Process for treating LED chip wastewater by using composite material
Through the composite material treatment process, the synergistic effects of materials such as chitosan, vermiculite, activated carbon, nano-alumina and nano-iron oxide are solved, and the complexity of wastewater treatment in the LED industry has been achieved, efficient purification and recycling are achieved, ensuring that wastewater meets standards. Emissions and environmental safety.
Patent Information
- Application Number
- CN202411197948.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-08-29
AI Technical Summary
The LED industry produces a wide variety of wastewater, complex water quality, and the existing technology is difficult to effectively treat and control, resulting in an increase in pollutant emissions and affecting the environment and enterprise development.
Using composite material treatment technology, including crude filtration, regulation tank treatment, ultrafiltration membrane filtration, reverse osmosis concentration, ion exchange resin treatment and ozone sterilization, using materials such as chitosan, vermiculite, activated carbon, nanoalumina and nanoiron oxide. The synergistic effect of adsorbing and removing heavy metal ions, organic pollutants and suspended substances in wastewater.
It realizes efficient purification and recycling of wastewater, ensures that the treated wastewater meets the discharge standards, the materials are non-toxic and easy to recycle, and will not cause secondary pollution to the environment, improving the efficiency and stability of wastewater treatment.
Smart Images

Figure SMS_1
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of chip wastewater treatment and relates to a process for treating LED chip wastewater using a composite material. Background Art
[0002] Light Emitting Diode (LED) is a semiconductor light-emitting device that converts electrical energy into light energy. With the improvement of LED technology, as a new type of high-efficiency solid light source, it is increasingly used in the two major fields of lighting and display. Compared with existing lighting equipment, LED lighting has the advantages of energy saving, low power consumption, safety and environmental protection, long life, strong structure, and saving installation space. At the same time, due to the high unit water consumption of LED products, the substantial increase in product output will inevitably cause a large amount of pollutants to be discharged during the production process, and the discharge of industrial wastewater has also shown a leap-forward growth. How to effectively treat these wastewaters while the industry is developing has become one of the main issues facing the industry and enterprises.
[0003] As an emerging high-tech industry, the LED industry has developed rapidly and inevitably produced a large amount of wastewater pollutants. How to effectively control and treat wastewater has also become a major issue in the industry. Due to different production processes and differences in the use of raw materials and chemicals, the LED industry wastewater has a wide variety of types and relatively complex water quality. Summary of the invention
[0004] The purpose of the present invention is to provide a process for treating LED chip wastewater using a composite material, which has the characteristics of high adsorption efficiency.
[0005] The purpose of the present invention can be achieved through the following technical solutions:
[0006] A process for treating LED chip wastewater using a composite material, the specific process of the process is as follows:
[0007] S1: The LED chip wastewater is firstly filtered through the grid to remove large particles of impurities and sediments in the wastewater;
[0008] S2: Collect the wastewater after coarse filtration, pass it into regulating tank 1, add 10% alkali solution by mass into regulating tank 1; then pass it into regulating tank 2, add 10% acid solution by mass into regulating tank 2, collect the wastewater after adjustment, add the composite material into the wastewater, and stir for 0.5h;
[0009] S3: filtering the wastewater treated in S2 through an ultrafiltration membrane to obtain a clear liquid;
[0010] S4: The clear liquid obtained in S3 is concentrated by a reverse osmosis membrane to a concentration of 2.5-6 times;
[0011] S5: passing the concentrated clear liquid from S4 through an ion exchange resin;
[0012] S6: passing ozone into the clear liquid obtained in S5 for sterilization, and discharging the treated waste liquid;
[0013] The preparation method of the composite material in S2 is as follows:
[0014] S2.1: Dissolve chitosan in acetic acid solution, stir at 150 r / min for 0.5 h, and prepare a mixed solution A with a mass fraction of 30-50%;
[0015] S2.2: Grind the vermiculite in a ball mill at a speed of 400 r / min for 0.5 h to obtain vermiculite powder with a particle size of 150 mesh;
[0016] S2.3: Add vermiculite powder into mixed solution A, wherein the mass ratio of vermiculite to chitosan is 2:3, and then add 0.5-2wt% glutaraldehyde, slowly heat from room temperature to 60°C and stir for 2h to obtain solid-liquid mixture B, filter and separate the solid-liquid mixture B, wash the filter residue with deionized water, and dry at 80°C for 12h to obtain mixture C;
[0017] S2.4: Mixture C, activated carbon, nano-aluminum oxide and nano-iron oxide in a mass ratio of 2:1:1:1 and grind them in a ball mill at a speed of 400 r / min for 0.5 h to obtain mixture D;
[0018] S2.5: Press the mixture D into a sheet at room temperature and a pressure of 10 MPa to obtain the composite material.
