Method for producing 1, 1, 1, 3, 5, 5, 5-heptafluoro-2-pentene
Through the effects of halogenated metal catalysts and activated carbon catalysts, the problem of HFO-1447 in the prior art is solved, and the manufacturing of high-purity HFO-1447 is achieved, the generation of by-products is avoided, and the resin deterioration is inhibited, and the resin is expanded. Scope of application of resin.
Patent Information
- Application Number
- CN202380035214.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-28
- Filing Date
- 2023-04-27
- Publication Date
- 2024-11-29
AI Technical Summary
The prior art is difficult to efficiently manufacture high-purity 1,1,1,3,5,5-heptafluoro-2-pentene (HFO-1447) and contains by-product propidene compounds and unreacted HFC- 458, resulting in resin deterioration.
3-chloro-hexafluoro-2-pentene reacts with hydrogen fluoride to form 3-chloro-1,1,1,3,5,5,5-heptafluoropentane in the presence of a halide metal catalyst and in activated carbon The hydrogen chloride reaction was carried out under the catalyst to produce high-purity HFO-1447.
High-efficiency manufacturing of high-purity HFO-1447 is achieved, the generation of by-products is avoided, the deterioration of the resin is suppressed, and the scope of application of the resin is expanded.
Smart Images

Figure BDA0005093265400000021 
Figure BDA0005093265400000091 
Figure BDA0005093265400000101
Abstract
Description
Technical Field
[0001] The present invention relates to a novel method for producing 1,1,1,3,5,5,5-heptafluoro-2-pentene (hereinafter sometimes referred to as "HFO-1447"), and in particular to a method for producing high-purity 1,1,1,3,5,5,5-heptafluoro-2-pentene. Background Art
[0002] Fluoroolefins are used as solvents, detergents, foaming agents, and intermediates for functional materials, and various production methods have been proposed. In particular, 1,1,1,3,5,5,5-heptafluoro-2-pentene has a C=C double bond and a fluorine substituent in the molecule, which are the starting points of the reaction, and is useful as a synthetic intermediate. In addition, 1,1,1,3,5,5,5-heptafluoro-2-pentene has no chlorine atoms in the molecule, so the ozone depletion potential is 0. Since it has a C=C double bond in the molecule, it decomposes into low molecular weight compounds even if it is released into the natural world. Since it has 7 fluorine atoms in the molecule, it is non-flammable and is a liquid at normal temperature and pressure. Therefore, it is also useful as a foaming agent. For example, in Example 5 of Patent Document 1, as shown in the following reaction formula, 1,1,1,3,3,5,5,5-octafluoropentane (hereinafter sometimes referred to as "HFC-458") is used as a raw material, and high surface AlF3 is used as a catalyst to carry out a dehydrofluorination reaction at a temperature of 330° C. to produce HFO-1447. Furthermore, Example 6 of Patent Document 1 describes the use of HFO-1447 in a blowing agent composition, and Example 7 describes the use of a mixed solvent containing HFO-1447 as a main component as a desiccant. However, the present inventors conducted additional tests on Patent Document 1 and found that bis(trifluoromethyl)propadiene (hereinafter sometimes referred to as "propadiene compound") not described in Patent Document 1 is produced as a by-product and is difficult to separate from (E)-HFO-1447 (boiling point: 52°C), and unreacted HFC-458 is difficult to separate from (Z)-HFO-1447 (boiling point: 78°C), and the yield is low when high-purity HFO-1447 is to be produced. In addition, according to the research of the present inventors, it is known that (E)-HFO-1447 containing propadiene compounds and (Z)-HFO-1447 containing HFC-458 are more likely to deteriorate the resin than high-purity (E)-HFO-1447 and (Z)-HFO-1447.
[0003]
[0004] Prior art literature
[0005] Patent Literature
[0006] Patent Document 1: Japanese Patent Application No. 2012-508778 Summary of the invention
[0007] Problem that the invention aims to solve
[0008] The present invention aims to provide a novel method for producing 1,1,1,3,5,5,5-heptafluoro-2-pentene (hereinafter sometimes referred to as "HFO-1447"), and in particular to provide a method for producing high-purity (especially purity exceeding 99%) HFO-1447. Another object of the present invention is to provide high-purity HFO-1447 and its use.
