Metal gate manufacturing method

By removing the dummy gate and deposition dielectric layer and etching the overhang of the convex during the metal gate production process, the problem of poor morphology regulation of the gate opening is solved, the integrity and yield of metal filling are improved, and the existing technology is solved Problem with high risk of metal gate defects.

CN119069343APending Publication Date: 2024-12-03SHANGHAI INTEGRATED CIRCUIT EQUIPMENT & MATERIALS INDUSTRY INNOVATION CENTER CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202310644784.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2023-06-01
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

When making a metal gate with high dielectric constant, the morphology of the gate area openings is poor during dry etching, resulting in a convex convexity on the side walls on both sides of the dummy gate, which makes the gate opening size smaller , affects the integrity of metal filling and seriously affects the electrical properties and yield of semiconductor devices.

Method used

By obtaining a prefabricated semiconductor structure, a portion of the dummy gate is removed and a dielectric layer is deposited on the sidewall surface, the dielectric layer and the sidewall are etched to remove the convex, and then the gate area is filled with metal to form a metal gate. The optional steps include lateral etching of the side walls through a trimming process to expand the gate opening and adding a specific gas during etching to control the selection ratio and gas flow.

Benefits of technology

Effectively regulate the morphology of the gate area, avoid the problem of incomplete metal filling, reduce the risk of defects, improve the yield of the metal gate, and protect the sidewall and dummy gate areas through the dielectric layer, simplifying the removal process of the overhanging convex.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069343A_ABST
    Figure CN119069343A_ABST
Patent Text Reader

Abstract

The invention relates to the field of semiconductor element manufacturing, and discloses a metal gate manufacturing method which comprises the following steps: obtaining a prefabricated semiconductor structural member which comprises a substrate, a dummy gate and a side wall; removing part of the pseudo gate to obtain a processed pseudo gate; depositing a dielectric layer on the surfaces of the processed pseudo gate and the side wall; etching the dielectric layer and the side wall positioned at the top end of the gate opening, and removing the suspended bulge and the dielectric layer on the side wall; removing the processed pseudo gate; and filling metal in the gate region to form a metal gate. According to the method, a part of the pseudo gate is removed firstly, at the moment, the suspended protrusion exists at the position, located at the top end of the gate opening, of the side wall, then the dielectric layer is deposited, the dielectric layer and the side wall located at the top end of the gate opening are etched, namely the suspended protrusion is etched away at the same time, and regulation and control over the morphology of the gate region are achieved. In addition, due to the fact that the hanging protrusions are removed, the grid electrode area can be well filled with metal, cavities in the filling process are avoided, the risk of forming defects is reduced, and the yield of the metal grid electrode is improved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present application relates to the field of semiconductor element manufacturing, and in particular to a method for manufacturing a metal gate. Background Art

[0002] Currently, when making a high-k metal gate, the manufacturing process includes: first, ion implantation and high-temperature annealing process in the source and drain regions, then growing a dummy gate in the gate region and performing a high-temperature annealing process, and finally removing the dummy gate in the gate region and subsequently performing a metal filling process to obtain a metal gate with a high dielectric constant.

[0003] When removing the dummy gate, the dry etching process is mainly used to directly etch the dummy gate, and then wet etching is used to remove the remaining dummy gate and polymer. During the dry etching process, the morphology of the gate area opening is poorly controlled, and the side walls on both sides of the dummy gate will overhang at the top of the gate opening, and the gate opening size will be smaller, which will cause the problem of incomplete metal filling when the gate area is subsequently filled with metal, seriously affecting the electrical performance and yield of the semiconductor device.

[0004] Therefore, how to solve the above technical problems should be the focus of technical personnel in this field. Summary of the invention

[0005] The purpose of the present application is to provide a method for manufacturing a metal gate to adjust the morphology of the gate region and reduce the risk of defects in the metal gate.

[0006] In order to solve the above technical problems, the present application provides a method for manufacturing a metal gate, comprising:

[0007] Obtaining a prefabricated semiconductor structure, wherein the prefabricated semiconductor structure comprises a substrate, a dummy gate and a sidewall;

[0008] removing part of the pseudo gate to obtain a processed pseudo gate;

[0009] Depositing a dielectric layer on the surface of the processed dummy gate and the sidewall;

[0010] Etching the dielectric layer and the side wall at the top of the gate opening to remove the overhang on the side wall and the dielectric layer;

[0011] removing the processed dummy gate;

[0012] The gate region is filled with metal to form a metal gate.

