Method and equipment for manufacturing solid oxide electrolytic cell

The activity of solid oxide electrolytic cell materials is improved through plasma etching and surface treatment technology, and the problem of low surface activity of electrolytes and electrodes is solved, the carbon dioxide conversion rate and reaction activity are improved, and the process temperature and equipment aging risks are reduced.

CN118996476APending Publication Date: 2024-11-22SHANGHAI BANGXIN SEMI TECHNOLOGY CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411229495.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-09-03
Publication Date
2024-11-22

AI Technical Summary

Technical Problem

The low surfactivity of electrolytes and electrode materials in existing solid oxide electrolytic cells leads to the problem of low carbon dioxide conversion.

Method used

The surface of electrolyte and electrode materials is modified using plasma etching and surface treatment technology, including plasma etching, plasma surface treatment, low-damage surface treatment and surface activation, to improve the specific surface area and reactive activity of the material.

Benefits of technology

The specific surface area and reactivity of the electrolytes and electrodes in solid oxide electrolytic cells are significantly improved, the carbon dioxide conversion rate is enhanced, the manufacturing process temperature is reduced, and the equipment aging is delayed.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118996476A_ABST
    Figure CN118996476A_ABST
Patent Text Reader

Abstract

The invention discloses a method and equipment for manufacturing a solid oxide electrolytic tank, and relates to the technical field of solid oxide electrolytic tanks. The manufacturing method of the solid oxide electrolytic cell comprises the following steps: preparing electrolyte; performing a surface process on the electrolyte, the surface process including at least one of plasma etching and plasma surface treatment; preparing an electrode on the surface of the electrolyte subjected to the first surface process; and carrying out plasma surface treatment on the solid oxide electrolytic tank. According to the technical scheme provided by the embodiment of the invention, the manufacturing method and equipment have the beneficial effects that the specific surface areas of electrolyte and electrodes in the solid oxide electrolytic tank can be increased, the activation rate of gas free radicals is increased, and the reaction activity is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the technical field of solid oxide electrolytic cells, and in particular to a method and equipment for manufacturing a solid oxide electrolytic cell. Background Art

[0002] Solid Oxide Electrolyzer Cells (SOEC) technology is an application of the reverse process of solid oxide fuel cells, which can convert electrical energy into chemical energy. It has attracted widespread attention from researchers because it uses renewable energy to efficiently synthesize chemicals such as fuels. The solid oxide electrolyzer has a fully solid-state structure, simple electrode reactions, stable system operation, and also has the advantages of high flexibility, long life, low cost, and the use of industrial waste heat. It is of great significance to reduce dependence on fossil energy and improve the ecological environment.

[0003] For solid oxide electrolytic cells used for carbon dioxide conversion, in the traditional manufacturing process, mechanical grinding is used to flatten the electrolyte surface; and conventional activation treatment is used for the solid oxide electrolytic cell. There are problems such as low carbon dioxide conversion rate and low reaction activity. Therefore, a solid oxide electrolytic cell manufacturing method and equipment are urgently needed to improve the above problems. Summary of the invention

[0004] In order to solve the problem in the prior art that the surface activity of electrolytes and electrode materials in solid oxide electrolytic cells is low, which in turn leads to low carbon dioxide conversion rate, the present application proposes a method and equipment for manufacturing a solid oxide electrolytic cell.

[0005] In a first aspect, a method for manufacturing a solid oxide electrolytic cell is provided, comprising:

[0006] preparing electrolyte;

[0007] Performing a first surface process on the electrolyte, wherein the first surface process comprises at least one of plasma etching and plasma surface treatment;

[0008] preparing an electrode on the surface of the electrolyte subjected to the first surface process;

[0009] A second surface treatment is performed on the solid oxide electrolytic cell, wherein the second surface treatment comprises at least one of surface activation and low damage surface treatment.

[0010] Further, a first surface process is performed on the electrolyte, comprising:

[0011] Plasma etching is performed on a first surface and a second surface of the electrolyte, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to carry electrodes;

[0012] Plasma surface treatment is performed on the first surface of the electrolyte and the second surface of the electrolyte after plasma etching.

