Display panel and preparation method thereof

By forming polygonal star holes on the seed layer and performing epitaxial growth, the problems of insufficient In content and uncontrollable V-shaped defects in Micro LED are solved, the luminescence efficiency and manufacturing efficiency of InGaN materials are improved, and high-quality Micro is achieved. LED production.

CN119008653AActive Publication Date: 2024-11-22COSLIGHT YUANXIN (HANGZHOU) OPTOELECTRONICS CO LTD
View PDF 8 Cites 0 Cited by

Patent Information

Application Number
CN202411098049.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-12
Publication Date
2024-11-22
Estimated Expiration
2044-08-12

AI Technical Summary

Technical Problem

In the prior art, the In content in the InGaN quantum well of the Micro LED display panel is difficult to reach more than 35%, resulting in low luminescence efficiency of the red LED and uncontrollable V-shaped defect formation process, affecting the quality and production efficiency of Micro LED.

Method used

The first opening of polygonal star shape is formed on the seed layer, releases stress and promotes doping of In atoms, forms high InGaN materials with high In content through epitaxial growth, controls the number and density of V-shaped defects, and improves the luminescence efficiency of Micro LEDs and manufacturing yield.

Benefits of technology

Through the design of polygonal star holes, the epitaxial growth process is effectively controlled, the doping rate of In is improved, the luminous efficiency and manufacturing efficiency of Micro LED are improved, the problems of insufficient In content and uncontrollable V-shaped defects are solved, and Micro LED is improved quality and production efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119008653A_ABST
    Figure CN119008653A_ABST
Patent Text Reader

Abstract

The display panel comprises a driving substrate layer and a light-emitting element layer which are stacked in the thickness direction, the light-emitting element layer comprises a plurality of Micro LEDs arranged in multiple rows and multiple columns, the light-emitting element layer further comprises a seed layer, a plurality of first open holes are formed in the seed layer, and a plurality of second open holes are formed in the seed layer. A plurality of first open holes are formed in the driving substrate layer, the cross section of each first open hole is of a polygonal star shape, each first open hole is provided with a sharp bottom, an opening of each first open hole faces the driving substrate layer, each Micro LED corresponds to at least one first open hole, second open holes are formed in the portions, corresponding to the first open holes, of the Micro LEDs, and the multiple first open holes are arranged in multiple rows and multiple columns. The invention further provides a preparation method of the display panel. The method has the advantages of being controllable in yield and high in production efficiency.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor technology, and in particular to a display panel and a method for preparing the display panel. Background Art

[0002] Micro LED display panels use Micro LEDs as light-emitting pixels for display. Micro LED display panels have the advantages of self-luminescence, high efficiency, low power consumption, high integration, high stability, and the ability to work around the clock.

[0003] How to improve the production efficiency of Micro LED display panels has always been pursued in this field. Summary of the invention

[0004] The present invention aims to solve one of the technical problems in the related art to a certain extent. To this end, the present invention provides a display panel and a method for preparing the display panel. The method for preparing the display panel has the advantages of controllable yield and high production efficiency.

[0005] In order to achieve the above-mentioned purpose, as a first aspect of the present invention, a display panel is provided, wherein the display panel includes a driving substrate layer and a light-emitting element layer stacked along a thickness direction, the light-emitting element layer includes a plurality of Micro LEDs arranged in multiple rows and columns, wherein the display panel also includes a seed layer, a plurality of first openings are formed on the seed layer, the cross-section of the first opening is configured as a polygonal star, the first opening has a pointed bottom, and the opening of the first opening faces the driving substrate layer, each of the Micro LEDs corresponds to at least one of the first openings, a second opening is formed on the portion of the Micro LED corresponding to the first opening, and the plurality of first openings are arranged in multiple rows and columns.

[0006] Optionally, the light-emitting element layer includes a plurality of pixel units, the pixel units include a plurality of Micro LEDs, and the Micro LEDs in the same pixel unit can emit light of a plurality of different colors.

[0007] Optionally, the pixel unit includes red light Micro LED, blue light Micro LED and green light Micro LED.

[0008] Optionally, the pixel unit includes two green Micro LEDs, and the two green Micro LEDs in the same pixel unit are located in the same column.

[0009] Optionally, the driving substrate layer includes a thin film transistor array layer and an anode pattern layer stacked along the thickness direction, the light-emitting element layer is arranged on the anode pattern layer, the anode pattern layer includes a plurality of anodes, and the plurality of anodes correspond one-to-one to the plurality of Micro LEDs, respectively, and the anodes are electrically connected to the corresponding thin film transistors in the thin film transistor array layer.

[0010] Optionally, the anode pattern layer further comprises a dielectric material layer, on which anode via holes corresponding to the plurality of anodes are formed, and the anodes are filled in the corresponding anode via holes.

[0011] Optionally, the cross-section of the first opening is configured as a hexagonal star.

[0012] Optionally, the sidewall of the first opening is covered with a material for forming the light emitting element layer.

[0013] Optionally, the first opening is filled with a dielectric material.

[0014] As a second aspect of the present invention, a method for preparing a display panel is provided, wherein the method comprises:

[0015] providing a substrate layer;

[0016] forming a seed layer on the substrate layer;

[0017] forming a mask layer on the seed layer;

[0018] Patterning the mask layer to obtain a first mask pattern having a plurality of circular openings;

[0019] Using the first mask pattern as a mask, etching the seed layer to form a plurality of first openings on the seed layer, wherein the cross section of the first opening is a polygonal star, and the cross-sectional area of ​​the first opening gradually decreases from the top to the bottom, and the first opening has a pointed bottom, and the plurality of first openings are arranged in a plurality of rows and columns;

[0020] Epitaxial growth is performed on a side of the seed layer away from the substrate layer to obtain a light-emitting chip including a plurality of Micro LEDs, each of the Micro LEDs corresponds to at least one of the first openings, a second opening is formed on a portion of the Micro LED corresponding to the first opening, and the plurality of first openings are arranged in a plurality of rows and columns;

[0021] The light emitting chip is bound to the driving substrate.

