Method for preparing photocatalytic quantum dot material and application
By illuminating the lead sulfide quantum dot material, passivation of quantum dot material is achieved, solving the problem of band limitation of silicon-based infrared detectors, improving the imaging effect and stability of infrared detectors, and expanding the detection range.
Patent Information
- Application Number
- CN202311786973.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-25
- Publication Date
- 2024-12-03
AI Technical Summary
The band limitations of existing silicon-based infrared detectors have limited applications in fields such as autonomous driving and night shooting, and are unable to effectively detect bands of 1650nm and above.
By performing visible light treatment on lead sulfide quantum dot material, catalyzing the exchange of ligand materials of active layer to achieve effective passivation of quantum dot (100) planes, photocatalyzed quantum dot materials with a broader spectrum response are prepared for preparation Infrared detector.
It significantly improves the imaging effect and stability of the infrared detector, expands the detection range, can effectively absorb light of 1650nm and above, and enhances the visual distance under conditions such as rain and fog.
Smart Images

Figure CN119060718A_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of photoelectric detector technology, and in particular to a method for preparing photocatalytic quantum dot materials and applications. Background Art
[0002] Since the 21st century, with the continuous advancement of semiconductor technology, image sensing technology has developed rapidly, and emerging fields such as smart phones and machine vision have flourished. Electronic camera technology based on silicon-based imaging chips has been widely used in all aspects of life and occupies a pivotal position in people's production and life. After nearly ten years of research and development, the resolution of silicon-based imaging arrays has gradually improved, the pixel scale has continued to expand, and the pixel size has gradually decreased. By 2021, Weipai Semiconductor has achieved the preparation of 0.5μm ultra-small pixel chips, and the pixel scale has reached 100 million. According to survey statistics, the silicon-based image sensor market has grown year by year. In 2018, the global complementary metal oxide semiconductor (CMOS) image sensor market size reached US$15.478 billion. However, due to the absorption of silicon, the detection band of silicon-based image sensors is only 1.1μm, and it is in the detection blind spot after the 1650nm band, which limits its wide application in fields such as autonomous driving and night shooting.
[0003] Compared with visible light, near-infrared light with a wavelength of 1650nm has many advantages such as wide penetration range, strong anti-interference ability, and harmlessness to human eyes. It has been widely used in communications, medical care, industry and other fields. At the same time, infrared imaging technology has greater application potential in emerging fields such as intelligent sensing, machine vision, and autonomous driving. For example, the visible distance of visible light in rainy and foggy weather is up to 600 to 1500 meters, while the penetration distance of infrared light in rainy and foggy weather is 4.5 times that of visible light, which greatly increases the visible distance in rainy and foggy weather, showing great application potential in the fields of assisted driving and autonomous driving.
[0004] To this end, it is necessary to develop an infrared detector with a higher detection range to solve the band limitations of current infrared detectors. Summary of the invention
[0005] In view of the above-mentioned deficiencies of the prior art, the present application provides a method and application of photocatalytic quantum dot materials, the purpose of which is to catalyze the exchange of active layer ligand materials by treating the active layer quantum dot materials with visible light, so as to provide sufficient energy, so that the exposed (100) surface of the larger quantum dots can have sufficient energy for adsorption, thereby achieving effective passivation of the quantum dot (100) surface and inhibiting the oxidation and agglomeration of the quantum dots. The infrared detector prepared by the quantum dot material has significantly improved imaging effect and stability.
[0006] To achieve the above objectives, this application provides the following technical solutions:
[0007] In a first aspect, the present invention provides a method for photocatalytic quantum dot materials, which comprises the following steps:
[0008] preparing a lead sulfide quantum dots (PbS CQDs) solution;
[0009] preparing a ligand solution containing a halide;
[0010] After the lead sulfide quantum dot solution and the ligand solution are mixed, they are placed under ultraviolet light for illumination treatment, and after the mixed solution is separated into layers, the ultraviolet light is turned off;
[0011] After separating the supernatant from the mixed solution, the precipitate is obtained and dried to obtain the photocatalytic quantum dot material.
[0012] Furthermore, the halide is selected from at least one of SnCl2, PbCl2, PbBr2, and PbI2; preferably, the halide is PbI2, PbBr2, and SnCl2.
