Sustained-release hydrogel of stem cell exosome and preparation method thereof
By using sodium alginate and other components in stem cell exosome hydrogels to form a three-dimensional network structure, the problem of exosome release too fast in the existing technology is solved, slow release and long-term biological repair are achieved, and biorepair efficiency is improved and security.
Patent Information
- Application Number
- CN202411009816.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-26
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The stem cell exosome hydrogel prepared by the prior art releases too quickly, resulting in poor sustainability of biorepair effect.
Sustained release hydrogel prepared by sodium alginate, pretreated nanomontmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer and methacrylic anhydride, through ultrasound Dispersion and polymerization form a three-dimensional network structure that encapsulates and slowly releases exosomes.
The slow release of exosomes is achieved, the biorepair efficiency is improved, the biorepair time is extended, the waste of exosomes is avoided, and biocompatibility and safety are ensured.
Smart Images

Figure CN119055835A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of biotechnology, and in particular relates to a sustained-release hydrogel of stem cell exosomes. Background Art
[0002] In the biomedical field, stem cell research has always attracted much attention. They have great potential due to their unique self-renewal and multidirectional differentiation capabilities, providing new possibilities for the treatment of various diseases, and stem cell exosomes, these tiny vesicles, play an important role in intercellular communication, tissue repair and regenerative medicine.
[0003] The tiny vesicles secreted by stem cells during physiological activities usually have a diameter between 40 and 160 nanometers. These exosomes are rich in a variety of biologically active molecules, such as proteins, nucleic acids (including mRNA, miRNA, etc.), lipids and other metabolites.
[0004] The functions of stem cell exosomes include:
[0005] 1. Intercellular communication.
[0006] 2. Tissue repair and regeneration.
[0007] 3. Immune regulation.
[0008] 4.Drug delivery system.
[0009] 5. Diagnostic markers.
[0010] Hydrogel is a polymer with a three-dimensional network structure that can swell in water and retain a large amount of water without dissolving. Due to its good biocompatibility, degradability and controllable physical and chemical properties, hydrogel has been widely used in drug delivery, tissue engineering and regenerative medicine.
[0011] Carrying exosomes by hydrogel can make the application of exosomes more convenient. However, the hydrogel prepared by the prior art releases exosomes too quickly, resulting in poor sustainability of the biorepair effect produced by the exosomes.
[0012] Based on this, a sustained-release hydrogel of stem cell exosomes is provided to solve the existing technical problems. Summary of the invention
[0013] The purpose of the present invention is to provide a sustained-release hydrogel of stem cell exosomes and a preparation method thereof, so as to solve the deficiencies in the prior art.
[0014] The technical solution adopted by the present invention is as follows:
[0015] A sustained-release hydrogel of stem cell exosomes comprises the following ingredients by weight: 2-3 parts of sodium alginate, 0.3-0.5 parts of pretreated nano-montmorillonite, 0.1-0.3 parts of aloe vera composite extract, 1.1-1.2 parts of hydroxypropyl-β-cyclodextrin, 6-8 parts of gelatin powder, 1-2 parts of moisturizer, 3.3-3.5 parts of methacrylic anhydride, and 20-30 parts of sterile water.
[0016] As a further technical solution, the method for preparing the pretreated nano-montmorillonite is:
[0017] (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion;
[0018] (2) adding sodium citrate solution dropwise to the nano-montmorillonite dispersion, adjusting the temperature to 50°C, keeping warm in a water bath, stirring while adding dropwise, and standing for 20-25 minutes after the addition is completed within 30 minutes;
[0019] (3) Continue to dropwise add sodium bicarbonate solution to the nano-montmorillonite dispersion, adjust the temperature to 70° C., keep warm in a water bath, and stir while dropping. After the dropwise addition is completed within 40 minutes, let stand for 30-40 minutes to obtain a mixed solution;
[0020] (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite.
[0021] As a further technical solution, the mixing ratio of the nano-montmorillonite and deionized water is 10-15 g: 200 mL;
[0022] The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1-1.2;
[0023] The mass fraction of the sodium citrate solution is 10%;
[0024] The mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2;
[0025] The mass fraction of sodium bicarbonate solution is 10%.
[0026] As a further technical solution, the centrifugal treatment is carried out at a centrifugal speed of 8000 r / min and for 15 min.