[0022] Optionally, epitaxial growth is performed on a side of the seed layer away from the substrate layer to obtain a light-emitting chip including a plurality of Micro LEDs, including:

[0023] forming a first light-emitting element mask pattern on the seed layer, wherein a plurality of first light-emitting element openings are formed on the first light-emitting element mask pattern, and the first light-emitting element openings correspond to a plurality of first openings;

[0024] Depositing a first light-emitting material to form a Micro LED in the first light-emitting element opening, wherein the light-emitting color of the Micro LED in the first light-emitting element opening matches the first light-emitting material;

[0025] removing the first light emitting element mask pattern to form a first dielectric material layer;

[0026] Patterning the first dielectric material layer to obtain a second light-emitting element mask pattern, wherein a plurality of second light-emitting element openings are formed on the second light-emitting element mask pattern, and the second light-emitting element openings correspond to the plurality of first openings;

[0027] Depositing a second light-emitting material to form a Micro LED in the second light-emitting element opening, wherein the light-emitting color of the Micro LED in the second light-emitting element opening matches the second light-emitting material;

[0028] removing the second light emitting element mask pattern to form a second dielectric material layer;

[0029] Patterning the second dielectric material layer to obtain a third light-emitting element mask pattern, wherein a plurality of third light-emitting element openings are formed on the third light-emitting element mask pattern, and the third light-emitting element openings correspond to the plurality of first openings;

[0030] A third light-emitting material is deposited to form a Micro LED in the third light-emitting element opening, wherein the light-emitting color of the Micro LED in the third light-emitting element opening matches the third light-emitting material.

[0031] Optionally, the step of binding the light emitting chip to a driving substrate includes:

[0032] Forming an anode pattern layer, wherein the anode pattern layer includes a dielectric material layer and a plurality of anodes, wherein a plurality of anode vias penetrating the dielectric material layer along a thickness direction are formed on the dielectric material layer, wherein the plurality of anode vias are arranged in a one-to-one correspondence with the plurality of anode vias, and the plurality of anode vias correspond to the plurality of Micro LEDs in a one-to-one correspondence;

[0033] A thin film transistor array chip is attached, wherein the thin film transistor array chip includes a thin film transistor array layer, the anode is electrically connected to the corresponding thin film transistor in the thin film transistor array layer, and the driving substrate includes the anode pattern layer and the thin film transistor array layer.

[0034] Optionally, the preparation method further comprises:

[0035] removing the substrate layer;

[0036] A transparent electrode layer is formed, wherein the transparent electrode layer is bonded to the seed layer.

[0037] In the embodiment of the present invention, the light emitting element layer is formed on the seed layer by epitaxial growth.

[0038] Before the step of epitaxial growth, a plurality of first openings with a polygonal star-shaped cross section are formed on the seed layer, and each corner is a V-shaped defect to release the stress accumulated in the material system. The stress in the area where the first opening is not formed on the seed layer 211 has been released, so that more In can be doped. Specifically, after the stress generated at the interface is released by the first opening and the second opening, In atoms are more easily doped into the quantum well and grow InGaN materials with a high In content, thereby making the Micro LED emit light at the required wavelength and efficiency, and emit light of the corresponding color.

[0039] Because the first opening is in the shape of a polygonal star, its formation process is easier to control. That is, when preparing the Micro LED provided in the embodiment of the present invention, the number, position and density of V-shaped defects in the seed layer are controlled by forming a polygonal star-shaped first opening, so that the epitaxial growth process can be better controlled, and the doping rate of In can be increased, thereby ultimately improving the yield of Micro LED manufacturing.

[0040] These features and advantages of the present invention will be disclosed in detail in the following specific embodiments and drawings. The best embodiments or means of the present invention will be described in detail in conjunction with the drawings, but they are not intended to limit the technical solutions of the present invention. In addition, there are multiple features, elements, and components that appear in each of the following texts and drawings, and different symbols or numbers are marked for convenience, but they all represent components with the same or similar structures or functions. BRIEF DESCRIPTION OF THE DRAWINGS

[0041] The present invention will be further described below in conjunction with the accompanying drawings:

[0042] Figure 1 A schematic diagram of the structure of a display panel provided by an embodiment of the present invention;

[0043] Figure 2A schematic diagram showing the arrangement of pixel units in a display panel provided by an embodiment of the present invention;

[0044] Figure 3 A schematic diagram of a partial structure of a display panel provided by an embodiment of the present invention;

[0045] Figure 4 is a top view schematic diagram after a first mask pattern is formed on the seed layer;

[0046] Figure 5 yes Figure 4 Schematic diagram of top view;

[0047] Figure 6 is a schematic diagram after the first opening is formed on the seed layer;

[0048] Figure 7 is a schematic top view showing the shape of the first opening;

[0049] Figure 8 is a schematic diagram showing an opening of a first light emitting element in a mask pattern of a first light emitting element;

[0050] Fig. 9 is a schematic top view showing an opening of a first light emitting element;

[0051] Fig.10 is a schematic diagram after a blue light emitting element is formed;

[0052] Fig.11 is a top view schematic diagram showing a blue light emitting element;

