Damper with wide, thin and flat conductive structure and manufacturing method thereof

By using a wide and flat conductive structure with a wide shape and a weft yarn to fix the multi-filament wire body in the dynamic coil horn, the problems of the shift and manufacturing steps of the conductive structure during the hot pressing process are solved, and the stability of the conductive structure is achieved Positioning and sound quality consistency reduces cost and fatigue resistance.

CN119031319APending Publication Date: 2024-11-26大原祐子
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310598987.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-05-25
Publication Date
2024-11-26

AI Technical Summary

Technical Problem

The conductive structures in existing dynamic coil speakers are easily deviated during the hot pressing process, resulting in different sound quality, and are complex in manufacturing steps, high in cost, and are prone to overheating and breaking.

Method used

Adopt a conductive structure with a wide and flat shape, fixing the multi-wire thread body through weft yarns, and using the weaving method of metal yarns to ensure that the conductive structure does not deviate during the hot pressing process, and uniformizing the hardness of the conductive structure through elastic adjustment areas and Resilience, reduce costs.

Benefits of technology

The stable positioning of the conductive structure is achieved, the manufacturing steps and costs are reduced, the overheating and breaking of the conductive structure is avoided, and the sound quality consistency and fatigue resistance are improved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119031319A_ABST
    Figure CN119031319A_ABST
Patent Text Reader

Abstract

The invention discloses a manufacturing method of a damper with a wide, thin and flat conductive structure. The method comprises the following steps: covering the outer surface of a core wire with a metal layer to form a metal yarn; the first interweaving part of the metal yarn is interwoven with the second interweaving part of the metal yarn to weave a multifilament yarn body; the two ends of the first interweaving parts are connected with the second interweaving parts, the first interweaving parts are parallel to each other, the second interweaving parts are parallel to each other, and the extending directions of the first interweaving parts and the second interweaving parts are different; the multiple warp yarns and the at least one multifilament yarn body are arranged at intervals, linearly extend and are parallel to each other; a plurality of weft yarns are interwoven between the warp yarns and the multifilament yarn bodies to weave the base material; soaking the base material in the resin solution; drying the base material; a body and a conductive structure are formed on the base material through hot pressing; and separating the body from the substrate while separating the conductive structure from the multifilament thread.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a wave damper and a manufacturing method thereof, in particular to a wave damper with a wide, thin and flat conductive structure and a manufacturing method thereof. Background Art

[0002] In a dynamic speaker, the conductive structure is responsible for transmitting the power alternating current to the voice coil, and the elastic wave is responsible for maintaining the correct position of the voice coil in the gap between the iron core of the magnet, ensuring that the voice coil reciprocates along the axis when subjected to force. The conductive structure is fixed to the body of the elastic wave, which can support the conductive structure, improve the fatigue resistance of the conductive structure and prevent it from breaking easily.

[0003] The conductive structure can be fixed on the body of the wave damper by using stitches. However, the stitches need to be manually operated with a sewing machine to sew the conductive structure to the surface of the body of the wave damper. Furthermore, the steps are quite complicated.

[0004] The conductive structure can be clamped by two main bodies. However, during the hot pressing process, the position of the conductive structure will shift away from the optimal position, thus affecting the common resonance efficiency of the elastic wave, voice coil and diaphragm. Furthermore, the offset of the conductive structure is different in each elastic wave, resulting in slightly different sound quality for each speaker. In addition, the steps are quite complicated.

[0005] Because the conductive structure is harder than the warp and weft yarns, and the elasticity and toughness of the conductive structure are worse than those of the warp and weft yarns, the area where the conductive structure passes is harder than other areas of the body of the spring wave, and the elasticity and toughness of the area where the conductive structure passes are worse than those of other areas of the body of the spring wave. Therefore, the hardness, elasticity and toughness of the spring wave are uneven, resulting in uneven elastic recovery force and fatigue resistance of the spring wave, making the spring wave easily deformed, thereby affecting the sound quality of the speaker output.

