Semiconductor structure and forming method thereof
By setting an isolation structure in the epitaxial layer of the semiconductor structure, the problems of parasitic capacitance effect and high manufacturing cost are solved, and the effects of reducing parasitic capacitance and increasing frequency are achieved.
Patent Information
- Application Number
- CN202411148016.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-20
- Publication Date
- 2024-11-29
AI Technical Summary
While increasing the operating frequency, the existing semiconductor structures are difficult to effectively reduce the parasitic capacitance effect, and the manufacturing process is complex and costly.
By providing an isolation structure in the epitaxial layer above the substrate, the isolation structure is flush with the epitaxial layer away from the substrate surface, and the orthogonal projection of the gate structure over the epitaxial layer covers the isolation structure, thereby reducing the Parasitic capacitance effect.
It realizes the reduction of the parasitic capacitance effect within the semiconductor structure, simplifies the manufacturing process, reduces the manufacturing cost, and improves the switching ratio and response speed.
Smart Images

Figure CN119050140A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the technical field of integrated circuit manufacturing, and in particular to a semiconductor structure and a forming method thereof. Background Art
[0002] Semiconductor structures with power electronic devices are developing in the direction of high power, high frequency and integration. In the 1980s, the current capacity of thyristors reached 6000 amperes and the blocking voltage was as high as 6500 volts. However, the operating frequency of such devices is relatively low. Increasing its operating frequency depends on how to accelerate the recombination rate of minority carriers in the base region (hereinafter referred to as minority carriers) during the device shutdown period and extract more carriers through the gate. Although reducing the minority carrier lifetime can effectively shorten the process of turning off the current, it leads to an increase in the forward voltage drop of the device during the conduction period. Therefore, the requirements of conversion speed and device on-state power loss must be taken into account. In order to increase the operating frequency of power devices, reducing parasitic capacitance is an effective means. However, the current method of reducing the parasitic capacitance between the gate and the drain in the transistor is relatively complicated and costly, and the effect of reducing parasitic capacitance is not significant.
[0003] Therefore, how to effectively reduce the parasitic capacitance effect in the semiconductor structure while simplifying the manufacturing process of the semiconductor structure and reducing the manufacturing cost of the semiconductor structure is a technical problem that needs to be solved urgently. Summary of the invention
[0004] The present invention provides a semiconductor structure and a method for forming the same, which are used to simplify the manufacturing process of the semiconductor structure and reduce the manufacturing cost of the semiconductor structure while effectively reducing the parasitic capacitance effect in the semiconductor structure.
[0005] According to some embodiments, the present invention provides a semiconductor structure, comprising:
[0006] A substrate, wherein the substrate includes first doping ions, and the substrate includes a front side and a back side that are relatively distributed;
[0007] an epitaxial layer, located on the front side of the substrate, wherein the epitaxial layer includes the first doping ions;
[0008] A gate structure, located on a surface of the epitaxial layer facing away from the substrate;
[0009] a drain electrode, located on the back side of the substrate;
[0010] An isolation structure is located in the epitaxial layer, a surface of the isolation structure facing away from the substrate is flush with a surface of the epitaxial layer facing away from the substrate, and an orthographic projection of the gate structure on the epitaxial layer covers the isolation structure.
[0011] In some embodiments, it also includes:
[0012] a well region located in the epitaxial layer, wherein the well region includes second doping ions, the conductivity type of the second doping ions is opposite to the conductivity type of the first doping ions, and the two well regions are distributed along a first direction on opposite sides of the orthographic projection of the gate structure on the epitaxial layer, and the first direction is parallel to the front surface of the substrate;
[0013] The source region is located in the well region, and there is a gap between the isolation structure and the well region.
[0014] In some embodiments, a depth of the isolation structure along a second direction is less than a depth of the well region along the second direction, and the second direction is perpendicular to the front surface of the substrate.
