Double-crosslinking structured emulsion gel as well as preparation method and application thereof

Through dual crosslinked structured emulsion gel technology, the combination of modified pea protein isolate and sodium alginate is used to solve the problems of poor water solubility and gel instability of plant essential oils, and efficient packaging and release of flavor substances is achieved. , suitable for a variety of application fields.

CN118985880APending Publication Date: 2024-11-22NORTHWEST A & F UNIV
View PDF 0 Cites 1 Cited by

Patent Information

Application Number
CN202411109919.4
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-13
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the prior art, poor water solubility and sensitivity to the external environment limit their application, and the functional properties of protein-based gels prepared by traditional single cross-linking methods are unstable, making it difficult to effectively regulate the release of hydrophobic flavor substances.

Method used

Using a dual crosslinked structured emulsion gel preparation method, modified pea protein isolate is combined with sodium alginate, and added glutamine transaminase and Ca2+ for curing treatment to form a gel with high hardness, chew resistance and water-retaining power. , and the flavour release characteristics of the gel are adjusted using electron beam irradiation modification technology.

Benefits of technology

It realizes efficient packaging and stable release of hydrophobic flavor substances, provides higher hardness, viscoelasticity and freeze-thaw stability, is suitable for different application needs, and is green and environmentally friendly, with high safety. It is suitable for food, medicine and cosmetics. field.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118985880A_ABST
    Figure CN118985880A_ABST
Patent Text Reader

Abstract

The invention discloses double-crosslinking structured emulsion gel as well as a preparation method and application thereof. The preparation method comprises the following steps: mixing a modified pea protein isolate dispersion liquid with an oil phase, carrying out high-speed shearing treatment to form an oil-in-water emulsion, then adding a sodium alginate dispersion liquid, and carrying out homogenization treatment to prepare a layer-by-layer assembled emulsion; or mixing the modified pea protein isolate dispersion liquid with a sodium alginate dispersion liquid for reaction to form a compound, then adding an oil phase, and performing shearing and homogenizing treatment to prepare a compound emulsion; and adding glutamine transaminase and Ca < 2 + > into the layer-by-layer assembled emulsion or the compound emulsion, and carrying out curing treatment, so as to prepare the double-crosslinking structured emulsion gel. The emulsion gel prepared by the invention has proper hardness and chewiness, good viscoelasticity and water holding capacity, can be used for designing food with good texture characteristics, and can be used for efficiently packaging and effectively releasing hydrophobic flavor substances.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of food processing, and in particular relates to a double-crosslinked structured emulsion gel and a preparation method and application thereof. Background Art

[0002] Plant essential oils contain a variety of bioactive compounds and have a special flavor, which can be used as natural flavors with health benefits. However, plant essential oils have poor water solubility, are sensitive to external environmental factors, and are prone to degradation, which limits their application in actual production. At present, emulsion gels are widely used to embed fat-soluble components, so that the active substances therein are well protected and their chemical stability is improved. In addition, the oil-water interface layer and the continuous matrix network provide a physical barrier for flavor release, and the release of flavor substances can be more accurately regulated by adjusting the emulsion and the continuous phase of the matrix.

[0003] Protein gels have attracted extensive attention from various industries and researchers due to their excellent properties. However, the growing demand for animal protein will lead to an increase in greenhouse gas emissions, which will put heavy pressure on the environment. Therefore, the use of plant protein instead of animal protein has become an economical and environmentally friendly necessary choice. In recent years, pea protein isolate has become the focus of plant protein development due to its low allergenicity, non-GMO safety, relatively balanced amino acid structure, easy digestibility and environmental friendliness. The use of protein non-thermal modification technology, such as pH shift, ultrasonic treatment, ball milling, and electron beam irradiation, can change the structure of the protein, thereby affecting the physicochemical properties and flavor release of protein-based emulsion gels. The oil-water interface is an important component of the emulsion-related carrier. The structure and composition of the emulsifier molecules will change the thickness and structure of the interface layer, affect the stability of the emulsion, and then affect the release characteristics of flavor substances in the oil phase.

[0004] Protein gels can be formed by heat coagulation or cold coagulation. Compared with traditional heat coagulation gels, cold coagulation gels have many superior properties and are more suitable for embedding heat-sensitive chemicals that are easily degraded. Common methods for preparing cold coagulation protein emulsion gels include acidification of glucose-δ-lactone, addition of divalent salts (such as Ca 2+ ) and glutamine transaminase (TG enzyme) crosslinking. However, the functional properties of gels prepared by traditional single crosslinking methods are usually limited, and protein-based gel systems are usually unstable. Therefore, the development of a pea protein isolate-based double-crosslinked structured emulsion gel with good physical properties and the ability to effectively regulate the release of hydrophobic flavor substances meets people's needs for green, healthy and good sensory experience, and has important application value. Summary of the invention

[0005] The main purpose of the present invention is to provide a double-crosslinked structured emulsion gel and a preparation method and application thereof, so as to overcome the deficiencies of the prior art.

[0006] In order to achieve the above-mentioned invention object, the technical solution adopted by the present invention includes:

[0007] The embodiment of the present invention provides a method for preparing a double-crosslinked structured emulsion gel, which comprises:

[0008] Providing a modified pea protein isolate dispersion, a sodium alginate dispersion and an oil phase; wherein the oil phase comprises plant essential oil and edible oil;

[0009] The modified pea protein isolate dispersion is mixed with an oil phase and subjected to high-speed shearing treatment to form an oil-in-water (O / W) emulsion, and then a sodium alginate dispersion is added and homogenized to obtain a layer-by-layer assembly emulsion; or, the modified pea protein isolate dispersion is mixed with a sodium alginate dispersion to form a complex, and then an oil phase is added and subjected to shearing and homogenization treatment to obtain a complex emulsion;

[0010] And, glutamine aminotransferase, Ca 2+ The double cross-linked structured emulsion gel is prepared by adding the emulsion into the layer-by-layer assembly emulsion or the composite emulsion and performing a curing treatment.

[0011] The embodiment of the present invention also provides a double-crosslinked structured emulsion gel prepared by the aforementioned preparation method.

[0012] The embodiment of the present invention also provides the use of the aforementioned double-crosslinked structured emulsion gel in the field of preparing food, medicine or cosmetics.

[0013] Compared with the prior art, the present invention has the following beneficial effects:

[0014] (1) Glutamine transaminase and Ca in the present invention 2+ The double-crosslinked latex gel was prepared by combined induction. Compared with the single-crosslinked latex gel, it has higher hardness, stronger chewiness, and good viscoelasticity, water holding capacity and freeze-thaw stability.

