Preparation method of L (+)-lithium lactate
By precisely controlling the reaction conditions and operating steps, the problems of low purity and yield in the traditional L(+)-lithium lactate preparation method are solved, and the preparation of L(+)-lithium lactate with high purity and high yield is achieved, reducing the Production costs and meet the requirements of green chemistry.
Patent Information
- Application Number
- CN202411562799.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-05
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The traditional preparation method of L(+)-lithium lactate has problems such as harsh reaction conditions, many by-products, low product purity and low yield, which limits its large-scale industrial production and application.
By precisely controlling the reaction conditions and operating steps, it includes heating and stirring and dissolving lithium hydroxide monohydrate in deionized water, adding 75% L(+)-lactic acid for insulation and stirring, adjusting the pH of the reaction solution to weak acidity, and filtration and concentration , crystallization dehydration and drying to obtain high purity L(+)-lithium lactate crystals.
It improves the purity and yield of L(+)-lithium lactate, reduces production costs, is easy to operate, is environmentally friendly, and does not produce harmful by-products, which is in line with the development trend of green chemistry.
Smart Images

Figure SMS_1 
Figure SMS_2 
Figure SMS_3
Abstract
Description
Technical Field
[0001] The invention relates to a method for preparing L(+)-lithium lactate, and belongs to the technical field of chemical industry. Background Art
[0002] As an important organic metal salt, L(+)-lithium lactate has broad application prospects in medicine as a chiral resolution agent, food additive, cosmetic moisturizer, and new lithium-ion battery electrolyte material due to its unique biological activity and physicochemical properties. However, traditional preparation methods often have problems such as harsh reaction conditions, many by-products, low product purity, and low yield, which limit its large-scale industrial production and application.
[0003] The document "Introduction to the Synthesis of Lithium Lactate [J], Sun Chunhong et al., Journal of Clinical Laboratory, 1983" introduces a method for synthesizing lithium lactate. The process of synthesis in this process is violent and requires the use of acetone for reverse analysis, which is somewhat dangerous. It is difficult to control the amount of acetone used during the reverse analysis process, and the purity and quality of the product will be affected if it is not cleaned up afterwards. With the advancement of science and technology and the increasing demand for high-purity chemicals, the market prospect of high-purity L(+)-lithium lactate is very broad. Especially in the fields of medicine and materials science, its demand will continue to grow. In addition, with the improvement of environmental awareness and the popularization of the concept of sustainable development, green and efficient preparation methods will also become an important direction for the preparation of L(+)-lithium lactate in the future. Summary of the invention
[0004] In order to address at least one problem existing in the above-mentioned prior art, the present invention provides a method for preparing L(+)-lithium lactate, which effectively improves the purity and yield of L(+)-lithium lactate and reduces the production cost by precisely controlling the reaction conditions and operation steps.
[0005] In order to achieve the above object, the present invention adopts the following technical scheme: a method for preparing L(+)-lithium lactate, comprising the following steps: (1) Synthesis: First, lithium hydroxide monohydrate is placed in deionized water, heated and stirred to dissolve, and then 75% L(+)-lactic acid is added, and the mixture is stirred and reacted at the same temperature until the reaction is complete. Then, L(+)-lactic acid is used to adjust the pH of the reaction solution to weak acidity, and then the solution is filtered and clarified to obtain a synthetic solution. (2) Concentrating: Concentrating the synthetic liquid until a large amount of material is produced and the mass ratio of solid to liquid is 5:1, thereby obtaining a concentrated mixture; (3) Crystallization and dehydration: The concentrated mixture is cooled to 20-30°C for crystallization. After the crystallization is completed, it is placed in a centrifuge for dehydration at a dehydration time of 20-30 min / centrifuge to obtain L(+)-lithium lactate crystals; (4) Drying: The L(+)-lithium lactate crystals are placed in an oven for drying for 8 to 12 hours to obtain an L(+)-lithium lactate product with a content of ≥99%.
[0006] Preferably, in step (1), the pH is 6-7.
[0007] Preferably, in step (1), the reaction time is 25 to 35 min, preferably 30 min.
[0008] Preferably, in step (1), the molar ratio of lithium hydroxide monohydrate to L(+)-lactic acid is 1:1.
[0009] Preferably, in step (2), the concentration temperature is 95-100°C.
[0010] Preferably, in step (3), the crystallization temperature is 25-30°C.
[0011] Preferably, in step (3), the dehydration time is 20 to 25 min / machine.
[0012] Preferably, in step (3), the dehydration speed is 950-1050 r / min, preferably 1000 r / min.
[0013] Preferably, in step (4), the drying time is 8 to 10 hours.
[0014] Preferably, in step (4), the drying temperature is 65-75°C, preferably 70°C.
[0015] Preferably, in step (1), a filter bag with four layers is used for filtering, and the filter bag is a 240-mesh polyester filter cloth.
[0016] Preferably, in step (1), the heating and dissolving temperature is 95-100°C, preferably 100°C.