[0027] As a further technical solution: the preparation method of the aloe composite extract is:
[0028] Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material;
[0029] The aloe vera composite material and water are mixed in a mass ratio of 1:15-18, and then pulped for 30 minutes to obtain a composite slurry;
[0030] The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes, and filtered to obtain a filtrate and a filter residue;
[0031] The filter residue is extracted twice more in the same way, the filtrates from the three times are combined, and 50% of the volume of the combined filtrate is added with anhydrous ethanol for alcohol precipitation. The product is placed at 4°C overnight for 12 hours, and then centrifuged at 5000 r / min to obtain the precipitate, which is then vacuum dried to obtain the product.
[0032] As a further technical solution, the heating reflux extraction temperature is 72°C.
[0033] As a further technical solution, the vacuum drying temperature is 55° C. and the time is 4 hours.
[0034] As a further technical solution: the moisturizing agent is glycerol.
[0035] A method for preparing a sustained-release hydrogel of stem cell exosomes comprises the following steps:
[0036] S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water;
[0037] S2 divides the sterile water into 3 equal portions;
[0038] S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution;
[0039] S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution;
[0040] S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution;
[0041] S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
[0042] In step S5, the desired carrying exosomes may be introduced.
[0043] Beneficial effects:
[0044] The hydrogel prepared by the present invention can form a three-dimensional network structure by physical or chemical cross-linking, thereby achieving encapsulation and sustained release of exosomes.
[0045] The sustained-release hydrogel of stem cell exosomes prepared by the present invention has multiple characteristics, including an excellent exosome delivery system, capable of carrying exosomes, and by combining exosomes with hydrogels, the exosomes can be slowly released after compounding to achieve the effect of biorepair; the sustained-release hydrogel of stem cell exosomes prepared by the present invention has excellent biocompatibility and is safe and reliable to use.
[0046] By improving the formula of the hydrogel, the network structure and composition of the prepared hydrogel are greatly improved compared with the existing hydrogel, and it can slowly release exosomes. By slowly releasing exosomes, it can play a long-term biorepair function, which not only greatly improves the biorepair efficiency, but also avoids the waste of exosomes.
[0047] Exosomes are introduced before the hydrogel undergoes polymerization reaction, and then a hydrogel with a three-dimensional network structure is formed. In this process, the exosomes will be wrapped inside or on the surface of the hydrogel, thereby achieving the encapsulation of the exosomes. The three-dimensional network structure of the sustained-release hydrogel prepared by the present invention can limit the free diffusion of the exosomes, so that it maintains a high local concentration for a certain period of time. In the initial stage, due to the high concentration of exosomes, the release amount of exosomes in a short time will be relatively high, and the subsequent release rate of exosomes will gradually decrease, forming a slow release mechanism, which can slowly release exosomes for a long time and form a long-term biological repair function. BRIEF DESCRIPTION OF THE DRAWINGS
[0048] Figure 1 This is the 0-day picture of the wound surface of mice carrying exosomes in Example 1;
[0049] Figure 2 This is a picture of the wound surface of mice carrying exosomes in Example 1 three days later;
[0050] Figure 3 This is a picture of the wound surface of mice carrying exosomes in Example 1 on day 6;
[0051] Figure 4 This is a picture of the wound surface of mice carrying exosomes in Example 1 on day 9;
[0052] Figure 5 This is a picture of the wound surface of mice carrying exosomes in Example 1 11 days later. DETAILED DESCRIPTION
[0053] The technical solutions in the embodiments of the present invention are described clearly and completely below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of them. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0054] Example 1
[0055] A sustained-release hydrogel of stem cell exosomes:
[0056]
[0057]
[0058] The preparation method of pretreated nano-montmorillonite is:
[0059] (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion;
[0060] (2) Add sodium citrate solution to the nano-montmorillonite dispersion, adjust the temperature to 50°C, keep warm in a water bath, stir while adding, and let stand for 20 minutes after the addition is completed in 30 minutes; the mixing ratio of nano-montmorillonite to deionized water is 10g:200mL;
[0061] The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1; the mass fraction of the sodium citrate solution is 10%;
[0062] (3) Continue to drop sodium bicarbonate solution into the nano-montmorillonite dispersion, adjust the temperature to 70°C, keep warm in a water bath, stir while dropping, and after the dropwise addition is completed for 40 minutes, let stand for 30 minutes to obtain a mixed solution; the mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2;
[0063] The mass fraction of sodium bicarbonate solution is 10%.
[0064] (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite; the centrifugal speed of the centrifugal treatment is 8000 r / min and the time is 15 min.