[0015] (2) The pea protein isolate in the present invention is modified by electron beam irradiation, and the formed emulsion gel is softer, has less viscoelasticity, and has better water holding capacity and freeze-thaw stability;

[0016] (3) The present invention uses sodium alginate as a texture modifier to prepare emulsions with different interface structures, thereby improving the hardness, chewing resistance, viscoelasticity and water holding capacity of the essential oil emulsion gel;

[0017] (4) The present invention utilizes electron beam irradiation modification technology and emulsion interface structure design to prepare double-crosslinked structured essential oil emulsion gels with different properties, and their flavor release characteristics are significantly different, which helps to rationally construct a gel system with appropriate texture according to specific application conditions, thereby obtaining products with different properties that meet the needs of different consumers;

[0018] (5) The preparation process provided by the present invention is green and environmentally friendly, easy to operate, and has mild reaction conditions. The prepared emulsion gel is highly safe, nutritious, and has good stability;

[0019] (6) The present invention realizes the high-value application of pea protein isolate, as well as the efficient encapsulation and effective release of hydrophobic flavor substances, and has broad application prospects in the fields of food, medicine, and cosmetics preparation. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments recorded in the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.

[0021] Figure 1 It is a hardness diagram of the emulsion gels with three different cross-linking modes in Example 1 of the present invention; different capital letters indicate that there are significant differences between the natural PPI emulsion gel samples (p<0.05), and different lowercase letters indicate that there are significant differences between the modified PPI emulsion gel samples (p<0.05);

[0022] Figure 2a-2c The texture characteristics of the emulsion gels with three different cross-linking modes in Example 1 of the present invention in the puncture test are shown in FIG. Figure 2a The force-time curve of natural PPI emulsion gel. Figure 2b is the force-time curve of the modified PPI emulsion gel. Figure 2c It is the strength diagram of the emulsion gel; different capital letters indicate that there are significant differences between the natural PPI emulsion gel samples (p<0.05), and different lowercase letters indicate that there are significant differences between the modified PPI emulsion gel samples (p<0.05);

[0023] Figure 3a-3f Graph showing the rheological properties of three different crosslinking methods of the latex gel in Example 1 of the present invention; Figure 3a-Figure 3b G′ frequency scanning curve of natural and modified PPI emulsion gel, Figure 3c-3d G″ frequency scanning curve of natural and modified PPI emulsion gel, Figure 3e-3fFlow scanning images representing natural and modified PPI emulsion gels, where the bar graphs are the apparent viscosities at a shear rate of 0.1 / s;

[0024] Figure 4 It is a water retention graph of three kinds of emulsion gels with different cross-linking modes in Example 1 of the present invention; different capital letters indicate that there are significant differences between natural PPI emulsion gel samples (p<0.05), and different lowercase letters indicate that there are significant differences between modified PPI emulsion gel samples (p<0.05);

[0025] Figure 5a-Figure 5b The natural ( Figure 5a ) and modified ( Figure 5b ) of PPI treated with different cross-linking agents to obtain the freeze-thaw stability of the emulsion gel;

[0026] Figure 6a-6c is the ζ-potential of the single PPI emulsion, PPI-SA composite emulsion and layer-by-layer assembly emulsion of the present invention ( Figure 6a )、Particle size( Figure 6b ) and particle size distribution diagram ( Figure 6c ); Different lowercase letters indicate significant differences among essential oil emulsion samples (p<0.05);

[0027] Figure 7a-7e The time-force curves of the emulsion gels in Examples 2 to 3 of the present invention and Comparative Examples 1 to 4 ( Figure 7a ),hardness( Figure 7b ), cohesion ( Figure 7c ), chewiness( Figure 7d ) and resiliency ( Figure 7e ) Figure; Different lowercase English letters represent significant differences among different emulsion gel samples (p<0.05);

[0028] Figure 8a-8d The frequency scanning of the emulsion gel in Examples 2 to 3 of the present invention and Comparative Examples 1 to 4 ( Figure 8a )、Flow Scan( Figure 8b ), apparent viscosity ( Figure 8c ) and shear stress ( Figure 8d )picture;

[0029] Fig. 9 The water holding capacity diagram of the emulsion gel in Examples 2 to 3 of the present invention and Comparative Examples 1 to 4; different lowercase English letters represent significant differences between different emulsion gel samples (p<0.05);

[0030] Figure 10a-Figure 10b The electronic nose sensor response radar diagram of the peppermint essential oil emulsion gel in Examples 2 to 3 of the present invention and Comparative Examples 1 to 4 ( Fig.10a ) and principal component analysis plots ( Fig.10b );

[0031] Fig.11 It is a cumulative release rate diagram of the double cross-linked PPI-SA complex emulsion gel (Example 3 and Comparative Example 4) and the layer-by-layer assembled emulsion gel (Example 2 and Comparative Example 3) formed by the natural and modified PPI in the present invention;

[0032] Figure 12a-12b The gas chromatography-mass spectrometry of the natural PPI-SA complex emulsion gel in Comparative Example 4 of the present invention is shown in FIG. Fig.12a ) and the gas chromatography-mass spectrometry of the modified PPI-SA composite emulsion gel in Example 3 ( Figure 12b );

[0033] Fig.13 The figure is a schematic diagram of the preparation process of a double cross-linked structured emulsion gel based on modified pea protein isolate in a typical embodiment of the present invention. DETAILED DESCRIPTION

[0034] In view of the defects of the prior art, the inventor of this case has proposed the technical solution of the present invention after long-term research and extensive practice. The technical solution of the present invention will be described clearly and completely below. Obviously, the described embodiments are part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0035] Specifically, as one aspect of the technical solution of the present invention, a method for preparing a double-crosslinked structured emulsion gel involves:

[0036] Providing a modified pea protein isolate (modified PPI) dispersion, a sodium alginate (SA) dispersion and an oil phase; wherein the oil phase comprises plant essential oil and edible oil;

[0037] The modified pea protein isolate dispersion is mixed with an oil phase and subjected to high-speed shearing treatment to form an oil-in-water (O / W) emulsion, and then a sodium alginate dispersion is added and homogenized to obtain a layer-by-layer assembly emulsion; or, the modified pea protein isolate dispersion is mixed with a sodium alginate dispersion to form a complex, and then an oil phase is added and subjected to shearing and homogenization treatment to obtain a complex emulsion;

[0038] And, glutamine transaminase (TG enzyme), Ca 2+ The double cross-linked structured emulsion gel is prepared by adding the emulsion into the layer-by-layer assembly emulsion or the composite emulsion and performing a curing treatment.

[0039] In some preferred embodiments, the protein in the modified pea protein isolate dispersion is obtained by electron beam irradiation (EBI) at a dose of 10 to 20 kGy.

[0040] In some preferred embodiments, the protein content in the modified pea protein isolate dispersion is 8-12 wt %.

[0041] In some preferred embodiments, the content of sodium alginate in the sodium alginate dispersion is 1-3 wt %.

[0042] In some preferred embodiments, the plant essential oil includes any one or more combinations of peppermint essential oil, thyme essential oil, and cinnamon essential oil, but is not limited thereto.

[0043] In some preferred embodiments, the edible oil includes any one or more combinations of medium chain triglycerides, corn oil, soybean oil, and rapeseed oil, but is not limited thereto.

[0044] In some preferred embodiments, the volume ratio of plant essential oil to edible oil in the oil phase is 10:1 to 1:2.

