, a composite copper substrate 1 for a COB mirror copper package carrier is described. The reason why copper (Cu, thermal conductivity: 403 W / mK, thermal expansion coefficient: 16.7 ppm / °C) is selected as the matrix material 9 in the composite copper substrate 1 for a COB mirror copper package carrier of the present invention is because of its high thermal conductivity. This property is important in the sense that the heat flow emitted from the semiconductor substrate is preferentially released to the outside through the matrix area. However, the large thermal expansion coefficient of copper constitutes a disadvantage in ensuring reliable integration with peripheral components with a small thermal expansion coefficient. On the other hand, for the particles 10 dispersed in the matrix material 9, cuprous oxide (Cu2O, thermal conductivity: 6.6 W / mK, thermal expansion coefficient: 2.7 ppm / °C) is selected because of its small thermal expansion coefficient. The cuprous oxide particles 10 can effectively suppress the increase of the apparent thermal expansion coefficient of the composite copper substrate 1, but have the disadvantage of reducing the apparent thermal conductivity of the composite copper substrate 1. The composite copper substrate 1 in which the copper matrix 9 and the cuprous oxide particles 10 coexist complement each other with respect to the disadvantages of each component. The copper substrate 9 of the composite copper substrate 1 for semiconductor devices of the present invention is as follows Figure 3 As shown in the schematic cross-sectional view of FIG. 1 , the composite copper substrate 1 has a basic structure in which cuprous oxide particles 10 are dispersed in a copper matrix 9. In this case, the characteristic values (thermal expansion coefficient and thermal conductivity) of the composite copper substrate 1 have values between those of the copper matrix 9 and those of the cuprous oxide particles 10 (thermal conductivity: 150 W / mK, thermal expansion coefficient: 10.5 ppm / °C, composition: Cu-50 vol% Cu2O). Figure 7 is a graph showing the relationship between the composition and thermal conductivity of the composite copper substrate 1, Figure 8: is a graph showing the relationship between the composition and thermal expansion coefficient of the composite copper substrate 1. It shows that as the content of the cuprous oxide particles 10 increases, both the thermal conductivity and the thermal expansion coefficient of the composite copper substrate 1 tend to decrease.
[0056] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0057] In this embodiment, cuprous oxide particles 10 are added to the copper matrix of the composite copper substrate 1 to reduce the apparent thermal expansion coefficient increased by the composite material construction, reduce the thermal stress or thermal strain generated by the copper substrate material during production or operation, improve the heat dissipation efficiency, reduce the possibility of deformation, degradation and rupture of various components, and thus increase the service life.
[0058] Embodiment 2
[0059] like Figure 1 As shown in the figure, a COB mirror copper package carrier 1 of this embodiment is characterized in that the composite copper substrate 1 includes: a metal layer 7, the metal layer 7 is included in the composite copper substrate 1; a copper layer 8, the copper layer 8 is included in the metal layer 7, and the thickness of the copper layer 8 is greater than 0.5 μm; a copper matrix 9, the copper matrix 9 is included in the copper layer 8; cuprous oxide particles 10, the cuprous oxide particles 10 are dispersed on the copper matrix 9; a dielectric layer 11, the dielectric layer 11 is arranged on one side of the composite copper substrate 1. A first colloid 21, the first colloid 21 covers the composite copper substrate 1; a mirror aluminum 3, the mirror aluminum 3 covers the first colloid 21; a second colloid 22, the second colloid 22 covers the mirror aluminum 3; a BT board 4, the BT board 4 is located above the second colloid 22; an ink layer 5, the ink 5 is located above the BT board 4; a circuit layer 6, the circuit layer 6 is located above the BT board 4 and is located inside the ink layer 5. The dielectric layer 11 is a resin layer containing dielectric powder 12 composed of dielectric particles with a particle size of 0.02μm to 2μm and copper foil dispersed in a resin composition containing epoxy resin, active ester resin, polyvinyl acetal resin and curing accelerator, and semi-cured, and the thickness is 0.5μm to 25μm.
