Die structure and process method of aluminum alloy low-pressure metal type tensile test piece

By designing the structure and process method of aluminum alloy low-pressure metal-type tensile test piece mold, the problem that existing molds cannot effectively detect the performance of low-pressure metal-type aluminum alloy is solved, and the effect of efficient detection and cost reduction without destroying castings is achieved. .

CN119086204AInactive Publication Date: 2024-12-06CHINA FAW CO LTD +1
View PDF 6 Cites 0 Cited by

Patent Information

Application Number
CN202411190806.1
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-28
Publication Date
2024-12-06
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

The existing tensile test rod sample molds are gravity metal molds, and they cannot effectively prepare the performance of low-pressure metal aluminum alloy castings, which are limited by the casting method and cooling conditions.

Method used

A mold structure of aluminum alloy low-pressure metal-type tensile test piece is designed, including a lower mold assembly and an upper mold assembly. It is fixed on the furnace cover by an L-shaped positioning block, and a gate sleeve made of ceramic material is used to prevent the aluminum liquid from being advanced. Cool and low pressure casting is carried out through specific steps and pressure stages to ensure the integrity and performance of the test piece.

Benefits of technology

It realizes efficient detection of thin-walled low-pressure metal-type aluminum alloy materials without destroying the castings, improving detection efficiency and reducing production costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119086204A_ABST
    Figure CN119086204A_ABST
Patent Text Reader

Abstract

The invention discloses a die structure and process method of an aluminum alloy low-pressure metal mold tensile test piece, and belongs to the technical field of aluminum alloy manufacturing, the die structure comprises a lower die assembly, the lower die assembly can be fixed on a furnace cover through an L-shaped positioning block, and the top of the lower die assembly can be in die assembly fit with an upper die assembly. The invention discloses a die structure and a process method of an aluminum alloy low-pressure metal mold tensile test piece, which can realize the preparation of a thin-wall type low-pressure metal mold aluminum alloy material tensile test piece, and can realize the performance detection of an aluminum alloy low-pressure metal mold process under the condition of not damaging a casting. The detection efficiency is improved; and the production cost is reduced.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention discloses a die structure and a process method for an aluminum alloy low-pressure metal mold tensile test piece, and belongs to the technical field of aluminum alloy manufacturing. Background Art

[0002] With the development of lightweight automobiles, the integration and thin-walling of castings are the main ways to achieve lightweight. The molding processes of aluminum alloy castings include gravity sand molds, low-pressure sand molds, low-pressure metal molds, and high-pressure casting. In order to make castings have excellent performance, low cost and high production efficiency, low-pressure metal mold casting has gradually become a commonly used casting production process. With the widespread use of thin-walled aluminum alloy castings, the performance requirements of castings are getting higher and higher. At present, the performance test of thin-walled parts can only be sampled on the main casting. Due to the size and structure of the casting, it is sometimes difficult to take out the main sample, resulting in the inability to test the casting performance. The commonly used tensile test bar specimen mold is a gravity metal mold mold. Due to the limitations of the casting method and cooling conditions, it is impossible to prepare a representative low-pressure metal mold casting performance. Summary of the invention

[0003] The purpose of the present invention is to solve the problem that the existing commonly used tensile test bar specimen mold is a gravity metal mold, which is limited by the casting method and cooling conditions and cannot prepare a representative low-pressure metal mold casting performance. A mold structure and process method for an aluminum alloy low-pressure metal mold tensile test piece are proposed.

[0004] The problem to be solved by the present invention is achieved by the following technical solutions:

[0005] The technical solution of the present invention is as follows:

[0006] According to a first aspect of an embodiment of the present invention, a mold structure for an aluminum alloy low-pressure metal mold tensile test piece is provided, comprising a lower mold assembly, wherein the lower mold assembly can be fixed on a furnace cover by an L-shaped positioning block, and the top of the lower mold assembly can be molded together with an upper mold assembly.

[0007] Preferably, the lower mold assembly includes a lower mold base plate with a gate in the middle, a gate sleeve matching the gate is provided on the top of the lower mold base plate, the gate sleeve is closed and arranged on the lower mold base plate through a lower mold positioning plate, a test piece positioning groove is provided on the lower mold positioning plate, and a through hole corresponding to the gate is provided in the test piece positioning groove.

