Formation method of semiconductor structure

The high-quality oxide layer is formed through ISSG and RTO oxidation treatment, and combined with high-temperature annealing treatment, the problem of insufficient quality of linear oxide layer in the STI isolation structure is solved, which significantly reduces leakage and interface defect density and improves the performance of semiconductor devices.

CN119028902AActive Publication Date: 2024-11-26ZHEJIANG ICSPROUT SEMICONDUCTOR CO LTD
View PDF 7 Cites 0 Cited by

Patent Information

Application Number
CN202411131870.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-16
Publication Date
2024-11-26
Estimated Expiration
2044-08-16

AI Technical Summary

Technical Problem

The quality of the linear oxide layer of the existing STI isolation structure needs to be improved, resulting in high leakage and interface defect density, affecting the performance of semiconductor devices.

Method used

Two oxidation treatment methods are used to form the first oxide layer and the second oxide layer in succession, and the medium is filled with high temperature annealing to improve the density and flatness of the oxide and reduce interface defects.

Benefits of technology

The quality of the sidewall oxide of the isolation structure is effectively improved, the leakage is reduced, the interface defect density between the isolation structure and the substrate is reduced, and the overall performance of the isolation structure is improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119028902A_ABST
    Figure CN119028902A_ABST
Patent Text Reader

Abstract

A forming method of a semiconductor structure comprises the following steps: providing a substrate; forming a groove in the substrate; performing first oxidation treatment on the side wall and the bottom of the groove in an ISSG mode to form a first oxidation layer; performing second oxidation treatment on the side wall and the bottom of the groove in an RTO mode, and forming a second oxidation layer between the first oxidation layer and the substrate; and after the second oxide layer is formed, filling a medium in the groove to form an isolation structure. The first oxide layer and the second oxide layer are formed by adopting an ISSG mode and an RTO mode in sequence, the quality of oxide on the side wall of the isolation structure can be further improved, electric leakage can be effectively reduced, and the defect density of an interface between the isolation structure and the substrate can be reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of semiconductor manufacturing, and in particular to a method for forming a semiconductor structure. Background Art

[0002] With the rapid development of semiconductor technology, the feature size of semiconductor devices has been significantly reduced, and higher requirements have been placed on chip manufacturing processes. One of the challenging issues is to fill the insulating medium between each film layer or in the trench evenly without holes to provide sufficient and effective isolation protection.

[0003] With the advancement of technology nodes and the entry of semiconductor processes into the deep submicron era, in order to meet the requirements of high-density integrated circuits and solve the bird's beak effect and white band effect in LOCOS isolation technology, the isolation between devices below 0.13μm has mostly been achieved using STI (Shallow Trench Isolation, STI) isolation structure.

[0004] However, the quality of the STI isolation structure formed by the prior art needs to be further improved. Summary of the invention

[0005] The problem solved by the present invention is how to further improve the quality of the linear oxide layer in the STI isolation structure.

[0006] In order to solve the above problems, the present invention provides a method for forming a semiconductor structure, comprising:

[0007] Providing a substrate; forming a trench in the substrate; performing a first oxidation treatment on the sidewalls and bottom of the trench by means of ISSG to form a first oxide layer; performing a second oxidation treatment on the sidewalls and bottom of the trench by means of RTO to form a second oxide layer between the first oxide layer and the substrate; after forming the second oxide layer, filling a dielectric in the trench to form an isolation structure.

[0008] Optionally, in the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the formed second oxide layer cooperates with the first oxide layer to form a linear stack.

[0009] Optionally, in the step of performing a first oxidation treatment on the sidewall and the bottom of the trench by means of ISSG, the thickness of the first oxide layer is to In the step of performing a second oxidation treatment on the sidewall and bottom of the trench by RTO, the thickness of the second oxide layer is formed in to within the range.

[0010] Optionally, in the step of performing a first oxidation treatment on the sidewall and the bottom of the trench by means of ISSG, the process temperature is in the range of 950° C. to 1150° C., and the process gas includes: hydrogen and oxygen.