[0060] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0061] This embodiment provides a composite copper substrate 1 with a dielectric layer 11 arranged on the outside, thereby improving the adhesion between the inner circuit surface of the inner core material and the conductive layer, forming a capacitor circuit layer with a low dielectric constant, and solving the problem that the concentrated electric field environment caused by the relatively high dielectric constant of traditional materials has a negative impact on the electrical performance and stability of the lighting chip, reducing the leakage current of the circuit, reducing the heat generation of the chip, and improving the performance of the chip.
[0062] Embodiment 3
[0063] like Figure 1 As shown, in the COB mirror copper package carrier 1 of this embodiment, the colloid 21, 22 used is a high thermal conductivity colloid, which is the colloid described in patent number JP1997040933A or JP2004210941A.
[0064] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0065] The high thermal conductivity colloid described in patent number JP1997040933A or JP2004210941A adopted in this embodiment has good thermal conductivity, is easy to conduct heat, and can quickly dissipate heat, thereby avoiding a large amount of heat accumulation that affects the normal operation of the chip and shortens the service life of the product, thereby achieving the technical effect of maintaining the normal operation of the product, improving heat dissipation efficiency, and extending the service life of the product.
[0066] Embodiment 4
[0067] like Figure 4 As shown in, this embodiment provides a composition of a dielectric layer 11, including epoxy resin, active ester resin, polyvinyl acetal resin and curing accelerator. Wherein, when the weight of the composition forming the dielectric layer 11 is 100 units, the content of the epoxy resin is preferably in the range of 25 unit weight to 60 unit weight. When the content of the epoxy resin is less than 25 unit weight, the adhesion between the copper foil with the dielectric layer and the dielectric layer, and the adhesion between the dielectric layer and the inner layer circuit. If the content of the epoxy resin exceeds 60 unit weight, it will lose the balance with other resin components, resulting in the deterioration of the dielectric properties as the dielectric layer and the deterioration of the closeness between the dielectric layer and the inner layer circuit.
[0068] The epoxy resin referred to here can be used without any particular problems, as long as it can be used for electrical or electronic material applications. Therefore, various known epoxy resins can be used. For example, bisphenol F type epoxy resin, bisphenol A type epoxy resin, phenol novolac type epoxy resin, o-cresol novolac type epoxy resin, biphenyl type epoxy resin, biphenyl novolac type epoxy resin, trihydroxyphenylmethane type epoxy resin, tetraphenylethane type epoxy resin, their hydride or halide can be used, and they can be used alone or in combination of two or more. Particularly preferred are bisphenol A type epoxy resin, bisphenol F type epoxy resin, bisphenol S type epoxy resin, novolac type epoxy resin, cresol novolac type epoxy resin, alicyclic etc., which have two or more epoxy groups in the molecule. Use one or more mixtures selected from epoxy resin, brominated epoxy resin and glycidylamine type epoxy resin.
[0069] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0070] An appropriate weight ratio of epoxy resin can be used to avoid losing the balance with other resin components, which would lead to deterioration of the dielectric properties of the dielectric layer and deterioration of the adhesion between the dielectric layer and the inner layer circuit. At the same time, the adhesion between the copper foil with the dielectric layer and the dielectric layer, as well as the adhesion between the dielectric layer and the inner layer circuit, is improved to achieve adhesion of the dielectric layer.
[0071] Embodiment 5
[0072] like Figure 4 As shown in , this embodiment provides a composition of a dielectric layer 11, including an epoxy resin, an active ester resin, a polyvinyl acetal resin and a curing accelerator. Among them, when the weight of the composition forming the dielectric layer 11 is 100 units, the content of the active ester resin is preferably in the range of 28 unit weights to 60 unit weights. If the content of the active ester resin is less than 28 unit weights, the curing reaction of the epoxy resin becomes insufficient, resulting in insufficient curing of the epoxy resin. If the content of the active ester resin exceeds 60 unit weights, the curing state of the epoxy resin does not change, and the reaction amount becomes excessive.
