Production method of antibacterial compound coating aluminum foil

By applying and drying the antibacterial compound coating on the aluminum foil, the problem of sticking and rolling of aluminum foil during processing is solved, and the production efficiency and product quality are improved.

CN118988642AInactive Publication Date: 2024-11-22JIANGXI KEMAO NEW MEDICINAL MATERIALS CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202410276659.3
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-03-12
Publication Date
2024-11-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the production and processing, existing aluminum foil paper is prone to be glued and rolled when unrolled due to external pulling, which affects processing efficiency and speed.

Method used

Using the production method of antibacterial compound coated aluminum foil, the coating is cured on the aluminum foil by adding antibacterial agent to the silicone resin solution and applying gravure and drying treatment.

Benefits of technology

It improves the production and processing efficiency and speed of aluminum foil, ensures sufficient curing of the coating, avoids quality problems in subsequent operations, and enhances the stability and quality of the product.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118988642A_ABST
    Figure CN118988642A_ABST
Patent Text Reader

Abstract

The invention provides a production method of an antibacterial compound coating aluminum foil, and belongs to the technical field of aluminum-foil papers.The production method of the antibacterial compound coating aluminum foil comprises the steps that firstly, No.120 solvent oil is added into silicon resin for dilution, a silicon resin adhesive agent, a cross-linking agent and a catalyst are added, then stirring is conducted through high-speed stirring, and then the silicon resin adhesive agent is obtained; according to the production of the aluminum foil, a curable compound coating is coated on one surface of the aluminum foil. And the bottom of the coating is fully measured and cured through heating and baking, so that the phenomenon that in subsequent operation or deep processing, roll sticking and rolling are caused during uncoiling, and subsequent processing and production are influenced is avoided, and the production and processing efficiency and speed of the aluminum-foil paper are improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of aluminum foil paper, and in particular relates to a production method of antibacterial compound coated aluminum foil. Background Art

[0002] Aluminum foil paper refers to paper made by pasting aluminum foil backing paper and aluminum foil backing. It is soft and easy to deform, just like paper, and it does not rebound after deformation. It can be qualitative, ensure light blocking, will not fall off, is not light-transmissive, has no pollution, and is cheap. It is used for moisture-proof and decorative packaging of high-end cigarettes, candies and other foods.

[0003] During the production and processing of existing aluminum foil, especially during deep processing, it is easy to cause sticking and curling when unrolling due to external pulling, which in turn affects its subsequent processing and affects the processing efficiency and speed. Summary of the invention

[0004] The purpose of the present invention is to provide a method for producing antibacterial compound coated aluminum foil, aiming to solve the problem in the prior art that aluminum foil paper is easily sticky and curled when unrolled during production and processing, especially during deep processing, due to external pulling, thereby affecting its subsequent processing and affecting the processing efficiency and speed.

[0005] To achieve the above object, the present invention provides the following technical solutions:

[0006] A method for producing an antibacterial compound coated aluminum foil, the specific preparation process is as follows:

[0007] The first step is to add No. 120 solvent oil into the silicone resin for dilution, and add a silicone resin adhesive, a cross-linking agent and a catalyst, and then stir the mixture by high-speed stirring to obtain a silicone resin solution;

[0008] In the second step, the antibacterial agent is added to the prepared silicone resin solution in a certain proportion to finally obtain the aluminum foil coating;

[0009] The third step is to apply the aluminum foil coating on the aluminum foil by gravure coating at a solid content of 1.0 g / ㎡;

[0010] In the fourth step, the coated aluminum foil is dried in four ovens to obtain a completely dried coated aluminum foil.

[0011] As a preferred solution of the present invention, the silicone resin is a colorless, transparent, light-viscosity liquid produced by Dow Corning Company, which has the characteristics of low curing temperature and short curing time, and the curing time is correspondingly shortened as the temperature increases.

[0012] As a preferred solution of the present invention, the drying temperature is 135° C.-268° C., the length of the drying tunnel is 9 m, and the rotation speed of the machine is 100 m / min.

[0013] As a preferred solution of the present invention, the ratio of the antibacterial agent to the silicone resin solution is 2-5:100.

