Rapid extrusion forming device for plastic wood processing
By periodically extracting air and water-cooling bonding components to uniformly cool the components, the problems of unstable negative pressure and uneven cooling during the molding process of plastic wood are solved, and the quality and performance of plastic wood products are improved.
Patent Information
- Application Number
- CN202411481024.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-10-23
- Publication Date
- 2024-12-03
AI Technical Summary
The existing extrusion devices for plastic wood processing are difficult to maintain a constant negative pressure environment during the molding process of wood plastic wood, resulting in problems such as bubbles, burrs, faults, etc., and uneven cooling affects the quality and performance of the finished product.
The air pressure utilization component is used to periodically extract air to prevent inappropriate negative pressure, and the water-cooled fitting component achieves uniform cooling of the wood plastic material through rollers and bubble sleeves.
It improves the appearance quality and structural strength of finished plastic wood products, reduces economic burden, ensures the stability of physical and mechanical properties, and meets the requirements of precise dimensionality.
Smart Images

Figure CN119058047A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of plastic wood processing, in particular to a rapid extrusion molding device for plastic wood processing. Background Art
[0002] The core functions of the extrusion device for plastic wood processing include feeding, extrusion and cooling. At the same time, the device ensures that the plastic wood particles can enter the extruder continuously and stably through a special feeding mechanism. The extruder, as the core part, extrudes the plastic wood material in a molten state through the rotation of the screw and the heating of the barrel to form the desired shape. Finally, the extruded plastic wood material undergoes a cooling process to fix its shape and prevent deformation, thereby realizing efficient processing and production of plastic wood materials.
[0003] However, there are still some problems with the existing extrusion devices for plastic wood processing:
[0004] First, in the key link of plastic wood extrusion molding, the presence of air must be eliminated to prevent bubbles from appearing in the finished plastic wood, thereby affecting its quality and performance. In order to achieve this goal, the existing technology usually uses a vacuum pump to provide a negative pressure environment. However, since the material of each batch of raw materials is difficult to be completely consistent, it is extremely difficult to maintain a constant and suitable negative pressure environment in the actual production process;
[0005] Specifically, when the negative pressure is too large, it will interfere with the normal flow and molding process of the plastic wood material, resulting in burrs on the surface of the finished plastic wood, and even causing serious problems such as faults or fractures. These problems not only damage the appearance quality of the plastic wood finished product, but also greatly reduce its structural strength and service life. On the other hand, if the negative pressure is too small, the air in the plastic wood material cannot be effectively removed, resulting in bubbles in the finished product. These bubbles not only destroy the overall aesthetics of the plastic wood finished product, but also seriously affect its physical and mechanical properties.
[0006] In addition, as a key equipment for providing a negative pressure environment, the vacuum pump is expensive, which undoubtedly increases the initial investment cost for small plastic wood processing companies, and the subsequent maintenance and debugging work also brings a heavy economic burden to the company.
[0007] Secondly, the prior art generally uses a nozzle to spray water to cool the surface of the plastic wood, but this method has a significant problem, that is, the nozzle cannot cover the entire part of the plastic wood, but can only be limited to cooling a specific area, which means that other areas of the plastic wood, especially the bottom, cannot be fully cooled, resulting in uneven cooling. Even if an attempt is made to install a nozzle at the bottom, it can still only cover a part, and comprehensive uniform cooling cannot be achieved;
[0008] In order to solve this problem, the prior art also adopts a method of placing the plastic wood in a water tank for cooling. However, when the plastic wood is placed in the water tank, its bottom will contact the bottom of the water tank, and this contact will hinder the heat exchange between the bottom of the plastic wood and the water tank, thereby causing uneven cooling of the bottom. This uneven cooling will further affect the shrinkage rate of the plastic wood, causing different shrinkage degrees in different parts, thereby causing stress to be generated;
[0009] The existence of stress poses a serious threat to the quality and performance of plastic wood products. It will cause serious problems such as cracks, deformation and even breakage of plastic wood during subsequent processing or use. In addition, uneven cooling will also cause dimensional instability of plastic wood products, making it unable to meet precise dimensional requirements, thus affecting its use effect in practical applications.
[0010] To this end, the present invention provides a rapid extrusion molding device for plastic wood processing. Summary of the invention
[0011] The object of the present invention is to provide a rapid extrusion molding device for plastic wood processing to solve the problems raised in the above background technology.