[0013] Optionally, before removing the processed dummy gate, the method further includes:

[0014] The surface of the side wall located on one side of the gate opening is laterally etched through a trimming process to expand the gate opening; the gate opening is in an inverted trapezoidal shape corresponding to the laterally etched region.

[0015] Optionally, when lateral etching is performed through an edge trimming process, an etching selectivity ratio of silicon nitride to silicon oxide is greater than 10.

[0016] Optionally, when lateral etching is performed through the trimming process, the etching selectivity ratio of silicon nitride to silicon oxide and silicon nitride to polysilicon is greater than 10, and at least one of bromide gas, chloride gas, oxygen and nitrogen is added to the etching gas, and the flow range of the added gas is 5 to 100 ml / min.

[0017] Optionally, the height difference of the laterally etched area on the sidewall is less than

[0018] Optionally, before laterally etching the surface of the sidewall located on the gate opening side by the trimming process, the method further includes:

[0019] The sidewall and the surface of the processed dummy gate are etched by a breakthrough etching process, wherein the etching selectivity ratio of silicon oxide is greater than 10.

[0020] Optionally, removing the processed dummy gate includes:

[0021] Etching the processed dummy gate by dry etching process;

[0022] The processed dummy gate remaining after dry etching is removed by a wet etching process.

[0023] Optionally, the thickness of the dielectric layer is less than

[0024] Optionally, removing part of the pseudo gate to obtain a processed pseudo gate includes:

[0025] A portion of the dummy gate is removed by a dry etching process to obtain a processed dummy gate.

[0026] Optionally, when etching the dielectric layer and the side wall at the top of the gate opening, the etching power ranges from 300 to 1000 W, and the selective etching ratio of the dielectric layer is greater than 10.

[0027] The present application provides a method for manufacturing a metal gate, comprising: obtaining a prefabricated semiconductor structure, wherein the prefabricated semiconductor structure comprises a substrate, a dummy gate and a sidewall; removing a portion of the dummy gate to obtain a processed dummy gate; depositing a dielectric layer on the surface of the processed dummy gate and the sidewall; etching the dielectric layer and the sidewall located at the top of the gate opening to remove the overhang on the sidewall and the dielectric layer; removing the processed dummy gate; and filling metal in the gate area to form a metal gate.

[0028] It can be seen that when making a metal gate, the present application first removes part of the pseudo-gate. At this time, there is an overhang at the position of the side wall at the top of the gate opening. Then a dielectric layer is deposited, and the dielectric layer and the side wall at the top of the gate opening are etched, that is, the overhang is etched away together, so as to achieve the regulation of the morphology of the gate area. Since the overhang is removed, the metal can be well filled in the gate area, avoiding the occurrence of voids during the filling process, reducing the risk of defects, and improving the yield of the metal gate. In addition, the present application first deposits the dielectric layer and then etches to remove the overhang, which can protect the side wall and pseudo-gate area, and the overhang is easier to remove. BRIEF DESCRIPTION OF THE DRAWINGS

[0029] In order to more clearly illustrate the embodiments of the present application or the technical solutions of the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present application. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative work.

[0030] Figure 1 This is a transmission electron microscope image after the dummy gate is removed when preparing the metal gate in the related art;

[0031] Figure 2 This is a transmission electron microscope image of a metal gate after preparation in the related art;

[0032] Figure 3 The process of the metal gate manufacturing method provided in the embodiment of the present application Figure 1 ;

[0033] Figures 4 to 7 The metal gate manufacturing process provided in the embodiment of the present application Figure 1 ;

[0034] Figure 8 The process of the metal gate manufacturing method provided in the embodiment of the present application Figure 2 ;

[0035] Figures 9 and 10 The metal gate manufacturing process provided in the embodiment of the present application Figure 2 ;

[0036] Fig.11 This is a transmission electron microscope image after the dummy gate is removed when preparing the metal gate in the embodiment of the present application;

[0037] In the figure, 1, substrate, 2, dummy gate, 3, side wall, 4, dielectric layer, 5, overhang, 6, dummy gate after processing, 31, silicon nitride, 32, silicon oxide. DETAILED DESCRIPTION

[0038] In order to enable those skilled in the art to better understand the present application, the present application is further described in detail below in conjunction with the accompanying drawings and specific implementation methods. Obviously, the described embodiments are only part of the embodiments of the present application, rather than all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in the field without making creative work are within the scope of protection of the present application.