[0013] Further, the process conditions for performing the first surface process on the electrolyte are:

[0014] Temperature 10℃-300℃; Pressure 1mTorr-100mTorr; Source power 100W-5000W; Bias power 10W-100W.

[0015] Furthermore, the gas used for plasma etching is an inert gas.

[0016] Furthermore, the gas used for plasma surface treatment of the first surface of the electrolyte after plasma etching and the second surface of the electrolyte is at least one of H2, O2, NF3, NH3, and raw material gas.

[0017] Further, a second surface process is performed on the solid oxide electrolytic cell, comprising:

[0018] Low-damage surface treatment for solid oxide electrolytic cells;

[0019] Surface activation of solid oxide electrolytic cells.

[0020] Furthermore, the process conditions for low-damage surface treatment of the solid oxide electrolytic cell are:

[0021] The temperature is 10℃-300℃; the pressure is 10mTorr-10Torr; the source power is 100W-5000W; the bias power is 10W-100W.

[0022] Furthermore, the gas used for low-damage surface treatment of the solid oxide electrolytic cell is at least one of He, N2, H2, O2, Ar, and raw gas.

[0023] Furthermore, the process conditions for surface activation of the solid oxide electrolytic cell are:

[0024] The temperature is 10℃-300℃; the pressure is 1mTorr-100mTorr; the source power is 100W-5000W; the bias power is 10W-100W.

[0025] Furthermore, the gas used for surface activation of the solid oxide electrolytic cell is at least one of H2, O2, NF3, NH3, and raw gas.

[0026] Further, preparing the electrolyte comprises:

[0027] Grinding the electrolyte powder material so that the particle size of the electrolyte powder material is within a first preset range;

[0028] Pressing the electrolyte powder material into an electrolyte;

[0029] The electrolyte is sintered at a high temperature to obtain an electrolyte.

[0030] Furthermore, preparing an electrode on the surface of the electrolyte after the first surface process, comprising:

[0031] Grinding the electrode powder material so that the particle size of the electrode powder material is within a second preset range;

[0032] preparing electrode slurry from electrode powder;

[0033] Applying the electrode slurry to the first surface of the electrolyte and the second surface of the electrolyte respectively, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to support the electrode;

[0034] The electrodes and the electrolyte are heat treated.

[0035] In a second aspect, a solid oxide electrolytic cell manufacturing device is provided, the manufacturing device is used to manufacture the solid oxide electrolytic cell described in the first aspect, comprising: a gas nozzle, an inductively coupled plasma coil, a quartz window, and a heater;

[0036] The quartz window is in a hollow truncated cone shape, the hollow part of the quartz window forms a reaction chamber, the inductively coupled plasma coil surrounds the outer surface of the quartz window, the heater is arranged at the bottom of the reaction chamber, and the gas nozzle is arranged at the top of the reaction chamber.

[0037] The beneficial effect brought about by the technical solution provided in the embodiments of the present application is: through the solid oxide electrolytic cell manufacturing method and equipment recorded in the embodiments of the present application, the specific surface area of ​​the electrolyte and the electrode in the solid oxide electrolytic cell can be increased, the activation rate of gas free radicals can be increased, and the reaction activity can be increased. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] In order to more clearly illustrate the technical solutions in the embodiments of the present application, the drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without creative work.

[0039] Figure 1 It is a schematic diagram of a method for manufacturing a solid oxide electrolytic cell provided in an embodiment of the present application;

[0040] Figure 2 is a schematic diagram of the surface morphology of the electrode material provided in the embodiment of the present application;

[0041] Figure 3is a schematic diagram of the electrolyte crystal structure provided in the embodiment of the present application;

[0042] Figure 4 It is a schematic diagram of a solid oxide electrolytic cell manufacturing device provided in an embodiment of the present application;

[0043] Figure 5 This is a schematic diagram of particle distribution when the solid oxide electrolysis cell manufacturing equipment provided in an embodiment of the present application is working. DETAILED DESCRIPTION

[0044] In order to make the purpose, technical solutions and advantages of this application clearer, the technical solutions in the implementation mode of this application will be clearly and completely described below in conjunction with the drawings in the implementation mode of this application. Obviously, the described implementation mode is only a part of the embodiments of this application, not all embodiments. Based on the embodiments in this application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of this application.