[0011] Optionally, in the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the process temperature is in the range of 850° C. to 1150° C., and the process gas includes: oxygen and nitrogen.

[0012] Optionally, the method further includes: performing a high temperature annealing process after filling a dielectric in the trench to form an isolation structure.

[0013] Optionally, in the step of performing high temperature annealing, the process temperature is in the range of 1000° C. to 1150° C., and the process time is in the range of 15 s to 20 s.

[0014] Optionally, in the step of performing high temperature annealing, the high temperature annealing is performed in a hydrogen-containing atmosphere.

[0015] Optionally, in the step of performing high temperature annealing treatment, the hydrogen-containing atmosphere includes: hydrogen.

[0016] Optionally, in the step of performing high temperature annealing treatment, the hydrogen-containing atmosphere further includes: an inert gas.

[0017] Optionally, in the step of performing high temperature annealing, the inert gas includes at least one of nitrogen and argon.

[0018] Compared with the prior art, the technical solution of the present invention has the following advantages:

[0019] In the technical solution of the present invention, after the trench is formed in the substrate, before the dielectric layer is filled in the trench to form an isolation structure, the sidewall and bottom of the trench are first oxidized by ISSG; and then the sidewall and bottom of the trench are second oxidized by RTO. The oxide grown by oxidation by ISSG has better overall uniformity and faster growth rate; the oxide grown by oxidation by RTO has higher density and surface flatness, fewer defects, and better passivation effect; therefore, the ISSG method and the RTO method are successively used to form the first oxide layer and the second oxide layer, which can further improve the quality of the oxide on the sidewall of the isolation structure, effectively reduce leakage, and reduce the defect density at the interface between the isolation structure and the substrate.

[0020] In an optional solution of the present invention, after the dielectric is filled in the trench to form an isolation structure, a high temperature annealing treatment is performed. After the isolation structure is formed, the high temperature annealing treatment is performed. The thermal effect of the high temperature annealing treatment can promote the structural relaxation of the formed oxide. The structural relaxation of the oxide material can not only improve the density, but also release the stress, which can effectively improve the quality of the formed isolation structure.

[0021] In an optional solution of the present invention, the high temperature annealing treatment after the isolation structure is formed is performed in a hydrogen-containing atmosphere. When the high temperature annealing is performed in a hydrogen-containing atmosphere, the hydrogen in the atmosphere can be effectively diffused in the material, thereby reacting with defects in the oxide to repair the defects and passivating the substrate surface to reduce the interface state. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figures 1 to 3 It is a structural schematic diagram of each step of a method for forming a semiconductor structure;

[0023] Figures 4 to 7 It is a structural schematic diagram of each step of an embodiment of a method for forming a semiconductor structure of the present invention. DETAILED DESCRIPTION

[0024] As can be seen from the background technology, the isolation structure formed by the prior art has the problem of quality needing to be improved. Now, in combination with a method for forming a semiconductor structure, the reasons why the quality of the isolation structure needs to be improved are analyzed:

[0025] refer to Figures 1 to 3 , showing a structural schematic diagram of each step of a method for forming a semiconductor structure.

[0026] The forming method comprises: Figure 1 As shown, the substrate 11 is cleaned to obtain a clean surface; after cleaning, an oxide layer 12 and a nitride layer 13 are sequentially formed on the surface of the substrate 11; through a photolithography process, a mask pattern is formed on the nitride layer 13 and then etched to form a groove 14 in the substrate 11.

[0027] After forming the groove 14, Figure 2 As shown, a linear oxide layer 15 is formed on the sidewall and bottom of the trench 14; then, as shown Figure 3 As shown, oxide is filled into the trench with the linear oxide layer 15 formed inside and excess oxide is removed to form an isolation structure 16; after the isolation structure 16 is formed, damage is repaired by rapid thermal oxidation, and the nitride layer is etched away.