[0009] Solutions for solving problems
[0010] The present invention provides the following solutions. [1]
[0012] A method for producing 1,1,1,3,5,5,5-heptafluoro-2-pentene, comprising:
[0013] (a) reacting 3-chloro-hexafluoro-2-pentene with hydrogen fluoride in the presence of a metal halogenide catalyst at a temperature exceeding -10°C and not more than 20°C to produce 3-chloro-1,1,1,3,5,5,5-heptafluoropentane, and
[0014] (b) Dehydrochlorinating the 3-chloro-1,1,1,3,5,5,5-heptafluoropentane obtained in (a) in the presence of an activated carbon catalyst to produce 1,1,1,3,5,5,5-heptafluoro-2-pentene. [2]
[0016] The method according to [1], wherein the metal halide catalyst is selected from antimony halide catalysts, tin halide catalysts, titanium halide catalysts, niobium halide catalysts, tantalum halide catalysts or combinations thereof. [3]
[0018] The method according to [1], wherein the halogenated metal catalyst is selected from antimony trichloride, antimony pentachloride, antimony trifluoride, antimony pentafluoride, tin tetrachloride, titanium tetrachloride, niobium pentafluoride, tantalum pentafluoride or a combination thereof. [4]
[0020] The method according to [1], wherein hydrogen fluoride is used in a molar equivalent ratio of 1 to 1.5 to 3-chloro-hexafluoro-2-pentene. [5]
[0022] The method according to [1], wherein the amount of the metal halogenide catalyst is 2 to 3 mol % based on 3-chloro-hexafluoro-2-pentene. [6]
[0024] The method according to [1], wherein the reaction in step (a) is carried out at a temperature of -5°C to 10°C. [7]
[0026] The method according to [1], wherein the metal halogenide catalyst is selected from antimony trichloride, antimony pentachloride, antimony trifluoride, antimony pentafluoride, tin tetrachloride, titanium tetrachloride, niobium pentafluoride, tantalum pentafluoride or a combination thereof, hydrogen fluoride is used in a 1 to 1.5 molar equivalent ratio relative to 3-chloro-hexafluoro-2-pentene, the amount of the metal halogenide catalyst is 2 to 3 mol% relative to 3-chloro-hexafluoro-2-pentene, and the reaction of step (a) is carried out at a temperature of -5°C to 10°C. [8]
[0028] High-purity 1,1,1,3,5,5,5-heptafluoro-2-pentene obtained by the method described in any one of [1] to [7]. [9]
[0030] The high-purity 1,1,1,3,5,5,5-heptafluoro-2-pentene according to [8] has a purity exceeding 99%.
[0031] Effects of the Invention
[0032] The present inventors have found that high-purity HFO-1447 can be efficiently obtained by changing the production method. According to the present invention, since allene compounds and HFC-458 are not generated or mixed, high-purity HFO-1447, especially HFO-1447 with a purity exceeding 99%, can be efficiently produced. In the case of HFO-1447 containing impurities produced by other production methods, resin degradation occurs, but in the case of the high-purity HFO-1447 of the present invention, resin degradation is suppressed, and the range of applicable resins is expanded. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 This is a schematic diagram of a reaction apparatus used for the dehydrochlorination reaction in step (b). DETAILED DESCRIPTION
[0034] [effect]
[0035] According to the present invention, 1,1,1,3,5,5,5-heptafluoro-2-pentene (HFO-1447) with high purity, especially purity exceeding 99%, can be efficiently produced. According to the research of the present inventors, HFO-1447 obtained by the method proposed in the prior art document (Patent Document 1) contains a raw material (HFC-458) and a product (propadiene compound) which are difficult to separate from HFO-1447 by purification, and high-purity HFO-1447 cannot be obtained efficiently. The present inventors have found that: (a) 3-chloro-1,1,1,5,5,5-hexafluoro-2-pentene (hereinafter sometimes referred to as "HCFO-1446"), which is easily available and easily separated from products, is reacted with hydrogen fluoride in the presence of a halogenated metal catalyst at a temperature of more than -10°C and less than 20°C to produce 3-chloro-1,1,1,3,5,5,5-heptafluoropentane (hereinafter sometimes referred to as "HCFC-457"), and (b) the obtained 3-chloro-1,1,1,3,5,5,5-heptafluoropentane is subjected to a dehydrochlorination reaction in the presence of an activated carbon catalyst to produce HFO-1447, thereby obtaining HFO-1447 that does not contain a propadiene compound. Since the HFO-1447 obtained by the method of the present invention does not contain raw materials or products that are difficult to separate, it is possible to efficiently obtain high-purity HFO-1447 that cannot be achieved in the prior art. Therefore, the high-purity HFO-1447 of the present invention is itself a new invention.
[0036] According to the research of the present inventors, it is also known that (E)-HFO-1447 containing a propadiene compound and (Z)-HFO-1447 containing HFC-458 are likely to degrade resins. Since the high-purity (E)-HFO-1447 and (Z)-HFO-1447 obtained by the method of the present invention do not contain propadiene compounds contained in HFO-1447 obtained by the method of the prior art, they are useful for all applications where resin deterioration is a problem.
