4N or more high-purity graphite as well as continuous gas phase preparation method and application thereof
Through the continuous gas phase preparation method, the deep purification of waste graphite is achieved using multi-stage gas phase treatment and synergistic additives, and the problem of difficulty in obtaining high-purity graphite in the existing technology is solved, and graphite with high purity and high tap density is obtained, and waste is reduced. The creation of things.
Patent Information
- Application Number
- CN202411136943.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-19
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2044-08-19
AI Technical Summary
It is difficult to obtain high-purity graphite above 4N, and it is easy to damage the graphitization degree and tap density of the graphite, and the wet process flow is long, the wastewater output is large, and the purification efficiency is not ideal.
Using the continuous gas phase preparation method, the graphite raw material is pretreated in an oxidative atmosphere and medium temperature by the first stage, the second stage is mixed with the synergistic additives in a low oxygen atmosphere and high temperature, and the third stage is treated with chlorine and fluorine gas , positive pressure treatment is carried out in an atmosphere of halogenated hydrocarbons, and the parameters control of each gas phase treatment are combined to achieve deep purification of graphite.
It successfully obtained high-purity graphite with a purity of above 4N, taking into account the good tap density and graphitization degree, and avoided the generation of a large amount of three wastes. The process has no wastewater and the waste gas is easy to deal with.
Smart Images

Figure CN119018889A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of waste graphite regeneration, and in particular relates to the field of ultrapure graphite preparation. Background Art
[0002] Graphite is a strategic resource. Due to its excellent electrical and thermal conductivity, lubricity, high temperature resistance and corrosion resistance, it is widely used in the semiconductor field, new energy, metallurgy, aerospace, refractory materials, nuclear energy and other fields. The higher the purity of graphite, the better its performance and the wider its application in high-tech industries. At present, with the development of the industry, a large amount of waste graphite has been retired year by year in the above-mentioned fields. Due to the high impurity content and damaged microstructure, it is difficult to directly reuse it in specific fields. Therefore, it is urgent to develop new methods for purifying waste graphite.
[0003] For graphite purification, the current mainstream means are acid-base wet method and heat treatment for impurity removal. For example, the Chinese patent document with publication number CN113675492A discloses a method for recovering graphite materials from waste lithium-ion batteries, which specifically records the use of strong alkali to pre-activate waste graphite, and then reactivate the graphite by microwave treatment to obtain graphite materials. The Chinese patent document with publication number CN117096485A discloses a method for selectively separating graphite from waste battery black powder, wherein the waste battery black powder containing graphite and positive electrode active material is slurried with water to obtain slurry, and then O3 is blown into the slurry and subjected to the first stage of modification treatment under light irradiation with a wavelength of 100 to 160 nm, and then a modifier is added for the second stage of modification treatment, and then a frother is added for flotation treatment; a graphite concentrate and a flotation tailing of positive electrode active material are obtained. For another example, a Chinese patent document with publication number CN118198570A discloses a high-rate recycled graphite negative electrode material, a preparation method and an application thereof, which specifically records that the waste graphite negative electrode sheet is cleaned with dimethyl carbonate, dried, and tapped to separate the waste graphite from the copper foil to obtain graphite to be recycled; then the graphite to be recycled is calcined at medium and high temperatures to obtain purified graphite.
[0004] In summary, the existing methods for treating waste graphite are mainly to regenerate it into negative electrode materials. This treatment idea and method is difficult to obtain high-purity graphite above 4N. In addition, it is easy to produce more three wastes. Summary of the invention
[0005] In view of the problem that it is difficult to obtain ultra-high purity graphite in the existing recycling process of waste graphite materials, the present invention provides a method for preparing high-purity graphite above 4N, aiming to prepare high-purity graphite above 4N that is suitable for higher application requirements.
[0006] The second object of the present invention is to provide high-purity graphite with a purity of 4N or above obtained by the preparation method.
[0007] The third object of the present invention is to provide an application of the high-purity graphite with a purity of 4N or above.
