Semiconductor device, preparation method, packaging method and semiconductor packaging structure

By forming conductive bumps in advance in the chip manufacturing process and using a barrier layer to protect them, the problems of insufficient preparation accuracy and device reliability in traditional processes are solved, and the stability and reliability of chip manufacturing are improved.

CN119028837APending Publication Date: 2024-11-26GUANGZHOU CANSEMI TECH INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411158273.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-22
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

Traditional chip manufacturing processes are difficult to meet the requirements of heterosquared conductive film packaging processes, resulting in insufficient preparation accuracy and device reliability. The conductive bump process affects the formed passivation layer, affecting the stability of the device and reliability.

Method used

Conductive bumps are formed in advance before forming the passivation layer, and the first and second barrier layers are used as etching stop layers and mask layers, respectively, to ensure the conductive connection and preparation accuracy of the top metal layer and the conductive bumps, avoiding the need for The conductive bump preparation is limited by the opening of the passivation layer.

Benefits of technology

It improves the preparation accuracy of conductive bumps and the performance and reliability of the device, ensures the protection effect of the passivation layer, enhances the stability and reliability of the device, and simplifies process difficulty.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028837A_ABST
    Figure CN119028837A_ABST
Patent Text Reader

Abstract

The embodiment of the invention relates to a semiconductor device, a preparation method, a packaging method and a semiconductor packaging structure, and the method comprises the steps: providing a substrate, and forming a top metal layer on the substrate; forming a conductive bump material layer, covering the top metal layer with the conductive bump material layer, and conductively connecting the conductive bump material layer with the top metal layer; etching the conductive bump material layer to form a conductive bump; forming a passivation layer including a first portion covering the top metal layer, a second portion covering a side surface of the conductive bump, and a third portion covering a top surface of the conductive bump; the third portion and at least a portion of the second portion are removed to expose the conductive bump out of the passivation layer. Therefore, the stability and reliability of the device are enhanced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor technology, and in particular to a method for preparing a semiconductor device, a method for packaging a semiconductor device, a semiconductor device, and a semiconductor packaging structure. Background Art

[0002] With the development of integrated circuits, traditional packaging technology can no longer meet the needs of large-scale integrated circuits, and ACF (Anisotropic Conductive Film) packaging technology has emerged. At present, ACF is widely used in the packaging between IC (Integrated Circuit) and LCD (Liquid Crystal Display), FPC (Flexible Printed Circuit) and LCD, IC and Film. This packaging process completely breaks the limitations of traditional packaging materials and processes and meets the packaging requirements of modern large-scale integrated circuit microelectronics.

[0003] In the traditional chip manufacturing process, after the passivation layer is formed on the surface of the chip, an etching process is performed to form an opening to expose part of the top metal layer. The chip can then be interconnected to the packaging substrate through packaging processes such as wire bonding. However, the structure formed in the traditional chip manufacturing process is difficult to meet the requirements of the ACF packaging process. In order to better apply the ACF packaging process, at present, the art forms a bump in the opening of the passivation layer and performs a flip chip packaging process, so that the conductive particles in the ACF are located between the bump and the packaging substrate, thereby achieving a conductive connection between the chip and the packaging substrate. However, there are still many problems to be overcome in the process of chip manufacturing, and the reliability of the product still needs to be improved. Summary of the invention

[0004] In view of this, embodiments of the present application provide a method for preparing a semiconductor device, a method for packaging a semiconductor device, a semiconductor device, and a semiconductor packaging structure to solve at least one problem existing in the background technology.

[0005] In a first aspect, an embodiment of the present application provides a method for preparing a semiconductor device, comprising:

[0006] providing a substrate having a top metal layer formed thereon;

[0007] forming a conductive bump material layer, wherein the conductive bump material layer covers the top metal layer, and the conductive bump material layer is conductively connected to the top metal layer;

[0008] Etching the conductive bump material layer to form a conductive bump;

[0009] forming a passivation layer, the passivation layer comprising a first portion covering the top metal layer, a second portion covering the side surface of the conductive bump, and a third portion covering the top surface of the conductive bump;

[0010] The third portion and at least a portion of the second portion are removed to expose the conductive bump outside the passivation layer.

[0011] In combination with the first aspect of the present application, in an optional implementation manner, before forming the conductive bump material layer, the preparation method further includes: forming a first barrier layer, the first barrier layer covering the top metal layer; the conductive bump material layer covering the first barrier layer; the first barrier layer is conductive, and the conductive bump material layer is conductively connected to the top metal layer through the first barrier layer;

[0012] When performing the step of etching the conductive bump material layer, the first barrier layer is used as an etching stop layer.

[0013] In combination with the first aspect of the present application, in an optional implementation, the material of the first barrier layer includes titanium nitride and / or titanium.

