Method for manufacturing battery electrode plate group and device for manufacturing battery electrode plate group
By setting positioning holes on the plates of the secondary battery and using positioning pins for main positioning, the problem of cumbersome and time-consuming process of plate lamination in the prior art is solved, and efficient and accurate plate group manufacturing is achieved, which improves the The energy density of the battery.
Patent Information
- Application Number
- CN202380035688.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2022-04-28
- Filing Date
- 2023-04-27
- Publication Date
- 2024-12-06
AI Technical Summary
In the prior art, when manufacturing a stacked secondary battery, the positioning and stacking process of the electrode plates is complicated and takes a long time, making it difficult to shorten the stacking time while maintaining high overlap accuracy.
By setting a rectangular plate of positioning holes on the solid electrolyte layer, temporary positioning and adjusting the communication state of the positioning holes, and then using a positioning pin for main positioning, the one-time accurate overlap of multiple plates is achieved.
While maintaining high overlap accuracy, the stacking time is significantly shortened, the manufacturing efficiency of the plate set for batteries is improved, and the efficient production of batteries with high energy density can be achieved.
Smart Images

Figure CN119096391A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a method for manufacturing a battery electrode plate group and a device for manufacturing a battery electrode plate group. Background Art
[0002] The laminated secondary battery has a battery electrode group having a structure in which different polarity electrodes (negative electrode plates and positive electrode plates) are alternately laminated with an electrolyte layer interposed therebetween. Such a secondary battery can achieve high energy density and is therefore expected to be applied to electric vehicles, large storage batteries, and the like.
[0003] In order to prevent the assembled secondary battery from short circuiting, the battery plate assembly, such as Figure 2 As shown in (B), the overlapping position of the active material layer in the surface direction is consistent with the negative plate and the positive plate. In other words, in the projection diagram of the battery electrode group projected from above the stacking direction, it is important that the projection area of the positive electrode active material layer is consistent with the projection area of the negative electrode active material layer. If the electrode plate with the offset overlapping position is exposed from the overlapping position of other electrode plates, not only the overlapping area of the electrode plates is reduced and the energy density is reduced, but also the active material is precipitated on the negative electrode plate (for example, lithium precipitation is prone to occur in the case of a lithium ion secondary battery) and short circuits and other major problems are caused.
[0004] Therefore, when manufacturing a stacked secondary battery (electrode plate group for a battery), it is required to accurately position and stack the two electrode plates so that the overlapping positions of the active material layers are aligned.
[0005] In secondary batteries, a technique is usually used to suppress the occurrence of short circuits by making the size (main surface area) of the negative plate (negative electrode active material layer) larger than the size (main surface area) of the positive plate (positive electrode active material layer). If this technique is used, since the sizes of the stacked plates are different, even if the plates are positioned based on the corners or sides of the plates, it is impossible to stack the plates while including the overlapping position (projected area) of the positive electrode active material layer within the overlapping position (projected area) of the negative electrode active material layer.
[0006] Therefore, a method of alternately stacking positive and negative plates provided with positioning holes through separators or solid electrolyte layers while inserting the positioning holes one by one into positioning pins erected on a stacking table, and a device capable of implementing the method (patent documents 1 to 4) are proposed. For example, patent document 1 records "an electrode combination method for alternately stacking and combining electrodes of different polarities, characterized in that electrodes are transferred to a moving fixture in sequence from electrode magazines (electrode magazines) in which multiple electrodes of the same polarity are maintained in a stacked state and electrodes of different polarities are arranged in an alternating position along the moving path of the fixture, and are stacked while being positioned relative to each other by positioning pins erected on the fixture."
[0007] Previous technical literature
[0008] Patent Literature
[0009] Patent Document 1: Japanese Patent Application Publication No. 2001-297755
[0010] Patent Document 2: Japanese Patent Application Publication No. 2000-260478
[0011] Patent Document 3: Japanese Patent Application Laid-Open No. 11-045739
[0012] Patent Document 4: Japanese Patent Application Publication No. 2011-165620 Summary of the invention
[0013] Technical issues to be solved by the invention
[0014] As in the stacking methods described in the above-mentioned patent documents, the method of positioning and stacking the plates one by one is easy to accurately position the plates and stack them with high stacking accuracy, but when stacking a predetermined number of plates, there are problems such as cumbersome operation and long time required. For example, in Example 1 of Patent Document 2, it is recorded that it takes 28 minutes to stack 8 positive electrodes and 9 negative electrodes with a separator.
[0015] An object of the present invention is to provide a manufacturing method and a manufacturing apparatus capable of stacking a plurality of electrode plates while maintaining high stacking accuracy and shortening the stacking time for a battery electrode plate group to be incorporated into an all-solid-state secondary battery.
[0016] Means for solving technical problems
[0017] As a result of various studies conducted by the present inventors, it was found that when stacking a plurality of electrode plates with a solid electrolyte layer, first, a plurality of electrode plates with positioning holes were stacked and temporarily positioned, and the positioning holes of each electrode plate were adjusted to be connected to each other, and then, the positioning pins were inserted into the connecting holes formed by the temporary positioning, thereby adjusting and controlling the overlapping positions of the plurality of temporarily positioned electrode plates in the surface direction at one time (all at once). Further studies were conducted based on these insights, and the present invention was completed.
[0018] That is, the above-mentioned problems are solved by the following means.
[0019] <1> A method for manufacturing a battery electrode plate assembly, wherein a plurality of rectangular positive electrode plates and a plurality of rectangular negative electrode plates are alternately stacked with a solid electrolyte layer interposed therebetween, the method comprising the following steps:
[0020] A step of alternately placing rectangular positive electrode plates and rectangular negative electrode plates having positioning holes with a solid electrolyte layer interposed therebetween and temporarily positioning them to obtain a temporarily stacked electrode plate group in which the positioning holes communicate with each other; and
[0021] For the connecting hole formed by connecting the positioning holes to each other, while limiting the change in the stacking direction of the opening side of one side of the connecting hole, the positioning pin is inserted from the opening side of the other side until it protrudes to the opening side of one side, thereby performing the main positioning process for the rectangular positive plate and the rectangular negative plate constituting the temporary stacked plate group.
[0022] <2> The manufacturing method according to <1>, wherein the main positioning step includes performing the main positioning by inserting the positioning pins and moving the rectangular positive electrode plate and the rectangular negative electrode plate in a direction perpendicular to the insertion direction.
[0023] <3> The manufacturing method according to <1> or <2>, wherein the positioning pin includes a pin body portion having a diameter smaller than an inner diameter of the positioning hole, and a tip portion extending from one end of the pin body portion.
[0024] <4> The manufacturing method according to <3>, wherein in the main positioning step, the pin body is inserted into the communicating hole while being guided by the tip portion.
[0025] <5> The manufacturing method according to any one of <1> to <4>, wherein at least one of the rectangular positive electrode plate and the rectangular negative electrode plate used in the step of obtaining the provisional laminated electrode plate group has a solid electrolyte layer on both main surfaces of the active material layer.
[0026] <6> The manufacturing method according to any one of <1> to <5>, wherein in the step of obtaining the provisionally laminated electrode plate group, the laminated rectangular positive electrode plates and rectangular negative electrode plates are corrected to be flat.
[0027] <7> The manufacturing method according to any one of <1> to <6>, wherein the rectangular positive electrode plate and / or the rectangular negative electrode plate used in the step of obtaining the temporary stacked electrode plate group has a substrate extension portion having a positioning hole on at least one side of the short side of the active material layer.
[0028] <8> The production method according to <7>, wherein the rectangular positive electrode plate and / or the rectangular negative electrode plate used in the step of obtaining the provisional laminated electrode plate group has two or more base extension portions.
[0029] <9> The production method according to <7> or <8>, wherein the base extension portion extends to both sides of the short side of the active material layer.
[0030] <10> The manufacturing method according to any one of <1> to <9>, wherein in the step of obtaining the temporary stacked electrode plate group, after the rectangular positive electrode plates and the rectangular negative electrode plates are alternately stacked, they are shaken in a direction perpendicular to the stacking direction to assist temporary positioning.
[0031] <11> A device for manufacturing a battery electrode plate group, the device comprising:
[0032] The electrode group accommodating frame has an accommodating space for accommodating rectangular positive electrode plates and rectangular negative electrode plates with positioning holes in an alternately stacked state with solid electrolyte layers interposed therebetween, and in the electrode group accommodating frame, by being accommodated in the accommodating space, a temporarily stacked electrode plate group is formed in which the rectangular positive electrode plates and the rectangular negative electrode plates are temporarily positioned and the positioning holes are connected to each other;
[0033] A positioning fixture is arranged to be movable forward or backward relative to the stacking direction of the temporary stacked electrode group, and is provided with a positioning pin inserted into the positioning hole; and
[0034] The limiting component is configured to be able to clamp the electrode plate group containing frame and move relative to the opposite position of the positioning fixture, and can move relatively close to or away from the positioning fixture. The limiting component has a limiting portion that limits the change in the stacking direction of the opening side of one side of the connecting hole formed by connecting the positioning holes to each other, and a pin receiving portion that is arranged on the limiting portion and receives the positioning pin.
[0035] <12> The manufacturing device according to <11>, comprising: an electrode plate conveying device that alternately conveys the rectangular positive electrode plate and the rectangular negative electrode plate into the storage space via the solid electrolyte layer; and
[0036] The frame conveying device conveys the plate group containing frame to between the positioning fixture and the limiting component.
[0037] <13> The manufacturing device according to <11> or <12>, wherein the positioning pin includes a pin body portion having a diameter smaller than an inner diameter of the positioning hole, and a tip portion extending from one end of the pin body portion.
[0038] <14> The manufacturing apparatus according to any one of <11> to <13>, wherein at least one of the rectangular positive electrode plate and the rectangular negative electrode plate housed in the electrode plate group housing frame has a solid electrolyte layer on both main surfaces of the active material layer.
[0039] <15> The manufacturing apparatus according to any one of <11> to <14>, comprising a straightening member for straightening the stacked rectangular positive electrode plates and rectangular negative electrode plates to be flat.
[0040] <16> The manufacturing device according to any one of <11> to <15>, wherein the rectangular positive electrode plate and / or the rectangular negative electrode plate accommodated in the electrode plate group accommodating frame has a substrate extension portion having a positioning hole on at least one side of the short side of the active material layer.
[0041] <17> The manufacturing apparatus according to <16>, wherein the rectangular positive electrode plate and / or the rectangular negative electrode plate accommodated in the electrode plate group accommodating frame has two or more base extending portions.
[0042] <18> The manufacturing apparatus according to <16> or <17>, wherein the base extension portion extends to both sides of the short side of the active material layer.
[0043] <19> The manufacturing apparatus according to any one of <11> to <18>, further comprising a shaking device for shaking the electrode plate group housing frame in a direction perpendicular to a stacking direction of the rectangular positive electrode plates and the rectangular negative electrode plates.
[0044] Effects of the Invention
[0045] The method and apparatus for manufacturing a battery electrode plate group of the present invention can stack a plurality of electrode plates in a short stacking time while maintaining (controlling) high stacking accuracy, thereby manufacturing a battery electrode plate group with high accuracy and high production efficiency.