[0008] The existing wet method of waste graphite has a long process, a large amount of wastewater output, and the purification efficiency and effect as well as the carbon yield are not ideal. It is difficult to stably obtain high-purity graphite above 4N. In addition, the existing purification method is also easy to damage the graphitization degree and tap density of the graphite. In view of this problem, the present invention has been studied in depth and provides the following solution:
[0009] A continuous gas phase preparation method for high-purity graphite above 4N, wherein the graphite raw material is preliminarily subjected to a first stage treatment under atmosphere A and temperature T1 to obtain a first stage material; the atmosphere A is an oxidizing atmosphere; the temperature T1 is 400-600°C;
[0010] The first-stage material and the synergistic additive are mixed and placed in an atmosphere furnace, and the second-stage treatment is performed in advance under atmosphere B and temperature T2 to obtain the second-stage material; then the atmosphere in the atmosphere furnace is switched to atmosphere C and the third-stage treatment is performed at temperature T3 and positive pressure to obtain high-purity graphite above 4N;
[0011] The synergistic additives include chloride and fluoride, the atmosphere B is a low-oxygen atmosphere with an oxygen content of less than 10v%; the temperature T2 is 900-1200°C;
[0012] The atmosphere C contains at least one functional gas selected from chlorine, fluorine and halogenated hydrocarbons, and the temperature T3 is 1300-1700°C.
[0013] The present invention provides a concept for gas-phase purification of graphite by continuous gas change, which combines the three-stage gas phase treatment process from the first stage to the third stage, and further cooperates with the joint control of parameters such as the atmosphere and temperature of each gas phase treatment, so as to achieve synergy, and can achieve deep purification of graphite based on the full atmosphere treatment method, and can obtain high-purity graphite with a purity of more than 4N and good tap density and degree of graphitization at a high carbon yield. In addition, the method of the present invention can avoid the output of a large amount of three wastes.
[0014] In the present invention, the graphite raw material is a graphite raw material with a graphite content of more than 95wt.%;
[0015] In the present invention, the graphite raw material includes waste graphite materials separated from waste batteries and waste semiconductors.
[0016] In the present invention, the atmosphere A is an atmosphere containing at least one of oxygen, ozone, carbon monoxide, and water, preferably an oxygen / water mixture, and further an oxygen / water mixture with a volume ratio of 1:0.5 to 2. The present invention shows that the use of the oxygen / water mixture for the first stage of treatment is conducive to further synergy with the subsequent gas phase treatment process, further optimizes the interlayer and surface of the graphite, improves the purification effect of the graphite, and is conducive to obtaining graphite with a high degree of graphitization and a tap density.
[0017] In the present invention, the temperature T1 may be 430 to 580°C.
[0018] In the present invention, the treatment time of the first stage treatment is 5 to 12 hours, and can further be 6 to 8 hours.
[0019] In the present invention, after the first stage of treatment, the particles may be crushed, for example, to a D50 not higher than 50 μm, and further to 25 to 45 μm.
[0020] In the present invention, the first-stage material and the synergistic auxiliary agent are mixed and placed in an atmosphere furnace, and the second stage of heat preservation is carried out in advance under atmosphere B and temperature T2, and then the atmosphere is switched to atmosphere C and pressurized at temperature T3 for the third stage of heat preservation.
[0021] In the present invention, in the synergistic auxiliary agent, the chloride includes one or more of sodium chloride, potassium chloride, lithium chloride, choline chloride, ammonium chloride, tetrapropylammonium chloride, methylammonium chloride, tetramethylammonium chloride, tetraethylammonium chloride, octadecyltrimethylammonium chloride, and thiopheneethylammonium chloride.
[0022] In the present invention, the fluoride includes one or more of fluorophosphate, hexafluorophosphate, sodium hexafluorophosphate, ammonium hexafluorophosphate, sodium monofluorophosphate, potassium hexafluorophosphate, lithium hexafluorophosphate, lithium difluorophosphate, nitrogen hexafluorophosphate, and methylamine hexafluorophosphate.
[0023] In the present invention, in the synergistic auxiliary agent, the weight portion of the chloride is 0.2 to 5 parts, further 1 to 3 parts; the weight portion of the fluoride is 0.1 to 20 parts, further 1 to 2 parts.
[0024] In the present invention, the synergistic auxiliary agent also includes a boron-containing auxiliary agent, which is further one or more of boron oxide, boron phthalate, boron trichloride, boron carbide, triethyl boron, boron trichloride, iron boride, magnesium boride, cobalt boride, nickel boride, potassium triethyl borohydride, sodium fluoroborate, fluoroboric acid, ammonium fluoroborate, potassium fluoroborate, lithium tetrafluoroborate, imidazole tetrafluoroborate, and nitric tetrafluoroborate.