[0014] As a preferred solution of the present invention, the high-speed mixer consists of a lifting assembly, a mounting seat, an external plate, an adjustment seat, a rotating shell, an electric roller and a plurality of transmission tubes. The mounting seat and the external plate are fixedly connected to each other, the lifting assembly is arranged on one side of the external plate, the adjustment seat is connected to the lifting mechanism, the rotating shell is fixedly connected to the upper end of the adjustment seat, the electric roller is rotatably connected to the lower inner wall of the rotating shell, and the plurality of transmission tubes are fixedly connected to the circumferential surface of the electric roller.

[0015] As a preferred solution of the present invention, the lifting assembly consists of a mounting plate, a first motor, a screw and a screw nut. The mounting plate is fixedly connected to one end of the external plate, the first motor is fixedly connected to the lower end of the mounting plate, the screw is rotatably connected to the upper end of the mounting plate, the screw nut is threadedly connected to the circumferential surface of the screw, and the screw nut is fixedly connected to one end of the adjustment seat.

[0016] As a preferred solution of the present invention, a limiting rod is fixedly connected to the upper end of the mounting plate, a stabilizing hole is opened at the upper end of the screw nut, and the screw nut is slidably connected to the outer surface of the limiting rod through the stabilizing hole, and an anti-drop plate is fixedly connected to the upper end of the limiting rod.

[0017] As a preferred scheme of the present invention, the gravure coating step is composed of multiple assembly plates, two support plates, a transmission device, two stabilizing bars, a placement plate, a second motor, a coating roller, a scattering tube and a transmission tube. The multiple assembly plates are fixedly connected to the upper end of the mounting seat, the two support plates are fixedly connected to the adjacent ends of the multiple assembly plates, the placement plate is fixedly connected to one end of one of the support plates, the second motor is fixedly connected to one end of the placement plate, the coating roller is rotatably connected to one end of the placement plate, the scattering tube is rotatably connected to one side inner wall of the coating roller, the transmission tube movably passes through one side inner wall of the coating roller and is connected to the scattering tube, and the transmission tube is rotatably connected to the scattering tube via a rotating shaft, the other end of the transmission tube is fixedly connected to the circumferential surface of the rotating shell, and the transmission tube is connected to the rotating shell.

[0018] As a preferred solution of the present invention, the drying step consists of a drying shell, a plurality of placement slots and a plurality of dryers, the drying shell is fixedly connected to the upper ends of the two support plates, the plurality of placement slots are all opened on the inner surface of the drying shell, and the plurality of dryers are fixedly connected to the plurality of placement slots.

[0019] As a preferred solution of the present invention, both ends of the drying shell are fixedly connected with heat insulation plates, the upper end of the rotating shell is rotatably connected with a sealing plate via a rotating shaft, and the upper end of the sealing plate is provided with a hand grip groove.

[0020] Compared with the prior art, the present invention has the following beneficial effects:

[0021] 1. The production of aluminum foil involves coating a curable compound coating on one side of the aluminum foil. The coating is fully cured by heating and baking to prevent sticking and curling during unwinding during subsequent operations or deep processing, which affects subsequent processing and production, thereby improving the efficiency and speed of aluminum foil production.

[0022] 2. When it is necessary to make aluminum foil coating, materials such as silicone resin adhesive, cross-linking agent and catalyst can be placed in the rotating shell, and then the driving electric roller can drive the two transmission tubes to rotate, which is convenient for stirring a variety of materials and improving the production level of aluminum foil coating. The screw nut can be extended and retracted through the rotation of the screw, which makes it convenient to lift and lower the adjustment seat and the rotating shell, and then it is convenient to replenish materials in the rotating shell.

[0023] 3. By adjusting the telescopic rod fixedly connected to the close ends of the seat and the external plate, the lifting stability of the adjusting seat can be improved. When the aluminum foil needs to be gravure coated, the aluminum foil can be placed on the circumferential surface of the transmission device, and then the coating can be transmitted to the scattering tube through the transmission tube, and the second motor can be started to drive the coating roller to rotate, and then the material in the scattering tube can be dispersed by centrifugal force to the circumferential surface of the coating roller, so that the coating roller is completely soaked in the coating. At this time, the aluminum foil can be transported by the drive of the transmission device. At the same time, the filter screen can be coated by the rotation of the coating roller, thereby improving the thoroughness of the coating of the aluminum foil.