[0014] In combination with the first aspect of the present application, in an optional implementation manner, before etching the conductive bump material layer, the preparation method further includes: forming a second barrier layer, the second barrier layer covering the conductive bump material layer; performing a patterning process on the second barrier layer;

[0015] When performing the step of etching the conductive bump material layer, the patterned second barrier layer is used as a mask layer.

[0016] In combination with the first aspect of the present application, in an optional implementation, the material of the second barrier layer includes titanium nitride and / or titanium.

[0017] In a second aspect, an embodiment of the present application provides a semiconductor device, which is manufactured using the semiconductor device manufacturing method as described in any one of the first aspects.

[0018] In a third aspect, an embodiment of the present application provides a method for packaging a semiconductor device, comprising:

[0019] Providing a first substrate and a second substrate, wherein the first substrate and / or the second substrate is prepared by the method for preparing a semiconductor device according to any one of the first aspects;

[0020] Arranging an adhesive layer on the first substrate and / or the second substrate, wherein the adhesive layer comprises an insulating adhesive layer and a plurality of conductive particles, wherein the plurality of conductive particles are encapsulated in the insulating adhesive layer;

[0021] The first substrate and the second substrate are bonded correspondingly, and the first substrate and the second substrate are conductively connected via the conductive particles.

[0022] In conjunction with the third aspect of the present application, in an optional implementation, the adhesive layer includes an anisotropic conductive adhesive film.

[0023] In a fourth aspect, an embodiment of the present application provides a semiconductor device, including:

[0024] a substrate having a top metal layer formed thereon;

[0025] A conductive bump is located on the top metal layer, and the conductive bump is conductively connected to the top metal layer;

[0026] A passivation layer covering the top metal layer, wherein the conductive bump is exposed outside the passivation layer;

[0027] Among them, it also includes: a first barrier layer, covering the top metal layer and located between the top metal layer and the conductive bump, the first barrier layer is conductive, and the conductive bump is conductively connected to the top metal layer through the first barrier layer; and / or, a second barrier layer, covering the top surface of the conductive bump, the second barrier layer is conductive.

[0028] In a fifth aspect, an embodiment of the present application provides a semiconductor packaging structure, comprising the semiconductor device as described in the fourth aspect.

[0029] The semiconductor device manufacturing method, semiconductor device packaging method, semiconductor device and semiconductor packaging structure provided in the embodiments of the present application have the following beneficial effects:

[0030] On the one hand, by providing a substrate, a top metal layer is formed on the substrate; forming a conductive bump material layer, the conductive bump material layer covers the top metal layer, and the conductive bump material layer is conductively connected to the top metal layer; etching the conductive bump material layer to form a conductive bump; forming a passivation layer, the passivation layer includes a first portion covering the top metal layer, a second portion covering the side surface of the conductive bump, and a third portion covering the top surface of the conductive bump; removing the third portion and at least part of the second portion to expose the conductive bump outside the passivation layer. Thus, compared with first forming a passivation layer, forming an opening in the passivation layer, and then forming a conductive bump in the opening, the embodiment of the present application forms a conductive bump in advance before forming the passivation layer, which can avoid the preparation of the conductive bump being restricted by the passivation layer opening, which is conducive to improving the preparation accuracy of the conductive bump, and then improving the performance and reliability of the device; and it can avoid the process of forming the conductive bump from affecting the formed passivation layer, thereby ensuring the protection effect of the passivation layer and further enhancing the stability and reliability of the device.

[0031] On the other hand, the first barrier layer covers the top metal layer and is located between the top metal layer and the conductive bump. In the process of forming the conductive bump, the first barrier layer can be used as an etching stop layer to avoid affecting the top metal layer, which is beneficial to improving the stability and reliability of the device. In addition, the first barrier layer is conductive and can ensure the conductive connection between the top metal layer and the conductive bump. The second barrier layer covers the top surface of the conductive bump. In the process of forming the conductive bump, the second barrier layer can be used as a mask layer, which is beneficial to improving the preparation accuracy of the conductive bump. In addition, the second barrier layer is conductive and can ensure the conductive connection between the conductive bump and other devices.

[0032] Additional aspects and advantages of the present application will be given in part in the description below, and in part will become apparent from the description below, or will be learned through the practice of the present application. BRIEF DESCRIPTION OF THE DRAWINGS

[0033] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:

[0034] Figures 1 to 3 It is a schematic diagram of the cross-sectional structure of a semiconductor device during the preparation process in the related art;

[0035] Figure 4 A schematic diagram of a process for preparing a semiconductor device according to an embodiment of the present application;

[0036] Figures 5 to 13 A schematic diagram of the cross-sectional structure of a semiconductor device during the preparation process provided by an embodiment of the present application;

[0037] Fig.14 A schematic cross-sectional structure diagram of a semiconductor device provided in an embodiment of the present application;

[0038] Fig.15 A schematic diagram of a process flow of a semiconductor device packaging method provided in an embodiment of the present application;

[0039] Figure 16 to Figure 17 A schematic diagram of a cross-sectional structure of a semiconductor device during a packaging process provided in an optional specific implementation manner of the present application;

[0040] Figure 18 to Figure 19 A schematic diagram of the cross-sectional structure of a semiconductor device during a packaging process is provided as another optional specific implementation manner of the present application.