[0019] Furthermore, the alkaline solution in S2 is one or more of ammonia water, sodium hydroxide solution, and potassium hydroxide solution.
[0020] Furthermore, the acid solution in S2 is one or more of hydrochloric acid solution and sulfuric acid solution.
[0021] Furthermore, the ultrafiltration membrane in S3 is a ceramic membrane, and the pore size of the ceramic membrane is 4 to 10 nm.
[0022] Furthermore, the ion exchange resin in S5 is a cation exchange resin.
[0023] Furthermore, the ozone introduction rate in S6 is 20 m / s, and the sterilization time is 1 h.
[0024] Furthermore, the volume fraction of the acetic acid solution in S2.1 is 2%.
[0025] Furthermore, the heating rate of slowly heating from room temperature to 60° C. in S2.3 is 2° C. / min.
[0026] Furthermore, the particle size of the mixture D in S2.4 is 150 mesh.
[0027] The present invention prepares a composite material, which combines multiple materials such as chitosan, vermiculite, activated carbon, nano-alumina and nano-iron oxide, and has a higher adsorption capacity and a faster adsorption rate. The composite material can simultaneously treat multiple pollutants in wastewater, including heavy metal ions, organic pollutants and suspended matter. The material itself is non-toxic and harmless, and is easy to recycle and treat, and will not cause secondary pollution to the environment.
[0028] Chitosan is a natural polymer flocculant with a large number of hydroxyl and amino groups distributed on its molecular chain. These groups can form stable complexes or chelates with heavy metal ions (such as zinc, lead, chromium, etc.) in wastewater, thereby removing them from wastewater. Chitosan can also adsorb organic pollutants in wastewater through hydrogen bonding, ion exchange, etc.; in addition, chitosan carries a positive charge in the solution, which can neutralize negatively charged particles (such as suspended matter, colloids, etc.) in wastewater, causing them to aggregate into larger flocs, which is convenient for subsequent precipitation and separation;
[0029] After grinding, vermiculite has a large specific surface area and pore structure, which can provide abundant adsorption sites and enhance the adsorption capacity of the composite material. At the same time, the layered structure of vermiculite also has a certain filtering effect, which can intercept suspended matter and colloidal particles in wastewater. After vermiculite and chitosan are compounded, the two have a synergistic effect in adsorption performance. Vermiculite increases the adsorption area of chitosan and improves its adsorption efficiency. Chitosan further enhances the adsorption performance of the composite material through its adsorption mechanism.
[0030] Therefore, the present invention first prepares the chitosan-vermiculite composite, and adds glutaraldehyde as a cross-linking agent during the preparation process to form a stronger chemical bond between chitosan and vermiculite, thereby improving the stability and mechanical strength of the composite material. At the same time, the cross-linking effect also helps to optimize the pore structure of the composite material and further improve its adsorption performance.
[0031] Activated carbon, nano-alumina and nano-iron oxide are also added to the composite material of the present invention. The activated carbon removes organic pollutants and chromaticity in wastewater through physical adsorption and chemical adsorption; the nano-alumina has a high specific surface area and surface activity and has an excellent adsorption effect on heavy metal ions; the nano-iron oxide has a certain catalytic effect and can promote the degradation of organic pollutants.