[0037] [(a) Process]
[0038] In step (a), 3-chloro-hexafluoro-2-pentene is reacted with hydrogen fluoride in the presence of a halogenated metal catalyst at a temperature of more than -10°C and less than 20°C to produce 3-chloro-1,1,1,3,5,5,5-heptafluoropentane. In step (a), it is characterized in that a fluorination reaction is carried out in a specific temperature range using a specific raw material in the presence of a specific catalyst. In step (a), since only one molecule of hydrogen fluoride (HF) is added to the raw material, there is almost no by-product, and the target product is obtained selectively.
[0039] 3-Chloro-hexafluoro-2-pentene as a production raw material can be easily produced by a known method or can be easily obtained as a reagent.
[0040] As the halogenated metal catalyst, for example, antimony halide catalyst, tin halide catalyst, titanium halide catalyst, niobium halide catalyst, tantalum halide catalyst, etc. can be cited, and they can be used alone or in combination of two or more. As the antimony halide catalyst, for example, antimony trichloride, antimony pentachloride, antimony trifluoride, antimony pentafluoride, etc. can be cited, as the tin halide catalyst, for example, tin tetrachloride, etc. can be cited, as the titanium halide catalyst, for example, titanium tetrachloride, etc. can be cited, as the niobium halide catalyst, for example, niobium pentafluoride, etc. can be cited, as the tantalum halide catalyst, for example, tantalum pentafluoride, etc. can be cited, and they can be used alone or in combination of two or more.
[0041] The hydrogen fluoride is preferably used in an amount of 0.5 to 10 molar equivalents, more preferably 0.5 to 3 molar equivalents, and most preferably 1 to 1.5 molar equivalents relative to 3-chloro-hexafluoro-2-pentene.
[0042] The amount of the metal halide catalyst is preferably 0.1 to 10 mol%, more preferably 0.5 to 5 mol%, and most preferably 2 to 3 mol%, based on 100 mol% of 3-chloro-hexafluoro-2-pentene.
[0043] The reaction temperature is higher than -10°C and 20°C or lower, more preferably -10°C to 15°C, and most preferably -5°C to 10°C.
[0044] In the liquid phase reaction, hydrogen fluoride can be liquefied and used as a solvent. Since the boiling point of hydrogen fluoride is about 20°C, the reaction is liquid phase within the temperature range of step (a). Therefore, as long as the temperature is adequately controlled, the reaction can be carried out without using a pressure-resistant container such as an autoclave.
[0045] [(b) Step]
[0046] In step (b), 3-chloro-1,1,1,3,5,5,5-heptafluoropentane obtained in step (a) is subjected to a dehydrochlorination reaction in the presence of an activated carbon catalyst to produce HFO-1447. In this dehydrochlorination reaction, only one hydrogen chloride molecule is removed, so the product is only a mixture of E / Z isomers of HFO-1447.
[0047] As an activated carbon catalyst, it can be an activated carbon catalyst commonly used in the dehydrochlorination reaction of halogenated alkanes, for example, coconut shell charcoal for gas purification, catalyst and catalyst carrier (granular Egret GX, SX, CX, XRC manufactured by Takeda Pharmaceutical Industries, PCB manufactured by Toyo Calgon, YASHIKORU, Kuraray coal GG, GC manufactured by Taihei Chemical Industry Co., Ltd.), etc., which can be used alone or in combination of two or more. Activated carbon can also be used as a carrier, so the shape of the activated carbon catalyst itself can be made into a desired shape without supporting the activated carbon on other carriers. As the shape of the carrier, for example, powder, granular, spherical, pelletized, cylindrical, honeycomb and other shapes can be cited.
[0048] The contact time with the catalyst is usually 0.1 to 300 seconds, preferably 5 to 120 seconds, and more preferably 10 to 60 seconds, but is not limited thereto and may be appropriately changed.
[0049] The reaction temperature is preferably 150°C to 350°C, more preferably 200°C to 300°C, most preferably 220°C to 250°C.
[0050] [Carrier gas]
[0051] When implementing the present invention, a carrier gas is used in the dilution of the raw material gas, the drying of the reactor, etc. In particular, the raw materials, reaction products and other substances can be adjusted in concentration by circulating the carrier gas and moved in the reaction device. The carrier gas is selected to be a gas that does not react with these substances. For example, nitrogen, rare gases (helium, neon, argon, etc.) and the like can be cited. When a carrier gas is used, the carrier gas is usually mixed and used in a ratio of 0 to 99%, more preferably 0 to 75%, and most preferably 0 to 50% relative to the total flow rate of the raw materials, reaction products and other substances.