[0053] Fig.12 is a schematic diagram showing an opening of a second light emitting element in a mask pattern of the second light emitting element;

[0054] Fig.13 is a schematic top view showing an opening of a second light emitting element;

[0055] Fig.14 is a schematic diagram after forming a green light emitting element;

[0056] Fig.15 is a top view schematic diagram showing a green light emitting element;

[0057] Fig.16 is a schematic diagram after removing the mask pattern of the second light emitting element;

[0058] Fig.17 is a schematic top view after removing the mask pattern of the second light emitting element;

[0059] Fig.18 is a schematic diagram after a dielectric material layer is formed;

[0060] Fig.19is a schematic diagram showing the anode via;

[0061] Fig. 20 is a schematic diagram after the anode is formed;

[0062] Fig.21 It is a schematic diagram showing the chip after the driver circuit board is attached;

[0063] Fig. 22 It is a schematic diagram showing the removal of the base substrate. DETAILED DESCRIPTION

[0064] Embodiments of the present invention are described in detail below, examples of which are shown in the accompanying drawings, wherein the same or similar reference numerals throughout represent the same or similar elements or elements with the same or similar functions. The embodiments in the implementation manner are intended to be used to explain the present invention and should not be construed as limiting the present invention.

[0065] References in this specification to "one embodiment" or "an example" or "an example" mean that a particular feature, structure, or characteristic described in conjunction with the embodiment itself may be included in at least one embodiment of the present patent disclosure. The appearance of the phrase "in one embodiment" in various places in the specification does not necessarily refer to the same embodiment.

[0066] When preparing red light Micro LEDs, epitaxial growth of red light InGaN quantum wells is a difficult point. The main reason is that In atoms are large in size, and when there is a large stress in the material system, it is difficult for In atoms to be doped into the quantum well. In related technologies, a maximum In content of 30% can be achieved. However, red light LEDs require an In content of more than 35% to be realized.

[0067] Therefore, how to increase the In content in the InGaN quantum well has become a technical problem that needs to be solved urgently in this field.

[0068] V-type defects are a type of bulk defect that is common in GaN materials. They are mainly caused by factors such as lattice mismatch. Especially in the preparation process of LED epitaxial structure, due to the low growth temperature, the growth between layers is destroyed, and V-type defects are easily formed in the quantum well area. After the formation of this V-type defect, when the light-emitting element layer is formed, it can make it easier for In atoms to be incorporated into the quantum well, thereby generating red light.

[0069] However, the current technology uses a completely uncontrollable method to form V-shaped defects, resulting in uncontrollable size and density of the V-shaped defects, and therefore cannot be applied to large-scale mass production.

[0070] In view of this, as a first aspect of the present invention, Figure 1As shown, a display panel is provided, the display panel includes a driving substrate layer 100 and a light-emitting element layer 200 stacked in a thickness direction, the light-emitting element layer 200 includes a plurality of Micro LEDs arranged in a plurality of rows and columns, wherein the light-emitting element layer further includes a seed layer 211, and a plurality of first openings 210 are formed on the seed layer 211, such as Figure 2 As shown, the cross section of the first opening 210 is configured as a polygonal star. Figure 1 As shown, the first opening 210 has a pointed bottom, and the opening of the first opening 210 faces the driving substrate layer 100, and each of the Micro LEDs corresponds to at least one first opening 210. Figure 3 As shown, a second opening 221 is formed on the portion of the Micro LED corresponding to the first opening 210, and a plurality of the first openings are arranged in multiple rows and columns.

[0071] In the embodiment of the present invention, a light-emitting element layer (eg, a red light-emitting element layer, a green light-emitting element layer, a blue light-emitting element layer) is formed on the seed layer 211 by epitaxial growth.

[0072] Before the step of epitaxial growth, a plurality of first openings 210 with a polygonal star-shaped cross section are formed on the seed layer 211, and each corner is a V-shaped defect to release the stress accumulated in the material system. The stress in the area where the first opening 210 is not formed on the seed layer 211 has been released, so that more In can be doped. Specifically, after the stress generated at the interface is released by the first opening 210 and the second opening 221, In atoms are more easily doped into the quantum well and grow InGaN materials with a high In content, thereby enabling the Micro LED (for example, red light Micro LED) to emit light at the required wavelength and efficiency, and emit light of the corresponding color (for example, red light with a wavelength of 620-625nm).

[0073] Because the first opening 210 is in the shape of a polygonal star, its formation process is easier to control. That is, when preparing the Micro LED provided by the embodiment of the present invention, the number, position and density of V-shaped defects in the seed layer 211 are controlled by forming the first opening 210 in the shape of a polygonal star, so that the epitaxial growth process can be better controlled, and the doping rate of In can be increased, thereby ultimately improving the yield of manufacturing Micro LEDs.

[0074] The cross-section of the first opening 210 is designed to be a polygonal star. The polygonal star structure means that the edge of the first opening 210 has multiple vertices and edges, and the second opening 221 formed by epitaxial growth is also constructed to have multiple vertices and edges. This structure helps to disperse the stress to multiple points instead of concentrating it at a single location, further reducing stress concentration, thereby improving the quality and luminous efficiency of Micro LED.

[0075] A plurality of first openings 211 form a first opening array, and a plurality of second openings 221 form a second opening array, further enhancing the stress release effect. The first openings 211 in the present application also adopt a more regular array layout, making the stress distribution more uniform, ensuring the accuracy and repeatability of each step of the process during the manufacturing process, thereby improving the manufacturing efficiency and making it easier to mass produce Micro LED chips.

