Device for verifying characteristics of phase change film and preparation method thereof

Through hard mask fixtures and ICP-RIE etching technology, the preparation process of phase change films is simplified, the problems of complicated processes and conversion failure in the existing technology are solved, and efficient preparation and verification of phase change film characteristics devices are achieved.

CN118984647APending Publication Date: 2024-11-19JIANGSU FREETEL COMM CO LTD +1
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411058221.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-02
Publication Date
2024-11-19

AI Technical Summary

Technical Problem

In the prior art, there are complex processes and prone to failure in the conversion process of phase-changing thin films from crystal to amorphous state, especially when the film thickness is thin, it is difficult for conventional annealing methods to achieve effective conversion.

Method used

Using hard mask fixtures and ICP-RIE etching technology, the phase change material film is deposited through the aligning marking method of large circular holes and small circular through holes, eliminating multiple photolithography alignment and etching processes, and directly forming the characteristics of the phase change film. Device.

Benefits of technology

The process flow is simplified, time and cost are reduced, and the effective preparation and characteristic verification of phase change films is achieved, avoiding film volatility and failure problems.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118984647A_ABST
    Figure CN118984647A_ABST
Patent Text Reader

Abstract

The invention discloses a device for verifying characteristics of a phase change film and a preparation method of the device, and relates to the technical field of phase change material inspection. The preparation method comprises the following steps: pretreating a substrate, and sequentially depositing a Ti film and a Pt film to form a bottom electrode; depositing a dielectric film; photoetching and etching to form a small circular through hole in the dielectric film; depositing a phase change material film in the small circular through hole; sequentially depositing a Ti thin film and a Pt thin film to form an upper electrode; and shielding the upper electrode by using another substrate, and etching the dielectric film at the edge to obtain the device for verifying the characteristics of the phase change film. Pattern deposition of the phase change thin film and the upper electrode is carried out by adopting a hard mask method, the process of multiple times of alignment photoetching is omitted, the process and time cost is reduced, dry etching is carried out by adopting a method of covering with another substrate for finally exposing the bottom electrode, and the technological process of photoetching is omitted. The problem of complicated device preparation process in the prior art is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of phase change material testing, and in particular to a device for verifying phase change film characteristics and a preparation method thereof. Background Art

[0002] Sulfur-based phase change materials have unique properties. They can undergo rapid and reversible transitions between crystalline and amorphous states, and the two states have huge differences in electrical and optical properties. This feature enables them to be used in the fields of optical disks, phase change memories, radio frequency switches, and other fields, and has made important progress in non-volatile memory devices and neuromorphic in-memory computing applications. The switching between the crystalline and amorphous states of phase change materials requires the use of external heating pulses. Depending on the temperature rise and the cooling rate, a crystalline or amorphous phase will be formed. To form an amorphous phase, a DC pulse with a high amplitude and a short time (about 100ns) is required to raise the material temperature to above the melting point temperature Tm and quickly quench (about 100ns), so that these atoms cool into an amorphous solid and lock their high resistance state; to form a crystalline phase, a DC pulse with a slightly higher amplitude and a slightly longer time (μs) is required to keep the material temperature above the crystallization temperature (Tcry) but below the melting point for a period of time (μs), so that the atoms form an orderly periodic arrangement and finally form a low resistance state. Phase-change memory exploits the transition of a material from an amorphous state (with atoms arranged in a disordered manner) to a crystalline state (with atoms tightly packed), which is accompanied by changes in electrical properties, for data storage and retrieval.