[0017] The beneficial effects of the present invention are as follows: the preparation method of the present invention effectively improves the purity and yield of L(+)-lithium lactate and reduces the production cost by precisely controlling the reaction conditions and operation steps; the preparation method of the present invention is easy to operate, environmentally friendly, and has no harmful by-products, which conforms to the development trend of green chemistry; the product obtained by the preparation method of the present invention has high purity and good stability, and can be widely used in multiple fields such as medicine, food, cosmetics and new materials. DETAILED DESCRIPTION
[0018] The following is a clear and complete description of the technical solutions in the implementation of the present invention. The described embodiments are only a part of the embodiments of the present invention, rather than all the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present invention. If the specific conditions are not specified in the embodiments, they are carried out according to the normal conditions or the conditions recommended by the manufacturer. If the manufacturer is not specified for the reagents, instruments, and components used, they are all conventional products that can be purchased commercially.
[0019] 1. Effect of different pH on L(+)-lithium lactate products In a 300L enamel reactor, lithium hydroxide monohydrate raw material was added in an amount as shown in Table 1 and 90kg of deionized water, heated to 100°C and stirred to dissolve, then 75% (mass fraction, the same below) L(+)-lactic acid was added in an amount as shown in Table 1, kept warm and stirred for 30min, and then L(+)-lactic acid was used to adjust the solution to different pH values, as shown in Table 1, filtered using 4 layers of 240-mesh polyester filter cloth, the filtrate was clarified and concentrated at 95°C until a large amount of material was produced, the mass ratio of solid to liquid was 5:1, and then cooled and crystallized, the crystallization temperature was 25°C, the crystallized material was placed in a centrifuge for dehydration, the dehydration time was controlled at 20min / machine, the speed was 1000r / min, the centrifuged material was placed in an oven at 70°C for 8h, and the L(+)-lithium lactate product results are shown in Table 1.
[0020] Table 1 Effect of different pH on L(+)-lithium lactate products
[0021] As can be seen from Table 1 above, pH has an effect on the content and yield of L(+)-lithium lactate: when pH is less than 6, the pH is too low and the acidity is too strong, resulting in the formation of insoluble matter on the surface of L(+)-lithium lactate, hindering the further reaction and reducing the yield; when pH is greater than 7, the pH is too high and lithium hydroxide is excessive, resulting in a decrease in the content of L(+)-lithium lactate. Therefore, pH is more suitable under weak acid conditions, and the optimal pH is 6~7.
[0022] 2. Effect of different crystallization temperatures on L(+)-lithium lactate products In a 300L enamel reactor, 15kg of lithium hydroxide monohydrate raw material and 90kg of deionized water were added, heated to 100°C and stirred to dissolve, then 32kg of 75% L(+)-lactic acid was added, and the mixture was stirred for 30min at a temperature of 100°C. The pH value of the solution was adjusted to 7 using L(+)-lactic acid, and the solution was filtered using 4 layers of 240-mesh polyester filter cloth. The filtrate was clarified and concentrated at 95°C until a large amount of material was produced, and the mass ratio of solid to liquid was 5:1. The product was cooled and crystallized, and the crystallization temperature was shown in Table 2. The crystallized material was placed in a centrifuge for dehydration, and the dehydration time was controlled at 20min / machine, and the speed was 1000r / min. The centrifuged material was placed in an oven and dried at 70°C for 8h. The L(+)-lithium lactate product results are shown in Table 2.
[0023] Table 2 Effect of different crystallization temperatures on L(+)-lithium lactate products
[0024] As can be seen from Table 2 above, different crystallization temperatures have an impact on the yield and content of L(+)-lithium lactate: when the crystallization temperature is greater than 30°C, too high a temperature will increase the solubility of L(+)-lithium lactate, increase the residual solute in the solution, and reduce the amount of crystallization, resulting in a greatly reduced yield; when the crystallization temperature is less than 20°C, the temperature is too low, and impurities will crystallize together with the target product, because at a lower temperature, the selective crystallization ability of the solute may be weakened, and some impurities that would not crystallize at a higher temperature may also be mixed into the crystals, thereby affecting the purity of the L(+)-lithium lactate product. Therefore, the crystallization temperature is more suitable at 20~30°C, and the optimal crystallization temperature is 25~30°C, which has a higher purity and yield.
[0025] 3. Effect of different dehydration time on L(+)-lithium lactate products In a 300L enamel reactor, 15kg of lithium hydroxide monohydrate raw material and 90kg of deionized water were added, heated to 100°C and stirred to dissolve, then 32kg of 75% L(+)-lactic acid was added, and the mixture was stirred for 30min at the temperature. Then, the pH of the solution was adjusted to 7 using L(+)-lactic acid, and the solution was filtered using 4 layers of 240-mesh polyester filter cloth. The filtrate was clarified and concentrated at 95°C until a large amount of material was produced, with a solid-liquid mass ratio of 5:1. The product was cooled and crystallized at a crystallization temperature of 25°C. The crystallized material was placed in a centrifuge for dehydration. The dehydration time is shown in Table 3. The centrifuged material was placed in an oven and dried at 70°C for 8h. The L(+)-lithium lactate product results are shown in Table 3.