[0076] In the embodiment of the present invention, there is no particular limitation on the specific shape of the first opening 210 , as long as the cross section thereof has a plurality of acute angles to form a V-shaped defect for relieving stress.

[0077] In the embodiment of the present invention, the first opening 210 can be formed on the seed layer 211 by an etching process. By controlling the process parameters during the etching process, different etching ratios can be achieved in different directions to form the first opening 210 on the seed layer 211.

[0078] Optionally, the material of the seed layer 211 may be a metal material or a semiconductor material, and such a material is easy to form a hole with a hexagonal star cross section. Therefore, as an optional embodiment, the cross section of the first opening 210 is a hexagonal star. It should be noted that the shape of the first opening 210 mainly depends on the material of the seed layer 211 and the determination of appropriate etching process conditions, and combined with real-time monitoring and feedback adjustment mechanism, a regular opening shape is prepared on the seed layer 211.

[0079] In the embodiment of the present invention, there is no special limitation on the type of material in the first opening 210. As an optional implementation, the sidewall of the first opening 210 is covered with a material for forming a light-emitting element layer. That is, after the first opening 210 is formed, the light-emitting element layer is directly formed by an epitaxial growth process, thereby reducing the process difficulty and improving the efficiency of preparing Micro LEDs.

[0080] For the display panel, the light-emitting element layer includes a plurality of pixel units, the pixel units include a plurality of Micro LEDs, and the Micro LEDs in the same pixel unit can emit light of a plurality of different colors.

[0081] The pixel unit may include red light Micro LED, green light Micro LED, and blue light Micro LED.

[0082] exist Figure 2 In the embodiment shown in , the pixel unit includes a red Micro LED 220R, two green Micro LEDs 220G, and a blue Micro LED 220B, and the two green Micro LEDs 220G of the same pixel unit are located in the same column to enhance the display effect of the display panel. .

[0083] It should be pointed out that although Figure 2 In the embodiment shown in FIG. 1 , each Micro LED corresponds to four first openings 210 , but the present invention is not limited thereto.

[0084] In the embodiment of the present invention, the specific structure of the driving substrate layer 100 is not particularly limited. The driving substrate layer includes a thin film transistor array layer 110 and an anode pattern layer 120 stacked in the thickness direction, and the light emitting element layer is arranged on the anode pattern layer 120. Fig. 20 As shown, the anode pattern layer 120 includes a plurality of anodes 122, and the plurality of anodes 122 correspond to the plurality of Micro LEDs one by one, and the anodes 122 are electrically connected to the corresponding thin film transistors in the thin film transistor array layer.

[0085] In the embodiment of the present invention, a metal material is used to form the anode 122. Optionally, the material of the anode 122 can be selected from at least one of Al, Cu, Ti, Ni, Au, and Ag.

[0086] The thin film transistor array layer may include a plurality of pixel circuits corresponding to the plurality of Micro LEDs one by one, and the corresponding Micro LEDs may be driven to emit light through the pixel circuits.

[0087] For ease of manufacturing, optionally, Fig. 20 As shown, the anode pattern layer 120 may further include a dielectric material layer 121 , on which anode vias corresponding to a plurality of anodes 122 are formed, and the anodes 122 are filled in the corresponding anode vias.

[0088] In the embodiment of the present invention, there is no particular limitation on the specific material of the dielectric material layer 121, as long as it can serve as an insulating spacer. For example, the material of the dielectric material layer 121 can be selected from one or more dielectric materials such as SiO2, SiNx, SiOCN, and SiOC.

[0089] The dielectric material layer 121 may be a single layer structure or a multi-layer structure formed by stacking multiple sub-layers. Optionally, the thickness of the dielectric material layer 121 is between 500 nm and 2500 nm.

[0090] In the embodiment of the present invention, there is no special limitation on the type of material in the first opening 210. As an optional implementation, the sidewall of the first opening 210 is covered with a material for forming a light-emitting element layer. That is, after the first opening 210 is formed, the light-emitting element layer is directly formed by an epitaxial growth process, thereby reducing the process difficulty and improving the efficiency of preparing Micro LEDs.

[0091] like Fig. 20 As shown, the material of the light-emitting element layer will grow on the side wall of the first opening 210 and the top surface of the seed layer 211. However, during the epitaxial growth process, the growth rate of the side wall of the first opening 210 is much lower than the growth rate of the top surface of the seed layer 211. Therefore, the thickness of the light-emitting element layer 3 grown on the side wall of the first opening 210 is much smaller than the thickness of the light-emitting element layer grown on the top surface of the seed layer 211. The light-emitting element layer grown on the side wall of the first opening 210 can inject more holes into the quantum well, change the light-emitting angle, and reduce the influence of the total reflection angle on the light output, thereby improving the light-emitting efficiency and light-emitting intensity.

[0092] Of course, the embodiment of the present invention is not limited thereto, and the material for forming the light emitting element layer may not be disposed in the first opening. In this embodiment, the dielectric material may be filled in the first opening 210 first.

[0093] In this embodiment, the first opening 210 is filled with a dielectric material, that is, the interior of the first opening 21 is occupied by the dielectric material. Therefore, the light-emitting element layer cannot grow in the first opening 210, but grows on the plane (top surface) of the seed layer 211 not covered by the dielectric material. The prepared Micro LED reduces the leakage channel, improves the electric field distribution, and improves the device reliability.

[0094] How to fill the dielectric material in the first opening 210 will be described below, and will not be described in detail here.

[0095] In the embodiment of the present invention, there is no special limitation on the depth of the first opening 210. Optionally, the depth of the first opening is between 200 nm and 10000 nm.