[0025] The present invention also shows that the use of a synergistic additive containing a boron additive can further enhance the purification effect of graphite, and is helpful in obtaining ultra-high purity graphite above 6N with a better degree of graphitization and tap density.
[0026] In the present invention, the weight portion of the boron-containing auxiliary agent in the synergistic auxiliary agent is less than or equal to 2 parts, and further 0.5 to 2 parts.
[0027] In the present invention, the weight ratio of the first stage material to the synergistic auxiliary agent is 100:0.1-10, further 100:0.5-2.
[0028] In the present invention, atmosphere B is air or oxygen diluted by a diluent gas; wherein the diluent gas includes at least one of nitrogen and an inert gas.
[0029] In the present invention, the oxygen content of atmosphere B is 2-5%.
[0030] In the present invention, T2 may further be 950 to 1150°C.
[0031] In the present invention, the second treatment period is 5 to 10 hours.
[0032] In the present invention, the second-stage material is pressurized in atmosphere C and temperature T3, which helps to synergistically enhance the purification effect of graphite, optimize its physical and chemical structure and carbon yield, and obtain ultra-high purity graphite with excellent tap density and degree of graphitization.
[0033] In the present invention, in the atmosphere C, the halogenated hydrocarbon is methane substituted with 2 to 3 halogens, or ethane substituted with 3 to 5 halogens. The halogen contains at least F and optionally Cl.
[0034] In addition to the functional gas, a diluent gas is also allowed to exist, and the diluent gas includes, for example, at least one of nitrogen and an inert gas.
[0035] In the present invention, the content of the functional gas in the atmosphere C may be 0.002 to 1%, and further may be 0.01 to 0.1%.
[0036] In the present invention, the positive pressure of the third treatment stage is above 1.5 atm (atm refers to standard atmospheric pressure), preferably 1.5 atm to 5 atm;
[0037] Preferably, the third treatment period is 8 to 12 hours.
[0038] In the present invention, after the third stage of treatment is completed, the step of switching the atmosphere in the atmosphere furnace to atmosphere D is also included, and then performing a fourth stage of treatment at a temperature T4 to obtain ultra-high purity graphite above 6N.
[0039] The present invention also shows that, based on the three-stage gas phase treatment, further coordination with the fourth stage gas phase treatment and the combined control of temperature and atmosphere can further enhance the purification effect and help to further obtain ultra-high purity graphite.
[0040] In the present invention, the atmosphere D is an atmosphere containing F-containing hydrocarbon gas;
[0041] The temperature T4 is 2600-3000°C;
[0042] Preferably, in the atmosphere D, the F-containing hydrocarbon gas is a C1-C3 alkane containing at least F and at least one H not replaced by a halogen; the halogen includes F and / or Cl;
[0043] Further, the F-containing hydrocarbon gas is a gas having a structure of formula 1;
[0044]
[0045] In the formula 1, among R1 to R3, at least one substituent is H or contains an H substituent, and the remaining substituents are halogen, methylene partially replaced by halogen, or methylene completely replaced by halogen; the halogen is Cl or F. Furthermore, the F-containing hydrocarbon gas is methane or ethane containing 1 to 2 CH groups that are not replaced by halogen.
[0046] In addition to the F-containing hydrocarbon gas, the atmosphere D also contains a diluent gas, and the diluent gas includes at least one of nitrogen and an inert gas. There is no particular requirement for the content of the F-containing hydrocarbon gas in the atmosphere D, and for example, it can be 0.001 to 0.1 v%, and further can be 0.002 to 0.005 v%.
[0047] Preferably, the fourth treatment period is 12 to 24 hours, and further 15 to 20 hours.
[0048] The present invention also includes high-purity graphite with a purity of 4N or above obtained by the preparation method.
[0049] The present invention also provides an application of high-purity graphite with a purity of 4N or above obtained by the preparation method, which is used to prepare at least one of high-purity silicon carbon, nuclear graphite, high-purity silicon carbide and fluorinated graphite.
[0050] In the present invention, the high-purity graphite of the present invention can be used to prepare products in graphite application scenarios with higher purity requirements based on existing conventional means.