[0013] Furthermore, the conditions of the light treatment are: the wavelength of the ultraviolet lamp is 300-600nm, and the intensity of the ultraviolet light is 50nW-1mW.
[0014] Preferably, the light treatment conditions are: the wavelength of the ultraviolet lamp is 365nm, and the light intensity of the ultraviolet lamp is 10uW.
[0015] In a second aspect, an embodiment of the present application provides a photocatalytic quantum dot material, which is prepared by the aforementioned method.
[0016] In a third aspect, an embodiment of the present application provides a quantum dot infrared detector, comprising a bottom electrode layer, an electron blocking layer, a p-type layer, an active layer, an electron transport layer, a strong n-type layer, and a top electrode layer, wherein the active layer is prepared by spin coating the aforementioned photocatalytic quantum dot material.
[0017] Preferably, the bottom electrode layer and the top electrode layer are made of indium tin oxide (ITO).
[0018] Preferably, the material of the strong n-type layer is SnO2.
[0019] Preferably, the material of the electron transport layer is C60.
[0020] Preferably, the material of the p-type layer is at least one of lead sulfide (PbS), 1,2-ethanedithiol, tetramethylsilane, and acetonitrile.
[0021] Preferably, the material of the electron blocking layer is NiO2 or NiO3.
[0022] Preferably, the electron blocking layer, the p-type layer, the active layer, the electron transport layer, and the strong n-type layer form a pin structure as a whole.
[0023] In a fourth aspect, an embodiment of the present application provides a method for preparing the aforementioned quantum dot infrared detector, comprising the following steps:
[0024] preparing an electron blocking layer on the bottom electrode layer;
[0025] Preparing a p-type layer material precursor liquid, and spin coating the p-type layer material precursor liquid on the electron blocking layer to prepare a p-type layer;
[0026] Providing an active layer material precursor, wherein the active layer material precursor is the aforementioned photocatalytic quantum dot material;
[0027] Spin coating an active layer material precursor on the p-type layer to prepare an active layer;
[0028] preparing an electron transport layer on the active layer;
[0029] preparing a strong n-type layer on the electron transport layer;
[0030] The top electron layer of the strong n-type layer is prepared by magnetron sputtering.
[0031] Compared with the prior art, the technical solution provided by this application has at least the following technical effects:
[0032] (1) By irradiating the active layer quantum dot material with visible light, the ligand material in the active layer is catalyzed to provide sufficient energy for the exposed (100) surface of the larger quantum dots to have sufficient energy for adsorption, thus achieving effective passivation of the (100) surface of the quantum dots and inhibiting the oxidation and aggregation of the quantum dots. The imaging effect and stability of the infrared detector prepared by the quantum dot material are significantly improved.
[0033] (2) By adjusting the intensity and wavelength of photocatalysis, it was found that the PL intensity of photocatalytic ligand exchange was the highest when using 365nm ultraviolet light for light in the wavelength range of 300-600nm. At the same time, it was found that linear adjustment was made from the light intensity of 50nW to 10mW, and it was found that the appropriate light intensity, 10uW, had the best photocatalytic performance, the best passivation, and could also avoid photooxidation. BRIEF DESCRIPTION OF THE DRAWINGS
[0034] The present application will be further described in detail below in conjunction with the accompanying drawings and preferred embodiments, but those skilled in the art will appreciate that these drawings are drawn only for the purpose of explaining the preferred embodiments and therefore should not be used as a limitation on the scope of the present application. In addition, unless otherwise specified, the drawings are only schematically representing the composition or structure of the described objects and may contain exaggerated displays, and the drawings are not necessarily drawn to scale.
[0035] Figure 1 Schematic diagram of the photocatalytic quantum dot material provided in the embodiments of the present application.
[0036] Figure 2 This is a schematic diagram of the structure of a quantum dot infrared detector provided in an embodiment of the present application.
[0037] Figure 3 The PL test results of the PbS-Sn / PbCl2 quantum dot material after photocatalysis by ultraviolet light of different wavelengths provided in the embodiments of the present application.
[0038] Figure 4 The PL test results of the PbS-Sn / PbCl2 quantum dot material after ultraviolet photocatalysis at different light intensities provided in the embodiments of the present application.