[0008] Preferably, the upper mold assembly includes an upper mold base plate, four connecting blocks are symmetrically arranged on the top of the upper mold base plate, a pressure block is arranged between the four connecting blocks, a push rod is arranged in the middle of the pressure block, and limiting columns are arranged near the four corners respectively, a test piece casting cavity is arranged at the bottom of the upper mold base plate, an ejection hole and an exhaust hole cooperating with the push rod are arranged at the bottom of the test piece casting cavity, the upper mold base plate is provided with a limiting hole cooperating with the limiting column, support blocks are symmetrically arranged between the pressure block and the upper mold base plate, a test piece positioning block cooperating with the test piece positioning groove is arranged at the bottom of the upper mold base plate, an upper mold positioning pin is arranged at the bottom of the upper mold base plate, and a positioning pin sleeve cooperating with the upper mold positioning pin is arranged on the lower mold positioning plate.

[0009] Preferably, the gate sleeve is made of ceramic material.

[0010] According to a second aspect of an embodiment of the present invention, a process for forming a low-pressure metal mold tensile test piece of an aluminum alloy is provided, which is applied to the mold structure of the low-pressure metal mold tensile test piece of the aluminum alloy described in the first aspect, comprising:

[0011] Step S1, separating the lower mold assembly and the upper mold assembly, applying thermal insulation coating on the molding positions of the lower mold assembly and the upper mold assembly, and then baking the lower mold assembly and the upper mold assembly;

[0012] Step S2, after the lower mold assembly and the upper mold assembly are heated up, the lower mold assembly is transferred to the furnace cover, and the gate is aligned with the gate of the furnace cover;

[0013] Step S3, closing the lower mold assembly and the upper mold assembly, matching the upper mold locating pin with the locating pin sleeve, and placing a support block under the pressing block;

[0014] Step S4, starting the low-pressure pouring furnace;

[0015] Step S5, after pouring is completed, the mold is opened, the support block is removed, and the pressing block is knocked to push the ejector rod to eject the test piece;

[0016] Step S6, cleaning the lower mold assembly and the upper mold assembly, and repeating the above steps.

[0017] Preferably, in step S1: the thermal insulation coating adopts 395 thermal insulation coating.

[0018] Preferably, in step S1: baking for two hours, heating to 250°C.

[0019] Preferably, in step S4:

[0020] In the first stage: the filling time is 3 seconds, the pressure is 70mbar, and the holding time is 20 seconds;

[0021] In the second stage: the filling time is 4 seconds, the pressure is 120mbar, and the holding time is 20 seconds;

[0022] In the third stage: the filling time is 9 seconds, the pressure is 220mbar, and the holding time is 20 seconds.

[0023] The present invention has the following beneficial effects compared with the prior art:

[0024] The invention discloses a mold structure and a process method for an aluminum alloy low-pressure metal mold tensile test piece. The invention can realize the preparation of a thin-walled low-pressure metal mold aluminum alloy material tensile test piece, and can realize the performance detection of the aluminum alloy low-pressure metal mold process without destroying the casting, thereby improving the detection efficiency and reducing the production cost. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 It is an isometric view of a mold structure of an aluminum alloy low-pressure metal mold tensile test piece of the present invention.

[0026] Figure 2 The isometric view of the lower die assembly in the die structure of an aluminum alloy low-pressure metal mold tensile test piece of the present invention.

[0027] Figure 3 The isometric view of the lower die assembly in the die structure of an aluminum alloy low-pressure metal mold tensile test piece of the present invention.

[0028] Figure 4 The utility model is an isometric view of an upper die assembly in a die structure of an aluminum alloy low-pressure metal mold tensile test piece according to the present invention.

[0029] Figure 5 The isometric view of the lower die assembly in the die structure of an aluminum alloy low-pressure metal mold tensile test piece of the present invention.

[0030] Figure 6 The present invention is a working state diagram of a mold structure of an aluminum alloy low-pressure metal mold tensile test piece.

[0031] Among them, 100-upper mold assembly, 200-lower mold assembly, 300-L-type positioning block, 400-test piece, 101-connecting block, 102-pressing block, 103-limiting column, 104-support block, 105-upper mold base plate, 106-upper mold positioning pin, 107-ejector rod, 108-limiting hole, 109-ejection hole, 110-test piece casting cavity, 111-test piece positioning block, 112-exhaust hole, 201-lower mold base plate, 202-lower mold positioning plate, 203-positioning pin sleeve, 204-gate sleeve, 205-gate, 206-test piece positioning groove. DETAILED DESCRIPTION

[0032] The following is based on the attached Figure 1-6The present invention is further described:

[0033] The technical solution of the present invention will be described clearly and completely below in conjunction with the accompanying drawings. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0034] In the description of the present invention, it should be noted that the terms "center", "up", "down", "left", "right", "vertical", "horizontal", "inside", "outside", etc. indicate directions or positional relationships based on the directions or positional relationships shown in the accompanying drawings. They are only for the convenience of describing the present invention and simplifying the description, and do not indicate or imply that the device or element referred to must have a specific direction, be constructed and operated in a specific direction. Therefore, they cannot be understood as limitations on the present invention.