[0024] 4. When the aluminum foil is coated and transported by the transmission device, the aluminum foil will pass through the drying shell. At this time, heat can be generated by the dryers fixedly connected in the multiple placement slots in the drying shell, thereby facilitating the curing of the coating coated on the surface of the aluminum foil, thereby improving the convenience and quality of the production of the aluminum foil, and the multiple support legs fixedly connected to the lower end of the mounting seat and the external plate can improve the support stability of the device. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] The accompanying drawings are used to provide a further understanding of the present invention and constitute a part of the specification. Together with the embodiments of the present invention, they are used to explain the present invention and do not constitute a limitation of the present invention. In the accompanying drawings:

[0026] Figure 1 It is the main stereoscopic view in the present invention;

[0027] Figure 2 It is a side perspective view of the present invention;

[0028] Figure 3 It is the main sectional stereogram in the present invention.

[0029] In the figure: 1. mounting base; 2. supporting leg; 3. external plate; 4. first motor; 5. mounting plate; 6. screw; 7. screw nut; 8. anti-slip plate; 9. limiting rod; 10. adjusting base; 11. rotating shell; 12. sealing plate; 13. hand buckle groove; 14. telescopic rod; 15. assembly plate; 16. support plate; 17. placement plate; 18. second motor; 19. drying shell; 20. heat insulation board; 21. transmission device; 22. stabilizing bar; 23. coating roller; 24. transmission tube; 25. dryer; 26. scattering tube. DETAILED DESCRIPTION

[0030] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0031] Example 1

[0032] The present invention provides the following technical solutions:

[0033] A method for producing an antibacterial compound coated aluminum foil, the specific preparation process is as follows:

[0034] The first step is to add No. 120 solvent oil into the silicone resin for dilution, and add a silicone resin adhesive, a cross-linking agent and a catalyst, and then stir the mixture by high-speed stirring to obtain a silicone resin solution;

[0035] In the second step, the antibacterial agent is added to the prepared silicone resin solution in a certain proportion to finally obtain the aluminum foil coating;

[0036] The third step is to apply the aluminum foil coating on the aluminum foil by gravure coating at a solid content of 1.0 g / ㎡;

[0037] The fourth step is to pass the coated aluminum foil through four ovens for drying to obtain a completely dried coated aluminum foil;

[0038] The silicone resin is a colorless, transparent, light-viscosity liquid produced by Dow Corning Company, which has the characteristics of low curing temperature and short curing time, and the curing time is shortened accordingly with the increase of temperature;

[0039] The drying temperature is 135°C-268°C, the length of the drying tunnel is 9m, and the speed of the machine is 100m / min;

[0040] The ratio of the antibacterial agent to the silicone resin solution is 2-5:100.

[0041] In a specific embodiment of the present invention, No. 120 solvent oil is added to the silicone resin for dilution, and a silicone resin adhesive, a cross-linking agent and a catalyst are added, and then stirred by high-speed stirring to obtain a silicone resin solution, and an antibacterial agent is added to the prepared silicone resin solution in a certain proportion to finally obtain an aluminum foil coating. The aluminum foil coating is coated on the aluminum foil at a solid content of 1.0 g / ㎡ by gravure coating. After the coating is completed, it is first heated and dried in four ovens to completely evaporate the residual solvent, so that the coating is fully cured to avoid anti-sticking, resulting in poor unwinding performance and the like, resulting in unstable product quality. The drying temperature and time of the oven vary according to different types of coatings, solid content, and coating thickness. Through years of production experience, the more suitable drying temperature is 135°C to 268°C. Baking methods include conventional drying ovens; infrared heaters, heating rollers, ovens, induction heaters, etc. The drying speed is affected by the length of the drying tunnel and the heating temperature. The present invention adopts a one-step curing method, which can provide efficient productivity. For example, the drying tunnel length is 9 meters, the temperature is above 198° C., and the machine running speed is 100 meters per minute.