[0003] For phase change materials, the crystallization temperature and melting point temperature of the material are the two most concerned temperatures. The transition between the crystalline phase and the amorphous phase is based on these two temperatures. For phase change films, different atomic structure conversions can be achieved under different temperature pulses. In the process of the phase change film changing from amorphous to crystalline, the annealing furnace method can be used to achieve the conversion of the process, and the RT test method can also be used to observe the change of resistance at different temperatures. The crystallization temperature of the phase change film can also be obtained, that is, the temperature point at which the resistance drops rapidly. However, the same method is used to make the phase change material realize the conversion from crystalline to amorphous, which is very difficult. When the temperature is too high, the conventional annealing method lasts for a long time, and the thickness of the film is very thin, and volatilization often occurs, and the re-conversion from crystalline to amorphous cannot be achieved. To achieve this process, it is necessary to use micro-nano processing methods to prepare phase change devices, such as sandwich structures to achieve phase change conversion. However, there are many thin film materials designed for phase change devices, which need to be realized through multiple photolithography alignment and etching methods. The process is complicated and prone to failure. Summary of the invention

[0004] In order to solve the above technical problems, the purpose of the present invention is to provide a device for verifying the characteristics of a phase change thin film and a method for preparing the same, so as to solve the problem of complicated device preparation process in the prior art.

[0005] The technical solution of the present invention to solve the above technical problem is as follows: a method for preparing a device for verifying the characteristics of a phase change thin film is provided, which comprises the following steps in sequence:

[0006] S1: Pt / Ti metal film: pre-treat the substrate, deposit Ti film and Pt film in sequence to form a bottom electrode;

[0007] S2: dielectric film: depositing a dielectric film on the bottom electrode obtained in step S1;

[0008] S3: forming small round through holes: coating the surface of the dielectric film obtained in step S2 with photoresist, then performing photolithography to form a photoresist small round hole pattern, then performing etching, and finally removing the photoresist, that is, forming small round through holes in the dielectric film;

[0009] S4: Phase change material film: a hard mask fixture is covered on the dielectric film obtained in step S3, so that the large circular hole on the hard mask fixture can overlap with the small circular through hole in step S3, and then a phase change material film is deposited in the small circular through hole in step S3 through the large circular hole;

[0010] S5: Pt / Ti metal film: a Ti film and a Pt film are sequentially deposited on the phase change material film obtained in step S4 to form an upper electrode;

[0011] S6: Removing the edge: using another substrate to cover the upper electrode obtained in step S5, etching and removing the dielectric film at the edge, and obtaining a device for verifying the characteristics of the phase change film.

[0012] On the basis of the above technical solution, the present invention can also be improved as follows:

[0013] Furthermore, in step S1, the material of the substrate is high-resistance silicon, glass, sapphire or is made by depositing an insulating film on a silicon wafer.

[0014] Furthermore, the insulating layer film material is SiO2 or Si3N4.

[0015] Furthermore, in step S1, the substrate is cleaned with acetone, alcohol and deionized water in sequence, and then baked at 110-130° C. to complete the substrate pretreatment process.

[0016] Further, the mixture was baked at 120°C.

[0017] Furthermore, in step S1, magnetron sputtering is used for deposition.

[0018] Furthermore, in step S1, the thickness of the Ti film is 18-22 nm.

[0019] Furthermore, in step S1, the thickness of the Ti film is 20 nm.

[0020] Furthermore, in step S1, the thickness of the Pt film is 110-130 nm.

[0021] Furthermore, in step S1, the thickness of the Pt film is 120 nm.

[0022] Furthermore, in step S2, the material of the dielectric film is Si3N4, SiO2, or AlN.

[0023] Further, in step S2, the material of the dielectric film is Si3N4.

[0024] Furthermore, in step S2, PECVD is used to deposit the dielectric film.

[0025] Further, in step S3, the photoresist is AZ6112.

[0026] Further, in step S3, ICP-RIE is used for etching.

[0027] Furthermore, the gas used in ICP-RIE is CH4 or SF6.

[0028] Further, in step S3, the diameter of the small round through hole is 6-10 μm.

[0029] Furthermore, in step S3, a concave first alignment mark discernible to the naked eye is simultaneously formed on the surface of the dielectric film by photolithography and etching.

[0030] Further, in step S4, the material of the phase change material film is Ge2Sb2Te5.

[0031] Further, in step S4, magnetron sputtering is used for deposition.

[0032] Further, in step S4, a large circular hole and a second alignment mark are provided on the hard mask fixture, and both the large circular hole and the second alignment mark are through holes.

