Method for producing heavy soda ash by using low-concentration sodium carbonate solution through one-step method

Heavy soda ash is produced by a low-concentration sodium carbonate solution in one-step method, using MVR evaporation and high-temperature pressure stirring tank dehydration, combined with flash dryer drying, the problems of high-temperature evaporation and complex processes in the existing technology are solved, and energy consumption is reduced and Simplified process.

CN118993110APending Publication Date: 2024-11-22HOHHOT JIUYU RESOURCE RECYCLING TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411231955.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-04
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

In the existing heavy soda ash production process, evaporation and concentration require high temperature pressure evaporation or air heating, resulting in high energy consumption, and the calcined block materials need to be crushed and screened, which has complex process and unreasonable ingredients ratios affect production.

Method used

A heavy soda ash is produced by a low-concentration sodium carbonate solution in one step. After evaporation and crystallization by MVR, solid-liquid separation is performed once, and then dehydrated in a high-temperature pressure stirring tank to avoid the loose crystal shape of sodium carbonate monohydrate under anhydrous conditions. Finally, Drying in a flash dryer simplifies the process and reduces energy consumption.

Benefits of technology

The steam calcination, crushing, screening and fine powder return to ingredients are completely avoided, which significantly reduces energy consumption, simplifies the process flow, and improves production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure BDA0005026440160000071
    Figure BDA0005026440160000071
  • Figure HDA0005026440170000011
    Figure HDA0005026440170000011
Patent Text Reader

Abstract

The invention discloses a method for producing heavy soda ash by using a low-concentration sodium carbonate solution through a one-step method. The method comprises the following steps: S1, evaporative crystallization; s2, primary solid-liquid separation; s3, dehydrating; s4, carrying out secondary solid-liquid separation; and S5, drying. The method has the advantages that after the low-concentration sodium carbonate solution is evaporated, crystallized, evaporated and concentrated to produce sodium carbonate monohydrate, the sodium carbonate monohydrate is subjected to primary solid-liquid separation, part of water is separated out, then the sodium carbonate monohydrate is converted into anhydrous sodium carbonate through high-temperature pressure stirring, and crystal forms are recombined in the conversion process; the condition that the powder is loose and the crystal form is broken after the sodium carbonate monohydrate is dehydrated under the anhydrous condition is completely avoided; and then secondary solid-liquid separation is carried out, and the obtained solid passes through a flash dryer to obtain powdery heavy soda ash, so that four procedures of steam calcination, crushing, screening and returning of fine powder to ingredients are omitted, the technological process is simplified, and the energy consumption is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical field:

[0001] The invention relates to the technical field of dense soda ash production, in particular to a method for producing dense soda ash using a low-concentration sodium carbonate solution in one step. Background technology:

[0002] Our company has developed a process for alkaline leaching of solid waste produced by electrolytic aluminum plants to recover the effective components. The concentration of the sodium carbonate solution obtained after alkaline leaching is about 10%. According to the common technology in the soda ash production industry, MVR is used for evaporation and concentration. After the sodium carbonate reaches the saturated concentration, sodium carbonate monohydrate is crystallized. The sodium carbonate monohydrate is indirectly heated and calcined by high-temperature steam to dehydrate and produce agglomerated anhydrous sodium carbonate. The agglomerated anhydrous sodium carbonate is then crushed and screened to obtain anhydrous sodium carbonate with a bulk density that meets the requirements, that is, heavy soda ash. The sieved fine material must be returned to the ingredients before calcination, and the proportion of ingredients reaches 40%. However, this method requires high-temperature pressure evaporation or air heating calcination at a temperature of 160°C to remove 14.51% of the crystal water after evaporation and concentration, which causes great energy consumption; and the calcined block material needs to be crushed and screened, and the fine powder is returned to the ingredients before calcination. The process is relatively complicated. If the proportion of ingredients is unreasonable, it will lead to insufficient fluidity of the product and affect normal production. Summary of the invention:

[0003] The object of the present invention is to provide a method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution.