[0028] At the sharp corners of the isolation structure 16, the electric field is easily concentrated, which can easily lead to a decrease in device performance. Therefore, after the trench 14 is formed and before the isolation structure 16 is formed, an oxide is formed on the sidewall and bottom of the trench 14 to avoid leakage problems caused by parasitic transistors, electric field concentration, etc., and at the same time, it can also repair the damage caused by etching.

[0029] like Figure 2 As shown, in the above method, the sidewall and bottom of the groove 14 are oxidized to form an oxide by ISSG (In-Situ Steam Generation). During the ISSG reaction, a large number of gas-phase active free radicals are generated, among which the oxygen atoms have a very high reactivity, which can easily cause the surface oxygen atoms to react before forming a regular arrangement, and Si-H bonds and Si-OH bonds are easily generated during the oxidation process, thereby causing surface defects.

[0030] In order to solve the above technical problem, the present invention provides a method for forming a semiconductor structure, comprising:

[0031] Providing a substrate; forming a trench in the substrate; performing a first oxidation treatment on the sidewalls and bottom of the trench by an ISSG method to form a first oxide layer, wherein the process gas used in the first oxidation treatment contains hydrogen; performing a second oxidation treatment on the sidewalls and bottom of the trench by an RTO method to form a second oxide layer between the first oxide layer and the substrate, wherein the process gas used in the second oxidation treatment does not contain hydrogen; after forming the second oxide layer, filling the trench with a dielectric to form an isolation structure.

[0032] In the technical solution of the present invention, after the groove is formed in the substrate, before the dielectric layer is filled in the groove to form an isolation structure, the sidewall and bottom of the groove are first oxidized by ISSG; and then the sidewall and bottom of the groove are second oxidized by RTO. The oxide grown by oxidation by ISSG has better overall uniformity and faster growth rate; the oxide grown by oxidation by RTO has higher density and surface flatness, fewer defects, and better passivation effect; therefore, the first oxide layer and the second oxide layer are formed by ISSG and RTO respectively, which can further improve the quality of the oxide on the sidewall of the isolation structure, effectively reduce leakage, and reduce the defect density at the interface between the isolation structure and the substrate.

[0033] In order to make the above-mentioned objects, features and advantages of the present invention more obvious and easy to understand, specific embodiments of the present invention are described in detail below with reference to the accompanying drawings.

[0034] refer to Figures 4 to 7 , showing a schematic structural diagram of each step of an embodiment of a semiconductor structure of the present invention.

[0035] The forming method comprises:

[0036] Providing a substrate 110;

[0037] forming a groove 120 in the substrate 110;

[0038] Performing a first oxidation treatment on the sidewall and the bottom of the trench 120 by means of ISSG to form a first oxide layer 131, wherein the process gas used in the first oxidation treatment includes hydrogen;

[0039] Performing a second oxidation treatment on the sidewall and the bottom of the trench 120 by RTO to form a second oxide layer 132 between the first oxide layer 131 and the substrate 110, wherein the process gas used in the second oxidation treatment does not contain hydrogen;

[0040] After forming the second oxide layer 132 , a dielectric is filled in the trench 120 to form an isolation structure 140 .

[0041] The technical solution of an embodiment of the method for forming a semiconductor structure of the present invention will be described in detail below with reference to the accompanying drawings.

[0042] First, refer to Figure 4 , providing a substrate 110.

[0043] The substrate 110 is used to improve the process operation platform and mechanical support.

[0044] In some embodiments of the present invention, the substrate 110 is a silicon substrate, and the material of the substrate 110 is silicon. Specifically, the material of the substrate 110 can be selected from single crystal silicon, polycrystalline silicon or amorphous silicon. In other embodiments, the material of the substrate can also be selected from silicon, germanium, gallium arsenide or silicon germanium compound; the substrate can also be selected from having an epitaxial layer or a silicon structure on an epitaxial layer; the substrate can also be other semiconductor materials.

[0045] It should be noted that, in some embodiments, after providing the substrate 110 , the surface of the substrate 110 is cleaned to obtain a clean substrate surface.

