Equipment for continuously preparing silicon-carbon negative electrode material

By using continuous preparation equipment in lithium-ion batteries, the silane vacuum adsorption and pyrolytic deposition process is separated to form a silicon carbon negative electrode material, solving the problems of process stability and cycling performance, and achieving more efficient preparation of silicon carbon material.

CN119034609APending Publication Date: 2024-11-29吴泽俊 +3
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411188349.2
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The process stability of silicon carbon negative electrode materials in existing lithium-ion batteries is poor, resulting in material structure collapse, SEI film failure and cycle performance. It is mainly due to adsorption and pyrolysis deposition in the same fluidized bed, which affects the complexity of the process. degree and uniformity of silane distribution.

Method used

Using continuous preparation equipment, the silane gas is saturated and adsorbed under vacuum environment through a silane vacuum adsorption unit. The deposition device carries out pyrolytic deposition treatment, and forms a cladding layer in the carbon source coating device to separate the adsorption and deposition processes to ensure the silane gas pair. Full filling and stable deposition of carbon support.

Benefits of technology

The process stability is significantly improved, the "floating silicon" problem is avoided, the circulation performance and process complexity of silicon carbon anode materials are improved, and the effective control of silane adsorption and deposition amount is achieved.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119034609A_ABST
    Figure CN119034609A_ABST
Patent Text Reader

Abstract

The embodiment of the invention discloses equipment for continuously preparing a silicon-carbon negative electrode material, and the equipment comprises a silane vacuum adsorption unit which is used for enabling a carbon carrier to adsorb silane gas in a saturated manner in a vacuum environment to obtain a carbon material which adsorbs the silane gas in a saturated manner; the deposition device is connected with the silane vacuum adsorption unit and is used for carrying out pyrolytic deposition treatment on the carbon material to obtain a silicon-carbon composite material of silane cracked and deposited nano silicon; and the carbon source coating device is connected with the deposition device and is used for coating the surface of the silicon-carbon composite material with the carbon source gas to obtain the silicon-carbon negative electrode material. According to the embodiment of the invention, the carbon carrier is subjected to saturated adsorption in the silane vacuum adsorption unit in a vacuum environment, so that pores of the carbon carrier are fully filled with silane gas; the carbon material is placed in the deposition device to be subjected to pyrolytic deposition treatment, the adsorption process and the deposition process are carried out in two reaction containers, the problem that the process stability is poor due to the fact that the adsorption process and the deposition process are carried out in the same fluidized bed body is solved, the process complexity is reduced, and the phenomenon of floating silicon on the surface of a carbon carrier is effectively avoided; the expansion rate of the material in the lithium intercalation and deintercalation process is reduced, and the battery cycle performance is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of lithium ion battery negative electrode materials, and in particular to a device for continuously preparing silicon-carbon negative electrode materials. Background Art

[0002] In recent years, lithium-ion batteries have been widely used in portable electronic devices, large-scale energy storage equipment, electric vehicles and other fields. Compared with the graphite anode commonly used in lithium-ion batteries, silicon materials have ultra-high theoretical specific capacity and low lithium desorption potential, which makes silicon materials one of the most promising choices for upgrading the carbon-based anode of lithium-ion batteries. However, as a semiconductor material, silicon itself has low electrical conductivity. During the electrochemical cycle, the insertion and extraction of lithium ions will cause the volume of the material to expand and contract by more than 300%. The mechanical force generated will gradually pulverize the material, causing structural collapse, and eventually leading to the separation of the electrode active material from the current collector, loss of electrical contact, and greatly reduced battery cycle performance. In addition, due to this volume effect, it is difficult for silicon to form a stable solid electrolyte interface (SEI) film in the electrolyte. Along with the destruction of the electrode structure, a new SEI film is continuously formed on the exposed silicon surface, exacerbating the corrosion and capacity decay of silicon.

[0003] At present, most silicon-carbon negative electrode materials are prepared by using monosilane gas as a silicon source and porous carbon as a carrier. The porous carbon carrier is placed in a fluidized bed reaction unit, and then nitrogen is introduced into it to exclude oxygen. After the temperature is raised to a specified temperature, an appropriate amount of silane gas is introduced, and the porous carbon is fluidized by the introduced gas flow. During this process, the gas is adsorbed simultaneously. Due to the high activity of silane, the nano-silicon generated by the cracking and dehydrogenation of silane at this temperature is deposited in the porous carbon carrier.

[0004] However, in the existing scheme, since adsorption and cracking dehydrogenation are carried out in the same reaction unit, with the deposition of nano-silicon, the specific surface area of ​​the reaction product gradually decreases, the weight of the reaction product continues to increase, the powder state continues to change, and the fluidization state is affected, so it is necessary to adjust processes such as gas flow rate and the ratio of reaction gas to carrier gas to ensure sufficient fluidization, resulting in poor process stability. In addition, the existing scheme has air intake entering from the bottom of the fluidized bed and diffuses out after passing through a porous carbon bed with a certain thickness. Therefore, the silane concentration in contact with the bottom or lower part of the bed is always higher than that in the middle and upper part of the bed. The high concentration of silane in the middle and lower part exceeds the amount that can be adsorbed by the porous carbon micropores or mesopores, resulting in the inevitable deposition of silane on the porous carbon surface. The surface "floating silicon" lacks the rigid restraint of the porous inner wall, and in the later repeated charge and discharge and lithium insertion and extraction process, it is easy to cause the destruction of the surface carbon coating and SEI film, thereby significantly reducing the cycle performance. Summary of the invention

[0005] In view of at least some of the problems and shortcomings in the prior art, an embodiment of the present invention discloses a device for continuously preparing silicon-carbon negative electrode materials.

