Edge sealing method for preventing PVB (polyvinyl butyral) adhesive layer from eroding PDLC (polymer dispersed liquid crystal) film

By cutting the conductive film on the edge of the surface of the PDLC film and forming grooves and applying barrier glue to cover the conductive film of the corresponding shape, the problem of PDLC film being eroded by the PVB glue layer is solved, extending the service life of the film and improving the film Exterior effect.

CN119024591APending Publication Date: 2024-11-26SHANGHAI MEMBRANE NEW MATERIAL TECH CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411007873.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-07-25
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The existing PDLC film has not been sealed, which makes the PDLC film in dimmed glass using PVB glue easily eroded, affecting its appearance and service life.

Method used

Cut the conductive film on the surface edge and electrode of the PDLC film to form a groove, and apply barrier glue to the groove and electrode, and then cover and bond the conductive films of corresponding shapes and sizes to form a cover to prevent PVB Erosion of the glue layer.

Benefits of technology

Effectively prevent PDLC film from being eroded, extending its service life and improving its appearance effect.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119024591A_ABST
    Figure CN119024591A_ABST
Patent Text Reader

Abstract

The invention discloses an edge sealing method for preventing a PVB (Polyvinyl Butyral) adhesive layer from eroding a PDLC (Polymer Dispersed Liquid Crystal) film, which is characterized by comprising the following steps: S1, cutting off the surface edge of the PDLC film and a conductive film at an electrode, and forming a groove in the surface edge of the PDLC film; s2, coating barrier glue in the grooves and on the electrodes; and S3, covering the grooves and the electrodes with a conductive film, and bonding the conductive film with the barrier glue. When the edge sealing method of the PDLC film is implemented, a laser cutting machine is used for cutting off the conducting film at the surface edge and the electrode of the PDLC film, grooves are formed at the surface edge and the electrode of the PDLC film, then barrier glue is coated in the grooves and on the electrode, and finally the conducting film corresponding to the grooves in shape and size covers the grooves and the electrode again. And the conductive film and the barrier glue are bonded to form a sealing cover, so that the edge of the PDLC film can be sealed, the PDLC film is prevented from being eroded, and the service life of the PDLC film is prolonged.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of PDLC, and more particularly to an edge sealing method for preventing PVB glue from corroding a PDLC film. Background Art

[0002] In recent decades, the emerging optoelectronic material known as polymer dispersed liquid crystal (PDLC) has always been a hot topic for scientific researchers. Polymer dispersed liquid crystal has the advantages of simple preparation process, short response time, fast speed, and no need for polarization devices. It has been gradually applied to electronic components such as light valves, gratings, light-transmitting projection screens, and dimming glass. Dimming glass is also called electronic curtains. Its working principle is: when the power of the dimming glass is turned off, the liquid crystal molecules in the dimming glass are in an irregular dispersion state, at this time the light is scattered, and the dimming glass is in an atomized state; when the power of the dimming glass is turned on, the liquid crystal molecules in the dimming glass are in a neatly arranged state, at this time the light can penetrate freely, and the dimming glass is in a transparent state. Because dimming glass has this dimming characteristic, it has been widely used in high-end places such as office buildings, medical institutions, and commercial displays.

[0003] However, the existing PDLC film is not edge-sealed, which causes the PDLC film in the dimming glass using PVB laminate to be easily corroded, affecting its appearance and service life. Summary of the invention

[0004] In view of the above-mentioned defects of the prior art, the present invention provides an edge sealing method for preventing a PVB adhesive layer from corroding a PDLC film.

[0005] The technical solution adopted by the present invention to solve the technical problem is: to disclose an edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film, characterized in that the edge sealing method comprises the following steps:

[0006] S1, cutting off the conductive film at the surface edge of the PDLC film and the electrode, and forming a groove at the surface edge of the PDLC film;

[0007] S2, applying barrier glue in the groove and on the electrode;

[0008] S3. Cover the groove and the electrode with a conductive film and bond them with a barrier adhesive.

[0009] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention, the groove is an annular groove surrounding the edge of the surface of the PDLC film.

[0010] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention, the step S1 further includes: erasing the liquid crystal in the groove and on the conductive film.

[0011] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film described in the present invention, step S3 specifically includes: re-covering the cut conductive film on the groove and the electrode and bonding it with the barrier adhesive, or covering the groove and the electrode with a conductive film of the same shape and size as the groove and bonding it with the barrier adhesive.

[0012] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention, the step S3 further includes:

[0013] S4. Wipe off excess barrier glue.

[0014] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention, the step S3 further includes:

[0015] S5. Place the portion of the PDLC film coated with the barrier adhesive into a curing device for curing.

[0016] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention, the distance between the groove and the edge of the PDLC film is 1-10 mm.

[0017] In the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention, the width of the groove is 0.5-10 mm.

[0018] The implementation of the edge sealing method for preventing the PVB adhesive layer from corroding the PDLC film of the present invention has the following beneficial effects: when implementing the edge sealing method for the PDLC film of the present invention, a laser cutter is used to cut the conductive film at the edge of the PDLC film surface and the electrode, a groove is formed at the edge of the PDLC film surface and the electrode, and then a barrier adhesive is applied to the groove and the electrode, and finally a conductive film corresponding to the shape and size of the groove is re-covered on the groove and the electrode, and the conductive film and the barrier adhesive are bonded to form a cover, thereby forming an edge seal for the edge of the PDLC film, preventing the PDLC film from being corroded, and extending the service life of the PDLC film. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention will be further described below with reference to the accompanying drawings and embodiments, in which:

[0020] Figure 1 It is a structural schematic diagram of the edge sealing method of the present invention for preventing the PVB adhesive layer from corroding the PDLC film;

[0021] Figure 2 The diagram is a flow chart of an edge sealing method for preventing a PVB adhesive layer from corroding a PDLC film according to the present invention. DETAILED DESCRIPTION

[0022] In order to make the objectives, technical solutions and advantages of the present invention more clear, the embodiments of the present invention will be further described in detail below with reference to the accompanying drawings.

