Method for sterilization and surface modification of culture plate

Through the three-gradient sterilization treatment of mixed solvent, ethylene oxide and hydrogen peroxide, combined with ultrasonic and oxidation treatment, the problem of poor sterilization effect of culture plates is solved, efficient sterilization and surface modification are achieved, and the culture plates are met Strict use requirements.

CN119055808AInactive Publication Date: 2024-12-03SHAOXING UNIVERSITY
View PDF 4 Cites 0 Cited by

Patent Information

Application Number
CN202411553996.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-11-04
Publication Date
2024-12-03
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing sterilization methods have poor sterilization effect and difficulty in cleaning the remains of bacterial seeds, especially the strict use requirements for culture plates cannot be met.

Method used

Using a three-gradient sterilization treatment of mixed solvents (ethanol and ether) combined with ethylene oxide and hydrogen peroxide, ultrasonic oscillation, steam permeation and oxidation treatment, an efficient sterilization and surface modification method is formed, and sodium percarbonate is used to stabilize oxygen release. , improve hydrophilicity.

Benefits of technology

It significantly improves the sterilization effect of the culture plate surface, reduces the sterilization time and residual problems, meets the use needs of the culture plate, and improves the surface hydrophilicity and oxidative stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure SMS_1
    Figure SMS_1
  • Figure SMS_2
    Figure SMS_2
Patent Text Reader

Abstract

The invention belongs to the technical field of cell culture, and particularly relates to a culture plate sterilization and surface modification method which comprises the following steps: washing a polystyrene culture plate by adopting a mixed organic solvent, carrying out liquid-phase sterilization and steam sterilization on ethylene oxide, and carrying out soaking hydrophilic treatment on hydrogen peroxide. The problem that the sterilization effect is poor is solved, the mixed solvent, ethylene oxide and hydrogen peroxide are used for forming different functional three-gradient sterilization treatment, the sterilization effect of the surface of the culture plate is greatly improved, meanwhile, hydrogen peroxide serves as an oxidation material, sodium percarbonate serves as a stabilizer and a catalyst, and release and stability of oxygen are guaranteed; and the surface hydrophilization effect is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the technical field of cell culture, and in particular relates to a method for sterilizing and surface modifying a culture plate. Background Art

[0002] Sterilization is a measure that uses external means to permanently deprive all microorganisms of their ability to grow and reproduce. At present, the main sterilization methods include chemical reagent sterilization, radiation sterilization, dry heat sterilization, moist heat sterilization and filtration sterilization. Chemical reagent sterilization mainly refers to ethylene oxide sterilization, radiation sterilization mainly refers to irradiation sterilization, dry heat sterilization mainly refers to sterilization by heating in an oven, moist heat sterilization mainly uses an autoclave, and filtration sterilization mainly refers to sterilization by filtration with a microporous membrane. Ethylene oxide sterilization is achieved by alkylating specific groups on microbial protein molecules, causing the protein to lose its reactive groups, hindering the normal biochemical reactions and metabolism of the protein, thereby achieving a sterilization effect. Radiation sterilization generally uses ultraviolet irradiation sterilization, which takes a long time, is inefficient, and requires long-term irradiation. Dry heat sterilization is a technique for sterilization in a dry environment (such as flame or dry hot air). Moist heat sterilization is a method of sterilization in saturated steam, boiling water or circulating steam. Filtration sterilization is a method of removing bacteria from liquid or air by physical retention to achieve the purpose of sterility. Although the above sterilization method can achieve good sterilization effect, the sterilization time is relatively long, and the residual bacteria bodies after sterilization are difficult to clean. The culture plate is a commonly used cell culture device, which needs to be strictly sterilized before use and effectively reduce the secondary deposition of bacteria. Therefore, the above simple sterilization treatment cannot meet the strict requirements for the use of culture plates. Summary of the invention

[0003] In view of the problems in the prior art, the present invention provides a method for sterilizing and surface modifying a culture plate, which solves the problem of poor sterilization effect. A three-gradient sterilization treatment with different functionalities is formed by using a mixed solvent, ethylene oxide and hydrogen peroxide, which greatly improves the sterilization effect of the culture plate surface. At the same time, hydrogen peroxide is used as an oxidizing material and sodium percarbonate is used as a stabilizer and catalyst to ensure the release and stability of oxygen, thereby improving the surface hydrophilization effect.

