Manufacturing method and device of integrated germanium-silicon HBT (Heterojunction Bipolar Transistor) by double polycrystal self-alignment bipolar process
Through the dual polycrystal self-aligning bipolar process, the vertical structure bipolar transistor is integrated in the SiGe heterojunction bipolar process, which solves the problem of high process complexity in the existing technology, and realizes high-performance SiGe HBT and longitudinal structure bipolar. The integration of pole transistors meets the needs of products such as high-speed computing and radio frequency amplifiers.
Patent Information
- Application Number
- CN202411218220.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-02
- Publication Date
- 2024-12-06
AI Technical Summary
The existing SiGe heterojunction bipolar process is difficult to achieve high-performance longitudinal structure bipolar transistors, and the process technology is difficult and complex, and cannot meet the needs of products such as high-speed computing and radio frequency amplifiers.
Using the dual polycrystalline self-aligning bipolar process, the device region is divided on the silicon substrate to form doped collector region and heterojunction inner base region, and combined with ion implantation and epitaxial growth technology, SiGe heterojunction is realized Integration of the inner base region and the polysilicon emitter region.
Without increasing process difficulty and complexity, the process integration of SiGe HBT and longitudinal structure bipolar transistors is achieved, providing high-performance NPN-type and PNP-type bipolar transistors to meet a variety of application needs.
Smart Images

Figure CN119092407A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of transistor manufacturing, and in particular relates to a manufacturing method and a device of a dual-polycrystalline self-aligned bipolar process integrated germanium silicon HBT. Background Art
[0002] Compared with the conventional silicon-based bipolar process, the SiGe heterojunction bipolar process introduces SiGe heterojunction technology, which replaces the silicon-doped base region with Ge-Si material (Si 1-X Ge X ), forming a SiGe heterojunction transistor (SiGe HBT), which can greatly improve the high-frequency characteristics of bipolar transistors. Due to the introduction of SiGe epitaxial base technology, the SiGe heterojunction bipolar process requires more lithography pattern area definition, higher process technology difficulty and more complex process flow structure implementation. Therefore, it often only has high-performance SiGe HBT transistors, but not high-performance vertical bipolar transistors. The bipolar transistors generated by parasitic means are far inferior to vertical bipolar transistors in terms of output characteristics, current gain, frequency characteristics, noise characteristics, etc., and cannot meet the development and application needs of products such as high-speed operational amplifiers, high-speed logarithmic amplifiers, and RF amplifiers.
[0003] In a set of bipolar processes, separately prepared vertical structure NPN bipolar transistors and vertical structure PNP bipolar transistors are integrated at the same time. Such a process is called a complementary bipolar process. Compared with conventional bipolar processes, complementary bipolar processes include high-performance VNPN devices and are compatible with high-performance VPNP devices. They have better performance indicators than conventional bipolar processes, but their overall manufacturing process is more complex, and the processing difficulty and manufacturing cost are also higher. The process integration of vertical structure bipolar transistors in SiGe heterojunction bipolar processes will further increase the difficulty of process technology and the complexity of process implementation.
[0004] In summary, it is necessary to design a method and semiconductor device for integrating high-performance vertical bipolar transistors using SiGe heterojunction process, so as to realize the process integration of SiGe HBT transistors and vertical bipolar transistors without significantly increasing the process difficulty and complexity. Summary of the invention
[0005] In view of the above-mentioned deficiencies in the prior art, the technical problem to be solved by the present invention is to provide a method for manufacturing a dual-polycrystalline self-aligned bipolar process integrated silicon-germanium HBT and a device.
[0006] In order to solve the above technical problems, the present invention provides the following technical solutions:
[0007] A method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT comprises the following steps:
[0008] S1. Providing a silicon substrate, dividing at least one first device region and at least one second device region on the silicon substrate, forming a first collector region of a first doping type in the first device region, forming a second collector region of a second doping type in the second device region, and forming a field oxygen isolation region at the periphery of each first collector region and each second collector region;
[0009] S2, forming an implanted intrinsic base region in the first collector region, wherein the doping type of the implanted intrinsic base region is opposite to the doping type of the first collector region;
[0010] S3, forming a first collector region selective injection region of a first doping type in the first collector region by ion implantation; forming a second collector region selective injection region of a second doping type in the second collector region by ion implantation;
[0011] S4, forming a Si Ge heterojunction inner base region in the second collector region, wherein the doping type of the Si Ge heterojunction inner base region is opposite to the doping type of the second collector region;
[0012] S5, forming a first external base region connected to the implanted intrinsic base region, and a second external base region connected to the Si Ge heterojunction intrinsic base region; the doping type of the first external base region is the same as the doping type of the implanted intrinsic base region, and the doping type of the second external base region is the same as the doping type of the Si Ge heterojunction intrinsic base region;
[0013] S6, forming a first emitter window above the first collector region, and forming a second emitter window above the second collector region;
[0014] S7. A first sidewall blocking structure and a first polysilicon emitter region are formed in the first emitter window, and a second sidewall blocking structure and a second polysilicon emitter region are formed in the second emitter window; the doping type of the first polysilicon emitter region is the same as the doping type of the first collector region, and the doping type of the second polysilicon emitter region is the same as the doping type of the second collector region.
[0015] Further, the first doping type is P-type doping, and the second doping type is N-type doping; or
[0016] The first doping type is N-type doping, and the second doping type is P-type doping; or
[0017] The first doping type and the second doping type are both P-type doping; or
[0018] The first doping type and the second doping type are both N-type doping.