[0012] To achieve the above-mentioned purpose, the present invention provides the following technical solutions: a rapid extrusion molding device for plastic wood processing, comprising a machine platform, a feeding unit is installed on the top of the machine platform, a molding die and a cooling unit are respectively installed and connected on the side of the machine platform away from the feeding unit, an air pressure utilization component for preventing inappropriate negative pressure from affecting the shaping of the plastic wood material is arranged on the top of the molding die, and a water cooling laminating component for improving the cooling effect of the plastic wood material is arranged inside the cooling unit;
[0013] The air pressure utilization component includes two air plug connecting rods that can remove the air inside the forming mold body through reciprocating motion;
[0014] The water-cooling laminating component comprises a plurality of rollers which can roll themselves to evenly cool the plastic-wood material, and the outer surface of each roller is sleeved with a bubble sleeve which can replenish water and cool the surface of the plastic-wood material.
[0015] Preferably, the air pressure utilization component also includes a plurality of transformer shells, which are linearly and equidistantly arranged and fixedly connected to the top of the molding mold, each of the transformer shells penetrates its upper and lower surfaces and extends to the inside of the molding mold to open an air hole, the tops of the two transformer shells located in the middle are fixedly connected to a supporting platform, the top of the supporting platform is fixedly connected to a driving motor, the output shaft of the driving motor penetrates the surface of the supporting platform, the top of the molding mold is rectangularly and equidistantly arranged and rotatably connected to a plurality of limit rods, the limit rods are arranged on both sides of the transformer shell located in the middle, and a hollow slide is slidably connected between the plurality of limit rods.
[0016] Preferably, a reciprocating groove is provided through the middle of the hollow slide, the bottom of the output shaft of the drive motor is fixedly connected to a crankshaft slidably connected to the inside of the reciprocating groove, each two transformer shells are slidably connected to an air plug connecting rod, the bottom of each air plug connecting rod is fixedly connected to the top of the hollow slide, a first one-way valve is installed on the bottom side of the inner wall of the transformer shell and at the center of the air hole, and a second one-way valve is installed on the top of the transformer shell and at the center of the air hole.
[0017] Preferably, a connecting shell is fixedly connected to the top of each transformer shell and concentric with the air hole, and a high-pressure pipe is fixedly connected to the top of the connecting shell. The high-pressure pipe has two input ends and one output end. The top of the molding mold is symmetrically fixedly connected to a clamping seat, and the output end of the high-pressure pipe is symmetrically fixedly connected to the inside of the clamping seat, and the output end of the high-pressure pipe extends to the inside of the cooling unit.
[0018] Preferably, the water-cooled fitting assembly also includes a water-cooled shell, which is fixedly connected to the inside of the cooling unit, and a number of fitting springs are symmetrically fixedly connected to both sides of the water-cooled shell, and the ends of the fitting springs away from the inner wall of the water-cooled shell are fixedly connected to rectangular blocks, each of the rollers is rotatably connected to the inside of every two rectangular blocks, and the bubble sleeves are provided with a number of water supply holes through the outer surface.
[0019] Preferably, when the second one-way valve and the first one-way valve are opened, their opening directions are both upward, the crankshaft is in a Z-shape with a right angle at the bend, the reciprocating groove is in a notch shape, the air plug connecting rod is in a mountain shape, and the middle part of the air plug connecting rod is protruding compared to the two sides, and the air plug connecting rod is oppositely arranged.
[0020] Preferably, the lower surface and side walls of the water-cooling shell are provided with flow grooves, the bubble sleeve is made of elastic material, and the distance between the rectangular block and the center line of the water-cooling shell gradually decreases from the side close to the forming mold body.
[0021] Preferably, an electric control panel is installed on the outer wall of the machine, and the electric control panel is electrically connected to the machine, the cooling unit and the driving motor.
[0022] Preferably, the feeding unit includes a feeding motor, a feeding shell, a feeding hopper, a spiral feeder and an electric heating tube.
[0023] Preferably, the cooling unit includes a water-cooling tank, a fan, a water pump and two electrically controlled valves.