[0023] like Figure 1 , 2 As shown, in the first embodiment of the edge sealing method for preventing the PVB glue layer from corroding the PDLC film of the present invention, the edge sealing method includes the following steps:

[0024] S1, cutting off the conductive film at the surface edge of the PDLC film 10 and the electrode 12, and forming a groove 11 at the surface edge of the PDLC film 10;

[0025] S2, applying barrier glue inside the groove 11 and on the electrode 12;

[0026] S3, covering the groove 11 and the electrode 12 with a conductive film and bonding them with a barrier adhesive.

[0027] Specifically, when cutting the conductive film, a laser cutter can be used to select one side of the PDLC film 10 and cut the conductive film with a groove width of 0.5-10 mm at a distance of 1-10 mm from the edge of the PDLC film 10 to form a groove 11, which will be described in detail later.

[0028] When implementing the edge sealing method of the PDLC film of the present invention, a laser cutter is used to cut the conductive film at the edge of the surface of the PDLC film 10 and the electrode 12, and a groove 11 is formed at the edge of the surface of the PDLC film 10 and the electrode 12. Then, a barrier glue is applied to the groove 11 and the electrode 12. Finally, a conductive film corresponding to the shape and size of the groove 11 is re-covered on the groove 11 and the electrode 12. The conductive film and the barrier glue are bonded to form a cover, thereby forming an edge seal for the edge of the PDLC film 10, preventing the PDLC film 10 from being corroded and extending the service life of the PDLC film 10.

[0029] It can be understood that there are two electrodes 12 in the present application, one of which is located on the same surface as the groove, and the other is located on the other surface.

[0030] Specifically, the groove 11 is an annular groove 11 surrounding the edge of the surface of the PDLC film 10 .

[0031] In a preferred embodiment, the PDLC film 10 is a rectangular PDLC film 10, and the annular groove 11 is a rectangular groove 11 corresponding to the shape of the PDLC film 10. In other embodiments, the size and shape of the annular groove 11 correspond to the size and shape of the PDLC film 10.

[0032] After the conductive film is cut off, step S1 further includes: erasing the liquid crystal in the groove 11 and on the conductive film.

[0033] In one embodiment, the step S3 specifically includes: re-covering the cut conductive film on the groove 11 and the electrode 12 and bonding them with a barrier adhesive.

[0034] In another embodiment, the step S3 specifically includes: covering the groove 11 and the electrode 12 with a conductive film having the same shape and size as the groove 11 and bonding the conductive film with a barrier adhesive.

[0035] After the conductive film is covered on the groove 11, the step S3 further includes:

[0036] S4. Wipe off excess barrier glue.

[0037] Furthermore, after step S3, the following steps are further included:

[0038] S5, placing the portion of the PDLC film 10 coated with the barrier adhesive into a curing device for curing.

[0039] Preferably, the distance between the groove 11 and the edge of the PDLC film 10 is 1-10 mm.

[0040] Preferably, the width of the groove 11 is 0.5-10 mm.

[0041] In addition, in the present invention, unless otherwise clearly specified and limited, the terms "connected", "connected", "stacked" and the like should be understood in a broad sense, for example, it can be fixedly connected, detachably connected, or integrated; it can be directly connected, or indirectly connected through an intermediate medium, it can be the internal connection of two elements or the interaction relationship between two elements. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0042] The above descriptions are merely embodiments of the present invention and are not intended to limit the patent scope of the present invention. Any equivalent structure or equivalent process transformation made using the contents of the present invention specification and drawings, or directly or indirectly applied in other related technical fields, are also included in the patent protection scope of the present invention.

Claims

1. A method for sealing an edge of a PDLC film to prevent PVB glue from corroding the PDLC film, characterized in that: The edge sealing method comprises the following steps: S1, cutting off the conductive film at the surface edge of the PDLC film and the electrode, and forming a groove at the surface edge of the PDLC film; S2, applying barrier glue in the groove and on the electrode; S3. Cover the groove and the electrode with a conductive film and bond them with a barrier adhesive.

2. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: The groove is an annular groove surrounding the edge of the surface of the PDLC film.

3. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: The step S1 also includes: erasing the liquid crystal in the groove and on the conductive film.

4. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: The step S3 specifically includes: covering the cut conductive film on the groove and the electrode again and bonding them with the barrier adhesive, or covering the groove and the electrode with a conductive film of the same shape and size as the groove and bonding them with the barrier adhesive.

5. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: After step S3, the following steps are also included: S4. Wipe off excess barrier glue.

6. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: After step S3, the following steps are also included: S5. Place the portion of the PDLC film coated with the barrier adhesive into a curing device for curing.

7. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: The distance between the groove and the edge of the PDLC film is 1-10 mm.

8. The edge sealing method for preventing PVB glue from corroding a PDLC film according to claim 1, characterized in that: The width of the groove is 0.5-10 mm.