[0041] Description of reference numerals:

[0042] 100, substrate; 110, interlayer dielectric layer; 120, top metal layer; 130, first barrier layer; 140, conductive bump material layer; 141, conductive bump; 150, second barrier layer; 160, first photoresist layer; 170, passivation layer; 171, first part; 172, second part; 173, third part; 174, opening; 180, second photoresist layer; 181, etching window; 10, first substrate; 20, second substrate; 11, first conductive connection structure; 21, second conductive connection structure; 30, bonding layer; 31, insulating adhesive layer; 32, conductive particles. DETAILED DESCRIPTION

[0043] The exemplary embodiments disclosed in the present application will be described in more detail below with reference to the accompanying drawings. Although the exemplary embodiments of the present application are shown in the accompanying drawings, it should be understood that the present application can be implemented in various forms and should not be limited by the specific embodiments described herein. On the contrary, these embodiments are provided to enable a more thorough understanding of the present application and to fully convey the scope disclosed in the present application to those skilled in the art.

[0044] In the following description, a large number of specific details are given to provide a more thorough understanding of the present application. However, it is obvious to those skilled in the art that the present application can be implemented without one or more of these details. In other examples, in order to avoid confusion with the present application, some technical features known in the art are not described; that is, all features of the actual embodiments are not described here, and well-known functions and structures are not described in detail.

[0045] In the drawings, the sizes of layers, regions, elements and their relative sizes may be exaggerated for clarity. Like reference numerals denote like elements throughout.

[0046] It should be understood that when an element or layer is referred to as "on ...", "adjacent to ...", "connected to" or "coupled to" other elements or layers, it can be directly on, adjacent to, connected to or coupled to other elements or layers, or there can be intervening elements or layers. On the contrary, when an element is referred to as "directly on ...", "directly adjacent to ...", "directly connected to" or "directly coupled to" other elements or layers, there is no intervening element or layer. It should be understood that although the terms first, second, third, etc. can be used to describe various elements, components, regions, layers and / or parts, these elements, components, regions, layers and / or parts should not be limited by these terms. These terms are only used to distinguish one element, component, region, layer or part from another element, component, region, layer or part. Therefore, without departing from the teachings of the present application, the first element, component, region, layer or part discussed below can be represented as the second element, component, region, layer or part. And when the second element, component, region, layer or part is discussed, it does not indicate that the present application necessarily has the first element, component, region, layer or part.

[0047] Spatially relative terms such as "under", "beneath", "below", "under", "above", "above", etc., may be used here for convenience of description to describe the relationship between an element or feature shown in the figure and other elements or features. It should be understood that in addition to the orientation shown in the figure, the spatial relationship terms are intended to also include different orientations of the device in use and operation. For example, if the device in the accompanying drawings is turned over, then the elements or features described as "under other elements" or "under it" or "under it" will be oriented as "on" other elements or features. Therefore, the exemplary terms "under" and "under" may include both upper and lower orientations. The device can be oriented otherwise (rotated 90 degrees or other orientations) and the spatial descriptors used herein are interpreted accordingly.

[0048] The purpose of the terms used herein is only to describe specific embodiments and is not intended to be limiting of the present application. When used herein, the singular forms "one", "an" and "said / the" are also intended to include plural forms, unless the context clearly indicates otherwise. It should also be understood that the terms "consisting of" and / or "comprising", when used in this specification, determine the presence of the features, integers, steps, operations, elements and / or parts, but do not exclude the presence or addition of one or more other features, integers, steps, operations, elements, parts and / or groups. When used herein, the term "and / or" includes any and all combinations of the relevant listed items.

[0049] In order to thoroughly understand the present application, detailed steps and detailed structures will be presented in the following description to illustrate the technical solution of the present application. The preferred embodiments of the present application are described in detail below, but in addition to these detailed descriptions, the present application may also have other implementation methods.