[0039] Figure 5 A current-voltage curve diagram of the operating point for performance screening of the quantum dot infrared detector provided in an embodiment of the present application. DETAILED DESCRIPTION
[0040] In order to make the purpose, technical scheme and advantages of the present application more clear, the concept of the present application and the technical effects produced are further described in detail below in conjunction with the accompanying drawings and embodiments, so as to fully understand the purpose, features and effects of the present application. It should be understood that the specific embodiments described herein are only used to explain the present application and are not used to limit the present application. Other embodiments obtained by technicians in this field without creative work are all within the scope of protection of the present application.
[0041] The embodiment of the present application can promote ligand exchange to provide sufficient energy by subjecting the active layer quantum dot material of the infrared detector to light treatment, so that the exposed (100) surface of the larger quantum dot has enough energy for adsorption, passivating surface defects, and reducing quantum dot agglomeration, ultimately improving the detection range and stability of the quantum dot infrared detector. The embodiment of the present application optimizes the intensity and wavelength of the light treatment and finds that the PL intensity of photocatalytic ligand exchange is the highest when using 365nm ultraviolet light; at the same time, linear adjustment is made at the light intensity of 50nW to 1mW, and it is found that the quantum dot passivation effect is best when using a light intensity of 10uW for photocatalysis, and it can avoid photooxidation, so that the infrared detector has the best performance.
[0042] Based on this, the present invention provides a method for preparing a photocatalytic quantum dot material, comprising the following steps: preparing a lead sulfide quantum dot (PbS CQDs) solution; preparing a ligand solution containing a halide; mixing the lead sulfide quantum dot solution with the ligand solution, and then placing the mixture under ultraviolet light for light treatment (such as Figure 1 As shown), after the mixed solution is layered, the ultraviolet light is turned off; after the supernatant is separated from the mixed solution, the precipitate is obtained, and the photocatalytic quantum dot material is obtained by drying.
[0043] In certain embodiments, the concentration of the PbS quantum dot solution is 5-15 mg / mL.
[0044] In some embodiments, the halide is selected from at least one of SnCl2, PbCl2, PbBr2, and PbI2, and the photocatalytic quantum dot material finally formed is PbS-Sn / PbX2, wherein X is at least one of Cl, Br, and I. In some preferred embodiments, the halide includes PbI2, PbBr2, and SnCl2, and the photocatalytic quantum dot material finally formed is PbS-Sn / PbCl2, i.e., the active layer material precursor for forming the active layer.
[0045] In some embodiments, the conditions for the light treatment are: the wavelength of the ultraviolet light is 300-600nm, and the intensity of the ultraviolet light is 50nW-1mW. In some preferred embodiments, the conditions for the light treatment are: the wavelength of the ultraviolet light is 365nm, and the intensity of the ultraviolet light is 10uW.
[0046] In some embodiments, the solvent in the ligand solution is any one of dimethylformamide or dimethyl sulfoxide. In some preferred embodiments, the solvent of the ligand solution is selected from dimethylformamide.
[0047] Based on this, an embodiment of the present application provides a photocatalytic quantum dot material, which is prepared by the aforementioned method.
[0048] Based on this, the present invention provides an infrared detector, whose structure from bottom to top is a bottom electrode layer 1, an electron blocking layer 2, a p-type layer 3, an active layer 4, an electron transport layer 5, a strong n-type layer 6, and a top electrode layer 7 (such as Figure 2 As shown), wherein the active layer 4 is made by spin coating the aforementioned photocatalytic quantum dot material.
[0049] In some preferred embodiments, the photocatalytic quantum dot material forming the active layer 4 is PbS-Sn / PbCl2.
[0050] In some embodiments, the bottom electrode layer 1 and the top electrode layer 7 are made of indium tin oxide (ITO).
[0051] In some embodiments, the material of the strong n-type layer 6 is SnO 2 .
[0052] In some embodiments, the material of the electron transport layer 5 is C60.
[0053] In some embodiments, the material of the p-type layer 3 is at least one of lead sulfide (PbS), 1,2-ethanedithiol, tetramethylsilane, and acetonitrile.
[0054] In some embodiments, the material of the electron blocking layer 2 is NiO2 or NiO3.