[0073] It is known that active ester compounds have linear structures and cyclic structures. However, in the present invention, aromatic active ester compounds having a cyclic structure are preferably used. These active ester compounds are compounds obtained by reacting a compound having a phenolic hydroxyl group with a compound having two or more groups that react with the phenolic hydroxyl group to form an ester bond. As the group formed by the ester bond reaction, for example, a carboxyl group and a haloformyl group (e.g., a chloroformyl group) can be cited.
[0074] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0075] The active ester resin in an appropriate weight ratio can be used to fully react with the epoxy resin to fully cure the epoxy resin without over-reacting.
[0076] Embodiment 6
[0077] like Figure 4 As shown in , this embodiment provides a composition of a dielectric layer 11, including epoxy resin, active ester resin, polyvinyl acetal resin and a curing accelerator. Wherein, when the weight of the composition forming the dielectric layer 11 is 100 units, the total content of the epoxy resin and the active ester resin is 78 to 95 units by weight. If the total content of the epoxy resin and the active ester resin is less than 78 units by weight, the dielectric properties of the formed dielectric layer are deteriorated. If the total content of the epoxy resin and the active ester resin exceeds 95 units by weight, the content of other components such as the polyvinyl acetal resin is small, resulting in poor fluidity of the composition.
[0078] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0079] By using an appropriate weight ratio of epoxy resin and active ester resin, degradation of dielectric properties of the formed dielectric layer can be avoided while ensuring the fluidity of the composition.
[0080] Embodiment 7
[0081] like Figure 4 As shown in , this embodiment provides a composition of a dielectric layer 11, including an epoxy resin, an active ester resin, a polyvinyl acetal resin, and a curing accelerator. Wherein, when the weight of the composition forming the dielectric layer 11 is 100 units, the content of the polyvinyl acetal resin is preferably 1 to 20 units by weight. When the content of the polyvinyl acetal resin is less than 1 unit by weight, it is difficult to ensure the fluidity of the resin. When the content of the polyvinyl acetal resin exceeds 20 units by weight, when the resin varnish is prepared using an organic solvent, the solubility in the organic solvent becomes poor.
[0082] In the present invention, the polyvinyl acetal resin is used to adjust the resin flow of the semi-cured dielectric layer formed by dispersing and mixing the dielectric powder in the resin composition. The polyvinyl acetal resin is obtained by reacting polyvinyl alcohol obtained by hydrolyzing polyvinyl acetate, which is a polymerization reaction product of vinyl acetate, with acetaldehyde or butyraldehyde. As the polyvinyl alcohol mentioned here, a hydrolyzed polymer of a copolymer of vinyl acetate and other vinyl monomers can also be used.
[0083] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0084] By using a polyvinyl acetal resin in an appropriate weight ratio, the solubility in an organic solvent can be maintained while ensuring the fluidity of the resin.
[0085] Embodiment 8
[0086] like Figure 4 As shown in , this embodiment provides a composition of a dielectric layer 11, including epoxy resin, active ester resin, polyvinyl alcohol acetal resin and a curing accelerator. Wherein, when the weight of the composition forming the dielectric layer 11 is 100 units, the content of the curing accelerator is preferably 0.05 to 2 units by weight. If the content of the curing accelerator is less than 0.05 units by weight, relative to the content of the epoxy resin, the curing of the epoxy resin and the active ester resin is insufficient, and the toughness of the cured dielectric layer is not improved. If the curing accelerator exceeds 2 units by weight, the curing reaction of the epoxy resin and the active ester resin is accelerated, and the cured dielectric layer becomes brittle, resulting in a decrease in the strength of the dielectric layer.
[0087] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0088] By using a curing accelerator in an appropriate weight ratio, the epoxy resin and the active ester resin can be fully cured to avoid the dielectric layer becoming brittle after curing, which leads to a decrease in the strength of the dielectric layer.