[0024] Compared with the prior art, the present invention has the following beneficial effects:
[0025] 1. The hollow slide plate drives the air plug connecting rod to reciprocate under the restriction of the limit rod by rotating the crankshaft, so that the space inside the transformer shell is periodically in a negative pressure state, thereby realizing the periodic extraction of air inside the molding die. Due to the periodic extraction of air, there is no need to adjust the parameters additionally, and the problem of frequent adjustment of the working efficiency of the vacuum pump due to differences in raw materials is effectively solved, which greatly improves the stability and efficiency of the production process. At the same time, the air pressure utilization component helps to minimize the impact of inconsistent raw materials on the production process, thereby improving the appearance quality of the plastic wood finished product, improving its structural strength and service life, and ensuring the physical and mechanical properties of the plastic wood finished product. In addition, since there is no need to adjust the parameters, the air pressure utilization component effectively reduces the risk of damage to the plastic wood material caused by inappropriate negative pressure under the advantage of periodic extraction of air;
[0026] Compared with the existing technology, the negative pressure provided by the vacuum pump is difficult to maintain a constant and suitable environment, resulting in bubbles, burrs, faults or fractures in the finished plastic wood. The air pressure utilization component extracts air through periodic negative pressure, effectively avoiding these problems. In addition, the vacuum pump is expensive as a key equipment, which increases the economic burden of small plastic wood processing companies. The air pressure utilization component provides a more economical and efficient option, which helps to reduce the company's initial investment cost and subsequent maintenance and commissioning costs.
[0027] Among them: the air holes are staggered, so that the air holes far away from each other will not extract air at the same time, and further take into account the air extraction in the middle and the side. Under the premise of effectively extracting air, it avoids interfering with the normal flow and molding process of the plastic wood material;
[0028] Among them: the two air plug connecting rods are set in opposite directions, that is, when one air plug connecting rod is moving and extracting air, the other one will not extract air, so that the air plug connecting rod can evenly extract the air inside the plastic wood material, avoiding the flow and molding problems of the plastic wood material caused by excessive local negative pressure. At the same time, this opposite setting can also help reduce the impact of inconsistent raw materials on the production process;
[0029] Among them: the air extracted by the air plug connecting rod will eventually enter the cooling unit, and then the hot air and cold water react in the cooling unit to generate bubbles. Removing the bubbles can slightly flush and clean the surface of the plastic wood board, thereby removing burrs and other small defects on the surface of the plastic wood board, thereby reducing the subsequent tedious steps of cleaning the surface of the plastic wood board;
[0030] Among them: the high-pressure pipe is designed with two input ends and one output end, so that the hot air extracted from the transformer shell can be mixed in the high-pressure pipe and injected into the water, and the mixing of the hot air helps to prevent excessive heat loss, so that thermal energy can be used more efficiently.
[0031] 2. The plastic wood board is continuously pushed by the accumulation of raw materials, so that the plastic wood board slides on the roller surface, and the water absorption characteristics of the bubble sleeve are used to achieve uniform cooling of the bottom, top and sides of the plastic wood board. Due to the improved cooling efficiency, the water-cooled laminating component helps all parts of the plastic wood board to achieve uniform shrinkage, thereby reducing the generation of stress. This uniform cooling method not only improves the quality and performance of the plastic wood finished product, but also improves its dimensional stability, enabling it to meet precise dimensional requirements, thereby improving the use effect of the plastic wood finished product in practical applications;
[0032] Compared with the existing technology, the water-cooled laminating assembly avoids the problem of uneven cooling caused by incomplete coverage of the nozzle or contact with the bottom of the water tank. At the same time, this cooling method of the water-cooled laminating assembly not only simplifies the production process, but also helps to reduce production costs, providing a more efficient and economical solution for the production of plastic wood panels;
[0033] Among them: the fitting spring can adapt to the difference in expansion and contraction rates of different parts of the plastic wood board. During the production process, the expansion and contraction rates of various parts of the plastic wood board will be different due to different materials and molding conditions. The expansion and contraction of the spring drives the roller to contact the plastic wood board, providing a certain guide for its natural deformation;