[0055] In some embodiments, the quantum dot infrared detector, in which the electron blocking layer 2 (p-type structure), the p-type layer 3 (p-type structure), the active layer 4 (i-type structure), the electron transport layer 5 (n-type structure), and the strong n-type layer 6 (n-type structure) as a whole form a large pin structure (light-emitting diode structure).
[0056] Based on this, an embodiment of the present application provides a method for preparing the aforementioned infrared detector, comprising the following steps: preparing an electron blocking layer 2 on a bottom electrode layer 1; preparing a p-type layer 3 material precursor, and spin coating the p-type layer 3 material precursor on the electron blocking layer 2 to prepare the p-type layer 3; preparing an active layer 4 material precursor, wherein the active layer 4 material precursor is the aforementioned photocatalytic quantum dot material; spin coating the active layer 4 material precursor on the p-type layer 3 to prepare the active layer 4; preparing an electron transport layer 5 on the active layer 4; preparing a strong n-type layer 6 on the electron transport layer 5; and preparing a top electron layer 7 on the strong n-type layer 6 by a magnetron sputtering method.
[0057] In some embodiments, the electron blocking layer 2 is prepared by vacuum magnetron sputtering.
[0058] In some embodiments, the p-type layer 3 material precursor solution includes lead sulfide (PbS), 1,2-ethanedithiol, tetramethylsilane, and acetonitrile.
[0059] In some embodiments, the active layer 4 material precursor is a PbS-Sn / PbCl2 quantum dot material.
[0060] The following will be combined with more specific embodiments to illustrate that the technical solution provided by the present application has outstanding substantive features and significant progress. It should be understood that these specific embodiments are not limitations of the present application.
[0061] Preparation of photocatalytic quantum dot materials
[0062] The present application embodiment provides a method for preparing a photocatalytic quantum dot material (active layer 4 precursor), and the specific steps are as follows:
[0063] (1) Preparation of lead sulfide (PbS) quantum dot solution: PbS quantum dots were weighed and completely dissolved in n-octane to prepare a 10 mg / mL PbS quantum dot solution;
[0064] (2) Prepare ligand solution: weigh PbI2, PbBr2, and SnCl2 in a glove box, add 10-30 mL of dimethylformamide to a centrifuge tube to prepare a ligand solution. Ultrasonic heating is performed in an ultrasonic cleaner while oscillating every few minutes to accelerate dissolution; the ligand solution is filtered into a clean glass bottle using a syringe and filter;
[0065] (3) Using a syringe and a filter head to filter the PbS quantum dot solution into a glass bottle containing the ligand solution, tighten the bottle cap, and place the glass bottle under an ultraviolet lamp for illumination (irradiation), wherein the wavelength range of the ultraviolet lamp is 300 to 600 nm and the illumination intensity is 50 nW to 10 mW; manually oscillate, wait for the solution to separate into layers, and then turn off the ultraviolet lamp;
[0066] (4) Add n-octane to the glass bottle, shake manually, wait for stratification, and use a dropper to suck out the upper clear liquid and the gray substance in the middle. Repeat twice, transfer the lower layer solution in the glass bottle to a centrifuge tube, centrifuge to separate the supernatant, and drain the solvent in a glove box. Dry to obtain PbS-Sn / PbCl2 quantum dot material.
[0067] The present invention sets up multiple groups of experiments for light treatment conditions, and the parameter conditions are shown in Table 1 below.
[0068] Table 1
[0069]
[0070]
[0071] The PbS-Sn / PbCl2 quantum dot materials obtained from each experimental group were subjected to photoluminescence spectroscopy (PL) testing.
[0072] Figure 3 The PL test results of PbS-Sn / PbCl2 quantum dot materials after photocatalysis by ultraviolet light of different wavelengths are shown, corresponding to six groups of experiments: R0, R1, R2, R3, R4, and R5, where R0 is the blank control group of quantum dot materials that have not been photocatalytically treated. Figure 3 It can be seen that within the wavelength range of 365 to 600 nm, as the wavelength of ultraviolet light gradually decreases, the photoluminescence intensity of the quantum dot material changes the most, the blue shift is the largest, and the effect is the best. However, as the wavelength of ultraviolet light further decreases, the photoluminescence intensity of the quantum dot material decreases and the blue shift decreases, indicating that the optimal wavelength of ultraviolet light for photocatalytic treatment is 365 nm.