[0015] In some embodiments, the isolation structure comprises:
[0016] An isolation trench extending from a surface of the epitaxial layer away from the substrate toward an interior of the substrate;
[0017] The insulating layer completely fills the isolation groove.
[0018] In some embodiments, the insulating layer is made of silicon oxide, silicon nitride, or a combination of the two.
[0019] In some embodiments, the isolation structures are distributed symmetrically about a center of an orthographic projection of the gate structure on the epitaxial layer.
[0020] In some embodiments, the width of the isolation structure is smaller than the width of the gate structure.
[0021] In some embodiments, the width of the isolation structure is greater than 20 nm, and the width of the isolation structure is less than 2 / 3 of the width of the gate structure.
[0022] According to some other embodiments, the present invention further provides a method for forming a semiconductor structure, comprising the following steps:
[0023] Providing a substrate, wherein the substrate includes first doping ions, and the substrate includes a front side and a back side that are relatively distributed;
[0024] forming an epitaxial layer on the front surface of the substrate, wherein the epitaxial layer includes the first doping ions;
[0025] forming an isolation structure in the epitaxial layer, wherein a surface of the isolation structure facing away from the substrate is flush with a surface of the epitaxial layer facing away from the substrate;
[0026] forming a gate structure on a surface of the epitaxial layer facing away from the substrate, wherein an orthographic projection of the gate structure on the epitaxial layer covers the isolation structure;
[0027] A drain electrode is formed covering the back side of the substrate.
[0028] In some embodiments, before forming the isolation structure in the epitaxial layer, the following steps are further included:
[0029] Two well regions spaced apart along a first direction and a source region located in each of the well regions are formed in the epitaxial layer, the well regions include second doped ions, the conductivity type of the second doped ions is opposite to the conductivity type of the first doped ions, and the first direction is parallel to the front side of the substrate.
[0030] In some embodiments, the specific steps of forming an isolation structure in the epitaxial layer include:
[0031] Etching the epitaxial layer between the two well regions to form an isolation trench, wherein a gap is provided between the isolation trench and the well region;
[0032] An insulating layer is formed to fill the isolation trench, and the isolation trench and the insulating layer together serve as the isolation structure.
[0033] In some embodiments, the insulating layer is made of silicon oxide, silicon nitride, or a combination of the two.
[0034] In some embodiments, the specific steps of etching the epitaxial layer between the two well regions to form an isolation trench include:
[0035] defining a gate region on the epitaxial layer;
[0036] The epitaxial layer between the two well regions is etched by a dry etching process to form the isolation grooves which are symmetrically distributed about the center of the gate region.
[0037] In some embodiments, the width of the isolation trench is greater than 20 nm, and the width of the isolation trench is less than 2 / 3 of the width of the gate region.
[0038] The semiconductor structure and the method for forming the same provided by the present invention provide an isolation structure in the epitaxial layer above the substrate, wherein the surface of the isolation structure facing away from the substrate is flush with the surface of the epitaxial layer facing away from the substrate, and the positive projection of the gate structure located above the epitaxial layer on the epitaxial layer covers the isolation structure, thereby reducing the area facing each other between the gate structure and the epitaxial layer, reducing the parasitic capacitance effect between the gate electrode (i.e., the gate conductive layer) and the drain electrode in the semiconductor structure, and increasing the switching ratio and response speed of the semiconductor structure. Moreover, the present invention only needs to provide an isolation structure in the epitaxial layer, which is simple to operate and has low cost, and helps to improve the manufacturing efficiency of the semiconductor structure. BRIEF DESCRIPTION OF THE DRAWINGS
[0039] Figure 1 is a schematic cross-sectional view of a semiconductor structure in a specific embodiment of the present invention;
[0040] Figure 2 is a flow chart of a method for forming a semiconductor structure in a specific embodiment of the present invention;
[0041] Figure 3 is a schematic cross-sectional view after forming a well region and a source region in a specific embodiment of the present invention;
[0042] Figure 4 is a schematic cross-sectional view after an isolation structure is formed in a specific embodiment of the present invention;
[0043] Figure 5 is a schematic cross-sectional view after the gate electrode is deposited in a specific embodiment of the present invention;
[0044] Figure 6 It is a schematic cross-sectional view after a gate structure is formed in a specific embodiment of the present invention. DETAILED DESCRIPTION
[0045] The specific implementation manner of the semiconductor structure and the method for forming the same provided by the present invention will be described in detail below with reference to the accompanying drawings.