[0042] Table 1-2 shows the minimum development prevention concentration of the antimicrobial agent in Example 1 and the results of the MIC test results (ppm):

[0043] Test strains Mic(ppm) Bacillus cereus (ATCC1178) spores 125 Salmonella (IF03163) 125 Escherichia coli (IF03301) 62.5 Pseudomonas aeruginosa 62.5 Staphylococcus aureus (ATCC6538P) 250 Enterococcus (ATCC8043) 125 Lactic acid bacteria (ATCC7468) 250 Enterohemorrhagic Escherichia coli (laboratory isolate) 125 Candida (IF01594) 250 Baking Yeast(IF01594) 250 Aspergillus niger (IF04407) 500 Chaetomium globosum (ATCC6205) 500 Penicillin (IF06345) 500 White moss fungus (IF06202) 500

[0044]

[0045]

[0046] The above table clearly shows that the device can inhibit E. coli ESC and Staphylococcus aureus by more than 99%, and the above table also shows that it has a significant inhibitory effect on viruses. According to the results verified by external testing agencies so far, it has even been confirmed that the inhibitory effect on the activity of SARS virus and avian epidemic virus (H5N1 type) has reached 100%.

[0047] Example 2

[0048] A method for producing an antimicrobial compound coated aluminum foil, comprising:

[0049] The high-speed mixer consists of a lifting assembly, a mounting seat 1, an external plate 3, an adjustment seat 10, a rotating shell 11, an electric roller and a plurality of transmission tubes 24. The mounting seat 1 and the external plate 3 are fixedly connected to each other, the lifting assembly is arranged on one side of the external plate 3, the adjusting seat 10 is connected to the lifting mechanism, the rotating shell 11 is fixedly connected to the upper end of the adjusting seat 10, the electric roller is rotatably connected to the lower inner wall of the rotating shell 11, and the plurality of transmission tubes 24 are all fixedly connected to the circumferential surface of the electric roller. The lifting assembly consists of a mounting plate 5, a first motor 4, a screw 6 and a screw nut 7. The mounting plate 5 is fixedly connected to one end of the external plate 3, the first motor 4 is fixedly connected to the lower end of the mounting plate 5, the screw 6 is rotatably connected to the upper end of the mounting plate 5, the screw nut 7 is threadedly connected to the circumferential surface of the screw 6, and the screw nut 7 is fixedly connected to one end of the adjusting seat 10.

[0050] In the present embodiment: when it is necessary to stir the silicone solution or aluminum foil coating, a variety of materials can be placed in the rotating shell 11, and then the electric roller is driven to rotate the multiple transmission tubes 24. At this time, the various materials can be stirred, and in actual use, the first motor 4 can be driven so that its output shaft drives the screw 6 to rotate, thereby driving the screw nut 7 threadedly connected to the circumferential surface of the screw 6 to move, thereby driving the adjustment seat 10 to change the height, thereby facilitating the lowering of the height of the rotating shell 11, and then facilitating the addition of materials into the rotating shell 11. It should be noted that the specific type of the first motor 4 to be used is selected by relevant technical personnel familiar with the field, and the above-mentioned first motor 4 and the like belong to the prior art and are not elaborated in this scheme.

[0051] For details, please refer to Figure 2 The upper end of the mounting plate 5 is fixedly connected with a limiting rod 9, the upper end of the screw nut 7 is provided with a stabilizing hole, and the screw nut 7 is slidably connected to the outer surface of the limiting rod 9 through the stabilizing hole, and the upper end of the limiting rod 9 is fixedly connected with an anti-slip plate 8. The gravure coating step is composed of a plurality of assembly plates 15, two support plates 16, a transmission device 21, two stabilizing bars 22, a placement plate 17, a second motor 18, a coating roller 23, a scattering tube 26 and a transmission tube 24. The plurality of assembly plates 15 are fixedly connected to the upper end of the mounting seat 1, and the two support plates 16 are fixedly connected to the plurality of assembly plates 15. The plate 15 is close to the end thereof, the placement plate 17 is fixedly connected to one end of one of the supporting plates 16, the second motor 18 is fixedly connected to one end of the placement plate 17, the coating roller 23 is rotatably connected to one end of the placement plate 17, the scattering tube 26 is rotatably connected to one side inner wall of the coating roller 23, the transmission tube 24 movably passes through one side inner wall of the coating roller 23 and is connected to the scattering tube 26, and the transmission tube 24 is rotatably connected to the scattering tube 26 via a rotating shaft, the other end of the transmission tube 24 is fixedly connected to the circumferential surface of the rotating shell 11, and the transmission tube 24 is connected to the rotating shell 11.