[0065] The preparation method of aloe vera compound extract is as follows:
[0066] Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material;
[0067] The aloe vera composite material and water were mixed in a mass ratio of 1:15, and then pulped for 30 minutes to obtain a composite slurry;
[0068] The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes and filtered to obtain a filtrate and a filter residue; the heating reflux extraction temperature was 72°C.
[0069] The filter residue is extracted twice again in the same way, the filtrates from the three extractions are combined, and 50% of the volume of the combined filtrates is added with anhydrous ethanol for alcohol precipitation. The mixture is placed at 4°C overnight and allowed to stand for 12 hours. The mixture is then centrifuged at 5000 r / min to obtain a precipitate, which is then vacuum dried to obtain the product; the vacuum drying temperature is 55°C and the time is 4 hours; the moisturizer is glycerin.
[0070] A method for preparing a sustained-release hydrogel of stem cell exosomes comprises the following steps:
[0071] S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water;
[0072] S2 divides the sterile water into 3 equal portions;
[0073] S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution;
[0074] S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution;
[0075] S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution;
[0076] S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
[0077] Example 2
[0078] A sustained-release hydrogel of stem cell exosomes:
[0079] Components Weight Sodium alginate 2.2 servings Pre-treated nano-montmorillonite 0.35 Aloe Vera Complex Extract 0.18 Hydroxypropyl-β-cyclodextrin 1.15 servings Gelatin powder 6.5 servings Moisturizer 1.2 servings Methacrylic Anhydride 3.4 servings Sterile water 23 servings
[0080] The preparation method of pretreated nano-montmorillonite is:
[0081] (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion;
[0082] (2) Add sodium citrate solution to the nano-montmorillonite dispersion, adjust the temperature to 50°C, keep warm in a water bath, stir while adding, and let stand for 20 minutes after the addition is completed in 30 minutes; the mixing ratio of nano-montmorillonite to deionized water is 10g:200mL;
[0083] The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1; the mass fraction of the sodium citrate solution is 10%;
[0084] (3) Continue to drop sodium bicarbonate solution into the nano-montmorillonite dispersion, adjust the temperature to 70°C, keep warm in a water bath, stir while dropping, and after the dropwise addition is completed for 40 minutes, let stand for 30 minutes to obtain a mixed solution; the mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2;
[0085] The mass fraction of sodium bicarbonate solution is 10%.
[0086] (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite; the centrifugal speed of the centrifugal treatment is 8000 r / min and the time is 15 min.
[0087] The preparation method of aloe vera compound extract is as follows:
[0088] Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material;
[0089] The aloe vera composite material and water were mixed in a mass ratio of 1:15, and then pulped for 30 minutes to obtain a composite slurry;
[0090] The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes and filtered to obtain a filtrate and a filter residue; the heating reflux extraction temperature was 72°C.
[0091] The filter residue is extracted twice again in the same way, the filtrates from the three extractions are combined, and 50% of the volume of the combined filtrates is added with anhydrous ethanol for alcohol precipitation. The mixture is placed at 4°C overnight and allowed to stand for 12 hours. The mixture is then centrifuged at 5000 r / min to obtain a precipitate, which is then vacuum dried to obtain the product; the vacuum drying temperature is 55°C and the time is 4 hours; the moisturizer is glycerin.
[0092] A method for preparing a sustained-release hydrogel of stem cell exosomes comprises the following steps:
[0093] S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water;
[0094] S2 divides the sterile water into 3 equal portions;
[0095] S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution;
[0096] S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution;
[0097] S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution;
[0098] S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
[0099] Example 3
[0100] A sustained-release hydrogel of stem cell exosomes:
[0101] Components Weight Sodium alginate 2.5 servings Pre-treated nano-montmorillonite 0.4 parts Aloe Vera Complex Extract 0.2 parts Hydroxypropyl-β-cyclodextrin 1.18 servings Gelatin powder 7 servings Moisturizer 1.6 servings Methacrylic Anhydride 3.4 servings Sterile water 25 servings
[0102] The preparation method of pretreated nano-montmorillonite is:
[0103] (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion;
[0104] (2) Add sodium citrate solution to the nano-montmorillonite dispersion, adjust the temperature to 50°C, keep warm in a water bath, stir while adding, and let stand for 20 minutes after the addition is completed in 30 minutes; the mixing ratio of nano-montmorillonite to deionized water is 10g:200mL;
[0105] The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1; the mass fraction of the sodium citrate solution is 10%;
[0106] (3) Continue to drop sodium bicarbonate solution into the nano-montmorillonite dispersion, adjust the temperature to 70°C, keep warm in a water bath, stir while dropping, and after the dropwise addition is completed for 40 minutes, let stand for 30 minutes to obtain a mixed solution; the mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2;
[0107] The mass fraction of sodium bicarbonate solution is 10%.