[0045] In some preferred embodiments, the preparation method specifically comprises:

[0046] The modified pea protein isolate dispersion is heated in a water bath at 80-90° C. for 25-35 minutes and rapidly cooled to room temperature, and the obtained modified pea protein isolate dispersion is homogenized at 9000-11000 rpm for 1-3 minutes, and then the oil phase is added and homogenized at 11000-13000 rpm for 1-3 minutes to form an O / W emulsion;

[0047] and adding a sodium alginate dispersion to the O / W emulsion and homogenizing it with a high-pressure homogenizer to obtain a layer-by-layer assembly emulsion; wherein the homogenization conditions include: fixed circulation at 45-55 MPa for three times;

[0048] Furthermore, the volume content of the oil phase in the layer-by-layer assembly emulsion is 15-25%.

[0049] In some preferred embodiments, the preparation method specifically comprises:

[0050] The modified pea protein isolate dispersion and the sodium alginate dispersion are mixed in equal volumes and stirred for 4 to 6 hours, then heated in a water bath at 80 to 90° C. for 25 to 35 minutes and rapidly cooled to room temperature to form a complex solution;

[0051] And, the composite solution is homogenized at 9000-11000 rpm for 1-3 min, then the oil phase is added and homogenized at 11000-13000 rpm for 1-3 min, and then homogenized by a high-pressure homogenizer to obtain a composite emulsion; wherein the homogenization conditions include: fixed circulation at 45-55 MPa for three times;

[0052] Furthermore, the volume content of the oil phase in the composite emulsion is 15-25%.

[0053] In some preferred embodiments, the preparation method specifically comprises: 2+ The mixture is added into the layer-by-layer assembly emulsion or the composite emulsion to form a mixed system, and then quickly vortexed to mix evenly. After incubation in a water bath, the mixture is stored overnight to form a double-crosslinked structured emulsion gel.

[0054] Furthermore, the mass ratio of the glutamine aminotransferase to the modified pea protein isolate is 35-45 U / g.

[0055] Furthermore, in the mixed system, Ca 2+ The concentration is 20~100mmol / L.

[0056] Furthermore, the conditions for the water bath incubation include: a temperature of 45 to 55° C. and a time of 50 to 70 minutes.

[0057] Furthermore, the temperature for overnight storage is 2-5°C.

[0058] In some more specific embodiments, the method for preparing the double cross-linked structured emulsion gel comprises the following steps:

[0059] S1. Dissolve modified pea protein isolate (PPI) powder in deionized water, stir at room temperature, and stand overnight to obtain a PPI dispersion; prepare a sodium alginate (SA) solution; and prepare an oil phase. Prepare an oil-in-water emulsion as follows:

[0060] Layer-by-layer assembly emulsion: The PPI dispersion is heated in a water bath for a certain period of time, rapidly cooled to room temperature, subjected to high-speed shear treatment of the PPI dispersion, and the oil phase is added to form a primary emulsion (i.e., O / W emulsion) after high-speed shear treatment, and then the SA dispersion is added, followed by homogenization treatment with a high-pressure homogenizer to form a layer-by-layer assembly emulsion.

[0061] Composite emulsion: PPI dispersion and SA dispersion are mixed and stirred, heated in a water bath for a certain period of time, and quickly cooled to room temperature. The PPI-SA composite solution is subjected to high-speed shear treatment, added to the oil phase, subjected to high-speed shear treatment, and then homogenized by a high-pressure homogenizer to form a composite emulsion.

[0062] S2, glutamine aminotransferase (TG enzyme) solution and Ca 2+ Add to the emulsion, vortex quickly to mix, incubate in a water bath, and store overnight to form an emulsion gel.

[0063] In a preferred embodiment of the present invention, the modified PPI powder in S1 is PPI powder treated with electron beam irradiation (EBI) at a dose of 10 to 20 kGy.

[0064] Preferably, the stirring time in S1 is 2 to 4 hours.

[0065] Preferably, the concentration of the PPI dispersion in S1 is 8-12 wt %.

[0066] Preferably, the concentration of the SA solution in S1 is 1-3 wt %.

[0067] Preferably, the method for preparing the oil phase in S1 is to mix essential oil and medium-chain triglycerides (MCT) in a volume ratio of 10:1 to 1:2, wherein the plant essential oil includes one or more of peppermint essential oil, thyme essential oil, and cinnamon essential oil, and is not limited thereto; medium-chain triglycerides can be replaced by edible oils and fats including corn oil, soybean oil, rapeseed oil, etc.

[0068] Preferably, in the preparation step of the layer-by-layer assembled emulsion described in S1, the conditions for water bath heating are 80-90°C, 30 min, the conditions for high-speed shear treatment of the PPI dispersion are homogenization at 9000-11000 rpm for 1-3 min, the amount of oil phase added (15-25% v / v, final concentration), the high-speed shear condition for forming the primary emulsion is homogenization at 11000-13000 rpm for 1-3 min, and the conditions for homogenization with a high-pressure homogenizer are fixed cycles at 45-55 MPa for three times.

[0069] Preferably, in the preparation step of the complex emulsion described in S1, the PPI dispersion and the SA dispersion are mixed and stirred in equal volumes for 4 to 6 hours, the conditions for water bath heating are 80 to 90°C for 30 minutes, the conditions for high-speed shear treatment of the PPI-SA complex are homogenization at 9000 to 11000 rpm for 1 to 3 minutes, the amount of oil phase added (15 to 25% v / v, final concentration), the conditions for high-speed shear treatment after adding the oil phase are homogenization at 11000 to 13000 rpm for 1 to 3 minutes, and the conditions for homogenization with a high-pressure homogenizer are fixed cycles at 45 to 55 MPa for three times.

[0070] Preferably, the amount of TG enzyme added in S2 is 35-45 U / g PPI (final system).

[0071] Preferably, the Ca in S2 2+ The concentration is 20-100 mM (final system).

[0072] Preferably, the water bath incubation conditions in S2 are 45-55° C. and 60 min.

[0073] Preferably, the overnight storage condition in S2 is 2-5°C.

[0074] Another aspect of the embodiments of the present invention further provides a double-crosslinked structured emulsion gel prepared by the aforementioned preparation method.

[0075] In some preferred embodiments, the schematic diagram of the preparation process of the double cross-linked structured emulsion gel in the present invention is as follows Fig.13 shown.

[0076] Another aspect of the embodiments of the present invention further provides use of the aforementioned double-crosslinked structured emulsion gel in the preparation of food, medicine or cosmetics.

[0077] The technical solution of the present invention is further described in detail below in conjunction with several preferred embodiments and drawings. This embodiment is implemented on the premise of the technical solution of the invention, and a detailed implementation method and specific operation process are given, but the protection scope of the present invention is not limited to the following embodiments.

[0078] Unless otherwise specified, the experimental materials used in the following examples can be purchased from conventional biochemical reagent companies.

[0079] Example 1

[0080] 1. Preparation of emulsion gels with different cross-linking methods

[0081] S1. Preparation of a stable oil-in-water emulsion of pea protein isolate (PPI). PPI treated with 15 kGy electron beam irradiation (EBI) and untreated PPI powder were dispersed in deionized water to prepare a PPI dispersion with a concentration of 5 wt%. After stirring at room temperature for 3 hours, the dispersion was allowed to stand overnight. The dispersion was heated in an 85 ° C water bath for 30 minutes and quickly cooled to room temperature. A certain amount of MCT (volume fraction Φ = 20%) was added to the dispersion, and a coarse emulsion was formed by high-speed shear dispersion (10000 rpm, 5 minutes), which was then circulated three times by a high-pressure homogenizer at 50 MPa to form an O / W emulsion.