[0045] Unless otherwise defined, the technical terms or scientific terms used in the present disclosure shall have the usual meanings understood by persons with ordinary skills in the field to which the present disclosure belongs. The words "first", "second" and similar words used in the present disclosure do not indicate any order, quantity or importance, but are only used to distinguish different components. Similarly, words such as "one", "one" or "the" do not indicate a quantity limitation, but indicate that there is at least one. The numbers in the drawings of the specification only indicate the distinction between various functional components or modules, and do not indicate the logical relationship between components or modules. Words such as "include" or "comprise" and similar words mean that the elements or objects appearing before the word include the elements or objects listed after the word and their equivalents, without excluding other elements or objects. Words such as "connect" or "connected" and similar words are not limited to physical or mechanical connections, but may include electrical connections, whether direct or indirect. "Up", "down", "left", "right" and the like are only used to indicate relative positional relationships. When the absolute position of the described object changes, the relative positional relationship may also change accordingly.

[0046] Hereinafter, various embodiments according to the present disclosure will be described in detail with reference to the accompanying drawings. It should be noted that in the accompanying drawings, the same reference numerals are given to components having substantially the same or similar structures and functions, and repeated descriptions thereof will be omitted.

[0047] In view of the problem in the prior art that the surface activity of electrolytes and electrode materials in solid oxide electrolytic cells is low, which in turn leads to a low carbon dioxide conversion rate, the present application proposes a method and equipment for manufacturing a solid oxide electrolytic cell.

[0048] In one embodiment, Figure 1 As shown, a method for manufacturing a solid oxide electrolytic cell comprises:

[0049] S100: preparing electrolyte;

[0050] S200: performing a first surface process on the electrolyte, wherein the first surface process includes at least one of plasma etching and plasma surface treatment;

[0051] S300: preparing an electrode on the electrolyte surface after the first surface process is performed;

[0052] S400: performing a second surface treatment on the solid oxide electrolytic cell, wherein the second surface treatment comprises at least one of surface activation and low-damage surface treatment.

[0053] The electrodes include: a positive electrode and a negative electrode.

[0054] Thinning the electrolyte surface using plasma etching can make the electrolyte have good thickness uniformity and better mechanical properties.

[0055] Plasma surface treatment technology is used to activate the electrolyte surface. The concentration of reactive gas free radicals is high, which can significantly improve the reaction activity, thereby increasing the specific surface area of ​​the electrolyte and the electrolyte reaction activity.

[0056] A first surface process is performed on the electrolyte, comprising:

[0057] S210: performing plasma etching on a first surface and a second surface of the electrolyte, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to carry electrodes;

[0058] S220: performing plasma surface treatment on the first surface of the electrolyte and the second surface of the electrolyte after plasma etching.

[0059] The process conditions for performing surface treatment on the electrolyte are:

[0060] Temperature 10℃-300℃; Pressure 1mTorr-100mTorr; Source power 100W-5000W; Bias power 10W-100W.

[0061] The gas used for plasma etching is an inert gas.

[0062] Preferably, the inert gas is Ar.

[0063] The gas used for plasma surface treatment of the first surface of the electrolyte after plasma etching and the second surface of the electrolyte is at least one of H2, O2, NF3, NH3, and raw material gas.

[0064] A second surface process is performed on the solid oxide electrolytic cell, comprising:

[0065] Low-damage surface treatment for solid oxide electrolytic cells;

[0066] Surface activation of solid oxide electrolytic cells.

[0067] The process conditions for low damage surface treatment of solid oxide electrolytic cells are:

[0068] The temperature is 10℃-300℃; the pressure is 10mTorr-10Torr; the source power is 100W-5000W; the bias power is 10W-100W.

[0069] The gas used for low-damage surface treatment of the solid oxide electrolytic cell is at least one of He, N2, H2, O2, Ar, and raw material gas.