[0052] [Reaction device]
[0053] Examples of the material of the reaction device include corrosion-resistant metals such as stainless steel, Inconel, monel, hastelloy, and nickel. Among these, nickel is preferred from the viewpoint of corrosion resistance.
[0054] As an apparatus for carrying out the dehydrochlorination reaction of step (b), for example, an apparatus having the following structure can be cited: a cylindrical tube equipped with a heater for adjusting the reaction temperature is filled with catalysts of various shapes, and the raw gas is caused to flow from one end of the tube to the other end. As for the direction in which the raw gas flows, when the cylindrical tube filled with the catalyst is extended in the vertical direction, the raw gas can flow little by little by gravity, so it is preferred to flow little by little uniformly from top to bottom. When the cylindrical tube is extended in the vertical direction and the raw gas flows from bottom to top, it is desirable to arrange a granular catalyst with a large particle size at the lower part of the cylindrical tube and a powdered catalyst with a small particle size at the upper part of the cylindrical tube from the aspect of reaction efficiency.
[0055] In the description of a specific example of an apparatus for carrying out the dehydrochlorination reaction in step (b), Figure 1 In the apparatus, the apparatus comprises a raw material storage tank 1 containing 3-chloro-1,1,1,3,5,5,5-heptachloropentane, a nitrogen bottle 2 for supplying nitrogen to an evaporator 4, a cylindrical catalyst tower 3 connected by a pipe and vertically erected by the raw material storage tank, the evaporator 4 arranged just in front of the catalyst tower, and a collection tank 5 located downstream of the catalyst tower. 3-Chloro-1,1,1,3,5,5,5-heptachloropentane (boiling point 89° C.) is injected into the evaporator 4 heated to a temperature above the boiling point in a liquid state by an injection pump (not shown), and is vaporized in the evaporator 4. The raw material gas is mixed with a carrier gas (nitrogen) in the evaporator 4, and the mixed gas contacts the catalyst while moving from the top to the bottom of the catalyst tower, thereby promoting the dehydrochlorination reaction. The reaction gas passing through the bottom of the catalyst tower passes through the collection tank filled with water, and the reaction product, unreacted raw material and hydrogen chloride are collected in the collection tank, and only the carrier gas is discharged to the outside of the reaction apparatus.
[0056] [Purification of HFO-1447]
[0057] The high-purity HFO-1447 of the present invention can be obtained by distilling and purifying the reaction liquid after the step (b).
[0058] [High purity HFO-1447]
[0059] The high-purity HFO-1447 obtained by the method of the present invention is characterized in that there are two isomers, the (E)-isomer and the (Z)-isomer, and the purity of each is more than 99%, preferably 99.5% or more, and more preferably 99.9% or more. It should be noted that in this specification, unless otherwise specified, "%" is a weight-based ratio when the total weight is set to 100%.
[0060] [Application of the high-purity HFO-1447 of the present invention]
[0061] The high-purity HFO-1447 of the present invention has low solubility in organic substances, particularly very low solubility in oils, but is compatible with organic solvents such as ethanol and 2-propanol. This property is useful in the following applications.
[0062] (1) Use as solvent and detergent
[0063] The high-purity HFO-1447 of the present invention can be mixed with organic solvents such as ketones such as acetone and acetophenone, nitriles such as acetonitrile and propionitrile, ethers such as diisopropyl ether, tert-butyl methyl ether, tetrahydrofuran, diglyme, 1,4-dioxane, sulfoxides such as dimethyl sulfoxide and cyclopentane, amides such as dimethylformamide, dimethylacetamide, N-methylpyrrolidone, hydrocarbons such as hexane, heptane, cyclohexane, benzene, toluene, and alcohols such as methanol, ethanol, and isopropanol in any proportion. Therefore, it can be used as a mixed solvent for a wide range of purposes. The boiling points of the high-purity HFO-1447 of the present invention are (E)-body: 52°C, (Z)-body: 78°C. Therefore, it can be easily volatilized and removed. Since the high-purity HFO-1447 of the present invention does not contain allene compounds as impurities, as verified in the examples described below, it will not solidify the resin when used.
[0064] More specific examples of its use as a detergent include the following three.
[0065] (i) Particle cleaning
[0066] Cleaning fluid used to remove fine particles from the surface of precision electronic components, etc.
[0067] (ii) Co-solvent Cleaning
[0068] Cleaning fluid used for cleaning liquid crystal boxes and panels, degreasing and drying of processed parts.
[0069] (iii) Cleaning for water removal and drying
[0070] Cleaning fluid for dehydrating and drying lenses, sensor packages, semiconductor wafers, and other precision parts.