[0046] The above and other features and advantages of the present invention will become more apparent from the following description with appropriate reference to the accompanying drawings. BRIEF DESCRIPTION OF THE DRAWINGS
[0047] Figure 1 It is a schematic diagram showing a preferred embodiment of an electrode plate used in the present invention. Figure 1 (A) is a schematic top view showing a preferred embodiment of the electrode plate, Figure 1 (B) is a schematic front view showing a preferred embodiment of the electrode plate, Figure 1 (C) is a schematic front view showing a preferred embodiment of an electrode plate with an electrolyte layer.
[0048] Figure 2 It is a schematic diagram showing a preferred embodiment of the battery electrode assembly in the present invention. Figure 2 (A) is a schematic plan view showing a preferred embodiment of a battery electrode assembly, Figure 2 (B) is a schematic front view showing a preferred embodiment of a battery electrode assembly.
[0049] Figure 3 This is a schematic overall view showing a preferred embodiment of the manufacturing apparatus for a battery electrode assembly of the present invention. Figure 3(A) is a schematic plan view showing a preferred embodiment of a manufacturing apparatus for a battery electrode assembly according to the present invention. Figure 3 (B) is a schematic left side view showing a preferred embodiment of the manufacturing apparatus for a battery electrode assembly of the present invention.
[0050] Figure 4 This is a schematic front view schematically showing a state in which a frame is arranged below an opening and closing gate in a preferred embodiment of the manufacturing apparatus for a battery electrode plate group of the present invention.
[0051] Figure 5 This is a schematic front view schematically showing an electrode plate group storage frame, a positioning jig, and a restricting member in a preferred embodiment of the manufacturing apparatus for an electrode plate group for a battery according to the present invention.
[0052] Figure 6 This is a schematic front view showing a preferred embodiment of a positioning pin vertically provided on a positioning fixture. DETAILED DESCRIPTION
[0053] In the present invention, "positioning" refers to adjusting the overlapping position (stacking position) of the electrode plate, which is usually performed by displacing the electrode plate in the surface direction (longitudinal and transverse) of the electrode plate. The "positioning" includes: "temporary positioning", which is roughly positioned to the extent that the positioning holes are connected and a connecting hole appears; and "main positioning", which is to adjust (correct) the overlapping position of the positive active material layer and the negative active material layer in the temporarily positioned electrode plate (the position in the surface direction of the electrode plate, position deviation, etc.) with high precision to prevent the active material layer on one side (usually the positive active material layer (projection area)) from being exposed from the active material layer on the other side (usually the negative active material layer (projection area)). Here, "high precision" (also referred to as high overlapping precision) refers to adjusting the overlapping position to the extent that the active material layer on one side (usually the positive active material layer) is prevented from being exposed from the active material layer on the other side (usually the negative active material layer). Specifically, it cannot be uniquely determined based on the size of the electrode plate (active material layer), the size difference between the positive electrode active material layer and the negative electrode active material layer, the diameter difference between the positioning hole and the positioning pin, etc., but the overlapping accuracy (gap) in the later-described embodiments can be set to less than 3.0 mm, preferably less than 2.0 mm, more preferably less than 1.0 mm, and further preferably less than 0.5 mm.
[0054] In the present invention, "the positioning holes are connected to each other" includes the following two methods: a method in which all positioning holes punched in the negative plate, the positive plate, and the solid electrolyte layer in some methods are connected in the stacking direction according to the punching position, the number of punchings, etc. of the positioning holes; and a method in which the positioning holes punched in the negative plate are connected to the positioning holes punched in the positive plate, and the positioning holes punched in the positive plate are connected to the positioning holes punched in the negative plate. That is, the method of connecting the positioning holes to each other includes: the first method, which connects a plurality of positioning holes arranged on a line in the stacking direction of the electrode plate regardless of the type of the electrode plate; and the second method, which connects a plurality of positioning holes arranged on a line in the stacking direction of the electrode plate according to each electrode plate. In the first method, among the positioning holes punched in the negative plate, the positive plate, and the solid electrolyte layer in some methods, a plurality of positioning holes arranged on a line in the stacking direction are connected. On the other hand, in the second aspect, among the positioning holes bored in the electrode plates of the same polarity, a plurality of positioning holes arranged in a line along the stacking direction are connected, whereas the positioning holes bored in the electrode plates of different polarities are not connected.
[0055] In the present invention, the "main surface" refers to a surface perpendicular to the thickness direction of a flat plate such as an electrode plate, and generally refers to a surface having the largest surface area.
[0056] Furthermore, regarding an electrode plate and the like, a “plane direction” refers to a direction within a plane of a main surface, specifically, a longitudinal direction and a lateral direction.
[0057] In the present invention, when describing the content, physical properties, etc. of a component by showing a numerical range, when the upper limit and lower limit of the numerical range are described separately, any upper limit and lower limit can be appropriately combined to set to a specific numerical range. On the other hand, when setting a plurality of numerical ranges represented by "to" for description, the upper limit and lower limit forming the numerical range are not limited to the specific combination recorded before and after the "to" as a specific combination, but can be set to a numerical range formed by appropriately combining the upper limit and lower limit of each numerical range. In addition, in the present invention, the numerical range represented by "to" refers to a range that includes the numerical values recorded before and after the "to" as the lower limit and upper limit.
[0058] Preferred embodiments of the production method and production apparatus of the present invention will be described in detail below, but the present invention is not limited to the preferred embodiments.
[0059] [Plate]
[0060] First, the electrode plate used in the present invention will be described.
[0061] In the present invention, a rectangular positive electrode plate and a rectangular negative electrode plate (sometimes simply referred to as a positive electrode plate or a negative electrode plate) are used as electrode plates. Therefore, in the present invention, when referred to as a "electrode plate", it refers to a general term for positive electrode plates and negative electrode plates unless otherwise specified.
[0062] Furthermore, the "electrode plate" used in the present invention can change its shape, structure, etc. during or after the manufacturing process of the present invention, and can be the same as or different from the "electrode plate" constituting the electrode plate group for a battery manufactured by the manufacturing process of the present invention. In the present invention, when distinguishing between the two, the "electrode plate" used in the present invention is sometimes referred to as a "lamination electrode plate", and the "electrode plate" constituting the electrode plate group for a battery is sometimes referred to as a "lamination completed electrode plate".
[0063] The electrode plate used in the present invention has a rectangular thin plate shape when viewed in a plan view and has at least one positioning hole.
[0064] like Figure 1 As shown, the region in which at least the active material layer is formed in the stacked electrode plate is rectangular in plan view, preferably in the shape of a rectangular thin plate. In the present invention, "rectangle" refers to a square shape including a square and a rectangle, but as long as it functions as a plate for a battery electrode group (all-solid-state secondary battery), it is not limited to a geometrically precise square shape, and can be roughly square according to the purpose, required characteristics, etc. In addition, the corner can also be set to a chamfered shape.
[0065] The stacking electrode has at least one positioning hole. The shape of the positioning hole is preferably a shape similar to the shape of the cross-section perpendicular to the axis of the positioning pin described later, for example, it can be circular, elliptical, polygonal or star-shaped, preferably circular. There is no special restriction on the inner diameter of the positioning hole, which is appropriately determined according to the size of the electrode group housing frame, the size of the electrode plate, etc. in order to form a connecting hole by temporary positioning. For example, it can be set to 1.0 to 6.0 mm. From the perspective of overlapping accuracy, the difference between the inner diameter of the positioning hole and the outer diameter in the pin body of the positioning pin is preferably 0.01 to 0.5 mm.
[0066] In the stacking electrode plate, the position where the positioning hole is set (positioning hole formation area) can be any position (area) of the stacking electrode plate. From the perspective of overlapping accuracy, it is preferably near the edge of the active material layer or the corner of the stacking electrode plate (including the substrate extension setting part described later). The number of positioning holes in one stacking electrode plate is appropriately determined according to the shape of the positioning hole, the positioning method, the overlapping accuracy, etc. From the perspective of overlapping accuracy, it is preferably more than 2, and more preferably 2 to 5. In addition, when the shape of the positioning hole is a polygon, a star, etc., the positioning hole can be 1. When a stacking electrode plate has multiple positioning holes, there is no special restriction on the formation position of each positioning hole, but it is preferably not close to one corner, etc. For example, it is preferably set at each of the multiple edge sides, and more preferably set at each of the multiple corners. At this time, the shortest spacing between the positioning holes can be appropriately determined according to the size of the stacking electrode plate, for example, when it is a stacking electrode plate of the size described later, it can be set to 15 to 100 mm.
[0067] like Figure 1 As shown in FIG. 1 , the stacked electrode plate has active material layers of the same polarity on both main surfaces thereof. The electrode plate having the positive active material layer is called a positive electrode plate, and the electrode plate having the negative active material layer is called a negative electrode plate.
[0068] In addition, the electrode plates used in the present invention may be the same or different in shape and positioning holes, and the positive electrode plates and the negative electrode plates are preferably the same.
[0069] The stacked electrode plate usually has a substrate and an active material layer disposed on the two main surfaces of the substrate. As the substrate, the material used as the collector of the all-solid-state secondary battery can be used without particular restriction, and metal plates (thin) such as aluminum, aluminum alloy, copper, copper alloy, stainless steel, nickel, iron, and titanium are generally used. The active material layer can be used as a layer of the active material layer of the all-solid-state secondary battery without particular restriction, and usually contains an active material and appropriately contains an inorganic solid electrolyte, a conductive aid, a binder, and other additives. There is no particular restriction on the various substances constituting the active material layer, and the usual components can be used. For example, as an active material, as long as it is an electrode active material for a secondary battery, a positive electrode active material and a negative electrode active material can be cited.
[0070] In the present invention, as the stacking electrode plate, a electrode plate having positioning holes at least at the position where the positioning holes of the electrode plates of the same polarity are connected during stacking is used. At this time, the connected positioning holes are arranged and arranged on a line along the stacking direction of the electrode plates. In the present invention, according to the punching position of the positioning holes of the stacking electrode plate, as the positive electrode plate and the negative electrode plate, it is also possible to use an electrode plate having positioning holes at the same position, for example, an electrode plate partially having positioning holes arranged on the same line along the stacking direction during stacking.
[0071] The size of the electrode plate (longitudinal length and lateral length of the main surface) is not particularly limited and can be appropriately determined according to the purpose, required characteristics, etc. For example, as a rectangular electrode plate, the short side of the active material layer can be set to 40 to 200 mm, and the long side can be set to 100 to 600 mm. In the present invention, from the viewpoint of preventing short circuits, it is preferred that the size of the negative electrode active material layer of the negative electrode plate is set to be larger than the size of the positive electrode active material layer of the positive electrode plate, and the size difference of the long side in the two-electrode active material layer can be set to 0.5 to 6 mm, and the size difference of the short side can be set to 0.5 to 6 mm. As long as it is within this range, the decrease in energy density when used as a battery can also be suppressed.