[0050] Figures 1 to 3 Schematic diagram of the cross-sectional structure of the MEMS device in the preparation process in the related art. As shown in the figure, in the related art, the preparation process of the conductive bump 141 generally includes: forming a passivation layer 170 covering the top metal layer 120; etching the passivation layer 170 to form an opening 174, the opening 174 exposing at least a portion of the top metal layer 120; forming a conductive bump material layer 140, the conductive bump material layer 140 is filled in the opening 174; etching the conductive bump material layer 140 to form a conductive bump 141 at the opening 174. It can be understood that in this process, if the process of etching the passivation layer 170 produces errors, the formed opening 174 has errors in position, shape and depth, and thus the prepared conductive bump 141 is difficult to be in a preset position, cannot form a preset shape, and even cannot achieve conductive connection with the top metal layer 120. Furthermore, the process of etching the conductive bump material layer 140 may damage the formed passivation layer 170 , affecting the protection effect of the passivation layer 170 , and further affecting the reliability of the device.

[0051] Please refer to Figure 2 Since the opening 174 is formed in the passivation layer 170, the conductive bump material layer 140 will be formed on the passivation layer 170 in a conformal manner, presenting an uneven surface, and the portion of the conductive bump material layer 140 used to prepare the conductive bump 141 is located in the opening 174, which is a recessed portion of the conductive bump material layer 140. Before etching the conductive bump material layer 140, a mask layer (not shown in the figure) covering the conductive bump material layer 140 is usually formed, and a patterning process is performed on the mask layer. The patterned mask layer covers the portion of the conductive bump material layer 140 used to prepare the conductive bump 141, and when etching the conductive bump material layer 140, the patterned mask layer can be used as a mask. However, the uneven surface morphology of the conductive bump material layer 140 greatly increases the difficulty of patterning the mask layer.

[0052] In some related technologies, a planarization process is performed to make the surface of the conductive bump material layer 140 flat, and then a mask layer is prepared. However, the accuracy of the planarization process will affect the thickness of the conductive bump 141 prepared subsequently, thereby affecting the reliability of the device; and the process of preparing the conductive bump 141 is complicated, affecting the production efficiency.

[0053] In view of this, the present application embodiment provides a method for preparing a MEMS device, please refer to Figure 4 , the preparation method comprises:

[0054] Step S401: providing a substrate, on which a top metal layer is formed;

[0055] Step S402: forming a conductive bump material layer, wherein the conductive bump material layer covers the top metal layer, and the conductive bump material layer is conductively connected to the top metal layer;

[0056] Step S403: etching the conductive bump material layer to form a conductive bump;

[0057] Step S404: forming a passivation layer, the passivation layer comprising a first portion covering the top metal layer, a second portion covering the side surface of the conductive bump, and a third portion covering the top surface of the conductive bump;

[0058] Step S405: removing the third portion and at least a portion of the second portion to expose the conductive bump outside the passivation layer.

[0059] The embodiment of the present application forms a conductive bump in advance before forming a passivation layer, thereby avoiding the preparation of the conductive bump being restricted by the opening of the passivation layer, which is beneficial to reducing the process difficulty, improving the preparation accuracy of the conductive bump, and further improving the performance and reliability of the device; and it can avoid the process of forming the conductive bump from affecting the formed passivation layer, thereby ensuring the protective effect of the passivation layer and further enhancing the stability and reliability of the device.

[0060] Please refer to Figure 5 , perform step S401: provide a substrate 100, and a top metal layer 120 is formed on the substrate 100.

[0061] The substrate 100 may be any suitable semiconductor substrate, such as a bulk silicon substrate, and may also be at least one of the following materials: SiGe, SiC, SiGeC, TnAs, GaAs, InP or other III-group and V-group compound semiconductors, including multilayer structures formed by these semiconductors, or silicon on insulator (SOI), silicon germanium on insulator (SiGeOI) and germanium on insulator (GeOI), or may also be double-side polished silicon wafers (DSP), or may also be ceramic substrates such as aluminum oxide, quartz or glass substrates, etc. This embodiment does not limit this.

[0062] The material of the top metal layer 120 may be any suitable conductive metal material, including but not limited to copper, gold, tungsten, aluminum, etc. In this embodiment, the material of the top metal layer 120 is specifically aluminum, for example.

[0063] Please continue to refer to Figure 5, an interlayer dielectric layer 110 is also formed on the substrate 100, and the top metal layer 120 covers the interlayer dielectric layer 110. It can be understood that Figure 5 The positional relationship between the substrate 100 and the top metal layer 120 is only schematically shown. In the actual structure, a device structure layer (not shown in the figure) is also formed on the substrate 100. Therefore, the interlayer dielectric layer 110 is formed on the substrate 100 to insulate and protect the device structure layer. In addition, a conductive via (not shown in the figure) is formed in the interlayer dielectric layer 110, so that the device structure layer is conductively connected to the top metal layer 120 through the conductive via.

[0064] Please refer to Figure 6 , executing step S402: forming a conductive bump material layer 140 , the conductive bump material layer 140 covers the top metal layer 120 , and the conductive bump material layer 140 is conductively connected to the top metal layer 120 .