[0006] The cross-section of the conventional conductive structure is circular. The circular conductive structure is usually formed by twisting a plurality of metal yarns. Each metal yarn has a portion located in the center. The portion located in the center is shielded by other metal yarns, and the heat generated is not easy to be discharged. There is a problem of heat accumulation, which causes the circular conductive structure to overheat easily.

[0007] Furthermore, the circular conductive structure is relatively thick and protrudes much from the surface of the damper body, so that the circular conductive structure is easily crushed by the mold or even broken.

[0008] In addition, the ends of the twisted circular conductive structure are spread out, and are not easy to be bonded to the contact point of the connection terminal and the coil of the voice coil by glue dispensing.

[0009] In addition, the colloid is prone to aging and losing its viscosity, causing the end of the circular conductive structure to easily spread apart and then separate from the contact point of the connection terminal and the coil of the voice coil.

[0010] Furthermore, the general metal yarn is entirely made of metal, which is relatively expensive.

[0011] In addition, at least twenty of the metal yarns must be twisted into a circular conductive structure, which results in a high manufacturing cost. Summary of the invention

[0012] The main purpose of the present invention is to provide a wave spring having a wide, thin and flat conductive structure and a manufacturing method thereof, which uses weft yarn to fix the multifilament line body and does not require any stitches.

[0013] Another object of the present invention is to provide a wave spring having a wide, thin and flat conductive structure and a method for manufacturing the same, wherein the multifilament wire body is fixed by weft yarn, and during the hot pressing process, the multifilament wire body is guaranteed not to be offset, and after being cut, the conductive structure is guaranteed to be located in the optimal position.

[0014] Another object of the present invention is to provide a wave damper having a wide, thin and flat conductive structure and a method for manufacturing the same, wherein the elastic adjustment region is used to adjust the hardness, elasticity and toughness of the region through which the conductive structure passes, so that the region through which the conductive structure passes becomes softer, more elastic and more tough.

[0015] Another object of the present invention is to provide a wave damper having a wide, thin and flat conductive structure and a manufacturing method thereof. The shape of the conductive structure and the weaving method of the metal yarns allow the metal yarns to be exposed and not be shielded by other metal yarns.

[0016] Another object of the present invention is to provide a wave damper having a wide, thin and flat conductive structure and a manufacturing method thereof, wherein the risk of the conductive structure being crushed is low.

[0017] Another object of the present invention is to provide a damper having a wide, thin and flat conductive structure and a manufacturing method thereof, wherein the solder portion can prevent the end of the conductive structure from spreading and is combined with a connecting terminal and a voice coil.

[0018] Another object of the present invention is to provide a wave damper having a wide, thin and flat conductive structure and a manufacturing method thereof, wherein the composition of the metal yarn can reduce the cost and maintain a certain conductivity.

[0019] Another object of the present invention is to provide a wave damper having a wide, thin and flat conductive structure and a manufacturing method thereof, wherein the weaving method of the metal yarn can weave a multifilament line body with a minimum number of yarns.

[0020] In order to achieve the above-mentioned purpose, the present invention provides a method for manufacturing a waveguide having a conductive structure with a wide, thin and flat shape, comprising the following steps: a metal layer is covered on the outer surface of a core wire to form a metal yarn; a plurality of first interlaced portions of a plurality of metal yarns are interlaced with a plurality of second interlaced portions of the metal yarns to weave a multifilament wire body with a wide, thin and flat shape; wherein the two ends of each of the first interlaced portions are respectively connected to a second interlaced portion, the first interlaced portions are parallel to each other, the second interlaced portions are parallel to each other, and the extensions of the first interlaced portions and the second interlaced portions are The invention relates to a method for knitting a substrate having a plurality of warp yarns and at least one multifilament yarn in different directions; a plurality of warp yarns are arranged at intervals from at least one multifilament yarn, and the warp yarns and the at least one multifilament yarn extend straight and parallel to each other; a plurality of weft yarns are interwoven between the warp yarns and the at least one multifilament yarn to weave a substrate; the substrate is immersed in a resin solution; the substrate is dried; a main body of a spring wave is formed on the substrate by heat press molding, and at least two conductive structures having a wide, thin and flat shape are formed on the at least one multifilament yarn by heat press molding; and the main body is separated from the substrate, and at the same time, the at least two conductive structures are separated from the at least one multifilament yarn.

