Manufacturing method of ingot-shaped target material and plasma corrosion resistant layer and plasma corrosion resistant surface structure
By preparing the ingot-shaped target and forming a plasma corrosion-resistant layer in the electronic gun evaporation machine, the problem of holes and particles contamination in the vacuum cavity of semiconductor equipment in the plasma spraying process is solved, the deposition efficiency and layer thickness control are improved, and the Etching resistance and protection effect.
Patent Information
- Application Number
- CN202311319093.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2023-05-23
- Filing Date
- 2023-10-12
- Publication Date
- 2024-11-26
AI Technical Summary
The vacuum cavity of existing semiconductor equipment is prone to pores and particle contamination during plasma spraying, and the deposition rate of electron gun evaporation is insufficient, making it difficult to form a plasma corrosion-resistant layer that meets the needs.
By using the method of preparing ingot-shaped targets, the ingot-shaped targets are formed by selecting plasma corrosion-resistant materials of various particle sizes, adding organic solvents, and ball milling method to mix, dry, screen, and pressurize the ingot-shaped targets, and the electron gun evaporation machine is used. The target material is used to form a plasma corrosion-resistant layer.
The deposition efficiency and stability of the plasma corrosion-resistant layer are improved, the layer thickness can be controlled more easily, and a higher quality plasma corrosion-resistant layer is provided, which enhances the etch resistance and protection effect of the vacuum cavity.
Smart Images

Figure CN119020733A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a surface structure and a manufacturing method thereof, in particular to a surface structure resistant to plasma erosion and a manufacturing method thereof. Background Art
[0002] In the semiconductor industry, plasma technology is widely used in semiconductor process equipment. As manufacturing process capabilities improve, the requirements for suppressing particle contamination become more stringent due to the reduction in line width. Therefore, semiconductor equipment manufacturers are committed to studying methods to suppress particle generation in the vacuum chamber of the process. At present, the vacuum chambers of most semiconductor equipment are made of aluminum materials, and the surface is treated by plasma spraying. However, the spraying process produces a large number of holes, allowing plasma to penetrate into the cavity substrate along the gap. This penetration can cause substrate peeling and subsequent particle contamination. In addition, due to the high porosity caused by spraying and the limitations of material selection, it is difficult to incorporate other elements into the material, so it is very difficult to improve the etching tolerance of the vacuum chamber by plasma spraying.
[0003] In addition, although electron gun evaporation can be used to form a denser plasma corrosion resistant layer, the electron gun evaporation process usually uses a granular target material to deposit the thin film. As a result, when the target material is heated and vaporized by the electron gun, the heat energy of the electron gun is easily lost, resulting in an insufficient deposition rate and an inability to efficiently deposit the film thickness required for the component film.
[0004] Therefore, how to solve the above problems is something that people with general knowledge in this field should consider. Summary of the invention
[0005] In order to solve the above problems, an object of the present invention is to provide a method for preparing an ingot-shaped target, a method for forming a plasma corrosion resistant layer using the ingot-shaped target, and a plasma corrosion resistant surface structure including the plasma corrosion resistant layer.
[0006] Based on the above purpose and other purposes, the present invention provides a method for preparing an ingot target material, which is suitable for placing the ingot target material into the target slot of an electron gun evaporator. The method for preparing an ingot target material includes the following steps: first, select a plurality of plasma corrosion resistant materials with a particle size of 20 microns to 100 microns, add an organic solvent, prepare a slurry, then use a ball mill to evenly mix, dry to remove the organic solvent, select a powder material of appropriate size through screening, add a sintering aid, and then pressurize to form an ingot blank, and finally sinter at high temperature to form an ingot target material. In one embodiment, the selected powder material can be Y 2 O 3 , YOF, YAG, and Al 2 O 3The materials are doped with 1-30% by weight of a lanthanide compound, wherein the lanthanide compound is selected from the group consisting of oxides, nitrides, and salt compounds of lanthanide.