[0046] like Figure 4 As shown, in some embodiments, the forming method further includes: after providing the substrate 110 , forming an oxide layer 111 and a nitride layer 112 on the substrate 110 .

[0047] The oxide layer 111 is used as a buffer layer between the nitride layer 112 and the substrate 110 to relieve the stress of the nitride layer 112 on the substrate 110 ; the nitride layer 112 is used to act as a stop layer in subsequent process steps.

[0048] In some embodiments, the oxide layer 111 may be formed on the surface of the substrate 110 by oxidizing the surface of the substrate 110 ; or the oxide layer 111 may be formed on the surface of the substrate 110 by deposition.

[0049] In some embodiments, the nitride layer 112 may be formed on the surface of the oxide layer 111 by nitriding the surface of the oxide layer; or the nitride layer 112 may be formed on the surface of the oxide layer 111 by deposition.

[0050] Continue to refer Figure 4 , a trench 120 is formed in the substrate 110 .

[0051] The trench 120 is used to provide a structural basis for forming an isolation structure.

[0052] Specific as Figure 4 As shown, the step of forming the groove 120 in the substrate 110 includes: forming a mask layer on the substrate 110, patterning the mask layer through a photolithography process to form a mask layer with a pattern; using the mask layer with the pattern as a mask, etching the substrate 110 to form the groove 120 in the substrate 110.

[0053] The mask layer is used for pattern transfer. For example, the mask layer may include a photoresist layer, and the mask layer is patterned by a photolithography process including exposure and development to form a mask layer with a pattern; wherein the pattern in the mask layer can define the position and size of the groove 120.

[0054] For example, in the step of etching the substrate 110 and forming the groove 120 in the substrate 110 , the substrate 110 may be etched by at least one of dry etching and wet etching.

[0055] Next, refer to Figure 5 , a first oxidation treatment is performed on the sidewall and bottom of the trench 120 by an ISSG method to form a first oxide layer 131 .

[0056] The first oxide layer 131 is used to round sharp corners and repair damage. The sidewall and bottom of the groove 120 are subjected to the first oxidation treatment by ISSG (In-Situ Steam Generation), which has the advantages of fast generation speed and good uniformity.

[0057] Specifically, in some embodiments, the substrate 110 is a silicon substrate; in the step of performing a first oxidation treatment on the sidewall and the bottom of the trench 120 by means of ISSG, the material of the formed first oxide layer 131 is silicon oxide.

[0058] In some embodiments of the present invention, in the step of performing a first oxidation treatment on the sidewall and the bottom of the trench 120 by means of ISSG, the thickness of the first oxide layer 131 is formed to be to The thickness of the formed first oxide layer 131 is appropriate, which can effectively round off the sharp corners and repair the etching damage while ensuring the process efficiency.

[0059] In some embodiments, in the step of performing a first oxidation treatment on the sidewall and the bottom of the trench 120 by means of ISSG, the process temperature is in the range of 950° C. to 1150° C., and the process gas includes: hydrogen and oxygen. The first oxidation treatment process temperature is suitable, which can effectively activate the process gas, and can effectively form a highly uniform first oxide layer 131 while ensuring the ISSG reaction efficiency.

[0060] Afterwards, refer to Figure 6 , a second oxidation treatment is performed on the sidewall and the bottom of the trench 120 by RTO to form a second oxide layer 132 between the first oxide layer 131 and the substrate 110 .

[0061] The second oxidation treatment is used to further repair the defects at the interface between the first oxide layer 131 and the substrate 110, so as to repair the interface defects and improve the quality of the isolation structure.

[0062] Specifically, in some embodiments, the substrate 110 is a silicon substrate; in the step of performing a second oxidation treatment on the sidewall and the bottom of the trench 120 by RTO, the material of the formed second oxide layer 132 is silicon oxide.

[0063] In some embodiments of the present invention, in the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the second oxide layer 132 formed cooperates with the first oxide layer 131 to form a linear stack 130. In the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the thickness of the second oxide layer 132 formed is determined by the technical requirements of the linear stack 130 and the thickness of the first oxide layer 131 formed.