[0072] The thickness of the substrate (especially the active material layer formation region) is not particularly limited and can be appropriately determined according to the application, required characteristics, strength (prevention of damage to the positioning holes), etc. For example, it can be 5 to 30 μm.
[0073] The thickness of the active material layer (provided on one main surface of the substrate) is not particularly limited and can be appropriately determined according to the application, required properties, etc. For example, it can be 30 to 300 μm.
[0074] The stacking electrode plate may be a rectangular electrode plate having positioning holes, and any electrode plate that is modified as appropriate may be used.
[0075] A stacking electrode plate as a preferred embodiment of the stacking electrode plate is shown in Figure 1 (A) and Figure 1 (B).
[0076] The stacking electrode plate 7A comprises: a substrate 8 having an active material layer forming region 8A which is rectangular in plan view, a pair of substrate extension portions (also referred to as lugs) 8B extending from the vicinity of both ends (long side edges) of one short side edge in a roughly rectangular protruding manner, and a lead portion 8C extending from the approximate center of the other short side edge in a roughly rectangular protruding manner; and an active material layer 8D, which is arranged on the two main surfaces of the active material layer forming region 8A. The lead portion 8C is a component that serves as a lead lug in a battery electrode plate assembly and an all-solid-state secondary battery. In a pair of substrate extension portions 8B, a circular positioning hole 8Ba is perforated in the approximate center portion thereof. In addition, the sizes of the substrate extension portion 8B and the lead portion 8C are appropriately determined.
[0077] Active material layer 8D is formed on both main surfaces of active material layer formation region 8A. Insulating portions 8E are formed along the short sides of active material layer 8D to seal the edges (end faces) with insulating resin for preventing short circuits with other stacked electrode plates.
[0078] Although no insulating portion is provided in the base extension portion 8B and the lead portion 8C of the lamination electrode plate 7A, an insulating portion may be provided from the viewpoint of preventing a short circuit.
[0079] The stacking electrode plate may be a form in which the stacking electrode plate 7A described above is appropriately modified.
[0080] For example, in the stacking electrode plate 7A, the base extension portion 8B and the lead portion 8C are provided on the short side edge of the substrate 11, but in the present invention, the stacking electrode plate can also be provided with the base extension portion and the lead portion on the long side edge of the base.
[0081] Furthermore, in the stacking electrode 7A, a pair (two) of substrate extension portions 8B (positioning holes 8Ba) are provided at the short side edge of one side of the active material layer forming region 8A, but in the present invention, it is also possible to provide a stacking electrode plate having one substrate extension portion (positioning hole) provided at the short side edge of one side of the active material layer forming region or to provide three or more stacking electrode plates.
[0082] Moreover, in the stacking electrode 7A, a pair of substrate extension portions 8B are provided on one short side edge of the active material layer forming region 8A, but in the present invention, a stacking electrode plate can also be provided with a pair of substrate extension portions on each of the two short side edges of the active material layer forming region. In this way, if a stacking electrode plate having a total of four substrate extension portions is used, not only can the positioning pins be inserted while reducing the loads involved in the substrate extension portions and the positioning holes, but also a higher overlapping accuracy can be achieved.
[0083] Furthermore, in the stacking electrode 7A, the positioning hole 8Ba is punched in the substrate extension portion 8B, but in the present invention, it is also possible to provide a stacking electrode with positioning holes in the active material layer or the lead portion without providing the substrate extension portion. In this case, if a plurality of positioning holes are punched, at least one positioning hole can be punched in the substrate extension portion or the lead portion, and the remaining positioning holes can be punched in the active material layer.
[0084] In addition, the insulating portion can be provided at a location where the electrode plates may short-circuit (contact) each other, for example, it can also be provided inside (inner surface) of the positioning hole other than the base extension portion and the lead portion.
[0085] The number of positioning holes can also be changed appropriately.
[0086] For example, the number of positioning holes perforated in one corner (including the substrate extension setting portion) is at least one, and can also be set to more than two. If operability, overlapping accuracy, etc. are considered, the number of positioning holes perforated in one corner is preferably one or two. When more than two positioning holes are perforated, there is no particular limitation on their configuration, for example, a configuration arranged along the short side direction or the long side direction of the substrate can be cited.
[0087] In the present invention, it is preferred that one of the positive and negative plates used as the stacked electrode plate 7A has a substrate extension portion, and it is one of the more preferred modes that both the positive and negative stacked electrode plates have a substrate extension portion, and it is also one of the more preferred modes that the positive electrode plate has a substrate extension portion and the negative electrode plate does not have a substrate extension portion. The electrode plate having a substrate extension portion can also adopt the above-mentioned deformation method. In addition, in the electrode plate without a substrate extension portion, the positioning hole 8Ba is provided in the active material layer or the lead-out portion as described later.
[0088] [Solid electrolyte layer]
[0089] The solid electrolyte layer is an electronically insulating electrolyte layer disposed between the positive electrode active material layer and the negative electrode active material layer in the battery electrode assembly, and any electrolyte layer used as a solid electrolyte layer of an all-solid-state secondary battery can be used without particular limitation.
[0090] The solid electrolyte layer can be used as a film formed by filming the material to be formed or a film formed, and can also be used as a layer formed on the active material layer of the stacked electrode or a layer stacked and arranged (pressed and bonded) on the active material layer. From the viewpoint of the manufacturing efficiency of the electrode plate group for the battery, it is preferably used as a layer formed on the active material layer of the stacked electrode or a layer stacked and arranged on the active material layer. From the viewpoint of preventing short circuits, etc., it is more preferably used as a layer formed on the negative electrode active material layer or a layer stacked and arranged on the negative electrode active material layer. Regarding the solid electrolyte layer for all-solid-state secondary batteries, when manufacturing the electrode plate group for the battery, the solid electrolyte layer can be used as an independent film or a layer attached to the electrode plate, which can improve the manufacturing efficiency of the electrode plate group for the battery. As the electrode plate having a solid electrolyte layer on the active material layer (sometimes referred to as a electrode plate with an electrolyte layer), there can be mentioned a negative electrode plate with an electrolyte layer and a positive electrode plate with an electrolyte layer. As the negative electrode plate 7B with an electrolyte layer and the positive electrode plate with an electrolyte layer, they are respectively as follows: Figure 1 As shown in (C), solid electrolyte layers 8F are stacked on each main surface of active material layer 8D, and other points are the same as electrode plate 7A.
[0091] The solid electrolyte layer generally contains an inorganic solid electrolyte and appropriately contains a binder and other additives. The substances constituting the solid electrolyte layer are not particularly limited, and common components can be used.
[0092] When a plate having positioning holes in the active material layer is used as a stacking plate in the solid electrolyte layer, a plate having positioning holes at positions corresponding to the positioning holes is used.
[0093] The size of the solid electrolyte layer is not particularly limited, and is usually set to the same size as the active material layer, preferably the same size as the negative electrode active material layer. The thickness of the solid electrolyte layer is not particularly limited, and can be appropriately determined according to the application, required characteristics, etc. For example, it can be set to 5 to 300 μm, and can also be set to 30 to 50 μm.
[0094] [Battery electrode assembly]
[0095] Next, a battery electrode plate group manufactured by the manufacturing method and the manufacturing apparatus of the present invention will be described.
[0096] A battery electrode plate group (also referred to as a battery electrode plate stack) is a battery electrode plate group in which a plurality of positive electrode plates and a plurality of negative electrode plates are alternately stacked with solid electrolyte layers interposed therebetween, and has a stacked structure of a plurality of negative electrode active material layers - solid electrolyte layers - positive electrode active material layers - solid electrolyte layers - negative electrode active material layers - ...
[0097] The number of stacked positive plates (negative plates) in the battery electrode assembly is not particularly limited and can be appropriately set depending on the application and required characteristics such as battery capacity and size, and can be set to, for example, 2 to 100.
[0098] The electrode plate (laminated electrode plate) constituting the electrode plate group for the battery may be the same as the laminated electrode plate or may be different from the laminated electrode plate. As an electrode plate different from the laminated electrode plate, for example, an electrode plate whose shape, structure, etc. of the laminated electrode plate is appropriately changed during or after the manufacturing process of the manufacturing method of the present invention can be cited. More specifically, an electrode plate from which the substrate extension portion of the laminated electrode plate is cut off can be cited.
[0099] The battery electrode plate group may include a fixing member for fixing the stacked state of the electrode plates, and a case (coating member) for covering the entirety.
[0100] The battery electrode group has an appropriate stacking state and shape according to the electrode plates used. Figure 1 A battery electrode assembly 9 as a preferred embodiment is shown in FIG. Figure 2 The battery electrode group 9 has the following structure: a negative electrode plate 7B with an electrolyte layer having a solid electrolyte layer provided on an active material layer of an electrode plate 7A and a positive electrode plate 7C corresponding to the electrode plate 7A, and five of each are alternately stacked in a direction in which the lead-out portions 8C of the negative electrode plate 7B with an electrolyte layer and the positive electrode plate 7C are on opposite sides.
[0101] In the present invention, a battery electrode assembly manufactured by using a stacking electrode plate or a negative electrode plate with an electrolyte layer without the base extension portion 8B instead of the stacking electrode plate 7A or the negative electrode plate with an electrolyte layer 7B is also a preferred embodiment. Figure 2 In the battery electrode plate group 9 shown, the negative electrode plate 7B with an electrolyte layer does not have the base extension portion 8B, and other than this, the battery electrode plate group 9 is the same.
[0102] [All-solid-state secondary battery]
[0103] As an all-solid-state secondary battery having a battery electrode group, the battery electrode group is a battery electrode group manufactured by the manufacturing method of the present invention or the manufacturing device of the present invention, and is the same as the known laminated all-solid-state secondary battery without any special restrictions. When installing the battery electrode group, the usual assembly steps such as connecting the negative plates to each other, setting the leads, and sealing them in the housing are performed.
[0104] [Method for manufacturing a battery plate assembly]
[0105] The manufacturing method of the battery electrode plate group of the present invention (sometimes referred to as the manufacturing method of the present invention) is a method for manufacturing a battery electrode plate group formed by alternately stacking a plurality of rectangular positive electrode plates and a plurality of rectangular negative electrode plates with a solid electrolyte layer interposed therebetween, in which a plurality of electrode plates are temporarily positioned and then positioned together, rather than a method for stacking a plurality of electrode plates while positioning them one by one. This manufacturing method of the present invention can position a plurality of electrode plates at once while maintaining high overlapping accuracy, and can achieve high production efficiency.
[0106] Specifically, the production method of the present invention includes the following step 1 and step 2.