[0007] In the above-mentioned method for preparing ingot target material, the organic solvent can be a polar solvent or a non-polar solvent, the drying temperature can be 80°C-120°C, the drying time can be 12-24 hours, the sieve aperture can be 300-2000 mesh, the pressure can be 1MPa-100MPa, the high temperature sintering temperature can be 800°C-2000°C, and the sintering time can be 1 hour-24 hours.
[0008] Based on the above and other purposes, the present invention provides a method for forming a plasma corrosion resistant layer, which includes placing an ingot target in a target slot of an electron gun evaporator, and bombarding the ingot target with an electron beam emitted by the electron gun evaporator to vaporize and deposit a plasma corrosion resistant layer on the surface of a substrate. In one embodiment, the deposition rate of the plasma corrosion resistant layer is 0.1-1.5nm / s, and the ingot target used is made by the method for preparing the ingot target mentioned above. In addition, the electron gun evaporator can be an ion-assisted electron gun evaporator. During the deposition of the plasma corrosion resistant layer, the ion-assisted electron gun evaporator satisfies at least one of the following working conditions: the electron beam current is 100-1500 mA, the working voltage is 100 V-1500 V, the argon gas flow rate in the target groove is 10-50 sccm, the oxygen gas flow rate in the target groove is 10-100 sccm, or the pressure in the target groove is 1.0x10-6-2.0x10-2 torr. In addition, the substrate is a vacuum chamber, and the surface of the substrate is the inner wall of the vacuum chamber. Moreover, during the deposition of the plasma corrosion resistant layer, the temperature of the vacuum chamber is 250C-3000C.
[0009] Based on the above and other purposes, the present invention provides a plasma-resistant surface structure, which is disposed on the surface of a substrate and includes a plasma-resistant layer formed by the above method for forming a plasma-resistant layer. In one embodiment, the plasma-resistant layer also includes a buffer layer, which is disposed between the substrate surface and the plasma-resistant layer and can be made of SiNx, Al 2 O 3 , Nb 2 O 5 、ZrO 2 , Al, Cr, Ti, Au, Ni and other materials.
[0010] In one embodiment, the plasma corrosion resistant layer further includes an optical layer disposed between the substrate surface and the plasma corrosion resistant layer. The optical layer and the plasma corrosion resistant layer have different refractive indices. The optical layer may be made of AlF 3MgF 2 、SiO 2 、SiH、Al 2 O 3 ,MgO,Nb 2 O 5 、ZrO 2 , WO 3 、TiO 2 , Al, Cr, Ti, Ag, Au, Ni and other materials. In one embodiment, the thickness of the plasma corrosion resistant layer is greater than 1 micron, the thickness of the buffer layer is between 0.01 micron and 1 micron, and the thickness of the optical layer is between 0.1 micron and 10 microns.
[0011] In the present invention, the thickness of the plasma corrosion resistant layer formed by the method of using ingot target materials is easier to control than that of the method of using powder or granular materials. In addition, because the density of the ingot target materials is higher and the energy of the electron beam bombarding the ingot target materials is less likely to dissipate, it has higher deposition efficiency and stability. In addition, the ingot target materials can easily evenly mix plasma corrosion resistant materials of different materials, thereby being able to provide a higher quality plasma corrosion resistant layer.
[0012] In order to achieve the above and other purposes, the present invention adopts technical means, components and their effects, and a preferred embodiment is described below with reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0013] Figure 1 A schematic diagram of an embodiment of a method for preparing an ingot-shaped target according to the present invention is provided.
[0014] Figure 2 The flowchart shown is an embodiment of a method for forming a plasma corrosion resistant layer according to the present invention.
[0015] Figure 3A FIG. 1 is a schematic diagram of one embodiment of a plasma resistant surface structure of the present invention.
[0016] Figure 3B FIG. 1 is a schematic diagram of another embodiment of the plasma resistant surface structure of the present invention.
