Method for manufacturing vertical power transistor and vertical power transistor

By applying a dielectric layer on the semiconductor material and utilizing multiple photoetching steps, the problem of difficult control of the trench depth and width of the vertical power transistor is solved, and efficient and controllable trench manufacturing is achieved, reducing process complexity and cost.

CN119069355APending Publication Date: 2024-12-03ROBERT BOSCH GMBH
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410696855.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-05-31
Filing Date
2024-05-31
Publication Date
2024-12-03

AI Technical Summary

Technical Problem

In the prior art, when manufacturing vertical power transistors, the depth and width of the trench are difficult to accurately control, resulting in unstable etching rates, complex processes and high costs.

Method used

The trench is achieved by applying a dielectric layer on the semiconductor material and generating trenches with different depths and widths using multiple lithography and etching steps, and the depth and width differences of the trench are controlled by the structured dielectric layer and the marking layer, and the trench is achieved by controlling the depth and width differences of the trench. controllable.

Benefits of technology

The efficient and controllable vertical power transistor is achieved, reducing process steps and costs, and improving the accuracy of trench depth and width.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119069355A_ABST
    Figure CN119069355A_ABST
Patent Text Reader

Abstract

The invention relates to a method for manufacturing a vertical power transistor. The vertical power transistor has a first trench of a first trench depth and a second trench of a second trench depth. The first trench depth and the second trench depth have a difference of at least 30%. Applying a dielectric layer on the semiconductor material, applying a first photoresist layer on the dielectric layer, creating a first opening having a first width in the first photoresist layer, exposing a first region of the dielectric layer, etching the first region to a determined depth, creating a first structured dielectric layer, removing the first photoresist layer, and forming a second structured dielectric layer on the first structured dielectric layer. Applying a second photoresist layer onto the first structured dielectric layer, creating a second opening having a second width in the second photoresist layer, exposing a second region of the dielectric layer, etching the second region to a surface of the semiconductor material, creating a second structured dielectric layer, removing the second photoresist layer, and removing the second structured dielectric layer; the further etching produces a first trench and a second trench starting from the second structured dielectric layer to the semiconductor material. The invention also relates to a corresponding vertical power transistor.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for manufacturing a vertical power transistor and a vertical power transistor. Background Art

[0002] Trench etching is necessary to produce vertical power transistors. The width of the trench can be easily varied by means of a corresponding mask layout. Structure sizes of less than 2 μm are mostly produced with the aid of plasma etching. In this case, the etching rate is determined by the width of the trench. The wider the trench, the higher the etching rate. The trenches have a depth difference of between 10% and 20%. This is affected by process fluctuations and can be controlled conditionally or is difficult to reproduce. Therefore, a large number of lithography and etching steps are required to produce trenches with different trench depths. This is both time-consuming and expensive. Summary of the invention

[0003] The object of the present invention is to overcome these disadvantages.

[0004] According to the present invention, a method for manufacturing a vertical power transistor is proposed, wherein the vertical power transistor has at least a first trench having a first trench depth and at least a second trench having a second trench depth, wherein the first trench and the second trench are alternately arranged spaced apart from each other in the lateral direction, and the first trench depth and the second trench depth have a difference of at least 30%, the method comprising: applying a dielectric layer to a semiconductor material and applying a first photoresist layer to the dielectric layer. The method further comprises: generating a first opening having a first width in the first photoresist layer by means of a first photolithography, wherein a first region of the dielectric layer is exposed; etching the first region of the dielectric layer at least to a certain depth of the dielectric layer, so as to generate a first structured dielectric layer; and removing the first photoresist layer. In addition, the method comprises: applying a second photoresist layer to the first structured dielectric layer, generating a second opening having a second width in the second photoresist layer by means of a second photolithography, wherein a second region of the dielectric layer is exposed; and etching the second region of the dielectric layer to the surface of the semiconductor material, so as to generate a second structured dielectric layer. The method further comprises removing the second photoresist layer and producing, by means of a further etching step, a first trench and a second trench extending from the second structured dielectric layer into the semiconductor material.