[0073] Figure 4 The PL test results of PbS-Sn / PbCl2 quantum dot materials after UV photocatalysis with different light intensities are shown, corresponding to five groups of experiments R6, R7, R8, R9, and R10. Figure 2 It can be seen that when the UV light intensity is in the linear range of 50nW-1mW, the photocatalytic PbS-Sn / PbCl2 quantum dot materials can achieve good photoluminescence intensity. Among them, when the UV light intensity is 10uW, the photocatalytic PbS-Sn / PbCl2 quantum dot material has the highest photoluminescence intensity. Figure 4 It can be seen that although the photoluminescence intensity (R8) of the PbS-Sn / PbCl2 quantum dot material obtained by photocatalysis with 1mW ultraviolet light intensity is not much different from the result of photocatalysis with 10uW ultraviolet light intensity (R6), it can be obviously found that the half-peak width of the R8 curve is significantly larger than that of the R6 curve, indicating that the dispersion of the quantum dots has deteriorated and the performance has deteriorated.
[0074] Quantum dot infrared detector and preparation method thereof
[0075] The present application embodiment provides a quantum dot infrared detector prepared using the aforementioned PbS-Sn / PbCl2 quantum dot material. Figure 1 As shown, the structure of the quantum dot infrared detector is, from bottom to top, a bottom electrode layer 1, an electron blocking layer 2, a p-type layer 3, an active layer 4, an electron transport layer 5, a strong n-type layer 6, and a top electrode layer 7. The material of the bottom electrode layer 1 and the top electrode layer 7 is an indium tin oxide film (ITO), the material of the electron blocking layer 2 is NiO2 or NiO3, the material of the p-type 3 is PbS-1,2-ethanedithiol (PbS-EDT), the material of the active layer 4 is the aforementioned PbS-Sn / PbCl2 photocatalytic quantum dot material, the material of the electron transport layer 5 is C60, and the material of the strong n-type layer 6 is a SnO2 layer.
[0076] In the quantum dot infrared detector provided in the embodiment of the present application, the active layer 4 (PbS-Sn / PbCl2 quantum dots) can absorb visible light and light with a cutoff wavelength of 1900nm, and can absorb the energy of photons under the irradiation of 1650nm light to generate light signals. The electron blocking layer 2, p-type layer 3, active layer 4, electron transport layer 5, and strong n-type layer 6 form an ohmic contact between the bottom electrode layer 1 and the top electrode layer 7. Under the irradiation of 1650nm light, the active layer 4 will generate electrons and vacancies, and the electrons will transfer along the electron transport layer 5 to the strong n-type layer 6; and transfer from the vacancies to the p-type layer 3. The electron blocking layer 2 prevents electrons from retrograde from the active layer 4 to the p-type layer 3. The p-type layer 3 forms a pn junction (light-emitting diode structure) with the strong n-type layer 6, and the p-type layer 3 generates carriers; as the bias voltage increases, the built-in potential of the initial built-in electric field begins to change. When the p-type layer 3 is completely depleted, the photocurrent is maximum, and the net photocurrent is obtained by subtracting the initial dark current from the photocurrent. The optical signal per unit area is the responsivity of 1650nm light.