[0017] Figure 3C FIG. 1 is a schematic diagram of another embodiment of the plasma resistant surface structure of the present invention. DETAILED DESCRIPTION
[0018] Please refer to Figure 1 , Figure 1A schematic diagram of an embodiment of the method for preparing an ingot target material of the present invention is provided. As shown in step S110, a plurality of plasma corrosion-resistant powder materials are selected, and the particle size of these powder materials is 20 microns to 100 microns. These powder materials are selected based on their required properties and compatibility with the intended application. In the present embodiment, these powder materials are usually doped with 1-30% by weight of a lanthanide compound, and the lanthanide compound is selected from the group consisting of oxides, nitrides, and salt compounds of lanthanide elements. Next, as shown in step S120, the selected powder material is combined with an appropriate organic solvent to form a slurry. The choice of organic solvent depends on the properties and compatibility of the powder material, and should be able to effectively wet the particles and promote uniform mixing. In the present embodiment, the material resistant to plasma corrosion may be silicon nitride (Si 3 N 4 ), silicon carbide (SiC), aluminum oxide (Al 2 O 3 ), tantalum nitride (TaN), and tantalum oxide (Ta 2 O 5 ). The organic solvent may be ethanol, isopropanol and acetone, but those skilled in the art should understand that the choice of organic solvent may vary depending on the actual situation.
[0019] Then, as shown in step S130, the slurry is subjected to ball milling. Ball milling is a mechanical processing method that uses rolling grinding balls to reduce particle size and achieve uniformity, wherein the composition of the grinding balls is carefully selected to minimize contamination. During the ball milling process, the slurry is placed in a milling chamber and grinding balls are added. The slurry in the milling chamber is then stirred at a controlled speed and a predetermined time. The parameters of the ball milling process, such as rotation speed and milling time, can be adjusted according to the situation to achieve the desired particle size and uniformity. In addition, the grinding balls can be made of different materials, such as stainless steel, aluminum oxide, zirconium oxide or tungsten carbide. The basis for selecting the grinding ball material includes factors such as the hardness of the powder material, the wear resistance of the grinding balls, and its compatibility with the powder material being processed.
[0020] After the grinding ball treatment, step S140 is implemented, and the slurry is dried at a controlled temperature and time to remove the solvent. During the drying process, the temperature and time are carefully controlled to ensure effective removal of the solvent without adversely affecting the powder material. The appropriate drying temperature and time depend on the specific solvent and powder material used. In this embodiment, the temperature and time are 60 to 120 degrees Celsius and 2 to 24 hours, respectively. Then, as shown in step S150, the dried powder material is screened using a screen of a specific size to obtain a uniform particle size distribution. The screen size is selected based on the desired particle size distribution and the requirements of the target material. In this embodiment, the screen aperture can be 300-2000 mesh, and the screen aperture size range is 40 microns to 200 microns, but the screen aperture and the screen aperture size may vary depending on the specific application and powder material.
[0021] Afterwards, as shown in step S160, before the sintering process, the powder material containing the sintering aid is pressurized under controlled pressure and temperature conditions to form a dense ingot-shaped blank. The pressurization conditions are crucial to achieving the desired shape, density and uniformity, which in turn affect the properties of the final target material. Appropriate pressurization conditions depend on the specific powder material, sintering aid and the desired shape of the target material. In this embodiment, the pressure is 1MPa-100MPa, and the temperature is, for example, in the range of room temperature to 200 degrees Celsius. The pressurization process can be performed using various techniques, such as uniaxial pressing, hot isostatic pressing or extrusion, depending on the specific application and material requirements.
[0022] Next, as shown in step S170, the screened powder material is sintered under high pressure and high temperature to promote densification and form a compact ingot target. During the sintering process, a sintering aid can be added to the powder mixture to promote densification and improve the sintering process. The selection of the sintering aid depends on the material used and the desired properties of the final target. The appropriate sintering temperature and time depend on the specific powder material used and the desired properties of the target. In this embodiment, the sintering temperature and sintering time are 1000 to 1800 degrees Celsius and 1 to 10 hours, respectively.