[0071] The high-purity HFO-1447 of the present invention has low surface tension (E body: 16.6mN / m; Z body: 18.9mN / m), high specific gravity (E body: 1.41g / cm 3 ; Z body: 1.44g / cm 3), and is easy to dry. Therefore, it is suitable for particle cleaning. In addition, the high-purity HFO-1447 of the present invention has low surface tension, low boiling point (E body: 52°C; Z body: 78°C), and non-flammability. Therefore, it is also suitable for co-solvent cleaning. In addition, the high-purity HFO-1447 of the present invention has low latent heat of evaporation (anti-condensation), non-flammability, compatibility with existing detergents (isopropyl alcohol), and high drying properties. Therefore, it is also suitable for dewatering and drying cleaning.
[0072] (2) Use as a foaming agent
[0073] By utilizing the miscibility of the high-purity HFO-1447 of the present invention with an organic solvent, it can be used to prepare a foamable composition of a thermosetting resin such as polyurethane or a thermoplastic resin such as polystyrene, polyethylene, and polypropylene.
[0074] Example
[0075] [Example 1] 3-Chloro-1,1,1,3,5,5,5-heptafluoropentane (HCFC-457) in the presence of SbCl5 catalyst at low temperature Synthesis
[0076]
[0077] 119.0 g (0.56 mol) of 3-chloro-1,1,1,5,5,5-hexafluoro-2-pentene (HCFO-1446) was added to a 100 ml PFA (perfluoroalkoxyalkane) reactor equipped with a thermometer, a -20°C refrigeration cycle condenser, and an inlet tube. While stirring the reaction solution at -10°C, 12.3 g (0.61 mol, 1.1 eq) of anhydrous HF (liquid) was introduced. Next, 4.09 g (13.7 mmol, 2.5 mol%) of SbCl5 was added and stirred at 0°C for 48 hours. After stirring for 48 hours, 10 g of water was added at 0°C to stop the reaction. The reaction solution was transferred to a separatory funnel for separation, and 130.29 g of an organic layer containing 3-chloro-1,1,1,3,5,5,5-heptafluoropentene was quantitatively obtained with a GC purity of 99%.
[0078] [Example 2, Example 3, Example 4, Example 5 (comparison), Example 6 (comparison)]
[0079] The reaction was carried out in the same manner as in Example 1 except that the reaction temperature, reaction time and HF equivalent were changed as described in Table 1. From the experimental results in Table 1, it can be seen that when a relatively low reaction temperature of 0 to 5°C, a relatively long reaction time of 24 to 48 hours, and an HF equivalent of 1 to 2 are used, the target HCFC-457 can be obtained at a yield of 70% or more. In particular, when the reaction temperature is 0°C, the selectivity of HCFC-457 is high even if the HF equivalent is more than the theoretical amount for HCFO-1446. When the HF equivalent is more than the theoretical amount for HCFO-1446 at 5°C, HCFC-457 is further fluorinated to produce 1,1,1,3,3,5,5,5-octafluoropentane (HFC-458). In addition, when the temperature is below -10°C, the reaction does not proceed at all. When the reaction temperature is raised to 90°C, if the reaction time is as short as 12 hours, the raw material HCFO-1446 remains and a large amount of HFC-458 is generated.
[0080] [Table 1]
[0081]
[0082] Note: The composition after reaction was determined by gas chromatography (GC) area ratio.
[0083] [Example 7] Dehydrochlorination of 3-chloro-1,1,1,3,5,5,5-heptafluoropentane using activated carbon catalyst Synthesis of 3,5,5,5-heptafluoro-2-pentene
[0084]
[0085] For the catalyst tower (φ20.0×400mm) filled with activated carbon pellets (Egret C2X4 / 6-2) as the reactor Figure 1The device was heated at 250°C for the catalyst tower and 150°C for the evaporator, nitrogen was circulated at 63 SCCM, and 3-chloro-1,1,1,3,5,5,5-heptafluoropentane (HCFC-457) was supplied at 25.7 ml / h (2.80 mmol / min, 63 SCCM), so that the flow rate of the mixed gas of HCFC-457 and N2 was 125 SCCM as a whole, and the product was contacted with activated carbon for 60 seconds, and the product was captured in a capture tank filled with 300 g of ice water cooled to -2°C. The pump was stopped after 47 minutes of supplying HCFC-457, and 23.22 g of the organic layer was recovered from the capture tank after no white smoke was observed in the capture tank. The recovered organic phase was quantified by NMR, and the results showed that no (ND) propadiene compounds and no (ND) HFC-458 were detected. The composition was 40.8% (E)-1,1,1,3,5,5,5-heptafluoro-2-pentene, 57.2% (Z)-1,1,1,3,5,5,5-heptafluoro-2-pentene, and 72.0% HCFC-45. 1,1,1,3,5,5,5-heptafluoro-2-pentene (a mixture of (E)-isomer and (Z)-isomer) was obtained with a conversion rate of 98% and a selectivity of >99%.