[0019] Furthermore, the step S1 includes the following sub-steps:
[0020] S101, providing a silicon substrate, and dividing at least one first device region and at least one second device region on the silicon substrate;
[0021] S102, forming a first heavily doped buried layer of a first doping type below the first device region, and forming a second heavily doped buried layer of a second doping type below the second device region;
[0022] S103, forming a first collector region of a first doping type in each first device region, the first collector region being located above the first heavily doped buried layer; forming a second collector region of a second doping type in each second device region, the second collector region being located above the second heavily doped buried layer;
[0023] S104, forming a field oxygen isolation region around each first collector region and each second collector region respectively.
[0024] Furthermore, the first collector region and the second collector region are formed by doping epitaxy, or by ion implantation doping and annealing;
[0025] The first heavily doped buried layer and the second heavily doped buried layer are formed by ion implantation and annealing process, or by epitaxial process;
[0026] The field oxygen isolation region is formed based on a trench isolation technology, based on a deep trench isolation technology combined with a PN junction isolation technology, or based on a local oxidation technology combined with a PN junction isolation technology.
[0027] Furthermore, the step S2 includes the following sub-steps:
[0028] S201, forming an intrinsic base region injection layer in the first collector region by ion implantation, wherein the doping type of the intrinsic base region injection layer is opposite to the doping type of the first collector region;
[0029] S202, forming a first dielectric layer on the silicon substrate by a deposition or oxidation process, and forming an injected intrinsic base region by an annealing process so that the intrinsic base region injection layer is annealed;
[0030] The S4 step includes the following sub-steps:
[0031] S401, etching and removing the first dielectric layer above the second collector region to expose the second collector region;
[0032] S402, performing Si Ge epitaxial growth on a silicon substrate to form a Si Ge epitaxial layer;
[0033] S403, etching and removing the Si Ge epitaxial layer outside the second collector region and the surrounding field oxygen isolation region, the etching stops in the first dielectric layer below the Si Ge epitaxial layer, and the remaining Si Ge epitaxial layer forms a Si Ge heterojunction intrinsic base region in the second collector region.
[0034] Furthermore, the step S5 includes the following sub-steps:
[0035] S501, etching and removing the first dielectric layer not covering the Si Ge epitaxial layer to expose the first collector region;
[0036] S502, forming a second dielectric layer on the silicon substrate;
[0037] S503, etching the second dielectric layer to form a first extrinsic base contact window in the first collector region and a second extrinsic base contact window in the second collector region;
[0038] S504, forming a first polysilicon layer on the silicon substrate;
[0039] S505, doping the first polysilicon layer to form a first doped polysilicon layer; the doping type of the first doped polysilicon layer above the first collector region is consistent with the doping type of the implanted intrinsic base region, and the doping type of the first doped polysilicon layer above the second collector region is consistent with the doping type of the Si Ge heterojunction intrinsic base region;
[0040] S506, etching the first doped polysilicon layer, retaining the first doped polysilicon layer above the first collector region and the surrounding field oxygen isolation region to form a first extrinsic base region, and retaining the first doped polysilicon layer on the Si Ge heterojunction intrinsic base region to form a second extrinsic base region.
[0041] Furthermore, the step S6 includes the following sub-steps:
[0042] S601, forming a third dielectric layer on the silicon substrate;
[0043] S602, etching the third dielectric layer and the first doped polysilicon layer, the etching stops in the second dielectric layer below the first doped polysilicon layer, forming a first emitter window in the first collector region, and forming a second emitter window in the second collector region.
[0044] Furthermore, the step S7 includes the following sub-steps:
[0045] S701, forming a fourth dielectric layer on the silicon substrate;
[0046] S702, etching the fourth dielectric layer in the first emitter window and the second emitter window, and etching stops in the second dielectric layer below the fourth dielectric layer;
[0047] S703, etching the exposed second dielectric layer to expose the implanted intrinsic base region at the bottom of the first emitter window and the Si Ge heterojunction intrinsic base region at the bottom of the second emitter window, and forming a first sidewall blocking structure in the first device region and a second sidewall blocking structure in the second device region;
[0048] S704, forming a second polysilicon layer on the silicon substrate;
[0049] S705, doping the second polysilicon layer to form a second doped polysilicon layer; wherein the second polysilicon layer located in an area above the first collector region is heavily doped with a first doping type, and the second polysilicon layer located in an area above the second collector region is heavily doped with a second doping type;
[0050] S706, etching and removing the second doped polysilicon layer outside the first emitter window and the second emitter window, using a rapid annealing process to form a first polysilicon emitter region in the first emitter window, forming a second polysilicon emitter region in the first emitter window, and diffusing the doped impurities in the first polysilicon emitter region into the implanted intrinsic base region at the bottom of the first emitter window, and diffusing the doped impurities in the second polysilicon emitter region into the Si Ge heterojunction intrinsic base region at the bottom of the second emitter window to form an emitter-base junction.
[0051] Furthermore, after executing step S7, the following steps are also executed:
[0052] S8. Form a collector contact electrode, a base contact electrode and an emitter contact electrode in each first device region and each second device region respectively.
[0053] A semiconductor device is manufactured by adopting a manufacturing method of integrating germanium silicon HBT using a double polycrystalline self-aligned bipolar process.