[0096] When the depth of the first opening 210 is less than 200nm, the hole injection path is limited, making it difficult for holes to be effectively transferred from the electrode to the light-emitting layer, thereby affecting the chip's luminous efficiency and brightness. In addition, the shallower first opening 210 is not convenient for releasing interface stress. When the depth of the first opening 210 is less than 1000nm, the leakage path inside the Micro LED will not be increased, and the current is more likely to pass through the expected path, avoiding the occurrence of leakage.

[0097] In the embodiment of the present invention, the specific structure and material of the light-emitting element layer are not particularly limited. As an optional implementation, the light-emitting element layer includes a superlattice layer, an n-type semiconductor layer, a barrier layer, a quantum well layer and a p-type semiconductor layer stacked in sequence, and the superlattice layer is formed on the seed layer.

[0098] In this embodiment, the superlattice layer is generally composed of thin layers of two or more different materials grown alternately, and the thickness of the thin layer is generally nanometer scale. This structure can introduce periodic potential barriers and potential wells to improve the injection efficiency and transmission characteristics of carriers. The n-type semiconductor layer is an electron-rich layer, which is mainly formed by donor impurity doping. In the LED, the n-type semiconductor layer serves as an electron injection layer, responsible for injecting electrons from the external circuit into the light-emitting area. This layer generally has a high electron mobility and a low resistivity to ensure that electrons can be efficiently transmitted to the quantum well layer. The barrier layer is generally located between the n-type semiconductor layer and the quantum well layer, or between the quantum well layers (if there are multiple quantum wells), and its main function is to limit the recombination of carriers (electrons and holes) in the quantum well layer, thereby improving the radiative recombination efficiency and reducing non-radiative recombination losses. The barrier layer has a higher band gap energy and can form a barrier to carriers, making it easier for them to recombine and emit light in the quantum well layer. The quantum well layer is the core light-emitting region, which is formed by a thinner semiconductor layer (usually a low band gap material) sandwiched between wider barrier layers. Due to the quantum size effect, the carriers (electrons and holes) in the quantum well layer are confined in a two-dimensional space, increasing the probability that they collide with each other and recombine to emit light. By adjusting the thickness, material and composition of the quantum well layer, the emission wavelength and spectral characteristics of the LED can be precisely controlled. The p-type semiconductor layer is a hole-rich layer, which is mainly formed by acceptor impurity doping. In the LED, the p-type semiconductor layer acts as a hole injection layer, responsible for injecting holes from the external circuit into the light-emitting area. Similar to the n-type semiconductor layer, the p-type semiconductor layer also needs to have a high hole mobility and a low resistivity to ensure that the holes can be efficiently transferred to the quantum well layer and recombine with electrons to emit light.

[0099] As a second aspect of the present invention, a method for preparing a display panel is provided, wherein the method comprises:

[0100] In step S210, a substrate layer is provided;

[0101] In step S220, a seed layer is formed on the substrate layer;

[0102] In step S230, a mask layer is formed on the seed layer;

[0103] In step S240, the mask layer is patterned to obtain a first mask pattern having a plurality of circular openings;

[0104] In step S250, the seed layer is etched using the first mask pattern as a mask to form a plurality of first openings on the seed layer, wherein the cross section of the first opening is a polygonal star, and the cross-sectional area of ​​the first opening gradually decreases from the top to the bottom, and the first opening has a pointed bottom, and the plurality of first openings are arranged in a plurality of rows and columns;

[0105] In step S260, epitaxial growth is performed on a side of the seed layer away from the substrate layer to obtain a light-emitting chip including a plurality of Micro LEDs, each of the Micro LEDs corresponds to at least one of the first openings, a second opening is formed on a portion of the Micro LED corresponding to the first opening, and the plurality of first openings are arranged in a plurality of rows and columns;

[0106] In step S270, the light emitting chip is bound to the driving substrate.

[0107] The manufacturing method provided in the embodiment of the present invention can manufacture the display panel provided in the first aspect of the present invention.

[0108] As described above, since the first opening is in the shape of a polygonal star, its formation process is easier to control. That is, when preparing the Micro LED in the light-emitting layer provided in the embodiment of the present invention, the number, position and density of V-shaped defects in the seed layer are controlled by forming a polygonal star-shaped first opening, so that the epitaxial growth process can be better controlled, and the doping rate of In can be increased, thereby ultimately improving the yield of manufacturing Micro LEDs.

[0109] In the embodiment of the present invention, the substrate layer may be a sapphire substrate, a silicon substrate, a silicon carbide substrate or the like.

[0110] In the embodiment of the present invention, the material of the seed layer is not particularly limited. The material of the seed layer can be a metal material such as copper, titanium, or a semiconductor material such as zinc oxide. The seed layer is the basis of epitaxial growth, and is usually a thin film prepared on the surface of the substrate layer by physical vapor deposition, chemical vapor deposition or other methods. The seed layer provides a starting point and guide for the subsequent growth of new crystal materials.

[0111] As an optional implementation, the material of the mask layer is SiO2. In other embodiments, the material of the mask layer may also be selected from SiN X , SiCN, SiOCN, SiOC or one or more thereof. The mask layer is used to isolate and protect a specific area in the seed layer. A corresponding process is selected according to the type of mask layer selected to form the mask layer on the seed layer.

[0112] The mask layer can be formed by any one of chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD). As an optional embodiment, the thickness of the mask layer can be between 50nm and 500nm, and the process temperature of the deposition process can be between 200°C and 750°C.