[0021] In some embodiments, the step of spacing the warp yarns from the at least one multifilament thread body further includes: the distance between the at least one multifilament thread body and the warp yarns on both sides thereof is greater than the distance between the warp yarns; wherein, the step of weaving the substrate further includes: the weft yarns define a first elastic adjustment area between a first side of the at least one multifilament thread body and the warp yarns closest to the first side of the at least one multifilament thread body, and the weft yarns define a second elastic adjustment area between a second side of the at least one multifilament thread body and the warp yarns closest to the second side of the at least one multifilament thread body, and the widths of the first elastic adjustment area and the second elastic adjustment area are equal.

[0022] In some embodiments, after the step of separating the body from the substrate, the method further comprises: soldering two ends of the conductive structures to form at least four solder portions.

[0023] In some embodiments, the core wire is made of cotton.

[0024] In some embodiments, the number of the metal yarns is seven.

[0025] In order to achieve the aforementioned objectives, the present invention provides a waveguide having a conductive structure that is wide, thin and flat, comprising a main body and at least two conductive structures. The main body is formed by interweaving a plurality of warp yarns and a plurality of weft yarns. The conductive structures are wide, thin and flat, spaced apart from the warp yarns, extending in a straight line and parallel to each other, and interwoven with the weft yarns. Each of the conductive structures is a multifilament body that is wide, thin and flat, and the multifilament body is interwoven by a plurality of first interwoven portions of a plurality of metal yarns and a plurality of second interwoven portions of the metal yarns. Each of the metal yarns is formed by a metal layer covering the outer surface of a core wire. The two ends of each of the first interwoven portions are respectively connected to a second interwoven portion, the first interwoven portions are parallel to each other, the second interwoven portions are parallel to each other, and the first interwoven portions extend in different directions from the second interwoven portions.

[0026] In some embodiments, the distance between the at least one multifilament thread and the warp yarns on both sides thereof is greater than the distance between the warp yarns, the weft yarns define a first elastic adjustment area between a first side of the at least one multifilament thread and the warp yarns closest to the first side of the at least one multifilament thread, and the weft yarns define a second elastic adjustment area between a second side of the at least one multifilament thread and the warp yarns closest to the second side of the at least one multifilament thread, and the widths of the first elastic adjustment area and the second elastic adjustment area are equal.

[0027] In some embodiments, the damper further includes at least four solder portions, which are respectively soldered on two ends of the conductive structures.

[0028] In some embodiments, the core wire is made of cotton.

[0029] In some embodiments, the number of the metal yarns is seven.

[0030] The effect of the present invention is that the multifilament thread body is fixed by weft yarn, no stitching is required, the manufacturing steps are reduced, and the manufacturing cost of the elastic wave is reduced.

[0031] Furthermore, by using weft yarn to fix the multifilament wire body, the multifilament wire body is guaranteed not to shift during the hot pressing process, and after being cut, the conductive structure is guaranteed to be located in the best position.

[0032] In addition, the hardness, elasticity and toughness of the area through which the conductive structure passes are jointly adjusted by the first elastic adjustment area and the second elastic adjustment area, so that the area through which the conductive structure passes becomes softer, more elastic and more tough, so that the hardness, elasticity and toughness of the area through which the conductive structure passes are comparable to other areas of the body.