[0051] The present invention also provides a product comprising the high-purity graphite with a purity of 4N or above obtained by the preparation method or made from the high-purity graphite.
[0052] Beneficial effects:
[0053] The present invention provides a method for preparing high-purity graphite by continuous gas change, which combines the three gas phase treatment processes of the first to third stages, and further cooperates with the joint control of parameters such as the atmosphere and temperature of each gas phase treatment, so as to achieve synergy, and can achieve deep purification of graphite based on the treatment method of the whole atmosphere, and can obtain high-purity graphite with a purity of more than 4N. In addition, the method of the present invention can avoid a large amount of three wastes. The research of the present invention also shows that the further joint control of the atmosphere of the first stage treatment, the boron-containing auxiliary agent and the fourth stage gas phase treatment process can further enhance the purification effect of graphite.
[0054] The process described in the present invention is a pure gas phase process, has no waste water, and the waste gas is easy to treat. BRIEF DESCRIPTION OF THE DRAWINGS
[0055] Figure 1 This is a SEM image of the graphite raw material before treatment in Example 1;
[0056] Figure 2 This is a SEM image of high-purity graphite after treatment in step 3 of Example 1;
[0057] Figure 3 This is a SEM image of high-purity graphite after treatment in step 4 of Example 1;
[0058] Figure 4 This is the XRD diagram of the high-purity graphite after treatment in step 4 of Example 1. DETAILED DESCRIPTION
[0059] The specific steps of the present invention are described below by way of examples. It should be understood that these examples are only for illustrating the present invention and are not intended to limit the scope of the present invention in any way. Various processes and methods not described in detail in the present invention are conventional methods known in the art.
[0060] The graphite raw material described in the present invention can be any raw material mainly containing graphite, for example, it can be waste graphite recovered from waste batteries.
[0061] In the present invention, there is no special requirement for the graphite content in the waste graphite, but considering the processing efficiency and effect, it is further preferably above 95wt.%, and can further be 98±1wt.%. In the following cases, as typical examples that can be implemented, unless otherwise stated, the selected graphite raw materials refer to graphite materials recycled from waste lithium-ion batteries and semiconductor industries, and the graphite purity is 98.2±0.2wt.%.
[0062] The optional waste graphite purification step of the present invention comprises:
[0063] Step 1: placing the graphite raw material in an atmosphere furnace, introducing atmosphere A and performing the first stage treatment at temperature T1, then taking out the material and crushing it to obtain a first stage material;
[0064] Step 2: After the first-stage material and the additive are evenly mixed, they are placed in an atmosphere furnace, atmosphere B is introduced, the temperature is raised to T2, and the temperature is kept for the second stage of treatment;
[0065] Step 3: Then switch the gas in the atmosphere furnace to atmosphere C, continuously program the temperature to T3, and pressurize and keep warm for the third stage of treatment to obtain three-stage material;
[0066] An optional scheme further includes step 4. After step 3, the gas is switched to atmosphere D, the system returns to normal pressure, the temperature is continuously raised to T4, the temperature is kept, and the system is naturally cooled to room temperature to obtain ultra-high purity graphite.
[0067] The gas A in step 1 is one or more of oxygen, ozone, carbon monoxide, and water, preferably an oxygen / water mixture containing water vapor. The pretreatment temperature in step 1 is 400-600°C, and the holding time is 5-12h. The D50 of the particles after crushing in step 1 is not higher than 50μm.
[0068] The auxiliary agent in step 2 is a chloride, a fluorine-containing auxiliary agent, and optionally includes a boron-containing auxiliary agent.
[0069] The chloride may be one or more of sodium chloride, potassium chloride, lithium chloride, choline chloride, ammonium chloride, tetrapropylammonium chloride, methylammonium chloride, tetramethylammonium chloride, tetraethylammonium chloride, octadecyltrimethylammonium chloride, and thiopheneethylammonium chloride.
[0070] The fluorine-containing auxiliary agent can be one or more of fluorophosphoric acid, hexafluorophosphoric acid, sodium hexafluorophosphate, ammonium hexafluorophosphate, sodium monofluorophosphate, potassium hexafluorophosphate, lithium hexafluorophosphate, lithium difluorophosphate, nitrogen hexafluorophosphate, and methylamine hexafluorophosphate.