[0004] The present invention is implemented by the following technical scheme: a method for producing heavy soda ash in one step using a low-concentration sodium carbonate solution, comprising the following steps:

[0005] S1: Evaporation crystallization

[0006] The low-concentration sodium carbonate is evaporated and concentrated by an MVR evaporator to produce sodium carbonate monohydrate to obtain a crystal slurry;

[0007] S2: Primary solid-liquid separation

[0008] The crystal slurry obtained in S1 is subjected to solid-liquid separation to obtain a sodium carbonate monohydrate slurry having a solid content of 40% to 60%;

[0009] S3: Dehydration

[0010] The sodium carbonate monohydrate slurry separated from S2 is sent to a high-temperature pressure stirring tank, the pressure in the tank is 0.2-0.6MPa, the temperature is 120-160°C, and stirred for 30-150min to obtain a sodium carbonate slurry without crystallization water containing free water;

[0011] S4: Secondary solid-liquid separation

[0012] The sodium hydroxide slurry containing free water and without crystallization water obtained in S3 is subjected to secondary solid-liquid separation;

[0013] S5: Dry

[0014] The solid separated from S4 is dried to obtain a heavy soda ash product.

[0015] Furthermore, in S1, the temperature of MVR evaporation is 90-95°C.

[0016] Furthermore, the primary solid-liquid separation in S2 is carried out in a thickener.

[0017] Furthermore, the secondary centrifugal separation in S4 is performed in a centrifuge.

[0018] Furthermore, the drying in S5 is performed in a flash dryer.

[0019] Furthermore, the flash air inlet temperature of the flash dryer is 160-300°C.

[0020] Furthermore, the mother liquor separated in S2 is sent back to S1 for re-evaporation and crystallization.

[0021] Furthermore, the mother liquor separated in S4 is sent back to S1 for re-evaporation and crystallization.

[0022] The invention has the advantages that a low-concentration sodium carbonate solution is evaporated, crystallized, and concentrated to produce sodium carbonate monohydrate, and then solid-liquid separation is performed to separate part of the water first, and then the sodium carbonate monohydrate is converted into anhydrous sodium carbonate through high-temperature pressure stirring, and the crystal form is recombined during the conversion process, which completely avoids the situation that the powder is loose and the crystal form is broken after the sodium carbonate monohydrate is dehydrated under anhydrous conditions; and then the solid is subjected to secondary solid-liquid separation, and the obtained solid is passed through a flash dryer to obtain powdered heavy soda ash, thereby eliminating four processes of steam calcination, crushing, screening, and fine powder returning to the ingredients, simplifying the process flow, and reducing energy consumption. Description of the drawings:

[0023] Figure 1 The overall structure diagram of the system for producing heavy soda ash from a low-concentration sodium carbonate solution in one step;

[0024] MVR evaporator 1, thickener 2, high temperature and pressure stirring tank 3, flash decompression barrel 4, centrifuge 5, flash dryer 6, low concentration sodium carbonate solution feeding pipe 7, heavy soda ash discharge pipe 8, mother liquor tank 9. Specific implementation method:

[0025] In the description of the present invention, it should be noted that, if the terms "center", "upper", "lower", "left", "right", "vertical", "horizontal", "inner", "outer", etc. appear, the orientation or position relationship indicated is based on the orientation or position relationship shown in the drawings, which is only for the convenience of describing the present invention and simplifying the description, and does not indicate or imply that the device or element referred to must have a specific orientation, be constructed and operated in a specific orientation, and therefore cannot be understood as limiting the present invention. In addition, if the terms "first", "second", "third" appear, they are only used for descriptive purposes and cannot be understood as indicating or implying relative importance.

[0026] Example 1: A method for producing heavy soda ash in one step using a low-concentration sodium carbonate solution, comprising the following steps:

[0027] S1: Evaporation crystallization

[0028] The low-concentration sodium carbonate is evaporated and concentrated by an MVR evaporator to produce sodium carbonate monohydrate to obtain a crystal slurry; the MVR evaporation temperature is 90°C.