[0034] Among them: the combination of the bubble sleeve and the water supply hole realizes the comprehensive and uniform cooling of the plastic wood board. When the bubble sleeve rotates with the roller, the side close to the plastic wood board is continuously compressed and stretched, thereby replenishing the water with lower temperature nearby to maintain the cooling effect. At the same time, when the bubble sleeve is compressed, the water inside the water supply hole will also fit with the plastic wood board, keeping it in a moist state, further enhancing the cooling effect;
[0035] Among them: the distance between the rectangular block and the center line of the water cooling shell gradually decreases from the side close to the forming mold body, and the shrinkage characteristics of the plastic wood board during the cooling process can be adapted through the constantly changing distance of the rectangular block. Since the plastic wood board will shrink during cooling, it is designed to be gradually close to the center line, which can better adapt to this shrinkage and avoid stress or deformation caused by uneven shrinkage;
[0036] Among them: through the resistance between the plastic wood board and the roller, the sliding friction in the prior art is converted into rolling friction. This conversion not only reduces the friction force, but also reduces the wear on the surface of the plastic wood board. At the same time, the rotation of the roller can also produce a slight grinding effect on the side wall of the plastic wood board. This grinding effect helps to remove minor defects and uneven parts on the surface of the plastic wood board, thereby reducing the steps and costs of subsequent processes. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 It is a frontal perspective schematic diagram of the main structure of the present invention;
[0038] Figure 2 It is a rear perspective schematic diagram of the main structure of the present invention;
[0039] Figure 3 For the present invention Figure 2 A magnified three-dimensional schematic diagram of the structure at center A;
[0040] Figure 4 For the present invention Figure 2 The enlarged three-dimensional schematic diagram of the structure at B in the middle;
[0041] Figure 5 It is a partially cutaway perspective schematic diagram of the air pressure utilization assembly of the present invention;
[0042] Figure 6 For the present invention Figure 5 The enlarged three-dimensional schematic diagram of the structure at C in the middle;
[0043] Figure 7 It is a cross-sectional perspective schematic diagram of the water-cooling bonding assembly of the present invention;
[0044] Figure 8 For the present invention Figure 7 The enlarged three-dimensional schematic diagram of the structure at D in the middle;
[0045] Fig. 9 It is a cross-sectional perspective schematic diagram of the air pressure utilization component of the present invention.
[0046] In the figure:
[0047] 11. Machine; 12. Loading unit; 13. Forming mold; 14. Cooling unit; 15. Electric control panel;
[0048] The air pressure utilization component includes: 21, transformer shell; 22, air hole; 23, bearing platform; 24, driving motor; 25, crankshaft; 26, limit rod; 27, hollow slide plate; 28, air plug connecting rod; 29, first one-way valve; 210, second one-way valve; 211, connecting shell; 212, high-pressure pipe;
[0049] The water-cooling fitting assembly includes: 31, water-cooling shell; 32, fitting spring; 33, rectangular block; 34, roller; 35, bubble sleeve; 36, water supply hole. DETAILED DESCRIPTION
[0050] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0051] See also Figures 1 to 9The present invention provides an embodiment: a rapid extrusion molding device for plastic wood processing, comprising a machine platform 11, a feeding unit 12 is installed on the top of the machine platform 11, a molding die 13 and a cooling unit 14 are respectively installed and connected on the side of the machine platform 11 away from the feeding unit 12, an air pressure utilization component for preventing inappropriate negative pressure from affecting the shaping of the plastic wood material is arranged on the top of the molding die 13, and a water cooling laminating component for improving the cooling effect of the plastic wood material is arranged inside the cooling unit 14;
[0052] The air pressure utilization assembly includes two air plug connecting rods 28 that can remove the air inside the molding die 13 through reciprocating motion;
[0053] The water-cooling laminating component includes a plurality of rollers 34 that can roll to evenly cool the plastic wood material. The outer surface of each roller 34 is sleeved with a bubble sleeve 35 that can replenish water and cool the surface of the plastic wood material.
[0054] The air pressure utilization component also includes a plurality of transformer shells 21, which are linearly and equidistantly arranged and fixedly connected to the top of the molding mold 13. Each transformer shell 21 penetrates its upper and lower surfaces and extends to the inside of the molding mold 13 to open an air hole 22. The tops of the two transformer shells 21 in the middle are fixedly connected to a supporting platform 23, and the tops of the supporting platforms 23 are fixedly connected to a driving motor 24. The output shaft of the driving motor 24 penetrates the surface of the supporting platform 23. The top of the molding mold 13 is rectangularly and equidistantly arranged and rotatably connected to a plurality of limit rods 26. The limit rods 26 are arranged on both sides of the transformer shell 21 in the middle, and a hollow slide 27 is slidably connected between the plurality of limit rods 26.
