Heat-preservation sintered brick prepared from municipal sludge and production process of heat-preservation sintered brick
By using raw materials such as urban sludge and specific processes to manufacture thermal insulation sintered bricks, the problems of low load strength and strong water absorption are solved in traditional bricks, density and water resistance are improved, and the durability of the building is extended.
Patent Information
- Application Number
- CN202411187524.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-28
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The low load-bearing strength and strong water absorption of traditional insulation sintered bricks lead to a decrease in strength after water absorption, which may cause moisture problems in the walls and affect the long-term durability of the building.
Using raw materials such as urban sludge, clay, fine fly ash, expanded perlite powder, slag, foaming agent, modifier, flux and silicone coating, through stirring, crushing, compacting and high-temperature firing Manufacture insulation sintered bricks and apply siloxane coating on the surface to form a waterproof film to reduce moisture penetration.
It improves the density and load-bearing strength of the brick body, reduces water absorption, enhances water resistance and durability, and extends the service life of the building.
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of building materials, in particular to a thermal insulation sintered brick utilizing urban sewage sludge and a production process thereof. Background Art
[0002] Thermal insulation fired bricks are mainly used in the exterior walls, interior walls and floors of buildings. Their main function is to provide excellent thermal insulation, reduce heat loss and improve the energy efficiency of buildings. Compared with ordinary fired bricks, thermal insulation fired bricks have better thermal insulation and lower thermal conductivity. Using sludge to make fired bricks is an effective way to treat sludge, which can transform sludge into useful building materials. This process not only helps to reduce the cost of sludge treatment, but also can use it as a raw material for building bricks.
[0003] Sludge insulation sintered brick is a thermal insulation brick made by sintering process using sludge as one of the main raw materials and combining it with other ingredients. This brick not only has the characteristics of thermal insulation, but also can effectively process and utilize sludge, with the dual advantages of environmental protection and resource conservation.
[0004] At present, the traditional thermal insulation fired bricks have many pores inside to improve the thermal insulation performance, which will cause the strength of thermal insulation fired bricks to be lower than that of ordinary fired bricks. At the same time, the porous structure of thermal insulation fired bricks makes them more absorbent. This will cause the strength of the brick body to decrease after absorbing water, and it may also cause wall moisture problems, affecting the long-term durability of the building. Summary of the invention
[0005] In view of the deficiencies of the prior art, the present invention provides a thermal insulation sintered brick using municipal sewage sludge and a production process thereof, which solves the problems of low bearing strength and strong water absorption.
[0006] To achieve the above objectives, the present invention is implemented through the following technical scheme: a thermal insulation sintered brick using urban sludge, the following raw materials in parts by weight: 50-80 parts of urban sludge, 50-80 parts of clay, 10-15 parts of fine fly ash, 5-10 parts of expanded perlite powder, 10-15 parts of slag, 1-3 parts of foaming agent, 1-3 parts of modifier, 1-3 parts of flux, 2-5 parts of refractory additive and 1-3 parts of silicone coating.
[0007] Preferably, the foaming agent includes any one or more combinations of sodium bicarbonate, magnesium hydroxide, polystyrene particles and wood powder.
[0008] Preferably, the modifier includes any one or more combinations of glass fiber, carbon fiber, polyvinyl alcohol, polyacrylate, sodium chloride and calcium chloride.
[0009] Preferably, the flux includes any one or more combinations of sodium fluoride, boric acid, sodium aluminate, sodium nitrate and calcium oxide.
[0010] Preferably, the refractory additive includes any one or more combinations of high-bauxite, corundum, calcium oxide, ceramic fiber and zircon.