[0107] Step 1: alternately placing rectangular positive electrode plates and rectangular negative electrode plates having positioning holes with a solid electrolyte layer interposed therebetween and temporarily positioning them to obtain a temporarily stacked electrode plate group in which the positioning holes communicate with each other in the stacking direction
[0108] Step 2: Inserting a positioning pin into the above-mentioned connecting hole formed in the step of obtaining the temporary stacked electrode plate group until the positioning pin protrudes from the other opening side to the one opening side while restricting the change in the stacking direction of the opening side (usually the area in the electrode plate where the positioning hole is punched), thereby mainly positioning the rectangular positive electrode plate and the rectangular negative electrode plate constituting the temporary stacked electrode plate group
[0109] [Equipment for manufacturing battery plate groups]
[0110] The manufacturing device of the battery electrode plate group of the present invention (sometimes referred to as the manufacturing device of the present invention) is a manufacturing device of the battery electrode plate group formed by alternately stacking a plurality of rectangular positive electrode plates and a plurality of rectangular negative electrode plates with a solid electrolyte layer interposed therebetween, and comprises: the following electrode plate group accommodating frame, temporarily stacking a plurality of electrode plates in a manner of forming a connecting hole in which positioning holes are connected to each other; the following positioning fixture, vertically provided with positioning pins inserted into the connecting hole to position the electrode plates; and the following limiting component, which is provided in a limiting portion that limits the change in the stacking direction of the opening side of one side of the connecting hole, and has a pin receiving portion that receives the positioning pin. The manufacturing device of the present invention having such a structure can appropriately implement the manufacturing method of the present invention, and can position a plurality of electrode plates at one time while maintaining high overlapping accuracy, thereby achieving high production efficiency.
[0111] The electrode group receiving frame has a receiving space, which receives the rectangular positive electrode plates and the rectangular negative electrode plates with positioning holes in an alternately stacked state with the solid electrolyte layer interposed therebetween. In the electrode group receiving frame, the rectangular positive electrode plates and the rectangular negative electrode plates with positioning holes are received in the receiving space, and the rectangular positive electrode plates and the rectangular negative electrode plates are temporarily positioned to form a temporarily stacked electrode group in which the positioning holes are connected to each other.
[0112] Positioning fixture: It is set to be able to move relatively to the front or back of the stacking direction of the temporary stacked plate group, and is vertically provided with positioning pins inserted into the positioning holes.
[0113] A limiting component: capable of clamping the electrode group containing frame to move relatively to the opposite position of the positioning fixture (positioning pin), and can move relatively close to or away from the positioning fixture, in which the limiting component has: a limiting portion, which limits the change in the stacking direction of the opening side of one side of the connecting holes that are connected to each other; and a pin receiving portion, which is arranged on the limiting portion and is used to receive the positioning pin (passed from the positioning hole)
[0114] The manufacturing device of the present invention only needs to have the above-mentioned electrode group containing frame, positioning fixture and limiting component, and may also appropriately have other structural devices (mechanisms), such as a conveying device for conveying the stacked electrode plates to the containing space, a device for transferring the electrode group containing frame or positioning fixture, etc.
[0115] Hereinafter, a preferred embodiment in which the plates are stacked in the horizontal direction using the negative plate 7B and the positive plate 7C with the electrolyte layer is given as an example, and the manufacturing method and the manufacturing device of the present invention are specifically described. However, the present invention is not limited to the preferred embodiment, and for example, the following embodiments are also included: the active material layers (main surfaces) of the plurality of plates are arranged in an upright state in a manner opposite to each other via the solid electrolyte layer, and the plates are arranged upright in the horizontal direction and stacked.
[0116] <Preferred embodiment of the production method of the present invention and the production device of the present invention>
[0117] In this preferred embodiment, using Figure 3 to Figure 5 A battery electrode plate group 9 is manufactured by a battery electrode plate group manufacturing apparatus 1 as one embodiment of a preferred manufacturing apparatus of the present invention.
[0118] like Figure 3 As shown, along the process of the manufacturing method, the manufacturing device 1 includes an electrode conveying device 2, an electrode group accommodating frame 3, and a frame conveying device ( Figure 3 Not shown in the figure. ), the positioning fixture 4 and the limiting component 5 integrated with the correction component 6.
[0119] In the manufacturing apparatus 1 , the direction in which the electrode plates are stacked (direction of gravity) is referred to as the up-down direction, and the advancing direction of the positioning pins 42 in this direction is referred to as the upward direction.
[0120] The structure of the production apparatus 1 will be described in sequence together with its modified examples.
[0121] like Figure 3 and Figure 4 As shown, the manufacturing device 1 comprises: conveyor belts 2A and 2B, which are used as plate conveying devices 2 for alternately conveying a plurality of rectangular positive plates and rectangular negative plates into a storage space through a solid electrolyte layer, and are arranged opposite to each other at intervals on a straight line; and an opening and closing gate 2C (at Figure 3 ), which is disposed between the conveyor belts 2A and 2B and located above the storage space 33 of the electrode group storage frame 3. The conveyor belt 2A is a conveyor belt that intermittently transports a plurality of negative electrode plates 7B with electrolyte layers toward the opening and closing gate 2C, and the conveyor belt 2B is a conveyor belt that intermittently transports a plurality of positive electrode plates 7C from the opposite direction of the conveyor belt 2A toward the opening and closing gate 2C. After placing one negative electrode plate 7B and one positive electrode plate 7C with electrolyte layers alternately transported from each conveyor belt 2A and 2B, the opening and closing gate 2C opens the gate and places them into the storage space 33 of the electrode group storage frame 3 located below.
[0122] The conveyor belts 2A and 2B are not particularly limited as long as they can convey the electrode plates 7B or 7C, and examples thereof include known conveying devices, various conveyor belts, mechanical arms, and manual conveying, and preferably conveyor belts. Furthermore, there are no particular limitations on the opening and closing gate 2C, and examples thereof include known opening and closing devices (mechanisms), such as a gate valve for a hopper, and the like.
[0123] In the present invention, the electrode plate conveying device is not limited to the above-mentioned method, and appropriate changes can be made. For example, it can be set to a structure in which the negative electrode plate with an electrolyte layer and the positive electrode plate are directly put into the storage space of the electrode plate group storage frame from two conveyor belts without using an opening and closing gate. In addition, it can also be set to a structure in which the negative electrode plate and the positive electrode plate with an electrolyte layer alternately placed on one conveyor belt are conveyed. When the negative electrode plate and the positive electrode plate with an electrolyte layer are conveyed by one conveyor belt, the impact when they are put into the opening and closing gate or the storage space can be reduced, and the breakage and damage of the electrode plate can be effectively prevented. Moreover, when the negative electrode plate with an electrolyte layer is not used, a third conveying device for conveying the solid electrolyte layer can also be provided. In addition, the manufacturing device of the present invention can also be provided without a electrode plate conveying device, but can be conveyed manually.
[0124] like Figure 3 to Figure 5 As shown, the manufacturing device 1 includes a plate assembly housing frame (sometimes simply referred to as a frame) 3. In particular, Figure 5 As shown, the frame 3 is a box (single-sided open frame) having a rectangular bottom 31 and a side wall (peripheral wall) 32 erected from the bottom 31 as described above, and has a storage space 33 surrounded by these components. The storage space 33 is stored in a state where a plurality of (specified number) negative plates 7B and positive plates 7C with electrolyte layers are alternately stacked across a solid electrolyte layer, so that the positioning holes 8Ba of the negative plates 7B with electrolyte layers and the positive plates 7C are set to be connected to each other, or the positioning holes 8Ba of the negative plates 7B with electrolyte layers and the positioning holes 8Ba of the positive plates 7C are connected to each other. The shape and size of this storage space 33 are determined according to the shape or size of the stacked electrode plates, the punching position, number, shape or size of the positioning holes, and the stacking speed. Usually, it is rectangular in plan view like the electrode plate, and the depth is appropriately determined according to the thickness and number of the stacked electrode plates. The internal dimensions of the frame 3 (the dimensions of the accommodating space 33) are set to a size relative to the dimensions of the electrode plates (the dimensions of the negative electrode plate 7B with electrolyte layers and the positive electrode plate 7C are larger at different times) to a size that allows a connecting hole to be formed in the positioning hole. For example, compared to the dimensions of the electrode plates, the longitudinal length (long side length) is preferably 0.1 to 1.0 mm larger, and the transverse length (short side length) is preferably 0.1 to 1.0 mm larger.
[0125] A hole 34 (see FIG. 1 ) is provided at a position of the bottom 31 corresponding to a positioning pin 42 provided upright on the positioning fixture 4 described later, through which the positioning pin 42 passes. Figure 5 ).
[0126] In the present invention, the frame is not limited to the above-mentioned form, and can be appropriately changed. For example, when stacking electrode plates in a vertical direction, a double-sided open frame having no bottom and consisting of side walls can be used.
[0127] Although in Figure 3 to Figure 5 Although not shown in the figure, the manufacturing device 1 includes a frame conveying device for conveying the frame 3 from the opening and closing gate 2C to between the positioning fixture 4 and the limiting member 5 described later. The frame conveying device is not particularly limited as long as it can convey the frame 3, and examples thereof include known conveying devices, various conveyor belts, robot arms, and manual conveying.
[0128] The manufacturing device 1 is provided with a frame conveying device, which enables the frame 3 to be relatively moved from the bottom of the opening and closing gate 2C to between the positioning fixture 4 and the limiting member 5. However, in the present invention, a structure in which a moving device is respectively provided on the positioning fixture and the limiting member, and the positioning fixture and the limiting member can be moved relative to the frame can also be set. As such a moving device, various conveying devices can be cited.
[0129] The manufacturing device 1 preferably has a correction component 6 that corrects the stacked electrode plates 7B and 7C in the storage space 33, especially the stacked portion of the active material layer 8D and the solid electrolyte layer 8F to be flat. The correction component 6 can correct (maintain) the electrode plates to be flat or make the electrode plates contact each other when the electrode plates are bent or when a space is formed between the stacked electrode plates, which helps to form the connecting hole. As such a correction component 6, a plate-like component, a block-like component, etc. with a flat surface can be cited, and a press can also be used. The correction component 6 is configured to be connected to a known conveying device, can move to the top of the frame 3, and can press the electrode plates (temporary stacked electrode plate group) accommodated in the storage space 33. There is no particular limitation as a pressing device for pressing the correction component 6 on the stacked electrode plates 7B and 7C. For example, a cam mechanism, a hydraulic piston, a press, a magnetic force, and a press based on the dead weight (gravity) of the correction component 6 can be cited.
[0130] In the present invention, the correction member is not limited to the above-mentioned embodiment, and can be appropriately modified. For example, the correction member can be integrated with the above-mentioned frame, the restriction member described later, or the positioning jig.
[0131] The manufacturing apparatus 1 includes a positioning jig 4 and a restricting member 5 that are relatively movable forward or backward in the stacking direction of the temporary stacked electrode plate group accommodated in the frame 3 (in the vertical direction of the temporary stacked electrode plate group).
[0132] like Figure 3 As shown in (B) of FIG. 1 , the positioning jig 4 and the limiting member 5 are configured in the manufacturing apparatus 1 so that the movable frame 3 is transported by the frame transport device, and the positioning jig 4 and the limiting member 5 are set at predetermined positions.