[0055] A reciprocating groove is provided through the middle of the hollow slide 27, and a crankshaft 25 slidably connected to the inside of the reciprocating groove is fixedly connected to the bottom of the output shaft of the driving motor 24. An air plug connecting rod 28 is slidably connected to the inside of each two transformer shells 21, and the bottom of each air plug connecting rod 28 is fixedly connected to the top of the hollow slide 27. A first one-way valve 29 is installed on the bottom side of the inner wall of the transformer shell 21 and at the center of the air hole 22, and a second one-way valve 210 is installed on the top of the transformer shell 21 and at the center of the air hole 22.
[0056] A connecting shell 211 is fixedly connected to the top of each transformer shell 21 and concentric with the air hole 22. A high-pressure pipe 212 is fixedly connected to the top of the connecting shell 211. The high-pressure pipe 212 has two input ends and one output end. A clamping seat is symmetrically fixedly connected to the top of the molding mold 13. The output end of the high-pressure pipe 212 is symmetrically fixedly connected to the inside of the clamping seat, and the output end of the high-pressure pipe 212 extends to the inside of the cooling unit 14.
[0057] The water-cooling fitting assembly also includes a water-cooling shell 31, which is fixedly connected to the inside of the cooling unit 14. A number of fitting springs 32 are symmetrically fixedly connected to both sides of the water-cooling shell 31. The ends of the fitting springs 32 away from the inner wall of the water-cooling shell 31 are fixedly connected to rectangular blocks 33. Each roller 34 is rotatably connected to the inside of every two rectangular blocks 33, and the bubble sleeves 35 are penetrated through the outer surface to open a number of water replenishment holes 36.
[0058] When the second one-way valve 210 and the first one-way valve 29 are opened, their opening directions are both upward, the crankshaft 25 is in a Z-shape with a right angle at the bend, the reciprocating groove is in a notch shape, the air plug connecting rod 28 is in a mountain shape, and the middle part of the air plug connecting rod 28 is protruding compared to the two sides, and the air plug connecting rod 28 is oppositely arranged.
[0059] The lower surface and side wall of the water-cooled shell 31 are provided with flow grooves. The bubble sleeve 35 is made of elastic material, specifically polyurethane foam material. The rectangular block 33 starts from the side close to the molding mold 13, and its distance from the center line of the water-cooled shell 31 gradually decreases.
[0060] An electric control panel 15 is installed on the outer wall of the machine platform 11 . The electric control panel 15 is electrically connected to the machine platform 11 , the cooling unit 14 and the driving motor 24 .
[0061] The feeding unit 12 includes a feeding motor, a feeding shell, a feeding hopper, a spiral feeder and an electric heating tube. The feeding motor is fixedly connected to the top of the machine 11, the feeding shell is fixedly connected to the top of the machine 11, the feeding hopper and the top of the feeding shell are interconnected, the spiral feeder is fixedly connected to the output shaft of the feeding motor, and the spiral feeder is rotatably connected to the inside of the feeding shell, and the electric heating tube is installed on the outer surface of the feeding shell.
[0062] The cooling unit 14 includes a water-cooling tank body, a fan, a water pump and two electrically controlled valves. The water-cooling tank body is fixedly connected to the top of the side of the machine 11 away from the loading unit 12. The fan is installed at one end of the water-cooling tank body away from the forming mold 13. The water pump is installed on the outside of the water-cooling tank body, and the input and output ends of the water pump are interconnected with the water-cooling tank body. One of the electrically controlled valves is installed at the connection between the water-cooling tank body and the forming mold 13, and the other electrically controlled valve is installed on the side of the water-cooling tank body away from the forming mold 13.
[0063] The working principle of the present invention in combination with the above is as follows:
[0064] The following is the initial state: the electrically controlled valves are all in the closed state, the water-cooling tank is filled with water, the second one-way valve 210 and the first one-way valve 29 are both in the closed state, the fitting spring 32 is not compressed, the bubble sleeve 35 is not compressed, and the bubble sleeve 35 absorbs water and expands, and the air plug connecting rod 28 is located in the middle of the transformer shell 21.
[0065] The following are the specific steps of the work:
[0066] Among them, the plastic wood material is melt-treated:
[0067] like Figure 1 and Figure 2 As shown, the operator first manipulates the electric control panel 15 and causes the electric control panel 15 to electrically control the feeding unit 12 to start. At this time, the output shaft of the feeding motor starts to rotate and drives the spiral feeder fixedly connected thereto to rotate together.