[0006] On the one hand, an embodiment of the present invention provides an apparatus for continuously preparing silicon-carbon negative electrode materials, for example, comprising: a silane vacuum adsorption unit, used to saturate a carbon carrier with silane gas under a vacuum environment to obtain a carbon material saturated with silane gas; a deposition device, connected to the silane vacuum adsorption unit, the deposition device being used to perform pyrolysis and deposition treatment on the carbon material saturated with silane gas to obtain a silicon-carbon composite material with nano-silicon deposited by silane decomposition; a carbon source coating device, connected to the deposition device, the carbon source coating device being used to coat the carbon source gas on the surface of the silicon-carbon composite material with nano-silicon deposited by silane decomposition to form a coating layer to obtain the silicon-carbon negative electrode material.

[0007] In the embodiment of the present invention, the carbon carrier is saturatedly adsorbed under a vacuum environment in a silane vacuum adsorption unit, thereby achieving sufficient filling of the pores of the carbon carrier with silane gas; the carbon material saturated with the silane gas is then placed in a deposition device for pyrolysis deposition treatment. Since the adsorption process and the deposition process are carried out in two reaction vessels, the problem of poor process stability caused by the adsorption treatment and the pyrolysis deposition treatment in the same fluidized bed body is avoided, thereby greatly reducing the complexity of the existing process.

[0008] In one embodiment of the present invention, the deposition device specifically includes: a silane pyrolysis unit, connected to the silane vacuum adsorption unit, the silane pyrolysis unit is used to heat the carbon material saturated with silane gas adsorption at a first temperature to obtain a first intermediate product; a silane cracking cooling unit, connected between the silane pyrolysis unit and the carbon source coating device, the silane cracking cooling unit is used to cool the first intermediate product to a second temperature to obtain the silicon-carbon composite material of the silane cracked and deposited nano-silicon; wherein the first temperature is 480-600°C, and the second temperature is less than or equal to 360°C.

[0009] In one embodiment of the present invention, the silane cracking cooling unit is also connected to the silane vacuum adsorption unit; the silane cracking cooling unit is also used for: when the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking reaches a first predetermined content, the silicon-carbon composite material of nano-silicon deposited by silane cracking is sent into the carbon source coating device; when the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking does not reach the first predetermined content, the silicon-carbon composite material of nano-silicon deposited by silane cracking is sent into the silane vacuum adsorption unit; wherein the first predetermined content is 45-60%.

[0010] In one embodiment of the present invention, the carbon source coating device specifically includes: an organic carbon source pyrolysis coating unit, connected to the silane cracking cooling unit, the organic carbon source pyrolysis coating unit is used to heat the silicon-carbon composite material of silane cracking and depositing nano-silicon at a third temperature under the protection of the inert atmosphere, and coat the carbon source gas on the surface of the silicon-carbon composite material of silane cracking and depositing nano-silicon, to obtain a second intermediate product; a cooling and discharging unit, connected to the organic carbon source pyrolysis coating unit, the cooling and discharging unit is used to cool the second intermediate product to a fourth temperature to obtain the silicon-carbon negative electrode material; wherein the third temperature is 500-750°C, and the fourth temperature is less than or equal to 50°C.

[0011] In one embodiment of the present invention, the silane vacuum adsorption unit includes: a first main body, the first main body has a first accommodating chamber, and the first main body is provided with a first silane input port and a first nitrogen input port; a first air pressure detection structure, which is arranged on the first main body and connected to the first accommodating chamber, and the first air pressure detection structure is used to measure the air pressure of the first accommodating chamber; a first oxygen content detection structure, which is arranged on the first main body and connected to the first accommodating chamber, and the first air pressure detection structure is used to measure the oxygen content of the first accommodating chamber.

[0012] In one embodiment of the present invention, the silane pyrolysis unit includes: a second body, the second body having a second accommodating chamber; a first heating structure, arranged on the first body, the first heating structure is used to heat the reactants in the second accommodating chamber; a second oxygen content detection structure, arranged on the second body and connected to the second accommodating chamber, the second air pressure detection structure is used to measure the oxygen content of the second accommodating chamber.

[0013] In one embodiment of the present invention, the silane cracking cold zone unit includes: a third main body, wherein the third main body has a third accommodating chamber; a first cooling structure, disposed on the third main body, the first cooling structure being used to cool the reactants in the third accommodating chamber; a third oxygen content detection structure, disposed on the third main body and connected to the third accommodating chamber, the third air pressure detection structure being used to measure the oxygen content of the third accommodating chamber.