[0033] Furthermore, the diameter of the large circular hole is larger than the diameter of the small circular through hole.

[0034] Furthermore, the diameter of the large circular hole is 1-5 mm.

[0035] Furthermore, in step S4, the second alignment mark on the hard mask fixture can be aligned with the concave first alignment mark in step S3 by naked eyes to achieve the overlap of the large circular hole and the small circular through hole.

[0036] The beneficial effects of adopting the above further technical solution are: the method of using the alignment mark for visual alignment does not require the use of photolithography alignment, thus eliminating the photolithography and etching process of the middle two layers of film, saving time and cost.

[0037] Furthermore, in step S5, the method and thickness of depositing the Ti film and the Pt film are the same as those in step S1.

[0038] Further, in step S6, ICP-RIE is used for etching.

[0039] The present invention also provides a device for verifying the characteristics of a phase-change thin film, which is prepared by the method.

[0040] The present invention also provides application of the device in phase change film property verification.

[0041] The present invention has the following beneficial effects:

[0042] Compared with the sandwich structure preparation process, the present invention adopts a hard mask method to carry out the pattern deposition of the phase change film and the upper electrode, eliminating the process of multiple alignment photolithography processes, reducing the process and time costs, and finally the method of exposing the bottom electrode uses another substrate covering method to perform dry etching, eliminating the photolithography process. BRIEF DESCRIPTION OF THE DRAWINGS

[0043] Figure 1 It is a schematic diagram of the cross-sectional structure of the device of the present invention;

[0044] Figure 2 It is a schematic diagram of the planar structure of the device of the present invention;

[0045] Figure 3 is a schematic diagram of a hard mask fixture;

[0046] Figure 4 Schematic diagram of etching the edge of the sample;

[0047] Figure 5 This is a test result diagram of the device of the present invention.

[0048] Among them, 1, substrate; 2, bottom electrode; 3, dielectric film; 4, phase change material film; 5, upper electrode; 6, first alignment mark; 7, second alignment mark; 8, large circular hole; 9, another substrate; DETAILED DESCRIPTION

[0049] The principles and features of the present invention are described below in conjunction with the accompanying drawings. The examples are only used to explain the present invention and are not used to limit the scope of the present invention. If specific conditions are not specified in the embodiments, they are carried out according to normal conditions or conditions recommended by the manufacturer. If the manufacturer is not specified for the reagents or instruments used, they are all conventional products that can be purchased commercially.

[0050] The substrate 1 and the bottom electrode 2 are used to transmit electrical signals; the dielectric film 3 is used to isolate the upper and lower electrodes; the phase change material film 4 is used as the main functional material; and the upper electrode 5 is used to transmit electrical signals.

[0051] Embodiment 1:

[0052] A device for verifying the characteristics of phase change thin films (see Figure 1-2 ), the preparation method thereof comprises the following steps in sequence:

[0053] S1: Pt / Ti metal film: The substrate 1 (high-resistance silicon) was cleaned with acetone, alcohol and deionized water in turn to remove grease and other organic impurities on the substrate 1, and then baked at 120°C to remove the water vapor during the cleaning process to obtain the pre-treated substrate 1, which was placed in a magnetron sputtering device and the back vacuum was evacuated to 5×10 -4 Pa, Ti film (thickness 20nm) and Pt film (thickness 120nm) are deposited in sequence, the Ti film serves as an adhesion layer, and the Pt film forms the bottom electrode 2;

[0054] S2: dielectric film 3: using PECVD (plasma enhanced chemical vapor deposition) to deposit dielectric film 3 (Si3N4) on the bottom electrode 2 obtained in step S1;