[0133] Positioning fixture 4 as long as Figure 3 and Figure 5The component shown is a positioning pin 42 erected on a base 41 on a flat plate. The axis vertical cross-sectional shape, erected position, and configuration of the positioning pin 42 are determined according to the shape, punching position, and configuration of the positioning hole 8Ba in the pole plates 7B and 7C. In the manufacturing device 1, one is erected at each corner of the rectangular base 41 of approximately the same size as the bottom 31 of the frame 3, and a total of four positioning pins 42 are erected. In the manufacturing device 1, two pairs of positioning pins 42 erected at the short side end of one side are used as negative plate pins inserted into the positioning hole 8Ba of the pole plate 7B, and two pairs of positioning pins 42 erected at the short side end of the other side are used as positive plate pins inserted into the positioning hole 8Ba of the pole plate 7C.
[0134] The shape of the positioning pin 42 is not particularly limited as long as it can be inserted into the positioning hole 8Ba and position the electrode plate. Figure 5 and Figure 6 As shown in (A), it is preferably provided with: a pin body (also referred to as a trunk) 42a having a diameter smaller than the inner diameter of the positioning hole 8Ba; and a tip (also referred to as a cone) 42b extending from one end of the pin body 42a. There is no particular limitation on the cross-sectional shape perpendicular to the axis of the tip 42b and the pin body 42a, and it can be, for example, circular, elliptical, polygonal, or star-shaped, preferably circular. As described later, the tip 42b plays a role in guiding the positioning pin 42 to be inserted into the connecting hole on the gradually enlarging peripheral side surface, and plays a role in assisting the overlapping position adjustment function of the pin body 42a. In addition, the pin body 42a plays the following overlapping position adjustment function, that is, by sequentially inserting the tip 42b into the connecting hole from the front end of the tip 42b, the outer peripheral surface contacts the inner periphery (inner surface) of the positioning hole 8Ba, thereby changing the pole plate whose overlapping position is offset, and adjusting it to a specified overlapping position. With such a pointed end 42 b, the positioning pin 42 can be easily inserted into the communicating hole formed in the temporarily stacked electrode plate group, and the breakage and damage of the substrate extension portion 8B caused by the insertion of the positioning pin 42 can be prevented, while achieving high-precision positioning of the electrode plate.
[0135] The outer diameter of the pin body 42a is appropriately determined according to the inner diameter of the positioning hole 8Ba, for example, it can be set to 1.0 to 8.0 mm. From the perspective of overlapping accuracy, the difference between the inner diameter of the positioning hole 8Ba and the outer diameter of the pin body 42a of the positioning pin 42 is set within the above range. The length of the pin body 42a can be appropriately determined as long as it can penetrate the positioning hole 8Ba of the temporary stacked electrode group. In addition, there are no special restrictions on the reduction rate ((maximum outer diameter-minimum outer diameter) / length) and length of the tip 42c, and they can be appropriately determined.
[0136] In the present invention, the positioning pin only needs to have a tip portion and a pin body portion with a gradually decreasing diameter, and various modifications can be made. Figure 6 As shown in (B), it is also possible to have a structure including a pin body 42a, a tip 42c extending from one end of the pin body 42a, and a rod 42d extending from the tip 42c in the same direction. Regarding the positioning pin having the rod 42d, the tip 42c enters after the rod 42d enters the communicating hole, so it is easy to insert the positioning pin 42 into the communicating hole.
[0137] like Figure 3 and Figure 5 As shown, the limiting component 5 only needs to be a component having a pin receiving portion (pin receiving hole) 52 punched in a flat base 51, and the punching position, configuration, etc. of the pin receiving portion 52 are determined corresponding to the vertical setting position, configuration, etc. of the positioning pin 42. The pin receiving portion 52 only needs to be formed to be able to insert the positioning pin 42, and the size is appropriately determined according to the outer diameter, insertion amount, etc. of the pin receiving portion 52. In the manufacturing device 1, a limiting surface 51b is protruding from the limiting component 5, and the limiting surface 51b contacts the upper surface of the temporary stacked electrode group when placed on the side wall 32 of the frame 3. The limiting component 5 has a pin receiving portion 52 instead of the positioning pin 42, and has a limiting surface 51b, and is basically the same as the positioning fixture 4 except that it has this. Specifically, the limiting component 5 is formed with one at each corner of the rectangular base 51 of approximately the same size as the bottom 31 of the frame 3, and a total of four pin receiving portions 52 are formed. The limiting component 5 is formed integrally with the above-mentioned correcting component 6. In the limiting surface 51b, the portion (area) located near the edge of the short side and opposite to the substrate extension portion 8B (positioning hole 8Ba) of the temporary stacked electrode group respectively acts as a limiting portion 51a for limiting the displacement of the substrate extension portion 8B, and the middle portion connecting the two limiting portions 51a acts as the above-mentioned correcting component 6.
[0138] There is no particular limitation on the relative movement mechanism that enables the limiting member 5 to move relatively closer to or farther from the positioning fixture 4, and various known moving devices (mechanisms) such as a cam mechanism and a hydraulic piston can be applied. In addition, a manual movement can also be adopted as the relative movement mechanism.
[0139] In the present invention, the positioning jig, the limiting member and the correcting member are not limited to the above-mentioned embodiments and can be appropriately modified. For example, the positioning jig and the limiting member can be movable relative to the frame, and the conveying device in this case is the same as the frame conveying device described above.
[0140] In the present invention, regarding the limiting components, each limiting part can be configured separately. For example, a negative electrode limiting component that is arranged on the substrate extension part of the negative electrode plate with an electrolyte layer and receives the negative electrode plate pin, and a positive electrode limiting component that is arranged on the substrate extension part of the positive electrode plate and receives the positive electrode plate pin can also be configured separately. In this case, the correction component can be continuously provided with any one of the negative electrode limiting component and the positive electrode limiting component and configured as an integral whole, or can be provided separately from the negative electrode limiting component and the positive electrode limiting component.
[0141] And, when relative to the temporary stacked plate group from Figure 3 On the contrary, when the positioning pin is inserted into the communication hole from the upper side to the lower side, that is, from the opening side of the frame 3 toward the bottom 31, the limiting member and the correcting member can be replaced by the bottom of the frame.
[0142] The manufacturing device 1 may be provided with a shaking device for shaking the frame 3 in the surface direction. The shaking device may be any shaking device as long as it can shake the frame 3, and various shaking devices may be applicable, and it may also be manual. The shaking device adjusts the overlapping position by shaking the frame 3 to move the electrode plates accommodated in the accommodation space 33 in the surface direction, thereby assisting the appearance of the connecting hole. The shaking device is configured to be connected to a known conveying device, can be moved to the side or bottom of the frame 3, and can shake the frame.
[0143] The manufacturing device 1 can replace the above-mentioned shaking device or in addition to the above-mentioned shaking device, further include a shaking device that shakes the frame 3 in the up-down direction or turns it upside down. The shaking device can be used as long as it can shake or turn the frame in the up-down direction. Various shaking devices and upside-down turning devices can be used, and it can also be done manually. The shaking device or the upside-down turning device moves the pole plate accommodated in the accommodation space in the up-down direction by shaking or turning the frame upside down, thereby avoiding the positioning pin and the pole plate from getting stuck in the main positioning process, and the auxiliary positioning pin completes the insertion. The shaking device or the upside-down turning device is also preferably configured as a device that can be shaken or turned upside down when the positioning fixture and the frame are integrated.
[0144] Each device constituting the production apparatus 1 may be formed of any appropriate material. Portions of the transport device and the like that come into contact with the active material layer are preferably formed of resin, rubber, or the like to prevent damage to the active material layer.
[0145] The manufacturing device 1 implements the method of inserting the positioning pin 42 into the communicating hole by relatively moving the positioning fixture 4 from the bottom (bottom 31) of the frame 3 toward the top (opening side of the frame 3), but in the present invention, it is also preferred to insert the positioning pin into the communicating hole by moving the positioning fixture from the top of the frame toward the bottom. As a manufacturing device capable of implementing this method, the bottom of the frame can function as a limiting component and a correcting component (the frame, the limiting component and the correcting component can be configured as an integral component). Therefore, in the above-mentioned manufacturing device, a structure without limiting components and correcting components can be set, and the positioning fixture can be set as a structure that can move relative to the frame. For example, it can be set to a structure in which the positioning fixture is set at a specified position, and the frame integrated with the limiting component, etc. is transported and moved to a position opposite to the positioning fixture by a frame conveying device. In addition, in this method, the correcting component can also be used as a component that is not integrated with the frame but separate, for example, the correcting component can be set on the pole plate (between the frame and the positioning fixture).
[0146] The manufacturing apparatus of the present invention can be configured by appropriately changing and combining the above-mentioned constituent elements such as the electrode assembly housing frame, the positioning jig, and the restricting member.
[0147] Next, as a preferred embodiment of the production method of the present invention, an embodiment using the production apparatus 1 will be described including the operation and effects of the production apparatus 1 .
[0148] In a manufacturing method as a preferred embodiment (hereinafter, sometimes referred to as the preferred manufacturing method of the present invention), the above-mentioned process of obtaining a temporary stacked electrode plate group and the process of performing the main positioning are performed, but other processes can also be performed before, between or after these processes. Specifically, the preferred manufacturing method of the present invention sequentially performs various processes such as a electrode plate manufacturing process, an electrode plate conveying process, a process of obtaining a temporary stacked electrode plate group, and a process of performing the main positioning. Moreover, various processes such as a fixing process, a removal process, a lead welding process, and a process of sealing in a shell can also be performed in sequence after the main positioning process. In addition, it is also preferred to appropriately perform a correction process and a shaking process (including an up and down shaking process and an up and down turning process).
[0149] In a preferred manufacturing method of the present invention, first, the negative electrode plate 7B and the positive electrode plate 7C with an electrolyte layer are manufactured as stacked electrode plates (electrode plate manufacturing step).
[0150] The negative electrode plate 7B with an electrolyte layer and the positive electrode plate 7C corresponding to the stacking electrode plate 7A can be produced according to a known method, and can usually be produced by forming an active material layer 8D on both main surfaces of the substrate 8. As a method for forming the active material layer 8D, a method of molding or film-forming (coating and drying) a composition containing an active material and appropriately containing an inorganic solid electrolyte, a binder, and other additives can be cited. The molding and film-forming methods and conditions can be appropriately determined.
[0151] The negative electrode plate 7B with an electrolyte layer is formed (laminated) with a solid electrolyte layer 8F on both main surfaces of the active material layer 8D in the laminated electrode 7A formed as described above. The method of forming the solid electrolyte layer 8F on the main surface of the active material layer 8D can be applied to various known methods, for example, a method of forming or film-forming on the main surface of the active material layer 8D, a method of transferring (pressing and bonding) the solid electrolyte layer 8F formed as described below to the main surface of the active material layer 8D, etc.
[0152] In addition, in the manufacturing method of the present invention, when the solid electrolyte layer is used separately from the pole plate 7A, the solid electrolyte layer is prepared. In the method for preparing the solid electrolyte layer, a composition containing an inorganic solid electrolyte and appropriately containing a binder and other additives is used to form or film on a substrate, and the method for preparing the pole plate is the same as the method for preparing the pole plate. However, when used in the manufacturing method of the present invention, the substrate is peeled off from the solid electrolyte layer.