[0065] The material of the conductive bump material layer 140 can be any suitable conductive material, including but not limited to metals such as copper, gold, tungsten, and aluminum. In this embodiment, the material of the conductive bump material layer 140 is specifically aluminum, for example.

[0066] In this embodiment, the process of forming the conductive bump material layer 140 may include a deposition process.

[0067] Please continue to refer to Figure 6 and Fig.10 Before forming the conductive bump material layer 140, the preparation method further includes: forming a first barrier layer 130, the first barrier layer 130 covers the top metal layer 120; the conductive bump material layer 140 covers the first barrier layer 130; the first barrier layer 130 is conductive, and the conductive bump material layer 140 is conductively connected to the top metal layer 120 through the first barrier layer 130; when performing the step of etching the conductive bump material layer 140, the first barrier layer 130 is used as an etching stop layer. Therefore, the first barrier layer 130 is conductive, which can ensure the conductive connection between the top metal layer 120 and the conductive bump material layer 140. When etching the conductive bump material layer 140 later, the first barrier layer 130 can be used as an etching stop layer to avoid damage to the top metal layer 120 caused by the etching process, thereby reducing the process difficulty.

[0068] Optionally, the material of the first barrier layer 130 includes titanium nitride and / or titanium. It can be understood that titanium nitride and titanium have good electrical conductivity, which can ensure the conductive connection between the conductive bump material layer 140 and the top metal layer 120; titanium nitride and titanium both have good chemical stability, and when used as an etching stop layer, they can ensure the etching barrier effect and avoid excessive etching affecting the top metal layer 120; titanium nitride and titanium can prevent material diffusion between the conductive bump material layer 140 and the top metal layer 120, which is beneficial to improving the reliability of the device.

[0069] In this embodiment, the process of forming the first barrier layer 130 may include a deposition process.

[0070] Please continue to refer to Figures 6 to 9 Before etching the conductive bump material layer 140, the preparation method further includes: forming a second barrier layer 150, the second barrier layer 150 covers the conductive bump material layer 140; performing a patterning process on the second barrier layer 150; when performing the step of etching the conductive bump material layer 140, the patterned second barrier layer 150 is used as a mask layer. It can be understood that by performing a patterning process on the second barrier layer 150, the position and shape of the conductive bump to be formed can be more accurately defined; in some related technologies, the patterned photoresist is usually directly used as the mask layer, but during the etching process, the photoresist is prone to deformation or damage, which in turn affects the etching effect, while the patterned second barrier layer 150 is used as the mask layer, which can avoid deformation or damage of the mask layer, which is conducive to ensuring the preparation accuracy of the conductive bump 141.

[0071] In this embodiment, the process of forming the second barrier layer 150 may include a deposition process.

[0072] Optionally, refer to Figures 7 to 9 , performing a patterning process on the second barrier layer 150 specifically includes:

[0073] forming a first photoresist layer 160 , wherein the first photoresist layer 160 covers the second barrier layer 150 ;

[0074] Performing exposure, development and other processes on the first photoresist layer 160 to retain a portion of the first photoresist layer 160;

[0075] The second barrier layer 150 is etched using the remaining portion of the first photoresist layer 160 as a mask.

[0076] Optionally, the material of the second barrier layer 150 includes titanium nitride and / or titanium. It can be understood that titanium nitride and titanium have good electrical conductivity, which can ensure the conductive connection between the conductive bump and other devices; both have good chemical stability, and when used as a mask layer, the mask layer can be prevented from being deformed or damaged, which is conducive to ensuring the etching barrier effect; titanium nitride and titanium can prevent material diffusion after the conductive bump is conductively connected to other devices, which is conducive to improving the reliability of the device.

[0077] Please refer to Fig.10, perform step S403: etch the conductive bump material layer 140 to form a conductive bump 141. Thus, before forming the passivation layer, the conductive bump 141 is formed first, so as to avoid the process of forming the conductive bump 141 from affecting the passivation layer, ensure the protection effect of the passivation layer, and help improve the reliability of the device; so that the position, shape, thickness and other characteristics of the conductive bump 141 are not restricted by the opening of the passivation layer, reduce the process difficulty, and help improve the preparation accuracy of the conductive bump 141.

[0078] Please refer to Fig.11 , step S404 is performed: forming a passivation layer 170, the passivation layer 170 includes a first portion 171 covering the top metal layer 120, a second portion 172 covering the side surface of the conductive bump 141, and a third portion 173 covering the top surface of the conductive bump 141. Thus, the passivation layer 170 is prepared after the conductive bump 141 is prepared, so that the passivation layer 170 is prevented from being affected by other processes, and the protection effect of the passivation layer 170 is greatly guaranteed.