[0039] In the following description, many specific details are set forth to facilitate a full understanding of the present invention, but the present invention may also be implemented in other ways different from those described herein, and those skilled in the art may make similar generalizations without violating the connotation of the present invention. Therefore, the present invention is not limited to the specific embodiments disclosed below.

[0040] As described in the background technology section, currently when removing the dummy gate, the morphology of the gate region opening is poorly controlled during the dry etching process, and the side walls on both sides of the dummy gate will have overhangs at the top of the gate opening, such as Figure 1 As shown in FIG. 1 , due to the presence of the overhang, the gate opening will gradually decrease during the metal deposition process, such as Figure 2 As shown, the problem of incomplete metal filling is prone to occur, which seriously affects the electrical performance and yield of semiconductor devices.

[0041] In view of this, the present application provides a method for manufacturing a metal gate, please refer to Figure 3 ,include:

[0042] Step S101: obtaining a prefabricated semiconductor structure, wherein the prefabricated semiconductor structure comprises a substrate, a dummy gate and a sidewall.

[0043] For a schematic diagram of prefabricated semiconductor structures, please refer to Figure 4 The dummy gate 2 and the sidewall 3 are both located on the substrate 1, and the sidewall 3 is located on both sides of the dummy gate 2. The sidewall includes silicon oxide 32 and silicon nitride 31, and the dummy gate 2 can be polysilicon.

[0044] The prefabricated semiconductor structural parts can be directly obtained already manufactured, or can be manufactured by oneself. The specific manufacturing process can refer to the relevant technology, which will not be described in detail here.

[0045] Step S102: removing part of the dummy gate to obtain a processed dummy gate.

[0046] After removing part of the dummy gate, a gate opening is formed in the gate region.

[0047] As an implementation method, removing part of the dummy gate to obtain a processed dummy gate includes:

[0048] A portion of the dummy gate is removed by a dry etching process to obtain a processed dummy gate.

[0049] Step S103: depositing a dielectric layer on the surface of the processed dummy gate and the sidewall.

[0050] Please refer to Figure 5 The upper surface of the processed dummy gate 6 is lower than the upper surface of the side wall 3 , and there is an overhang 5 at the top of the gate opening of the side wall 3 , and the dielectric layer 4 covers the side wall 3 and the upper surface of the processed dummy gate 6 .

[0051] The dielectric layer 4 may be a silicon oxide layer, and the deposition method may be chemical vapor deposition, plasma enhanced chemical vapor deposition, etc.

[0052] The thickness of the dielectric layer 4 is less than For example, the thickness of the dielectric layer 4 can be wait.

[0053] Step S104: etching the dielectric layer and the side wall at the top of the gate opening to remove the overhang on the side wall and the dielectric layer.

[0054] Please refer to Figure 6 , the dielectric layer is completely etched away, the sidewall at the top of the gate opening is partially etched away, and the overhang is also etched away. It should be noted that the silicon oxide on the sidewall is also partially etched away.

[0055] As an implementation method, when etching the dielectric layer and the side wall at the top of the gate opening, the etching power range is 300-1000W, and the selective etching ratio of the dielectric layer is greater than 10. The etching energy and the selective etching ratio of the dielectric layer are relatively large, the dielectric layer is etched more, and the etching of other film layer structures is relatively small, which plays a protective role.

[0056] In solving the overhang problem in this embodiment, a dielectric layer is first deposited and then etched. On the one hand, the overhang can be more easily etched away. On the other hand, the dielectric layer also has a protective effect to prevent other structures from being damaged.

[0057] Step S105: removing the processed dummy gate.

[0058] Please refer to Figure 7 , the dummy gate is completely removed, a groove is formed between the two side walls 3, and metal is subsequently filled in the groove.

[0059] Step S106: filling the gate region with metal to form a metal gate.

[0060] The process of filling metal can refer to the relevant technology and will not be described in detail here.

[0061] When making the metal gate in this embodiment, part of the pseudo gate is first removed. At this time, there is an overhang at the position of the side wall at the top of the gate opening. Then a dielectric layer is deposited, and the dielectric layer and the side wall at the top of the gate opening are etched, that is, the overhang is etched away together, so as to achieve the control of the morphology of the gate area. Since the overhang is removed, the metal can be well filled in the gate area, avoiding the occurrence of voids during the filling process, reducing the risk of defects, and improving the yield of the metal gate. In addition, the present application first deposits the dielectric layer and then etches to remove the overhang, which can protect the side wall and the pseudo gate area, and the overhang is easier to remove.