[0014] In one embodiment of the present invention, the carbon source pyrolysis coating unit includes: a fourth main body, the fourth main body having a fourth accommodating chamber, and the fourth main body is provided with a fourth nitrogen inlet and a carbon source gas inlet; a second heating structure, arranged on the fourth main body, the second heating structure is used to heat the reactants in the fourth accommodating chamber; a fourth oxygen content detection structure, arranged on the fourth main body and connected to the fourth accommodating chamber, the fourth air pressure detection structure is used to measure the oxygen content of the fourth accommodating chamber.

[0015] In one embodiment of the present invention, it also includes a pipeline assembly, which includes: a first pipeline connected between the silane vacuum adsorption unit and the silane pyrolysis unit; a second pipeline connected between the silane pyrolysis unit and the silane cracking cooling unit; a third pipeline connected between the silane cracking cooling unit and the silane vacuum adsorption unit; a fourth pipeline connected between the silane cracking cooling unit and the carbon source pyrolysis coating unit; wherein the silane vacuum adsorption unit is provided with a first valve, the first valve is connected to the first pipeline and is used to control the opening and closing of the first pipeline; the silane pyrolysis unit includes a second valve, the second valve is connected to the second pipeline and is used to control the opening and closing of the second pipeline; the silane cracking cooling unit includes a third valve and a fourth valve, the third valve is connected to the third pipeline and is used to control the opening and closing of the third pipeline, and the fourth valve is connected to the fourth pipeline and is used to control the opening and closing of the fourth pipeline.

[0016] In one embodiment of the present invention, it also includes: a tail gas conveying unit, the deposition device, the silane vacuum adsorption unit and the carbon source coating device are respectively connected to the tail gas conveying unit, and the tail gas conveying unit is used to treat the tail gas in the deposition device, the silane vacuum adsorption unit and the carbon source coating device; and / or, a feed conveying unit, connected to the silane vacuum adsorption unit, the feed conveying unit is used to convey the carbon carrier to the silane vacuum adsorption unit; and / or, an exhaust unit, the deposition device, the silane vacuum adsorption unit and the carbon source coating device are respectively connected to the tail gas conveying unit, and the exhaust unit is used to vacuum the deposition device, the silane vacuum adsorption unit and the carbon source coating device.

[0017] It can be seen from the above that the above technical features of the present invention can have one or more of the following beneficial effects: the embodiment of the present invention performs saturated adsorption of the carbon carrier under a vacuum environment in a silane vacuum adsorption unit, thereby avoiding the need to introduce a large amount of nitrogen as a carrier gas in the mainstream process of using a fluidized bed, saving costs, and more importantly, achieving sufficient filling of the pores of the carbon carrier with silane gas; the carbon material saturated with silane gas is then placed in a deposition device for pyrolysis and deposition treatment. The adsorption process and the deposition process are carried out in two reaction vessels, thereby avoiding the problem of poor process stability caused by the currently commonly used adsorption and pyrolysis deposition treatments in the same fluidized bed, thereby greatly reducing the complexity of the existing process, and achieving effective control of the silane adsorption and deposition amounts through a circulation method, thereby avoiding the problem of "floating silicon" on the surface of the carbon carrier, and significantly improving the stability of the process. BRIEF DESCRIPTION OF THE DRAWINGS

[0018] In order to more clearly illustrate the technical solutions of the embodiments of the present invention, the accompanying drawings required for use in the description of the embodiments will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other accompanying drawings can be obtained based on these accompanying drawings without paying creative work.

[0019] Figure 1 A schematic diagram of the structure of an apparatus for continuously preparing silicon-carbon negative electrode materials provided in an embodiment of the present invention.

[0020] Figure 2 Another schematic diagram of the structure of the equipment for continuously preparing silicon-carbon negative electrode materials provided in an embodiment of the present invention.

[0021] Description of reference numerals:

[0022] 10-equipment for continuously preparing silicon-carbon negative electrode materials; 100-feeding and conveying unit; 110-carrier gas channel;

[0023] 200-silane vacuum adsorption unit; 201-first main body; 2011-first silane input port; 2012-first nitrogen input port; 203-first air pressure detection structure; 204-first oxygen content detection structure; 205-first valve;

[0024] 300-deposition device; 310-silane pyrolysis unit; 311-second body; 312-first heating structure; 314-second oxygen content detection structure; 315-second valve; 320-silane cracking cooling unit; 321-third body; 322-first cooling structure; 324-third oxygen content detection structure; 325-third valve; 326-fourth valve;

[0025] 400-carbon source coating device; 410-organic carbon source pyrolysis coating unit; 411-fourth main body; 4111-fourth nitrogen input port; 4112-carbon source gas input port; 412-second heating structure; 414-fourth oxygen content detection structure; 415-fifth valve; 420-cooling and discharging unit;

[0026] 500-pipeline assembly; 510-first pipe; 520-second pipe; 530-third pipe; 540-fourth pipe; 550-fifth pipe;

[0027] 600-exhaust gas delivery unit; 700-exhaust unit. DETAILED DESCRIPTION

[0028] In order to make the purpose, technical solution and advantages of the present invention clearer, the technical solution of the present invention will be clearly and completely described below in conjunction with the specific embodiments of the present invention and the corresponding drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0029] It should be noted that the terms "first", "second", etc. in the specification and claims of the present invention and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequence. It should be understood that the terms used in this way can be interchangeable where appropriate, so that the embodiments of the present invention described herein can be implemented in an order other than those illustrated or described herein. In addition, the terms "including" and "having" and any variations thereof are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device that includes a series of steps or units is not necessarily limited to those steps or units that are clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.