[0113] like Figure 4 and Figure 5 As shown in , a seed layer 211 is formed on a substrate layer 500, and a mask pattern 400 is formed on the seed layer 211, and a circular opening 410 is formed on the mask pattern 400 and penetrates the mask pattern 400 along the thickness direction. In the embodiment of the present invention, there is no special limitation on the number of first openings corresponding to each light-emitting element. Because the light-emitting element is a MicroLED, the size of the first opening is determined. As an optional embodiment, the diameter of the circular opening 410 can be between 100nm and 2000nm, so that each Micro LED can correspond to at least 4 first openings.

[0114] The mask layer may be patterned by a photolithography process to obtain a mask pattern 400 having a plurality of circular openings. Specifically, an exposure machine may be selected to project the pattern to be produced onto the mask layer, or the desired pattern may be directly engraved onto the mask layer by laser irradiation, and then a plurality of circular openings may be formed on the mask layer by an etching process. It should be noted that after the patterning is completed, the circular openings should penetrate the mask layer along the thickness direction of the mask layer, but the etching depth should also be controlled to avoid etching the seed layer.

[0115] like Figure 6 and Figure 7As shown, by controlling the process parameters during the etching process, different etching ratios can be achieved in different directions to form a polygonal star-shaped first opening 210 on the seed layer 211. The seed layer 211 is etched using the mask pattern as a mask, and a plurality of first openings 210 are formed on the seed layer 211 by precisely controlling the etching process parameters. Specifically, in this embodiment, the cross-section of the first opening 210 is a hexagonal star. In this embodiment, KOH is selected to perform wet etching on the seed layer 211. In other embodiments, one or more solutions of NaOH, NH3OH, DHF, BOE, HCl, and HNO3 may also be selected for wet etching. As described above, the deepest depth of the first opening 210 may be between 200nm and 1000nm.

[0116] After forming the first opening, the mask pattern 400 may be removed. In the embodiment of the present invention, the mask pattern 400 on the seed layer may be removed by dry etching, wet etching, or the like.

[0117] In the embodiment of the present invention, there is no particular limitation on how to specifically perform step S260, as long as multiple types of Micro LEDs can be grown. Figures 8 to 17 As shown in , epitaxial growth is performed on the side of the seed layer away from the substrate layer to obtain a light-emitting chip including a plurality of Micro LEDs, including:

[0118] A first light emitting element mask pattern 410 is formed on the seed layer. A plurality of first light emitting element openings 411 are formed on the first light emitting element mask pattern. The first light emitting element openings 411 correspond to the plurality of first openings 210 (see Figure 8 and Fig. 9 );

[0119] Depositing a first light-emitting material to form a Micro LED in the first light-emitting element opening, wherein the light-emitting color of the Micro LED in the first light-emitting element opening matches the first light-emitting material;

[0120] removing the first light emitting element mask pattern to form a first dielectric material layer;

[0121] The first dielectric material layer is patterned to obtain a second light emitting element mask pattern 420 (see Fig.12 ), a plurality of second light emitting element openings 421 are formed on the second light emitting element mask pattern, and the second light emitting element openings 421 correspond to the plurality of first openings (see Fig.13 );

[0122] Depositing a second light-emitting material to form a Micro LED in the second light-emitting element opening, wherein the light-emitting color of the Micro LED in the second light-emitting element opening matches the second light-emitting material;

[0123] like Fig.16 and Fig.17 As shown, the second light emitting element mask pattern is removed to form a third dielectric material layer;

[0124] Patterning the third dielectric material layer to obtain a third light-emitting element mask pattern, wherein a plurality of third light-emitting element openings are formed on the third light-emitting element mask pattern, and the third light-emitting element openings correspond to the plurality of first openings;

[0125] A third light-emitting material is deposited to form a Micro LED in the third light-emitting element opening, wherein the light-emitting color of the Micro LED in the third light-emitting element opening matches the third light-emitting material.

[0126] The material of the first light emitting element mask pattern 410 can be selected from SiO2, SiN X , one or more of SiCN, SiOCN, and SiOC.

[0127] The first light-emitting element mask pattern 410 can be formed by any one of chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD). As an optional embodiment, the thickness of the first light-emitting element mask pattern 410 can be between 50nm and 500nm, and the process temperature of the deposition process can be between 200°C and 750°C.

[0128] Epitaxial growth is performed on the side of the seed layer 211 away from the substrate layer 500 to obtain a light-emitting element layer. Epitaxial growth is to grow a single crystal film on the seed layer 211 (single crystal substrate), for example, a red light Micro LED. The red light Micro LED 220R grows in accordance with the crystal phase extension of the seed layer 211, and its crystal structure is an extension of the crystal structure of the seed layer 211. By selecting a substrate with a specific crystal direction and orientation, the epitaxial layer can be guided to grow in a specific direction. The crystal quality, thickness and uniformity of the seed layer 211 have an important influence on epitaxial growth. The seed layer 211 with good crystal quality can guide the new crystal material to grow in a specific direction to obtain high-quality crystals. In addition, growth parameters such as temperature, pressure, and atmosphere need to be precisely controlled to ensure that the growth rate and morphology of the crystal meet the requirements. For example, too high a temperature may lead to an increase in crystal defects, while too low a temperature may lead to a too slow growth rate. During the crystal growth process, measures need to be taken to reduce the introduction of impurities and defects. These impurities and defects may have an adverse effect on the electrical, optical and magnetic properties of the crystal.

[0129] The epitaxial growth mechanism of the green light Micro LED 220G and the blue light Micro LED 220B is consistent with the growth mechanism of the red light Micro LED 220R, and will not be described here.