[0070] The process conditions for surface activation of solid oxide electrolytic cells are:

[0071] The temperature is 10℃-300℃; the pressure is 1mTorr-100mTorr; the source power is 100W-5000W; the bias power is 10W-100W.

[0072] The gas used for surface activation of the solid oxide electrolytic cell is at least one of H2, O2, NF3, NH3 and raw gas.

[0073] When performing the second surface process on the solid oxide electrolytic cell, the second surface process is performed on the electrolyte and the electrode at the same time to increase the surface porous structure and increase the specific surface area; at the same time, the crystal damage is repaired and the carrier transport channel and the carrier mobility are optimized.

[0074] After the above process, the electrode material is treated with plasma pores, and the specific surface area increases. Figure 2 As shown. Among them, Figure 2 Part (a) shows the surface morphology of the electrode in the solid oxide electrolytic cell manufactured using the conventional process; Figure 2 Part (b) shows the surface morphology of the electrode manufactured by the solid oxide electrolytic cell manufacturing method provided by the present application. The surface voids of the electrode manufactured by the solid oxide electrolytic cell manufacturing method provided by the present application are more uniform and dense, and the specific surface area is increased.

[0075] This is because during the process of manufacturing the solid oxide electrolytic cell provided in the present application, the surface of the electrolyte crystal structure is over-repaired, making the distorted lattice structure regular, such as Figure 3 shown.

[0076] Figure 3 The coordinates in (a) show the crystal orientation.

[0077] Figure 3 Parts (b) and (c) show the lattice repair process and the lattice repair result, respectively.

[0078] The preparation of the electrolyte comprises:

[0079] S110: grinding the electrolyte powder material so that the particle size of the electrolyte powder material is within a first preset range;

[0080] S120: pressing the electrolyte powder material into an electrolyte;

[0081] S130: Sintering the electrolyte at high temperature to obtain an electrolyte.

[0082] The first preset range is used to characterize the particle size range of the electrolyte powder material particles of the compressed electrolyte.

[0083] Preferably, the first preset range is 20-30 nm.

[0084] The electrode is prepared on the electrolyte surface after the first surface process, comprising:

[0085] S310: grinding the electrode powder material so that the particle size of the electrode powder material is within a second preset range;

[0086] S320: preparing electrode powder into electrode slurry;

[0087] S330: applying the electrode slurry to the first surface of the electrolyte and the second surface of the electrolyte respectively, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to support the electrode;

[0088] S340: performing heat treatment on the electrodes and the electrolyte.

[0089] The second preset range is used to characterize the particle size range of the electrode powder material particles for pressing the electrode.

[0090] Preferably, the maximum value of the second preset range is 200 μm.

[0091] The beneficial effects brought about by using the technical solutions provided in the above-mentioned embodiments are as follows: through the solid oxide electrolytic cell manufacturing method and equipment recorded in the embodiments of the present application, the gas free radical activation rate in the manufacturing process of the solid oxide electrolyte can be improved, the specific surface area of ​​the electrolyte and the electrode in the solid oxide electrolytic cell can be increased, and the reaction activity of the solid oxide electrolytic cell during operation can be increased; it is also possible to reduce the temperature of the process of manufacturing the solid oxide electrolytic cell, relax the equipment requirements, and delay the aging of the manufacturing equipment.

[0092] Compared with the traditional manufacturing method of providing energy through a direct current electric field when manufacturing a solid oxide electrolytic cell, the present application uses plasma to provide energy to avoid powering the reaction chamber. Plasma can be generated in various ways, such as through at least one of laser, radio frequency, and microwave.

[0093] Compared with the traditional solid oxide electrolysis cell manufacturing process. It is possible to integrate multiple reactions (activation, surface treatment, CO2 electrolysis process, etc.) and multiple processes (electrolyte thinning, electrolyte activation, electrode surface activation, electrolysis process, etc.) in one reaction chamber, and switch the operation mode of the reaction chamber to achieve the conversion of the process, significantly improving production efficiency, without the need for additional activation devices, and saving production equipment; compared with the conventional electrolysis of CO2, the temperature is as high as 600℃-800℃, this application performs the process under relatively low temperature conditions (10℃-300℃), alleviating the stringent requirements on equipment.