[0030] It should also be noted that the division of multiple embodiments in the present invention is only for the convenience of description and should not constitute a special limitation. The features in various embodiments can be combined and referenced to each other without contradiction.

[0031] See also Figure 1 , an embodiment of the present invention provides an apparatus 10 for continuously preparing silicon-carbon negative electrode materials, for example, including a silane vacuum adsorption unit 200, a deposition device 300 and a carbon source coating device 400. Among them, the silane vacuum adsorption unit 200 is, for example, arranged on one side of the deposition device 300 and connected to the deposition device 300, and the carbon source coating device 400 is, for example, arranged on the other side of the deposition device 300 and connected to the deposition device 300. The silane vacuum adsorption unit 200 is, for example, used to saturate the carbon carrier with silane gas under a vacuum environment to obtain a carbon material saturated with silane gas adsorption, the deposition device 300 is, for example, used to perform pyrolysis deposition treatment on the carbon material saturated with silane gas adsorption to obtain a silicon-carbon composite material with nano-silicon deposited by silane cracking, and the carbon source coating device 400 is, for example, used to coat the carbon source gas on the surface of the silicon-carbon composite material with nano-silicon deposited by silane cracking to form a coating layer to obtain the silicon-carbon negative electrode material.

[0032] For example, the carbon carrier can be placed in the silane vacuum adsorption unit 200 for saturated adsorption of silane gas to obtain a carbon material saturated with silane gas adsorption, and then the carbon material saturated with silane gas adsorption enters the deposition device 300 for pyrolysis deposition treatment to obtain a silicon-carbon composite material with silane cracking and depositing nano-silicon, and then the silicon-carbon composite material with silane cracking and depositing nano-silicon enters the carbon source coating device for carbon source gas coating to obtain a silicon-carbon negative electrode material.

[0033] For example, the carbon carrier mentioned above is a porous carbon material, and the silane gas mentioned above is monosilane gas. The pyrolysis deposition treatment mentioned above is a dehydrogenation cracking reaction of silane in the carbon material saturated with silane gas at high temperature, and the silane will dehydrogenate at high temperature to generate nano-silicon deposited in the pores of the carbon carrier to obtain a silicon-carbon composite material with cracked and deposited nano-silicon.

[0034] The embodiment of the present invention performs saturated adsorption of the carbon carrier in a vacuum environment in a silane vacuum adsorption unit, thereby avoiding the need to introduce a large amount of nitrogen as a carrier gas in the mainstream process of using a fluidized bed, saving costs, and more importantly, achieving sufficient filling of the pores of the carbon carrier with silane gas; then the carbon material saturated with silane gas is placed in a deposition device for pyrolysis and deposition treatment, and the adsorption process and the pyrolysis and deposition process are carried out in two reaction vessels, thereby avoiding the problem of poor process stability caused by the currently commonly used adsorption treatment and pyrolysis and deposition treatment in the same fluidized bed body, thereby greatly reducing the complexity of the existing process.

[0035] See also Figure 1 , the deposition device 300 specifically includes: a silane pyrolysis unit 310 and a silane cracking cooling unit 320, the silane vacuum adsorption unit 200 is, for example, disposed on the first side of the silane pyrolysis unit 310 and connected to the silane pyrolysis unit 310, and the silane cracking cooling unit 320 is, for example, disposed on the second side of the silane pyrolysis unit 310 and connected to the silane pyrolysis unit 310. The silane pyrolysis unit 310 is, for example, used to heat the carbon material saturated with silane gas adsorption at a first temperature to obtain a first intermediate product; the silane cracking cooling unit 320 is, for example, used to cool the first intermediate product to a second temperature to obtain the silicon-carbon composite material of the silane cracked and deposited nano-silicon. The first temperature is 480-600°C, and the second temperature is less than or equal to 360°C.

[0036] Based on the above, in a specific embodiment, the silane cracking cooling unit 320 is also connected to the silane vacuum adsorption unit 200, and the silane cracking cooling unit 320 is also used for: when the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking reaches a first predetermined content, the silicon-carbon composite material of nano-silicon deposited by silane cracking is sent to the carbon source coating device 400; when the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking does not reach the first predetermined content, the silicon-carbon composite material of nano-silicon deposited by silane cracking is sent to the silane vacuum adsorption unit 200; wherein the first predetermined content is 45-60%. For example, the user detects the silicon content of the silicon-carbon composite material of nano-silicon deposited by silane cracking in the silane cracking cooling unit 320. When the silicon content reaches 45-60%, the silicon-carbon composite material of nano-silicon deposited by silane cracking can enter the carbon source coating device 400 for subsequent carbon source coating treatment. When the silicon content does not reach 45-60%, the silicon-carbon composite material of nano-silicon deposited by silane cracking needs to enter the silane vacuum adsorption unit 200 to repeat the silane saturation adsorption and pyrolysis deposition treatment until the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking reaches 45-60%.