[0089] The dielectric layer is manufactured according to the material parameter range given in the above embodiments 4 to 8, and its dielectric constant ratio is shown in the following table:
[0090]
[0091]
[0092] Embodiment 9
[0093] like Figure 4 As shown, this embodiment provides a method for manufacturing a COB mirror copper package carrier, comprising the following steps:
[0094] S1: Remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding strength between the copper surface and the photosensitive dry film;
[0095] S2: Paste the photosensitive dry film on the board surface;
[0096] S3: Exposure and development to form a clear circuit pattern on the board to make a circuit layer;
[0097] S4: Remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding force between the copper surface and the ink;
[0098] S5: Scrape and print the ink evenly on the board surface and let it stand for 15 minutes;
[0099] S6: Push the ink into the oven for pre-baking to remove the organic solvent in the ink and partially harden the ink surface;
[0100] S7: Exposure, selectively forming unexposed areas and exposed areas on the ink surface to achieve solder mask phase transfer;
[0101] S8: Development, removing the ink coating on the unexposed area on the plate surface;
[0102] S9: Curing the ink in an oven;
[0103] S10: Paste a film on the back of the board to make it adhesive;
[0104] S11: Copper is plated with metal to prevent oxidation and enhance heat dissipation;
[0105] S12: bonding the copper plate and the mirror aluminum together by high temperature hot pressing;
[0106] S13: placing buffer auxiliary materials, and performing vacuum hot pressing on the pre-bonding to completely bond and solidify the BT and the mirror aluminum;
[0107] S14: Glue protective films on both sides of the laminated back plate to prevent the mirror surface from being scratched and contaminated.
[0108] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0109] The present method can be used to manufacture any carrier board of the above-mentioned embodiments one to three, possessing their advantages and achieving their corresponding technical effects.
[0110] Embodiment 10
[0111] like Figure 4 As shown, this embodiment provides a method for manufacturing a COB mirror copper package carrier, comprising the following steps:
[0112] S1': remove the substrate oxide layer, increase the roughness of the copper surface, and improve the bonding strength between the copper surface and the photosensitive dry film;
[0113] S2': Paste the photosensitive dry film on the board surface;
[0114] S3': Exposure and development to form a clear circuit pattern on the board to make a circuit layer;
[0115] S4': Check the circuit for open and short circuit to ensure electrical safety;
[0116] S5': remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding force between the copper surface and the ink;
[0117] S6': Scrape and print the ink evenly on the board surface and let it stand for 15 minutes;
[0118] S7': push the ink into the oven for pre-baking to remove the organic solvent in the ink and partially harden the ink surface;
[0119] S8': Exposure, selectively forming unexposed areas and exposed areas on the ink surface to achieve solder mask phase transfer;
[0120] S9': Development, removing the ink coating in the unexposed area on the plate surface;
[0121] S10': curing the ink in an oven;
[0122] S11': Paste a film on the back of the board to make it adhesive;
[0123] S12': metallizing the copper to prevent oxidation and enhance heat dissipation;
[0124] S13': bonding the copper plate and the mirror aluminum together by high temperature hot pressing;
[0125] S14': placing buffer auxiliary materials, and performing vacuum hot pressing on the pre-bonding to completely bond and solidify the BT and the mirror aluminum;
[0126] S15': Paste protective film on both sides of the laminated plate to prevent scratches and contamination on the mirror surface.
[0127] The technical solutions in the above embodiments of the present application have at least the following technical effects or advantages:
[0128] Compared with the ninth embodiment, this embodiment adds a new step S4' in the steps. The inspection of the open and short circuits of the lines can verify whether there are any errors in the early production of the product. If there is a short circuit, timely repairs are performed to avoid continuing to process the short-circuited products in the later production steps, resulting in defective and bad products, thereby achieving the technical effect of improving the yield and quality rate.
[0129] Although the preferred embodiments of the present invention have been described, those skilled in the art may make other changes and modifications to these embodiments once they have learned the basic creative concept. Therefore, the appended claims are intended to be interpreted as including the preferred embodiments and all changes and modifications that fall within the scope of the present invention.
