Rigid bending PCB and manufacturing method thereof
By designing specific line directions and copper layer layout on rigid substrates, combined with gong plate and press plate curve technology, the problem of difficult to control the tolerance of cracking and deep-controlled gong residual thickness during PCB bending process is solved, and high-efficiency and low-cost rigidity is achieved Bending PCB production meets the needs of high bending angle and bending resistance.
Patent Information
- Application Number
- CN202411301656.7
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-18
- Publication Date
- 2024-12-03
- Estimated Expiration
- Not applicable · inactive patent
AI Technical Summary
The existing multi-layer rigid PCB boards are prone to cracking during bending, and the tolerance of the residual thickness of the depth control gong is difficult to control, which affects electrical performance, has high manufacturing threshold and high cost.
Using the design of specific line directions and copper layer layout on the rigid substrate, the bend area with a predetermined thickness is produced through the gong plate process and the pressing plate curve process, combined with the soft green oil layer and the high resin content thin plate, and the deep-controlled gong plate process is used to subside Groove machining ensures strength and accuracy of the bending area.
It effectively improves the bending capability of the PCB, controls the residual thickness tolerance of the depth control gong at ±0.025mm, reduces production costs, simplifies the production process, and achieves a maximum bendable angle of 180° and 50 times without cracking.
Smart Images

Figure CN119071997A_ABST
Abstract
Description
Technical Field
[0001] The embodiments of the present invention relate to the technical field of PCB manufacturing methods, and in particular to a rigid bent PCB and a manufacturing method thereof. Background Art
[0002] PCB bending board is usually made of rigid-flexible board, which has both the durability of rigid PCB and the adaptability of flexible PCB. Moreover, the rigid-flexible board is light and thin, compact in structure, which helps to increase assembly flexibility, improve reliability, and realize three-dimensional assembly under different assembly conditions. It is especially suitable for the latest portable electronics and high-end medical and automotive equipment. Although the rigid-flexible board product is good, the manufacturing threshold is high. It requires both hard board and soft board to be made, and the production process is complicated and the cost is high.
[0003] The residual thickness tolerance of multi-layer rigid PCB boards is generally ±0.1mm. The uniformity of the residual thickness is difficult to control. If the residual thickness is too small, it is easy to damage the circuit and expose the copper, affecting the electrical performance. If the residual thickness is too large, the flexibility is poor and the substrate is prone to cracking when bent. The high-precision requirement of the depth control gong has always been a problem in machining. Summary of the invention
[0004] The technical problem to be solved by the embodiments of the present invention is to provide a method for manufacturing a rigid bending PCB, which can effectively improve the bending ability of the PCB.
[0005] A further technical problem to be solved by the embodiments of the present invention is to provide a rigid bendable PCB with good bending ability.
[0006] In order to solve the above technical problems, the present invention provides the following technical solutions: A method for manufacturing a rigid bending PCB, comprising the following steps: A first semi-finished product is obtained by forming a circuit pattern on a rigid substrate, wherein the rigid substrate comprises a first rigid region, a second rigid region, and bending regions respectively connected to the first rigid region and the second rigid region on opposite sides, wherein the circuit pattern comprises a first circuit pattern located in the first rigid region, a second circuit pattern located in the second rigid region, and a third circuit pattern located on one side surface of the bending region and correspondingly connected to the first circuit pattern and the second circuit pattern at opposite ends, wherein each circuit in the third circuit pattern extends in a straight line and is perpendicular to a bending center axis of the bending region when the bending region is bent; Using a gong plate process to process the outer edge of the PCB on the first semi-finished product to obtain a second semi-finished product; Using a plate bending process to make the surface of the second semi-finished product flat; and A second semi-finished product with a flat surface is fixed on a pad, and one side of the second semi-finished product provided with the third circuit pattern is attached to the pad. A controlled depth gong process is adopted and a groove is processed on the surface of the side of the bending area of the second semi-finished product away from the pad through two gong processes: rough gong and fine gong, so that the bending area has a predetermined thickness.