[0082] S2. Glutamine transaminase (TGase) and CaCl2 were added to the above O / W emulsions separately and mixed. In the single cross-linking group, only TGase 40U / g protein or 50mM CaCl2 was added. In the double cross-linking group, the amount of TGase added to the emulsion gel was 40U / g protein, and the final concentration of CaCl2 was 50mM. After rapid vortex mixing, the emulsion gel was heated in a 50℃ water bath for 60min, cooled to room temperature, and allowed to stand for 24h to obtain three emulsion gels with different cross-linking methods.

[0083] 2. Determination of texture and mechanical properties

[0084] Test method: Put the three emulsion gels that have been cured overnight in a vial, and use the texture profile analysis (TPA) mode and puncture mode of the physical property tester to measure the gel strength. Use a P / 0.5R cylindrical probe, and the measurement parameters are: trigger force 5g, pre-test speed 1.0mm / s, test speed 1.0mm / s, post-test speed 1.0mm / s, puncture distance 10.0mm, and measurement temperature 25°C. Repeat the test at least three times for each sample.

[0085] Figure 1 The hardness of PPI emulsion gels induced by different crosslinking methods is shown. For natural and modified PPIs, compared with those induced by TGase or Ca 2+ Single treatment, TGase and Ca 2+ The hardness of the double cross-linked latex gel treated with the combined treatment was significantly improved (p<0.05) (increased by about 6 times). In addition, the increase in the hardness of the double cross-linked latex gel modified by EBI was significantly lower than that of the untreated PPI double cross-linked gel, which indicates that the hardness of the PPI double cross-linked latex gel can be reduced after the EBI modification of protein. This is because the EBI treatment mainly changes the molecular structure of PPI, thereby changing the interaction between molecules in the protein-based latex gel and affecting the texture properties of the gel.

[0086] The remaining parameters obtained by TPA are shown in Table 1. 2+ The single cross-linked latex gel has the highest adhesion, indicating that the latex gel has the greatest viscosity. There is no significant difference in the elasticity of all samples (p>0.05), which may be related to the rupture of the latex gel after the first compression. Since the latex gel underwent partial irreversible deformation after the first compression and did not return to the initial state, the cohesion decreased seriously. Regardless of whether it was treated with EBI, the chewiness of the latex gel had the same trend as the hardness of the gel. The latex gel induced by double cross-linking had the greatest chewiness; and the chewiness of the double cross-linked latex gel after EBI treatment was lower than that of the untreated sample, indicating that after irradiation treatment, the taste of the latex gel became softer and more delicate. Because the latex gel underwent irreversible deformation during the compression process, the recovery of all samples was low.

[0087] Table 1 TPA ​​parameters of unmodified (0 kGy) and modified (15 kGy) PPI emulsion gels

[0088]

[0089] Note: Different lowercase letters in the same column indicate significant differences among natural PPI emulsion gel samples (p<0.05), and different uppercase letters in the same column indicate significant differences among 15kGy EBI modified PPI emulsion gel samples (p<0.05).

[0090] The force-time curves of natural and modified PPI emulsion gel samples in puncture mode are shown in Figure 2. Figure 2a and 2b As shown in Figure 2, all the latex gels were broken during the puncture process. The strength of the latex gel was tested using the puncture mode. Figure 2c As shown in the figure, the gel strength of the double-crosslinked latex is significantly greater than that of the single-crosslinked latex gel sample (p < 0.05). 2+ The latex gel treated with double cross-linking of TG and TG had a greater rupture strength and broke earliest ( Figure 2a and 2b As shown), it shows that the double cross-linked latex gel has a more solid texture, which makes it less resistant to external deformation. In addition, EBI treatment can reduce the strength of the double cross-linked latex gel, thereby increasing its ability to resist deformation.

[0091] 3. Rheological property determination

[0092] Test method: Use a dynamic shear rheometer to perform dynamic frequency scanning and flow scanning. The fixture selects parallel plates with a diameter of 40 mm, and a layer of latex gel is placed between the parallel plates. In the linear viscoelastic region, a fixed strain of 1% is selected, and a frequency scan is performed within the scanning range of 0.1-100 rad / s, and the storage modulus (G′) and loss modulus (G″) of the latex gel are recorded. -1 The apparent viscosity (η) was recorded as a function of shear rate within a range of shear rates.

[0093] Depend on Figure 3a-3d It can be seen that in the entire frequency range of 0.1-100 rad / s, the G′ of all PPI emulsion gel samples is much larger than G″, indicating that all samples exhibit obvious solid-like behavior, indicating that the TG enzyme and / or Ca 2+ In addition, regardless of whether EBI was used for modification, TGase and Ca 2+ The G′ and G″ of the double-crosslinked PPI latex gel treated with the combined treatment were greater than those of the single-crosslinked latex gel, indicating that Ca 2+ The addition of Ca effectively improved the viscoelasticity of the TG enzyme-induced PPI emulsion gel. 2+ It can neutralize the negative charge on the protein surface, shield static electricity, reduce electrostatic repulsion, and promote the formation of calcium bridges between PPI molecules, further strengthening the interaction between proteins and promoting protein aggregation. Figure 3a-3fIt can be seen that the viscoelasticity of the latex gel formed by the irradiated PPI is lower than that of the latex gel formed by the natural PPI, indicating that the network structure of the latex gel formed by the modified PPI is looser and softer, while the unmodified gel is more compact, which is consistent with the hardness result. This may be because the PPI treated with EBI, then subjected to heat denaturation and TGase and / or Ca 2+ The addition of Ca promotes the excessive unfolding of the PPI structure and introduces too many hydrophobic groups, which leads to protein aggregation and precipitation before gel formation, inhibiting the development of the gel structure, forming a non-uniform aggregation network structure, and reducing the viscoelasticity of the latex gel. In the single cross-linked latex gel, it can be observed that the Ca 2+ The viscoelasticity of the gel induced by Ca is greater than that of the gel induced by TGase, so 2+ May be more effective as a cross-linking agent than TGase.

[0094] The apparent viscosity of the latex gels of single / double cross-linked natural and EBI-modified PPIs is shown in Figure 3e and 3f As shown in the figure, the apparent viscosity of all emulsion gels decreases significantly with the increase of shear rate and tends to be stable, showing a shear thinning phenomenon and all of them have pseudoplasticity. The apparent viscosity of the double-crosslinked emulsion gel is greater than that of the single-crosslinked gel. In addition, the apparent viscosity of the gel formed by PPI after EBI treatment also decreases.

[0095] 4. Water holding capacity determination

[0096] Test method: The water holding capacity (WHC) of the emulsion gel was measured according to the method described in the literature. Weigh 3g of fresh emulsion gel sample and place it in a 10mL centrifuge tube. Centrifuge at 8000rpm for 20min, then use filter paper to absorb the precipitated water. The centrifuge tube containing the emulsion gel sample was accurately weighed before and after centrifugation. The calculation formula of WHC is as follows:

[0097] WHC=(W2-W0) / (W1-W0)×100%

[0098] W2 is the weight (g) of the centrifuge tube containing the emulsion gel after centrifugation; W1 is the weight (g) of the centrifuge tube containing the emulsion gel before centrifugation, and W0 is the weight (g) of the centrifuge tube. Repeat the measurement three times.