[0153] In a preferred production method of the present invention, the produced stacking electrode plate is then transported to the frame 3 (electrode plate transporting step).
[0154] Specifically, if Figure 3 and Figure 4 As shown in FIG. 1 , negative electrode plates 7B with electrolyte layers are placed on conveyor belt 2A at a predetermined interval, and positive electrode plates 7C are placed on conveyor belt 2B at a predetermined interval. At this time, the two electrode plates are placed on conveyor belts 2A and 2B in a manner such that the substrate extension portions 8B (positioning holes 8Ba) are located on opposite sides of the long side direction of the electrode plates with one main surface facing upward. In a preferred manufacturing method of the present invention, as Figure 3As shown in the figure, the electrode plates 7B and 7C are arranged on the conveyor belts 2A and 2B in such a manner that the substrate extension portion 8B of the negative electrode plate 7B with the electrolyte layer is on the side of the positioning fixture 4 and the substrate extension portion 8B of the positive electrode plate 7C is on the side opposite to the positioning fixture 4. In this state, the two conveyor belts 2A and 2B are driven to alternately transfer the negative electrode plate 7B with the electrolyte layer and the positive electrode plate 7C to the opening and closing gate 2C. There is no particular limitation on the method of alternating transfer, and for example, various methods such as a method of adjusting the arrangement position and interval of the two electrode plates placed on the conveyor belts 2A and 2B and a method of intermittently driving the conveyor belts 2A and 2B can be cited.
[0155] In the preferred manufacturing method of the present invention, the next step is to transport (put) the electrode plates into the accommodation space 33 and obtain a temporary stacked electrode plate group.
[0156] When carrying out this process, Figure 3 (B) and Figure 4 As shown, the frame 3 is transported to the lower side of the opening and closing gate 2C (the lower side in the gravity direction) by the frame transport device. In this state, a predetermined number of plates are transferred and placed on the closed opening and closing gate 2C, and then the opening and closing gate 2C is opened, and the plates on the opening and closing gate 2C are transferred (put) into the frame 3 (accommodation space 33). The transfer can be performed by transferring the plates transferred to the opening and closing gate 2C one by one, or by transferring multiple plates at a time.
[0157] Thus, in the storage space 33 of the frame 3, a plurality of (specified number) of negative plates 7B with electrolyte layers and positive plates 7C are alternately stored and placed with the main surfaces in contact with each other, sandwiching the solid electrolyte layer. Here, since the size of the storage space 33, the size of the two plates, the shape of the positioning hole 8Ba, the inner diameter, etc. are set as described above, the plates placed (stored) in the storage space 33 are temporarily positioned, and in the same polarity plate group, the positioning holes 8Ba that are continuous along the stacking direction will not completely deviate from other positioning holes 8Ba in the surface direction, and at least a part will overlap. As a result, the positioning holes 8Ba of the negative plate 7B with electrolyte layer are connected to each other with a gap in the stacking direction (gravity direction) (in the overlapping area), and a connecting hole appears inside each positioning hole 8Ba. In addition, the positioning holes 8Ba of the positive plate 7C are also similarly connected to each other with a gap in the stacking direction, and a connecting hole appears inside each positioning hole 8Ba.
[0158] In this way, a provisional laminated electrode plate group is obtained in which the positioning holes 8Ba communicate with each other.
[0159] In the preferred manufacturing method of the present invention, when the stacking electrode plate 7B or 7C is bent or when a space is formed between the stacked electrode plates, it is preferred to correct the stacking electrode plate 7B or 7C to be flat (correction process). The correction process can be performed by pressing the temporary stacked electrode plate group by the above-mentioned correction component 6, but the pressing is released in the process of performing the main positioning described later. The correction process can be performed in the process of obtaining the above-mentioned temporary stacked electrode plate group, but it can also be performed before or after the process of obtaining the temporary stacked electrode plate group. If it is performed before or in the middle of the process of obtaining the above-mentioned temporary stacked electrode plate group, it can assist the appearance of the connecting hole or increase the size of the connecting hole.
[0160] In the preferred manufacturing method of the present invention, it is preferred to appropriately use the above-mentioned shaking device to shake the frame 3 in the plane direction (shaking process). In this way, the overlapping position of the electrode plates accommodated in the accommodation space 33 can be adjusted, and the appearance of the connecting hole can be assisted or the size of the connecting hole can be increased. The shaking process can be performed in the process of obtaining the above-mentioned temporary stacked electrode plate group, and can also be performed before or after the process of obtaining the temporary stacked electrode plate group.
[0161] In the preferred manufacturing method of the present invention, it is preferred that the frame 3 is appropriately shaken in the up-down direction or turned upside down (up-down shaking process or up-down turning process) instead of the above-mentioned shaking process or in addition to the above-mentioned shaking process. In this way, the electrode plate accommodated in the accommodation space 33 is moved in the up-down direction to avoid the positioning pin 42 and the electrode plate being stuck in the main positioning process, and the auxiliary positioning pin 42 is inserted. The up-down shaking process or the up-down turning process can be performed in the middle of the main positioning process.
[0162] In a preferred manufacturing method of the present invention, a main positioning step is then performed.
[0163] When carrying out this process, Figure 5 As shown, first, the frame 3 containing the temporary stacked electrode group is transported between the positioning fixture 4 and the limiting component 5 which are arranged away from each other in the direction of gravity by the above-mentioned frame conveying device, and then, the limiting component 5 is placed on the frame 3 in a state where the temporary stacked electrode group is in contact with the limiting portion 51a of the limiting component 5. As a result, the substrate extension portion 8B of the temporary stacked electrode group is restricted by the limiting portion 51a. In addition, the axis of the positioning hole 8Ba (communication hole) and the axis of the positioning pin 42 are located on a straight line along the direction of gravity. In addition, the hole 34 of the frame 3 and the axis of the pin receiving portion 52 of the limiting component 5 are also located on the above-mentioned straight line.
[0164] Then, in this state, the relative movement mechanism is driven to move the positioning fixture 4 relative to the limiting component 5. In this way, the positioning pin 42 of the positioning fixture 4 first passes through the hole 34 of the frame 3 and the tip 42b enters the connecting hole, then the pin body 42a enters the connecting hole, and finally reaches the pin receiving portion 52 of the limiting component 5, completing the insertion of the positioning pin 42 into the positioning hole 8Ba (inserted until it protrudes from the other opening side of the connecting hole to the opening side of one side). Here, the tip 42b that initially enters the connecting hole guides the pin body 42a to enter the connecting hole through the gradually expanding peripheral side surface, and assists in adjusting the overlapping position of the pin body 42a. Moreover, since the inner diameter of the positioning hole 8Ba and the outer diameter of the pin body 42a are set as described above, the pin body 42a enters the connecting hole immediately after the tip 42b, thereby enabling its outer peripheral surface to contact the inner peripheral surface of the positioning hole 8Ba, so that the pole plate with an offset overlapping position is changed in its surface direction (horizontal direction) and positioned at a specified overlapping position. Moreover, in the process of inserting the positioning pin 42, the change of the stacking direction (gravity direction) of the substrate extension part 8B is limited by the limiting part 51a configured in the state of contacting the temporary stacked electrode group, especially the change of the stacking direction of the substrate extension part 8B located on the side of the limiting component 5, that is, the opening side (limiting part 51a side) of one side of the connecting hole is limited. As a result, the substrate extension part 8B maintains a horizontal state, and the positioning pin 42 quickly enters and inserts into the connecting hole without damaging the substrate extension part 8B. Here, among the four positioning pins 42 erected on the base 41, two pairs of positioning pins (negative plate pins) 42 erected on the end of one side of the short side are inserted into the positioning hole 8Ba of the negative plate 7B to mainly position the negative plates 7B, and two pairs of positioning pins (positive plate pins) 42 erected on the end of the other side are inserted into the positioning hole 8Ba of the positive plate 7C to mainly position the positive plates 7C.
[0165] In the above series of actions, the mechanism by which each electrode plate is positioned by the insertion of the positioning pin 42 is the same as the positioning mechanism described in the above patent documents, but in the present invention, the electrode plate located on the side of the positioning fixture 4 is positioned toward the side of the limiting component 5 to the stacked electrode plates continuously or intermittently in sequence by the single insertion of the positioning pin 42.
[0166] In this way, the pin body 42a plays the role of adjusting the overlapping position. As a result, the base extension portion 8B, especially the positioning hole 8Ba, can be prevented from being damaged or broken, and the plurality of plates can be moved along the surface direction (a direction perpendicular to the insertion direction of the positioning pin 42) and the overlapping position of the plates can be adjusted with high precision, thereby precisely performing the main positioning of the temporarily positioned temporary stacked plate group.
[0167] As described above, the preferred production method of the present invention can easily produce a battery electrode plate assembly.
[0168] In a preferred production method of the present invention, the battery electrode assembly produced as described above can be further subjected to the following post-processing steps.
[0169] For example, there can be cited a process of driving the above-mentioned relative movement mechanism to move the positioning fixture 4 in a direction away from the limiting component 5 and pull the positioning pin 42 out of the positioning hole 8Ba; a process of cutting off the positioning pin 42 inserted into the positioning hole 8Ba from the base 41; and a process of cutting off the substrate extension portion 8B with the positioning pin 42 inserted from the electrode plate 7A, etc.
[0170] In addition, there can be cited the process of taking out the battery plate group from the storage space 33, the process of removing unnecessary layers on the upper and lower surfaces of the battery plate group and setting a substrate (collector), the process of welding leads to multiple lead portions 8C in the same polarity plates, the process of sealing the battery plate group in a shell, and the process of pressing the battery plate group.
[0171] In addition, before or after the above-mentioned post-processing step, there may be a step of fixing the electrode plates constituting the battery electrode plate group. The fixing step can generally be performed by sealing the peripheral surface of the battery electrode plate group with various resins or the like.
[0172] The present invention is not limited to the above-mentioned preferred production method of the present invention, and can be modified appropriately.
[0173] For example, in the preferred manufacturing method of the present invention, the substrate extension portions 8B of the positive electrode plate 7C and the negative electrode plate 7B are arranged on the opposite sides of the long side direction of the electrode plate and stacked, but in the present invention, as in the later-described embodiment 1, the substrate extension portions of the positive electrode plate and the negative electrode plate can also be arranged on the same side of the long side direction of the electrode plate and stacked. In this case, the positioning pins are inserted into the positioning holes of the positive electrode plate and the negative electrode plate to position the positive electrode plate and the negative electrode plate together.
[0174] In the preferred manufacturing method of the present invention described above, the method of alternately stacking the negative electrode plates 7B and the positive electrode plates 7C with electrolyte layers is described, but in the present invention, as the electrode plates arranged at the bottom and top layers of the manufactured battery electrode group, it is also possible to use an electrode plate having an active material layer and a solid electrolyte layer only on the main surface of one side of the substrate. If such an electrode plate is used, with the completion of the main positioning process, a battery electrode group with a stacked structure suitable for assembly into an all-solid-state secondary battery can be manufactured.