[0077] The present application embodiment provides a method for preparing the above quantum dot infrared detector, and the specific steps are as follows:
[0078] (1) preparing an electron blocking layer 2 on the bottom electrode layer 1 by a magnetron sputtering method;
[0079] (2) preparing a p-type layer 3 on the electron blocking layer 2 by spin coating layer by layer: uniformly mixing a 10-40 mg / mL quantum dot solution with tetramethylsilane as solvent and PbS as solute with an acetonitrile solution with a 1,2-ethanedithiol content of 0.01% to 1% to prepare a p-type layer 3 material precursor solution, placing the p-type layer 3 material precursor solution on the electron blocking layer 2 by spin coating layer by layer, wherein the spin coating thickness is 20 nm; oxidizing in a high oxygen environment for 10 to 20 h to increase the doping concentration of PbS;
[0080] (3) Prepare the active layer 4 material precursor: weigh PbS quantum dots, completely dissolve them in n-octane, and prepare a 5-15 mg / mL PbS quantum dot solution; weigh PbI2, PbBr2, and SnCl2 in a glove box, add them to a centrifuge tube, and add 10-30 mL of dimethylformamide to prepare a ligand solution. Ultrasonic heating is performed in an ultrasonic cleaning machine while oscillating every few minutes to accelerate dissolution; the ligand solution is filtered into a clean glass bottle using a syringe and a filter; the PbS quantum dot solution is filtered into a glass bottle containing the ligand solution using a syringe and a filter, the bottle cap is tightened, and the glass bottle is placed under an ultraviolet lamp for illumination (irradiation) treatment, wherein the wavelength range of the ultraviolet lamp is 365nm and the illumination intensity is 10uW; manual oscillation is performed, waiting for the solution to stratify, and then the ultraviolet lamp is turned off; n-octane is added to the glass bottle, manual oscillation is performed, waiting for stratification, and the upper clear liquid and the gray substance in the middle are sucked out with a dropper, and the lower layer solution in the glass bottle is transferred to a centrifuge tube, the supernatant is separated by centrifugation, and the solvent is drained in a glove box, and dried to obtain the PbS-Sn / PbCl2 quantum dot material, i.e., the active layer 4 material precursor;
[0081] (4) Spin coating the active layer 4 on the p-type layer 3: In a glove box, add monobutylamine and dimethylformamide to a centrifuge tube respectively, shake evenly, and prepare an amine solution; add the amine solution to the centrifuge tube containing the PbS-Sn / PbCl2 solid in (3) to a concentration of 200-400 mg / mL, and use a small oscillator to slowly shake for 1-2 minutes to completely dissolve the quantum dots; transfer the solution to a small centrifuge tube and centrifuge at 3000r for 30s-1min; turn on the power of the gelling machine and the vacuum pump, set the speed to 2500r / min, the time to 40s, and the acceleration to 500; adsorb the p-type layer 3 on the tray and blow off the surface dust with an ear bulb; spin coat the PbS-Sn / PbCl2 / amine solution; adjust the temperature of the hot plate to 30-60°C, anneal for 3-5min, and remove the amine solution; remove the device and store it in the glove box for 1-3 days (maturation) to prepare the active layer 4;
[0082] (5) Preparing an electron transport layer 5 on the active layer 4: placing the active layer 4 on a thermal evaporation instrument; adjusting the current, and controlling the rate of thermal evaporation of the C60 source by a film thickness meter, and thermally evaporating the C60 to a thickness of 10 to 20 nm to complete the thermal evaporation, thereby forming the electron transport layer 5;
[0083] (6) Preparing a strong n-type layer 6 on the electron transport layer 5: placing the electron transport layer 5 on an atomic layer deposition platform and evacuating the layer; heating the device substrate platform and the tin source to a preset temperature and then performing atomic layer deposition; after reaching the number of cycles, a 20 to 40 nm thick SnO2 layer is obtained to form a strong n-type layer 6; closing the device and taking out the device;
[0084] (7) The top electron layer 7 is prepared by magnetron sputtering on the strong n-type layer 6: the magnetron sputtering method is used to prepare the top electron layer 7. -3 ~10 -2 The top electron layer 7 was prepared by sputtering indium tin oxide at 1 pa, wherein the oxygen-argon ratio was 0.3:66.3, the sputtering power was 80 W, and the sputtering time was 20 min. Finally, the following was obtained: Figure 2 The quantum dot infrared detector shown.
[0085] The specific implementation of the present application also provides a comparative implementation of the present application example. In the comparative implementation, in the specific steps for preparing the quantum dot infrared detector, except that the precursor (PbS-Sn / PbCl2 quantum dot material) used to prepare the active layer is not subjected to ultraviolet light photocatalytic treatment, the other conditions and parameters are the same as those of the present application example. The quantum dot infrared detector prepared by the application example and the comparative implementation is tested for performance using an Agilent B1500A semiconductor analyzer.