[0032] Chitosan vermiculite complex and activated carbon can work together to remove organic matter and heavy metal ions in wastewater. Chitosan vermiculite complex forms chemical bonds or electrostatic effects with heavy metal ions and organic matter in wastewater through its surface functional groups such as amino and hydroxyl groups to achieve adsorption; while activated carbon uses its porous structure and high specific surface area to capture pollutants in wastewater through physical adsorption. The combination of the two can expand the adsorption range, improve the adsorption efficiency, and form a synergistic adsorption mechanism. The synergistic effect between them can enhance the adsorption effect and improve the efficiency of wastewater treatment. Nano-alumina and nano-iron oxide can promote oxidation reactions in wastewater as catalysts. Nano-alumina can catalyze the oxidation reaction of organic matter in wastewater, while nano-iron oxide can accelerate the oxidation reaction. When the two exist at the same time, they can promote each other, form a synergistic catalytic oxidation mechanism, and improve the efficiency of wastewater treatment. In the catalytic oxidation process, the microorganisms adsorbed on the surface of activated carbon can use the oxidants catalyzed by nano-alumina and nano-iron oxide to further degrade organic matter, thereby combining biodegradation with catalytic oxidation. At the same time, they can also be combined with activated carbon and chitosan vermiculite complexes to remove organic matter in wastewater by combining catalytic oxidation with adsorption. Nano-alumina and nano-iron oxide remove heavy metal ions by generating insoluble precipitates. At the same time, chitosan vermiculite complexes and activated carbon participate in this process and further remove heavy metal pollution in wastewater through adsorption.
[0033] In the present invention, large suspended matter such as solid waste and debris in wastewater is firstly removed by grid filtration to prevent clogging of subsequent treatment equipment, and then the water volume and water quality of wastewater are adjusted by two regulating tanks to make the subsequent treatment process more stable, and then composite materials are added to adsorb and remove suspended matter, colloidal substances, heavy metal ions and organic pollutants in wastewater; after the adsorption is completed, suspended matter, bacteria, colloidal substances and some macromolecular organic matter in wastewater are removed by ultrafiltration treatment; deep desalination is carried out by reverse osmosis treatment to remove impurities such as inorganic salts, organic matter, viruses in wastewater; and residual pollutants such as heavy metal ions in wastewater are removed by cation exchange resin; finally, ozone is used for sterilization to discharge the treated wastewater that meets the standards.
[0034] Beneficial effects of the present invention:
[0035] The present invention uses a composite material to treat LED chip wastewater. The chitosan, vermiculite, activated carbon and nano-alumina in the composite material adsorb heavy metal ions, organic pollutants and suspended matter in the wastewater onto the surface or pores of the material through physical adsorption and chemical adsorption. The present invention first prepares a chitosan-vermiculite composite, and adds glutaraldehyde as a cross-linking agent to form a stronger chemical bond between chitosan and vermiculite, thereby improving the stability and mechanical strength of the chitosan-vermiculite composite. The cross-linking effect also helps to optimize the pore structure of the chitosan-vermiculite composite, further improving its adsorption performance. Then, activated carbon, nano-alumina and nano-iron oxide are added to remove organic pollutants, chromaticity and heavy metal ions in the wastewater while promoting the degradation of organic pollutants.
[0036] The present invention realizes efficient purification, recycling and reuse of wastewater and biosafety assurance through comprehensive application of physical, chemical and biological means. DETAILED DESCRIPTION
[0037] In order to further illustrate the technical means and effects adopted by the present invention to achieve the predetermined invention purpose, the specific implementation methods, structures, features and effects of the present invention are described in detail below in combination with the embodiments.