[0064] In some embodiments, in the step of performing a second oxidation treatment on the sidewall and the bottom of the trench 120 by RTO, the thickness of the second oxide layer 132 is formed to be to The thickness of the formed second oxide layer 132 is appropriate, and the thickness ratio between the second oxide layer 132 and the first oxide layer 131 is appropriate, so that the linear stack 130 can be formed quickly and effectively, the process efficiency is ensured, and the formed linear stack 130 has better quality, fewer defects, and higher quality.

[0065] In some embodiments, in the step of performing a second oxidation treatment on the sidewall and the bottom of the trench 120 by RTO, the process temperature is in the range of 850° C. to 1150° C., and the process gas includes: oxygen and nitrogen. In the process of performing a second oxidation treatment on the sidewall and the bottom of the trench 120 by RTO, there is no hydrogen, and no Si-H bond or Si-OH bond is formed. The formed oxide structure has higher density and flatness, fewer defects, and better passivation effect.

[0066] refer to Figure 7 After forming the second oxide layer 132 , a dielectric is filled in the trench 120 to form an isolation structure 140 .

[0067] Specifically, Figure 7 As shown, the step of filling the dielectric in the trench 120 to form the isolation structure 140 includes: filling the dielectric material into the trench 120, the formed dielectric material fills the trench 120 and extends onto the nitride layer and the oxide layer 111; removing excess dielectric material, retaining the dielectric material in the trench 140, and forming the isolation structure 140.

[0068] In some embodiments, in the step of filling the dielectric material into the trench 120, the dielectric material can be filled into the trench 120 by HDPCVD (High Density Plasma Chemical Vapor Deposition); in the step of removing excess dielectric material on the nitride layer and the oxide layer 111, the nitride layer can be used as a stop layer, and CMP (Chemical Mechanical Polishing) can be used to remove excess dielectric material on the nitride layer and the oxide layer 111, thereby forming the isolation structure 140.

[0069] It should be noted that in some embodiments, after removing the excess dielectric material and forming the isolation structure 140, the formation method further includes: removing the nitride layer 112 (such as Figure 6 As shown). For example, the nitride layer 112 can be removed by wet etching.

[0070] In some embodiments of the present invention, the formation method further comprises: performing high temperature annealing after filling the dielectric in the trench 120 to form the isolation structure 140. The thermal effect of the high temperature annealing can promote the structural relaxation of the formed oxide, thereby achieving the effect of improving density and relieving stress.

[0071] In some embodiments, in the step of high temperature annealing, the process temperature is in the range of 1000° C. to 1150° C., and the process time is in the range of 15s to 20s. The temperature and time of high temperature annealing are suitable, which can effectively balance the thermal budget and annealing effect, and can control the process analysis while improving the quality of the isolation structure.

[0072] In some embodiments, in the step of performing high temperature annealing, the high temperature annealing is performed in a hydrogen-containing atmosphere. When performing high temperature annealing in a hydrogen-containing atmosphere, the hydrogen in the atmosphere can be effectively diffused in the material, thereby reacting with defects in the oxide to repair the defects and passivating the substrate surface to reduce the interface state. For example, in the step of performing high temperature annealing, the hydrogen-containing atmosphere includes: hydrogen.

[0073] In some embodiments, in the step of performing high temperature annealing, the hydrogen-containing atmosphere further comprises: an inert gas. The atmosphere in which the high temperature annealing is performed also comprises: an inert gas to play a protective role. For example, in the step of performing high temperature annealing, the inert gas comprises at least one of nitrogen and argon.

[0074] In summary, after the trench is formed in the substrate, before the dielectric layer is filled in the trench to form an isolation structure, the sidewall and bottom of the trench are first oxidized by the ISSG method; and then the sidewall and bottom of the trench are second oxidized by the RTO method. The oxide grown by oxidation by the ISSG method has better overall uniformity and a faster growth rate; the oxide grown by oxidation by the RTO method has higher density and surface flatness, fewer defects, and better passivation effect; therefore, the ISSG method and the RTO method are successively used to form the first oxide layer and the second oxide layer, which can further improve the quality of the oxide on the sidewall of the isolation structure, and can effectively reduce leakage and reduce the defect density at the interface between the isolation structure and the substrate.