[0071] The boron-containing additive is one or more of boron oxide, boron phthalate, boron trichloride, boron carbide, triethyl boron, boron trichloride, iron boride, magnesium boride, cobalt boride, nickel boride, potassium triethyl borohydride, sodium fluoroborate, fluoroboric acid, ammonium fluoroborate, potassium fluoroborate, lithium tetrafluoroborate, imidazole tetrafluoroborate, and nitric tetrafluoroborate.
[0072] In step 2, the mass ratio of the first-stage material to the chloride is 100:0.2-5, the mass ratio of the first-stage material to the fluorine-containing additive is 100:0.1-2, and the mass ratio of the first-stage material to the boron-containing additive is 100:0.5-2.
[0073] The heating rate described in step 2 is 2-10°C / min, atmosphere B refers to a mixed gas of oxygen and inert gas (one or more of nitrogen, argon, helium), in which the volume fraction of oxygen is 2-5%; the insulation temperature is 900-1200°C, and the insulation time is 5-10h.
[0074] In step three, the atmosphere C is one or more of chlorine, fluorine, and halogenated hydrocarbons, with a volume fraction of 0.002-1%, and the remaining gas is an inert gas; the heating rate is 2-5°C / min, the system pressure is 1.2-3atm, the insulation temperature is 1300-1700°C, and the insulation time is 8-12h.
[0075] The atmosphere D described in step 4 is a F-containing hydrocarbon gas with a volume fraction of 0.001-0.01%, and the remaining gas is an inert gas; the heating rate is 2-5°C / min, the insulation temperature is 2600-3000°C, and the insulation time is 12-24h.
[0076] The following is a specific implementation plan:
[0077] Example 1
[0078] Step 1: Place the graphite raw material in an atmosphere furnace, introduce gas A (oxygen in this case) and keep it at temperature T1 (450±10℃ in this case) for 8h, then crush it to D50 of 30.5μm to obtain a section of material;
[0079] Step 2: After the first-stage material and the auxiliary agent are evenly mixed, they are placed in an atmosphere furnace, gas B (3v% oxygen-Ar mixed gas) is introduced, the temperature is raised to T2 (1000℃±20℃) at a rate of 5℃ / min, and the temperature is kept for 8 hours; the auxiliary agent includes chloride (choline chloride) and fluoride (fluorophosphoric acid) in a weight ratio of 1:1; the weight ratio of the first-stage material and the auxiliary agent is 100:0.5;
[0080] Step 3: After the treatment in step 2 is completed, the atmosphere is switched to gas C (0.01v% F2-Ar mixed gas), the temperature is raised to T3 (1400℃±20℃) at a rate of 5℃ / min, and kept at a pressure of 2atm for 10h; three-stage material is obtained;
[0081] Step 4: After step 3, switch the atmosphere to gas D (0.005v% formula A -Ar mixed gas), and restore the pressure in the atmosphere furnace to normal pressure, raise the temperature to T4 (2700℃±50℃) at a rate of 5℃ / min and keep it for 20h; cool naturally to room temperature to obtain ultra-high purity graphite.
[0082] In the present invention, the purity of the graphite of the three-stage material is 99.994% (4N grade), and the purity of the ultra-high purity graphite in step 4 is 99.99992% (6N grade). The further effects of the obtained graphite are shown in Table 1.
[0083] Example 2
[0084] Compared with Example 1, the only difference is that the conditions of step 1 are changed, and the experimental groups are:
[0085] Group A: atmosphere A is water vapor atmosphere;
[0086] Group B: atmosphere A is a water vapor-oxygen mixture with a volume ratio of 1:1;
[0087] Group C: The temperature T1 is 550℃±10℃, the holding time is 6h, and the particles are crushed to D50 of 41.5μm after holding.
[0088] Other operations and parameters are the same as in Example 1.
[0089] Example 3
[0090] Compared with Example 1, the only difference is that the conditions of step 2 are changed, and the experimental groups are:
[0091] Group A: The chloride in the auxiliary agent is sodium chloride, and the fluoride is hexafluorophosphoric acid; the weight ratio of chloride to fluoride is 2:1; the weight ratio of the first-stage material to the auxiliary agent is 100:1;
[0092] Group B: The additives also include a boron-containing additive (boron oxide), wherein the weight ratio of chloride, fluoride, and boron-containing additive is 1:1:1; the weight ratio of the first-stage material to the additive is 100:0.5;
[0093] Group C: The additives include tetraethylammonium chloride (chloride), sodium fluoroborate (boride), and potassium hexafluorophosphate (fluoride) in a mass ratio of 1:1:1.