[0086] [Example 8] Distillation purification of 1,1,1,3,5,5,5-heptafluoro-2-pentene obtained in [Example 7]
[0087] 150.0 g of a crude liquid with a composition of (E)-HFO-1447 / (Z)-HFO-1447 / propylene compound / HFC-458 / HCFC-457=40.8% / 57.2% / ND / ND / 2.0% was purified by distillation at a reflux ratio of 100 / 1 in a KIRIYAMA PAC (filler: SUS mesh) distillation tower having 10 theoretical stages. As a result, 55.0 g of (E)-HFO-1447 with a GC purity of >99% was obtained with a yield of 90% (the remaining 10% of the E-form was obtained as a low-purity fraction), and 80.7 g of (Z)-HFO-1447 with a GC purity of >99% was obtained with a yield of 94% (the remaining 6% of the Z-form was obtained as a low-purity fraction).
[0088] [Example 9 (Comparison)] Based on the dehydrogenation reaction of 1,1,1,3,3,5,5,5-octafluoropentane using AlF3 catalyst, Synthesis of 1,1,3,5,5,5-heptafluoro-2-pentene
[0089]
[0090] For a catalyst tower filled with AlF3 catalyst as a reactor Figure 1The device was heated at 330°C for the catalyst tower and 150°C for the evaporator, nitrogen was circulated at 31 SCCM, and 1,1,1,3,3,5,5,5-octafluoropentane (HFC-458) was supplied at 35.8 ml / h (4.2 mmol / min, 94 SCCM) at the same time, so that the flow rate of the mixed gas of HFC-458 and N2 was 125 SCCM as a whole, and the mixed gas was contacted with the AlF3 catalyst for 60 seconds, and the product was captured in a capture tank filled with 200 g of water cooled to -2°C. After supplying HFC-458 for 60 minutes, the pump was stopped, and after no white smoke was observed in the capture tank, 34.5 g of the organic phase was recovered from the capture tank. The recovered organic phase was quantified by NMR and the result was a composition of 4.3% of propadiene compounds, 37.6% of (E)-HFO-1447, 2.4% of HFC-458, and 55.6% of (Z)-HFO-1447. 1,1,1,3,5,5,5-heptafluoro-2-pentene (a mixture of (E)-isomer and (Z)-isomer) was obtained with a conversion rate of 97.6% and a selectivity of 93.2%.
[0091] [Example 10 (comparison), Example 11 (comparison)]
[0092] The reaction was carried out in the same manner as in Example 9 except that the heating temperature of the catalyst column was set as shown in Table 2. Although the by-product amount of propadiene compound decreased by lowering the reaction temperature, the ratio of unreacted HFC-458 increased.
[0093] [Table 2]
[0094]
[0095] Note: The composition after reaction was determined by gas chromatography (GC) area ratio.
[0096] [Example 12 (Comparison)] The distillation of 1,1,1,3,5,5,5-heptafluoro-2-pentene obtained by the method of [Example 11 (Comparison)] Distillation purification
[0097] 152.0 g of a crude liquid having a composition of (E)-HFO-1447 / (Z)-HFO-1447 / propylene compound / HFC-458=37.1% / 55.3% / 1.4% / 6.3% was purified by distillation at a reflux ratio of 200 / 1 in a KIRIYAMAPAC distillation tower (filler: SUS mesh) having 10 theoretical stages. As a result, 26.4 g of (E)-HFO-1447 having a GC purity of >99% was obtained at a yield of 45% (the remaining 55% of the E-form was obtained as a low-purity fraction), and 39.0 g of (Z)-HFO-1447 having a GC purity of >99% was obtained at a yield of 51% (the remaining 49% of the Z-form was obtained as a low-purity fraction). It was found that although each isomer was obtained at a high purity, if impurities were excluded, the amount of low-purity fractions would increase and the yield of the target product would decrease.