[0007] Furthermore, a copper layer having the same thickness as the copper of the third circuit pattern is provided in a non-circuit region on a surface of one side of the bending region where the third circuit pattern is provided.
[0008] Furthermore, the side surface of the second semi-finished product provided with the third circuit pattern is covered with a soft green oil layer, the soft green oil layer completely covers the bending area and the boundary of the soft green oil layer exceeds a predetermined size of the bending area.
[0009] Furthermore, during the rough gong process, a residual thickness of 0.05 mm is reserved in each direction of the designed trough area at the boundaries, and is not removed. During the fine gong process, the residual thickness is processed into place according to the median value of the residual thickness.
[0010] Furthermore, the rigid substrate is formed by laminating a plurality of thin plates, and densely arranged copper dots are provided on the laminating surface of each thin plate at a position corresponding to the bending area.
[0011] Furthermore, the thin plate is a 1080 or 2116 thin plate with a high resin content.
[0012] Furthermore, the specific operation control of the depth control gong plate includes: A height detection point is set outside the designed periphery of the sink trough to measure the actual board height in front of the gong board. The selection requirements of the height detection point are as follows: the height detection point is required to be selected on the copper surface covered with green oil, there is no hole or line within 3mm of the center of the height detection point, and the depth of the gong board is measured downward from the oil-covered copper surface; Number of detection points: For a trough with a maximum distance of ≤20mm in the width of the sink trough, 2 detection points are designed, and the detection points are selected at the appropriate point near the far end of the sink trough. When the sink trough size is greater than 20mm, the number of detection points is appropriately increased, and the detection point distance is required to be ≤20mm; Set up residual thickness gongs with detection points to measure wood fiberboard, and make regional height detection points on the wood fiberboard; The sinking grooves with different residual thickness requirements are made in "T" pattern. Both rough gong and fine gong are made in "T" pattern. The gong belt corresponds to the tool to directly add the residual thickness requirements. The gong plate depth is in metric units and is made according to the MI median value. The depth control gong belt is gonged downward from the board surface, and the depth is negative. The residual thickness control gong belt is gonged upward from the wood fiberboard, and the depth is positive. When gonging, the knife path is from right to left with upper and lower knives, and the knife spacing is 0.6mm; When processing the sink groove on the depth-controlled gong plate, a C-vertical flat-bottom milling cutter is used.
[0013] Furthermore, the fixing of the second semi-finished product with a flat surface on the backing plate specifically includes: Set up wooden pads; Leveling the plate surface of the backing plate using a leveling belt; and The second semi-finished product is placed on the surface of the pad and fixed on the pad by vacuum adsorption.
[0014] Furthermore, the tolerance of the bottom wall thickness of the trough is controlled within ±0.025 mm.
[0015] On the other hand, the present invention further provides a rigid-bent PCB, which is manufactured by the rigid-bent PCB manufacturing method as described in any one of the above items.
[0016] By adopting the above technical scheme, the embodiment of the present invention has at least the following beneficial effects: the present invention can well avoid the related lines from breaking when the bending area is bent accordingly by reasonably designing the line direction in the bending area; in addition, when the depth-controlled gong is used to sink the groove, the depth-controlled gong sinking accuracy can be effectively improved through two gong plate processes, namely, rough gong first and fine gong second. The residual thickness tolerance of the depth-controlled gong can be ±0.025mm, so that it is convenient to use a rigid substrate to make a rigid bending PCB, effectively replacing a soft-rigid combination board, making the production process simpler, reducing the production cost, and improving the production capacity. Moreover, according to testing, the maximum bending angle of the obtained rigid bending PCB can reach 180°, and it can withstand 50 bendings without cracking, which well meets the customer's assembly requirements. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the following briefly introduces the drawings required for use in the embodiments or the description of the prior art. Obviously, the drawings described below are some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0018] Figure 1 The present invention is a flowchart of an optional embodiment of the method for manufacturing a rigid-bend PCB.
[0019] Figure 2 This is a schematic structural diagram of a controlled deep gong sinking tank in an optional embodiment of the method for manufacturing a rigid-bent PCB of the present invention.