[0130] As an optional implementation, after depositing the material of the first light-emitting element mask pattern, the formed material layer can be smoothed using a CMP process to obtain a first light-emitting element mask layer, and then the first light-emitting element mask layer can be subjected to a composition process (for example, a composition process combining photolithography and dry etching) to obtain a first light-emitting element mask pattern 410.

[0131] Specifically, in Fig.10 and Fig.11 In the embodiment described in, the Micro LED in the opening of the first light-emitting element is a blue light Micro LED 220B. The blue light Micro LED 220B is formed by an epitaxial growth process. The structure of the blue light Micro LED 220B includes but is not limited to a superlattice layer (AlGaN / GaN, 10nm-500nm), an n-type (In) GaN layer (200nm-800nm), a carrier barrier layer AlGaN (5nm-20nm), a high In component quantum well layer InGaN (2nm-10nm), a p-type (In) GaN layer (50-300 nanometers), etc. The process temperature of the epitaxial growth is between 600°C and 1100°C.

[0132] exist Fig.14 and Fig.15 In the embodiment shown in , the Micro LED in the opening of the second light-emitting element is a green Micro LED 220G. The green Micro LED 220G is formed by an epitaxial growth process. The structure of the green Micro LED 220G includes but is not limited to a superlattice layer (AlGaN / GaN, 10nm-500nm), an n-type (In) GaN layer (200nm-800nm), a carrier barrier layer AlGaN (5nm-20nm), a high In component quantum well layer InGaN (2nm-10nm), a p-type (In) GaN layer (50-300 nanometers), etc. The process temperature of the epitaxial growth is between 600°C and 1100°C.

[0133] After the green Micro LED 220G is formed, the second light emitting element mask pattern 420 may be removed by wet etching.

[0134] The material of the third dielectric material layer is selected from SiO2, SiN X, one or more of SiCN, SiOCN, and SiOC.

[0135] The third dielectric material layer can be formed by any one of chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD). As an optional embodiment, the thickness of the third dielectric material layer can be between 50nm and 500nm, and the process temperature of the deposition process can be between 200°C and 750°C.

[0136] As an optional implementation, the third dielectric material may be deposited first, and then polished by a CMP process to obtain a third dielectric material layer.

[0137] In this embodiment, the substrate layer 500 is a silicon substrate. In other embodiments, the substrate may also be a sapphire substrate or a silicon carbide substrate.

[0138] In the embodiment of the present invention, there is no special limitation on how to bind the light emitting chip to the driving substrate. For example, the Micro LED on the light emitting chip can be transferred to the driving substrate by mass transfer to achieve binding. As an optional implementation, Fig. 20 As shown, the step of binding the light emitting chip to the driving substrate includes:

[0139] Forming an anode pattern layer, wherein the anode pattern layer includes a dielectric material layer 121 and a plurality of anodes 122, wherein a plurality of anode vias penetrating the dielectric material layer along a thickness direction are formed on the dielectric material layer 121, wherein the plurality of anode vias are arranged one-to-one in the plurality of anode vias, and the plurality of anode vias correspond one-to-one to the plurality of Micro LEDs;

[0140] like Fig.21 As shown, a thin film transistor array chip is attached, wherein the thin film transistor array chip includes a thin film transistor array layer 110, the anode is electrically connected to the corresponding thin film transistor in the thin film transistor array layer, wherein the driving substrate includes the anode graphic layer and the thin film transistor array layer.

[0141] As an optional implementation, forming the anode pattern layer may include:

[0142] like Fig.18 As shown, a dielectric material layer 121 is formed;

[0143] like Fig.19 As shown, a plurality of anode vias are formed on the dielectric material layer 121;

[0144] like Fig. 20 As shown, a plurality of anodes 122 are formed.

[0145] The material of the dielectric material layer is selected from SiO2, SiN X , one or more of SiCN, SiOCN, and SiOC.

[0146] The dielectric material layer can be formed by any one of chemical vapor deposition (CVD), physical vapor deposition (PVD), and atomic layer deposition (ALD). As an optional embodiment, the thickness of the third dielectric material layer can be between 50nm and 500nm, and the process temperature of the deposition process can be between 200°C and 750°C.

[0147] As an optional implementation, a dielectric material may be deposited first, and then polished using a CMP process to obtain a dielectric material layer.

[0148] It should be noted that the display panel needs to be packaged, and accordingly, the preparation method further includes:

[0149] like Fig. 22 As shown, the substrate layer is removed;

[0150] like Figure 1 As shown, a transparent electrode layer 300 is formed, and the transparent electrode layer 300 is attached to the seed layer.

[0151] As an optional implementation, the substrate layer may be removed by grinding and / or CMP process. The material of the transparent electrode layer 300 may be ITO.

[0152] In the embodiment of the present invention, edge metal electrodes and a protective layer may be further formed and then packaged.

[0153] The above are only specific embodiments of the present invention, but the protection scope of the present invention is not limited thereto. Those skilled in the art should understand that the present invention includes but is not limited to the contents described in the drawings and the above specific embodiments. Any modification that does not deviate from the functional and structural principles of the present invention will be included in the scope of the claims.

Claims

1. A display panel, comprising a driving substrate layer and a light-emitting element layer stacked in a thickness direction, wherein the light-emitting element layer comprises a plurality of Micro LEDs arranged in a plurality of rows and columns, characterized in that: The light-emitting element layer also includes a seed layer, on which a plurality of first openings are formed, the cross-section of the first openings being configured as a polygonal star, the first openings having a pointed bottom, and the openings of the first openings facing the driving substrate layer, each of the Micro LEDs corresponding to at least one of the first openings, a second opening being formed on a portion of the Micro LED corresponding to the first opening, and the plurality of first openings being arranged in multiple rows and columns.