[0079] In this embodiment, the material of the passivation layer 170 may include silicon nitride.

[0080] Please refer to Fig.14 , performing step S405: removing the third portion 173 and at least part of the second portion 172 to expose the conductive bump 141 outside the passivation layer 170. Thus, the conductive bump 141 is exposed outside the passivation layer 170, so that the conductive bump 141 is conductively connected to other devices.

[0081] In this embodiment, the process of removing the third portion 173 and at least a portion of the second portion 172 may include photolithography and etching processes.

[0082] Specifically, please refer to Figure 12 to Figure 14 , removing the third portion 173 and at least a portion of the second portion 172 may include:

[0083] forming a second photoresist layer 180 , wherein the second photoresist layer 180 covers the passivation layer 170 ;

[0084] Performing exposure, development and other processes on the second photoresist layer 180 to form an etching window 181 in the second photoresist, wherein the etching window 181 exposes the third portion 173;

[0085] The passivation layer 170 is etched using the second photoresist layer 180 having the etching window 181 as a mask to remove the third portion 173 and at least a portion of the second portion 172 .

[0086] Accordingly, an embodiment of the present application provides a semiconductor device, which is manufactured using the method for manufacturing a semiconductor device provided in the above embodiment.

[0087] The present application also provides a method for packaging a semiconductor device. Fig.15 , the packaging method includes:

[0088] Step S1501: providing a first substrate and a second substrate, wherein the first substrate and / or the second substrate is prepared by the method for preparing a semiconductor device provided in the above embodiment;

[0089] Step S1502: a bonding layer is provided on the first substrate and / or the second substrate, wherein the bonding layer comprises an insulating adhesive layer and a plurality of conductive particles, wherein the plurality of conductive particles are coated in the insulating adhesive layer;

[0090] Step S1503: bonding the first substrate and the second substrate correspondingly, and the first substrate and the second substrate are conductively connected via conductive particles.

[0091] It can be understood that the first substrate and / or the second substrate prepared by the method for preparing the semiconductor device provided by the above embodiment has good stability and reliability; on this basis, the adhesiveness of the adhesive layer is used to achieve a firm connection between the first substrate and the second substrate, replacing the traditional welding or bonding process, simplifying the packaging process, and using the conductive particles in the adhesive layer to achieve a conductive connection between the first substrate and the second substrate, which can achieve a micro-pitch connection and is conducive to device miniaturization. Therefore, while improving the stability and reliability of the device, the packaging material and process costs are reduced, and the production efficiency is improved.

[0092] Optionally, refer to Fig.16 and Fig.17 , the first substrate 10 and the second substrate 20 are bonded correspondingly, and the first substrate 10 and the second substrate 20 are conductively connected through the conductive particles 32, specifically including:

[0093] Place the first substrate 10 and the second substrate 20 correspondingly;

[0094] Performing a heating process on the first substrate 10 and / or the second substrate 20 provided with the adhesive layer 30 to melt the adhesive layer 30;

[0095] A pressurization process is performed on the first substrate 10 and / or the second substrate 20 to compress the adhesive layer 30 and aggregate the conductive particles 32 , so that the first substrate 10 and the second substrate 20 are conductively connected through the conductive particles 32 .

[0096] Optionally, the bonding layer 30 includes anisotropic conductive film. ACF is a transparent polymer connecting material with three major properties: bonding, conductivity, and insulation. It is conductive in the vertical direction and insulated in the horizontal direction. Therefore, short circuit can be avoided after packaging, which is beneficial to improving the reliability of the device.

[0097] It can be understood that in the actual structure, a conductive connection structure is formed on the first substrate 10 and the second substrate 20, and the first substrate 10 and the second substrate 20 are correspondingly bonded, which can be understood as the corresponding bonding of the conductive connection structures on the first substrate 10 and the second substrate 20. In the first substrate 10 and / or the second substrate 20 prepared by the method for preparing a semiconductor device provided by the above embodiment, the conductive connection structure can be understood as the conductive bump 141.

[0098] As an optional specific implementation, please refer to Fig.16 and Fig.17 , a method for packaging a semiconductor device, comprising:

[0099] Providing a first substrate 10, on which a first conductive connection structure 11 is formed;

[0100] Providing a second substrate 20, on which a second conductive connection structure 21 is formed;

[0101] A bonding layer 30 is disposed on the first substrate 10. The bonding layer 30 includes an insulating adhesive layer 31 and a plurality of conductive particles 32. The plurality of conductive particles 32 are encapsulated in the insulating adhesive layer 31.