[0020] Figure 3 This is a schematic diagram of the structure of forming a copper layer in a bending area according to an embodiment of a method for manufacturing a rigid bending PCB of the present invention.
[0021] Figure 4The following are actual photos of rigid bending plates of different shapes at different bending angles manufactured according to an embodiment of the method for manufacturing a rigid bending PCB of the present invention.
[0022] Figure 5 This is a photo of a bending area of a rigid bending plate in a bending state, which is manufactured according to an embodiment of the method for manufacturing a rigid bending PCB of the present invention. DETAILED DESCRIPTION
[0023] In order to make the purpose, technical solution and advantages of the embodiments of the present invention clearer, the technical solution in the embodiments of the present invention will be clearly and completely described below in conjunction with the drawings in the embodiments of the present invention. Obviously, the described embodiments are part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] In addition, the term "and / or" in this article is only a description of the association relationship of associated objects, indicating that there can be three relationships. For example, A and / or B can represent: A exists alone, A and B exist at the same time, and B exists alone. In addition, the character " / " in this article, unless otherwise specified, generally means that the associated objects before and after are in an "or" relationship.
[0025] The embodiments of the present invention are further described in detail below in conjunction with the accompanying drawings.
[0026] like Figure 1 and Figure 2 As shown, an embodiment of the present invention provides a method for manufacturing a rigid bending PCB, comprising the following steps: S1, forming a circuit pattern, that is, forming a circuit pattern 3 on a rigid substrate 1 to obtain a first semi-finished product, wherein the rigid substrate 1 includes a first rigid region 10, a second rigid region 12, and bending regions 14 respectively connected to the first rigid region 10 and the second rigid region 12 on opposite sides, and the circuit pattern 3 includes a first circuit pattern 30 located in the first rigid region 10, a second circuit pattern 32 located in the second rigid region 12, and a third circuit pattern 34 located on one side of the bending region 14 and connected to the first circuit pattern 30 and the second circuit pattern 32 at opposite ends, and each line in the third circuit pattern 34 extends in a straight line and is perpendicular to the bending center axis of the bending region 14 when it is bent; S2, gong processing the board edge, that is, using the gong process to process the outer edge of the PCB on the first semi-finished product to obtain the second semi-finished product; S3, plate bending, i.e., using a plate bending process to make the surface of the second semi-finished product flat; and S4, controlled depth gong grooving, that is: fix the second semi-finished product with a flat surface on the pad, and affix one side of the second semi-finished product provided with the third circuit pattern to the pad, and adopt a controlled depth gong process and go through two gong processes, first rough gong and then fine gong, to machine a groove 16 on the surface of the bending area 14 of the second semi-finished product away from the pad so that the bending area 14 has a predetermined thickness.
[0027] The present invention can effectively avoid the relevant circuits from breaking when the bending area 14 is bent accordingly by reasonably designing the line direction in the bending area 14 (it can be understood that, according to the circuit design of the PCB itself, the circuit pattern mentioned here includes at least the outer layer circuit pattern, and also includes the inner layer circuit pattern when necessary); in addition, when the depth of the gong is controlled, the two gong processes of rough gong and fine gong can effectively improve the accuracy of the depth of the gong, and the residual thickness tolerance of the depth of the gong can be ±0.025mm, so that it is convenient to use the rigid substrate 1 to make a rigid bending PCB, effectively replacing the soft and hard combination board, making the production process simpler, reducing the production cost and improving the production capacity. Moreover, according to tests, the maximum bending angle of the obtained rigid bending PCB can reach 180° (such as Figure 4 As shown in the figure), it can withstand 50 bending times without cracking, which satisfies the assembly needs of customers.
[0028] In another embodiment of the present invention, Figure 3 As shown, a copper layer 36 having the same thickness as the copper of the third circuit pattern 34 is provided in a non-circuit region on a side surface of the bending region 14 having the third circuit pattern 34. In this embodiment, a copper layer having the same thickness as the copper of the circuit is also provided in the non-circuit region of the bending region 14, so that the bending region 14 can be subjected to balanced forces at various locations when being bent and can maintain synchronous deformation, thereby avoiding stress concentration and fracture of the copper of the circuit. Figure 5 shown.