2. The display panel according to claim 1, characterized in that: The light-emitting element layer includes a plurality of pixel units, each of which includes a plurality of Micro LEDs, and the Micro LEDs in the same pixel unit can emit light of a plurality of different colors.

3. The display panel according to claim 2, characterized in that: The pixel units include red light Micro LED, blue light Micro LED and green light Micro LED.

4. The display panel according to claim 3, characterized in that: The pixel unit includes two green Micro LEDs, and the two green Micro LEDs in the same pixel unit are located in the same column.

5. The display panel according to claim 1, characterized in that: The driving substrate layer includes a thin film transistor array layer and an anode pattern layer stacked along the thickness direction, the light-emitting element layer is arranged on the anode pattern layer, the anode pattern layer includes a plurality of anodes, and the plurality of anodes correspond one-to-one to the plurality of Micro LEDs, respectively, and the anodes are electrically connected to the corresponding thin film transistors in the thin film transistor array layer.

6. The display panel according to claim 5, characterized in that: The anode pattern layer further comprises a dielectric material layer, on which anode via holes corresponding to the plurality of anodes are formed, and the anodes are filled in the corresponding anode via holes.

7. The display panel according to any one of claims 1 to 6, characterized in that: The cross section of the first opening is configured as a hexagonal star.

8. The display panel according to any one of claims 1 to 6, characterized in that: The sidewall of the first opening is covered with a material for forming the light emitting element layer.

9. The display panel according to any one of claims 1 to 6, characterized in that: The first opening is filled with a dielectric material.

10. A method for preparing a display panel, characterized in that: The preparation method comprises: providing a substrate layer; forming a seed layer on the substrate layer; forming a mask layer on the seed layer; Patterning the mask layer to obtain a first mask pattern having a plurality of circular openings; Using the first mask pattern as a mask, etching the seed layer to form a plurality of first openings on the seed layer, wherein the cross section of the first opening is a polygonal star, and the cross-sectional area of ​​the first opening gradually decreases from the top to the bottom, and the first opening has a pointed bottom, and the plurality of first openings are arranged in a plurality of rows and columns; Epitaxial growth is performed on a side of the seed layer away from the substrate layer to obtain a light-emitting chip including a plurality of Micro LEDs, each of the Micro LEDs corresponds to at least one of the first openings, a second opening is formed on a portion of the Micro LED corresponding to the first opening, and the plurality of first openings are arranged in a plurality of rows and columns; The light emitting chip is bound to the driving substrate.

11. The preparation method according to claim 10, characterized in that: The step of performing epitaxial growth on a side of the seed layer away from the substrate layer to obtain a light-emitting chip including a plurality of Micro LEDs comprises: forming a first light-emitting element mask pattern on the seed layer, wherein a plurality of first light-emitting element openings are formed on the first light-emitting element mask pattern, and the first light-emitting element openings correspond to a plurality of first openings; Depositing a first light-emitting material to form a Micro LED in the first light-emitting element opening, wherein the light-emitting color of the Micro LED in the first light-emitting element opening matches the first light-emitting material; removing the first light emitting element mask pattern to form a first dielectric material layer; Patterning the first dielectric material layer to obtain a second light-emitting element mask pattern, wherein a plurality of second light-emitting element openings are formed on the second light-emitting element mask pattern, and the second light-emitting element openings correspond to the plurality of first openings; Depositing a second light-emitting material to form a Micro LED in the second light-emitting element opening, wherein the light-emitting color of the Micro LED in the second light-emitting element opening matches the second light-emitting material; removing the second light emitting element mask pattern to form a second dielectric material layer; Patterning the second dielectric material layer to obtain a third light-emitting element mask pattern, wherein a plurality of third light-emitting element openings are formed on the third light-emitting element mask pattern, and the third light-emitting element openings correspond to the plurality of first openings; A third light-emitting material is deposited to form a Micro LED in the third light-emitting element opening, wherein the light-emitting color of the Micro LED in the third light-emitting element opening matches the third light-emitting material.

12. The preparation method according to claim 10, characterized in that: The step of binding the light emitting chip to the driving substrate comprises: Forming an anode pattern layer, wherein the anode pattern layer includes a dielectric material layer and a plurality of anodes, wherein a plurality of anode vias penetrating the dielectric material layer along a thickness direction are formed on the dielectric material layer, wherein the plurality of anode vias are arranged in a one-to-one correspondence with the plurality of anode vias, and the plurality of anode vias correspond to the plurality of Micro LEDs in a one-to-one correspondence; A thin film transistor array chip is attached, wherein the thin film transistor array chip includes a thin film transistor array layer, the anode is electrically connected to the corresponding thin film transistor in the thin film transistor array layer, and the driving substrate includes the anode pattern layer and the thin film transistor array layer.

13. The preparation method according to any one of claims 10 to 12, characterized in that: The preparation method further comprises: removing the substrate layer; A transparent electrode layer is formed, wherein the transparent electrode layer is bonded to the seed layer.

Citation Information

Patent Citations

  • Fluorescent powder-free white light pyramid array nitride-based semiconductor LED and preparation method thereof

    CN106098875A

  • Micro-LED Device structure and manufacture method thereof

    CN108281456A

  • Light-emitting device

    JP2006013500A

  • Method of the pyramid-shaped light emitting diode using a selective electrode

    KR1020160098661A

  • Growth of cubic crystalline phase structure on silicon substrates and devices comprising the cubic crystalline phase structure

    US20170092485A1