[0108] (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite; the centrifugal speed of the centrifugal treatment is 8000 r / min and the time is 15 min.
[0109] The preparation method of aloe vera compound extract is as follows:
[0110] Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material;
[0111] The aloe vera composite material and water were mixed in a mass ratio of 1:15, and then pulped for 30 minutes to obtain a composite slurry;
[0112] The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes and filtered to obtain a filtrate and a filter residue; the heating reflux extraction temperature was 72°C.
[0113] The filter residue is extracted twice again in the same way, the filtrates from the three extractions are combined, and 50% of the volume of the combined filtrates is added with anhydrous ethanol for alcohol precipitation. The mixture is placed at 4°C overnight and allowed to stand for 12 hours. The mixture is then centrifuged at 5000 r / min to obtain a precipitate, which is then vacuum dried to obtain the product; the vacuum drying temperature is 55°C and the time is 4 hours; the moisturizer is glycerin.
[0114] A method for preparing a sustained-release hydrogel of stem cell exosomes comprises the following steps:
[0115] S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water;
[0116] S2 divides the sterile water into 3 equal portions;
[0117] S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution;
[0118] S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution;
[0119] S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution;
[0120] S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
[0121] Example 4
[0122] A sustained-release hydrogel of stem cell exosomes:
[0123] Components Weight Sodium alginate 2.6 servings Pre-treated nano-montmorillonite 0.45 Aloe Vera Complex Extract 0.24 Hydroxypropyl-β-cyclodextrin 1.16 servings Gelatin powder 6 servings Moisturizer 2 servings Methacrylic Anhydride 3.4 servings Sterile water 28 servings
[0124] The preparation method of pretreated nano-montmorillonite is:
[0125] (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion;
[0126] (2) Add sodium citrate solution to the nano-montmorillonite dispersion, adjust the temperature to 50°C, keep warm in a water bath, stir while adding, and let stand for 20 minutes after the addition is completed in 30 minutes; the mixing ratio of nano-montmorillonite to deionized water is 10g:200mL;
[0127] The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1; the mass fraction of the sodium citrate solution is 10%;
[0128] (3) Continue to drop sodium bicarbonate solution into the nano-montmorillonite dispersion, adjust the temperature to 70°C, keep warm in a water bath, stir while dropping, and after the dropwise addition is completed for 40 minutes, let stand for 30 minutes to obtain a mixed solution; the mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2;
[0129] The mass fraction of sodium bicarbonate solution is 10%.
[0130] (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite; the centrifugal speed of the centrifugal treatment is 8000 r / min and the time is 15 min.
[0131] The preparation method of aloe vera compound extract is as follows:
[0132] Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material;
[0133] The aloe vera composite material and water were mixed in a mass ratio of 1:15, and then pulped for 30 minutes to obtain a composite slurry;
[0134] The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes and filtered to obtain a filtrate and a filter residue; the heating reflux extraction temperature was 72°C.
[0135] The filter residue is extracted twice again in the same way, the filtrates from the three extractions are combined, and 50% of the volume of the combined filtrates is added with anhydrous ethanol for alcohol precipitation. The mixture is placed at 4°C overnight and allowed to stand for 12 hours. The mixture is then centrifuged at 5000 r / min to obtain a precipitate, which is then vacuum dried to obtain the product; the vacuum drying temperature is 55°C and the time is 4 hours; the moisturizer is glycerin.