[0055] S3: Forming small round through holes: After baking the dielectric film 3 obtained in step S2 at 120°C for 5 minutes, place it on a spin coating device and drip it with positive photoresist AZ6112, then slowly rotate it for 10 seconds at a speed of 1000 rad / s, and then quickly rotate it for 30 seconds at a speed of 3000 rad / s, so that the photoresist is evenly coated on the surface of the dielectric film 3; cover it with a mask (the mask has an array of small round hole patterns and a first alignment mark 6 pattern), and then perform photolithography with an exposure time of 6 seconds. After exposure, the developer is placed in the developer for about 45 seconds, and then a microscope is used for examination. After confirming that the photolithography is completed, the film is hardened at 120°C to form a photoresist small circular hole pattern and a first alignment mark 6 pattern, and then ICP-RIE (inductively coupled plasma-reactive ion etching) is used for etching. The gas used for ICP-RIE dry etching is CH4. Finally, the photoresist is removed, that is, a small circular through hole (with a diameter of 8 μm) and a concave first alignment mark 6 that can be distinguished by the naked eye are formed in the dielectric film 3;

[0056] S4: Phase change material film 4: Cover the dielectric film 3 obtained in step S3 with a hard mask fixture (see Figure 3, the hard mask fixture is provided with an array of large circular holes 8 and a second alignment mark 7, both of which are through holes, the diameter of the large circular hole 8 is 3 mm, and the size of the second alignment mark 7 is 2×4 mm), the second alignment mark 7 on the hard mask fixture can be aligned with the concave first alignment mark 6 in step S3 by naked eyes, so that the large circular holes 8 covering the hard mask fixture can overlap with the small circular through holes in step S3, and after being fixed with high-temperature tape, a phase change material film 4 (Ge2Sb2Te5) is deposited in the small circular through holes in step S3 through the large circular holes 8 by magnetron sputtering;

[0057] S5: Pt / Ti metal film: a Ti film and a Pt film are sequentially deposited on the phase change material film 4 obtained in step S4, the method and thickness are the same as in step S1, to form an upper electrode 5;

[0058] S6: Remove the edge: remove the covering hard mask fixture, and use another substrate 9 to cover the upper electrode 5 (see Figure 4 ), protect the layers of film in the center area from being etched, fix them with tape, and then use ICP-RIE to etch and remove the dielectric film 3 at the edge. The sample after dry etching can expose the bottom electrode 2, so that an electrical signal can be applied to the upper electrode 5 and the bottom electrode 2 to test the phase change characteristics of the phase change film, thereby obtaining a device for verifying the characteristics of the phase change film.

[0059] Embodiment 2:

[0060] A device for verifying the characteristics of a phase change thin film, the preparation method of which comprises the following steps in sequence:

[0061] S1: Pt / Ti metal film: The substrate 1 (glass) was cleaned with acetone, alcohol and deionized water in turn to remove grease and other organic impurities on the substrate 1, and then baked at 110°C to remove water vapor during the cleaning process to obtain a pre-treated substrate 1, which was placed in a magnetron sputtering device and the back vacuum was evacuated to 5×10 -4 Pa, Ti film (thickness 18nm) and Pt film (thickness 110nm) are deposited in sequence, the Ti film serves as an adhesion layer, and the Pt film forms the bottom electrode 2;

[0062] S2: dielectric film 3: a dielectric film 3 (SiO2) is deposited on the bottom electrode 2 obtained in step S1 by PECVD (plasma enhanced chemical vapor deposition);

[0063] S3: Forming small round through holes: After baking the dielectric film 3 obtained in step S2 at 120°C for 5 minutes, place it on a spin coating device and drip it with positive photoresist AZ6112, then slowly rotate it for 10 seconds at a speed of 1000 rad / s, and then quickly rotate it for 30 seconds at a speed of 3000 rad / s, so that the photoresist is evenly coated on the surface of the dielectric film 3; cover it with a mask (the mask has an array of small round hole patterns and a first alignment mark 6 pattern), and then perform photolithography with an exposure time of 6 seconds. After exposure, the developer is placed in the developer for about 45 seconds, and then a microscope is used for examination. After confirming that the photolithography is completed, the film is hardened at 120°C to form a photoresist small circular hole pattern and a first alignment mark 6 pattern, and then ICP-RIE (inductively coupled plasma-reactive ion etching) is used for etching. The gas used for ICP-RIE dry etching is SF6. Finally, the photoresist is removed, that is, a small circular through hole (with a diameter of 6 μm) and a concave first alignment mark 6 that can be distinguished by the naked eye are formed in the dielectric film 3;