[0023] In addition, in this embodiment, the sintering aid includes metal oxides, borides, carbides and nitrides, and certain organic compounds such as waxes, polymers and surfactants. The sintering aid is usually added in a ratio of 0.1 to 10% by weight of the powder material, and the specific ratio depends on the specific application and material requirements.
[0024] As mentioned above, lanthanide compounds can be added to the powder material for preparing the ingot target material in order to enhance the plasma corrosion resistance of the final target material. Lanthanide compounds may include, but are not limited to, lanthanide elements such as lanthanum (La), cerium (Ce), praseodymium (Pr), neodymium (Nd), promethium (Pm), samarium (Sm), europium (Europium), gadolinium (Gd), dysprosium (Tb), dysprosium (Dy), holmium (Ho), erbium (Er), thulium (Tm), yttrium (Yb) and lutetium (Lu). These compounds are usually added to the powder material in a ratio of 1% to 30% by weight. In addition, lanthanide compounds can be selected from the group consisting of oxides, nitrides and salt compounds containing lanthanide elements. These compounds can be used alone or in combination, depending on the specific requirements of the target material and its intended application. Among them, lanthanum oxide (Lanthanum Oxide, La 2 O 3 ), Cerium Oxide (Cerium Oxide, CeO 2 ) and neodymium oxide (Neodymium Oxide, Nd 2 O 3 ) can be oxide compounds, while lanthanum nitride (Lanthanum Nitride, LaN), cerium nitride (CeN) and neodymium nitride (Neodymium Nitride, NdN) can be nitride compounds, and lanthanum fluoride (Lanthanum Fluoride, LaF 3 ), Cerium Chloride (Cerium Chloride, CeCl 3 ) and Neodymium Bromide (NdBr 3 ) etc. may be salt compounds.
[0025] In the above step S120, the selected powder material is combined with an appropriate organic solvent to form a slurry. The organic solvent can be a polar solvent or a non-polar solvent, depending on the compatibility of the organic solvent with the powder material. Polar solvents include, for example, water, ethanol, isopropanol and acetone, while non-polar solvents include, for example, toluene, hexane and heptane. The basis for selecting the solvent includes its ability to wet the powder particles, its evaporation rate and its compatibility with the powder material.
[0026] Next, please refer to Figure 2 , Figure 2 The flowchart of the method for forming a plasma corrosion resistant layer according to an embodiment of the present invention is shown. First, please refer to step S210, an ingot target is placed in a target slot of an electron gun evaporator. Then, step S220 is performed to bombard the ingot target with an electron beam generated by the electron gun evaporator to evaporate the ingot target. Then, as step S230, a plasma corrosion resistant layer 110 (such as Figure 3A As shown in FIG. 1 , the plasma corrosion resistant layer 110 protects the substrate from being affected by plasma corrosion during the plasma treatment. Figure 1 The ingot target is manufactured by the method for preparing the ingot target, and the electron gun evaporator is an ion-assisted electron gun evaporator (Ion-Beam Assisted E-Gun Evaporator).
[0027] Compared with the use of granular materials, the use of ingot targets can increase the deposition rate and make the formed plasma corrosion resistant layer have a thicker deposition thickness in the same time, which may be attributed to the following factors. First, the material density is different: the ingot target is denser and more compact than the powder or granular material, which makes the evaporation process more uniform when the material is bombarded by the electron beam, so it can more effectively increase the deposition rate and save the time required to reach the thickness of the deposition layer. Secondly,. In addition, the ingot target can provide a more stable and uniform surface, allowing the electron beam to interact with it more consistently, ensuring a more stable and uniform evaporation process. Therefore, the final thickness and quality of the plasma corrosion resistant layer can be better controlled. In addition, because the ingot target is doped with lanthanide elements, the characteristics of the plasma corrosion resistant layer can be changed.