[0011] A production process of thermal insulation sintered bricks using municipal sludge comprises the following steps:
[0012] S1. Harmless treatment of sludge
[0013] First, the municipal sludge is put into a treatment tank with a stirring mechanism, and phosphate is added to the treatment tank. The stirring mechanism is started to allow the phosphate to fully contact the sludge, and the heavy metals in the sludge are converted into insoluble precipitates. After the reaction is completed, the precipitates are separated from the liquid phase by sedimentation; the liquid phase sludge after preliminary treatment is put into a belt filter press for mechanical dehydration treatment to remove the water in the sludge, and then the sludge and ion exchange resin are put into a stirring tank to mix the ion exchange resin with the sludge, so that the resin is fully in contact with the heavy metal ions in the sludge to continue to adsorb and remove the heavy metal ions in the sludge, and the treated sludge is separated from the resin and put into a drying device to further reduce the water content in the sludge by hot air drying;
[0014] S2. Raw material mixing
[0015] The dried sludge is put into a pulverizer and crushed into particles, and then the sludge particles, clay, fine fly ash, expanded perlite powder and slag are put into a mixing device, and mixed at a speed of 200-500r / min, and during the mixing process, a foaming agent, a modifier, a flux, a refractory additive and siloxane are added to the mixing device in sequence, and the mixing is continued until the mixture is completely mixed;
[0016] S3. Compacting
[0017] Put the mixed raw materials into the mold first, and then place the mold neatly on the vibration equipment to compact the raw materials in the mold and reduce the gaps; then use the molding equipment to press and form the bricks;
[0018] S4. Firing
[0019] First, the formed bricks are placed in a drying box at 80-100°C for preliminary drying, and then the dried bricks are stacked in a high-temperature kiln, and the high-temperature kiln is vacuumed and fired at 900-1100°C for 12-24 hours. After the firing is completed, the sintered bricks are slowly cooled in the kiln;
[0020] S5. Surface treatment
[0021] After cooling, use a brushing device to apply the silicone coating on the surface of the sintered brick. After the first application, dry it in the sun until it is completely dry. Repeat the above operation to apply two to three layers to obtain a formed thermal insulation sintered brick.
[0022] The present invention provides a thermal insulation sintered brick using urban sewage sludge and its production process.
[0023] Beneficial effects:
[0024] 1. The present invention first reduces the pores generated during the sintering process by reducing the proportion of expanded perlite powder in the raw materials, and more effectively reduces the pores inside the brick body and increases the density of the brick body by first vibrating and then pressing under high pressure during compaction and molding; secondly, the glass fiber and carbon fiber used in the modifier can improve the strength and toughness of the brick, and further improve the bearing strength of the formed sintered brick.
[0025] 2. The present invention forms a waterproof film by applying a silicone coating on the surface after firing, which can also reduce the penetration of water to enhance the water resistance and durability of the brick, and can also reduce its water absorption while increasing the density of the brick. DETAILED DESCRIPTION
[0026] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0027] Embodiment 1:
[0028] An embodiment of the present invention provides a thermal insulation sintered brick using municipal sludge, comprising the following raw materials in parts by weight: 50 parts of municipal sludge, 50 parts of clay, 10 parts of fine fly ash, 5 parts of expanded perlite powder, 10 parts of slag, 1 part of foaming agent, 1 part of modifier, 1 part of flux, 2 parts of refractory additives and 1 part of siloxane coating.
[0029] The foaming agent includes any one or more combinations of sodium bicarbonate, magnesium hydroxide, polystyrene particles and wood powder.
[0030] The modifier includes any one or more combinations of glass fiber, carbon fiber, polyvinyl alcohol, polyacrylate, sodium chloride and calcium chloride. Glass fiber and carbon fiber can improve the strength and toughness of bricks; polyvinyl alcohol and polyacrylate can improve the water resistance of bricks; sodium chloride and calcium chloride can reduce the freezing point of bricks and increase the freeze-thaw resistance and cold resistance.
[0031] The flux includes any one or more combinations of sodium fluoride, boric acid, sodium aluminate, sodium nitrate and calcium oxide. The use of the flux can effectively optimize the sintering process and improve the final quality of the brick body, and can reduce the sintering temperature and improve the melting performance during the sintering process.
[0032] Refractory additives include any one or more combinations of high-bauxite, corundum, calcium oxide, ceramic fiber and zircon. High-bauxite and corundum can improve the high temperature resistance and wear resistance of the brick; ceramic fiber can improve the fire resistance and thermal insulation performance of the brick, while enhancing the strength and stability of its structure; calcium oxide can enhance the fire resistance and corrosion resistance of the brick and improve its high temperature stability.
[0033] The porosity generated during the sintering process is reduced by reducing the proportion of expanded perlite powder in the raw materials, and the porosity inside the brick body is more effectively reduced and the density of the brick body is increased by first vibrating and then pressing under high pressure during compaction. Secondly, the glass fiber and carbon fiber used in the modifier can improve the strength and toughness of the brick, and further improve the bearing strength of the formed sintered brick.
[0034] A production process of thermal insulation sintered bricks using municipal sludge comprises the following steps:
[0035] S1. Harmless treatment of sludge
[0036] First, the municipal sludge is put into a treatment tank with a stirring mechanism, and phosphate is added into the treatment tank. The stirring mechanism is started to allow the phosphate to fully contact the sludge, and the heavy metals in the sludge are converted into insoluble precipitates. After the reaction is completed, the precipitates are separated from the liquid phase by sedimentation; the liquid phase sludge after preliminary treatment is put into a belt filter press for mechanical dehydration treatment to remove the moisture in the sludge, and then the sludge and ion exchange resin are put into a stirring tank to mix the ion exchange resin with the sludge so that the resin and the heavy metal ions in the sludge are fully contacted to continue to adsorb and remove the heavy metal ions in the sludge; the treated sludge is separated from the resin and put into a drying equipment to further reduce the moisture in the sludge by hot air drying; the heavy metal ions in the sludge are adsorbed and removed by phosphate and ion exchange resin to avoid the impact of heavy metal ions on the environment and human health.