[0094] It should be understood that although Figure 1 The steps in the flowchart are shown in sequence as indicated by the arrows, but these steps are not necessarily executed in the order indicated by the arrows. Unless otherwise specified in this document, there is no strict order restriction for the execution of these steps, and these steps can be executed in other orders. Moreover, Figure 1 At least part of the steps may include multiple sub-steps or multiple stages. These sub-steps or stages are not necessarily executed at the same time, but can be executed at different times. The execution order of these sub-steps or stages is not necessarily sequential, but can be executed in turn or alternately with other steps or at least part of the sub-steps or stages of other steps.

[0095] In other embodiments, Figure 4 As shown, a solid oxide electrolytic cell manufacturing device is used to manufacture the solid oxide electrolytic cell described in the first aspect, comprising: a gas nozzle 100, an inductively coupled plasma coil 200, a quartz window 300, and a heater 400;

[0096] The quartz window 300 is in the shape of a hollow truncated cone. The hollow portion of the quartz window 300 forms a reaction chamber. The inductively coupled plasma coil 200 surrounds the outer surface of the quartz window 300. The heater 400 is disposed at the bottom of the reaction chamber. The gas nozzle 100 is disposed at the top of the reaction chamber.

[0097] A cooling fan 500 is also provided outside the reaction chamber to generate gas convection outside the reaction chamber to cool the reaction chamber.

[0098] At least one layer of ion grid 600 is disposed above the heater 400 , and after being connected to a reference potential, the plasma gas in the reaction chamber is guided to move in a directional manner.

[0099] Preferably, two layers of ion grid are provided.

[0100] Preferably, the ion grid is grounded.

[0101] During operation, the gas distribution in the reaction chamber is as follows: Figure 5 As shown, there are a large number of electrically neutral highly active free radicals between the lower ion grid 610 and the solid oxide electrolysis cell 700; there is a metastable nuclear reaction gas between the lower ion grid 610 and the upper ion grid 620; and there is an activated plasma between the upper ion grid 620 and the reaction chamber.

[0102] The solid oxide electrolytic cell manufactured using the above-mentioned equipment according to the solid oxide electrolytic cell manufacturing method has an increased specific surface area of ​​the electrolyte and the electrode, thereby increasing the reaction activity of the solid oxide electrolytic cell during operation.

[0103] In the process of thinning the electrolyte surface by plasma etching and in the process of activating the electrolyte surface by plasma surface treatment, plasma is generated by the same reaction chamber, and the generated plasma is applied to the surface of the electrolyte and the electrode in the solid oxide electrolytic cell for surface treatment. It is only necessary to change the corresponding reaction gas, temperature, pressure, source power and bias power configuration for the two processes of plasma etching and plasma surface treatment.

[0104] All the above optional technical solutions can be arbitrarily combined to form optional embodiments of the present application, which will not be described one by one here.

[0105] Embodiment 1

[0106] A method for manufacturing a solid oxide electrolytic cell, such as Figure 1 As shown, including:

[0107] S100: preparing electrolyte;

[0108] S200: performing a first surface process on the electrolyte, wherein the first surface process includes at least one of plasma etching and plasma surface treatment;

[0109] S300: preparing an electrode on the electrolyte surface after the first surface process is performed;

[0110] S400: performing a second surface treatment on the solid oxide electrolytic cell, wherein the second surface treatment comprises at least one of surface activation and low-damage surface treatment.

[0111] Embodiment 2

[0112] Based on Example 1,

[0113] A first surface process is performed on the electrolyte, comprising:

[0114] S210: performing plasma etching on a first surface and a second surface of the electrolyte, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to carry electrodes;

[0115] S220: performing plasma surface treatment on the first surface of the electrolyte and the second surface of the electrolyte after plasma etching.

[0116] The process conditions for performing the first surface process on the electrolyte are:

[0117] Temperature 10℃-300℃; Pressure 1mTorr-100mTorr; Source power 100W-5000W; Bias power 10W-100W.