[0062] Please refer to Figure 8 Based on the above embodiments, in one embodiment of the present application, a metal gate manufacturing method includes:

[0063] Step S201: obtaining a prefabricated semiconductor structure, wherein the prefabricated semiconductor structure comprises a substrate, a dummy gate and a sidewall.

[0064] Step S202: removing part of the dummy gate to obtain a processed dummy gate.

[0065] Step S203: depositing a dielectric layer on the surface of the processed dummy gate and the sidewall.

[0066] Step S204: etching the dielectric layer and the side wall at the top of the gate opening to remove the overhang on the side wall and the dielectric layer.

[0067] Step S205: performing a trimming process to laterally etch the surface of the side wall located on one side of the gate opening to expand the gate opening; the gate opening has an inverted trapezoidal shape corresponding to the laterally etched region.

[0068] Please refer to Fig. 9 The shape of the side wall 3 on one side of the gate opening is adjusted by a trimming process, so that the gate opening is enlarged and smooth.

[0069] When lateral etching is performed through the trimming process, the etching selectivity ratio of silicon nitride to silicon oxide and silicon nitride to polysilicon is greater than 10, and at least one of bromide gas, chloride gas, oxygen and nitrogen is added to the etching gas, and the flow range of the added gas is 5 to 100 ml / min.

[0070] The bromide gas includes, but is not limited to, hydrogen bromide, and the chloride gas includes, but is not limited to, hydrogen chloride.

[0071] The flow rate of the added gas can be 5ml / min, 10ml / min, 30ml / min, 50ml / min, 80ml / min, 100ml / min, etc. The etching selectivity can be adjusted by adjusting the flow rate of the added gas, that is, adjusting the proportion of the added gas in the etching gas.

[0072] The outermost area of ​​the side wall that contacts the dummy gate is silicon nitride, and the inner side of the silicon nitride is silicon oxide. When the sidewall is etched laterally through the trimming process, the etching selectivity of silicon nitride to silicon oxide and silicon nitride to polysilicon is greater than 10, and the etching rate of silicon nitride is greater, so that the sidewall lateral etching area is an inclined surface. Among them, the etching amount of the sidewall lateral etching area gradually increases in the direction away from the substrate, so that the gate opening and the part corresponding to the lateral etching are inverted trapezoidal.

[0073] In order to control the morphology difference, the height difference H of the laterally etched area on the sidewall is less than The height difference of the lateral etching area is the height between the highest point of the side wall top and the bottom of the lateral etching area, such as Fig.10 shown.

[0074] In one embodiment of the present application, before laterally etching the surface of the sidewall located on one side of the gate opening by a trimming process, the method further includes:

[0075] The sidewall and the surface of the processed dummy gate are etched by a breakthrough etching process, wherein the etching selectivity ratio of silicon oxide is greater than 10.

[0076] The silicon oxide etching selectivity ratio during break through (BT) etching is greater than 10. The reason is that when etching the dielectric layer and the overhang, the silicon oxide on the side wall will also be etched a little. When performing break through (BT) etching, it is necessary to control the etching of the silicon oxide on the side wall to avoid etching a large amount of silicon oxide on the side wall, which affects the morphology.

[0077] Step S206: removing the processed dummy gate.

[0078] Please refer to Fig.10 The dummy gate is completely removed, and a groove is formed between the two sidewalls. At this time, the TEM image of the structure is as follows Fig.11 shown.

[0079] As an implementable method, removing the processed dummy gate includes:

[0080] Step S2061: etching the processed dummy gate by dry etching process.

[0081] The etching in this step is main etching (ME). After the treatment, the dummy gate is almost completely etched after the main etching, with only a small amount of residue. The residue can be further removed by wet etching in step S2062.

[0082] Step S2062: removing the processed dummy gate remaining after dry etching by a wet etching process.

[0083] It should be noted that in this step, the residual dummy gate is removed by wet etching, and the residual polymer is also removed at the same time.

[0084] Step S207: filling the gate region with metal to form a metal gate.

[0085] The metal gate manufacturing method in the present application is described below using a specific case.