[0038] Example 1
[0039] S1: The LED chip wastewater is firstly filtered through the grid to remove large particles of impurities and sediments in the wastewater;
[0040] S2: Collect the wastewater after coarse filtration, pass it into regulating tank 1, add 10% ammonia water by mass into regulating tank 1; then pass it into regulating tank 2, add 10% hydrochloric acid solution by mass into regulating tank 2, collect the wastewater after adjustment, add the composite material into the wastewater, and stir for 0.5h;
[0041] S3: The wastewater treated by S2 is filtered through an ultrafiltration membrane, the ultrafiltration membrane is a ceramic membrane, the pore size of the ceramic membrane is 4nm, and a clear liquid is obtained after filtration;
[0042] S4: The clear liquid obtained in S3 is concentrated by 5 times through a reverse osmosis membrane;
[0043] S5: passing the concentrated clear liquid from S4 through a cation exchange resin;
[0044] S6: Pass ozone into the clear liquid obtained in S5 for sterilization, the ozone flow rate is 20m / s, the sterilization time is 1h, and the treated waste liquid is discharged;
[0045] The preparation method of the composite material in S2 is as follows:
[0046] S2.1: Dissolve chitosan in acetic acid solution with a volume fraction of 2%, stir at a speed of 150 r / min for 0.5 h, and prepare a mixed solution A with a mass fraction of 40%;
[0047] S2.2: Grind the vermiculite in a ball mill at a speed of 400 r / min for 0.5 h to obtain vermiculite powder with a particle size of 150 mesh;
[0048] S2.3: Add vermiculite powder into mixed solution A, wherein the mass ratio of vermiculite to chitosan is 2:3, and then add 1wt% glutaraldehyde, slowly heat up from room temperature to 60°C and stir for 2h, with a heating rate of 2°C / min, to obtain a solid-liquid mixture B, filter and separate the solid-liquid mixture B, wash the filter residue with deionized water, and dry at 80°C for 12h to obtain a mixture C;
[0049] S2.4: Mixture C, activated carbon, nano-alumina and nano-iron oxide are mixed and ground in a mass ratio of 2:1:1:1, and ground in a ball mill at a speed of 400 r / min for 0.5 h to obtain mixture D, wherein the particle size of mixture D is 150 mesh;
[0050] S2.5: Press the mixture D into a sheet at room temperature and a pressure of 10 MPa to obtain the composite material.
[0051] Example 2
[0052] S1: The LED chip wastewater is firstly filtered through the grid to remove large particles of impurities and sediments in the wastewater;
[0053] S2: Collect the wastewater after coarse filtration, pass it into regulating tank 1, add a 10% sodium hydroxide solution by mass into regulating tank 1; then pass it into regulating tank 2, add a 10% sulfuric acid solution by mass into regulating tank 2, collect the wastewater after adjustment, add the composite material into the wastewater, and stir for 0.5h;
[0054] S3: The wastewater treated by S2 is filtered through an ultrafiltration membrane, the ultrafiltration membrane is a ceramic membrane, the pore size of the ceramic membrane is 10nm, and a clear liquid is obtained after filtration;
[0055] S4: The clear liquid obtained in S3 is concentrated by a reverse osmosis membrane to 2.5 times;
[0056] S5: passing the concentrated clear liquid from S4 through a cation exchange resin;
[0057] S6: Pass ozone into the clear liquid obtained in S5 for sterilization, the ozone flow rate is 20m / s, the sterilization time is 1h, and the treated waste liquid is discharged;
[0058] The preparation method of the composite material in S2 is as follows:
[0059] S2.1: Dissolve chitosan in acetic acid solution with a volume fraction of 2%, stir at a speed of 150 r / min for 0.5 h, and prepare a mixed solution A with a mass fraction of 30%;
[0060] S2.2: Grind the vermiculite in a ball mill at a speed of 400 r / min for 0.5 h to obtain vermiculite powder with a particle size of 150 mesh;
[0061] S2.3: Add vermiculite powder into mixed solution A, wherein the mass ratio of vermiculite to chitosan is 2:3, and then add 0.5wt% glutaraldehyde, slowly heat up from room temperature to 60°C and stir for 2h, with a heating rate of 2°C / min, to obtain a solid-liquid mixture B, filter and separate the solid-liquid mixture B, wash the filter residue with deionized water, and dry at 80°C for 12h to obtain a mixture C;
[0062] S2.4: Mixture C, activated carbon, nano-alumina and nano-iron oxide are mixed and ground in a mass ratio of 2:1:1:1, and ground in a ball mill at a speed of 400 r / min for 0.5 h to obtain mixture D, wherein the particle size of mixture D is 150 mesh;
[0063] S2.5: Press the mixture D into a sheet at room temperature and a pressure of 10 MPa to obtain the composite material.