[0118] The gas used for plasma etching is an inert gas.

[0119] Preferably, the inert gas is Ar.

[0120] The gas used for plasma surface treatment of the first surface of the electrolyte after plasma etching and the second surface of the electrolyte is at least one of H2, O2, NF3, NH3, and raw material gas.

[0121] A second surface process is performed on the solid oxide electrolytic cell, comprising:

[0122] Low-damage surface treatment for solid oxide electrolytic cells;

[0123] Surface activation of solid oxide electrolytic cells.

[0124] The process conditions for low damage surface treatment of solid oxide electrolytic cells are:

[0125] The temperature is 10℃-300℃; the pressure is 10mTorr-10Torr; the source power is 100W-5000W; the bias power is 10W-100W.

[0126] The gas used for low-damage surface treatment of the solid oxide electrolytic cell is at least one of He, N2, H2, O2, Ar, and raw material gas.

[0127] The process conditions for surface activation of solid oxide electrolytic cells are:

[0128] The temperature is 10℃-300℃; the pressure is 1mTorr-100mTorr; the source power is 100W-5000W; the bias power is 10W-100W.

[0129] The gas used for surface activation of the solid oxide electrolytic cell is at least one of H2, O2, NF3, NH3 and raw gas.

[0130] The preparation of the electrolyte comprises:

[0131] S110: grinding the electrolyte powder material so that the particle size of the electrolyte powder material is within a first preset range;

[0132] S120: pressing the electrolyte powder material into an electrolyte;

[0133] S130: Sintering the electrolyte at high temperature to obtain an electrolyte.

[0134] The electrode is prepared on the electrolyte surface after the first surface process, comprising:

[0135] S310: grinding the electrode powder material so that the particle size of the electrode powder material is within a second preset range;

[0136] S320: preparing electrode powder into electrode slurry;

[0137] S330: applying the electrode slurry to the first surface of the electrolyte and the second surface of the electrolyte respectively, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to support the electrode;

[0138] S340: performing heat treatment on the electrodes and the electrolyte.

[0139] The beneficial effects brought about by using the technical solutions provided in the above-mentioned embodiments are as follows: through the solid oxide electrolytic cell manufacturing method and equipment recorded in the embodiments of the present application, the gas free radical activation rate in the manufacturing process of the solid oxide electrolyte can be improved, the specific surface area of ​​the electrolyte and the electrode in the solid oxide electrolytic cell can be increased, and the reaction activity of the solid oxide electrolytic cell during operation can be increased; it is also possible to reduce the temperature of the process of manufacturing the solid oxide electrolytic cell, relax the equipment requirements, and delay the aging of the manufacturing equipment.

[0140] The method for manufacturing the solid oxide electrolytic cell described in Example 1 will not be described in detail here.

[0141] Embodiment 3

[0142] A solid oxide electrolytic cell manufacturing device, such as Figure 4 As shown, the solid oxide electrolytic cell described in Example 1 or Example 2 is used to manufacture the solid oxide electrolytic cell, including: a gas nozzle, an inductively coupled plasma coil, a quartz window, and a heater;

[0143] The quartz window is in a hollow truncated cone shape, the hollow part of the quartz window forms a reaction chamber, the inductively coupled plasma coil surrounds the outer surface of the quartz window, the heater is arranged at the bottom of the reaction chamber, and the gas nozzle is arranged at the top of the reaction chamber.

[0144] The solid oxide electrolytic cell manufactured using the above-mentioned equipment according to the solid oxide electrolytic cell manufacturing method has an increased specific surface area of ​​the electrolyte and the electrode, thereby increasing the reaction activity of the solid oxide electrolytic cell during operation.

[0145] The solid oxide electrolytic cell manufacturing method described in Example 1 and Example 2 will not be described in detail here.

[0146] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may also include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.