[0052] In this embodiment: when the screw nut 7 moves, it can slide on the outer surface of the limiting rod 9 through the hole, thereby improving the vertical sliding stability of the screw nut 7, and the anti-slip plate 8 can prevent the screw nut 7 from being damaged due to excessive sliding. When it is necessary to apply paint to the aluminum foil, the aluminum foil can be placed on the circumferential surface of the transmission device 21, and then the paint in the rotating shell 11 is transmitted to the scattering tube 26 through the transmission tube 24, and then the second motor 18 can be driven to rotate its output shaft, thereby driving the coating roller 23 to rotate, and then the inner wall thereof The scattering tube 26 will rotate along with the coating roller 23. At this time, the paint filled in the scattering tube 26 can be scattered by centrifugal force, and the coating roller 23 can be soaked with the paint. The coating roller 23 itself will rotate, so that the aluminum foil placed on the circumferential surface of the transmission device 21 can be coated, so that the aluminum foil can be completely and thoroughly coated with the paint. It should be noted that the specific type of the second motor 18 to be used is selected by relevant technical personnel familiar with this field, and the above-mentioned second motor 18 and the like belong to the prior art and will not be elaborated in this scheme.

[0053] For details, please refer to Figure 1 The drying step consists of a drying shell 19, a plurality of placement slots and a plurality of dryers 25. The drying shell 19 is fixedly connected to the upper ends of the two supporting plates 16. The plurality of placement slots are all opened on the inner surface of the drying shell 19. The plurality of dryers 25 are all fixedly connected to the plurality of placement slots. Both ends of the drying shell 19 are fixedly connected with heat insulation plates 20. The upper end of the rotating shell 11 is rotatably connected with a sealing plate 12 through a rotating shaft. A hand buckle slot 13 is opened at the upper end of the sealing plate 12.

[0054] In this embodiment: when the aluminum foil is driven and transferred by the transmission device 21, the aluminum foil can pass through the drying shell 19. At this time, the coating applied on the aluminum foil can be cured through the multiple transmission tubes 24 fixedly connected in the multiple placement grooves. The heat insulation plate 20 fixedly connected at both ends of the drying shell 19 can prevent the heat loss in the drying shell 19. The rotating shell 11 can be opened and closed by rotating the sealing plate 12. The hand buckle groove 13 can improve the convenience of rotating the sealing plate 12.

[0055] The working principle and use process of the present invention:

[0056] The first step is to add No. 120 solvent oil into the silicone resin for dilution, and add a silicone resin adhesive, a cross-linking agent and a catalyst, and then stir the mixture by high-speed stirring to obtain a silicone resin solution;

[0057] In the second step, the antibacterial agent is added to the prepared silicone resin solution in a certain proportion to finally obtain the aluminum foil coating;

[0058] The third step is to apply the aluminum foil coating on the aluminum foil by gravure coating at a solid content of 1.0 g / ㎡;

[0059] In the fourth step, the coated aluminum foil is dried in four ovens to obtain a completely dried coated aluminum foil.

[0060] Finally, it should be noted that the above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art can still modify the technical solutions described in the aforementioned embodiments or replace some of the technical features therein by equivalents. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present invention shall be included in the protection scope of the present invention.

Claims

1. A method for producing an antimicrobial compound coated aluminum foil, characterized in that: The specific preparation process is as follows: The first step is to add No. 120 solvent oil to the silicone resin for dilution, and add a silicone resin adhesive, a cross-linking agent and a catalyst, and then stir with a high-speed stirrer to obtain a silicone resin solution; In the second step, the antibacterial agent is added to the prepared silicone resin solution in a certain proportion to finally obtain the aluminum foil coating; The third step is to apply the aluminum foil coating on the aluminum foil by gravure coating at a solid content of 1.0 g / ㎡; In the fourth step, the coated aluminum foil is dried in four ovens to obtain a completely dried coated aluminum foil.

2. The method for producing an antimicrobial compound coated aluminum foil according to claim 1, characterized in that: The silicone resin is a colorless, transparent, light-viscosity liquid produced by Dow Corning Company, which has the characteristics of low curing temperature and short curing time, and the curing time is shortened accordingly with the increase of temperature.

3. The method for producing an antimicrobial compound coated aluminum foil according to claim 2, characterized in that: The drying temperature is 135° C.-268° C., the length of the drying tunnel is 9 m, and the rotation speed of the machine is 100 m / min.