[0064] Example 3
[0065] S1: The LED chip wastewater is firstly filtered through the grid to remove large particles of impurities and sediments in the wastewater;
[0066] S2: Collect the wastewater after coarse filtration, pass it into regulating tank 1, add a 10% potassium hydroxide solution by mass into regulating tank 1; then pass it into regulating tank 2, add a 10% hydrochloric acid solution by mass into regulating tank 2, collect the wastewater after adjustment, add the composite material into the wastewater, and stir for 0.5h;
[0067] S3: The wastewater treated by S2 is filtered through an ultrafiltration membrane, the ultrafiltration membrane is a ceramic membrane, the pore size of the ceramic membrane is 7nm, and a clear liquid is obtained after filtration;
[0068] S4: The clear liquid obtained in S3 is concentrated by a reverse osmosis membrane and concentrated 6 times;
[0069] S5: passing the concentrated clear liquid from S4 through a cation exchange resin;
[0070] S6: Pass ozone into the clear liquid obtained in S5 for sterilization, the ozone flow rate is 20m / s, the sterilization time is 1h, and the treated waste liquid is discharged;
[0071] The preparation method of the composite material in S2 is as follows:
[0072] S2.1: Dissolve chitosan in acetic acid solution with a volume fraction of 2%, stir at a speed of 150 r / min for 0.5 h, and prepare a mixed solution A with a mass fraction of 50%;
[0073] S2.2: Grind the vermiculite in a ball mill at a speed of 400 r / min for 0.5 h to obtain vermiculite powder with a particle size of 150 mesh;
[0074] S2.3: Add vermiculite powder into mixed solution A, wherein the mass ratio of vermiculite to chitosan is 2:3, and then add 2wt% glutaraldehyde, slowly heat up from room temperature to 60°C and stir for 2h, and the heating rate is 2°C / min to obtain solid-liquid mixture B, filter and separate the solid-liquid mixture B, wash the filter residue with deionized water, and dry at 80°C for 12h to obtain mixture C;
[0075] S2.4: Mixture C, activated carbon, nano-alumina and nano-iron oxide are mixed and ground in a mass ratio of 2:1:1:1, and ground in a ball mill at a speed of 400 r / min for 0.5 h to obtain mixture D, wherein the particle size of mixture D is 150 mesh;
[0076] S2.5: Press the mixture D into a sheet at room temperature and a pressure of 10 MPa to obtain the composite material.
[0077] Comparative Example 1
[0078] In this comparative example, no vermiculite was added during the preparation of the composite material, and the remaining steps were consistent with those of Example 1.
[0079] Comparative Example 2
[0080] In this comparative example, chitosan was not added during the preparation of the composite material, and the remaining steps were consistent with those of Example 1.
[0081] Comparative Example 3
[0082] In this comparative example, no activated carbon was added during the preparation of the composite material, and the remaining steps were consistent with those of Example 1.
[0083] Comparative Example 4
[0084] In this comparative example, nano-alumina was not added in the preparation of the composite material, and the remaining steps were consistent with those in Example 1.