[0037] S2. Raw material mixing
[0038] The dried sludge is put into a pulverizer and crushed into particles. The sludge particles, clay, fine fly ash, expanded perlite powder and slag are then put into a mixing device and stirred at a speed of 200 r / min. During the stirring process, a foaming agent, a modifier, a flux, a refractory additive and siloxane are sequentially added into the mixing device and the stirring is continued until the mixture is completely mixed.
[0039] S3. Compacting
[0040] Put the mixed raw materials into the mold first, and then place the mold neatly on the vibration equipment to compact the raw materials in the mold and reduce the gaps; then use the molding equipment to press and form the bricks;
[0041] S4. Firing
[0042] First, the formed bricks are placed in a drying box at 80°C for preliminary drying, and then the dried bricks are stacked in a high-temperature kiln, which is vacuumed and fired at 900°C for 12 hours. After firing, the sintered bricks are slowly cooled in the kiln;
[0043] S5. Surface treatment
[0044] After cooling, use a brushing device to apply the silicone coating on the surface of the sintered brick. After the first application, dry it in the sun until it is completely dry. Repeat the above operation to apply two to three layers to obtain a formed thermal insulation sintered brick.
[0045] Embodiment 2:
[0046] An embodiment of the present invention provides a thermal insulation sintered brick using municipal sludge, comprising the following raw materials in parts by weight: 80 parts of municipal sludge, 80 parts of clay, 15 parts of fine fly ash, 10 parts of expanded perlite powder, 15 parts of slag, 3 parts of foaming agent, 3 parts of modifier, 3 parts of flux, 5 parts of refractory additive and 3 parts of siloxane coating.
[0047] The foaming agent includes any one or more combinations of sodium bicarbonate, magnesium hydroxide, polystyrene particles and wood powder.
[0048] The modifier includes any one or more combinations of glass fiber, carbon fiber, polyvinyl alcohol, polyacrylate, sodium chloride and calcium chloride. Glass fiber and carbon fiber can improve the strength and toughness of bricks; polyvinyl alcohol and polyacrylate can improve the water resistance of bricks; sodium chloride and calcium chloride can reduce the freezing point of bricks and increase the freeze-thaw resistance and cold resistance.
[0049] The flux includes any one or more combinations of sodium fluoride, boric acid, sodium aluminate, sodium nitrate and calcium oxide. The use of the flux can effectively optimize the sintering process and improve the final quality of the brick body, and can reduce the sintering temperature and improve the melting performance during the sintering process.
[0050] Refractory additives include any one or more combinations of high-bauxite, corundum, calcium oxide, ceramic fiber and zircon. High-bauxite and corundum can improve the high temperature resistance and wear resistance of the brick; ceramic fiber can improve the fire resistance and thermal insulation performance of the brick, while enhancing the strength and stability of its structure; calcium oxide can enhance the fire resistance and corrosion resistance of the brick and improve its high temperature stability.
[0051] The porosity generated during the sintering process is reduced by reducing the proportion of expanded perlite powder in the raw materials, and the porosity inside the brick body is more effectively reduced and the density of the brick body is increased by first vibrating and then pressing under high pressure during compaction. Secondly, the glass fiber and carbon fiber used in the modifier can improve the strength and toughness of the brick, and further improve the bearing strength of the formed sintered brick.
[0052] A production process of thermal insulation sintered bricks using municipal sludge comprises the following steps:
[0053] S1. Harmless treatment of sludge
[0054] First, the municipal sludge is put into a treatment tank with a stirring mechanism, and phosphate is added into the treatment tank. The stirring mechanism is started to allow the phosphate to fully contact the sludge, and the heavy metals in the sludge are converted into insoluble precipitates. After the reaction is completed, the precipitates are separated from the liquid phase by sedimentation; the liquid phase sludge after preliminary treatment is put into a belt filter press for mechanical dehydration treatment to remove the moisture in the sludge, and then the sludge and ion exchange resin are put into a stirring tank to mix the ion exchange resin with the sludge so that the resin and the heavy metal ions in the sludge are fully contacted to continue to adsorb and remove the heavy metal ions in the sludge; the treated sludge is separated from the resin and put into a drying equipment to further reduce the moisture in the sludge by hot air drying; the heavy metal ions in the sludge are adsorbed and removed by phosphate and ion exchange resin to avoid the impact of heavy metal ions on the environment and human health.