[0028] In addition, in the process of forming the plasma corrosion resistant layer 110 of the present embodiment, the electron beam current of the electron gun evaporator is between 100mA and 1500mA when the electron gun evaporator is in operation, and the working voltage of the electron gun evaporator is in the range of 100V-1500V. In the target groove of the electron gun evaporator, the argon flow rate is maintained between 10sccm and 50sccm, and the oxygen flow rate is maintained between 10sccm and 100sccm, and the pressure is maintained between 1.0x10-6 and 2.0x10-2 torr. In addition, in the process of forming the plasma corrosion resistant layer 110, the deposition rate is in the range of 0.1 to 1.5nm / s. In the present embodiment, the plasma corrosion resistant layer 110 is formed by depositing it on the inner wall of the vacuum chamber. In the process of depositing the plasma corrosion resistant layer 110, the temperature of the vacuum chamber is maintained in the range of 25°C to 300°C. Compared with the prior art, this method can deposit a thicker plasma corrosion resistant layer 110 on the inner wall of the vacuum chamber to reduce stress without causing film peeling, thereby improving the etching tolerance of the vacuum chamber.
[0029] Next, please refer to Figure 3A , Figure 3A The figure shows a schematic diagram of one embodiment of the plasma resistant surface structure of the present invention. The plasma resistant surface structure 100 is disposed on the surface of the substrate 10 to provide a protective effect to the substrate 10. The plasma resistant surface structure 100 includes at least a plasma corrosion resistant layer 110. The plasma corrosion resistant layer 110 is composed of Figure 2 The manufacturing process shown in FIG. 1 is shown in FIG. 2 . In this embodiment, the thickness of the plasma corrosion resistant layer is greater than 1 micron. The thickness of the plasma corrosion resistant layer 110 is an important factor affecting its corrosion resistance, optical properties and durability. The ideal thickness depends on the specific application requirements and can be controlled during the deposition process. A thicker plasma corrosion resistant layer 110 may provide better protection, but may also result in reduced transmittance or increased stress within the layer. In the above embodiment, the thickness of the plasma corrosion resistant layer 110 is greater than 1 micron, but is not limited to this.
[0030] In addition, please refer to Figure 3B In another embodiment, the plasma resistant surface structure 100 further includes a buffer layer 120 to further enhance the adhesion of the plasma corrosion resistant layer to the inner wall of the vacuum chamber. The buffer layer 120 is placed between the surface of the substrate 10 and the plasma corrosion resistant layer 110. The buffer layer 120 acts as an intermediate layer to help improve adhesion, reduce stress and optimize overall performance. The buffer layer 120 can be composed of a variety of materials, including silicon nitride (SiNx), aluminum oxide (Al 2 O 3 ), niobium pentoxide (Nb 2 O 5 )、ZrO 2 ), aluminum (Al), chromium (Cr), titanium (Ti), gold (Au) and nickel (Ni). These materials offer a wide range of properties, and the buffer layer 120 can be customized according to specific applications and requirements. The thickness of the buffer layer 120 is also a key parameter that affects the overall performance of the plasma-resistant surface structure 100. The buffer layer 120 acts as a medium between the substrate 10 and the plasma corrosion-resistant layer 110, which helps to reduce stress, enhance adhesion and optimize the optical properties of the structure. The optimal thickness of the buffer layer depends on the material used, the intended application and the compatibility with the plasma corrosion-resistant layer 110. By carefully controlling the thickness of the buffer layer, the mechanical, thermal and optical properties of the plasma corrosion-resistant layer 110 can be optimized to ensure optimal performance in a wide range of applications. In the above embodiment, the thickness of the buffer layer is between 0.01 microns and 1 micron, but is not limited to this.