[0099] Protein-based emulsion gels are three-dimensional porous materials. Strong water-holding capacity can better retain water, nutrients and other nutrients in food, and plays an important role in the formation of food texture. The water-holding capacity of emulsion gels treated with different crosslinkers is as follows: Figure 4 As shown, after TGase and / or Ca 2+The induced emulsion gels all have good water holding capacity. It can be concluded that the addition of crosslinking agent causes the PPI emulsion to form a strong and uniform porous three-dimensional network structure, which can better retain water in the gel by increasing capillary force and the formation of hydrogen bonds during gel formation. The water holding capacity of the emulsion gel induced by double crosslinking is greater. This may be because the addition of TG enzyme promotes protein aggregation and can catalyze the formation of covalent bonds between glutamine residues and lysine residues within or between PPI molecules, thereby improving water holding capacity. 2+ The addition of further increases the cross-linking degree of PPI molecules, reduces the pore size of the latex gel network, and enhances the capillary force, thereby significantly improving the water retention of the double cross-linking-induced latex gel. Figure 4 It can be seen that EBI treatment can increase the TGase and / or Ca 2+ The water-holding capacity of the induced single / double cross-linked latex gels may be due to the fact that the PPIs pretreated with EBI expose more hydrophobic groups, increasing the hydrophobic interactions between proteins and water molecules. In addition, the non-uniform aggregation network structure of the latex gels obtained by EBI treatment may provide greater resistance to the overflow of internal water in the latex gels during centrifugation.

[0100] 5. Freeze-thaw stability analysis

[0101] Test method: Weigh 3g of wet gel in a 10mL centrifuge tube, freeze it at -20℃ overnight, thaw it at 37℃ for 60min, centrifuge it at 8000rpm for 15min, remove excess water, and weigh it again. Repeat the freeze-thaw cycle 5 times, and measure the water holding capacity of the emulsion gel sample after each freeze-thaw cycle to reflect the freeze-thaw stability of the emulsion gel. Repeat the test for each sample at least three times.

[0102] Having good freeze-thaw stability is an important prerequisite for the application of emulsion gel in frozen ready-to-eat foods. Figure 5a-Figure 5b It can be seen that after freeze-thaw cycles, the water holding capacity of each group of samples decreased significantly with the increase in the number of times. This is because repeated freezing and thawing caused the low-density ice crystals formed in the emulsion gel to nucleate, aggregate, and expand in volume during the phase change process, and the ice crystal size increased, resulting in an increase in the internal voids of the gel and a decrease in water holding capacity. The protein also experienced freeze concentration and irreversible aggregation, and the network structure formed was uneven and porous, unable to retain more water. The water holding capacity of the emulsion gel cross-linked by TG enzyme is significantly higher than that of the Ca 2+ The induced single cross-linked gel has higher freeze-thaw stability, which may be because the addition of TGase promotes the formation of covalent bonds within the PPI molecules, forming a more stable structure and effectively alleviating the destruction of ice crystals. 2+ The addition of Ca significantly improved the freeze-thaw stability of the TGase-induced emulsion gel. 2+The concentration is favorable to resist the destruction of the gel network structure through the coordination of electrostatic screening and ionic bridging. Figure 5a and 5b It can be seen that the emulsion gel formed by PPI treated with EBI has higher freeze-thaw stability, which may be because the PPI structure after EBI treatment unfolds, exposing too many hydrophobic groups, causing protein aggregation and precipitation before gel formation, and the cross-linking degree of the composite system is reduced, which reduces the degree of phase separation of the gel system caused by low-density ice crystals.

[0103] As can be seen from the results of this example, compared with only TG enzyme or Ca 2+ Single induction, by TGase and Ca 2+ The hardness, viscoelasticity, water holding capacity and freeze-thaw stability of the double-crosslinked latex gel treated with EBI were significantly improved (p<0.05). Compared with unmodified PPI, the double-crosslinked latex gel formed by PPI treated with EBI was softer, had less viscoelasticity, and stronger water holding capacity and freeze-thaw stability.

[0104] Example 2

[0105] S1. Dissolve the PPI powder treated with 15 kGy EBI in deionized water, stir at room temperature for 3 h, and let stand overnight to obtain a 10 wt% PPI dispersion. Prepare a 2 wt% SA solution. Mix peppermint essential oil and MCT in a volume ratio of 1:3 as the oil phase. Prepare an essential oil emulsion as follows:

[0106] Layer-by-layer assembly emulsion: Heat 10wt% PPI dispersion in a water bath at 85℃ for 30min, quickly cool to room temperature, homogenize the PPI dispersion at 10000rpm for 2min, add oil phase (peppermint oil: MCT = 1:3, 20% v / v, final concentration), and homogenize at 12000rpm for 2min to form a primary emulsion, then add 2wt% SA dispersion, and then pass through a high-pressure homogenizer for three fixed cycles at 50MPa to form a layer-by-layer assembly emulsion.

[0107] S2, TG enzyme solution and Ca 2+ Add to the emulsion, vortex quickly to mix, then incubate in a 50℃ water bath for 60min, and store at 4℃ overnight to form an emulsion gel, which is recorded as 15-PPISA-CC. In the final system, the activity of TG enzyme is 40U / g (PPI), Ca 2+ The concentration is 25 mM.

[0108] Example 3

[0109] S1. Dissolve the PPI powder treated with 15 kGy EBI in deionized water, stir at room temperature for 3 h, and let stand overnight to obtain a 10 wt% PPI dispersion. Prepare a 2 wt% SA solution. Mix peppermint essential oil and MCT in a volume ratio of 1:3 as the oil phase. Prepare an essential oil emulsion as follows:

[0110] Composite emulsion: 10wt% PPI dispersion and 2wt% SA dispersion were mixed and stirred in equal volumes for 5h, heated in a water bath at 85°C for 30min, and rapidly cooled to room temperature. The PPI-SA complex was homogenized at 10000rpm for 2min, and the oil phase (peppermint oil: MCT = 1:3, 20% v / v, final concentration) was added, homogenized at 12000rpm for 2min, and then passed through a high-pressure homogenizer at 50MPa for three fixed cycles to form a composite emulsion.

[0111] S2, TG enzyme solution and Ca 2+ Add to the emulsion, vortex quickly to mix, then incubate in a 50℃ water bath for 60min, and store at 4℃ overnight to form an emulsion gel, which is recorded as 15-PPISA-HH. In the final system, the activity of TG enzyme is 40U / g (PPI), Ca 2+ The concentration is 25 mM.

[0112] Comparative Example 1

[0113] The same as Example 2, except that SA was not added, and the PPI powder treated with 15 kGy EBI in S1 was replaced with natural PPI powder. The final concentration of PPI was 5 wt%, recorded as 0-PPI.