[0004] In order to achieve the above technical objectives, the technical solution of the present invention is: A method for sterilizing and surface modifying a culture plate comprises the following steps: Step 1, soaking the culture plate in a mixed solvent for 20-30 minutes, ultrasonically oscillating for 5-10 minutes, taking out and drying to obtain a culture plate with a clean surface, the material of the culture plate is polystyrene, the mixed solvent is a mixed solvent of ethanol and ether, and the volume ratio of ethanol to ether is 2-3:2, the soaking temperature is 20-30°C, the ultrasonic frequency of the ultrasonic oscillation is 80-100kHz, the temperature is 5-10°C; the drying temperature is 70-80°C; this step utilizes the solubility and penetration characteristics of ethanol and ether to form a homogeneous mixed solvent, when the culture plate is placed in the mixed solvent, ultrasonic oscillation can remove the floating dust on the surface, and the bactericidal effect of ethanol, the penetration effect of ether and the solubility of ethanol-ether can achieve a preliminary sterilization effect; ultrasonic oscillation can accelerate the penetration of ether and also accelerate the penetration of ethanol, thereby achieving a good preliminary sterilization effect and surface cleaning effect; after ultrasonic oscillation, the surface impurities are removed, and during the process of taking out and drying, the ether and ethanol are completely evaporated and removed to obtain a preliminary clean culture plate; Step 2, passing ethylene oxide into ether and stirring evenly to form a dissolving solution, then immersing the clean culture plate in the dissolving solution and letting it stand for 0.5-2h, sealing and heating and letting it stand for 2-4h, taking it out after cooling, and drying it to obtain a secondary sterilized culture plate, wherein the concentration of ethylene oxide in ether is 0.8-1.2g / L, the stirring speed is 100-200r / min, the standing temperature is 5-10°C, the sealing and heating and standing temperature is 40-50°C; the cooling temperature is 0-5°C ; The drying temperature is 40-50°C, and the dried gas is purged into ethanol; this step utilizes the solubility of ethylene oxide in ether to form a dissolving solution, and the culture is immersed in the ethylene oxide ether solution to achieve excellent bacterial killing effect; during the sealed temperature rise and static state, the ether and ethylene oxide form a vapor state to form a double permeation system, thereby improving the excellent permeation sterilization effect; during the cooling process, the ether and ethylene oxide are converted into liquid to form a dissolving solution, and the culture plate is directly taken out to achieve solid-liquid separation; Step 3, placing the secondary sterilized culture plate in distilled water for ultrasonic treatment for 20-30 minutes, taking it out and drying it to obtain a dry culture plate, then spraying hydrogen peroxide on the surface of the culture plate and letting it stand for 1-3 hours, finally spraying sodium percarbonate solution on the surface of the hydrogen peroxide, letting it stand at a constant temperature, washing it with ethanol and then drying it to obtain a sterilized culture plate with hydrophilic surface modification, wherein the ultrasonic frequency of the ultrasonic treatment is 80-90kHz, the temperature is 10-20°C, the drying temperature is 50-60°C, the time is 2-3h, the mass concentration of the hydrogen peroxide is 10-15%, and the spray amount is 5-7mL / cm 2 The concentration of the sodium percarbonate solution is 0.1-0.2 g / L, and the spray volume is 2-3 mL / cm 2, the temperature of the constant temperature static is 60-70°C; this step uses ultrasound to completely disperse and peel off the bacterial corpses on the secondary sterilized culture plate, which has a good separation effect and obtains a clean and dry culture plate; hydrogen peroxide is sprayed on the culture plate to form a surface liquid film, and the hydrogen peroxide will slowly decompose to form oxygen, which can not only completely kill the remaining bacteria, but also form surface oxidation on the polystyrene material; sodium percarbonate solution can overlap and dissolve with the hydrogen peroxide liquid film, and sodium percarbonate is invaded into the hydrogen peroxide, and it will decompose itself to produce hydrogen peroxide and sodium carbonate, thereby ensuring the stability of the content of hydrogen peroxide. Secondly, sodium carbonate can hydrolyze in water to produce hydroxide, and the hydroxide can promote the decomposition of hydrogen peroxide to form oxygen and water, thereby ensuring the oxygen concentration, achieving stable oxidation of polystyrene, greatly improving the oxidation area and oxidation degree of the polystyrene surface, and achieving the stability of the hydrophilicity of the polystyrene surface.