[0033] In addition, the conductive structure is wide, thin and flat, and based on the weaving method of the metal yarn, the metal yarn is exposed and will not be blocked by other metal yarns. The heat generated can be easily discharged without the problem of heat accumulation, so the conductive structure will not overheat.

[0034] In addition, the conductive structure is wide, thin and flat, and only slightly protrudes from the surface of the body, so the risk of being crushed by the mold is low.

[0035] Also, the solder portion can prevent the end of the conductive structure from being scattered and directly connect to the contact point of the connection terminal and the coil of the voice coil.

[0036] It is worth mentioning that the inner layer of each metal yarn is a core wire, and the outer layer of each metal yarn is a metal layer, which can not only reduce the cost but also maintain a certain electrical conductivity.

[0037] It is worth mentioning that, based on the weaving method of the metal yarns, only seven metal yarns are needed to weave a multifilament wire body and cut into two conductive structures, so the manufacturing cost is relatively low. BRIEF DESCRIPTION OF THE DRAWINGS

[0038] Figure 1 is a flow block diagram of the method of the present invention;

[0039] Figure 2 is a schematic diagram of step S10 of the method of the present invention;

[0040] Figure 3 is a schematic diagram of step S20 of the method of the present invention;

[0041] Figure 4 yes Figure 3 A cross-sectional view of line VI-VI;

[0042] Figure 5 is a schematic diagram of step S30 of the method of the present invention;

[0043] Figure 6 is a schematic diagram of step S40 of the method of the present invention;

[0044] Figure 7 is a schematic diagram of step S50 of the method of the present invention;

[0045] Figure 8 is a schematic diagram of step S60 of the method of the present invention;

[0046] Fig. 9 is a schematic diagram of step S70 of the method of the present invention;

[0047] Fig.10 is a schematic diagram of step S80 of the method of the present invention;

[0048] Fig.11 is a schematic diagram of step S90 of the method of the present invention;

[0049] Fig.12 is a three-dimensional diagram of the spring wave of the present invention;

[0050] Fig.13 is a stereogram of a speaker of the present invention;

[0051] Fig.14 is an exploded view of the speaker of the present invention;

[0052] Fig.15 It is a cross-sectional view of the speaker of the present invention.

[0053] Description of Figure Numbers

[0054] 10:Metallic Yarn

[0055] 11:Metal layer

[0056] 12: Core wire

[0057] 13: First interweaving section

[0058] 14: Second interweaving section

[0059] 20:Multifilament thread

[0060] 21: First side

[0061] 22: Second side

[0062] 30: Warp

[0063] 40: Weft

[0064] 50: Base material

[0065] 61: First elastic adjustment area

[0066] 62: Second elastic adjustment area

[0067] 70: Resin tank

[0068] 71: Resin solution

[0069] 81: First baking sheet

[0070] 82: Second baking sheet

[0071] 91: First mold

[0072] 911: Groove

[0073] 912: Pressing surface

[0074] 92: Second mold

[0075] 921: Groove

[0076] 922: Molding surface

[0077] 110: First cutter

[0078] 120: Second cutter

[0079] 130:Welding tools

[0080] 200:Ball

[0081] 210:Ontology

[0082] 211: Wave

[0083] 2111: Crest

[0084] 2112: Trough

[0085] 220: Conductive structure

[0086] 230:Soldering Department

[0087] 300: Speaker

[0088] 310: Speaker body

[0089] 311: Base

[0090] 312: Magnetic return device

[0091] 313: Frame

[0092] 314: Diaphragm

[0093] 315: Dust cover

[0094] 316: Overhang

[0095] 317: Connecting terminal

[0096] 320: Voice coil

[0097] 321: Coil

[0098] D1,D2: distance

[0099] S10~S90: Steps DETAILED DESCRIPTION

[0100] The following is a more detailed description of the embodiments of the present invention with reference to the accompanying drawings and element symbols, so that those skilled in the art can implement the embodiments according to the embodiments after reading the specification.