[0029] In another embodiment of the present invention, Figure 2 As shown, the side surface of the second semi-finished product provided with the third circuit pattern 34 is covered with a soft green oil layer 5, and the soft green oil layer 5 completely covers the bending area 14 and the boundary of the soft green oil layer 5 exceeds the predetermined size of the bending area 14. In this embodiment, by providing the soft green oil layer 5, it is beneficial to improve the bending performance of the bending area 14, and prevent the ordinary ink covered in the conventional PCB processing process from bending, cracking, and whitening. Preferably, the predetermined size is not less than 1.0 mm.
[0030] In another embodiment of the present invention, Figure 2 As shown, during the roughing process, the width of the reserved residual thickness of the designed sink groove 16 area is 0.05mm (i.e. Figure 2The boundary shown by the dotted line A) is processed in place according to the median value of the residual thickness during the fine gong (i.e. Figure 2 The boundary is shown by the solid line B in the middle). In this embodiment, the machining accuracy of the gong plate can be effectively improved by reserving a residual thickness of appropriate width during the rough gong process and machining in place according to the median value of the residual thickness during the fine gong process.
[0031] In another embodiment of the present invention, the rigid substrate 1 is formed by laminating a plurality of thin plates, and a densely arranged copper point is provided on the laminating surface of each thin plate at a position corresponding to the bending area 14 and without a circuit pattern. In this embodiment, by laminating a plurality of thin plates to form the rigid substrate 1, it is advantageous to pre-form an inner layer circuit pattern on the plate surface of the thin plate when necessary, and by providing a densely arranged copper point on the laminating surface at a position corresponding to the bending area 14 and without a circuit pattern, it is advantageous to improve the uniformity of the laminating thickness.
[0032] In another embodiment of the present invention, the thin plate is a 1080 or 2116 thin plate with a high resin content. The thin plate with a high resin content is used in this embodiment, which is beneficial to improving the bending resistance. For non-laminated PCBs, a rigid substrate with a high resin content can also be used. Generally, a resin content greater than 50% (mass fraction) can be regarded as a high resin content. In the embodiment of the present invention, the preferred resin content is 55-70% (mass fraction).
[0033] In another embodiment of the present invention, the specific operation control of the depth control gong plate includes: A height detection point (also called a probe point) is set outside the designed periphery of the sink 16 to measure the actual board height in front of the gong plate. The selection requirements of the height detection point are as follows: the height detection point is required to be selected on the copper surface covered with green oil, and there is no hole or line within 3mm of the center of the height detection point. The depth of the gong plate should be measured downward from the oil-covered copper surface; the number of probe points: for a groove with a maximum distance of 16 ≤20mm in width, 2 probe points are designed. The probe points are selected at the position adjacent to the far end of the sink 16. When the size of the sink 16 is greater than 20mm, the number of probe points is appropriately increased, and the distance between the probe points is required to be ≤20mm. In specific implementation, the probe point coordinates X-Y- or regional probe points X-Y-G85 X-Y- (rectangular diagonal coordinates) can be set through the probe point instruction "T98" of the gong machine. The gong machine automatically increases the detection density in this rectangular area according to the density set by the machine. When selecting and formulating the regional control points, first confirm that there are no holes and line positions that need to be avoided within the range); Set up residual thickness gong with probe points to measure wood fiberboard, make regional height detection points on the wood fiberboard, add "M47" command after the probe is completed, and then produce the board; The sinking grooves with different residual thickness requirements are made in "T" pattern. Both rough gong and fine gong are made in "T" pattern. The gong belt corresponds to the tool to directly add the residual thickness requirements. The gong plate depth is in metric units and is made according to the MI median value. The depth control gong belt is gonged downward from the board surface, and the depth is negative. The residual thickness control gong belt is gonged upward from the wood fiberboard, and the depth is positive. When gonging, the knife path is from right to left with upper and lower knives, and the knife spacing is 0.6mm; When processing the sink groove on the depth-controlled gong plate, a C-vertical flat-bottom milling cutter is used.