[0175] Furthermore, in the present invention, as the stacked electrode plate of the manufactured battery electrode group, an electrode plate having an active material layer and a solid electrolyte layer only on one main surface of the substrate can be used. If such an electrode plate is used, there is no need to mix double-sided electrode plates and single-sided electrode plates, and the transport device can be simplified.
[0176] Moreover, in the present invention, it is also preferred to insert the positioning pin into the communicating hole by moving the positioning fixture from the upper side of the frame (the opening side of the frame) toward the lower side (the bottom). In this method, the bottom of the frame can function as a limiting component and a correcting component. Therefore, the manufacturing method involved in the above preferred method can be implemented as follows, that is, without using limiting components and correcting components, by moving the positioning fixture toward the bottom relative to the temporary stacked plate group temporarily positioned in the storage space of the frame.
[0177] In addition, a manufacturing device 1 is used in the preferred manufacturing method of the present invention, but the manufacturing device used in the manufacturing method of the present invention is not limited to the manufacturing device 1. For example, a manufacturing device can be used that is composed of appropriately changing and combining various components such as a plate group containing frame, a positioning fixture, and a limiting component.
[0178] As described above, the method and apparatus for manufacturing a battery electrode plate group of the present invention can stack a plurality of electrode plates in a short stacking time while maintaining (controlling) high stacking accuracy, thereby manufacturing a battery electrode plate group with high accuracy and high production efficiency.
[0179] Furthermore, even when a negative electrode plate larger than a positive electrode plate is used, high stacking accuracy can be maintained, and a battery electrode plate group capable of highly suppressing the occurrence of short circuits can be manufactured with high production efficiency. In particular, from the viewpoint of preventing the occurrence of short circuits, the size of the negative electrode plate relative to the positive electrode plate can be set to a minimum, so that a battery electrode plate group capable of achieving high energy density can be manufactured with high production efficiency while suppressing the occurrence of short circuits.
[0180] Furthermore, the manufacturing method and manufacturing device of the battery electrode group of the present invention can position a plurality of electrode plates at the same time, so even if the number of stacked electrode plates increases, high production efficiency can be achieved while maintaining high overlapping accuracy. Therefore, in the present invention, the more the number of stacked electrode plates, the more obvious the effect becomes.
[0181] In the present invention for manufacturing a laminated electrode group for an all-solid-state secondary battery, the production efficiency of the electrode group for the battery can be further improved by using the above preferred embodiment of using a negative electrode plate with an electrolyte layer as the negative electrode plate and the solid electrolyte layer.
[0182] As described above, in the present invention in which the limiting component 5 and the positioning pin fixture 4 are used to position the stacked electrode plates, by appropriately changing the punching position, the number of punchings, etc. of the positioning holes of the electrode plates, it is possible to apply the present invention to the manufacture of battery electrode plates with an increased number of stacked electrode plates, battery electrode plates using stacked electrode plates with an increased surface area of the main surface of the active material layer, and battery electrode plates using stacked electrode plates with an increased quantity of the active material layer (the mass of the active material layer), without impairing the above-mentioned excellent effects.
[0183] Example
[0184] The present invention will be described in further detail below with reference to the Examples, but the present invention is not limited thereto and should not be construed. In the following Examples, unless otherwise specified, the "parts" and "%" representing the composition are based on mass. In the present invention, "room temperature" means 25°C.
[0185] In an embodiment, Figure 3 In the manufacturing apparatus 1 shown, the frame 3, the positioning jig 4, and the restricting member 5 were fabricated to manufacture a battery electrode plate assembly, and the stacking accuracy and the time required for positioning in the obtained battery electrode plate assembly were measured.
[0186] The production of the stacking electrode plates and the production of the battery electrode plate group are performed in an argon atmosphere with a dew point of -60°C or less or in a dry atmosphere.
[0187] <Manufacturing of frame 3A (used in Example 1 and comparative example)>
[0188] The frame 3A having the following dimensions was produced using metal aluminum: Two holes 34 penetrating in the thickness direction were bored at positions of the bottom 31 corresponding to the positioning pins 42 of the positioning member 4A.
[0189] Inner dimensions of the accommodation space 33: long side (vertical) 121.0 mm, short side (horizontal) 43.0 mm
[0190] <Preparation of frame 3B (used in Examples 2 to 4)>
[0191] A frame body 3B is manufactured which is the same as the frame body 3A except that four holes 34 penetrating in the thickness direction are bored at positions of the bottom 31 corresponding to the positioning pins 42 of the positioning member 4B.
[0192] <Preparation of Positioning Jig 4A (used in Example 1 and Comparative Example)>
[0193] A positioning jig 4A having the following dimensions was produced using metal aluminum.
[0194] Dimensions of base 41: Same as the outer dimensions of frame 3A
[0195] Positioning pins 42: Two positioning pins 42 are provided at positions corresponding to the positioning holes 8Ba on one short side of the base 41, and are provided vertically at intervals of 30 mm (center-to-center distance) along the short side.
[0196] Pin body 42a: diameter (outer diameter) 4.0 mm
[0197] <Preparation of positioning jig 4B (used in Examples 2 to 4)>
[0198] A positioning jig 4B is manufactured which is identical to the positioning jig 4A except that two positioning pins 42 are erected at intervals of 30 mm along the two short sides of the base 41 at positions corresponding to the positioning holes 8Ba, for a total of four positioning pins 42 .
[0199] <Manufacturing of Restriction Member 5A (used in Example 1 and Comparative Example)>
[0200] The restriction member 5A having the following dimensions was produced using metal aluminum.
[0201] Dimensions of base 51: Same as the outer dimensions of frame 3A
[0202] Pin receiving portion 52: Two holes are punched at positions corresponding to the positioning pins 42 of the positioning member 4A.
[0203] Pin receiving portion 52: diameter 4.1 mm
[0204] The four edges of the base 51 are cut to protrude and provide a limiting surface 51 b (height 40 mm) having the same size as the inner dimension of the accommodation space 33 .
[0205] <Manufacturing of Restriction Member 5B (used in Examples 2 to 4)>
[0206] A restriction member 5B is manufactured which is the same as the restriction member 5A except that a total of four pin receiving portions 52 are provided at positions corresponding to the positioning pins 42 of the positioning member 4B on both short sides of the base 51 .
[0207] Next, the negative electrode plate 7B and the positive electrode plate 7C with an electrolyte layer were produced as the stacking electrode plate 7A.
[0208] <Preparation of negative electrode plate 7B with electrolyte layer>
[0209] (Making of base material)
[0210] A substrate having the following dimensions is cut out from a 10 μm thick stainless steel foil (hereinafter referred to as stainless steel foil) and has two substrate extension portions 8B at both ends of one short side edge and one lead portion 8C in the center of the other short side edge.
[0211] Dimensions of the active material layer forming region 8A: long side 100.0 mm, short side 42.0 mm
[0212] The external dimensions of the substrate (negative electrode plate) including the substrate extension portion 8B and the lead portion 8C are: long side 120.0 mm, short side 42.0 mm
[0213] The length of the substrate extension portion 8B and the lead portion 8C in the long side direction: 10.0 mm
[0214] Inner diameter of the positioning hole 8Ba bored in the base extension portion 8B: 4.1 mm
[0215] The interval of the short side direction of the positioning hole 8Ba: 30mm
[0216] (Manufacturing of negative plate)
[0217] A slurry containing a negative electrode mixture was prepared using 53 parts by mass of natural graphite as a negative electrode active material, 45 parts by mass of argyrodite sulfide solid electrolyte (Li6PS5Cl), 2 parts by mass of a rubber-based binder (solid content conversion value), and a tetralin-anisole mixed solvent. Next, the obtained slurry containing a negative electrode mixture was applied and dried on both sides (active material layer forming area 8A) of the above-mentioned substrate (collector) in such a manner that the film thickness after application and drying was 130 μm, thereby producing a negative electrode plate having a negative electrode active material layer on both sides.
[0218] (Fabrication of Solid Electrolyte Layer)
[0219] A slurry containing a solid electrolyte was prepared using 98 parts by mass of a argyrodite sulfide solid electrolyte (Li6PS5Cl), 2 parts by mass of a rubber-based binder (solid content conversion value), and a tetralin-anisole mixed solvent. Next, the obtained slurry containing a solid electrolyte was applied and dried on one surface of a stainless steel foil having a thickness of 10 μm in such a manner that the film thickness after application and drying became 120 μm. In this way, a laminate of two solid electrolyte layers and stainless steel foils having the same dimensions as the long and short sides of the above-mentioned negative electrode active material layer was prepared.
[0220] (Preparation of Negative Electrode Plate 7B with Electrolyte Layer)
[0221] After the solid electrolyte layer of each laminate was stacked on each negative electrode active material layer of the manufactured negative electrode plate and pressed, the stainless steel foil was peeled off from the solid electrolyte layer. In addition, the quantitative (mass per unit area) of the negative electrode active material layer and the solid electrolyte layer did not change (decrease) by the pressing process.
[0222] Thus, the Figure 1The negative electrode plate with an electrolyte layer (referred to as “negative electrode plate with an active material layer” in Table 1) shown in (C) 7B.
[0223] <Production of positive electrode plate 7C>
[0224] (Making of base material)
[0225] A substrate having the following dimensions and having two substrate extension portions 8B at both ends of one short side edge and one lead portion 8C at the center of the other short side edge was cut out from a stainless steel foil having a thickness of 10 μm.
[0226] The size of the active material layer forming area 8A: long side 96.0 mm, short side 40.0 mm
[0227] The outer dimensions of the substrate (positive electrode plate) including the substrate extension portion 8B and the lead portion 8C are: long side 120.0 mm, short side 40.0 mm
[0228] The length of the substrate extension portion 8B and the lead portion 8C in the long side direction: 12.0 mm
[0229] Inner diameter of the positioning hole 8Ba bored in the base extension portion 8B: 4.1 mm
[0230] The interval of the short side direction of the positioning hole 8Ba: 30mm
[0231] (Manufacturing of Positive Electrode Plate 7C)
[0232] Using positive electrode active material NCM523 (LiNi 0.5 Co 0.2 Mn 0.3 A slurry containing a positive electrode mixture was prepared by using 66 parts by mass of a substance in which the surface of the particles is coated with LiNbO3), 30 parts by mass of a argyrodite sulfide solid electrolyte (Li6PS5Cl), 3 parts by mass of VGCF (carbon fiber manufactured by Showadenko KK) as a conductive aid, 1 part by mass of a rubber-based binder (solid content conversion value), and a tetralin-anisole mixed solvent. Next, the obtained slurry containing the positive electrode mixture was applied and dried on both sides (active material layer forming area 8A) of the above-mentioned substrate (collector) in such a way that the film thickness after coating and drying became 90 μm. In this way, a positive electrode active material layer having positive electrode active material layers on both sides was prepared. Figure 1 The electrode plate 7A shown in (B) is a positive electrode plate 7C.
[0233] [Example 1]
[0234] The battery plate group of Example 1 was manufactured by alternately stacking ten negative electrode plates 7B and positive electrode plates 7C with electrolyte layers, with the substrate extension portions 8B of the two electrode plates 7B and 7C located on the same side of the long side direction of the electrode plates (one-side extraction).