[0114] Comparative Example 2

[0115] The same as Example 2, except that SA was not added and the final concentration of PPI was 5 wt %, recorded as 15-PPI.

[0116] Comparative Example 3

[0117] The same as Example 2, except that the PPI powder treated with 15 kGy EBI in S1 is replaced with natural PPI powder, which is recorded as 0-PPISA-CC.

[0118] Comparative Example 4

[0119] The same as Example 3, except that the PPI powder treated with 15 kGy EBI in S1 is replaced with natural PPI powder, which is recorded as 0-PPISA-HH.

[0120] In order to further illustrate the technical effect of the present invention, the performance of the six emulsion gels obtained in Examples 2-3 and Comparative Examples 1-4 was measured and their applications in embedding peppermint essential oil were studied.

[0121] 1. Zeta potential, particle size and particle size distribution of essential oil emulsions

[0122] Test method: The average particle size and particle size distribution of 6 essential oil emulsions were determined using a laser particle size analyzer. The particle charge (ζ-potential) was measured using a Zetasizer Nano ZS instrument. Each sample was measured at least three times.

[0123] like Figure 6a , the potential values ​​of all emulsion samples were negative. Compared with the emulsion system stabilized by PPI alone, the absolute value of the potential in the emulsion system formed by the addition of anionic polysaccharide SA increased significantly (p<0.05), indicating that the addition of SA would enhance the stability of the emulsion. In addition, the absolute value of the potential of the complex emulsion of PPI and SA was higher than that of the layered emulsion system, indicating that a more stable protein-polysaccharide complex was formed when PPI and SA were heated together. The ζ-potential of PPI treated with EBI was significantly lower than that before treatment in the emulsion stabilized by itself and the layered emulsion and complex emulsion formed with SA (p<0.05). This may be because EBI treatment can cause changes in the structure of PPI, and the breakage of the polypeptide chain also exposes the negatively charged amino acids in the molecule to the surface of the protein, and also increases the active sites for reaction with SA.

[0124] The particle size of the emulsion is Figure 6b . After the addition of SA, the particle size of the emulsion changed significantly (p<0.05). The particle size of the emulsion without SA was larger, of which the PPI emulsion without EBI treatment was 24.25μm, and the particle size of the PPI emulsion after EBI treatment was 22.83μm. After the addition of SA, the particle size of the layer-by-layer assembly emulsion of PPI and SA decreased to 18.11μm and 16.47μm, and the particle size of the PPI and SA complex emulsion further decreased to 13.65μm and 11.08μm, indicating that the addition of SA can improve the emulsification of PPI. At the same time, the further decrease in the particle size of the complex emulsion also reflects that a more stable protein-polysaccharide complex is formed when PPI and SA are heated together. In addition, after EBI treatment, the particle sizes of single PPI emulsion, PPI and SA composite emulsion and layer-by-layer assembly emulsion were significantly reduced (p<0.05). This may be because after EBI treatment, the hydrophobic groups inside the PPI molecules were exposed, thereby promoting the binding of protein and oil and better stabilizing the emulsion.

[0125] The particle size distribution of the emulsion is Figure 6c. The particle size of the preheated unmodified PPI emulsion showed a bimodal distribution, and the particle size distribution range was wide, with an average particle size of about 24.25 μm. This was mainly because heating the natural spherical PPI above the denaturation temperature would cause the PPI to unfold and form aggregates of different sizes through hydrophobic interactions and / or intermolecular disulfide bonds, thereby affecting the stability of the emulsion. After EBI treatment, the particle size distribution of the emulsion showed a more uniform unimodal distribution, and the proportion of large particles increased, which may be due to the accelerated unfolding and aggregation of PPI after EBI modification and heating treatment. The composite emulsion of PPI and SA showed a uniform unimodal distribution, and its average particle size was smaller than that of the layer-by-layer assembly emulsion. This may be because PPI and SA formed a stable complex during the thermal deformation process, increasing the steric effect and electrostatic repulsion, inhibiting the aggregation of oil droplets, thereby reducing the emulsion particle size and improving the stability of the system.

[0126] 2. Determination of texture properties

[0127] The test method is the same as described in Example 1.

[0128] Depend on Figure 7a and 7b It can be seen that when SA is added to the system, the hardness of the double cross-linked latex gel increases significantly (p<0.05), and compared with the composite latex gel, the layer-by-layer assembled latex gel has a higher hardness (p<0.05). This may be because when SA is added before emulsification, SA will interact with PPI to form a complex and then stabilize the emulsion. When SA is added after the primary emulsion is formed using PPI, more SA will migrate to the external water phase of the emulsion, increasing the number of polymer molecules in the continuous phase, thereby increasing the cross-linking density. And as a strong gelling agent, SA can quickly react with Ca 2+ The gelation occurred, forming an "egg box" model structure, which significantly increased the hardness of the protein gel. In addition, after the addition of SA to the EBI-modified PPI, the hardness of the composite latex gel and the layer-by-layer assembled latex gel was significantly reduced (p < 0.05). It may be that the EBI-modified PPI, after heat denaturation and TGase and / or Ca 2+ After treatment, the structure was over-expanded, aggregation and precipitation occurred before gel formation, forming a non-uniform aggregation network structure. In addition, the expansion of the PPI molecular structure also affected the Ca 2+ The "egg-box" structure between SA and the gel leads to a decrease in the hardness of the gel. Figure 7c It can be seen that the cohesion of the layer-by-layer latex gel is poor, which may be because the gel structure breaks after the first compression. The chewiness of the gel is consistent with the hardness, which increases significantly with the addition of SA, especially the layer-by-layer latex gel has a greater chewiness ( Figure 7d Due to the irreversible rupture that occurred during compression, the recovery of each group of latex gels was very low ( Figure 7e).

[0129] From the above results, it can be seen that compared with the composite latex, the latex gel formed by double crosslinking of the layer-by-layer assembled latex can obtain higher strength, higher chewiness and hardness. In addition, the PPI treated with EBI will form a non-uniform aggregation network when forming a gel, which will reduce the hardness of the gel.

[0130] 3. Rheological property determination

[0131] The test method is the same as described in Example 1.

[0132] Rheological properties of emulsion gels such as Figure 8a and 8b As shown in the figure, the elastic modulus G′ of all gel samples is greater than the viscous modulus G″, indicating that the latex gels formed by double cross-linking are more elastic and show typical solid-like behavior. In addition, regardless of whether PPI is modified by EBI, G′ and G″ show the same change pattern, that is, PPI-SA layer-by-layer assembled latex gel>PPI-SA composite latex gel>PPI latex gel. This shows that the addition of polysaccharide SA can give the PPI latex gel system greater viscoelasticity and higher gel strength, which may be due to the fact that SA can react with Ca 2+ The "egg-box" model structure was formed, which significantly increased the cross-linking degree of the protein gel. Moreover, compared with the emulsion gel formed by PPI alone, the emulsion gel sample showed more obvious frequency dependence after the addition of SA. Compared with the composite emulsion, the emulsion gel formed by the layer-by-layer assembled emulsion had greater viscoelasticity and showed better gel properties, which can be attributed to the increased cross-linking density in the layer-by-layer assembled emulsion gel and the higher viscosity and strong gelation of SA. It can also be observed that after pre-treating PPI with EBI, the gel G′ and G″ of the layer-by-layer emulsion gel sample decreased significantly, which may be because the EBI modification unfolded the molecular structure of PPI and affected the Ca 2+ The "egg box" structure with SA.