[0055] S2. Raw material mixing
[0056] The dried sludge is put into a pulverizer and crushed into particles. The sludge particles, clay, fine fly ash, expanded perlite powder and slag are then put into a mixing device and stirred at a speed of 500 r / min. During the stirring process, a foaming agent, a modifier, a flux, a refractory additive and siloxane are sequentially added into the mixing device and the stirring is continued until the mixture is completely mixed.
[0057] S3. Compacting
[0058] Put the mixed raw materials into the mold first, and then place the mold neatly on the vibration equipment to compact the raw materials in the mold and reduce the gaps; then use the molding equipment to press and form the bricks;
[0059] S4. Firing
[0060] First, the formed bricks are placed in a drying box at 100°C for preliminary drying. The dried bricks are then stacked in a high-temperature kiln, which is then vacuumed and fired at 1100°C for 24 hours. After firing, the sintered bricks are slowly cooled in the kiln.
[0061] S5. Surface treatment
[0062] After cooling, use a brushing device to apply the silicone coating on the surface of the sintered brick. After the first application, dry it in the sun until it is completely dry. Repeat the above operation to apply two to three layers to obtain a formed thermal insulation sintered brick.
[0063] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A thermal insulation sintered brick using municipal sludge, characterized in that: The invention comprises the following raw materials in parts by weight: 50-80 parts of municipal sewage sludge, 50-80 parts of clay, 10-15 parts of fine fly ash, 5-10 parts of expanded perlite powder, 10-15 parts of slag, 1-3 parts of foaming agent, 1-3 parts of modifier, 1-3 parts of flux, 2-5 parts of refractory additive and 1-3 parts of siloxane coating.
2. The thermal insulation sintered brick using municipal sludge according to claim 1, characterized in that: The foaming agent includes any one or more combinations of sodium bicarbonate, magnesium hydroxide, polystyrene particles and wood powder.
3. The thermal insulation sintered brick using municipal sludge according to claim 1, characterized in that: The modifier includes any one or more combinations of glass fiber, carbon fiber, polyvinyl alcohol, polyacrylate, sodium chloride and calcium chloride.
4. The thermal insulation sintered brick using municipal sludge according to claim 1, characterized in that: The flux comprises any one or more combinations of sodium fluoride, boric acid, sodium aluminate, sodium nitrate and calcium oxide.
5. The thermal insulation sintered brick using municipal sludge according to claim 1, characterized in that: The refractory additive includes any one or more combinations of high-bauxite, corundum, calcium oxide, ceramic fiber and zircon.
6. The production process of thermal insulation fired bricks using municipal sewage sludge according to any one of claims 1 to 5, characterized in that: The following steps are involved: S1. Harmless treatment of sludge First, the municipal sludge is put into a treatment tank with a stirring mechanism, and phosphate is added to the treatment tank. The stirring mechanism is started to allow the phosphate to fully contact the sludge, and the heavy metals in the sludge are converted into insoluble precipitates. After the reaction is completed, the precipitates are separated from the liquid phase by sedimentation; the liquid phase sludge after preliminary treatment is put into a belt filter press for mechanical dehydration treatment to remove the water in the sludge, and then the sludge and ion exchange resin are put into a stirring tank to mix the ion exchange resin with the sludge, so that the resin is fully in contact with the heavy metal ions in the sludge to continue to adsorb and remove the heavy metal ions in the sludge, and the treated sludge is separated from the resin and put into a drying device to further reduce the water content in the sludge by hot air drying; S2. Raw material mixing The dried sludge is put into a pulverizer and crushed into particles, and then the sludge particles, clay, fine fly ash, expanded perlite powder and slag are put into a mixing device, and mixed at a speed of 200-500r / min, and during the mixing process, a foaming agent, a modifier, a flux, a refractory additive and siloxane are added to the mixing device in sequence, and the mixing is continued until the mixture is completely mixed; S3. Compacting Put the mixed raw materials into the mold first, and then place the mold neatly on the vibration equipment to compact the raw materials in the mold and reduce the gaps; then use the molding equipment to press and form the bricks; S4. Firing First, the formed bricks are placed in a drying box at 80-100°C for preliminary drying, and then the dried bricks are stacked in a high-temperature kiln, and the high-temperature kiln is vacuumed and fired at 900-1100°C for 12-24 hours. After the firing is completed, the sintered bricks are slowly cooled in the kiln; S5. Surface treatment After cooling, use a brushing device to apply the silicone coating on the surface of the sintered brick. After the first application, dry it in the sun until it is completely dry. Repeat the above operation to apply two to three layers to obtain a formed thermal insulation sintered brick.