[0098] [Example 13 (Comparison)] Dehydrogenation of 1,1,1,3,3,5,5,5-octafluoropentane using activated carbon catalyst Synthesis of 1,1,1,3,5,5,5-heptafluoro-2-pentene
[0099]
[0100] For the catalyst tower (φ20.0×400mm) filled with activated carbon pellets (Egret C2X4 / 6-2) as the reactor Figure 1 The device was heated at 250°C for the catalyst tower and 150°C for the evaporator, nitrogen was circulated at 63 SCCM, and 1,1,1,3,3,5,5,5-octafluoropentane (HFC-458) was supplied at 23.9 ml / h (2.8 mmol / min, 63 SCCM) at the same time, so that the flow rate of the mixed gas of HFC-458 and N2 was 125 SCCM as a whole, and the product was contacted with activated carbon for 60 seconds, and captured in a capture tank filled with 200 g of ice water cooled to -2°C. After supplying HFC-458 for 51 minutes, the pump was stopped, and after no white smoke was observed in the capture tank, 26.93 g of the organic phase was recovered from the capture tank. The recovered organic phase was quantified by NMR, and the result showed that no allene compound (ND) was detected, and the composition was 76.3% of HFC-458, 7.8% of (E)-HFO-1447, and 15.9% of (Z)-HFO-1447. HFO-1447 (a mixture of (E)-isomer and (Z)-isomer) was obtained at a conversion rate of 23.7% and a selectivity of >99%. When HFO-1447 is produced by dehydrofluorination of HFC-458, it is known that the desorption reaction is difficult to occur, and a large amount of HFC-458 as a raw material remains in the product.
[0101] [Example 14] Resin material test for (E)-HFO-1447 with GC purity > 99%
[0102] Place a 10.0mm×10.0mm×1.0mm test piece of pre-measured size and weight in a 20ml glass bottle, add 5g of (E)-HFO-1447 with GC purity>99% and seal tightly. Store in a thermostatic bath heated to 52°C for 3 hours. After the specified time, take out the glass bottle from the thermostatic bath, cool it naturally at room temperature, unseal the glass bottle, measure the state of the solution, the size and weight of the test piece, and observe the changes. The results are shown in Table 3. The evaluation criteria are as follows.
[0103] ○: There is no corrosion or damage to the resin, no weight change, and no volume change.
[0104] △: There is no corrosion or damage to the resin, but there are changes in weight and volume.
[0105] ×: There is corrosion and damage to the resin.
[0106] [Example 15 (Comparison)] Resin material test of (E)-HFO-1447 containing 3 wt% of allene compound
[0107] Evaluation was performed in the same manner as in Example 14. The results are shown in Table 3. The reason for setting the concentration of the propadiene compound to 3% by weight is that, based on the experimental results of Example 11 (Comparison), it was assumed that the (E)-HFO-1447 obtained by the production method of Patent Document 1 contained the propadiene compound at a ratio of about 97% by weight of (E)-HFO-1447:3% by weight.
[0108] [Example 16] Resin material test for (Z)-HFO-1447 with GC purity > 99%
[0109] The evaluation was carried out in the same manner as in [Example 14] except that the heating temperature was 77° C. The results are shown in Table 4.
[0110] [Example 17 (Comparison)] Resin material test of (Z)-HFO-1447 containing 10 wt% HFC-458
[0111] The evaluation was performed in the same manner as in Example 14 except that the heating temperature was 77° C. The results are shown in Table 4. The reason for setting the concentration of HFC-458 to 10% by weight is that, based on the experimental results of Example 11 (comparison), it was assumed that (Z)-HFO-1447 obtained by the method of Patent Document 1 contained HFC-458 at a ratio of about 90% by weight:10% by weight.
[0112] [Example 18] Elastomer material test for (E)-HFO-1447 with GC purity > 99%
[0113] Evaluation was performed in the same manner as in Example 14. The results are shown in Table 5.
[0114] [Example 19 (Comparison)] Elastomer material test of (E)-HFO-1447 containing 3 wt% of propadiene compound
[0115] Evaluation was performed in the same manner as in Example 14. The results are shown in Table 5. The reason for setting the concentration of the propadiene compound to 3% by weight is that, based on the experimental results of Example 11 (Comparison), it was assumed that the (E)-HFO-1447 obtained by the production method of Patent Document 1 contained propadiene compounds at a ratio of (E)-HFO-1447:propadiene compounds of approximately 97% by weight:3% by weight.
[0116] [Table 3]
[0117] Table 3. Resistance test for (E)-HFO-1447 and (E)-HFO-1447 containing allene compound
[0118]
[0119] As can be seen from the test results in Table 3, the production method of the present invention can efficiently produce high-purity (E)-HFO-1447 without corrosion and damage to the resin or weight change. If precision distillation is performed according to the existing production method, high-purity (E)-HFO-1447 can also be obtained, but the yield is significantly reduced in order to remove the low-purity fraction.
[0120] [Table 4]
[0121] Table 4. Resistance test for (Z)-HFO-1447 and (Z)-HFO-1447 containing HFC-458
[0122]
[0123] As can be seen from the test results in Table 4, the production method of the present invention can efficiently produce high-purity (Z)-HFO-1447 with no corrosion or damage to the resin, or with little weight change. If precision distillation is performed according to the conventional production method, high-purity (Z)-HFO-1447 can also be obtained, but the yield is significantly reduced in order to remove the low-purity fraction.