[0046] This specific embodiment provides a semiconductor structure, Figure 1 Schematic diagram of a cross-sectional view of a semiconductor structure in a specific embodiment of the present invention. Figure 1 As shown, the semiconductor structure comprises:
[0047] A substrate 10, wherein the substrate 10 includes first doping ions, and the substrate 10 includes a front side and a back side that are relatively distributed;
[0048] An epitaxial layer 11, located on the front surface of the substrate 10, wherein the epitaxial layer 11 includes the first doping ions;
[0049] A gate structure, located on a surface of the epitaxial layer 11 facing away from the substrate 10;
[0050] A drain electrode 17, located on the back side of the substrate 10;
[0051] The isolation structure 12 is located in the epitaxial layer 11 . The surface of the isolation structure 12 facing away from the substrate 10 is flush with the surface of the epitaxial layer 11 facing away from the substrate 10 , and the orthographic projection of the gate structure on the epitaxial layer 11 covers the isolation structure 12 .
[0052] Specifically, the semiconductor structure may be, but is not limited to, an IGBT. The substrate 10 may be a silicon substrate or a silicon carbide substrate. Since the silicon carbide substrate has the advantages of high hardness, high mechanical strength, stable chemical properties, etc., this specific embodiment takes the substrate 10 as a silicon carbide substrate as an example for explanation. In one example, the substrate 10 is heavily doped with N-type ions (that is, the first doped ions are N-type ions). The epitaxial layer 11 made of silicon carbide is epitaxially grown on the front surface of the substrate 10, and the epitaxial layer 11 is also doped with N-type ions, and the doping concentration of the N-type ions in the epitaxial layer 11 is less than the doping concentration of the N-type ions in the substrate 10. The gate structure includes a gate dielectric layer 13 located on the surface of the epitaxial layer 11 away from the substrate 10 and a gate conductive layer 14 covering the gate dielectric layer 13. In one example, the material of the gate dielectric layer 13 includes an oxide material (e.g., silicon dioxide), and the material of the gate conductive layer 14 includes a polysilicon material. The drain electrode 17 is a metal electrode, and the drain electrode 17 covers the back side of the substrate 10. The isolation structure 12 is in the epitaxial layer 11, and the surface of the isolation structure 12 facing away from the substrate 10 is flush with the surface of the epitaxial layer 11 facing away from the substrate 10, that is, the top surface of the isolation structure 12 is exposed to the top surface of the epitaxial layer 11. The orthographic projection of the gate structure on the epitaxial layer 11 covers the isolation structure 12, which means that the orthographic projection of the gate structure on the top surface of the epitaxial layer 11 at least partially overlaps with the isolation structure 12. In one example, the orthographic projection of the gate structure on the top surface of the epitaxial layer 11 completely covers the isolation structure 12.
[0053] In this specific embodiment, the isolation structure is arranged in the epitaxial layer 11, and the orthographic projection of the gate structure on the epitaxial layer 11 covers the isolation structure 12, thereby reducing the area of the gate structure facing the epitaxial layer, at least increasing the distance between part of the gate conductive layer 14 and the epitaxial layer 11, and thus reducing the parasitic capacitance effect between the gate electrode and the drain electrode in the semiconductor structure. Moreover, in this specific embodiment, only the isolation structure 12 needs to be arranged in the epitaxial layer 11, which is simple to operate and low in cost, and helps to improve the manufacturing efficiency of the semiconductor structure.