[0035] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "connected", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.

[0036] like Figure 1 As shown, the first embodiment of the present invention provides a mold structure for an aluminum alloy low-pressure metal mold tensile test piece based on the prior art, including a lower mold assembly 200. The lower mold assembly 200 can be fixed on the furnace cover by an L-shaped positioning block 300, and the top of the lower mold assembly 200 can be molded together with the upper mold assembly 100.

[0037] like Figure 2 and 3 As shown, the lower mold assembly 200 includes a lower mold base plate 201 with a gate 205 in the middle, a gate sleeve 204 matching the gate 205 is arranged on the top of the lower mold base plate 201, and the gate sleeve 204 is sealed and installed on the lower mold base plate 201 through a lower mold positioning plate 202, and a test piece positioning groove 206 is arranged on the lower mold positioning plate 202, and a through hole is arranged in the test piece positioning groove 206 for matching the gate 205. The gate sleeve 204 is made of ceramic material to prevent the aluminum liquid from solidifying prematurely and failing to fill the mold, and to prevent the upper and lower molds from not being tightly closed and the aluminum liquid from overflowing from the gap.

[0038] like Figure 4 and 5As shown, the upper mold assembly 100 includes an upper mold base plate 105, four connecting blocks 101 are symmetrically installed on the top of the upper mold base plate 105, a pressure block 102 is installed between the four connecting blocks 101, a push rod 107 is provided in the middle of the pressure block 102, and limiting columns 103 are respectively provided near the four corners, a test piece casting cavity 110 is provided at the bottom of the upper mold base plate 105, and an ejection hole 109 and an exhaust hole 112 cooperating with the push rod 107 are provided at the bottom of the test piece casting cavity 110. The exhaust hole 112 mainly functions to discharge the gas in the cavity during the low-pressure punching process to prevent the sample from being entrained and affecting the performance of the casting. The upper mold base plate 105 is provided with a limiting hole 108 that cooperates with the limiting column 103, and a support block 104 is symmetrically installed between the pressure block 102 and the upper mold base plate 105. A test piece positioning block 110 that cooperates with the test piece positioning groove 206 is provided at the bottom of the upper mold base plate 105, an upper mold positioning pin 106 is installed at the bottom of the upper mold base plate 105, and a positioning pin sleeve 203 that cooperates with the upper mold positioning pin 106 is installed on the lower mold positioning plate 202.

[0039] The second embodiment of the present invention provides a process for forming a low-pressure metal mold tensile test piece of an aluminum alloy based on the first embodiment, and the specific steps are as follows:

[0040] Step S1, separate the lower mold assembly 200 and the upper mold assembly 100, apply thermal insulation paint to the molding positions of the lower mold assembly 200 and the upper mold assembly 100, and use 395 thermal insulation paint. Then bake the lower mold assembly 200 and the upper mold assembly 100 for two hours and heat to 250°C;

[0041] Step S2, after the lower mold assembly 200 and the upper mold assembly 100 are heated up, the lower mold assembly 200 is transferred to the furnace cover, and the gate 205 is aligned with the gate of the furnace cover;

[0042] Step S3, closing the lower mold assembly 200 and the upper mold assembly 100, matching the upper mold locating pin 106 with the locating pin sleeve 203, and placing the support block 104 under the pressing block 102;

[0043] Step S4, starting the low-pressure pouring furnace, wherein:

[0044] In the first stage: the filling time is 3 seconds, the pressure is 70mbar, and the holding time is 20 seconds;

[0045] In the second stage: the filling time is 4 seconds, the pressure is 120mbar, and the holding time is 20 seconds;

[0046] In the third stage: the filling time is 9 seconds, the pressure is 220mbar, and the holding time is 20 seconds.

[0047] Step S5, after pouring is completed, the mold is opened, the support block 104 is removed, and the pressing block 102 is knocked to push the ejector rod 107 to eject the test piece 400. Figure 6As shown;

[0048] Step S6, clean the lower mold assembly 200 and the upper mold assembly 100, and repeat the above steps.

[0049] Although the embodiments of the present invention have been disclosed above, they are not limited to the applications listed in the specification and the embodiments. It can be fully applied to various fields suitable for the present invention. For those familiar with the art, additional modifications can be easily realized. Therefore, without departing from the general concept defined by the claims and equivalent scope, the present invention is not limited to the specific details and the illustrations shown and described here.