[0102] The first conductive connection structure 11 of the first substrate 10 is correspondingly joined to the second conductive connection structure 21 of the second substrate 20, and the first conductive connection structure 11 and the second conductive connection structure 21 are conductively connected via the conductive particles 32;

[0103] The first substrate 10 and the second substrate 20 are manufactured by the method for manufacturing a semiconductor device provided in the above embodiment, the first conductive connection structure 11 is a conductive bump 141 , and the second conductive connection structure 21 is a conductive bump 141 .

[0104] It can be understood that in this specific implementation, the first substrate 10 and the second substrate 20 are manufactured by the method for manufacturing a semiconductor device provided by the above embodiment, and the first conductive connection structure 11 and the second conductive connection structure 21 are conductive bumps 141 .

[0105] As another optional specific implementation, please refer to Fig.18 and Fig.19 , a semiconductor device packaging method, comprising:

[0106] Providing a first substrate 10, on which a first conductive connection structure 11 is formed;

[0107] Providing a second substrate 20, on which a second conductive connection structure 21 is formed;

[0108] A bonding layer 30 is disposed on the first substrate 10. The bonding layer 30 includes an insulating adhesive layer 31 and a plurality of conductive particles 32. The plurality of conductive particles 32 are encapsulated in the insulating adhesive layer 31.

[0109] The first conductive connection structure 11 of the first substrate 10 is correspondingly joined to the second conductive connection structure 21 of the second substrate 20, and the first conductive connection structure 11 and the second conductive connection structure 21 are conductively connected via the conductive particles 32;

[0110] The second substrate 20 is manufactured by the method for manufacturing a semiconductor device provided by the above embodiment, and the second conductive connection structure 21 is a conductive bump 141 .

[0111] It can be understood that in this specific embodiment, the second substrate 20 is prepared by the method for preparing the semiconductor device provided in the above embodiment, and the second conductive connection structure 21 can be understood as a conductive bump 141. In an actual packaging process, the second substrate 20 can be a device substrate, the first substrate 10 can be a packaging substrate, and the first conductive connection structure 11 can be a pad on the packaging substrate. Of course, this embodiment does not exclude the case where the first conductive connection structure 11 is a conductive bump 141 when the first substrate 10 is not prepared by the method for preparing the semiconductor device provided in the above embodiment.

[0112] It should be noted that, in this embodiment, the first substrate 10 and / or the second substrate 20 is prepared by the method for preparing the semiconductor device provided in the above embodiment as the first condition, and the bonding layer 30 is set on the first substrate 10 and / or the second substrate 20 as the second condition, and there can be multiple combinations of the first condition and the second condition. The aforementioned optional specific implementation only schematically shows that the first condition is that the first substrate 10 and the second substrate 20 are prepared by the method for preparing the semiconductor device provided in the above embodiment, and the second condition is a combination of setting the bonding layer 30 on the first substrate 10; the aforementioned another optional specific implementation only schematically shows that the first condition is that the second substrate 20 is prepared by the method for preparing the semiconductor device provided in the above embodiment, and the second condition is a combination of setting the bonding layer 30 on the first substrate 10. Those skilled in the art can understand other combinations in combination with the aforementioned two optional specific implementations, so they are not listed here one by one.

[0113] The present application also provides a semiconductor device. Fig.14 ,include:

[0114] A substrate 100, on which a top metal layer 120 is formed;

[0115] A conductive bump 141 is located on the top metal layer 120 , and the conductive bump 141 is conductively connected to the top metal layer 120 ;

[0116] A passivation layer 170 covers the top metal layer 120 , and the conductive bump 141 is exposed outside the passivation layer 170 ;

[0117] It also includes: a first barrier layer 130, covering the top metal layer 120 and located between the top metal layer 120 and the conductive bump 141, the first barrier layer 130 is conductive, and the conductive bump 141 is conductively connected to the top metal layer 120 through the first barrier layer 130; and / or, a second barrier layer 150, covering the top surface of the conductive bump 141, and the second barrier layer 150 is conductive.

[0118] Therefore, by setting the first barrier layer 130 to cover the top metal layer 120 and be located between the top metal layer 120 and the conductive bump 141, in the process of forming the conductive bump 141, the first barrier layer 130 can be used as an etching stop layer to avoid affecting the top metal layer 120, which is beneficial to improving the stability and reliability of the device, and the first barrier layer 130 is conductive and can ensure the conductive connection between the top metal layer 120 and the conductive bump 141; the second barrier layer 150 covers the top surface of the conductive bump 141, and in the process of forming the conductive bump 141, the second barrier layer 150 can be used as a mask layer, which is beneficial to improving the preparation accuracy of the conductive bump 141, and the second barrier layer 150 is conductive and can ensure the conductive connection between the conductive bump 141 and other devices.