[0068] Then the operator pours the plastic wood raw materials into the loading hopper, and the raw materials naturally fall into the loading shell under the action of gravity. As the spiral feeder rotates, the spiral feeder pushes the raw materials forward.
[0069] At the same time, when the feeding unit 12 is started, the electric heating tube begins to heat up and transfers the heat to the feeding shell closely attached thereto, thereby heating the plastic wood raw material in the shell. As the raw material continues to move forward under the push of the spiral feeder, the plastic wood raw material is gradually exposed to higher temperatures and begins to undergo a transition from a solid state to a molten state.
[0070] Among them, the plastic wood material is extruded and formed:
[0071] like Figure 1 and Figure 2 As shown, as the molten plastic wood raw materials are continuously transported by subsequent raw materials, they are pushed forward. During this process, the molten raw materials are affected by the pushing force, the restriction of the inner wall of the molding mold 13 and the lower temperature inside the molding mold 13. The synergistic effect of these factors causes the molten plastic wood material to gradually cool and shape.
[0072] Among them, prevent the presence of air from affecting the forming of plastic wood panels:
[0073] like Figure 2 and Figure 3 , Figure 5 and Figure 6 as well as Fig. 9 As shown, in the above process, the operator also needs to operate the electric control panel 15 and make the electric control panel 15 electrically control the drive motor 24 to start.
[0074] At this time, the output shaft of the drive motor 24 starts to rotate and drives the crankshaft 25 fixedly connected thereto to rotate together. Due to the rotation of the crankshaft 25, the crankshaft 25 will cause the hollow slide 27 to have a tendency to rotate synchronously. However, the hollow slide 27 is restricted by a number of limit rods 26 and can only slide therebetween. In order to comply with the tendency of the crankshaft 25 to rotate, the rotation of the crankshaft 25 will drive the hollow slide 27 to slide back and forth between the limit rods 26. At the same time, the reciprocating sliding of the hollow slide 27 also drives the synchronous movement of the gas plug connecting rod 28 fixedly connected to the top of the hollow slide 27.
[0075] The movement of the air plug connecting rod 28 will cause the space inside two of the transformer shells 21 to increase, while the space inside the other two transformer shells 21 will decrease. When the space inside two of the transformer shells 21 increases, the number of internal air molecules decreases relatively, thereby causing the air pressure to drop and generating negative pressure. Under the action of the negative pressure, the air inside the molding mold 13 is pulled, and based on the chimney effect, the hot air flow will move upward. At this time, the air inside the molding mold 13 passes through the air hole 22 and pushes the first one-way valve 29 to open it, and enters the two transformer shells 21 with increased internal space to balance the air pressure.
[0076] The transformer shell 21 with a reduced internal space will generate high pressure. This is because the reduction in space leads to a relative increase in the number of air molecules inside, which in turn causes the air pressure to rise. In order to balance the air pressure, the air inside the transformer shell 21 with a reduced internal space will enter the high-pressure pipe 212 through the second one-way valve 210 and the connecting shell 211. Since the high-pressure pipe 212 has two input ends and one output end, its design allows the air from different transformer shells 21 to be mixed and output, further enhancing the air pressure balancing effect.
[0077] As the crankshaft 25 continues to rotate, the transformer shell 21, whose space is constantly reduced and increased, will repeat the action of suction and exhaust. Since the air holes 22 performing the same action are staggered, air is sucked from the middle and the sides, ensuring the uniform removal of air from the inside of the molding mold 13. At the same time, since every two air holes 22 are periodically suctioned and two groups are provided, the efficiency of air extraction can be guaranteed. In addition, the periodic suction method will not affect the molding process of the plastic wood board, that is, it will not cause burrs or breakage. This is because the suction action is periodic and the suction force is moderate, which will not cause excessive disturbance to the plastic wood board being formed.
[0078] In such an environment, the air inside the molding mold 13 is continuously reduced, which helps the plastic wood board to be shaped during the cooling process. Reducing air flow can reduce temperature fluctuations on the surface of the plastic wood board, thereby reducing deformation or cracks caused by uneven temperature. At the same time, lower air flow can also reduce the evaporation of moisture on the surface of the plastic wood board, helping to maintain its moist state and further promoting uniform cooling and shaping.