[0029] S2: Primary solid-liquid separation

[0030] The crystal slurry obtained in S1 is subjected to solid-liquid separation; specifically, it is carried out in a thickener to obtain a sodium carbonate monohydrate slurry with a solid content of 40%;

[0031] S3: Dehydration

[0032] The sodium carbonate monohydrate slurry separated from S2 is sent to a high-temperature pressure stirring tank with a pressure of 0.2 MPa and a temperature of 120°C, and stirred for 150 minutes to obtain a sodium carbonate slurry without crystallization water containing free water;

[0033] S4: Secondary solid-liquid separation

[0034] The sodium sulfate slurry containing free water and no crystallization water obtained in S3 is subjected to secondary solid-liquid separation; specifically, the separation is carried out in a centrifuge;

[0035] S5: Dry

[0036] The solid separated from S4 is dried. Specifically, the drying is carried out in a flash dryer with a flash air inlet temperature of 160° C. to obtain a heavy soda ash product.

[0037] The mother liquor separated from S2 and S4 is collected and sent back to S1 for re-evaporation and crystallization.

[0038] Example 2: A method for producing heavy soda ash in one step using a low-concentration sodium carbonate solution, comprising the following steps:

[0039] S1: Evaporation crystallization

[0040] The low concentration sodium carbonate is evaporated and concentrated by MVR evaporator to produce sodium carbonate monohydrate to obtain a crystal slurry; the MVR evaporation temperature is 905°C.

[0041] S2: Primary solid-liquid separation

[0042] The crystal slurry obtained in S1 is subjected to solid-liquid separation; specifically, it is carried out in a thickener to obtain a sodium carbonate monohydrate slurry with a solid content of 50%;

[0043] S3: Dehydration

[0044] The solid separated from S2 was sent to a high-temperature pressure stirring tank with a pressure of 0.35 MPa and a temperature of 135°C, and stirred for 90 minutes to obtain a sodium hydroxide slurry containing free water and without crystallization water;

[0045] S4: Secondary solid-liquid separation

[0046] The sodium sulfate slurry containing free water and no crystallization water obtained in S3 is subjected to secondary solid-liquid separation; specifically, the separation is carried out in a centrifuge;

[0047] S5: Dry

[0048] The solid separated from S4 is dried. Specifically, the drying is carried out in a flash dryer with a flash air inlet temperature of 230° C. to obtain a heavy soda ash product.

[0049] The mother liquor separated from S2 and S4 is collected and sent back to S1 for re-evaporation and crystallization.

[0050] Example 3: A method for producing heavy soda ash in one step using a low-concentration sodium carbonate solution, comprising the following steps:

[0051] S1: Evaporation crystallization

[0052] The low-concentration sodium carbonate is evaporated and concentrated by MVR evaporator 1 to produce sodium carbonate monohydrate to obtain a crystal slurry; the MVR evaporation temperature is 93°C.

[0053] S2: Primary solid-liquid separation

[0054] The crystal slurry obtained in S1 is subjected to solid-liquid separation; specifically, it is carried out in a thickener to obtain a sodium carbonate monohydrate slurry with a solid content of 60%;

[0055] S3: Dehydration

[0056] The sodium carbonate monohydrate slurry separated from S2 is sent to a high-temperature pressure stirring tank with a pressure of 0.6 MPa and a temperature of 160°C, and stirred for 30 minutes to obtain a sodium carbonate slurry without crystallization water containing free water;

[0057] S4: Secondary solid-liquid separation

[0058] The sodium sulfate slurry containing free water and no crystallization water obtained in S3 is depressurized and then subjected to secondary solid-liquid separation; specifically, the separation is carried out in a centrifuge;

[0059] S5: Dry

[0060] The solid separated from S4 is dried. Specifically, the drying is carried out in a flash dryer. The flash air inlet temperature of the flash dryer is 300° C. to obtain a heavy soda ash product.

[0061] The mother liquor separated from S2 and S4 is collected and sent back to S1 for re-evaporation and crystallization.