[0133] The flow scan results are as follows Figure 8c As the shear rate increases, the apparent viscosity of all emulsion gel samples first drops sharply and then tends to be stable, showing the characteristics of shear thinning. This may be because in the emulsion gel system, PPI and SA are entangled with each other. As the shear rate increases, the entangled macromolecules are subjected to shear stress changes ( Figure 8d), resulting in spatial displacement, elongation and disentanglement of polymer molecules, the gel network structure is destroyed, and the flow resistance is reduced. The viscosity of the composite emulsion gel and the layer-by-layer assembled emulsion gel with SA added is greater than that of the PPI emulsion gel, indicating that the addition of SA increases the viscosity of the emulsion gel. Since SA itself has the characteristics of high viscosity, especially the layer-by-layer assembled emulsion gel, when SA is evenly distributed on the surface of the emulsion stabilized by PPI, due to flocculation, the effective volume fraction of the dispersed phase increases, resulting in a significant increase in its apparent viscosity. Moreover, the apparent viscosity of the emulsion gel sample increased after EBI treatment, which may be due to the unfolding of the PPI molecular structure after EBI treatment, and the presence of more covalent interactions catalyzed by TG enzymes in the emulsion gel. When the shear stress increases, the spatial movement of the PPI molecules is more strongly constrained, showing a higher apparent viscosity.

[0134] 4. Determination of water holding properties

[0135] The test method is the same as described in Example 1.

[0136] like Fig. 9 As shown in the figure, after adding SA to the protein emulsion system, the TG enzyme and Ca 2+ Under the double cross-linking, the water holding capacity of the layered latex gel and the composite latex gel formed is higher (p<0.05), especially the layered latex gel, which indicates that the introduction of SA is conducive to the formation of a tighter gel network, and more SA in the layered latex exists in the external water phase, which reduces the molecular distance in the continuous phase, more effectively increases the cross-linking density, and can more effectively intercept water molecules. Therefore, the layered latex gel has a higher water holding capacity, followed by the composite latex gel, and the single PPI latex gel is the smallest. At the same time, EBI modification also significantly improves the water holding capacity of the composite latex gel system, but EBI treatment has little effect on the water holding capacity of PPI latex gel and layered latex gel.

[0137] 5. Flavor Release Assay

[0138] (1) Electronic nose analysis

[0139] Test method: The difference in aroma release in 6 kinds of peppermint essential oil emulsion gels was determined by electronic nose instrument analysis. A certain amount of emulsion gel sample was weighed into a 40mL electronic nose test vial and the bottle cap was immediately closed 40s before the test. Within 5s before the start of the test, the air replenishment needle and the injection needle were quickly inserted into the bottle. The test was performed for 30s, and the air flow rate was maintained at 300mL / min. Each sample was repeated 10 times, and the difference between different samples was analyzed by principal component analysis.

[0140] like Fig.10aAs shown in the figure, all the emulsion gel samples showed the same radar distribution morphology, indicating that they have similar odor fingerprints. The response values ​​of different emulsion gel samples on sensors S2 and S7 are significant. This is because the aroma of different essential oil emulsion gel samples mainly depends on volatile substances such as oxygen-containing compounds, alcohols and aromatic esters in the aroma of peppermint essential oil. The response values ​​of sensors S2 and S7 are ranked as follows: complex emulsion gel>layer emulsion gel>PPI emulsion gel. In addition, it can also be found that the emulsion gel sample formed by PPI after EBI treatment has a higher response value, indicating that the volatile aroma of peppermint essential oil can move to the headspace faster. The response value of the emulsion gel sample without SA is the lowest, which may be due to the fact that the protein exposed more hydrophobic areas after heat denaturation treatment, and interactions such as adsorption and complexation occurred with highly hydrophobic aroma compounds. In addition, compared with the emulsion system with SA added, the emulsion stabilized by a single protein is more likely to escape aroma when emulsified by high-speed shear, resulting in a decrease in the response value. Compared with the layered emulsion gel, the composite emulsion gel, especially the composite emulsion gel formed by PPI and SA after EBI treatment, has a lower cross-linking density, lower viscoelasticity, and softer texture, which allows the volatile aroma substances in the peppermint essential oil to move faster to the headspace. In addition, the droplets of the composite emulsion are smaller than those of the layered emulsion, so its aroma release is faster.

[0141] Principal component analysis Fig.10b As shown in the figure, the main components 1 and 2 of different latex gel samples are 99.58% and 0.42%, respectively. Therefore, these two main components represent the main characteristics of the six groups of latex gel samples. The odor response distribution areas of the layered latex gels and composite latex gels formed by PPI and SA before and after EBI treatment are well separated, indicating that the odors of the four groups of latex gels are significantly different.

[0142] (2) Cumulative release rate determination

[0143] Test method: According to the results of principal component analysis, natural and EBI modified PPI and SA formed different interfaces of peppermint essential oil emulsion gels with significant odor differences were selected, and their cumulative release percentage was determined using a heating-assisted method. The emulsion gel was cut into small pieces of equal volume, 5 g was weighed and placed in 40 mL of 50% ethanol solution, and heated in a water bath at 80°C during the test to accelerate the release. The analysis was performed using an ultraviolet spectrophotometer at 310 nm. The peppermint essential oil-ethanol standard curve (y=0.7441x+0.0222, R 2 =0.9985) to calculate the content of peppermint essential oil in the supernatant, and the cumulative release rate (%) of peppermint essential oil in each group of samples was calculated as follows:

[0144] Cumulative release rate (%) = M t / M0×100

[0145] Among them, M t and M0 represent the mass of peppermint essential oil released within time t and the initial mass of peppermint essential oil loaded in the sample, respectively.

[0146] The results are as follows Fig.11 As shown, compared with the layer-by-layer assembled latex gel, the cumulative release rate of peppermint essential oil aroma compounds in the composite emulsion gel is faster and the release amount is higher. This may be because the composite emulsion gel has a smaller viscoelasticity and a softer texture, which promotes the release of peppermint essential oil. The layer-by-layer emulsion gel has a harder texture and greater viscoelasticity, and using it to embed peppermint essential oil can achieve a certain sustained release effect. The emulsion gel prepared by EBI-modified PPI can promote the more effective release of volatile aroma substances in the peppermint essential oil it embeds. This may be because the EBI modification reduces the texture and rheological properties of the emulsion gel, which is conducive to the faster release of aroma substances from the gel matrix.