[0054] The present invention proposes a process manufacturing technology for integrating Si Ge heterojunction transistors in a dual polycrystalline self-aligned bipolar process, which can realize the process integration of dual polycrystalline self-aligned bipolar transistors and Si Ge heterojunction bipolar transistors without significantly increasing the process difficulty and process complexity; both silicon-based dual polycrystalline self-aligned bipolar transistors and Si Ge heterojunction bipolar transistors include two types, NPN and PNP, which can meet a variety of different application requirements. BRIEF DESCRIPTION OF THE DRAWINGS
[0055] The drawings described herein are used to provide a further understanding of the present application and constitute a part of the present application. The illustrative embodiments of the present application and their descriptions are used to explain the present application and do not constitute an improper limitation on the present application. In the drawings:
[0056] Figure 1The flowchart of one embodiment of the method for manufacturing a dual-poly self-aligned bipolar process integrated germanium silicon HBT of the present invention.
[0057] Figure 2 It is a schematic diagram of the structure after a heavily doped buried layer, a collector region and a field oxygen isolation region are formed on a silicon substrate.
[0058] Figure 3 It is a schematic diagram of the structure after the implantation of the intrinsic base region and the first dielectric layer.
[0059] Figure 4 This is a schematic diagram of the structure after the collector region is selectively implanted.
[0060] Figure 5 This is a schematic diagram of the structure after the first dielectric layer above the second collector region is removed by etching.
[0061] Figure 6 Schematic diagram of the structure after forming the Si Ge epitaxial layer.
[0062] Figure 7 Schematic diagram of the structure after etching the Si Ge epitaxial layer to form the Si Ge heterojunction base region.
[0063] Figure 8 It is a schematic diagram of the structure after the second dielectric layer is formed.
[0064] Fig. 9 A schematic diagram of the structure after etching the second dielectric layer to form an external base region contact window.
[0065] Fig.10 It is a schematic diagram of the structure after the first doped polysilicon layer is formed.
[0066] Fig.11 This is a schematic diagram of the structure after etching the first doped polysilicon layer to form an external base region.
[0067] Fig.12 It is a schematic diagram of the structure after the third dielectric layer is formed.
[0068] Fig.13 Schematic diagram of the structure after etching the third dielectric layer to form an emitter window.
[0069] Fig.14 It is a schematic diagram of the structure after the fourth dielectric layer is formed.
[0070] Fig.15 This is a schematic diagram of the structure after etching the fourth dielectric layer in the emitter window.
[0071] Fig.16 Schematic diagram of the structure after etching the second dielectric layer to expose the implanted intrinsic base region and the Si Ge heterojunction intrinsic base region.
[0072] Fig.17 It is a schematic diagram of the structure after forming the second doped polysilicon layer.
[0073] Fig.18 This is a schematic diagram of the structure after etching the second doped polysilicon layer to form a polysilicon emitter region.
[0074] The accompanying drawings in the specification are numeraled as follows:
[0075] first collector region-100; first heavily doped buried layer-110; implanted intrinsic base region-120; first collector region selective implanted region-130; first extrinsic base region contact window-140; first extrinsic base region-150; first emitter window-160; first sidewall blocking structure-270; first polysilicon emitter region-180;
[0076] second collector region-200; second heavily doped buried layer-210; Si Ge heterojunction inner base region-220; second collector region selective implantation region-230; second extrinsic base region contact window-240; second extrinsic base region-250; second emitter window-260; second sidewall blocking structure-270; second polysilicon emitter region-280;
[0077] Silicon substrate-300; field oxygen isolation region-301; first dielectric layer-310; Si Ge epitaxial layer-320; second dielectric layer-330; first doped polysilicon layer-340; third dielectric layer-350; fourth dielectric layer-360; second doped polysilicon layer-370. DETAILED DESCRIPTION
[0078] The following describes the implementation methods of the present invention through specific examples. The illustrations provided in the following embodiments are only used to schematically illustrate the basic concept of the present invention. The following embodiments and features in the embodiments may be combined with each other without conflict.
[0079] See also Figure 1 , Figure 1 The flowchart of an embodiment of the method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT of the present invention. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT of this embodiment comprises the following steps:
[0080] S1. Please refer to Figure 2 , provide a silicon substrate 300, divide at least one first device region and at least one second device region on the silicon substrate 300, form a first collector region 100 of a first doping type in the first device region, form a second collector region 200 of a second doping type in the second device region, and form a field oxygen isolation region 301 around each first collector region 100 and each second collector region 200. This step may include the following sub-steps:
[0081] S101. Provide a silicon substrate 300, divide A device regions on the silicon substrate 300, and the A device regions include B first device regions and C second device regions (i.e., A=B+C). The first device region is used to form a first collector region 100, and the second device region is used to form a second collector region 200. The silicon substrate 300 is a structural layer and a supporting layer of a semiconductor device. In this embodiment, the silicon substrate 300 can be a single crystal silicon material, or other substrate materials such as silicon on insulator (SOI).
[0082] S102, forming a first heavily doped buried layer 110 of a first doping type below the first device region, and forming a second heavily doped buried layer 210 of a second doping type below the second device region; the doping type of the heavily doped buried layer (i.e., the first heavily doped buried layer 110 and the second heavily doped buried layer 210) is determined according to the doping type required by the corresponding collector region (i.e., the first collector region 100 and the second collector region 200). The heavily doped buried layer can be formed by ion implantation and annealing process or epitaxial process, and finally the Rc resistance of the bipolar transistor is formed by the heavily doped buried layer, and connected to the heavily doped penetration region formed in the corresponding collector region, so as to further reduce the Rc resistance.