[0005] It can be seen from the above description that the present invention has the following advantages: 1. The present invention solves the problem of poor sterilization effect. A three-gradient sterilization treatment with different functionalities is formed by using a mixed solvent, ethylene oxide and hydrogen peroxide, which greatly improves the sterilization effect on the surface of the culture plate. At the same time, hydrogen peroxide is used as an oxidizing material and sodium percarbonate is used as a stabilizer and catalyst to ensure the release and stability of oxygen, thereby improving the surface hydrophilization effect.

[0006] 2. The present invention utilizes ethanol and ether to form a mixed solvent, utilizes the cleaning and sterilizing effects of ethanol to form a surface cleaning effect, and reduces the influence of surface floating dust and impurities.

[0007] 3. The present invention utilizes a low boiling point system of ether and ethylene oxide to form a high-efficiency sterilization effect combining liquid phase immersion sterilization and steam penetration sterilization, which greatly improves the sterilization efficiency, reduces sterilization dead corners, and meets the use requirements of the culture plate. DETAILED DESCRIPTION

[0008] The present invention is described in detail with reference to the embodiments, but no limitation is imposed on the claims of the present invention.

[0009] Example 1 A method for sterilizing and surface modifying a culture plate comprises the following steps: Step 1, placing a polystyrene culture plate in a 1:1 volume ratio ethanol-ether mixed solvent at a constant temperature of 20° C. for 20 minutes, oscillating at a frequency of 80 kHz at 5° C. for 50 minutes, and drying at 70° C. after taking out to obtain a culture plate with a clean surface; Step 2, introducing ethylene oxide into ether and stirring evenly to form a solution with a concentration of 0.8 g / L, then immersing a clean culture plate in the solution and standing at 5°C for 0.5 h, sealing and standing at 40°C for 2 h, cooling to 0°C and then taking out, drying at 40°C to obtain a secondary sterilized culture plate, and blowing the dried gas into ethanol for recovery; Step 3: Place the secondary sterilized culture dish in distilled water and ultrasonically treat it at 800kHz and 10°C for 20min. After taking it out, dry it at 50°C for 2h to obtain a dry culture dish. Then, add 10% hydrogen peroxide at 5mL / cm 2 The culture plate was sprayed with a spray volume of 2 mL / cm 2 The surface of the hydrogen peroxide solution was sprayed with a spray amount of , and the plate was kept at a constant temperature of 60°C. After washing with ethanol, the plate was dried to obtain a sterilized culture plate with a hydrophilic surface modification.