[0037] Further, see Figure 1 , the carbon source coating device 400 specifically includes: an organic carbon source pyrolysis coating unit 410 and a cooling and discharging unit 420. The silane cracking cooling unit 320 is, for example, disposed on the first side of the organic carbon source pyrolysis coating unit 410 and connected to the organic carbon source pyrolysis coating unit 410, and the cooling and discharging unit 420 is, for example, disposed on the second side of the organic carbon source pyrolysis coating unit 410 and connected to the organic carbon source pyrolysis coating unit 410. By disposing the silane vacuum adsorption unit 200 and the silane cracking cooling unit 320 on different sides of the silane pyrolysis unit 310, and the silane cracking cooling unit 320 and the cooling and discharging unit 420 on different sides of the organic carbon source pyrolysis coating unit 410, the silane vacuum adsorption unit 200, the silane pyrolysis unit 310, the silane cracking cooling unit 320, the organic carbon source pyrolysis coating unit 410 and the cooling and discharging unit 420 can form a complete production line, and facilitate the reasonable movement of the reactants on the production line.

[0038] According to the above, the organic carbon source pyrolysis coating unit 410 is used, for example, to heat the silicon-carbon composite material of nano-silicon deposited by silane cracking at a third temperature under the protection of the inert atmosphere, and to coat the carbon source gas on the surface of the silicon-carbon composite material of nano-silicon deposited by silane cracking, to obtain a second intermediate product. The cooling and discharging unit 420 is used, for example, to cool the second intermediate product to a fourth temperature to obtain the silicon-carbon negative electrode material. The third temperature is 500-750°C, and the fourth temperature is less than or equal to 50°C.

[0039] See also Figure 1 The device 10 for continuously preparing silicon-carbon negative electrode materials further includes, for example, a pipeline assembly 500, which includes, for example, a first pipeline 510, a second pipeline 520, a third pipeline 530, a fourth pipeline 540, and a fifth pipeline 550. The first pipeline 510 is, for example, connected between the silane vacuum adsorption unit 200 and the silane pyrolysis unit 310, the second pipeline 520 is, for example, connected between the silane pyrolysis unit 310 and the silane cracking cooling unit 320, the third pipeline 530 is, for example, connected between the silane cracking cooling unit 320 and the silane vacuum adsorption unit 200, the fourth pipeline 540 is, for example, connected between the silane cracking cooling unit 320 and the carbon source pyrolysis coating unit 410, and the fifth pipeline 550 is, for example, connected between the carbon source pyrolysis coating unit 410 and the cooling and discharging unit 420. The silane vacuum adsorption unit 200 is, for example, provided with a first valve 205, which is connected to the first pipeline 510 and is used to control the opening and closing of the first pipeline 510. The silane pyrolysis unit 310 includes a second valve 315, which is connected to the second pipeline 520 and is used to control the opening and closing of the second pipeline 520. The silane cracking and cooling unit 320 includes a third valve 325 and a fourth valve 326, the third valve 325 is connected to the third pipeline 530 and is used to control the opening and closing of the third pipeline 530, and the fourth valve 326 is connected to the fourth pipeline 540 and is used to control the opening and closing of the fourth pipeline 540. The carbon source pyrolysis and coating unit 410, for example, includes a fifth valve 415, which is connected to the fifth pipeline 550 and is used to control the opening and closing of the fifth pipeline 550.

[0040] Furthermore, see Figure 1, the equipment 10 for continuously preparing silicon-carbon negative electrode materials also includes, for example, a tail gas conveying unit 600, a feed conveying unit 100 and / or a gas extraction unit 700. Among them, the deposition device 300, the silane vacuum adsorption unit 200 and the carbon source coating device 500 are, for example, respectively connected to the tail gas conveying unit 600, and the tail gas conveying unit 600 is used to treat the tail gas in the deposition device 300, the silane vacuum adsorption unit 200 and the carbon source coating device 400. The feed conveying unit 100 is, for example, connected to the silane vacuum adsorption unit 200, and the feed conveying unit 100 is used to convey the carbon carrier to the silane vacuum adsorption unit 200. For example, the feed conveying unit 100 is, for example, connected to the third pipeline 530, and the carbon carrier is, for example, conveyed to the silane vacuum adsorption unit 200 through the third pipeline 530. Of course, the specific position setting of the feed conveying unit 100 can be changed according to actual conditions, and this application is not limited to this. The feed conveying unit 100 further includes a carrier channel 110, which is used to introduce carrier gas. The deposition device 300, the silane vacuum adsorption unit 200 and the carbon source coating device 500 are also connected to a vacuum unit 700, for example, respectively. The vacuum unit 700 is used to vacuumize the deposition device 300, the silane vacuum adsorption unit 200 and the carbon source coating device 400. For example, the vacuum unit 700 is a vacuum pump.

[0041] In a specific embodiment, see also Figure 2 , the silane vacuum adsorption unit 200 includes, for example, a first main body 201, a first air pressure detection structure 203 and a first oxygen content detection structure 204. The first main body 201 includes, for example, a first accommodating chamber, and the reactants react in the first accommodating chamber. The first main body 201 is also provided with, for example, a first silane input port 2011 and a first nitrogen input port 2012. The first air pressure detection structure 203 is, for example, disposed on the first main body 201 and connected to the first accommodating chamber. The first air pressure detection structure 203 is used to measure the air pressure of the first accommodating chamber. For example, the first air pressure detection structure 203 is, for example, an air pressure detector. The first oxygen content detection structure 204 is, for example, disposed on the first main body 201 and connected to the first accommodating chamber. The first oxygen content detection structure 204 is used to measure the oxygen content of the first accommodating chamber. For example, the first oxygen content detection structure 204 is, for example, an oxygen content detector.