[0086] Figure 5 The current-voltage curve of the working point for the performance screening of quantum dot infrared detectors, where the solid line represents the photocurrent-voltage curve of the working point, and the solid line represents the dark current-voltage curve of the working point; the present application embodiment selected the "9a2 RBZ P3", "9a2 RBZ P6" working points of the photocatalytic quantum dot infrared detector and the "9D1 P7" working point of the non-photocatalytic quantum dot infrared detector for testing. Figure 5 It can be seen that the dark current of the two working points of the quantum dot infrared detectors using photocatalysis, "9a2 RBZ P3" and "9a2 RBZ P6", is much lower than that of the quantum infrared detector without photocatalysis, "9D1 P7". 2 (-1V) drops to less than 1uA / cm 2 The dark current density is reduced by an order of magnitude, which means that the weak light detection performance of the quantum dot infrared detector after photocatalysis can be significantly improved. At the same time, the photoresponse current of the quantum dot infrared detector after photocatalysis is 30uA, which is significantly improved compared with the photoresponse current value (10uA) without photocatalysis, thereby greatly improving the brightness of the film.
[0087] In summary, the detection performance of quantum dot infrared detectors prepared by photocatalytic passivation can be significantly improved compared with traditional quantum dot infrared detectors.
[0088] The present application is described in detail above. Specific examples are used in the present application to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the present application and its core ideas. It should be pointed out that for ordinary technicians in this technical field, without departing from the principles of the present application, several improvements and modifications can be made to the present application, and these improvements and modifications also fall within the scope of protection of the claims of the present application.
Claims
1. A method for preparing a photocatalytic quantum dot material, characterized in that: The method comprises the following steps: preparing a lead sulfide quantum dot solution; preparing a ligand solution containing a halide; After the lead sulfide quantum dot solution and the ligand solution are mixed, they are placed under ultraviolet light for illumination treatment, and after the mixed solution is separated into layers, the ultraviolet light is turned off; After separating the supernatant from the mixed solution, the precipitate is obtained and dried to obtain the photocatalytic quantum dot material.
2. The method according to claim 1, characterized in that The halide is selected from at least one of SnCl2, PbCl2, PbBr2, and PbI2.
3. The method according to claim 2, characterized in that The halides are PbI2, PbBr2, and SnCl2.
4. The method according to claim 1, characterized in that: The conditions of the light treatment are: the wavelength of ultraviolet light is 300-600nm, and the intensity of ultraviolet light is 50nW-1mW.
5. The method according to claim 4, characterized in that The light treatment conditions are: the wavelength of the ultraviolet lamp is 365nm, and the intensity of the ultraviolet lamp is 10uW.
6. A photocatalytic quantum dot material, characterized in that: It is prepared by the method according to claim 1.
7. A quantum dot infrared detector, characterized in that: The method comprises a bottom electrode layer, an electron blocking layer, a p-type layer, an active layer, an electron transport layer, a strong n-type layer, and a top electrode layer. The active layer is prepared by spin coating the photocatalytic quantum dot material according to claim 6.
8. The quantum dot infrared detector according to claim 7, characterized in that: The active layer is prepared by spin coating of PbS-Sn / PbCl2 photocatalytic quantum dot material.
9. The quantum dot infrared detector according to claim 7, characterized in that: The materials of the bottom electrode layer and the top electrode layer are indium tin oxide; the material of the strong n-type layer is SnO2; the material of the electron transport layer is C60; the material of the p-type layer is at least one of lead sulfide, 1,2-ethanedithiol, tetramethylsilane, and acetonitrile; the material of the electron blocking layer is NiO2 or NiO3; the electron blocking layer, p-type layer, active layer, electron transport layer, and strong n-type layer form a pin structure as a whole.
10. The method for preparing the quantum dot infrared detector according to claim 7, characterized in that: The preparation method comprises the following steps: preparing an electron blocking layer on the bottom electrode layer; Preparing a p-type layer material precursor liquid, and spin coating the p-type layer material precursor liquid on the electron blocking layer to prepare a p-type layer; Providing an active layer material precursor, wherein the active layer material precursor is the photocatalytic quantum dot material according to claim 6; Spin coating an active layer material precursor on the p-type layer to prepare an active layer; preparing an electron transport layer on the active layer; preparing a strong n-type layer on the electron transport layer; The top electron layer of the strong n-type layer is prepared by magnetron sputtering.