[0124] [Table 5]
[0125] Table 5. Resistance test of elastomers of (E)-HFO-1447 and (E)-HFO-1447 containing allene compounds
[0126]
[0127] As can be seen from the test results in Table 5, the production method of the present invention can efficiently produce high-purity (E)-HFO-1447 with no elastomer corrosion, weight change, volume change, or little weight change and volume change. If precision distillation is performed according to the existing production method, high-purity (E)-HFO-1447 can also be obtained, but the yield is significantly reduced in order to remove the low-purity fraction.
[0128] [Example 20] Compatibility test of (E)-HFO-1447 and (Z)-HFO-1447 with GC purity > 99% with alcohol solvents
[0129] Appropriate amounts of (E)-HFO-1447 or (Z)-HFO-1447 with a GC purity of >99% and an alcohol solvent were added to each 20 ml glass bottle, and the presence or absence of phase separation was visually observed. The results are shown in Table 6. The evaluation criteria are as follows.
[0130] 0: No phase separation, compatible.
[0131] △: Phase separation was observed, but the phases were compatible with stirring.
[0132] ×: Phase separation.
[0133] [Example 21 (Comparison)] Compatibility test of commercially available fluorobutene and perfluoroheptene with alcohol solvents
[0134] Evaluation was performed in the same manner as in Example 20. The results are shown in Table 6.
[0135] [Table 6]
[0136]
[0137] As can be seen from the test results in Table 6, according to the manufacturing method of the present invention, high-purity (E) or (Z)-HFO-1447 that is compatible with alcohol solvents, especially isopropyl alcohol (2-propanol) can be efficiently manufactured. On the other hand, commercially available fluorine-based detergents of fluorobutene and perfluoroheptene all have compatibility problems with isopropyl alcohol. In particular, since isopropyl alcohol is used as a detergent for semiconductor wafers, it is believed that the high-purity HFO-1447 of the present invention is also mixed with other cleaning solvents and is useful in detergent applications.
[0138] From the above results, it was found that (E) and (Z)-HFO-1447 produced by the method of the present invention are produced without containing by-products that are produced in the reaction system and are difficult to remove, and that degradation of the resin can be suppressed by high purification, making them suitable for detergent applications.
Claims
1. A method for producing 1,1,1,3,5,5,5-heptafluoro-2-pentene, the method comprising: (a) reacting 3-chloro-hexafluoro-2-pentene with hydrogen fluoride in the presence of a metal halogenide catalyst at a temperature exceeding -10°C and not more than 20°C to produce 3-chloro-1,1,1,3,5,5,5-heptafluoropentane, and (b) Dehydrochlorinating the 3-chloro-1,1,1,3,5,5,5-heptafluoropentane obtained in (a) in the presence of an activated carbon catalyst to produce 1,1,1,3,5,5,5-heptafluoro-2-pentene.
2. The method according to claim 1, wherein: The halogenated metal catalyst is selected from antimony halide catalysts, tin halide catalysts, titanium halide catalysts, niobium halide catalysts, tantalum halide catalysts or combinations thereof.
3. The method according to claim 1, wherein: The halogenated metal catalyst is selected from antimony trichloride, antimony pentachloride, antimony trifluoride, antimony pentafluoride, tin tetrachloride, titanium tetrachloride, niobium pentafluoride, tantalum pentafluoride or a combination thereof.
4. The method according to claim 1, wherein: Hydrogen fluoride is used in a molar equivalent ratio of 1 to 1.5 to 3-chloro-hexafluoro-2-pentene.
5. The method according to claim 1, wherein: The amount of the halogenated metal catalyst is 2 to 3 mol % relative to 3-chloro-hexafluoro-2-pentene.
6. The method according to claim 1, wherein: The reaction of step (a) is carried out at a temperature of -5°C to 10°C.
7. The method according to claim 1, wherein: The metal halogenide catalyst is selected from antimony trichloride, antimony pentachloride, antimony trifluoride, antimony pentafluoride, tin tetrachloride, titanium tetrachloride, niobium pentafluoride, tantalum pentafluoride or a combination thereof, hydrogen fluoride is used in a 1 to 1.5 molar equivalent ratio relative to 3-chloro-hexafluoro-2-pentene, the amount of the metal halogenide catalyst is 2 to 3 mol% relative to 3-chloro-hexafluoro-2-pentene, and the reaction of step (a) is carried out at a temperature of -5°C to 10°C.
8. High-purity 1,1,1,3,5,5,5-heptafluoro-2-pentene obtained by the method according to any one of claims 1 to 7.
9. The high-purity 1,1,1,3,5,5,5-heptafluoro-2-pentene according to claim 8, wherein the purity thereof exceeds 99%.