[0083] According to actual needs, the first doping type and the second doping type can be opposite, for example, the first doping type can be N-type doping, and the second doping type can be P-type doping; or, the first doping type can also be P-type doping, and the second doping type can also be N-type doping. The first doping type and the second doping type can also be the same, for example, the first doping type and the second doping type can both be P-type doping, or both be N-type doping. In this embodiment, the first doping type is N-type doping, and the second doping type is P-type doping, that is, the first heavily doped buried layer 110 is an N-type heavily doped buried layer, and the second heavily doped buried layer 210 is a P-type heavily doped buried layer.
[0084] S103, a first collector region 100 of a first doping type is formed in each first device region (i.e., the first collector region 100 is an N-type collector region), and the first collector region 100 is located above the first heavily doped buried layer 110; a second collector region 200 of a second doping type is formed in each second device region (i.e., the second collector region 200 is a P-type collector region), and the second collector region 200 is located above the second heavily doped buried layer 210. The collector region can be formed by doping epitaxy, or by ion implantation doping and annealing; in this embodiment, the first collector region 100 is used to form a silicon-based vertical structure bipolar transistor, and the second collector region 200 is used to form a Si Ge heterojunction transistor.
[0085] S104, forming a field oxygen isolation region 301 at the periphery of each collector region (i.e., each first collector region 100 and each second collector region 200). The etching of the field oxygen isolation region 301 can be formed based on the trench isolation technology or the deep trench isolation technology + PN junction isolation technology, or can be formed based on the local oxidation technology + PN junction isolation technology; the field oxygen isolation region 301 needs to completely surround the device region, so that the N-type collector region and the N-type heavily doped buried layer of the first device region are isolated from other structures, and the P-type collector region and the P-type heavily doped buried layer of the second device region are isolated from other structures.
[0086] S2. Please refer to Figure 3 , forming an implanted intrinsic base region 120 in the first collector region 100, wherein the doping type of the implanted intrinsic base region 120 is opposite to the doping type of the first collector region 100. This step may include the following sub-steps:
[0087] S201 , forming an intrinsic base region injection layer in the first collector region 100 by ion implantation, wherein the doping type of the intrinsic base region injection layer is opposite to the doping type of the first collector region 100 .
[0088] S202, forming a first dielectric layer 310 on the silicon substrate 300 by a deposition or oxidation process, wherein the first dielectric layer 310 covers each of the collector regions and each of the field oxygen isolation regions 301; and forming an implanted intrinsic base region 120 by an annealing process after annealing the intrinsic base region implantation layer. The first dielectric layer 310 may be silicon oxide, silicon nitride, or a combination of silicon oxide and silicon nitride formed by chemical vapor deposition, or silicon oxide formed by thermal oxidation, and the implanted intrinsic base region 120 of the first collector region 100 may be formed by rapid annealing, or by conventional furnace tube thermal annealing.
[0089] S3. Please refer to Figure 4 , a first collector region selective injection region 130 of a first doping type is formed in the first collector region 100 by ion implantation; and a second collector region selective injection region 230 of a second doping type is formed in the second collector region 200 by ion implantation. The method for forming the collector region selective injection region (i.e., the first collector region selective injection region 130 and the second collector region selective injection region 230) is:
[0090] A photolithography process is adopted to form a photoresist barrier layer, and the photoresist barrier layer is used as a mask to perform a first ion implantation in the silicon substrate 300 through the first dielectric layer 310, and the ion implantation area is B first collector regions 100, and a first collector region selective implantation area 130 is formed in the first collector region 100, and the doping type of the first collector region selective implantation area 130 is consistent with the doping type of the first collector region 100 and the first heavily doped buried layer 110 thereunder. Afterwards, a second ion implantation is performed in the silicon substrate 300 through the first dielectric layer 310, and the ion implantation area is C second collector regions 200, and a second collector region selective implantation area 230 is formed in the second collector region 200, and the doping type of the second collector region selective implantation area 230 is consistent with the doping type of the second collector region 200 and the second heavily doped buried layer 210 thereunder.
[0091] S4. Please refer to Figure 5 , Figure 6 and Figure 7 , forming a Si Ge heterojunction inner base region 220 in the second collector region 200, and the doping type of the Si Ge epitaxial layer 320 is opposite to the doping type of the second collector region 200. This step may include the following sub-steps:
[0092] S401, please refer to Figure 5 The first dielectric layer 310 above the second collector region 200 is removed by etching using a photolithography process and an etching process to expose the second collector region 200 .
[0093] S402, please refer to Figure 6 , epitaxial growth of Si Ge is performed on the silicon substrate 300 to form a Si Ge epitaxial layer 320; the Si Ge epitaxial layer 320 covers the exposed second collector region 200, the first collector region 100 and the first dielectric layer 310 at the position of the field oxygen isolation region 301. The Si Ge epitaxial layer 320 is formed by an epitaxial growth process, and the film layer structure includes but is not limited to a combination of a doped or undoped Si layer and a doped or undoped Si 1-XGeX layer of different Ge components, and the doping type of the Si Ge epitaxial layer 320 is opposite to that of the second collector region 200 and the second heavily doped buried layer 210 thereunder.