[0147] (3) Gas chromatography-mass spectrometry analysis

[0148] Test method: The natural and EBI-modified PPI and SA composite emulsion gels that performed well in electronic nose analysis and cumulative release rate determination were analyzed by gas chromatography-mass spectrometry. The volatile compound components in the emulsion gel were determined by gas chromatography-mass spectrometry. 1.5g of the emulsion gel was weighed and placed in a 20mL special headspace bottle and injected by solid phase microextraction. After equilibration at 40℃ for 15min, a three-in-one extraction head (DVB / CAR / PDMS) was used for extraction for 40min and analysis for 5min. Gas chromatography conditions: the chromatographic column was a 30m×0.25mm×0.25μm capillary column (HP-5MS); the injection port temperature was 250℃; the carrier gas flow rate was 1.0mL / min; the injection mode was split 30%. The heating process was: after maintaining 40℃ for 40min, the temperature was increased to 120℃ at 4℃ / min, and the temperature was increased to 220℃ at 5℃ / min and maintained for 5min. Mass spectrometry conditions: EI ion source, electron energy 70 eV; mass scanning range 36-550 m / z.

[0149] The separation and identification results are shown in Table 2. The main aroma components in the composite essential oil emulsion gel sample belong to terpenes, alcohols, ketones, esters and other substances. 20 flavor substances with relatively high percentages were selected and sorted according to their retention time. It can be seen that most of the flavor substances in peppermint essential oil belong to terpenoid compounds, among which menthol, menthone and menthyl acetate have the largest peak area and the highest relative percentage, and are the main source of the unique aroma of peppermint. Moreover, the relative contents of these aromatic substances in the composite emulsion gel before and after EBI modification are different. The main manifestation is that compared with the unmodified PPI, the content of characteristic mint aroma compounds such as D-isomenthol, menthone, levomenthenone, isomenthol, pulegol, and DL-menthol is higher in the PPI-SA composite emulsion gel after EBI modification, which is manifested by the larger peak height and peak area of ​​the corresponding retention time in the gas chromatography-mass spectrometry ( Fig.12a and 12b ), thus the improvement of the texture and rheological properties of the essential oil emulsion gel will weaken the release of aroma substances in the essential oil. The hardness of the emulsion gel formed by the protein after EBI treatment will be significantly reduced, the cross-linking density of its matrix will be lower, the viscoelasticity will be smaller, and the texture will be softer. Therefore, the volatile aroma substances in the peppermint essential oil can move to the headspace faster, and the content of the characteristic peppermint aroma compounds in the essential oil emulsion gel after EBI treatment will be higher. However, the content of substances such as D-limonene, octanol, pulegone, piperitone, and menthyl acetate did not weaken with the improvement of the texture and rheological properties of the system. On the contrary, their release rate increased. This may be because the release of aromatic compounds is also related to their own properties and experimental operations.

[0150] Table 2 Main flavor compounds and their contents in the mint essential oil aroma of the composite emulsion gels formed by EBI-modified and unmodified PPI and SA

[0151]

[0152]

[0153] In addition, the inventors of this case also referred to the aforementioned embodiments and conducted experiments with other raw materials, process operations, and process conditions described in this specification, and obtained relatively ideal results.

[0154] It should be understood that the technical solution of the present invention is not limited to the above-mentioned specific implementation cases. Any technical deformation made according to the technical solution of the present invention without departing from the scope of protection of the purpose of the present invention and the claims shall fall within the protection scope of the present invention.

Claims

1. A method for preparing a double cross-linked structured emulsion gel, characterized in that: include: Providing a modified pea protein isolate dispersion, a sodium alginate dispersion and an oil phase; wherein the oil phase comprises plant essential oil and edible oil; The modified pea protein isolate dispersion is mixed with an oil phase and subjected to high-speed shearing treatment to form an oil-in-water emulsion, and then a sodium alginate dispersion is added and homogenized to obtain a layer-by-layer assembly emulsion; or, the modified pea protein isolate dispersion is mixed with a sodium alginate dispersion to form a complex, and then an oil phase is added and subjected to shearing and homogenization treatment to obtain a complex emulsion; And, glutamine aminotransferase, Ca 2+ The double cross-linked structured emulsion gel is prepared by adding the emulsion into the layer-by-layer assembly emulsion or the composite emulsion and performing a curing treatment.

2. The preparation method according to claim 1, characterized in that: The protein in the modified pea protein isolate dispersion is obtained by irradiating the electron beam with a dosage of 10 to 20 kGy.

3. The preparation method according to claim 1, characterized in that: The protein content in the modified pea protein isolate dispersion is 8-12 wt %; and / or, the content of sodium alginate in the sodium alginate dispersion is 1 to 3 wt%; And / or, the plant essential oil includes any one or more combinations of peppermint essential oil, thyme essential oil, and cinnamon essential oil; And / or, the edible oil includes any one or more combinations of medium chain triglycerides, corn oil, soybean oil, and rapeseed oil; And / or, the volume ratio of plant essential oil to edible oil in the oil phase is 10:1 to 1:

2.

4. The preparation method according to claim 1, characterized in that: Specifically include: The modified pea protein isolate dispersion is heated in a water bath at 80-90° C. for 25-35 minutes and rapidly cooled to room temperature, homogenized at 9000-11000 rpm for 1-3 minutes, and then the oil phase is added and homogenized at 11000-13000 rpm for 1-3 minutes to form an oil-in-water emulsion; and adding a sodium alginate dispersion to the oil-in-water emulsion and homogenizing it with a high-pressure homogenizer to obtain a layer-by-layer assembly emulsion; wherein the homogenization conditions include: fixed circulation at 45-55 MPa for three times; Preferably, the volume content of the oil phase in the layer-by-layer assembly emulsion is 15-25%.

5. The preparation method according to claim 1, characterized in that: Specifically include: The modified pea protein isolate dispersion and the sodium alginate dispersion are mixed in equal volumes and stirred for 4 to 6 hours, then heated in a water bath at 80 to 90° C. for 25 to 35 minutes and rapidly cooled to room temperature to form a complex solution; And, the composite solution is homogenized at 9000-11000 rpm for 1-3 min, then the oil phase is added and homogenized at 11000-13000 rpm for 1-3 min, and then homogenized by a high-pressure homogenizer to obtain a composite emulsion; wherein the homogenization conditions include: fixed circulation at 45-55 MPa for three times; Preferably, the volume content of the oil phase in the composite emulsion is 15-25%.

6. The preparation method according to claim 1, characterized in that: Specifically include: Glutamine transaminase, Ca 2+ The mixture is added into the layer-by-layer assembly emulsion or the composite emulsion to form a mixed system, and then quickly vortexed to mix evenly. After incubation in a water bath, the mixture is stored overnight to form a double-crosslinked structured emulsion gel.

7. The preparation method according to claim 6, characterized in that: The mass ratio of the glutamine transaminase to the modified pea protein isolate is 35-45 U / g; And / or, in the mixed system, Ca 2+ The concentration is 20~100mmol / L.

8. The preparation method according to claim 6, characterized in that: The conditions of the water bath incubation include: a temperature of 45 to 55° C. and a time of 50 to 70 minutes; And / or, the temperature for overnight storage is 2-5°C.

9. A double-crosslinked structured emulsion gel prepared by the preparation method according to any one of claims 1 to 8.

10. Use of the double-crosslinked structured emulsion gel according to claim 9 in the preparation of food, medicine or cosmetics.

Citation Information

Cited By

  • Quinoa protein and sodium alginate compound emulsion gel as well as preparation method and application thereof

    CN122056374A