[0062] Comparative Example: A method for producing heavy soda ash from a low-concentration sodium carbonate solution, comprising the following steps:

[0063] S1: After evaporation and concentration of a low concentration sodium carbonate solution, solid-liquid separation is performed to obtain a sodium carbonate monohydrate solid containing 8% free water;

[0064] S2: The sodium carbonate monohydrate solid obtained in S1 is calcined with high-temperature steam at 160°C to remove crystal water and evaporate free water to obtain anhydrous sodium carbonate. The steam calcination efficiency is 75%;

[0065] S3: crushing and screening the anhydrous sodium carbonate obtained in S2 to separate anhydrous sodium carbonate powder with finer particle size, and obtaining a heavy sodium carbonate product with qualified particle size;

[0066] S4: The anhydrous sodium carbonate powder separated in S3 is returned to the high-temperature calcination process for batching, and the calcination, crushing and screening processes are repeated, with a return ratio of 40%.

[0067] The reaction conditions of Examples 1 to 3 and the comparative example are summarized as shown in the following table:

[0068]

[0069] As can be seen from the above table, taking the production of 1 ton of heavy soda ash as an example, starting from the concentration, the methods of Examples 1 to 3 can save more than 46% of energy consumption compared with the comparative example.

[0070] Example 4: Example 1 to Example 3 adopts Figure 1The system implementation of a one-step method for producing heavy soda ash from a low-concentration sodium carbonate solution is shown, the system comprises an MVR evaporator 1, a thickener 2, a high-temperature pressure stirring tank 3, a flash decompression drum 4, a centrifuge 5, and a flash dryer 6, a low-concentration sodium carbonate solution feed pipe 7 is connected to the inlet of the MVR evaporator 1, the outlet of the MVR evaporator 1 is connected to the inlet of the thickener 2, the slurry outlet of the thickener 2 is connected to the inlet of the high-temperature pressure stirring tank 3, the outlet of the high-temperature pressure stirring tank 3 is connected to the inlet of the flash decompression drum 4, the outlet of the flash decompression drum 4 is connected to the inlet of the centrifuge 5, the slurry outlet of the centrifuge 5 is connected to the inlet of the flash dryer 6, and the outlet of the flash dryer 6 is connected to a heavy soda ash discharge pipe 8. The overflow port of the thickener 2 is connected to the inlet of the mother liquor tank 9, the liquid outlet of the centrifuge 5 is connected to the inlet of the mother liquor tank 9, and the outlet of the mother liquor tank 9 is connected to the inlet of the MVR evaporator 1.

[0071] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or replace some or all of the technical features therein with equivalents. However, these modifications or replacements do not cause the essence of the corresponding technical solutions to deviate from the scope of the technical solutions of the embodiments of the present invention.

Claims

1. A method for producing heavy soda ash in one step using a low-concentration sodium carbonate solution, characterized in that: It includes the following steps: S1: Evaporation crystallization The low-concentration sodium carbonate is evaporated and concentrated by an MVR evaporator to produce sodium carbonate monohydrate to obtain a crystal slurry; S2: Primary solid-liquid separation The crystal slurry obtained in S1 is subjected to solid-liquid separation to obtain a sodium carbonate monohydrate slurry having a solid content of 40% to 60%; S3: Dehydration The sodium carbonate monohydrate slurry separated from S2 is sent to a high-temperature pressure stirring tank, the pressure in the tank is 0.2-0.6MPa, the temperature is 120-160°C, and stirred for 30-150min to obtain a sodium carbonate slurry without crystallization water containing free water; S4: Secondary solid-liquid separation The sodium hydroxide slurry containing free water and without crystallization water obtained in S3 is subjected to secondary solid-liquid separation; S5: Dry The solid separated from S4 is dried to obtain a heavy soda ash product.

2. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 1, characterized in that: In S1, the temperature of MVR evaporation is 90-95°C.

3. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 1, characterized in that: The primary solid-liquid separation in S2 is carried out in a thickener.

4. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 1, characterized in that: The secondary centrifugal separation in S4 is performed in a centrifuge.

5. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 1, characterized in that: The drying in S5 is performed in a flash dryer.

6. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 5, characterized in that: The flash inlet air temperature of the flash dryer is 160-300°C.

7. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 1, characterized in that: The mother liquor separated from S2 is sent back to S1 for re-evaporation and crystallization.

8. The method for producing heavy soda ash by one-step method using a low-concentration sodium carbonate solution according to claim 1, characterized in that: The mother liquor separated in S4 is sent back to S1 for re-evaporation and crystallization.