[0054] In some embodiments, the semiconductor structure further comprises:
[0055] A well region 15, located in the epitaxial layer 11, the well region 15 includes second doping ions, the conductivity type of the second doping ions is opposite to the conductivity type of the first doping ions, and the two well regions 15 are distributed along a first direction D1 on opposite sides of the orthographic projection of the gate structure on the epitaxial layer 11, and the first direction D1 is parallel to the front surface of the substrate 10;
[0056] The source region 16 is located in the well region 15 , and there is a gap between the isolation structure 12 and the well region 15 .
[0057] For example, the epitaxial layer 11 has two well regions 15 arranged at intervals along the first direction D1, each well region 15 has a source region 16, the depth of the source region 16 along the second direction D2 is less than the depth of the well region 15 along the second direction D2, and the projection of the gate structure on the top surface of the epitaxial layer 11 is located between the two well regions 15. The second direction D2 is perpendicular to the front side of the substrate 10. In one example, the well region 15 is doped with P-type ions (that is, the second doped ions are P-type ions), and the source region 16 is doped with N-type ions. The semiconductor structure also includes a source electrode ( Figure 1 ). In one example, the source electrode 16 is a metal electrode. The larger the capacitance between the gate structure and the source region 16, the stronger the control capability of the well region 15, thereby making the power consumption of the semiconductor structure lower. The gate structure is the main position for controlling the well region 15 near the source region 16, while the middle position of the gate structure has almost no effect on the on and off of the well region 15. Therefore, a gap is provided between the isolation structure 12 and the well region 15 (that is, the isolation structure 12 is not in contact with the contact 15), so as to reduce the parasitic capacitance effect between the gate conductive layer 14 and the drain electrode 17, and reduce the influence on the capacitance effect between the gate structure and the source region 16, thereby reducing the power consumption of the semiconductor structure while increasing the switching ratio of the semiconductor structure, and improving the response speed and device frequency of the semiconductor structure.
[0058] In some embodiments, a depth of the isolation structure 12 along the second direction D2 is less than a depth of the well region 15 along the second direction D2 , and the second direction D2 is perpendicular to the front surface of the substrate 10 .
[0059] Specifically, the depth of the isolation structure 12 along the second direction D2 is less than the depth of the well region 15 along the second direction D2, thereby avoiding excessive resistance of the epitaxial layer 11 and improving the performance of the semiconductor structure. In one example, the depth of the isolation structure 12 along the second direction D2 is less than or equal to 2 / 3 of the depth of the well region 15 along the second direction D2.
[0060] In some embodiments, the isolation structure 12 includes:
[0061] An isolation trench extending from a surface of the epitaxial layer 11 away from the substrate 10 toward the interior of the substrate 10;
[0062] The insulating layer completely fills the isolation groove.
[0063] In some embodiments, the insulating layer is made of silicon oxide, silicon nitride, or a combination of the two.
[0064] In this specific implementation, the isolation groove is formed by etching the epitaxial layer 11, and the isolation structure 12 is formed by filling the isolation groove with the insulating layer. Not only is the process simple, but it is also convenient to flexibly adjust the depth and position of the isolation structure 12 as needed, thereby improving the flexibility of the semiconductor structure manufacturing. In one example, the cross-sectional shape of the isolation groove can be rectangular or arc-shaped.
[0065] In some embodiments, the isolation structure 12 is distributed symmetrically about the center of the orthographic projection of the gate structure on the epitaxial layer 11 .
[0066] Specifically, since the two well regions 15 are distributed on opposite sides of the gate structure along the first direction D1, the isolation structure 12 is symmetrically distributed about the center of the positive projection of the gate structure on the epitaxial layer 11, which helps to improve the uniformity of the current in the semiconductor structure. At the same time, since the distance between the center position of the gate structure and the drain electrode 17 has the greatest influence on the parasitic capacitance effect between the gate structure and the drain electrode 17, the isolation structure 12 is symmetrically distributed about the center of the positive projection of the gate structure on the epitaxial layer 11, so that the parasitic capacitance between the gate structure and the drain electrode 17 can be further reduced, thereby further increasing the switching ratio of the semiconductor structure.