[0086] Step 1: removing part of the dummy gate in the prefabricated semiconductor structure by a dry etching process to obtain a processed dummy gate, wherein the prefabricated semiconductor structure includes a substrate, a dummy gate and a sidewall;

[0087] Step 2, depositing a dielectric layer on the surface of the processed dummy gate and the sidewall;

[0088] Step 3, etching the dielectric layer and the side wall at the top of the gate opening by dry etching process, removing the overhang on the side wall and the dielectric layer; wherein the etching power range is 300 to 1000 W, and the selective etching ratio of the dielectric layer is greater than 10;

[0089] Step 4, etching the sidewall and the surface of the processed dummy gate by a BT etching process; wherein the etching selectivity ratio for silicon oxide is greater than 10;

[0090] Step 5, performing a lateral etching on the surface of the sidewall located on one side of the gate opening by a trimming process to expand the gate opening; the lateral etching region corresponding to the gate opening is in an inverted trapezoidal shape; wherein the etching selectivity ratio of silicon nitride to silicon oxide and silicon nitride to polysilicon is greater than 10;

[0091] Step 6, removing the processed dummy gate through a main etching process;

[0092] Step 7: removing the remaining processed dummy gate by a wet etching process to form a groove between the two side walls, i.e., a gate opening;

[0093] Step 8: Fill the gate opening with metal to form a metal gate line.

[0094] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.

[0095] The above is a detailed introduction to the metal gate manufacturing method provided by the present application. This article uses specific examples to illustrate the principles and implementation methods of the present application. The description of the above embodiments is only used to help understand the method and its core idea of ​​the present application. It should be pointed out that for ordinary technicians in this technical field, without departing from the principles of the present application, several improvements and modifications can be made to the present application, and these improvements and modifications also fall within the scope of protection of the claims of the present application.

Claims

1. A method for manufacturing a metal gate, characterized in that: include: Obtaining a prefabricated semiconductor structure, wherein the prefabricated semiconductor structure comprises a substrate, a dummy gate and a sidewall; removing part of the pseudo gate to obtain a processed pseudo gate; Depositing a dielectric layer on the surface of the processed dummy gate and the sidewall; Etching the dielectric layer and the side wall at the top of the gate opening to remove the overhang on the side wall and the dielectric layer; removing the processed dummy gate; The gate region is filled with metal to form a metal gate.

2. The method for manufacturing a metal gate according to claim 1, wherein: Before removing the processed dummy gate, the method further includes: The surface of the side wall located on one side of the gate opening is laterally etched by a trimming process to expand the gate opening; the gate opening is in an inverted trapezoidal shape corresponding to the laterally etched region.

3. The method for manufacturing a metal gate according to claim 2, wherein: When lateral etching is performed through an edge trimming process, the etching selectivity ratio of silicon nitride to silicon oxide is greater than 10.

4. The method for manufacturing a metal gate according to claim 2, wherein: When lateral etching is performed through the trimming process, the etching selectivity ratio of silicon nitride to silicon oxide and silicon nitride to polysilicon is greater than 10, and at least one of bromide gas, chloride gas, oxygen and nitrogen is added to the etching gas, and the flow range of the added gas is 5 to 100 ml / min.

5. The method for manufacturing a metal gate according to claim 2, wherein: The height difference of the laterally etched area on the sidewall is less than 6. The method for manufacturing a metal gate according to claim 2, wherein: Before laterally etching the surface of the sidewall located on one side of the gate opening by the trimming process, the method further includes: The sidewall and the surface of the processed dummy gate are etched by a breakthrough etching process, wherein the etching selectivity ratio of silicon oxide is greater than 10.

7. The method for manufacturing a metal gate according to claim 2, wherein: Removing the processed dummy gate includes: Etching the processed dummy gate by dry etching process; The processed dummy gate remaining after dry etching is removed by a wet etching process.

8. The method for manufacturing a metal gate according to claim 1, wherein: The thickness of the dielectric layer is less than 9. The method for manufacturing a metal gate according to claim 1, wherein: Removing part of the pseudo gate to obtain a processed pseudo gate includes: A portion of the dummy gate is removed by a dry etching process to obtain a processed dummy gate.

10. The method for manufacturing a metal gate according to any one of claims 1 to 9, characterized in that: When etching the dielectric layer and the side wall at the top of the gate opening, the etching power ranges from 300 to 1000 W, and the selective etching ratio of the dielectric layer is greater than 10.