[0075] Moreover, after the dielectric is filled in the trench to form the isolation structure, a high temperature annealing treatment is performed. After the isolation structure is formed, the high temperature annealing treatment is performed. The thermal effect of the high temperature annealing treatment can promote the structural relaxation of the formed oxide. The structural relaxation of the oxide material can not only improve the density, but also release the stress, which can effectively improve the quality of the formed isolation structure.

[0076] In addition, the high temperature annealing treatment after the isolation structure is formed is performed in a hydrogen-containing atmosphere. In the high temperature annealing in the hydrogen-containing atmosphere, the hydrogen in the atmosphere can be effectively diffused in the material, thereby reacting with the defects in the oxide to repair the defects and passivating the substrate surface to reduce the interface state.

[0077] Although the present invention is disclosed as above, the present invention is not limited thereto. Any person skilled in the art can make various changes and modifications without departing from the spirit and scope of the present invention. Therefore, the protection scope of the present invention shall be subject to the scope defined by the claims.

Claims

1. A method for forming a semiconductor structure, characterized in that: include: providing a substrate; forming a trench in the substrate; Performing a first oxidation treatment on the sidewall and bottom of the trench by means of ISSG to form a first oxide layer; Performing a second oxidation treatment on the sidewall and bottom of the trench by RTO to form a second oxide layer between the first oxide layer and the substrate; After forming the second oxide layer, a dielectric is filled in the trench to form an isolation structure.

2. The forming method according to claim 1, characterized in that: In the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the formed second oxide layer cooperates with the first oxide layer to form a linear stack.

3. The forming method according to claim 2, characterized in that: In the step of performing a first oxidation treatment on the sidewall and the bottom of the trench by means of ISSG, the thickness of the first oxide layer is formed to be to within the scope; In the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the thickness of the second oxide layer is formed to be to within the range.

4. The forming method according to claim 1, characterized in that: In the step of performing a first oxidation treatment on the sidewall and the bottom of the trench by means of ISSG, the process temperature is in the range of 950° C. to 1150° C., and the process gas includes: hydrogen and oxygen.

5. The forming method according to claim 1, characterized in that: In the step of performing a second oxidation treatment on the sidewall and the bottom of the trench by RTO, the process temperature is in the range of 850° C. to 1150° C., and the process gas includes: oxygen and nitrogen.

6. The forming method according to claim 1, characterized in that: Also includes: After the dielectric is filled in the trench to form an isolation structure, a high temperature annealing process is performed.

7. The forming method according to claim 6, characterized in that: In the step of performing high temperature annealing treatment, the process temperature is in the range of 1000° C. to 1150° C., and the process time is in the range of 15 s to 20 s.

8. The forming method according to claim 6, characterized in that: In the step of performing a high temperature annealing treatment, a high temperature annealing treatment is performed in a hydrogen-containing atmosphere.

9. The forming method according to claim 8, characterized in that: In the step of performing high temperature annealing treatment, the hydrogen-containing atmosphere includes: hydrogen.

10. The forming method according to claim 8, characterized in that: In the step of performing high temperature annealing treatment, the hydrogen-containing atmosphere further comprises: an inert gas.

11. The forming method according to claim 10, characterized in that: In the step of performing high temperature annealing treatment, the inert gas includes at least one of nitrogen and argon.

Citation Information

Patent Citations

  • Isolation structure of shallow plough groove and manufacturing method thereof

    CN101295664A

  • Manufacturing method of shallow trench structure and flash memory

    CN101740456A

  • Manufacturing method of shallow trench isolation structure

    CN101930941A

  • Manufacturing method of shallow trench isolation

    CN102222636A

  • Method for forming shallow channel isolation region

    CN103579076A