[0101] Figure 1 is a flow chart of the method of the present invention, Figure 2 is a schematic diagram of step S10 of the method of the present invention, Figure 3 is a schematic diagram of step S20 of the method of the present invention, Figure 4 yes Figure 3 The cross-sectional view of line VI-VI, Figure 5 is a schematic diagram of step S30 of the method of the present invention, Figure 6 is a schematic diagram of step S40 of the method of the present invention, Figure 7 is a schematic diagram of step S50 of the method of the present invention, Figure 8 is a schematic diagram of step S60 of the method of the present invention, Fig. 9 is a schematic diagram of step S70 of the method of the present invention, Fig.10 is a schematic diagram of step S80 of the method of the present invention, Fig.11 Schematic diagram of step S90 of the method of the present invention. The present invention provides a method for manufacturing a wave damper having a wide, thin and flat conductive structure, comprising the following steps:

[0102] Step S10, as Figure 1 and Figure 2 As shown, a metal layer 11 covers the outer surface of a core wire 12 to form a metal yarn 10. More specifically, the material of the core wire 12 may be non-conductive, lower in cost than the metal layer, and better in supporting the metal layer 11, such as cotton. The material of the metal layer 11 may be conductive, such as copper, aluminum, silver, other metals or alloys.

[0103] Step S20, as Figure 1 , Figure 3 and Figure 4 As shown, a plurality of first interlaced portions 13 of a plurality of metal yarns 10 are interlaced with a plurality of second interlaced portions 14 of the metal yarns 10 to weave a wide, thin and flat multifilament body 20; two ends of each first interlaced portion 13 are respectively connected to a second interlaced portion 14, the first interlaced portions 13 are parallel to each other, the second interlaced portions 14 are parallel to each other, and the first interlaced portions 13 and the second interlaced portions 14 extend in different directions. Preferably, the number of the metal yarns 10 is seven.

[0104] Step S30, as Figure 1 and Figure 5 As shown, a plurality of warp yarns 30 and two multifilament threads 20 are spaced apart on a loom (not shown), and the two ends of the warp yarns 30 and the multifilament threads 20 are fixed on the loom, so that the warp yarns 30 and the multifilament threads 20 extend in a straight line and are parallel to each other; and the distance D1 between each multifilament thread 20 and the warp yarns 30 on both sides thereof is greater than the distance D2 between the warp yarns 30.

[0105] Step S40, as Figure 1 and Figure 6As shown, a plurality of weft yarns 40 are interwoven between the warp yarns 30 and the multifilament yarns 20 by a loom to weave a substrate 50; and the weft yarns 40 define a first elastic adjustment region 61 between a first side 21 of each multifilament yarn 20 and the warp yarns 30 closest to the first side 21 of each multifilament yarn 20, and the weft yarns 40 define a second elastic adjustment region 62 between a second side 22 of each multifilament yarn 20 and the warp yarns 30 closest to the second side 22 of each multifilament yarn 20.

[0106] Step S50, as Figure 1 and Figure 7 As shown, the substrate 50 is immersed in a resin solution 71 in a resin tank 70, so that the multifilament yarns 20, the warp yarns 30 and the weft yarns 40 absorb and adhere to the resin.

[0107] Step S60, as Figure 1 and Figure 8 As shown, the temperature of a first baking plate 81 and a second baking plate 82 is used to remove moisture and volatile substances from the resin on the substrate 50 to dry the substrate 50; and the resin penetrates into the substrate 50 and adheres to the multifilament yarns 20, the warp yarns 30 and the weft yarns 40 to form a resin solid layer (not shown).