[0042] As mentioned above, see Figure 2The silane pyrolysis unit 310 includes, for example, a second body 311, a first heating structure 312, and a second oxygen content detection structure 314. The second body 311 includes, for example, a second accommodating chamber, and the reactants react, for example, in the second accommodating chamber. The first heating structure 312 is, for example, disposed on the second body 311. The first heating structure 312 is used to heat the reactants in the second accommodating chamber. The first heating structure 312 is, for example, sleeved on the second body 311. For example, the first heating structure 312 is, for example, a heater. Of course, it can also be other structures that can be heated, and the present application does not limit this. The second oxygen content detection structure 314 is, for example, disposed on the second body 311 and connected to the second accommodating chamber. The second oxygen content detection structure 314 is used to measure the oxygen content of the second accommodating chamber. For example, the second oxygen content detection structure 314 is, for example, an oxygen content detector.

[0043] See also Figure 2 , the silane cracking cold zone unit 320, for example, includes a third main body 321, a first cooling structure 322 and a third oxygen content detection structure 324. Among them, the third main body 321, for example, has a third accommodating chamber, and the reactant, for example, reacts in the third accommodating chamber. The first cooling structure 322, for example, is arranged on the third main body 321, and the first cooling structure 322 is used to cool the reactant in the third accommodating chamber. The first cooling structure 322, for example, is sleeved on the third main body 311, and the first cooling structure 322, for example, contains a coolant. For example, the first cooling structure 322 is, for example, a cooler, and of course, it can also be other structures that can be cooled, and the present application does not limit this. The third oxygen content detection structure 324, for example, is arranged on the third main body 321 and is connected to the third accommodating chamber. The third air pressure detection structure is used to measure the oxygen content of the third accommodating chamber. For example, the third oxygen content detection structure 324 is, for example, an oxygen content detector.

[0044] In addition, see Figure 2, the carbon source pyrolysis coating unit 410, for example, includes a fourth main body 411, a second heating structure 412 and a fourth oxygen content detection structure 414. The fourth main body 411 has a fourth accommodating chamber, and the reactants react, for example, in the fourth accommodating chamber. The fourth main body 411 is provided with a fourth nitrogen inlet 4111 and a carbon source gas inlet 4112. The second heating structure 412 is provided on the fourth main body 411, and the second heating structure 412 is used to heat the reactants in the fourth accommodating chamber. For example, the second heating structure 412 is, for example, a heater, and of course, it can also be other structures that can be heated, and the present application does not limit this. The fourth oxygen content detection structure 414 is provided on the fourth main body 411 and is connected to the fourth accommodating chamber. The fourth air pressure detection structure 414 is used to measure the oxygen content of the fourth accommodating chamber. For example, the fourth oxygen content detection structure 414 is, for example, an oxygen content detector.

[0045] For example, the production process of preparing silicon-carbon negative electrode materials using the equipment 10 for continuously preparing silicon-carbon negative electrode materials is briefly described below.

[0046] S1) After adding the carbon carrier to the feed conveying unit 100, the carrier gas channel 110 is opened, so that the carbon carrier is transported to the first accommodation chamber of the silane vacuum adsorption unit 200 with nitrogen as the carrier gas. After the vacuum unit 700 is opened to evacuate the first accommodation chamber to the first vacuum degree, the first nitrogen input port 2012 is opened to introduce nitrogen to the first air pressure. The first oxygen content detection structure 204 is used to detect whether the oxygen content in the first accommodation chamber reaches the predetermined oxygen content. If not, the above operation is repeated until the predetermined oxygen content is reached. If reached, the vacuum is evacuated to the second vacuum degree through the vacuum unit 700, and then the first silane input port 2011 is opened to introduce silane gas to the first air pressure. Among them, the first vacuum degree is 100Pa, the second vacuum degree is 10Pa, and the first air pressure is 10 5 Pa, the predetermined oxygen content is 20ppm.

[0047] S2) While executing S1), the silane pyrolysis unit 310 is subjected to oxygen removal treatment and the oxygen content is controlled to be less than 20ppm, and the temperature is heated to the corresponding reaction temperature of 480-600°C. Then the first valve 205 of the silane vacuum adsorption unit 200 is opened, and the carbon material saturated with silane gas adsorption enters the second accommodating chamber of the silane pyrolysis unit 310 through the first pipe 510 by its own gravity. Under the heating of the first heating structure 312, the carbon material saturated with silane gas adsorption is evenly heated so that the silane is pyrolyzed to form ultrafine nano-silicon deposited in the porous carbon pores to obtain the first intermediate product. A small amount of overflowed silane and dust mixed in the nitrogen protective gas are treated by the tail gas treatment unit 600.