[0064] S4: Phase change material film 4: A hard mask fixture is covered on the dielectric film 3 obtained in step S3 (the hard mask fixture is provided with an array of large circular holes 8 and a second alignment mark 7, both of which are through holes, the diameter of the large circular hole 8 is 1 mm, and the size of the second alignment mark 7 is 2×4 mm), the second alignment mark 7 on the hard mask fixture can be aligned with the concave first alignment mark 6 in step S3 by naked eyes, so that the large circular hole 8 on the hard mask fixture can overlap with the small circular through hole in step S3, and after being fixed with high-temperature tape, a phase change material film 4 (Ge2Sb2Te5) is deposited in the small circular through hole in step S3 through the large circular hole 8 by magnetron sputtering;

[0065] S5: Pt / Ti metal film: a Ti film and a Pt film are sequentially deposited on the phase change material film 4 obtained in step S4, the method and thickness are the same as in step S1, to form an upper electrode 5;

[0066] S6: Remove the edge: remove the covering hard mask fixture, use another substrate 9 to cover the upper electrode 5 to protect the layers of film in the central area from being etched, fix it with tape, and use ICP-RIE to etch and remove the dielectric film 3 at the edge. The sample after dry etching can expose the bottom electrode 2, so that an electrical signal can be applied to the upper electrode 5 and the bottom electrode 2 to test the phase change characteristics of the phase change film, and obtain a device for verifying the characteristics of the phase change film.

[0067] Embodiment 3:

[0068] A device for verifying the characteristics of a phase change thin film, the preparation method of which comprises the following steps in sequence:

[0069] S1: Pt / Ti metal film: The substrate 1 (sapphire) was cleaned with acetone, alcohol and deionized water in turn to remove grease and other organic impurities on the substrate 1, and then baked at 130°C to remove the water vapor during the cleaning process. The pre-treated substrate 1 was placed in a magnetron sputtering device and the back vacuum was evacuated to 5×10 -4 Pa, Ti film (thickness 22nm) and Pt film (thickness 130nm) are deposited in sequence, the Ti film serves as an adhesion layer, and the Pt film forms the bottom electrode 2;

[0070] S2: dielectric film 3: a dielectric film 3 (AlN) is deposited on the bottom electrode 2 obtained in step S1 by PECVD (plasma enhanced chemical vapor deposition);

[0071] S3: Forming small round through holes: After baking the dielectric film 3 obtained in step S2 at 120°C for 5 minutes, place it on a spin coating device and drip it with positive photoresist AZ6112, then slowly rotate it for 10 seconds at a speed of 1000 rad / s, and then quickly rotate it for 30 seconds at a speed of 3000 rad / s, so that the photoresist is evenly coated on the surface of the dielectric film 3; cover it with a mask (the mask has an array of small round hole patterns and a first alignment mark 6 pattern), and then perform photolithography with an exposure time of 6 seconds. After exposure, the developer is placed in the developer for about 45 seconds, and then a microscope is used for examination. After confirming that the photolithography is completed, the film is hardened at 120°C to form a photoresist small circular hole pattern and a first alignment mark 6 pattern, and then ICP-RIE (inductively coupled plasma-reactive ion etching) is used for etching. The gas used for ICP-RIE dry etching is CH4. Finally, the photoresist is removed, that is, a small circular through hole (with a diameter of 10 μm) and a concave first alignment mark 6 that can be distinguished by the naked eye are formed in the dielectric film 3;