[0136] A method for preparing a sustained-release hydrogel of stem cell exosomes comprises the following steps:
[0137] S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water;
[0138] S2 divides the sterile water into 3 equal portions;
[0139] S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution;
[0140] S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution;
[0141] S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution;
[0142] S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
[0143] Example 5
[0144] A sustained-release hydrogel of stem cell exosomes:
[0145] Components Weight Sodium alginate 3 servings Pre-treated nano-montmorillonite 0.5 serving Aloe Vera Complex Extract 0.3 parts Hydroxypropyl-β-cyclodextrin 1.2 servings Gelatin powder 8 servings Moisturizer 2 servings Methacrylic Anhydride 3.5 servings Sterile water 30 servings
[0146] The preparation method of pretreated nano-montmorillonite is:
[0147] (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion;
[0148] (2) Add sodium citrate solution to the nano-montmorillonite dispersion, adjust the temperature to 50°C, keep warm in a water bath, stir while adding, and let stand for 20 minutes after the addition is completed in 30 minutes; the mixing ratio of nano-montmorillonite to deionized water is 10g:200mL;
[0149] The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1; the mass fraction of the sodium citrate solution is 10%;
[0150] (3) Continue to drop sodium bicarbonate solution into the nano-montmorillonite dispersion, adjust the temperature to 70°C, keep warm in a water bath, stir while dropping, and after the dropwise addition is completed for 40 minutes, let stand for 30 minutes to obtain a mixed solution; the mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2;
[0151] The mass fraction of sodium bicarbonate solution is 10%.
[0152] (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite; the centrifugal speed of the centrifugal treatment is 8000 r / min and the time is 15 min.
[0153] The preparation method of aloe vera compound extract is as follows:
[0154] Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material;
[0155] The aloe vera composite material and water were mixed in a mass ratio of 1:15, and then pulped for 30 minutes to obtain a composite slurry;
[0156] The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes and filtered to obtain a filtrate and a filter residue; the heating reflux extraction temperature was 72°C.
[0157] The filter residue is extracted twice again in the same way, the filtrates from the three extractions are combined, and 50% of the volume of the combined filtrates is added with anhydrous ethanol for alcohol precipitation. The mixture is placed at 4°C overnight and allowed to stand for 12 hours. The mixture is then centrifuged at 5000 r / min to obtain a precipitate, which is then vacuum dried to obtain the product; the vacuum drying temperature is 55°C and the time is 4 hours; the moisturizer is glycerin.
[0158] A method for preparing a sustained-release hydrogel of stem cell exosomes comprises the following steps:
[0159] S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water;
[0160] S2 divides the sterile water into 3 equal portions;
[0161] S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution;
[0162] S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution;
[0163] S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution;
[0164] S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
[0165] Comparative Example 1:
[0166] Based on Example 1, no pretreated nano-montmorillonite is added, and the rest of the technical solutions remain unchanged.
[0167] Comparative Example 2:
[0168] Based on Example 1, no aloe vera composite extract is added, and the rest of the technical solutions remain unchanged.
[0169] test:
[0170] The same exosomes (stem cell exosomes) were introduced into both the example and comparative example samples, and the exosome concentration was (180 μg / mL);
[0171] Establishment of mouse wound model:
[0172] SD rats were randomly divided into 8 groups. The hair on the back of the mice was shaved with a shaver, and the back was depilatory treated with a depilatory cream until there was no hair. A full-thickness skin defect with a diameter of 15 mm was prepared, and the day was recorded as day 0.
[0173] Then, the samples of the embodiment and the comparative example after the introduction of exosomes were coated on the wound surface (250 μL), respectively, once every 5 days, and the other group was coated with the same amount of the hydrogel of embodiment 1 without adding exosomes as the control group;
[0174] Table 1
[0175] Healing time / day Example 1 11 Example 2 9 Example 3 10 Example 4 11 Example 5 10 Comparative Example 1 13 Comparative Example 2 15 Control group 21
[0176] It can be seen from Table 1 that the hydrogel prepared by the present invention can improve the healing time of the wound after carrying exosomes.
[0177] Taking Example 1 as the basic sample, the percentage of exosome release at different times was compared with that of exosomes (concentration of 180 μg / mL):
[0178] Table 2
[0179] Time / h Release amount% 1 5 10 20 20 36 30 46 40 53 50 60 60 65 70 69
[0180] As can be seen from Table 2, the release rate of exosomes in the hydrogel was relatively fast in the initial stage. As time went on, the release rate of exosomes gradually decreased, and the sustained-release effect was obvious.
[0181] The above description is only a preferred embodiment of the present invention, but the present invention is not limited to the scope of implementation shown. Any changes made in accordance with the concept of the present invention, or modifications to equivalent embodiments with equivalent changes, which still do not exceed the spirit covered by the specification, should be within the protection scope of the present invention.