[0130] Obviously, those skilled in the art can make various changes and modifications to the present invention without departing from the spirit and scope of the present invention. Thus, if these modifications and variations of the present invention fall within the scope of the claims of the present invention and their equivalents, the present invention is also intended to include these modifications and variations.
Claims
1. A COB mirror copper package carrier, characterized in that: The COB packaging carrier comprises: a composite copper substrate (1), characterized in that the composite copper substrate (1) comprises: A metal layer (7), the metal layer (7) being contained in the composite copper substrate (1); A copper layer (8), the copper layer (8) being contained in the metal layer (7), and having a thickness of 0.5 μm or more; A copper matrix (9), wherein the copper matrix (9) is contained in the copper layer (8); Cuprous oxide particles (10), the cuprous oxide particles (10) being dispersed on the copper matrix (9); A dielectric layer (11), wherein the dielectric layer (11) is arranged on one side of the composite copper substrate (1); A first colloid (21), wherein the first colloid (21) covers the composite copper substrate (1); Mirror aluminum (3), the mirror aluminum (3) covers the first colloid (21); A second colloid (22), wherein the second colloid (22) covers the mirror aluminum (3); A BT board (4), wherein the BT board (4) is located above the second colloid (22); An ink layer (5), wherein the ink (5) is located above the BT board (4); A circuit layer (6), wherein the circuit layer (6) is located above the BT board (4) and inside the ink layer (5).
2. A COB mirror copper package carrier as claimed in claim 1, characterized in that: The colloid used for the first colloid (21) and the second colloid (22) is a high thermal conductive colloid.
3. A COB mirror copper package carrier as claimed in claim 1, characterized in that: The ink layer (5) uses white thermosetting ink.
4. A COB mirror copper package carrier as claimed in claim 1, characterized in that: The metal layer (7) is at least one metal selected from Ni, Sn, Ag, Au, Pt, Pd and Zn, and the thickness of the metal layer (7) is 0.4 to 100 μm.
5. A COB mirror copper package carrier as claimed in claim 1, characterized in that: The dielectric layer (11) is a dielectric powder-containing resin layer obtained by dispersing dielectric powder (12) in a resin composition containing epoxy resin, active ester resin, polyvinyl acetal resin and a curing accelerator and semi-curing the dielectric powder.
6. A COB mirror copper package carrier according to claim 5, characterized in that: The dielectric powder is a powder composed of dielectric particles having a particle size of 0.02 μm to 2 μm and copper foil.
7. The COB mirror copper package carrier according to claim 1, characterized in that: The thickness of the dielectric layer (11) is 0.5 μm to 25 μm.
8. A method for manufacturing a COB mirror copper package carrier, comprising the following steps: S1: Remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding strength between the copper surface and the photosensitive dry film; S2: Paste the photosensitive dry film on the board surface; S3: Exposure and development to form a clear circuit pattern on the board to make a circuit layer; S4: Remove the oxide layer of the substrate, increase the roughness of the copper surface, and improve the bonding force between the copper surface and the ink; S5: Scrape and print the ink evenly on the board surface and let it stand for 15 minutes; S6: Push the ink into the oven for pre-baking to remove the organic solvent in the ink and partially harden the ink surface; S7: Exposure, selectively forming unexposed areas and exposed areas on the ink surface to achieve solder mask phase transfer; S8: Development, removing the ink coating on the unexposed area on the plate surface; S9: Curing the ink in an oven; S10: Paste a film on the back of the board to make it adhesive; S11: Copper is plated with metal to prevent oxidation and enhance heat dissipation; S12: bonding the copper plate and the mirror aluminum together by high temperature hot pressing; S13: placing buffer auxiliary materials, and performing vacuum hot pressing on the pre-bonding to completely bond and solidify the BT and the mirror aluminum; S14: Glue protective films on both sides of the laminated back plate to prevent the mirror surface from being scratched and contaminated.
9. A method for manufacturing a COB mirror copper package carrier as claimed in claim 8, characterized in that: Between S3 and S4, a step can be added: check the circuit open and short circuits through electrical testing or AOI equipment to ensure electrical safety.