[0034] The relevant control parameters of the depth control gong plate are shown in the following table:
[0035] This embodiment optimizes and controls each link of the depth control gong sinking trough, and can well control the processing quality and precision of the sinking trough 16. For example, the C-vertical flat bottom milling cutter is used, and the bottom surface of the depth control gong is smoother and flatter than that of the ordinary fishtail type milling cutter, and the residual thickness uniformity is better controlled, the bending force is uniform, and the bending resistance is good; In another embodiment of the present invention, fixing the second semi-finished product with a flat surface on the backing plate specifically includes: Set up wooden pads; Leveling the plate surface of the backing plate using a leveling belt; and The second semi-finished product is placed on the surface of the pad and fixed on the pad by vacuum adsorption.
[0036] In this embodiment, the pad gong is leveled and the second semi-finished product to be processed is fixed on the pad gong by the vacuum adsorption function of the machine, thereby preventing the influence of the pad thickness tolerance and the plate bending hole on the depth control gong accuracy. The Z-axis optical ruler of the gong machine in front of the gong automatically detects the point of the pad, automatically detects the height and automatically calculates the compensation depth, so as to better control the uniformity of the residual thickness of the sink.
[0037] In another embodiment of the present invention, the tolerance of the bottom wall thickness of the sink 16 is controlled within ±0.025 mm. By adopting the above-mentioned depth-controlled gong sink operation control, the tolerance of the bottom wall thickness of the sink 16 can be controlled within ±0.025 mm, and the processability of the bottom wall thickness is conducive to ensuring the bendability.
[0038] On the other hand, an embodiment of the present invention further provides a rigid bending PCB, which is manufactured by the rigid bending PCB manufacturing method as described in any of the above embodiments. Figure 4 shown.
[0039] After testing, the rigid bending PCB produced by the rigid bending PCB production method described in any of the above embodiments has good bending performance, the maximum bending angle can reach 180°, and it can withstand 50 bendings without cracking, which well meets the customer's assembly requirements. The corresponding relationship between the relevant bending angle and the bending area length is shown in the following table:
[0040] The complete process flow of PCB production generally includes: board opening, printing inner layer circuits, etching, pressing, drilling, copper plate electroplating, printing outer layer circuits, graphic electroplating, etching, coating of solder mask ink, coating of soft green oil layer, gong periphery, initial board washing, plate bending, pad milling, controlled depth gong sinking tank, secondary board washing, testing, FQC and other steps. It can be understood that the present invention application only improves some of the steps, and the improvement methods include: optimizing the original traditional steps (for example: printing outer layer circuits, pressing, printing inner layer circuits, gong periphery, pad milling, controlled depth gong sinking tank, etc.), and adding new steps (for example: coating of soft green oil layer, plate bending), so the description focuses on these corresponding improved steps, and no further elaboration is given for the steps that are the same as the traditional steps.
[0041] The embodiments of the present invention are described above in conjunction with the accompanying drawings, but the present invention is not limited to the above-mentioned specific implementation methods. The above-mentioned specific implementation methods are merely illustrative and not restrictive. Under the enlightenment of the present invention, ordinary technicians in this field can also make many variations without departing from the creative purpose of the present invention and the scope of protection of the claims, which all fall within the scope of protection of this patent.
Claims
1. A method for manufacturing a rigid bending PCB, characterized in that: The following steps are involved: A first semi-finished product is obtained by forming a circuit pattern on a rigid substrate, wherein the rigid substrate comprises a first rigid region, a second rigid region, and bending regions respectively connected to the first rigid region and the second rigid region on opposite sides, wherein the circuit pattern comprises a first circuit pattern located in the first rigid region, a second circuit pattern located in the second rigid region, and a third circuit pattern located on one side surface of the bending region and correspondingly connected to the first circuit pattern and the second circuit pattern at opposite ends, wherein each circuit in the third circuit pattern extends in a straight line and is perpendicular to a bending center axis of the bending region when the bending region is bent; Using a gong plate process to process the outer edge of the PCB on the first semi-finished product to obtain a second semi-finished product; Using a plate bending process to make the surface of the second semi-finished product flat; and A second semi-finished product with a flat surface is fixed on a pad, and one side of the second semi-finished product provided with the third circuit pattern is attached to the pad. A controlled depth gong process is adopted and a groove is processed on the surface of the side of the bending area of the second semi-finished product away from the pad through two gong processes: rough gong and fine gong, so that the bending area has a predetermined thickness.