[0026] Table 3 Effect of different dehydration time on L(+)-lithium lactate products
[0027] It can be seen from Table 3 above that, under a certain dehydration speed, different dehydration times have an impact on the content and yield of the product: when the dehydration time is less than 20 min / machine, the dehydration time is insufficient, and more water may remain in the product, because the presence of water will dilute the lithium lactate, so that in the product of the same quality, the proportion of lithium lactate decreases, that is, the actual content of lithium lactate decreases; when the dehydration time is greater than 30 min / machine, too long dehydration time will increase energy consumption and production time cost, and will also reduce the yield and production efficiency. Therefore, the dehydration time of 20~30 min / machine is more suitable, and 20~25 min / machine is more preferred.
[0028] 4. Effect of different drying times on L(+)-lithium lactate products In a 300L enamel reactor, 15kg of lithium hydroxide monohydrate raw material and 90kg of deionized water were added, heated to 100°C and stirred to dissolve, then 32kg of 75% L(+)-lactic acid was added, and the mixture was stirred for 30min at the temperature. Then, the pH of the solution was adjusted to 7 using L(+)-lactic acid, and the solution was filtered using 4 layers of 240-mesh polyester filter cloth. The filtrate was clarified and concentrated at 95°C until a large amount of material was produced, with a solid-liquid mass ratio of 5:1. The product was cooled and crystallized at a crystallization temperature of 25°C. The crystallized material was placed in a centrifuge for dehydration, with a dehydration time of 20min / machine. The centrifuged material was placed in an oven for drying, and the drying conditions are shown in Table 4. The L(+)-lithium lactate product results are shown in Table 4.
[0029] Table 4 Effect of different drying times on L(+)-lithium lactate products
[0030] It can be seen from Table 4 above that, under a certain drying temperature, different drying times have an impact on the content and yield of the product: if the drying time is less than 8 hours, insufficient drying time may cause more residual moisture in the lithium lactate; if the drying time is greater than 12 hours, the drying time is too long, resulting in chemical changes in the lithium lactate and the stability of the lithium lactate, thereby reducing its content. Therefore, a drying time of 8-12 / h is more appropriate, and 8-10 / h is more preferred.
[0031] In summary, the preparation method of the present invention effectively improves the purity of L(+)-lithium lactate to ≥99% and the yield to ≥70% by precisely controlling the reaction conditions and operation steps, reduces the production cost, is easy to operate, is environmentally friendly, and has no harmful by-products, which is in line with the development trend of green chemistry. The obtained product has high purity and good stability.
[0032] It will be apparent to those skilled in the art that the present invention is not limited to the details of the exemplary embodiments described above, and that the present invention can be implemented in other specific forms without departing from the spirit and essential features of the present invention. Therefore, the embodiments should be considered exemplary and non-restrictive in all respects, and the scope of the present invention is defined by the appended claims rather than the above description, and it is intended that all changes falling within the meaning and scope of the equivalent elements of the claims be included in the present invention.
[0033] In addition, it should be understood that although the present specification is described according to implementation modes, not every implementation mode contains only one independent technical solution. This description of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment may also be appropriately combined to form other implementation modes that can be understood by those skilled in the art.
Claims
1. A method for preparing L(+)-lithium lactate, characterized in that: The following steps are involved: (1) Synthesis: First, lithium hydroxide monohydrate is placed in deionized water, heated to 90-100°C and stirred to dissolve, then 75% L(+)-lactic acid is added, and the mixture is stirred and reacted at the same temperature. After the reaction is completed, the pH of the reaction solution is adjusted to weak acidity, and then filtered. The filtrate is clarified to obtain a synthetic solution; (2) Concentrating: concentrating the synthetic liquid at 95-100° C. to a solid-liquid ratio of 5:1 to obtain a concentrated mixture; (3) Crystallization and dehydration: The concentrated mixture is cooled to 20-30°C for crystallization. After the crystallization is completed, it is placed in a centrifuge for dehydration at a dehydration time of 20-30 min / centrifuge to obtain L(+)-lithium lactate crystals; (4) Drying: The L(+)-lithium lactate crystals are placed in an oven for drying for 8 to 12 hours to obtain an L(+)-lithium lactate product with a content of ≥99%.
2. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (1), the pH is 6-7.
3. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (1), the reaction time is 25 to 35 minutes.
4. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (1), the molar ratio of lithium hydroxide monohydrate to L(+)-lactic acid is 1:
1.
5. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (3), the crystallization temperature is 25-30°C.
6. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (3), the dehydration time is 20-25 min / machine.
7. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (3), the dehydration speed is 950~1050r / min.
8. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (4), the drying time is 8 to 10 hours.
9. The method for preparing L(+)-lithium lactate according to claim 1, characterized in that: In step (4), the drying temperature is 65-75°C.
Citation Information
Patent Citations
Preparation method for lithium titanate material