[0119] Optionally, the material of the first barrier layer 130 includes titanium nitride and / or titanium. It can be understood that titanium nitride and titanium have good electrical conductivity, which can ensure the conductive connection between the conductive bump 141 and the top metal layer 120; both have good chemical stability, and when used as an etching stop layer, they can ensure the etching barrier effect and avoid excessive etching affecting the top metal layer 120; titanium nitride and titanium can prevent material diffusion between the conductive bump 141 and the top metal layer 120, which is beneficial to improving the reliability of the device.

[0120] Optionally, the material of the second barrier layer 150 includes titanium nitride and / or titanium. It can be understood that titanium nitride and titanium have good electrical conductivity, which can ensure the conductive connection between the conductive bump 141 and other devices; both have good chemical stability, and when used as a mask layer, the mask layer can be prevented from being deformed or damaged, which is conducive to ensuring the etching blocking effect; titanium nitride and titanium can block the diffusion of materials after the conductive bump 141 is conductively connected to other devices, which is conducive to improving the reliability of the device.

[0121] Correspondingly, an embodiment of the present application also provides a semiconductor packaging structure, including the semiconductor device provided by the aforementioned embodiment.

[0122] It should be noted that the semiconductor device embodiments, semiconductor device preparation method embodiments and semiconductor device packaging method embodiments provided in the present application belong to the same concept; the technical features in the technical solutions recorded in each embodiment can be combined arbitrarily without conflict.

[0123] It should be understood that the above embodiments are exemplary and are not intended to include all possible implementations. Various modifications and changes may also be made on the basis of the above embodiments without departing from the scope of the present disclosure. Similarly, the various technical features of the above embodiments may also be combined arbitrarily to form other embodiments of the present application that may not be clearly described. Therefore, the above embodiments only express several implementations of the present application and do not limit the scope of protection of the patent of this application.

Claims

1. A method for preparing a semiconductor device, characterized in that: include: providing a substrate having a top metal layer formed thereon; forming a conductive bump material layer, wherein the conductive bump material layer covers the top metal layer, and the conductive bump material layer is conductively connected to the top metal layer; Etching the conductive bump material layer to form a conductive bump; forming a passivation layer, the passivation layer comprising a first portion covering the top metal layer, a second portion covering the side surface of the conductive bump, and a third portion covering the top surface of the conductive bump; The third portion and at least a portion of the second portion are removed to expose the conductive bump outside the passivation layer.

2. The method for preparing a semiconductor device according to claim 1, wherein: Before forming the conductive bump material layer, the preparation method further includes: forming a first barrier layer, the first barrier layer covering the top metal layer; the conductive bump material layer covering the first barrier layer; the first barrier layer is conductive, and the conductive bump material layer is conductively connected to the top metal layer through the first barrier layer; When performing the step of etching the conductive bump material layer, the first barrier layer is used as an etching stop layer.

3. The method for preparing a semiconductor device according to claim 2, characterized in that: The material of the first barrier layer includes titanium nitride and / or titanium.

4. The method for preparing a semiconductor device according to claim 1, wherein: Before etching the conductive bump material layer, the preparation method further includes: forming a second barrier layer, the second barrier layer covering the conductive bump material layer; performing a patterning process on the second barrier layer; When performing the step of etching the conductive bump material layer, the patterned second barrier layer is used as a mask layer.

5. The method for preparing a semiconductor device according to claim 4, characterized in that: The material of the second barrier layer includes titanium nitride and / or titanium.

6. A semiconductor device, characterized in that: The semiconductor device is prepared by the method for preparing the semiconductor device according to any one of claims 1 to 5.

7. A method for packaging a semiconductor device, characterized in that: include: Providing a first substrate and a second substrate, wherein the first substrate and / or the second substrate is prepared by the method for preparing a semiconductor device according to any one of claims 1 to 5; Arranging an adhesive layer on the first substrate and / or the second substrate, wherein the adhesive layer comprises an insulating adhesive layer and a plurality of conductive particles, wherein the plurality of conductive particles are encapsulated in the insulating adhesive layer; The first substrate and the second substrate are bonded correspondingly, and the first substrate and the second substrate are conductively connected via the conductive particles.

8. The method for packaging a semiconductor device according to claim 7, wherein: The bonding layer includes anisotropic conductive adhesive film.

9. A semiconductor device, characterized in that: include: a substrate having a top metal layer formed thereon; A conductive bump is located on the top metal layer, and the conductive bump is conductively connected to the top metal layer; A passivation layer covering the top metal layer, wherein the conductive bump is exposed outside the passivation layer; Among them, it also includes: a first barrier layer, covering the top metal layer and located between the top metal layer and the conductive bump, the first barrier layer is conductive, and the conductive bump is conductively connected to the top metal layer through the first barrier layer; and / or, a second barrier layer, covering the top surface of the conductive bump, the second barrier layer is conductive.

10. A semiconductor packaging structure, characterized in that: Comprising the semiconductor device as claimed in claim 9.