2. The method for manufacturing a rigid bending PCB according to claim 1, characterized in that: A copper layer having the same thickness as the copper of the third circuit pattern is provided in a non-circuit region on a surface of one side of the bending region where the third circuit pattern is provided.
3. The method for manufacturing a rigid bending PCB according to claim 2, characterized in that: The side surface of the second semi-finished product provided with the third circuit pattern is covered with a soft green oil layer, the soft green oil layer completely covers the bending area and the boundary of the soft green oil layer exceeds a predetermined size of the bending area.
4. The method for manufacturing a rigid bending PCB according to claim 1, characterized in that: During the roughing process, a residual thickness of 0.05mm is reserved in all directions of the designed trough area, and is not removed. During the fine gong process, the residual thickness is processed into place according to the median value of the residual thickness.
5. The method for manufacturing a rigid bending PCB according to claim 1, characterized in that: The rigid substrate is formed by pressing a plurality of thin plates together, and densely arranged copper dots are provided at the position corresponding to the bending area on the pressing surface of each thin plate.
6. The method for manufacturing a rigid bending PCB according to claim 5, characterized in that: The thin plate is a 1080 or 2116 thin plate with high resin content.
7. The method for manufacturing a rigid bending PCB according to claim 1, characterized in that: The specific operation control of the depth control gong plate includes: A height detection point is set outside the designed periphery of the sink trough to measure the actual board height in front of the gong board. The selection requirements of the height detection point are as follows: the height detection point is required to be selected on the copper surface covered with green oil, there is no hole or line within 3mm of the center of the height detection point, and the depth of the gong board is measured downward from the oil-covered copper surface; Number of detection points: For a trough with a maximum distance of ≤20mm in the width of the sink trough, 2 detection points are designed, and the detection points are selected at the appropriate point near the far end of the sink trough. When the sink trough size is greater than 20mm, the number of detection points is appropriately increased, and the detection point distance is required to be ≤20mm; Set up residual thickness gongs with detection points to measure wood fiberboard, and make regional height detection points on the wood fiberboard; The troughs with different residual thickness requirements are made in "T" pattern. Both rough and fine gongs are made in "T" pattern. The gong belt corresponds to the tool to directly add the residual thickness requirements. The gong plate depth is in metric units and is made according to the MI median value. The depth control gong belt gongs downward from the board surface, and the depth uses a negative value. The residual thickness control gong belt gongs upward from the wood fiberboard, and the depth uses a positive value. When gonging, the knife path is from right to left with upper and lower knives, and the knife spacing is 0.6mm; When processing the sink groove on the depth-controlled gong plate, a C-vertical flat-bottom milling cutter is used.
8. The method for manufacturing a rigid bending PCB according to claim 1, characterized in that: The method of fixing the second semi-finished product with a flat surface on the backing plate specifically includes: Set up wooden pads; Leveling the plate surface of the backing plate using a leveling belt; and The second semi-finished product is placed on the surface of the pad and fixed on the pad by vacuum adsorption.
9. The method for manufacturing a rigid bending PCB according to claim 1, characterized in that: The tolerance of the bottom wall thickness of the sink is controlled within ±0.025 mm.
10. A rigid bending PCB, characterized in that: The rigid-bend PCB is manufactured by the rigid-bend PCB manufacturing method as described in any one of claims 1 to 9.
Citation Information
Patent Citations
Flexible circuit board and mobile terminal
CN105430883A
Depth control method for copper block of buried copper plate
CN108289376A
Half-bent printed circuit board and making method thereof
CN108419384A
Manufacture method of semi-soft board
CN110856377A
Technological process for manufacturing rigid bent plate