Claims
1. A sustained-release hydrogel of stem cell exosomes, characterized in that: The invention comprises the following ingredients by weight: 2-3 parts of sodium alginate, 0.3-0.5 parts of pretreated nano-montmorillonite, 0.1-0.3 parts of aloe compound extract, 1.1-1.2 parts of hydroxypropyl-β-cyclodextrin, 6-8 parts of gelatin powder, 1-2 parts of moisturizing agent, 3.3-3.5 parts of methacrylic anhydride and 20-30 parts of sterile water.
2. The sustained-release hydrogel of stem cell exosomes according to claim 1, characterized in that: The method for preparing the pretreated nano-montmorillonite is as follows: (1) First, nano-montmorillonite was added to deionized water and ultrasonically dispersed for 3 minutes to obtain a nano-montmorillonite dispersion; (2) adding sodium citrate solution dropwise to the nano-montmorillonite dispersion, adjusting the temperature to 50°C, keeping warm in a water bath, stirring while adding dropwise, and standing for 20-25 minutes after the addition is completed within 30 minutes; (3) Continue to dropwise add sodium bicarbonate solution to the nano-montmorillonite dispersion, adjust the temperature to 70° C., keep warm in a water bath, and stir while dropping. After the dropwise addition is completed within 40 minutes, let stand for 30-40 minutes to obtain a mixed solution; (4) The mixed solution obtained in step (3) is centrifuged, filtered, washed with water until neutral, and dried to constant weight to obtain pretreated nano-montmorillonite.
3. The sustained-release hydrogel of stem cell exosomes according to claim 2, characterized in that: The mixing ratio of the nano-montmorillonite and deionized water is 10-15 g: 200 mL; The mixing mass ratio of the nano-montmorillonite dispersion and the sodium citrate solution is 4:1-1.2; The mass fraction of the sodium citrate solution is 10%; The mass ratio of sodium citrate solution to sodium bicarbonate solution is 1:2; The mass fraction of sodium bicarbonate solution is 10%.
4. The sustained-release hydrogel of stem cell exosomes according to claim 2, characterized in that: The centrifugal treatment was performed at a centrifugal speed of 8000 r / min and for 15 min.
5. The sustained-release hydrogel of stem cell exosomes according to claim 1, characterized in that: The preparation method of the aloe composite extract is as follows: Firstly, aloe vera and wheat germ are mixed to obtain an aloe vera composite material; The aloe vera composite material and water are mixed in a mass ratio of 1:15-18, and then pulped for 30 minutes to obtain a composite slurry; The composite slurry was subjected to heating reflux extraction for 12 hours, and then centrifuged at a speed of 4500 r / min for 15 minutes, and filtered to obtain a filtrate and a filter residue; The filter residue is extracted twice more in the same way, the filtrates from the three times are combined, and 50% of the volume of the combined filtrate is added with anhydrous ethanol for alcohol precipitation. The product is placed at 4°C overnight for 12 hours, and then centrifuged at 5000 r / min to obtain the precipitate, which is then vacuum dried to obtain the product.
6. The sustained-release hydrogel of stem cell exosomes according to claim 5, characterized in that: The heating reflux extraction temperature is 72°C.
7. The sustained-release hydrogel of stem cell exosomes according to claim 5, characterized in that: The vacuum drying temperature is 55° C. and the time is 4 hours.
8. The sustained-release hydrogel of stem cell exosomes according to claim 1, characterized in that: The humectant is glycerin.
9. The method for preparing a sustained-release hydrogel of stem cell exosomes according to claim 1, characterized in that: The following steps are involved: S1 weighs the following parts by weight: sodium alginate, pretreated nano-montmorillonite, aloe vera composite extract, hydroxypropyl-β-cyclodextrin, gelatin powder, moisturizer, methacrylic anhydride, and sterile water; S2 divides the sterile water into 3 equal portions; S3: stirring and mixing sodium alginate, pretreated nano-montmorillonite and 1 part of sterile water for 10 minutes to obtain a first mixed solution; S4: stirring and mixing the aloe vera compound extract, hydroxypropyl-β-cyclodextrin, and 1 part of sterile water for 15 minutes to obtain a second mixed solution; S5: stirring and mixing the gelatin powder, the moisturizer and 1 part of sterile water for 10 minutes to obtain a third mixed solution; S6: The first mixed solution, the second mixed solution, and the third mixed solution are added together in sequence, and then stirred and mixed for 10 minutes, and then methacrylic anhydride is added, and the stirring and mixing is continued for 30 minutes. After ultrasonic dispersion for 5 minutes, a sustained-release hydrogel of stem cell exosomes is obtained.
Citation Information
Cited By
Exosome systems, products and methods
GB2705366A