[0079] Among them, the cooling and shaping of plastic wood board:
[0080] like Figure 2 and Figure 4 as well as Figure 7 and Figure 8 As shown, when the plastic wood board is being formed and is about to pass through the forming die 13 , the operator manipulates the electric control panel 15 and enables the electric control panel 15 to electrically control the cooling unit 14 to start.
[0081] At this time, the electric control valve closest to the forming mold 13 is opened, allowing the formed and continuous plastic wood board to continue to be pushed into the water-cooling tank by the subsequent raw materials.
[0082] As the cooling unit 14 is started, the water pump starts to work, circulating the water inside the water-cooling tank, and the fan also starts to rotate, generating cold air to further cool the plastic wood board.
[0083] When the plastic wood board enters the water-cooling tank, it will first contact the roller 34 and the bubble sleeve 35. Since the roller 34 is connected to the fitting spring 32 through the rectangular block 33, and due to this connection method, when the plastic wood board contacts the roller 34 and the bubble sleeve 35, the fitting spring 32 will be elastically compressed, and then the elastically moving roller 34 can not only limit the plastic wood board to prevent it from excessive deformation, but also ensure the stability of the plastic wood board during the cooling process. At the same time, since the water-cooling shell 31 and the water-cooling tank are interconnected, the upper and lower surfaces of the plastic wood board will contact the cooling water, thereby achieving a rapid and uniform cooling effect.
[0084] The bubble sleeve 35, as a component sleeved on the outer surface of the roller 34, has the characteristic of absorbing water and expanding. Therefore, when the plastic wood board contacts the bubble sleeve 35 and pushes it to rotate, the water inside the bubble sleeve 35 will be discharged. As the roller 34 and the bubble sleeve 35 continue to rotate, the initial side of the bubble sleeve 35 in contact with the plastic wood board will absorb water again because it is no longer pushed by the plastic wood board. The cold water here ensures the uniformity of cooling and enables the bubble sleeve 35 to always fit with the surface of the plastic wood board, providing a continuous cooling effect.
[0085] In addition, during the contact between the plastic wood board and the bubble sleeve 35, the water inside the water supply hole 36 is always in contact with the plastic wood board, further enhancing the cooling effect. Through the elastic limitation of the plastic wood board and the water absorption and drainage functions of the bubble sleeve 35, combined with the design of the water supply hole 36 to keep the water in contact with the side wall of the plastic wood board, the stability of the plastic wood board during the cooling process and the uniformity of the cooling effect are ensured.
[0086] In addition, since the rectangular block 33 starts from the side close to the forming mold 13, its distance from the center line of the water-cooling shell 31 gradually decreases, and then the plastic wood board can always fit with the roller 34 due to the shrinkage effect during the continuous cooling process. At the same time, the side wall of the plastic wood will become smoother due to continuous friction as the plastic wood board itself is continuously pushed by the subsequent raw materials and the roller 34 and the bubble sleeve 35 rotate. This not only improves the quality of the plastic wood board, but also reduces the grinding and finishing work in the subsequent processing steps.
[0087] At the same time, in the above steps, the hot air discharged into the high-pressure pipe 212 will be mixed at the output end and discharged into the water-cooling tank. When the hot air contacts the cold water, bubbles will be generated. These bubbles will generate a slight impact force when they burst. Since the plastic wood board has been water-cooled at this time, the impact force of the bubbles will not affect the appearance of the plastic wood. On the contrary, this tiny impact force can also flush the surface of the plastic wood board, reduce subsequent cleaning steps, and further improve production efficiency.
[0088] Finally, when the formed plastic wood board is about to pass through the water cooling tank, the operator electrically controls the electric control valve away from the machine 11 to open through the electric control panel 15, so that the evenly cooled and formed plastic wood board can continue to be transmitted from the water cooling tank.
[0089] At this time, the operator can carry out subsequent processing work on the plastic wood board.
[0090] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the presence of other identical elements in the process, method, article or device including the elements.
[0091] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A rapid extrusion molding device for plastic wood processing, comprising a machine platform (11), a feeding unit (12) is installed on the top of the machine platform (11), and a molding die (13) and a cooling unit (14) are respectively installed and connected on the side of the machine platform (11) away from the feeding unit (12), characterized in that: The top of the molding die (13) is provided with an air pressure utilization component for preventing inappropriate negative pressure from affecting the shaping of the plastic wood material, and the interior of the cooling unit (14) is provided with a water cooling laminating component for improving the cooling effect of the plastic wood material; The air pressure utilization component comprises two air plug connecting rods (28) which can discharge the air inside the forming mold (13) through reciprocating motion; The water-cooling laminating component comprises a plurality of rollers (34) which can roll themselves to evenly cool the plastic-wood material, and the outer surface of each roller (34) is sleeved with a bubble sleeve (35) which can replenish water and cool the surface of the plastic-wood material.