[0094] S403, please refer to Figure 7, the Si Ge epitaxial layer 320 outside the second collector region 200 and the surrounding field oxygen isolation region 301 is etched and removed by using a photolithography process and a dry etching process, and the etching stops in the first dielectric layer 310 below the Si Ge epitaxial layer 320, and the remaining Si Ge epitaxial layer 320 forms a Si Ge heterojunction intrinsic base region 220 in the second collector region 200. A portion of the Si Ge epitaxial layer 320 on the field oxygen isolation region 301 around the second collector region 200 can also be removed. Specifically, when etching the Si Ge epitaxial layer 320, a photolithography process is first used to form a photoresist barrier layer, and the photoresist barrier layer is used as a mask to etch the Si Ge epitaxial layer 320 except for the second collector region 200 and the surrounding part of the field oxygen isolation region 301.
[0095] S5. Please refer to Figure 7 , Figure 8 , Fig. 9 , Fig.10 and Fig.11 , forming a first external base region 150 connected to the implanted intrinsic base region 120, and a second external base region 250 connected to the Si Ge heterojunction intrinsic base region 220; the doping type of the first external base region 150 is the same as the doping type of the implanted intrinsic base region 120, and the doping type of the second external base region 250 is the same as the doping type of the Si Ge heterojunction intrinsic base region 220. This step may include the following sub-steps:
[0096] S501, please continue reading Figure 7 , the first dielectric layer 310 not covering the Si Ge epitaxial layer 320 is etched away (i.e., the first dielectric layer 310 outside the second collector region 200 and the surrounding portion of the field oxygen isolation region 301 is removed), exposing the first collector region 100. The etching process in this step can be a dry etching process or a wet etching process.
[0097] S502, please refer to Figure 8 , a deposition process is used to form a second dielectric layer 330 on the silicon substrate 300, and the second dielectric layer 330 contacts and covers the first collector region 100, the Si Ge epitaxial layer 320 of the second collector region 200 and each field oxygen isolation region 301. In this embodiment, the second dielectric layer 330 is silicon oxide, silicon nitride, or a combination of silicon oxide and silicon nitride formed by chemical vapor deposition.
[0098] S503, please refer to Fig. 9, the second dielectric layer 330 is etched by photolithography and etching, and a first external base contact window 140 is formed in the first collector region 100, and a second external base contact window 240 is formed in the second collector region 200; the first external base contact window 140 exposes part of the implanted intrinsic base region 120 and part of the field oxygen isolation region 301 around it, and the second external base contact window 240 exposes part of the outer Si Ge epitaxial layer 320. Specifically, when etching the second dielectric layer 330, a photolithography process is used to first form a photoresist barrier layer, and the photoresist barrier layer is used as a mask, and then an etching process is used to etch the external base contact windows (i.e., the first external base contact window 140 and the second external base contact window 240) of the implanted intrinsic base region 120 in the first collector region 100 and the Si Ge heterojunction intrinsic base region 220 in the second collector region 200. The etching process in this step can be a dry etching process or a wet etching process.
[0099] S504, please refer to Fig.10 , a first polysilicon layer is formed on the silicon substrate 300 by a deposition process; the first polysilicon layer covers the remaining second dielectric layer 330 , the exposed Si Ge epitaxial layer 320 of the first collector region 100 and the second collector region 200 .
[0100] S505, please continue reading Fig.10 , the first polysilicon layer is doped by photolithography and ion implantation to form a first doped polysilicon layer 340; wherein the doping type of the first doped polysilicon layer 340 above the first collector region 100 is consistent with the doping type of the implanted intrinsic base region 120 of the first collector region 100, and the doping type of the first doped polysilicon layer 340 above the second collector region 200 is consistent with the doping type of the Si Ge heterojunction intrinsic base region 220 of the second collector region 200. Of course, the first doped polysilicon layer 340 can also be formed by a doped polysilicon chemical vapor deposition process.
[0101] S506, please refer to Fig.11 , the first doped polysilicon layer 340 is etched by using a photolithography process and a dry etching process, the first doped polysilicon layer 340 is retained on the first collector region 100 and the surrounding field oxygen isolation region 301 to form the first extrinsic base region 150, and the first doped polysilicon layer 340 on the Si Ge heterojunction intrinsic base region 220 is retained to form the second extrinsic base region 250. In this embodiment, when etching the first doped polysilicon layer 340, a photolithography process is first used to form a photoresist barrier layer, and then the photoresist barrier layer is used as a mask to dry-etch the first doped polysilicon layer 340.
[0102] S6. Please refer to Fig.12 and Fig.13, forming a first emitter window 160 above the first collector region 100, and forming a second emitter window 260 above the second collector region 200. This step may include the following sub-steps:
[0103] S601, please refer to Fig.12 , a deposition process is used to form a third dielectric layer 350 on the silicon substrate 300, and the third dielectric layer 350 covers the first doped polysilicon layer 340 and the second dielectric layer 330. The third dielectric layer 350 is formed by chemical vapor deposition and can be silicon oxide, silicon nitride, or a combination of silicon oxide and silicon nitride.
[0104] S602, please refer to Fig.13 The third dielectric layer 350 and the first doped polysilicon layer 340 are etched by photolithography and dry etching, and the etching stops in the second dielectric layer 330 below the first doped polysilicon layer 340, thereby forming a first emitter window 160 in the first collector region 100 and a second emitter window 260 in the second collector region 200.