[0094] Group D: atmosphere B is 4% oxygen-Ar atmosphere, wherein the temperature T2 is (1100℃±20℃), and the holding time is 6h;
[0095] Other operations and parameters are the same as in Example 1.
[0096] Example 4
[0097] Compared with Example 1, the only difference is that the conditions of step 3 are changed, and the experimental groups are:
[0098] Group A: Atmosphere C is 0.1v% chlorine-Ar mixed gas, T3 is 1500±20℃, insulation pressure is 3atm, and insulation time is 5h;
[0099] Group B: Atmosphere C is 0.05v% halogenated hydrocarbon (formula A-Ar mixed gas, and T3 is 1600±20℃, the insulation pressure is 2atm, and the insulation time is 6h;
[0100] Other operations and parameters are the same as in Example 1.
[0101] Example 5
[0102] Compared with Example 1, the only difference is that the conditions of step 4 are changed, and the experimental groups are:
[0103] Step 4: After step 3, switch the atmosphere to gas D (0.003v% formula B -Ar mixed gas), and restore the pressure in the atmosphere furnace to normal pressure, raise the temperature to T4 (2800℃±50℃) at a rate of 4℃ / min and keep it for 15h; cool naturally to room temperature to obtain ultra-high purity graphite.
[0104] Comparative Example 1
[0105] Compared with Example 1, the only difference is that step 1 is omitted, and the graphite raw material is directly used as the raw material for step 2 and subsequent treatment. Other operations and parameters are the same as in Example 1.
[0106] Comparative Example 2
[0107] Compared with Example 1, the only difference is that in step 2, an auxiliary agent is missing. Other operations and parameters are the same as in Example 1.
[0108] Comparative Example 3
[0109] Compared with Example 1, the only difference is that in step 2, the auxiliary agent is a single chloride, and the amount of the auxiliary agent and other conditions are the same as in Example 1. Other operations and parameters are the same as in Example 1.
[0110] Comparative Example 4
[0111] Compared with Example 1, the only difference is that in step 2, the auxiliary agent is a single fluoride, and the amount of the auxiliary agent and other conditions are the same as in Example 1. Other operations and parameters are the same as in Example 1.
[0112] Comparative Example 5
[0113] Compared with Example 1, the only difference is that step 3 is missing. Other operations and parameters are the same as in Example 1.
[0114] Comparative Example 6
[0115] Compared with Example 1, the only difference is that in step 3, the pressure in the treatment stage is normal pressure. Other operations and parameters are the same as in Example 1.
[0116] The results of each embodiment are shown in Table 1;
[0117] Table 1
[0118]
[0119] The results of each comparative example are shown in Table 2
[0120] Table 2
[0121]
[0122] It can be seen from Table 1 and Table 2 that in each Example 1 of the present invention, 6N grade ultra-high purity graphite can be obtained. Not only that, it also takes into account the high carbon yield, high graphitization purity and tap density that are difficult to achieve in the industry.
Claims
1. A continuous gas phase preparation method for high purity graphite above 4N, characterized in that: The graphite raw material is pre-treated in the first stage under the atmosphere A and the temperature T1 to obtain a first stage material; the atmosphere A is an oxidizing atmosphere; the temperature T1 is 400-600°C; The first-stage material and the synergistic additive are mixed and placed in an atmosphere furnace, and the second-stage treatment is performed in advance under atmosphere B and temperature T2 to obtain the second-stage material; then the atmosphere of the atmosphere furnace is switched to atmosphere C and the third-stage treatment is performed at temperature T3 and positive pressure to obtain high-purity graphite above 4N; The synergistic additives include chloride and fluoride, the atmosphere B is a low-oxygen atmosphere with an oxygen content of less than 10v%; the temperature T2 is 900-1200°C; The atmosphere C contains at least one functional gas selected from chlorine, fluorine and halogenated hydrocarbons, and the temperature T3 is 1300-1700°C.
2. The continuous gas phase preparation method of 4N or higher high purity graphite according to claim 1, characterized in that: The graphite raw material is a graphite raw material with a graphite content of more than 95wt.%; Preferably, the graphite raw material includes waste graphite materials separated from waste batteries and waste semiconductors.