[0108] Step S70, as Figure 1 and Fig. 9 As shown, the substrate 50 is placed between a first mold 91 and a second mold 92, and the multifilament wire bodies 20 are aligned with the two grooves 911 of the first mold 91 and the two grooves 921 of the second mold 92; when the first mold 91 and the second mold 92 are molded together, a pressing surface 912 of the first mold 91 and a molding surface 922 of the second mold 92 are pressed together on the substrate 50 to form a plurality of wave portions 211 of a main body 210 of a wave spring 200 (see Fig.10 ) and a center hole pre-cut area 212, each wave portion 211 includes a wave crest 2111 and a wave valley 2112, and the multifilament wire bodies 20 are located in the grooves 911 of the first mold 91 and the grooves 921 of the second mold 92, and the pressing surface 912 and the forming surface 922 jointly press the multifilament wire bodies 20 to form two wide, thin and flat conductive structures 220 (see Fig.10 ); and a heating device (not shown) heats a first mold 91 and a second mold 92 to 190-270° C. The high temperature of the first mold 91 and the second mold 92 can soften the resin, which can not only break the resin but also fill the gaps with the resin, so that the various parts of the resin are connected to form the final shape of a resin solid layer to cover the surfaces of the warp yarns 30, the weft yarns 40 and the conductive structures 220 of the main body 210.

[0109] Step S80, as Figure 1 and Fig.10 As shown, a first cutter 110 and a second cutter 120 jointly separate the main body 210 from the substrate 50 , and at the same time, the first cutter 110 and the second cutter 120 jointly separate the conductive structures 220 from the multifilament wire bodies 20 .

[0110] Step S90, as Figure 1 and Fig.11 As shown, a welding tool 130 is used to solder two ends of the conductive structures 220 to form eight solder portions 230 .

[0111] Fig.12 FIG. 2 is a three-dimensional diagram of the wave damper 200 of the present invention. Fig.12 Please refer to Figures 2 to 11 The present invention provides a damper 200 having a wide, thin and flat conductive structure 220 , including a body 210 , four conductive structures 220 and eight solder portions 230 .

[0112] like Figure 6 As shown, the main body 210 is formed by interweaving a plurality of warp yarns 30 and a plurality of weft yarns 40 .

[0113] like Figure 6 As shown, each conductive structure 220 is wide, thin and flat, spaced apart from the warp yarns 30, extending in a straight line and parallel to each other, and interlaced with the weft yarns 40. Figure 3 and Figure 4 As shown, each conductive structure 220 is a multifilament body 20 that is wide, thin and flat, and the multifilament body 20 is formed by interweaving a plurality of first interwoven portions 13 of a plurality of metal yarns 10 and a plurality of second interwoven portions 14 of the metal yarns 10. Figure 2 As shown, each metal yarn 10 is formed by a metal layer 11 covering the outer surface of a core wire 12. Figure 3 and Figure 4 As shown, two ends of each first interlaced portion 13 are respectively connected to a second interlaced portion 14 , the first interlaced portions 13 are parallel to each other, the second interlaced portions 14 are parallel to each other, and the first interlaced portions 13 and the second interlaced portions 14 extend in different directions.

[0114] like Fig.12 As shown, the solder portions 230 are respectively formed by soldering at two ends of the conductive structures 220 .

[0115] Fig.13 is a three-dimensional diagram of the speaker 300 of the present invention, Fig.14 is an exploded view of the speaker 300 of the present invention, Fig.15 3 is a cross-sectional view of the speaker 300 of the present invention. Fig.13 , Fig.14 and Fig.15 As shown, the present invention provides a speaker 300, including a speaker body 310, a voice coil 320 and the above-mentioned damper 200. The speaker body 310 includes a base 311, a magnetic return device 312, an outer frame 313, a diaphragm 314, a dust cover 315, a suspension 316 and a plurality of connection terminals 317. The magnetic return device 312 is disposed on the base 311, the voice coil 320 is disposed in the magnetic return device 312 and has a coil 321, the outer frame 313 is disposed above the magnetic return device 312, the diaphragm 314 is sleeved on the voice coil 320, the dust cover 315 is disposed on a central hole of the diaphragm 314, the suspension 316 is disposed between the top edge of the diaphragm 314 and the outer frame 313, and each connection terminal 317 is disposed on the outer frame 313 and has a contact point. The damper 200 is sleeved on the voice coil 320. Two ends of the conductive structures 220 are respectively connected to the contact points of the connecting terminals 317 and the coil 321 of the voice coil 320 through the solder portions 230 .