[0010] Example 2 A method for sterilizing and surface modifying a culture plate comprises the following steps: Step 1, placing a polystyrene culture plate in a mixed solvent of ethanol and ether with a volume ratio of 3:2 and immersing it at a constant temperature of 30°C for 30 minutes, oscillating it at an ultrasonic frequency of 100 kHz at 10°C for 10 minutes, and then taking it out and drying it at 80°C to obtain a culture plate with a clean surface; Step 2, introducing ethylene oxide into ether and stirring evenly to form a solution with a concentration of 1.2 g / L, then immersing a clean culture plate in the solution and standing at 10° C. for 2 hours, sealing and standing at 50° C. for 4 hours, cooling to 5° C. and then taking it out, drying it at 50° C. to obtain a secondary sterilized culture plate, and blowing the dried gas into ethanol for recovery; Step 3: Place the secondary sterilized culture dish in distilled water and ultrasonically treat it at 90kHz and 20°C for 30min. After taking it out, dry it at 60°C for 3h to obtain a dry culture dish. Then, add 15% hydrogen peroxide at 7mL / cm 2 The culture plate was sprayed with a spray volume of 100 ml / cm2 and allowed to stand at 30°C for 2 h. Then, a sodium percarbonate solution with a concentration of 0.2 g / L was sprayed at a rate of 3 mL / cm2. 2 The surface of the hydrogen peroxide solution was sprayed with a spray amount of , and the plate was kept at a constant temperature of 70°C. After washing with ethanol, the plate was dried to obtain a sterilized culture plate with a hydrophilic surface modification.

[0011] Example 3 A method for sterilizing and surface modifying a culture plate comprises the following steps: Step 1, placing a polystyrene culture plate in a mixed solvent of ethanol and ether with a volume ratio of 3:2 and immersing it at a constant temperature of 25°C for 25 minutes, oscillating it at an ultrasonic frequency of 90kHz at 8°C for 10 minutes, and drying it at 75°C after taking it out to obtain a culture plate with a clean surface; Step 2, ethylene oxide is introduced into ether and stirred evenly to form a solution with a concentration of 1 g / L, and then a clean polystyrene culture plate is immersed in the solution and allowed to stand at 8° C. for 1 hour, sealed and allowed to stand at 45° C. for 3 hours, taken out after cooling to 3° C., and dried at 45° C. to obtain a secondary sterilized culture plate, and the dried gas is purged into ethanol for recovery; Step 3: Place the secondary sterilized culture dish in distilled water and ultrasonically treat it at 90kHz and 15°C for 25min. After taking it out, dry it at 55°C for 3h to obtain a dry culture dish. Then, add 12% hydrogen peroxide at 6mL / cm 2 The culture plate was sprayed with a spray volume of 100 ml / cm2 and allowed to stand at 30°C for 2 h. Then, a sodium percarbonate solution with a concentration of 0.2 g / L was sprayed at a rate of 3 mL / cm2. 2 The surface of the hydrogen peroxide solution was sprayed with a spray amount of , and the plate was kept at a constant temperature of 65°C. After washing with ethanol, the plate was dried to obtain a sterilized culture plate with a hydrophilic surface modification.

[0012] Comparative Example 1 A culture plate sterilization process comprises the following steps: Step 1, placing a polystyrene culture plate in a mixed solvent of ethanol and ether with a volume ratio of 3:2 and immersing it at a constant temperature of 25°C for 25 minutes, oscillating it at an ultrasonic frequency of 90kHz at 8°C for 10 minutes, and drying it at 85°C after taking it out to obtain a culture plate with a clean surface; Step 2, ethylene oxide is introduced into ether and stirred evenly to form a solution with a concentration of 1 g / L, and then a clean polystyrene culture plate is immersed in the solution and allowed to stand at 8° C. for 1 hour, sealed and allowed to stand at 45° C. for 3 hours, taken out after cooling to 3° C., and dried at 45° C. to obtain a secondary sterilized culture plate, and the dried gas is purged into ethanol for recovery; Step 3, placing the secondary sterilized culture plate in distilled water, and ultrasonically treating it at 85kHz and 50°C for 25min, taking it out and drying it at 115°C to obtain a dry culture plate.

[0013] Comparative Example 2 A culture plate sterilization treatment comprises the following steps: placing a polystyrene culture plate in an ethanol-ether mixed solvent with a volume ratio of 3:2 and immersing it at a constant temperature of 25°C for 25 minutes, oscillating it at an ultrasonic frequency of 90kHz at 8°C for 10 minutes, and drying it at 85°C after taking it out to obtain a culture plate with a clean surface.

[0014] Comparative Example 3 A commercially available, non-sterile polystyrene culture plate.