[0031] In addition, please refer to Figure 3CIn other embodiments, the plasma-resistant surface structure 100 further includes an optical layer 130, which is intended to further enhance the optical properties of the plasma-resistant surface structure 100 and is disposed between the surface of the substrate 10 and the plasma-resistant layer 110. Since the optical layer 130 is located between the surface of the substrate 10 and the plasma-resistant layer 110, the optical layer 130 can be prevented from being corroded by plasma. The optical layer 130 can be composed of different materials with specific optical properties, such as refractive index, absorption or reflection properties, etc., to match the plasma-resistant layer 110 and help optimize the overall performance of the plasma-resistant surface structure 100. The material selection of the optical layer 130 depends on the required optical properties and the specific requirements of the application. For example, aluminum fluoride (AlF 3 ), magnesium fluoride (MgF 2 ), silicon dioxide (SiO 2 ), silane (SiH), aluminum oxide (Al 2 O 3 ), magnesium oxide (MgO), hafnium pentoxide (Nb 2 O 5 )、ZrO 2 ), tungsten trioxide (WO 3 ), titanium dioxide (TiO 2 ), aluminum (Al), chromium (Cr), titanium (Ti), silver (Ag), gold (Au) and nickel (Ni). By carefully selecting and combining the materials used in the optical layer 130, the plasma-resistant surface structure 100 can be fine-tuned to achieve the desired transmittance, reflectivity and other optical properties to meet a wide range of application requirements. In the present embodiment, the thickness of the optical layer varies between 0.1 microns and 10 microns, but is not limited to this. In addition, in the vacuum cavity of the semiconductor equipment, the above-mentioned plasma-resistant surface structure 100 is applied to the viewing window to ensure good optical performance and stability in a high plasma environment. The viewing window is the interface between the inside and outside of the vacuum cavity, allowing technicians to observe and monitor the process inside the vacuum cavity. Therefore, a viewing window with good plasma resistance is essential to ensure the normal operation of the equipment.
[0032] The invention is described above, but it is not intended to limit the scope of the patent rights claimed by the invention. Any changes or modifications made by those skilled in the art without departing from the spirit or scope of this patent shall be considered as equivalent changes or designs completed under the spirit disclosed by the invention and shall be included in the claims of the invention.
Claims
1. A method for preparing an ingot-shaped target material, wherein the ingot-shaped target material is suitable for being placed in a target slot of an electron gun evaporation machine, characterized in that: The method for preparing an ingot-shaped target material comprises: (a) selecting one or more powder materials resistant to plasma corrosion, wherein the particle size of the powder material is 20 microns to 100 microns; (b) adding an organic solvent to prepare a slurry from the powder material; (c) uniformly mixing the slurry by a ball mill; (d) drying to remove the organic solvent; (e) Screening to obtain powder materials of appropriate size; (f) adding a sintering aid to the powder material; (g) pressing to form an ingot-shaped blank; (h) High temperature sintering to form an ingot-shaped target.
2. The method for preparing an ingot target material according to claim 1, characterized in that: The powder material is selected from the group consisting of Y2O3, YOF, YAG, and Al2O3.
3. The method for preparing an ingot target according to claim 1 or claim 2, characterized in that: The powder material is doped with 1-30% by weight of a lanthanide compound, which is selected from the group consisting of oxides, nitrides and salt compounds of the lanthanide.
4. The method for preparing an ingot target material according to claim 1, characterized in that: In step (b), the organic solvent may be a polar solvent or a non-polar solvent.
5. The method for preparing an ingot target material according to claim 1, characterized in that: In step (c), the grinding balls used in the ball milling method are made of aluminum oxide or zirconium oxide.
6. The method for preparing an ingot target material according to claim 1, characterized in that: In step (d), the drying temperature is 80° C.-120° C., and the drying time is 12-24 hours.
7. The method for preparing an ingot target material according to claim 1, characterized in that: The mesh size of the screen selected in step (e) is 300-2000 mesh.