[0116] In summary, the method of the present invention utilizes the weft yarns 40 to fix the multifilament thread bodies 20 , and does not require any stitches, thereby reducing the manufacturing steps and lowering the manufacturing cost of the elastic wave 200 .

[0117] Furthermore, the method of the present invention uses the weft yarns 40 to fix the multifilament wire bodies 20, so that the multifilament wire bodies 20 can be firmly fixed in the optimal position. During the hot pressing process, the multifilament wire bodies 20 are guaranteed not to deviate. After the multifilament wire bodies 20 are cut, the conductive structures 220 are guaranteed to be located in the optimal position, thereby improving the common resonance efficiency of the elastic wave 200, the voice coil 320 and the diaphragm 314, and the sound quality of each speaker 300 can be kept consistent.

[0118] In addition, because the conductive structures 220 are harder than the warp yarns 30 and the weft yarns 40, and the elasticity and toughness of the conductive structures 220 are worse than those of the warp yarns 30 and the weft yarns 40, the area through which the conductive structures 220 pass is harder than other areas of the body 210, and the elasticity and toughness of the area through which the conductive structures 220 pass are worse than other areas of the body 210. The damper 200 of the present invention can adjust the hardness, elasticity and toughness of the area through which the conductive structures 220 pass through the first elastic adjustment areas 61 and the second elastic adjustment areas 62, so that the area through which the conductive structures 220 pass becomes softer, more elastic and more tough, so that the hardness, elasticity and toughness of the area through which the conductive structures 220 pass are comparable to those of other areas of the body 210. Therefore, the damper 200 has uniform hardness, elasticity and toughness, uniform elastic recovery force and fatigue resistance, is not easy to deform and crack, and improves the sound quality output by the speaker 300.

[0119] In addition, the conductive structures 220 are wide, thin and flat, and based on the weaving method of the metal yarns 10, the top and bottom surfaces of the first interwoven portion 13 and the second interwoven portion 14 of each metal yarn 10 are exposed and will not be shielded by other metal yarns 10. The heat generated can be easily discharged without the problem of heat accumulation, and thus the conductive structures 220 will not overheat.

[0120] Furthermore, the conductive structures 220 are wide, thin and flat, and only slightly protrude from the surface of the body 210, so the risk of being crushed by the first mold 91 and the second mold 92 is low. For the sake of safety, the first mold 91 and the second mold 92 both form a plurality of grooves 911 and 921, which can protect the conductive structures 220 and ensure that the conductive structures 220 will not be crushed by the first mold 91 and the second mold 92. Since the conductive structures 220 only slightly protrude from the surface of the body 210, the depth of the grooves 911 and 921 does not need to be chiseled too deep, thereby reducing the manufacturing cost of the mold.

[0121] Furthermore, the solder portions 230 can not only prevent the ends of the conductive structures 220 from being separated, but can also be directly combined with the contact points of the connection terminals 317 and the coil 321 of the voice coil 320. Even after long-term use, the fixing effect of the solder portions 230 remains unchanged, and the ends of the conductive structures 220 will not be separated from the contact points of the connection terminals 317 and the coil 321 of the voice coil 320.

[0122] It is worth mentioning that the inner layer of each metal yarn 10 is a core wire 12, and the outer layer of each metal yarn 10 is a metal layer 11, which can not only reduce the cost but also maintain a certain electrical conductivity.

[0123] It is worth mentioning that, based on the weaving method of the metal yarns 10, only seven (the minimum number) of the metal yarns 10 are needed to weave a multifilament wire body 20 and cut into two conductive structures 220, so the manufacturing cost is relatively low.