[0072] S4: Phase change material film 4: A hard mask fixture is covered on the dielectric film 3 obtained in step S3 (the hard mask fixture is provided with an array of large circular holes 8 and a second alignment mark 7, both of which are through holes, the diameter of the large circular hole 8 is 5 mm, and the size of the second alignment mark 7 is 2×4 mm), the second alignment mark 7 on the hard mask fixture can be aligned with the concave first alignment mark 6 in step S3 by naked eyes, so that the large circular hole 8 on the hard mask fixture can overlap with the small circular through hole in step S3, after being fixed with high-temperature tape, the phase change material film 4 (Ge2Sb2Te5) is deposited in the small circular through hole in step S3 through the large circular hole 8 by magnetron sputtering;

[0073] S5: Pt / Ti metal film: a Ti film and a Pt film are sequentially deposited on the phase change material film 4 obtained in step S4, the method and thickness are the same as in step S1, to form an upper electrode 5;

[0074] S6: Remove the edge: remove the covering hard mask fixture, use another substrate 9 to cover the upper electrode 5 to protect the layers of film in the central area from being etched, fix it with tape, and use ICP-RIE to etch and remove the dielectric film 3 at the edge. The sample after dry etching can expose the bottom electrode 2, so that an electrical signal can be applied to the upper electrode 5 and the bottom electrode 2 to test the phase change characteristics of the phase change film, and obtain a device for verifying the characteristics of the phase change film.

[0075] Test example

[0076] 1. Testing the phase change characteristics of Ge2Sb2Te5

[0077] The device for verifying the characteristics of the phase change film prepared in Example 1 was tested. The specific testing method is as follows: when a voltage pulse signal is applied to the upper electrode 5 and the bottom electrode 2 using a probe, two characteristics of a high resistance state and a low resistance state can be obtained. The results are shown in FIG. Figure 5 .

[0078] Depend on Figure 5 It can be seen that 300 tests can be carried out under a specific pulse voltage without failure. Therefore, it can be determined that the Ge2Sb2Te5 film deposited in Example 1 has phase change properties and can be used as a phase change film for a phase change device in the future.

[0079] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for preparing a phase change thin film device for verifying its characteristics, characterized in that: The following steps are included in sequence: S1: Pt / Ti metal film: pre-treat the substrate (1), deposit a Ti film and a Pt film in sequence to form a bottom electrode (2); S2: dielectric film (3): depositing a dielectric film (3) on the bottom electrode (2) obtained in step S1; S3: forming small circular through holes: coating the surface of the dielectric film (3) obtained in step S2 with photoresist, then performing photolithography to form a photoresist small circular hole pattern, then performing etching, and finally removing the photoresist, i.e. forming small circular through holes in the dielectric film (3); S4: Phase change material film (4): Cover the dielectric film (3) obtained in step S3 with a hard mask fixture, so that the large circular hole (8) on the hard mask fixture can overlap with the small circular through hole in step S3, and then deposit the phase change material film (4) in the small circular through hole in step S3 through the large circular hole (8); S5: Pt / Ti metal film: a Ti film and a Pt film are sequentially deposited on the phase change material film (4) obtained in step S4 to form an upper electrode (5); S6: removing the edge: using another substrate (9) to cover the upper electrode (5) obtained in step S5, etching and removing the dielectric film (3) at the edge, thereby obtaining a device for verifying the characteristics of the phase change film.

2. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S1, the material of the substrate (1) is high-resistance silicon, glass or sapphire.

3. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S1, the substrate (1) is cleaned with acetone, alcohol and deionized water in sequence, and then baked at 110-130° C. to complete the pretreatment process of the substrate (1).

4. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S1, magnetron sputtering is used for deposition.

5. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S2, the material of the dielectric film (3) is Si3N4, SiO2, or AlN.

6. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S3, the photoresist is AZ6112.

7. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S3, ICP-RIE is used for etching.

8. The method for preparing a phase change thin film characteristic device according to claim 1, characterized in that: In step S4, the material of the phase change material film (4) is Ge2Sb2Te5.

9. A device for verifying the characteristics of a phase-change thin film, prepared by the method for preparing a device for verifying the characteristics of a phase-change thin film according to any one of claims 1 to 8.

10. Application of the device for verifying the characteristics of a phase change thin film as claimed in claim 9 in verifying the characteristics of a phase change thin film.