8. The method for preparing an ingot target material according to claim 1, characterized in that: In step (f), the sintering aid is a solid phase sintering aid or a polymer sintering aid.
9. The method for preparing an ingot target material according to claim 1, characterized in that: In step (g), the pressure is 1 MPa-100 MPa.
10. The method for preparing an ingot target material according to claim 1, wherein: In step (h), the high temperature sintering temperature is 800° C.-2000° C., and the sintering time is 1 hour-24 hours.
11. A method for forming a plasma corrosion resistant layer, characterized in that: include: Placing an ingot-shaped target material in a target slot of an electron gun evaporation machine; and The ingot target is bombarded with an electron beam emitted by the electron gun evaporator to vaporize the ingot target and deposit a plasma corrosion resistant layer on the surface of a substrate.
12. The method for forming a plasma corrosion resistant layer according to claim 11, wherein: The ingot target is manufactured by the method for manufacturing an ingot target according to any one of claims 1 to 10.
13. The method for forming a plasma corrosion resistant layer according to claim 11, wherein: The electron gun evaporation machine is an ion-assisted electron gun evaporation machine.
14. The method for forming a plasma corrosion resistant layer according to claim 11, wherein: The deposition rate of the plasma corrosion resistant layer is 0.1-1.5 nm / s.
15. The method for forming a plasma corrosion resistant layer according to claim 11, wherein: During the deposition of the plasma corrosion resistant layer, the electron gun evaporator satisfies at least one of the following working conditions: The electron beam current is 100-1500mA; Working voltage 100V-1500V; The argon gas flow rate in the target groove is 10-50 sccm; The oxygen gas flow rate in the target groove is 10-100 sccm; and The pressure in the target tank is 1.0x10-6-2.0x10-2 torr.
16. The method for forming a plasma corrosion resistant layer according to claim 11, wherein: The substrate is a vacuum chamber, and the surface of the substrate is the inner wall of the vacuum chamber.
17. The method for forming a plasma corrosion resistant layer according to claim 16, wherein: During the deposition of the plasma corrosion resistant layer, the temperature of the vacuum chamber is 250°C-3000°C.
18. A plasma resistant surface structure, disposed on a surface of a substrate, characterized in that: The plasma resistant surface structure includes: A plasma corrosion resistant layer is formed by the method for forming a plasma corrosion resistant layer according to any one of claims 11 to 17.
19. The plasma resistant surface structure according to claim 18, wherein: The invention also comprises a buffer layer, which is arranged between the surface of the substrate and the plasma corrosion resistant layer.
20. The plasma resistant surface structure according to claim 19, wherein: The buffer layer is selected from the group consisting of SiNx, Al2O3, Nb2O5, ZrO2, Al, Cr, Ti, Au, and Ni.
21. The plasma resistant surface structure according to claim 18, wherein: The plasma corrosion resistant layer is light-transmissive.
22. The plasma resistant surface structure according to claim 18, wherein: The optical layer is also included. The optical layer is disposed between the surface of the substrate and the plasma corrosion resistant layer. The optical layer and the plasma corrosion resistant layer have different refractive indices.
23. The plasma resistant surface structure according to claim 22, characterized in that: The optical layer is selected from the group consisting of AlF3, MgF2, SiO2, SiH, Al2O3, MgO, Nb2O5, ZrO2, WO3, TiO2, Al, Cr, Ti, Ag, Au, and Ni.
24. The plasma resistant surface structure according to claim 18, wherein: The thickness of the plasma corrosion resistant layer is greater than 1 micron.
25. The plasma resistant surface structure according to claim 19 or claim 24, characterized in that: The thickness of the buffer layer is between 0.01 micrometer and 1 micrometer.
26. The plasma resistant surface structure according to claim 22 or claim 24, characterized in that: The thickness of the optical layer is between 0.1 micrometers and 10 micrometers.