4. The method for producing an antimicrobial compound coated aluminum foil according to claim 3, characterized in that: The ratio of the antibacterial agent to the silicone resin solution is 2-5:

100.

5. The method for producing an antimicrobial compound coated aluminum foil according to claim 4, characterized in that: The high-speed mixer is composed of a lifting assembly, a mounting seat (1), an external plate (3), an adjustment seat (10), a rotating shell (11), an electric roller and a plurality of transmission tubes (24); the mounting seat (1) and the external plate (3) are fixedly connected to each other; the lifting assembly is arranged on one side of the external plate (3); the adjustment seat (10) is connected to the lifting mechanism; the rotating shell (11) is fixedly connected to the upper end of the adjustment seat (10); the electric roller is rotatably connected to the lower inner wall of the rotating shell (11); and the plurality of transmission tubes (24) are fixedly connected to the circumferential surface of the electric roller.

6. The method for producing an antimicrobial compound coated aluminum foil according to claim 5, characterized in that: The lifting assembly is composed of a mounting plate (5), a first motor (4), a screw rod (6) and a screw rod nut (7); the mounting plate (5) is fixedly connected to one end of the external plate (3); the first motor (4) is fixedly connected to the lower end of the mounting plate (5); the screw rod (6) is rotatably connected to the upper end of the mounting plate (5); the screw rod nut (7) is threadedly connected to the circumferential surface of the screw rod (6); and the screw rod nut (7) is fixedly connected to one end of the adjustment seat (10).

7. The method for producing an antimicrobial compound coated aluminum foil according to claim 6, characterized in that: The upper end of the mounting plate (5) is fixedly connected to a limiting rod (9), the upper end of the screw nut (7) is provided with a stabilizing hole, and the screw nut (7) is slidably connected to the outer surface of the limiting rod (9) through the stabilizing hole, and the upper end of the limiting rod (9) is fixedly connected to an anti-slip plate (8).

8. The method for producing an antimicrobial compound coated aluminum foil according to claim 7, characterized in that: The gravure coating step comprises a plurality of assembly plates (15), two support plates (16), a transmission device (21), two stabilizing bars (22), a placement plate (17), a second motor (18), a coating roller (23), a scattering tube (26) and a transmission tube (24), wherein the plurality of assembly plates (15) are fixedly connected to the upper end of the mounting base (1), the two support plates (16) are fixedly connected to the adjacent ends of the plurality of assembly plates (15), the placement plate (17) is fixedly connected to one end of one of the support plates (16), and the second motor ( 18) is fixedly connected to one end of the mounting plate (17), the coating roller (23) is rotatably connected to one end of the mounting plate (17), the scattering tube (26) is rotatably connected to one side inner wall of the coating roller (23), the transmission tube (24) movably passes through one side inner wall of the coating roller (23) and is connected to the scattering tube (26), and the transmission tube (24) and the scattering tube (26) are rotatably connected via a rotating shaft, the other end of the transmission tube (24) is fixedly connected to the circumferential surface of the rotating shell (11), and the transmission tube (24) is connected to the rotating shell (11).

9. The method for producing an antimicrobial compound coated aluminum foil according to claim 8, characterized in that: The drying step is composed of a drying shell (19), a plurality of placement grooves and a plurality of dryers (25), wherein the drying shell (19) is fixedly connected to the upper ends of the two supporting plates (16), the plurality of placement grooves are all opened on the inner surface of the drying shell (19), and the plurality of dryers (25) are all fixedly connected to the plurality of placement grooves.

10. The method for producing an antimicrobial compound coated aluminum foil according to claim 9, characterized in that: Both ends of the drying shell (19) are fixedly connected with heat insulation plates (20), the upper end of the rotating shell (11) is rotatably connected with a sealing plate (12) via a rotating shaft, and the upper end of the sealing plate (12) is provided with a hand grip groove (13).

Citation Information

Patent Citations

  • Aluminum foil paper and preparation method thereof

    CN108797219A

  • Preparation equipment and preparation process of aluminum-foil paper antibacterial coating

    CN111501407A

  • Stirring equipment for chemical industry

    CN116059865A

  • Coating device for electrical conduction optimization protective agent

    CN214183785U

  • Stirring device for coating

    CN216878944U