[0005] The advantage here is that vertical power transistors with controllable large trench depths can be manufactured.

[0006] In an improved configuration, a marking layer is produced within the dielectric layer, which marking layer marks the specific depth of the dielectric layer.

[0007] It is advantageous here that the determined depth is independent of the dielectric layer thickness.

[0008] In another configuration, the first width and the second width are the same size.

[0009] The advantage here is that trenches of different depths can be produced despite the same width.

[0010] According to the present invention, a method for manufacturing a vertical power transistor is also proposed. The vertical power transistor has at least a first trench with a first trench width and at least a second trench with a second trench width, wherein the first trench depth and the second trench depth have a difference of at least 30%, and the method comprises: applying a dielectric layer to a semiconductor material and applying a photoresist layer to the dielectric layer. The method also comprises: generating a first opening with a first width and a second opening with a second width in the photoresist layer by means of photolithography, wherein the first opening and the second opening are alternately arranged spaced apart from each other in the lateral direction, wherein the first width and the second width are different in size, the first opening exposes a first region of the dielectric layer and the second opening exposes a second region of the dielectric layer, etching the first region and the first region to generate a structured dielectric layer; and generating the first trench and the second trench from the structured dielectric layer to the semiconductor material by means of a further etching step.

[0011] The advantage here is that the manufacture of vertical power transistors is cost-effective.

[0012] In an extended configuration, the semiconductor material includes Si, SiC or GaN.

[0013] In another configuration, the dielectric layer includes SiN or SiO 2 .

[0014] An advantage here is that the dielectric layer is of high quality.

[0015] The vertical power transistor comprises a semiconductor material, at least a first trench having a first trench depth and a second trench having a second trench depth. According to the invention, the first trench depth and the second trench depth have a difference of at least 30%.

[0016] The advantages here are the small cell size and the high penetration field strength.

[0017] In one embodiment, the semiconductor material comprises Si, SiC or GaN.

[0018] Further advantages can be derived from the following description of the embodiments or from the technical solution. BRIEF DESCRIPTION OF THE DRAWINGS

[0019] The present invention is explained below with reference to preferred embodiments and the accompanying drawings. The accompanying drawings show:

[0020] Figure 1 is a method for manufacturing a vertical power transistor according to the present invention,

[0021] Figure 2 is another method for manufacturing a vertical power transistor according to the present invention, and

[0022] Figure 3 It is an intermediate result after executing step 110 according to the method of the present invention. DETAILED DESCRIPTION

[0023] Figure 1 A method 100 for manufacturing a vertical power transistor according to the present invention is shown, the vertical power transistor having at least a first trench having a first trench depth and at least a second trench having a second trench depth, wherein the first trench and the second trench are alternately arranged spaced apart from each other in the lateral direction, and the first trench depth and the second trench depth have a difference of at least 30%. The method 100 starts with step 101, in which a dielectric layer is applied to a semiconductor material. The semiconductor material comprises, for example, Si, SiC or GaN, and the dielectric layer comprises SiN or SiO 2 . In a subsequent step 102, a first photoresist layer is applied to the dielectric layer. In a subsequent step 103, a first opening having a first width is produced in the first photoresist layer by means of a first photolithography. A first region of the dielectric layer is exposed. In a subsequent step 104, the first region of the dielectric layer is etched at least to a certain depth of the dielectric layer. The dielectric layer is thereby structured or a first structured dielectric layer is produced. Alternatively, the dielectric layer below the first opening can be completely removed. The structured first photoresist layer is used here as a protective mask for the part of the dielectric layer that is to be etched in a later step. A shallower trench is defined by means of the first opening. The first photoresist layer is removed in a subsequent step 105. In a subsequent step 106, a second photoresist layer is applied to the first structured dielectric layer. In a subsequent step 107, a second opening having a second width is produced in the second photoresist layer by means of a second photolithography. A second region of the dielectric layer is exposed. In a subsequent step 108, the second region of the dielectric layer is etched to the surface of the semiconductor material. A second structured dielectric layer is produced here. In other words, the surface of the semiconductor material is partially exposed. The second opening defines the size of the deeper trench. In a subsequent step 109, the second photoresist layer is removed. In a subsequent step 110, the first trench and the second trench are produced by means of a further etching step. Etching steps 104, 108 and 110 are carried out, for example, by means of plasma etching. If the dielectric layer is removed to a certain depth in step 104, etching of the semiconductor material for the first trench begins with a time delay, because some parts of the hard mask, i.e. the remnants of the dielectric layer, are located below the first opening, and these parts must be removed by means of the same etching step 110. Here, the selectivity of the hard mask, i.e. the first structured dielectric layer, and the determined depth determine the depth difference of the trench. Therefore, the trench width and the trench depth are decoupled from each other.