3. The continuous gas phase preparation method of 4N or higher high purity graphite according to claim 1, characterized in that: The atmosphere A is an atmosphere containing at least one of oxygen, ozone, carbon monoxide and water, preferably an oxygen / water mixture; Preferably, the treatment time of the first treatment is 5 to 12 hours.
4. The continuous gas phase preparation method of 4N or higher high purity graphite according to claim 1, characterized in that: In the synergistic auxiliary agent, the chloride includes one or more of sodium chloride, potassium chloride, lithium chloride, choline chloride, ammonium chloride, tetrapropylammonium chloride, methylammonium chloride, tetramethylammonium chloride, tetraethylammonium chloride, octadecyltrimethylammonium chloride, and thiopheneethylammonium chloride; Preferably, the fluoride includes one or more of fluorophosphate, hexafluorophosphate, sodium hexafluorophosphate, ammonium hexafluorophosphate, sodium monofluorophosphate, potassium hexafluorophosphate, lithium hexafluorophosphate, lithium difluorophosphate, nitrogen hexafluorophosphate, and methylamine hexafluorophosphate; Preferably, in the synergistic auxiliary agent, the weight portion of the chloride is 0.2 to 5 parts, and the weight portion of the fluoride is 0.1 to 20 parts; Preferably, the synergistic auxiliary agent further comprises a boron-containing auxiliary agent, which is further one or more of boron oxide, boron phthalate, boron trichloride, boron carbide, triethyl boron, boron trichloride, iron boride, magnesium boride, cobalt boride, nickel boride, potassium triethyl borohydride, sodium fluoroborate, fluoroboric acid, ammonium fluoroborate, potassium fluoroborate, lithium tetrafluoroborate, imidazole tetrafluoroborate, and nitric tetrafluoroborate; Preferably, in the synergistic auxiliary agent, the weight portion of the boron-containing auxiliary agent is less than or equal to 2 parts, and further 0.5 to 2 parts; Preferably, the weight ratio of the first stage material to the synergistic auxiliary agent is 100:0.1-10.
5. The continuous gas phase preparation method of 4N or higher high purity graphite according to claim 1, characterized in that: Atmosphere B is air or oxygen diluted by a diluent gas; wherein the diluent gas includes at least one of nitrogen and an inert gas; Preferably, the oxygen content of atmosphere B is 2-5%; Preferably, the second treatment period is 5 to 10 hours.
6. The continuous gas phase preparation method of 4N or higher high purity graphite according to claim 1, characterized in that: The positive pressure in the third treatment stage is above 1.5 atm, preferably 1.5 atm to 5 atm; Preferably, the third treatment period is 8 to 12 hours.
7. The continuous gas phase preparation method of 4N or higher high purity graphite according to any one of claims 1 to 6, characterized in that: After the third stage of treatment is completed, the step of switching the atmosphere in the atmosphere furnace to atmosphere D and then performing the fourth stage of treatment at temperature T4 to obtain ultra-high purity graphite above 6N; The atmosphere D is an atmosphere containing F-containing hydrocarbon gas; The temperature T4 is 2600-3000°C; Preferably, in the atmosphere D, the F-containing hydrocarbon gas is a C1-C3 alkane containing at least F and at least one H not replaced by a halogen; the halogen includes F and / or Cl; Preferably, the fourth treatment period is 12 to 24 hours.
8. High-purity graphite with a purity of 4N or above obtained by the preparation method according to any one of claims 1 to 7.
9. An application of high purity graphite of 4N or above obtained by the preparation method according to any one of claims 1 to 7, characterized in that: It is used to prepare at least one of high-purity silicon carbon, nuclear graphite, high-purity silicon carbide and fluorinated graphite.
10. A product comprising high-purity graphite with a purity of 4N or above obtained by the preparation method according to any one of claims 1 to 7 or made from the high-purity graphite.
Citation Information
Patent Citations
Method for recycling graphite material from waste lithium ion battery, graphite material and supercapacitor
CN113675492A
Method for selectively separating and regenerating graphite from waste battery black powder
CN117096485A
High-rate regenerated graphite negative electrode material as well as preparation method and application thereof
CN118198570A
Purification and graphitization method of graphite material
CN102126721A
Preparation method of high-purity graphite
CN105271216A