[0105] S7, see Fig.14 , Fig.15 , Fig.16 , Fig.17 and Fig.18 , forming a first sidewall blocking structure 270 and a first polysilicon emitter region 180 in the first emitter window 160, and forming a second sidewall blocking structure 270 and a second polysilicon emitter region 280 in the second emitter window 260; the doping type of the first polysilicon emitter region 180 is the same as the doping type of the first collector region 100, and the doping type of the second polysilicon emitter region 280 is the same as the doping type of the second collector region 200. This step may include the following sub-steps:
[0106] S701, please refer to Fig.14 , a deposition process is used to form a fourth dielectric layer 360 on the silicon substrate 300, and the fourth dielectric layer 360 covers the remaining second dielectric layer 330, the first emitter window 160 and the second emitter window 260. The fourth dielectric layer 360 is a combination of a multi-layer composite structure formed by chemical vapor deposition, which is related to the spacer process used later.
[0107] S702, please refer to Fig.15 , using a spacer process, dry-etching the fourth dielectric layer 360 in the first emitter window 160 and the second emitter window 260, and the etching stops in the second dielectric layer 330 below the fourth dielectric layer 360. The fourth dielectric layer 360 can also be etched by a photolithography process plus an etching process.
[0108] S703, please refer to Fig.16 , an etching process is used to etch the exposed second dielectric layer 330, exposing the implanted intrinsic base region 120 at the bottom of the first emitter window 160 and the Si Ge heterojunction intrinsic base region 220 at the bottom of the second emitter window 260, and forming a first sidewall blocking structure 270 for isolating the device emitter and base in the first device region, and forming a second sidewall blocking structure 270 for isolating the device emitter and base in the second device region. The etching process in this step can be a dry etching process or a wet etching process.
[0109] S704, please refer to Fig.17 A second polysilicon layer is formed on the silicon substrate 300 by a deposition process, and the second polysilicon layer covers the remaining fourth dielectric layer 360 , the implanted intrinsic base region 120 at the bottom of the first emitter window 160 , and the Si Ge heterojunction intrinsic base region 220 at the bottom of the second emitter window 260 .
[0110] S705, please continue reading Fig.17 , the second polysilicon layer is doped by photolithography and ion implantation to form a second doped polysilicon layer 370. The second polysilicon layer located above the first collector region 100 is heavily doped with the first doping type, and the second polysilicon layer located above the second collector region 200 is heavily doped with the second doping type.
[0111] S706, please refer to Fig.18 , using photolithography and dry etching processes to etch away the second doped polysilicon layer 370 outside the first emitter window 160 and the second emitter window 260; using a rapid annealing process, the remaining second doped polysilicon layer 370 of the first emitter window 160 forms a first polysilicon emitter region 180, and the remaining second doped polysilicon layer 370 of the second emitter window 260 forms a second polysilicon emitter region 280, and the impurities doped in the first polysilicon emitter region 180 are diffused into the implanted intrinsic base region 120 at the bottom of the first emitter window 160, and the impurities doped in the second polysilicon emitter region 280 are diffused into the Si Ge heterojunction intrinsic base region 220 at the bottom of the second emitter window 260 to form an emitter-base junction.
[0112] After executing the step S7, the following steps may also be performed:
[0113] S8. Form a collector contact electrode, a base contact electrode and an emitter contact electrode (not shown in the figure) in each first device region and each second device region, respectively. The collector contact electrode in the first device region forms an ohmic contact with the first collector region 100, the base contact electrode in the first device region forms an ohmic contact with the first external base region 150, and the emitter contact electrode in the first device region forms an ohmic contact with the first polysilicon emitter region 180; the collector contact electrode in the second device region forms an ohmic contact with the second collector region 200, the base contact electrode in the second device region forms an ohmic contact with the second external base region 250, and the emitter contact electrode in the second device region forms an ohmic contact with the second polysilicon emitter region 280.
[0114] In this step, metal can be deposited by vapor phase and etched to form collector contact electrodes, base contact electrodes and emitter contact electrodes to lead out electrodes of each bipolar transistor. In addition, according to different application requirements, it may also involve a common processing flow in the field of semiconductor technology, such as a combination of silicide, ILD dielectric layer, multi-layer metal wiring, IMD dielectric layer, various contact holes and through holes, passivation layer and other processes. The processes for forming collector contact electrodes, base contact electrodes and emitter contact electrodes are all prior art and will not be described in detail here.
[0115] At present, the mainstream Si Ge bipolar process solutions in the industry are divided into two types: the first is a conventional Si Ge bipolar process integrating NPN Si Ge heterojunction bipolar transistors and PNP lateral structure bipolar transistors, and the second is a Si Ge complementary bipolar process integrating NPN Si Ge heterojunction bipolar transistors and PNP Si Ge heterojunction bipolar transistors. Compared with the first process solution, the Si Ge bipolar and process solution proposed in this embodiment integrates high-performance PNP vertical structure bipolar transistors, which can form symmetrical complementarity with NPN Si Ge heterojunction bipolar transistors to achieve complementary push-pull applications, and can support the development of high-speed and high-precision logarithmic amplifiers, differential amplifiers, logarithmic amplifiers, radio frequency amplifiers and other field products; compared with the second process solution, the Si Ge bipolar and process solution proposed in this embodiment only requires one type of Si Ge epitaxial equipment, and the process complexity is greatly reduced, which has a more significant cost advantage. In addition, the Si Ge epitaxial base region of the Si Ge heterojunction bipolar transistor in the present invention is realized by a non-selective growth process. Compared with the selective Si Ge epitaxial growth process, the non-selective Si Ge epitaxial growth process is less difficult to develop, and the required process flow and device structure complexity are also less complex, which is conducive to improving process stability.