[0024] Alternatively, steps 106 to 109 may be performed after applying the dielectric layer in step 101 , followed by steps 103 to 105 , so that the deeper trenches are defined first and then the shallower trenches.

[0025] In one embodiment, a marking layer is produced in the dielectric layer during step 101. Here, a material for the dielectric layer is first deposited to a certain height on the semiconductor material, for example SiN or SiO. 2 Subsequently, a marking layer composed of another material is deposited on the dielectric layer. The marking layer comprises, for example, polysilicon and has a thickness of 20 nm. Alternatively, a marking layer composed of SiO 2 Composition, namely SiO 2 In the case of a hard mask, SiN can be used as a marking layer. In the case of a SiN hard mask, SiO 2 As a marking layer. The marking layer has a layer thickness between 20 nm and 100 nm. Subsequently, the material for the dielectric layer is deposited further until the desired dielectric layer thickness. Alternatively, the etching step 104 can be performed in a time-coupled manner so that the etching in the dielectric layer is stopped.

[0026] Additionally or alternatively, the first width and the second width are of the same size. This means that grooves of the same width but different depths can be manufactured in this way.

[0027] The vertical power transistor is then completed using a process from the prior art.

[0028] Figure 2 Another method 200 for manufacturing a vertical power transistor according to the present invention is shown, the vertical power transistor having at least a first trench having a first trench depth and at least a second trench having a second trench depth, wherein the first trench depth and the second trench depth have a difference of at least 30%. The method 200 starts with step 201, in which a dielectric layer is applied to a semiconductor material. The semiconductor material comprises, for example, Si, SiC or GaN, and the dielectric layer comprises SiN or SiO 2. In a subsequent step 202, a first photoresist layer is applied to the dielectric layer. In a subsequent step 203, a first opening having a first width and a second opening having a second width are generated in the photoresist layer by means of photolithography, wherein the first width and the second width are different in size. Here, the first opening and the second opening are alternately arranged spaced apart from each other in the lateral direction, wherein the first opening exposes a first region of the dielectric layer and the second opening exposes a second region of the dielectric layer. In other words, the first opening and the second opening are generated simultaneously in one step. In a subsequent step 204, the first region and the second region of the dielectric layer are etched. A structured dielectric layer is generated here, wherein, for example, the first width is narrower than the second width, so that the surface of the semiconductor material is exposed below the second opening, while the dielectric material is still below the first opening. This is due to the lower etching rate of the narrower opening or width. In a subsequent step 211, a first trench and a second trench are generated starting from the structured dielectric layer and ending in the semiconductor material by means of a further etching step. The etching of the semiconductor material starts with a time delay for the first trench, since parts of the hard mask are located below the first opening, which parts must be removed by means of the same etching step 211. The depth differences between the trenches are determined by the selectivity of the hard mask or the structured dielectric layer together with the hard mask residues below the first opening relative to the semiconductor material to be etched and the different widths of the trenches. In this further method according to the invention, the trench width and the trench depth are coupled to one another, wherein a significant depth difference of the trenches can be produced with a single lithography step, which is controllable.