[0067] In some embodiments, the width of the isolation structure 12 is smaller than the width of the gate structure.
[0068] In some embodiments, the width of the isolation structure 12 is greater than 20 nm, and the width of the isolation structure 12 is less than 2 / 3 of the width of the gate structure.
[0069] For example, the width of the isolation structure 12 along the first direction D1 is greater than 20 nm, so that it is convenient to form the isolation groove by etching process, and it is convenient to deposit the insulating layer filling the isolation groove by deposition process (such as chemical vapor deposition process). The width of the isolation structure along the first direction D1 is less than 2 / 3 of the width of the gate structure along the first direction D1, so as to avoid causing the resistance of the epitaxial layer 11 to be too large, so as to achieve a balance between the resistance of the epitaxial layer 11 and the gate-drain capacitance (i.e., the parasitic capacitance between the gate structure and the drain electrode 17).
[0070] This specific embodiment also provides a method for forming a semiconductor structure. Figure 2 is a flow chart of a method for forming a semiconductor structure in a specific embodiment of the present invention. The schematic diagram of the semiconductor structure formed in this specific embodiment can be found in Figure 1 .like Figure 1 and Figure 2 As shown, the method for forming the semiconductor structure comprises the following steps:
[0071] Step S21, providing a substrate 10, wherein the substrate 10 includes first doping ions, and the substrate 10 includes a front side and a back side that are relatively distributed;
[0072] Step S22, forming an epitaxial layer 11 on the front surface of the substrate 10, wherein the epitaxial layer 11 includes the first doping ions;
[0073] Step S23, forming an isolation structure 12 in the epitaxial layer 11, wherein a surface of the isolation structure 12 facing away from the substrate 10 is flush with a surface of the epitaxial layer 11 facing away from the substrate 10;
[0074] Step S24, forming a gate structure on a surface of the epitaxial layer 11 facing away from the substrate 10, wherein the orthographic projection of the gate structure on the epitaxial layer 11 covers the isolation structure 12;
[0075] Step S25 , forming a drain electrode 17 covering the back side of the substrate 10 .
[0076] Figure 3 1 is a schematic cross-sectional view of a specific embodiment of the present invention after forming a well region and a source region. In some embodiments, before forming the isolation structure 12 in the epitaxial layer 11, the following steps are also included:
[0077] Two well regions 15 arranged in a first direction D1 and a source region 16 located in each well region 15 are formed in the epitaxial layer 11, wherein the well region 15 includes second doping ions, and the conductivity type of the second doping ions is opposite to the conductivity type of the first doping ions. The first direction D1 is parallel to the front side of the substrate 10. Figure 3 shown.
[0078] For example, the substrate 10 made of silicon carbide is heavily doped with N-type ions (i.e., the first doped ions are N-type ions). The epitaxial layer 11 made of silicon carbide is epitaxially grown on the front surface of the substrate 10, and the epitaxial layer 11 is also doped with N-type ions, and the doping concentration of the N-type ions in the epitaxial layer 11 is less than the doping concentration of the N-type ions in the substrate 10. After forming the epitaxial layer 11, the well region 15 is formed by injecting P-type ions into the epitaxial layer 11. The source region 16 is formed by injecting N-type ions into the epitaxial layer 11.
[0079] Figure 4 2 is a schematic cross-sectional view of a specific embodiment of the present invention after forming an isolation structure. In some embodiments, the specific steps of forming the isolation structure in the epitaxial layer include:
[0080] Etching the epitaxial layer 11 between the two well regions 15 to form an isolation trench 121, with a gap between the isolation trench 121 and the well region 15;
[0081] An insulating layer 122 is formed to fill the isolation trench 121. The isolation trench 121 and the insulating layer 122 together serve as the isolation structure 12. Figure 1 and Figure 4 shown.