[0116] In summary, this embodiment proposes a process manufacturing technology for integrating Si Ge heterojunction transistors in a dual polycrystalline self-aligned bipolar process, which can realize the process integration of dual polycrystalline self-aligned bipolar transistors and Si Ge heterojunction bipolar transistors without significantly increasing the process difficulty and process complexity; both silicon-based dual polycrystalline self-aligned bipolar transistors and Si Ge heterojunction bipolar transistors include two types, NPN and PNP, which can meet a variety of different application requirements.
[0117] This embodiment also discloses a semiconductor device, which is manufactured by the manufacturing method of integrating germanium silicon HBT by dual polycrystalline self-aligned bipolar process as in any of the above embodiments. The semiconductor device of this embodiment integrates silicon-based vertical structure bipolar transistors and Si Ge heterojunction bipolar transistors at the same time; both vertical structure bipolar transistors and Si Ge heterojunction bipolar transistors can be NPN or PNP transistors. In addition, both vertical structure bipolar transistors and Si Ge heterojunction bipolar transistors can be prepared at the same time by setting different doping, such as high-voltage bipolar transistors and high-speed bipolar transistors; for vertical structure bipolar transistors, different types of vertical structure bipolar transistors can also be prepared at the same time by setting different doping types; no limitation is made here.
[0118] For example, in an optional embodiment, a PNP type vertical structure bipolar transistor and an NPN type Si Ge heterojunction bipolar transistor are integrated on the semiconductor device. Compared with the parasitic LPNP or SPNP devices of the conventional Si Ge bipolar process, the performance of the PNP type vertical structure bipolar transistor integrated in the semiconductor device of the present invention is greatly improved, and it can form symmetrical complementarity with the NPN type Si Ge heterojunction bipolar transistor to realize complementary push-pull applications, and support the development of push-pull operational amplifiers, differential amplifiers and other products.
[0119] In another optional example, the semiconductor device is integrated with a high-voltage NPN type vertical structure bipolar transistor and a high-speed NPN type Si Ge heterojunction bipolar transistor, or integrated with a high-voltage PNP type vertical structure bipolar transistor and a high-speed NPN type Si Ge heterojunction bipolar transistor, or integrated with high-speed and high-voltage NPN type Si Ge heterojunction bipolar transistors, which can meet the needs of related applications such as high-voltage output while achieving RF application performance, and support the development of high-speed logarithmic amplifiers, RF amplifiers and other products.
[0120] The above embodiments only express the preferred implementation modes of the present invention, and the descriptions thereof are relatively specific and detailed, but they cannot be understood as limiting the scope of the invention patent. It should be pointed out that, for those of ordinary skill in the art, several variations and improvements can be made without departing from the concept of the present invention, and these all belong to the protection scope of the present invention. Therefore, the protection scope of the patent of the present invention shall be subject to the attached claims.
Claims
1. A method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT, characterized in that: The following steps are involved: S1. Providing a silicon substrate, dividing at least one first device region and at least one second device region on the silicon substrate, forming a first collector region of a first doping type in the first device region, forming a second collector region of a second doping type in the second device region, and forming a field oxygen isolation region at the periphery of each first collector region and each second collector region; S2, forming an implanted intrinsic base region in the first collector region, wherein the doping type of the implanted intrinsic base region is opposite to the doping type of the first collector region; S3, forming a first collector region selective implantation region of a first doping type in the first collector region by ion implantation; forming a second collector region selective implantation region of a second doping type in the second collector region by ion implantation; S4, forming a SiGe heterojunction inner base region in the second collector region, wherein the doping type of the SiGe heterojunction inner base region is opposite to the doping type of the second collector region; S5, forming a first external base region connected to the implanted intrinsic base region, and a second external base region connected to the SiGe heterojunction intrinsic base region; the doping type of the first external base region is the same as the doping type of the implanted intrinsic base region, and the doping type of the second external base region is the same as the doping type of the SiGe heterojunction intrinsic base region; S6, forming a first emitter window above the first collector region, and forming a second emitter window above the second collector region; S7. A first sidewall blocking structure and a first polysilicon emitter region are formed in the first emitter window, and a second sidewall blocking structure and a second polysilicon emitter region are formed in the second emitter window; the doping type of the first polysilicon emitter region is the same as the doping type of the first collector region, and the doping type of the second polysilicon emitter region is the same as the doping type of the second collector region.
2. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT according to claim 1, characterized in that: The first doping type is P-type doping, and the second doping type is N-type doping; or The first doping type is N-type doping, and the second doping type is P-type doping; or The first doping type and the second doping type are both P-type doping; or The first doping type and the second doping type are both N-type doping.
3. The manufacturing method and device of the dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT according to claim 1 or 2, characterized in that: The S1 step includes the following sub-steps: S101, providing a silicon substrate, and dividing at least one first device region and at least one second device region on the silicon substrate; S102, forming a first heavily doped buried layer of a first doping type below the first device region, and forming a second heavily doped buried layer of a second doping type below the second device region; S103, forming a first collector region of a first doping type in each first device region, the first collector region being located above the first heavily doped buried layer; forming a second collector region of a second doping type in each second device region, the second collector region being located above the second heavily doped buried layer; S104, forming a field oxygen isolation region around each first collector region and each second collector region respectively.
4. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT according to claim 3, characterized in that: The first collector region and the second collector region are formed by doping epitaxy, or by ion implantation doping and annealing; The first heavily doped buried layer and the second heavily doped buried layer are formed by ion implantation and annealing process, or by epitaxial process; The field oxygen isolation region is formed based on a trench isolation technology, based on a deep trench isolation technology combined with a PN junction isolation technology, or based on a local oxidation technology combined with a PN junction isolation technology.
5. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT according to claim 3, characterized in that: The S2 step includes the following sub-steps: S201, forming an intrinsic base region injection layer in the first collector region by ion implantation, wherein the doping type of the intrinsic base region injection layer is opposite to the doping type of the first collector region; S202, forming a first dielectric layer on the silicon substrate by a deposition or oxidation process, and forming an injected intrinsic base region by an annealing process so that the intrinsic base region injection layer is annealed; The S4 step includes the following sub-steps: S401, etching and removing the first dielectric layer above the second collector region to expose the second collector region; S402, performing SiGe epitaxial growth on the silicon substrate to form a SiGe epitaxial layer; S403, etching and removing the SiGe epitaxial layer outside the second collector region and the surrounding field oxygen isolation region, the etching stops in the first dielectric layer below the SiGe epitaxial layer, and the remaining SiGe epitaxial layer forms a SiGe heterojunction intrinsic base region in the second collector region.
6. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT according to claim 5, characterized in that: The S5 step includes the following sub-steps: S501, etching and removing the first dielectric layer not covering the SiGe epitaxial layer to expose the first collector region; S502, forming a second dielectric layer on the silicon substrate; S503, etching the second dielectric layer to form a first extrinsic base contact window in the first collector region and a second extrinsic base contact window in the second collector region; S504, forming a first polysilicon layer on the silicon substrate; S505, doping the first polysilicon layer to form a first doped polysilicon layer; the doping type of the first doped polysilicon layer above the first collector region is consistent with the doping type injected into the intrinsic base region, and the doping type of the first doped polysilicon layer above the second collector region is consistent with the doping type of the SiGe heterojunction intrinsic base region; S506, etching the first doped polysilicon layer, retaining the first doped polysilicon layer above the first collector region and the surrounding field oxygen isolation region to form a first extrinsic base region, and retaining the first doped polysilicon layer on the SiGe heterojunction intrinsic base region to form a second extrinsic base region.
7. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated silicon germanium HBT according to claim 6, characterized in that: The S6 step includes the following sub-steps: S601, forming a third dielectric layer on the silicon substrate; S602, etching the third dielectric layer and the first doped polysilicon layer, the etching stops in the second dielectric layer below the first doped polysilicon layer, forming a first emitter window in the first collector region, and forming a second emitter window in the second collector region.
8. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated germanium silicon HBT according to claim 7, characterized in that: The S7 step includes the following sub-steps: S701, forming a fourth dielectric layer on the silicon substrate; S702, etching the fourth dielectric layer in the first emitter window and the second emitter window, and etching stops in the second dielectric layer below the fourth dielectric layer; S703, etching the exposed second dielectric layer to expose the implanted intrinsic base region at the bottom of the first emitter window and the SiGe heterojunction intrinsic base region at the bottom of the second emitter window, and forming a first sidewall blocking structure in the first device region and a second sidewall blocking structure in the second device region; S704, forming a second polysilicon layer on the silicon substrate; S705, doping the second polysilicon layer to form a second doped polysilicon layer; wherein the second polysilicon layer located in an area above the first collector region is heavily doped with a first doping type, and the second polysilicon layer located in an area above the second collector region is heavily doped with a second doping type; S706, etching and removing the second doped polysilicon layer outside the first emitter window and the second emitter window, using a rapid annealing process to form a first polysilicon emitter region in the first emitter window, forming a second polysilicon emitter region in the first emitter window, and diffusing the doped impurities in the first polysilicon emitter region into the implanted intrinsic base region at the bottom of the first emitter window, and diffusing the doped impurities in the second polysilicon emitter region into the SiGe heterojunction intrinsic base region at the bottom of the second emitter window to form an emitter-base junction.
9. The method for manufacturing a dual polycrystalline self-aligned bipolar process integrated silicon germanium HBT according to claim 1, characterized in that: After executing the step S7, the following steps are further performed: S8. Form a collector contact electrode, a base contact electrode and an emitter contact electrode in each first device region and each second device region respectively.
10. A semiconductor device, characterized in that: The method for manufacturing a double polycrystalline self-aligned bipolar process integrated germanium silicon HBT is adopted as claimed in any one of claims 1 to 9.
Citation Information
Patent Citations
Mixed crystal face double polycrystal BiCMOS (Bipolar Complementary Metal Oxide Semiconductor) integrated device and manufacturing method thereof
CN102738155A
Manufacturing method for PNP triode integrated with germanium-silicon heterojunction NPN triode
CN103107087A
Manufacturing method of self-aligned germanium-silicon HBT device using non-selective epitaxy
CN108257867A
Integrating silicon-BJT to a silicon-germanium-HBT manufacturing process
CN110875249A
Method for integrating double-layer polycrystalline silicon self-aligned vertical bipolar transistor in germanium-silicon bipolar process and semiconductor device
CN116779541A