[0029] The vertical power transistor is then completed using a process from the prior art.

[0030] Figure 3 The method for manufacturing a vertical power transistor according to the present invention is shown in FIG. Figure 1 300 after step 110 in FIG. 301 shows a semiconductor material 301 on which a dielectric layer 302 is applied. In this exemplary embodiment, a marking layer 303 is arranged in the dielectric layer 302. Starting from the surface of the dielectric layer 302, a first trench 304 and a second trench 305 extend into the semiconductor material 301. The semiconductor material 301 here comprises, for example, Si, SiC or GaN.

[0031] Alternatively and in Figure 3 Not shown in FIG. 3 , the marking layer 303 may be omitted, so that the dielectric layer 302 is arranged in one portion on the semiconductor material 301 .

[0032] The invention is not limited to two different groove depths. A large number of grooves with different groove depths can be produced.

[0033] Vertical power transistors with trenches of different depths are used, for example, in electric drive trains of electric or hybrid vehicles, for example in DC / DC converters or inverters, and in vehicle charging devices.

Claims

1. A method (100) for manufacturing a vertical power transistor having at least a first trench having a first trench depth and at least a second trench having a second trench depth, wherein: The first grooves and the second grooves are alternately arranged to be spaced apart from each other in a lateral direction, and the first groove depth and the second groove depth have a difference of at least 30%, and the method comprises the following steps: applying (101) a dielectric layer onto the semiconductor material, applying (102) a first photoresist layer onto the dielectric layer, Producing (103) a first opening having a first width in the first photoresist layer by means of a first photolithography, wherein a first region of the dielectric layer is exposed, etching (104) the first region of the dielectric layer at least to a determined depth of the dielectric layer, so that a first structured dielectric layer is produced, removing (105) the first photoresist layer, applying (106) a second photoresist layer onto the first structured dielectric layer, generating (107) a second opening having a second width in the second photoresist layer by means of a second photolithography, wherein a second region of the dielectric layer is exposed, etching (108) the second region of the dielectric layer down to the surface of the semiconductor material so that a second structured dielectric layer is produced, removing (109) the second photoresist layer, and The first trench and the second trench are produced (110) starting from the second structured dielectric layer into the semiconductor material by means of a further etching step.

2. The method (100) according to claim 1, characterized in that: A marking layer is created within the dielectric layer, the marking layer marking the determined depth of the dielectric layer.

3. The method (100) according to claim 1 or 2, characterized in that: The first width and the second width are the same in size.

4. A method (200) for manufacturing a vertical power transistor having at least a first trench having a first trench depth and at least a second trench having a second trench depth, wherein: The first groove depth and the second groove depth have a difference of at least 30%, and the method has the following steps: applying a dielectric layer (201) onto the semiconductor material, applying (202) a photoresist layer onto the dielectric layer, A first opening having a first width and a second opening having a second width are generated (203) in the photoresist layer by means of photolithography, wherein the first opening and the second opening are alternately arranged spaced apart from each other in a lateral direction, wherein the first width and the second width are different in size, and the first opening exposes a first region of the dielectric layer and the second opening exposes a second region of the dielectric layer, etching (204) the first region and the second region of the dielectric layer so that a structured dielectric layer is produced, The first trench and the second trench are produced (211) starting from the structured dielectric layer and extending into the semiconductor material by means of a further etching step.

5. The method (100, 200) according to any one of the preceding claims, characterized in that The semiconductor material includes Si, SiC or GaN.

6. The method (100, 200) according to any one of the preceding claims, characterized in that The dielectric layer includes SiN or SiO2.

7. A vertical power transistor comprising a semiconductor material (301), at least a first trench (302) having a first trench depth and at least a second trench (303) having a second trench depth, characterized in that The first trench depth and the second trench depth have a difference of at least 30%.

8. The vertical power transistor according to claim 7, characterized in that: The semiconductor material (301) includes Si, SiC or GaN.