2. A rapid extrusion molding device for plastic wood processing according to claim 1, characterized in that: The air pressure utilization component also includes a plurality of transformer shells (21), which are all linearly and equidistantly arranged and fixedly connected to the top of the molding mold (13), and each transformer shell (21) is provided with an air hole (22) penetrating its upper and lower surfaces and extending to the inside of the molding mold (13). The tops of the two transformer shells (21) located in the middle are fixedly connected to a bearing platform (23), and the tops of the bearing platforms (23) are fixedly connected to a driving motor (24), and the output shaft of the driving motor (24) penetrates the surface of the bearing platform (23). The top of the molding mold (13) is rotatably connected to a plurality of limit rods (26) arranged equidistantly in a rectangular shape, and the limit rods (26) are all arranged on both sides of the transformer shell (21) located in the middle, and a hollow slide plate (27) is slidably connected between the plurality of limit rods (26).
3. A rapid extrusion molding device for plastic wood processing according to claim 2, characterized in that: A reciprocating groove is formed through the middle of the hollow slide plate (27); a crankshaft (25) slidably connected to the inside of the reciprocating groove is fixedly connected to the bottom of the output shaft of the drive motor (24); a gas plug connecting rod (28) is slidably connected to the inside of each of the two transformer shells (21); the bottom of each gas plug connecting rod (28) is fixedly connected to the top of the hollow slide plate (27); a first one-way valve (29) is installed on the bottom side of the inner wall of the transformer shell (21) and at the center of the air hole (22); and a second one-way valve (210) is installed on the top of the transformer shell (21) and at the center of the air hole (22).
4. A rapid extrusion molding device for plastic wood processing according to claim 3, characterized in that: A connecting shell (211) is fixedly connected to the top of each transformer shell (21) and concentric with the air hole (22); a high-pressure pipe (212) is fixedly connected to the top of each connecting shell (211); the high-pressure pipe (212) has two input ends and one output end; a clamping seat is symmetrically fixedly connected to the top of the molding die (13); the output end of the high-pressure pipe (212) is symmetrically fixedly connected to the inside of the clamping seat, and the output end of the high-pressure pipe (212) extends to the inside of the cooling unit (14).
5. The rapid extrusion molding device for wood plastic processing according to claim 1, characterized in that: The water-cooling fitting assembly also includes a water-cooling shell (31), the water-cooling shell (31) is fixedly connected to the inside of the cooling unit (14), and a plurality of fitting springs (32) are symmetrically fixedly connected to both sides of the water-cooling shell (31), and one end of the fitting spring (32) away from the inner wall of the water-cooling shell (31) is fixedly connected to a rectangular block (33), each of the rollers (34) is rotatably connected to the inside of each two rectangular blocks (33), and the bubble sleeves (35) are each provided with a plurality of water replenishing holes (36) through the outer surface.
6. A rapid extrusion molding device for plastic wood processing according to claim 3, characterized in that: When the second one-way valve (210) and the first one-way valve (29) are opened, their opening directions are both upward, the crankshaft (25) is in a Z-shape with a right angle at the bend, the reciprocating groove is in a slot shape, the gas plug connecting rod (28) is in a mountain shape, and the middle part of the gas plug connecting rod (28) is in a convex state compared to the two sides, and the gas plug connecting rod (28) is arranged oppositely.
7. A rapid extrusion molding device for wood plastic processing according to claim 5, characterized in that: The lower surface and side wall of the water-cooling shell (31) are both provided with flow grooves, the bubble sleeve (35) is made of elastic material, and the distance between the rectangular block (33) and the center line of the water-cooling shell (31) gradually decreases from the side close to the forming mold (13).
8. The rapid extrusion molding device for plastic wood processing according to claim 1 is characterized in that: An electric control panel (15) is installed on the outer wall of the machine platform (11), and the electric control panel (15) is electrically connected to the machine platform (11), the cooling unit (14) and the driving motor (24).