[0082] In some embodiments, the material of the insulating layer 122 is silicon oxide, silicon nitride, or a combination of the two.
[0083] In some embodiments, the specific steps of etching the epitaxial layer 11 between the two well regions 15 to form the isolation trench 121 include:
[0084] defining a gate region on the epitaxial layer 11;
[0085] The epitaxial layer 11 between the two well regions 15 is etched by dry etching process to form the isolation grooves 121 which are symmetrically distributed about the center of the gate region.
[0086] In some embodiments, the width of the isolation trench 121 is greater than 20 nm, and the width of the isolation trench 121 is less than 2 / 3 of the width of the gate region.
[0087] For example, after forming the well region 15 and the source region 16, the gate region is defined in the epitaxial layer 11, and the gate region is located between the two well regions 15 arranged at intervals along the first direction D1. The epitaxial layer 11 between the two well regions 15 is etched using a dry etching process to form the isolation groove 121 that is symmetrically distributed about the center of the gate region. The etching parameters of the dry etching process are adjusted so that the width of the isolation groove 121 is greater than 20 nm, and the width of the isolation groove 121 is less than 2 / 3 of the width of the gate region. Thereafter, a chemical vapor deposition process is used to deposit silicon oxide or silicon nitride material in the isolation groove 121 to form the insulating layer 122 that fills the isolation groove 121. The isolation groove 121 and the insulating layer 122 together serve as the isolation structure 12, such as Figure 1 and Figure 4 shown.
[0088] Figure 5 is a schematic cross-sectional view after the gate electrode is deposited in a specific embodiment of the present invention, Figure 6 1 is a schematic cross-sectional view of a gate structure after being formed in a specific embodiment of the present invention. For example, after forming the isolation structure 12, a gate dielectric layer 13 covering the top surface of the epitaxial layer 11 (i.e., the surface of the epitaxial layer 11 facing away from the substrate 10) and a gate conductive layer 14 covering the gate dielectric layer 13 are formed. Figure 5 The gate dielectric layer 13 and the gate conductive layer 14 outside the gate region are removed, and the remaining gate dielectric layer 13 and the gate conductive layer 14 above the gate region serve together as the gate structure, as shown in FIG. Figure 6 Afterwards, a metal material is deposited on the back side of the substrate 10 to form the drain electrode 17, as shown in FIG. Figure 1 shown.
[0089] The semiconductor structure and its formation method provided in this specific embodiment are provided by setting an isolation structure in the epitaxial layer above the substrate, wherein the surface of the isolation structure facing away from the substrate is flush with the surface of the epitaxial layer facing away from the substrate, and the positive projection of the gate structure located above the epitaxial layer on the epitaxial layer covers the isolation structure, thereby reducing the area facing each other between the gate structure and the epitaxial layer, reducing the parasitic capacitance effect between the gate electrode (i.e., the gate conductive layer) and the drain electrode in the semiconductor structure, and increasing the switching ratio and response speed of the semiconductor structure. Moreover, this specific embodiment only needs to set the isolation structure in the epitaxial layer, which is simple to operate and low in cost, and helps to improve the manufacturing efficiency of the semiconductor structure.
[0090] The above is only a preferred embodiment of the present invention. It should be pointed out that ordinary technicians in this technical field can make several improvements and modifications without departing from the principle of the present invention. These improvements and modifications should also be regarded as the scope of protection of the present invention.
Claims
1. A semiconductor structure, It is characterized in that include: A substrate, wherein the substrate includes first doping ions, and the substrate includes a front side and a back side that are relatively distributed; an epitaxial layer, located on the front side of the substrate, wherein the epitaxial layer includes the first doping ions; A gate structure, located on a surface of the epitaxial layer facing away from the substrate; a drain electrode, located on the back side of the substrate; An isolation structure is located in the epitaxial layer, a surface of the isolation structure facing away from the substrate is flush with a surface of the epitaxial layer facing away from the substrate, and an orthographic projection of the gate structure on the epitaxial layer covers the isolation structure.