[0124] The above description is only used to explain the preferred embodiments of the present invention, and is not intended to limit the present invention in any form. Therefore, any modifications or changes made to the present invention under the same inventive spirit should still be included in the scope of protection intended by the present invention.

Claims

1. A method for manufacturing a wave damper having a wide, thin and flat conductive structure, comprising the following steps: The metal layer covers the outer surface of a core wire to form a metal yarn; A plurality of first interlaced portions of a plurality of metal yarns are interlaced with a plurality of second interlaced portions of the metal yarns to weave a multifilament thread body that is wide, thin and flat; wherein, Two ends of each of the first interlaced parts are respectively connected to the second interlaced parts, the first interlaced parts are parallel to each other, the second interlaced parts are parallel to each other, and the first interlaced parts and the second interlaced parts extend in different directions; A plurality of warp yarns are arranged at intervals from at least one multifilament yarn body, and the warp yarns and the at least one multifilament yarn body extend in a straight line and are parallel to each other; interweaving a plurality of weft yarns between the warp yarns and the at least one multifilament yarn to weave a base material; The substrate is immersed in a resin solution; Drying the substrate; The main body of the elastic wave is formed by hot pressing on the substrate, and at least two wide, thin and flat conductive structures are formed by hot pressing on the at least one multifilament wire body; as well as The main body is separated from the substrate, and the at least two conductive structures are separated from the at least one multifilament wire body.

2. The method according to claim 1, wherein: The step of spacing the warp yarns from the at least one multifilament thread body further includes: the distance between the at least one multifilament thread body and the warp yarns on both sides thereof is greater than the distance between the warp yarns; wherein, the step of weaving the substrate further includes: the weft yarns define a first elastic adjustment area between the first side of the at least one multifilament thread body and the warp yarns closest to the first side of the at least one multifilament thread body, and the weft yarns define a second elastic adjustment area between the second side of the at least one multifilament thread body and the warp yarns closest to the second side of the at least one multifilament thread body, and the widths of the first elastic adjustment area and the second elastic adjustment area are equal.

3. The method according to claim 1, wherein: After the step of separating the body from the substrate, the method further includes: soldering two ends of the conductive structure to form at least four solder portions.

4. The method according to claim 1, wherein: The material of the core line is cotton.

5. The method according to claim 1, wherein: The number of the metal yarns is seven.

6. A wave damper having a wide, thin and flat conductive structure, comprising: The body is made of a plurality of warp yarns interwoven with a plurality of weft yarns; as well as At least two conductive structures, which are wide, thin and flat, are spaced apart from the warp yarns, extend straight and parallel to each other, and are interlaced with the weft yarns; Wherein, each of the conductive structures is a wide, thin and flat multifilament wire body, and the multifilament wire body is formed by interweaving a plurality of first interwoven portions of a plurality of metal yarns and a plurality of second interwoven portions of the metal yarns; Wherein, each of the metal yarns is formed by a metal layer covering the outer surface of a core wire; and The two ends of each of the first interlaced parts are respectively connected to the second interlaced parts, the first interlaced parts are parallel to each other, the second interlaced parts are parallel to each other, and the first interlaced parts and the second interlaced parts extend in different directions.

7. The wave damper according to claim 6, wherein: The distance between the at least one multifilament thread body and the warp yarns on both sides thereof is greater than the distance between the warp yarns. The weft yarn defines a first elastic adjustment area between the first side of the at least one multifilament thread body and the warp yarn closest to the first side of the at least one multifilament thread body. The weft yarn defines a second elastic adjustment area between the second side of the at least one multifilament thread body and the warp yarn closest to the second side of the at least one multifilament thread body. The widths of the first elastic adjustment area and the second elastic adjustment area are equal. 8 . The damper according to claim 6 , further comprising at least four solder portions, respectively formed by soldering at two ends of the conductive structure.

9. The wave damper according to claim 6, wherein: The material of the core line is cotton.