[0085] Comparative Example 5
[0086] In this comparative example, nano iron oxide is not added in the preparation of the composite material, and the remaining steps are consistent with those in Example 1.
[0087] The discharged waste liquid was tested according to GB 39731-2020 standard for the embodiments and comparative examples, and the experimental results are summarized in the following table:
[0088]
[0089] Experiments have shown that the addition of composite materials has significantly improved the effect of wastewater treatment.
[0090] The above description is only a preferred embodiment of the present invention and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technical personnel in this field can make some changes or modify the technical contents disclosed above into equivalent embodiments without departing from the scope of the technical solution of the present invention. However, any brief modifications, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the scope of the technical solution of the present invention.
Claims
1. A process for treating LED chip wastewater using a composite material, characterized in that: The specific process of the process is as follows: S1: The LED chip wastewater is firstly filtered through the grid to remove large particles of impurities and sediments in the wastewater; S2: Collect the wastewater after coarse filtration, pass it into regulating tank 1, add 10% alkali solution by mass into regulating tank 1; then pass it into regulating tank 2, add 10% acid solution by mass into regulating tank 2, collect the wastewater after adjustment, add the composite material into the wastewater, and stir for 0.5h; S3: filtering the wastewater treated in S2 through an ultrafiltration membrane to obtain a clear liquid; S4: The clear liquid obtained in S3 is concentrated by a reverse osmosis membrane to a concentration of 2.5-6 times; S5: passing the concentrated clear liquid from S4 through an ion exchange resin; S6: passing ozone into the clear liquid obtained in S5 for sterilization, and discharging the treated waste liquid; The preparation method of the composite material in S2 is as follows: S2.1: Dissolve chitosan in acetic acid solution, stir at 150 r / min for 0.5 h, and prepare a mixed solution A with a mass fraction of 30-50%; S2.2: Grind the vermiculite in a ball mill at a speed of 400 r / min for 0.5 h to obtain vermiculite powder with a particle size of 150 mesh; S2.3: Add vermiculite powder into mixed solution A, wherein the mass ratio of vermiculite to chitosan is 2:3, and then add 0.5-2wt% glutaraldehyde, slowly heat from room temperature to 60°C and stir for 2h to obtain solid-liquid mixture B, filter and separate the solid-liquid mixture B, wash the filter residue with deionized water, and dry at 80°C for 12h to obtain mixture C; S2.4: Mixture C, activated carbon, nano-aluminum oxide and nano-iron oxide in a mass ratio of 2:1:1:1 and grind them in a ball mill at a speed of 400 r / min for 0.5 h to obtain mixture D; S2.5: Press the mixture D into a sheet at room temperature and a pressure of 10 MPa to obtain the composite material.
2. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The alkali solution in S2 is one or more of ammonia water, sodium hydroxide solution and potassium hydroxide solution.
3. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The acid solution in S2 is one or more of hydrochloric acid solution and sulfuric acid solution.
4. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The ultrafiltration membrane in S3 is a ceramic membrane, and the pore size of the ceramic membrane is 4-10 nm.
5. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The ion exchange resin in S5 is a cation exchange resin.
6. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The ozone flow rate in S6 is 20 m / s, and the sterilization time is 1 h.
7. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The volume fraction of the acetic acid solution in S2.1 is 2%.
8. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The heating rate of slowly heating from room temperature to 60°C in S2.3 is 2°C / min.
9. The process for treating LED chip wastewater using a composite material according to claim 1, characterized in that: The particle size of the mixture D in S2.4 is 150 mesh.
Citation Information
Patent Citations
Modified vermiculite mercury removal adsorbent, preparation method and application thereof
CN104888717A
Iron modified chitosan / vermiculite composite material capable of removing anionic and cationic heavy metals at same time and preparation method and application thereof
CN108620033A
Preparation method of catalyst for removing ammonia nitrogen in desulfurization waste water through Fenton-like reaction
CN109364926A
Reclaimed water zero discharge treatment method and device