[0048] S3) While executing S1), the silane cracking cold zone unit 320 is subjected to oxygen removal treatment and the oxygen content is controlled to be less than 20ppm. Then the second valve 315 of the silane pyrolysis unit 310 is opened, and the first intermediate product enters the third containing chamber of the silane cracking cold zone unit 320 through the second pipe 520 by its own gravity. When the temperature of the silane cracking cold zone unit 320 is lower than 360°C, the first intermediate product is cooled in the silane cracking cold zone unit 320 to obtain a silicon-carbon composite material of cracked and deposited nano-silicon. The silicon content in the silicon-carbon composite material of cracked and deposited nano-silicon is detected. If the silicon content does not reach 45-60%, the third valve 325 of the silane cracking cold zone unit 320 is opened to allow the silicon-carbon composite material of cracked and deposited nano-silicon to enter the silane vacuum adsorption unit 200 through the third pipe 530. Repeat the above steps until the silicon content in the silicon-carbon composite material of cracked and deposited nano-silicon in the silane cracking cold zone unit 320 reaches 45-60%. The dust mixed in the nitrogen protective gas is treated by the tail gas treatment unit 600 .

[0049] S4) While executing S1), the carbon source pyrolysis coating unit 410 is subjected to oxygen removal treatment and the oxygen content is controlled to be less than 20ppm, and the temperature is heated to the corresponding reaction temperature of 500-750°C. Then the fourth valve 326 of the silane cracking cold zone unit 320 and the fourth nitrogen inlet 4111 of the carbon source pyrolysis coating unit 410 are opened, and the silicon-carbon composite material of the cracked and deposited nano-silicon enters the fourth accommodating chamber of the carbon source pyrolysis coating unit 410 through the fourth pipeline 540 under the protection of nitrogen by its own gravity. The carbon source gas inlet 4112 is opened, and one or more of acetylene, propylene, and methane are used as carbon source gas. The carbon source gas is thermally cracked into carbon atoms and hydrogen atoms, and the carbon atoms are deposited and coated on the outer surface of the silicon-carbon composite material of the cracked and deposited nano-silicon to complete the coating treatment to obtain the second intermediate product. The undecomposed acetylene and the dust mixed in the nitrogen protective gas are treated by the tail gas treatment unit 600.

[0050] S5) While executing S4), the cooling and discharging unit 420 is subjected to oxygen removal treatment and the oxygen content is controlled to be less than 20 ppm. Then the fifth valve 415 of the carbon source pyrolysis and coating unit 410 is opened, and the second intermediate product enters the cooling and discharging unit 420 through the fifth pipeline 550 by its own gravity, and the second intermediate product is cooled to less than 50° C. to obtain a silicon-carbon negative electrode material.

[0051] The embodiment of the present invention performs saturated adsorption of the carbon carrier under a vacuum environment in a silane vacuum adsorption unit, thereby achieving sufficient filling of the pores of the carbon carrier with silane gas; then the carbon material saturated with silane gas is placed in a deposition device for pyrolysis deposition treatment. Since the adsorption process and the deposition process are carried out in two reaction vessels, the problem of poor process stability caused by the adsorption and pyrolysis deposition treatments in the same fluidized bed is avoided, thereby greatly reducing the complexity of the existing process. The effective control of the silane adsorption and deposition amounts is achieved in a circulating manner, thereby avoiding the problem of "floating silicon" on the surface of the carbon carrier, and significantly improving the stability of the process.

[0052] It can be understood that the aforementioned embodiments are merely exemplary descriptions of the present invention. The technical solutions of the various embodiments can be arbitrarily combined and used in combination, provided that the technical features do not conflict, the structures do not contradict, and the purpose of the present invention is not violated.

[0053] Finally, it should be noted that the above embodiments are only used to illustrate the technical solutions of the present invention, rather than to limit it. Although the present invention has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that they can still modify the technical solutions described in the aforementioned embodiments, or make equivalent replacements for some of the technical features therein. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the embodiments of the present invention.

Claims

1. A device for continuously preparing silicon-carbon negative electrode materials, characterized in that: include: A silane vacuum adsorption unit is used to saturate the carbon carrier with silane gas under a vacuum environment to obtain a carbon material saturated with silane gas; A deposition device connected to the silane vacuum adsorption unit, the deposition device is used to perform a pyrolysis deposition process on the carbon material saturated with silane gas adsorption to obtain a silicon-carbon composite material with nano-silicon deposited by silane decomposition; A carbon source coating device is connected to the deposition device and is used to coat the carbon source gas on the surface of the silicon-carbon composite material deposited by silane cracking and nano-silicon to form a coating layer to obtain the silicon-carbon negative electrode material.

2. The device for continuously preparing silicon-carbon negative electrode materials according to claim 1, characterized in that: The deposition device specifically comprises: A silane pyrolysis unit connected to the silane vacuum adsorption unit, the silane pyrolysis unit is used to heat the carbon material saturated with silane gas at a first temperature to obtain a first intermediate product; A silane cracking cooling unit is connected between the silane pyrolysis unit and the carbon source coating device, and is used to cool the first intermediate product to a second temperature to obtain the silicon-carbon composite material of the silane cracking deposited nano-silicon; Wherein, the first temperature is 480-600°C, and the second temperature is less than or equal to 360°C.