2. The semiconductor structure according to claim 1, It is characterized in that Also includes: a well region located in the epitaxial layer, wherein the well region includes second doping ions, the conductivity type of the second doping ions is opposite to the conductivity type of the first doping ions, and the two well regions are distributed along a first direction on opposite sides of the orthographic projection of the gate structure on the epitaxial layer, and the first direction is parallel to the front surface of the substrate; The source region is located in the well region, and there is a gap between the isolation structure and the well region.
3. The semiconductor structure according to claim 2, It is characterized in that A depth of the isolation structure along a second direction is smaller than a depth of the well region along the second direction, and the second direction is perpendicular to the front surface of the substrate.
4. The semiconductor structure according to claim 2, It is characterized in that The isolation structure comprises: An isolation trench extending from a surface of the epitaxial layer away from the substrate toward an interior of the substrate; The insulating layer completely fills the isolation groove.
5. The semiconductor structure according to claim 4, It is characterized in that The material of the insulating layer is any one of silicon oxide and silicon nitride, or a combination of the two.
6. The semiconductor structure according to claim 1, It is characterized in that The isolation structures are distributed symmetrically about a center of an orthographic projection of the gate structure on the epitaxial layer.
7. The semiconductor structure according to claim 1, It is characterized in that The width of the isolation structure is smaller than the width of the gate structure.
8. The semiconductor structure according to claim 7, It is characterized in that The width of the isolation structure is greater than 20 nm, and the width of the isolation structure is less than 2 / 3 of the width of the gate structure.
9. A method for forming a semiconductor structure, It is characterized in that The steps include: Providing a substrate, wherein the substrate includes first doping ions, and the substrate includes a front side and a back side that are relatively distributed; forming an epitaxial layer on the front surface of the substrate, wherein the epitaxial layer includes the first doping ions; forming an isolation structure in the epitaxial layer, wherein a surface of the isolation structure facing away from the substrate is flush with a surface of the epitaxial layer facing away from the substrate; forming a gate structure on a surface of the epitaxial layer facing away from the substrate, wherein an orthographic projection of the gate structure on the epitaxial layer covers the isolation structure; A drain electrode is formed covering the back side of the substrate.
10. The method for forming a semiconductor structure according to claim 9, It is characterized in that Before forming the isolation structure in the epitaxial layer, the method further includes the following steps: Two well regions spaced apart along a first direction and a source region located in each of the well regions are formed in the epitaxial layer, the well regions include second doped ions, the conductivity type of the second doped ions is opposite to the conductivity type of the first doped ions, and the first direction is parallel to the front side of the substrate.
11. The method for forming a semiconductor structure according to claim 9, It is characterized in that The specific steps of forming an isolation structure in the epitaxial layer include: Etching the epitaxial layer between the two well regions to form an isolation trench, wherein a gap is provided between the isolation trench and the well region; An insulating layer is formed to fill the isolation trench, and the isolation trench and the insulating layer together serve as the isolation structure.
12. The method for forming a semiconductor structure according to claim 11, It is characterized in that The material of the insulating layer is any one of silicon oxide and silicon nitride, or a combination of the two.
13. The method for forming a semiconductor structure according to claim 11, It is characterized in that The specific steps of etching the epitaxial layer between the two well regions to form an isolation trench include: defining a gate region on the epitaxial layer; The epitaxial layer between the two well regions is etched by a dry etching process to form the isolation grooves which are symmetrically distributed about the center of the gate region.
14. The method for forming a semiconductor structure according to claim 13, It is characterized in that The width of the isolation trench is greater than 20 nm, and the width of the isolation trench is less than 2 / 3 of the width of the gate region.