Claims

1. A method for manufacturing a solid oxide electrolytic cell, characterized in that: include: preparing electrolyte; Performing a first surface process on the electrolyte, wherein the first surface process comprises at least one of plasma etching and plasma surface treatment; preparing an electrode on the surface of the electrolyte subjected to the first surface process; A second surface treatment is performed on the solid oxide electrolytic cell, wherein the second surface treatment comprises at least one of surface activation and low-damage surface treatment.

2. The method for manufacturing a solid oxide electrolytic cell according to claim 1, characterized in that: The performing of a plasma surface treatment on the electrolyte comprises: Plasma etching is performed on a first surface and a second surface of the electrolyte, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to support the electrode; Plasma surface treatment is performed on the first surface of the electrolyte and the second surface of the electrolyte after plasma etching.

3. The method for manufacturing a solid oxide electrolytic cell according to claim 2, characterized in that: The process conditions for performing the first surface process on the electrolyte are: Temperature 10℃-300℃; Pressure 1mTorr-100mTorr; Source power 100W-5000W; Bias power 10W-100W.

4. The method for manufacturing a solid oxide electrolytic cell according to claim 2 or 3, characterized in that: The gas used for the plasma etching is an inert gas.

5. The method for manufacturing a solid oxide electrolytic cell according to claim 2 or 3, characterized in that: The gas used for plasma surface treatment of the first surface of the electrolyte after plasma etching and the second surface of the electrolyte is at least one of H2, O2, NF3, NH3, and raw material gas.

6. The method for manufacturing a solid oxide electrolytic cell according to claim 1, characterized in that: Performing a second surface process on the solid oxide electrolytic cell comprises: performing low-damage surface treatment on the solid oxide electrolytic cell; The solid oxide electrolytic cell is subjected to surface activation.

7. The method for manufacturing a solid oxide electrolytic cell according to claim 6, characterized in that: The process conditions for low-damage surface treatment of the solid oxide electrolytic cell are: The temperature is 10℃-300℃; the pressure is 10mTorr-10Torr; the source power is 100W-5000W; the bias power is 10W-100W.

8. The method for manufacturing a solid oxide electrolytic cell according to claim 6 or 7, characterized in that: The gas used for low-damage surface treatment of the solid oxide electrolytic cell is at least one of He, N2, H2, O2, Ar, and raw material gas.

9. The method for manufacturing a solid oxide electrolytic cell according to claim 6, characterized in that: The process conditions for surface activation of the solid oxide electrolytic cell are: The temperature is 10℃-300℃; the pressure is 1mTorr-100mTorr; the source power is 100W-5000W; the bias power is 10W-100W.

10. The method for manufacturing a solid oxide electrolytic cell according to claim 6 or 9, characterized in that: The gas used for surface activation of the solid oxide electrolytic cell is at least one of H2, O2, NF3, NH3 and raw gas.

11. The method for manufacturing a solid oxide electrolytic cell according to claim 1, characterized in that: The preparation of the electrolyte comprises: Grinding the electrolyte powder material so that the particle size of the electrolyte powder material is within a first preset range; Pressing the electrolyte powder material into an electrolyte; The electrolyte is sintered at a high temperature to obtain the electrolyte.

12. The method for manufacturing a solid oxide electrolytic cell according to claim 1, characterized in that: The step of preparing an electrode on the surface of the electrolyte after the first surface process is performed comprises: Grinding the electrode powder material so that the particle size of the electrode powder material is within a second preset range; preparing the electrode powder into electrode slurry; Applying the electrode slurry to a first surface of the electrolyte and a second surface of the electrolyte respectively, wherein the first surface and the second surface are opposite surfaces of the electrolyte and are used to support the electrode; The electrode and the electrolyte are heat treated.

13. A solid oxide electrolytic cell manufacturing device, characterized in that: The manufacturing equipment is used to manufacture the solid oxide electrolytic cell according to any one of claims 1 to 12, comprising: a gas nozzle, an inductively coupled plasma coil, a quartz window, and a heater; The quartz window is in the shape of a hollow truncated cone, the hollow part of the quartz window forms a reaction chamber, the inductively coupled plasma coil surrounds the outer surface of the quartz window, the heater is arranged at the bottom of the reaction chamber, and the gas nozzle is arranged at the top of the reaction chamber.