3. The device for continuously preparing silicon-carbon negative electrode materials according to claim 2, characterized in that: The silane cracking and cooling unit is also connected to the silane vacuum adsorption unit; The silane cracking cooling unit is also used for: when the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking reaches a first predetermined content, sending the silicon-carbon composite material of nano-silicon deposited by silane cracking into the carbon source coating device; when the silicon content in the silicon-carbon composite material of nano-silicon deposited by silane cracking does not reach the first predetermined content, sending the silicon-carbon composite material of nano-silicon deposited by silane cracking into the silane vacuum adsorption unit; wherein the first predetermined content is 45-60%.

4. The device for continuously preparing silicon-carbon negative electrode materials according to claim 3, characterized in that: The carbon source coating device specifically comprises: An organic carbon source pyrolysis and coating unit is connected to the silane cracking and cooling unit, and is used to heat the silicon-carbon composite material of nano-silicon deposited by silane cracking at a third temperature under the protection of the inert atmosphere, and coat the carbon source gas on the surface of the silicon-carbon composite material of nano-silicon deposited by silane cracking, to obtain a second intermediate product; A cooling and discharging unit connected to the organic carbon source pyrolysis and coating unit, the cooling and discharging unit is used to cool the second intermediate product to a fourth temperature to obtain the silicon-carbon negative electrode material; Wherein, the third temperature is 500-750°C, and the fourth temperature is less than or equal to 50°C.

5. The device for continuously preparing silicon-carbon negative electrode materials according to claim 4, characterized in that: The silane vacuum adsorption unit comprises: A first main body, wherein the first main body has a first accommodating cavity, and the first main body is provided with a first silane input port and a first nitrogen input port; a first air pressure detection structure, disposed on the first main body and connected to the first accommodating cavity, the first air pressure detection structure being used to measure the air pressure of the first accommodating cavity; The first oxygen content detection structure is disposed on the first main body and communicated with the first accommodating chamber. The first air pressure detection structure is used to measure the oxygen content of the first accommodating chamber.

6. The device for continuously preparing silicon-carbon negative electrode materials according to claim 4, characterized in that: The silane pyrolysis unit comprises: A second body, wherein the second body has a second accommodating cavity; A first heating structure is disposed on the first main body, and the first heating structure is used to heat the reactant in the second accommodating chamber; The second oxygen content detection structure is disposed on the second main body and communicated with the second accommodating chamber. The second air pressure detection structure is used to measure the oxygen content of the second accommodating chamber.

7. The device for continuously preparing silicon-carbon negative electrode materials according to claim 4, characterized in that: The silane cracking cold zone unit comprises: A third body, wherein the third body has a third accommodating cavity; A first cooling structure is provided on the third main body, and the first cooling structure is used to cool the reactants in the third accommodating chamber; The third oxygen content detection structure is disposed on the third main body and communicated with the third accommodating chamber. The third air pressure detection structure is used to measure the oxygen content of the third accommodating chamber.

8. The device for continuously preparing silicon-carbon negative electrode materials according to claim 4, characterized in that: The carbon source pyrolysis coating unit comprises: A fourth main body, wherein the fourth main body has a fourth accommodating cavity, and the fourth main body is provided with a fourth nitrogen gas input port and a carbon source gas input port; A second heating structure is disposed on the fourth main body, and the second heating structure is used to heat the reactant in the fourth accommodating chamber; The fourth oxygen content detection structure is disposed on the fourth main body and communicated with the fourth accommodating chamber. The fourth air pressure detection structure is used to measure the oxygen content of the fourth accommodating chamber.

9. The device for continuously preparing silicon-carbon negative electrode materials according to any one of claims 4 to 8, characterized in that: Also included is a pipeline assembly, the pipeline assembly comprising: A first pipeline connected between the silane vacuum adsorption unit and the silane pyrolysis unit; a second pipeline connected between the silane pyrolysis unit and the silane cracking and cooling unit; A third pipeline is connected between the silane cracking and cooling unit and the silane vacuum adsorption unit; a fourth pipeline connected between the silane cracking and cooling unit and the carbon source pyrolysis and coating unit; Among them, the silane vacuum adsorption unit is provided with a first valve, which is connected to the first pipeline and is used to control the opening and closing of the first pipeline; the silane pyrolysis unit includes a second valve, which is connected to the second pipeline and is used to control the opening and closing of the second pipeline; the silane cracking and cooling unit includes a third valve and a fourth valve, the third valve is connected to the third pipeline and is used to control the opening and closing of the third pipeline, and the fourth valve is connected to the fourth pipeline and is used to control the opening and closing of the fourth pipeline.

10. The device for continuously preparing silicon-carbon negative electrode materials according to claim 9, characterized in that: Also includes: A tail gas delivery unit, the deposition device, the silane vacuum adsorption unit and the carbon source coating device are respectively connected to the tail gas delivery unit, and the tail gas delivery unit is used to process the tail gas in the deposition device, the silane vacuum adsorption unit and the carbon source coating device; and / or, a feed conveying unit connected to the silane vacuum adsorption unit, the feed conveying unit being used to convey the carbon carrier to the silane vacuum adsorption unit; and / or, The vacuum unit, the deposition device, the silane vacuum adsorption unit and the carbon source coating device are respectively connected to the tail gas delivery unit, and the vacuum unit is used to vacuum the deposition device, the silane vacuum adsorption unit and the carbon source coating device.