[0015] Performance Testing The culture plates of Examples 1-3 and Comparative Examples 1-3 were used as test samples. Water drops were added to the culture plates to detect the contact angle between the water drops and the culture plates. The hydrophilicity of the culture plates was represented by the water contact angle. The results are as follows:

[0016] The above data show that the polystyrene culture plate treated with hydrogen peroxide exhibits good hydrophilicity, which is in sharp contrast to the products of Comparative Examples 1-3.

[0017] Sterilization effect The culture plates of Example 1-3 and Comparative Example 1-3 were used as test samples to conduct a sterilization effect test. The culture medium was directly added to the culture plate and cultured at a constant temperature for 72 hours. The results are as follows:

[0018] It is understood that the above specific description of the present invention is only used to illustrate the present invention and is not limited to the technical solutions described in the embodiments of the present invention. Those skilled in the art should understand that the present invention can still be modified or replaced by equivalents to achieve the same technical effects; as long as the use requirements are met, they are within the protection scope of the present invention.

Claims

1. A method for sterilizing and surface modifying a culture plate, characterized in that: The steps include: Step 1, soaking the culture plate in a mixed solvent for 20-30 minutes, ultrasonically vibrating for 5-10 minutes, taking out and drying to obtain a culture plate with a clean surface; Step 2, introducing ethylene oxide into ether and stirring evenly to form a dissolving solution, then immersing a clean culture plate in the dissolving solution and letting it stand for 0.5-2 hours, sealing and heating and letting it stand for 2-4 hours, taking it out after cooling, and drying it to obtain a secondary sterilized culture plate; Step 3, placing the secondary sterilized culture plate in distilled water for ultrasonic treatment for 20-30 minutes, taking it out and drying it to obtain a dry culture plate, then spraying hydrogen peroxide on the surface of the culture plate and letting it stand for 1-3 hours, and finally spraying sodium percarbonate solution on the surface of the hydrogen peroxide and letting it stand at a constant temperature, washing with ethanol and then drying it to obtain a sterilized culture plate with a hydrophilic surface modification to obtain a sterilized culture plate with a hydrophilic surface modification.

2. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The material of the culture plate in step 1 is polystyrene.

3. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The mixed solvent in step 1 is a mixed solvent of ethanol and ether, and the volume ratio of ethanol to ether is 2-3:2, and the soaking temperature is 20-30°C.

4. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The ultrasonic frequency of the ultrasonic oscillation in step 1 is 80-100 kHz, and the temperature is 5-10°C; the temperature of the drying is 70-80°C.

5. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The concentration of ethylene oxide in diethyl ether in step 2 is 0.8-1.2 g / L, and the stirring speed is 100-200 r / min.

6. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The standing temperature in step 2 is 5-10°C, the sealing and heating standing temperature is 40-50°C; and the cooling temperature is 0-5°C.

7. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The drying temperature in step 2 is 40-50° C., and the dried gas is purged into the ethanol.

8. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: In the step 3, the ultrasonic treatment has an ultrasonic frequency of 80-90 kHz and a temperature of 10-20° C., and the drying temperature is 50-60° C. and the drying time is 2-3 h.

9. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The mass concentration of hydrogen peroxide in step 3 is 10-15%, and the spray volume is 5-7 mL / cm 2 .

10. The method for sterilizing and surface modifying a culture plate according to claim 1, characterized in that: The concentration of the sodium percarbonate solution in step 3 is 0.1-0.2 g / L, and the spray volume is 2-3 mL / cm 2 The constant temperature standing temperature is 60-70°C.

Citation Information

Patent Citations

  • Method for producing hydrophilized cellulose fiber, and method for reducing oxidized cellulose fiber

    CN103328715A

  • Surface treatment method for disposable plastic petri dish

    CN104974366A

  • Method for sterilizing cell culture plate and performing surface hydrophilic modification treatment

    CN116726220A

  • Drying solvent for cleaning and its production

    JP1993117692A