Claims

1. A mold structure for an aluminum alloy low-pressure metal mold tensile test piece, characterized in that: It comprises a lower die assembly (200), wherein the lower die assembly (200) can be fixed on the furnace cover via an L-shaped positioning block (300), and the top of the lower die assembly (200) can be molded together with the upper die assembly (100).

2. The mold structure of the aluminum alloy low-pressure metal mold tensile test piece according to claim 1, characterized in that: The lower mold assembly (200) comprises a lower mold base plate (201) with a gate (205) in the middle, a gate sleeve (204) matched with the gate (205) is arranged on the top of the lower mold base plate (201), the gate sleeve (204) is closed and arranged on the lower mold base plate (201) through a lower mold positioning plate (202), a test piece positioning groove (206) is arranged on the lower mold positioning plate (202), and a through hole corresponding to the gate (205) is arranged in the test piece positioning groove (206).

3. The mold structure of the aluminum alloy low-pressure metal mold tensile test piece according to claim 2, characterized in that: The upper mold assembly (100) comprises an upper mold base plate (105), four connecting blocks (101) are symmetrically arranged on the top of the upper mold base plate (105), a pressing block (102) is arranged between the four connecting blocks (101), a push rod (107) is arranged in the middle of the pressing block (102), and limiting columns (103) are respectively arranged near the four corners, a test piece casting cavity (110) is arranged at the bottom of the upper mold base plate (105), and an ejection hole (109) and an exhaust hole (109) cooperating with the push rod (107) are arranged at the bottom of the test piece casting cavity (110). 112), the upper mold base plate (105) is provided with a limiting hole (108) that cooperates with the limiting column (103), a support block (104) is symmetrically arranged between the pressure block (102) and the upper mold base plate (105), a test piece positioning block (111) that cooperates with the test piece positioning groove (206) is arranged at the bottom of the upper mold base plate (105), an upper mold positioning pin (106) is arranged at the bottom of the upper mold base plate (105), and a positioning pin sleeve (203) that cooperates with the upper mold positioning pin (106) is arranged on the lower mold positioning plate (202).

4. The mold structure of the aluminum alloy low-pressure metal mold tensile test piece according to claim 2 or 3, characterized in that: The gate sleeve (204) is made of ceramic material.

5. A process for producing a low-pressure metal mold tensile test piece of an aluminum alloy, applied to the mold structure of the low-pressure metal mold tensile test piece of an aluminum alloy according to any one of claims 1 to 4, characterized in that: include: Step S1, separating the lower mold assembly (200) and the upper mold assembly (100), applying a heat-insulating coating to the molding positions of the lower mold assembly (200) and the upper mold assembly (100), and then baking the lower mold assembly (200) and the upper mold assembly (100); Step S2, after the lower mold assembly (200) and the upper mold assembly (100) are heated up, the lower mold assembly (200) is transferred to the furnace cover, and the gate (205) is aligned with the gate of the furnace cover; Step S3, closing the lower mold assembly (200) and the upper mold assembly (100), matching the upper mold locating pin (106) with the locating pin sleeve (203), and placing the support block (104) under the pressing block (102); Step S4, starting the low-pressure pouring furnace; Step S5, after pouring is completed, the mold is opened, the support block (104) is removed, and the pressing block (102) is knocked to push the ejector rod (107) to eject the test piece (400); Step S6, cleaning the lower mold assembly (200) and the upper mold assembly (100), and repeating the above steps.

6. The process for preparing a low-pressure aluminum alloy metal mold tensile test piece according to claim 5, characterized in that: In the step S1: the thermal insulation coating adopts 395 thermal insulation coating.

7. The process for preparing a low-pressure aluminum alloy metal mold tensile test piece according to claim 5, characterized in that: In the step S1: baking for two hours, heating to 250°C.

8. The process for preparing a low-pressure aluminum alloy metal mold tensile test piece according to claim 5, characterized in that: In step S4: In the first stage: the filling time is 3 seconds, the pressure is 70mbar, and the holding time is 20 seconds; In the second stage: the filling time is 4 seconds, the pressure is 120mbar, and the holding time is 20 seconds; In the third stage: the filling time is 9 seconds, the pressure is 220mbar, and the holding time is 20 seconds.

Citation Information

Patent Citations

  • Casting method of thin-wall aluminum alloy casting

    CN110976806A

  • Method for preparing aluminum alloy engine cylinder cover by using tilted pouring process

    CN111069575A

  • Aluminum alloy integrated brake caliper low-pressure die and production process

    CN118455490A

  • Multifunctional metal type casting sample horizontal group compound die utensil

    CN206981716U

  • Device for producing casting and production thereof

    JP1997234553A