[0235] Specifically, the negative electrode plate 7B and the positive electrode plate 7C with the electrolyte layer are manually placed one by one in the storage space 33 of the frame 3A in this order, and 10 plates are stacked and stored respectively. As a result, the pole plates 7B and 7C are temporarily positioned by the storage space 33, and there are connecting holes 8Ba perforated in the substrate extension portions 8B of the pole plates 7B and 7C that are connected to each other in the stacking direction. In this way, a temporary stacked pole plate group consisting of 10 pole plates 7B and 7C is obtained. In addition, no bending is observed in the pole plates 7B and 7C, and no space is observed between the pole plates of the temporary stacked pole plate group. Therefore, in Example 1, the process of correcting the pole plates to be flat is not performed.
[0236] Next, a limiting component 5A is placed on the frame 3A that accommodates the obtained temporary stacked electrode group, and a positioning fixture 4A is arranged below the frame 3A. At this time, the limiting portion 51a limits the vertical movement of the substrate extension portion 8B of the temporary stacked electrode group. In addition, the axis of the connecting hole appearing in the positioning hole 8Ba, the axis of the positioning pin 42 erected on the positioning fixture 4A, and the pin receiving portion 52 of the limiting component 5A are located on a vertical line. In this state, the positioning fixture 4A is manually moved upward toward the limiting component 5A at a speed of about 3 cm / minute, so that the positioning pin 42 is inserted into the connecting hole and finally advances to the pin receiving portion 52 of the limiting component 5A. In this way, a total of 20 electrodes 7B and 7C are positioned together to manufacture the electrode plate group for the battery of Example 1.
[0237] [Example 2]
[0238] In the manufacturing method of the electrode plate group for a battery of Example 1, in the storage space 33 of the frame 3B used instead of the frame 3A, the negative electrode plates 7B with electrolyte layers and the positive electrode plates 7C are alternately stacked in a configuration where the substrate extension portions 8B are located on opposite sides of each other in the long side direction of the electrode plates (taken out on both sides), and the positioning fixture 4B and the limiting member 5B are used instead of the positioning fixture 4A and the limiting member 5A, and the negative electrode plates 7B with electrolyte layers and the positive electrode plates 7C are respectively mainly positioned separately. Otherwise, a battery electrode plate group equivalent to Example 1 is manufactured in the same manner as the manufacturing method of the electrode plate group for a battery. Figure 2 The battery electrode plate assembly 9 shown is a battery electrode plate assembly according to a second embodiment.
[0239] [Example 3]
[0240] The battery electrode plate assembly of Example 3 was manufactured in the same manner as the battery electrode plate assembly of Example 2 except that 20 negative electrode plates 7B and 20 positive electrode plates 7C with electrolyte layers were alternately stacked.
[0241] [Example 4]
[0242] The battery electrode plate assembly of Example 4 was manufactured in the same manner as the battery electrode plate assembly of Example 2 except that 40 negative electrode plates 7B and 40 positive electrode plates 7C with electrolyte layers were alternately stacked.
[0243] [Comparative Example 1]
[0244] In the manufacturing method of the battery electrode plate group of Example 1, the manufacturing of the battery electrode plate group was attempted in the same manner as the manufacturing method of the battery electrode plate group of Example 1, except that the restriction member 5 was not used. However, although the electrode plates 7B and 7C could be temporarily positioned, the positioning pins 42 could not be inserted into the positioning pin holes 8Ba (communication holes), and the battery electrode plate group could not be manufactured.
[0245] [Comparative Example 2]
[0246] In the manufacturing method of the battery electrode plate group of Example 1, the battery electrode plate group of Comparative Example 2 was manufactured in the same manner as the manufacturing method of the battery electrode plate group of Example 1, except that the positioning holes 8Ba of the negative electrode plate 7B with an electrolyte layer and the positive electrode plate 7C were manually inserted into the positioning pins 42 of the positioning fixture 4A one by one, and a total of 20 plates were stacked.
[0247] In addition, in Comparative Example 2, the frame 3A is pre-arranged on the positioning fixture 4A, and each time a pole plate is arranged in the accommodation space 33 of the frame 3A, the limiting component 5A is arranged on the positioning hole 8Ba. After the positioning hole 8Ba of each pole plate is completely inserted into the positioning pin 42, the limiting component 5 is removed to arrange (accommodate) the next pole plate.
[0248] [Comparative Example 3]
[0249] In the manufacturing method of the battery electrode plate group of Example 1, the internal dimensions of the frame 3A (the dimensions of the storage space 33) were changed to 120.0 mm on the long side and 42.0 mm on the short side, and the battery electrode plate group was manufactured in the same manner as the manufacturing method of the battery electrode plate group of Example 1. However, the prescribed number of electrode plates 7B and 7C could not be accommodated (temporarily positioned) in the storage space 33 of the frame 3A, and a temporarily stacked electrode plate group could not be obtained. As a result, the positioning pin 42 could not be inserted into the positioning pin hole 8Ba, and the battery electrode plate group could not be manufactured.
[0250] [Comparative Example 4]
[0251] In the manufacturing method of the battery electrode plate group of Example 1, the manufacturing of the battery electrode plate group was attempted in the same manner as the manufacturing method of the battery electrode plate group of Example 1 except that the frame 3A was not used. However, no communicating hole appeared inside the positioning hole 8Ba (temporary positioning could not be performed), and a temporary stacked electrode plate group could not be obtained. As a result, the positioning pin 42 could not be inserted into the positioning pin hole 8Ba, and the battery electrode plate group could not be manufactured.
[0252] <Evaluation of Overlap Accuracy>
[0253] The overlap accuracy of the manufactured battery electrode plate group was evaluated by measuring the remaining amount (gap) of the positive electrode plate 7C up to the allowable limit position of the overlap position of the positive electrode plate 7C with respect to the negative electrode plate 7B with an electrolyte layer.
[0254] In this evaluation, from the viewpoint of preventing short circuits from occurring, the allowed limit position of the overlapping position of the positive electrode plate 7C is set to the position where the positive electrode plate 7C (active material layer forming area 8A) does not expose the position of each edge of the long side and short side of the negative electrode plate 7B with an electrolyte layer (active material layer forming area 8A), that is, the position of the negative electrode plate 7B with an electrolyte layer (active material layer forming area 8A). It is assumed that when the center lines of the short side direction of the positive electrode plate 7C and the negative electrode plate 7B with an electrolyte layer are stacked in unison, each long side edge of the positive electrode plate 7C has a margin of 1 mm in the short side direction relative to the negative electrode plate 7B with an electrolyte layer. Therefore, in this evaluation, the larger the gap, the higher the overlap accuracy of the battery plates can be stacked.
[0255] Specifically, an X-ray transmission image was observed perpendicularly from the stacking direction using a high-resolution 3D X-ray microscope: nano3DX (trade name, manufactured by Rigaku Corporation) at the long side end of the stacked electrode group. In the X-ray transmission image, the long side end of the negative electrode plate 7B (active material layer formation area 8A) located further below and offset to the outside can be observed. With respect to the obtained X-ray transmission image, the gap distance (offset) between the negative electrode plate and the positive electrode plate (active material layer formation area 8A) at the position closest to the positive electrode plate and the negative electrode plate was measured on both sides of the long side end, and the minimum offsets obtained were added and divided by 2, thereby evaluating the margin (gap) of the positive electrode plate 7C.
[0256] In addition, in Comparative Examples 1, 3, and 4, no battery electrode plate group was produced, and therefore the overlapping accuracy could not be evaluated, which is indicated by "×" in Table 1.
[0257] <Evaluation of production efficiency>
[0258] In the manufacture of the battery electrode plate group in Examples 1 to 4 and Comparative Example 2, the time required to stack a predetermined number of negative electrode plates 7B and positive electrode plates 7C with electrolyte layers for main positioning (to insert the positioning pins 42 into the communicating holes without damaging the substrate extension portion 8B and reach the pin receiving portion 52) was measured from the start of the movement of the positioning fixture 4. The measured time was converted into the time required to alternately stack 10 negative electrode plates 7B and 10 positive electrode plates 7C with electrolyte layers for main positioning (actual positioning time / (20 plates / actual number of stacked plates)), and the obtained time was set as "the time required for positioning 20 plates". The results are shown in Table 1.
[0259] As described above, in Comparative Examples 1, 3, and 4, no battery electrode plate groups could be produced, and thus the present test was not conducted (indicated by "×" in Table 1).
[0260] <Damage evaluation of active material layer and solid electrolyte layer>
[0261] The battery electrode groups manufactured in Examples 1 to 4 and Comparative Example 2 were visually checked for defects such as defects in the negative electrode active material layer and the solid electrolyte layer of the negative electrode plate 7B with an electrolyte layer. The results are shown in Table 1. This test is a reference test for evaluating whether a battery electrode group can be manufactured without causing defects in the active material layer.
[0262] As described above, in Comparative Examples 1, 3, and 4, no battery electrode plate groups could be produced, and thus the present test was not conducted (indicated by "×" in Table 1).
[0263]
[0264] From the results shown in Table 1, the following can be seen.
[0265] Comparative Example 1, which does not use the limiting component 5A, can temporarily position the negative electrode plate 7B and the positive electrode plate 7C with the electrolyte layer, but cannot insert the positioning pin 42 into the connecting holes of the negative electrode plate 7B and the positive electrode plate 7C with the electrolyte layer. In addition, in Comparative Example 2, which uses the limiting component 5A to position the negative electrode plate 7B and the positive electrode plate 7C with the electrolyte layer one by one, although the overlapping accuracy is sufficient, the time required for stacking increases significantly, and the production efficiency is poor. In addition, in Comparative Example 3, in which the internal dimensions of the accommodating space 33 of the frame 3A are set to the same dimensions as the negative electrode plate 7B and the positive electrode plate 7C with the electrolyte layer, the specified number of negative electrode plates 7B and the positive electrode plate 7C with the electrolyte layer cannot be accommodated in the accommodating space 33. In addition, in Comparative Example 4, which does not use the frame 3A, the connecting hole cannot be made to appear in the positioning hole 8Ba, and the negative electrode plate 7B and the positive electrode plate 7C with the electrolyte layer cannot be temporarily positioned.
[0266] In contrast, it can be seen that in Examples 1 to 4 in which a frame 3, a positioning fixture 4 and a limiting component 5 are used, and in which the positioning pin 42 is inserted into the connecting hole that appears in the process of obtaining a temporary stacked electrode plate group during the main positioning process, although the time required for stacking is short, the negative electrode plates 7B and the positive electrode plates 7C with electrolyte layers can still be alternately stacked with high overlapping accuracy, and damage to the active material layer and the solid electrolyte layer can be prevented.
[0267] From the above results, it can be seen that the method and apparatus for manufacturing a battery electrode plate group of the present invention can manufacture a battery electrode plate group with high precision and high production efficiency.
[0268] The present invention has been described together with its embodiments, but unless otherwise specified, we do not intend the present invention to be limited to any of the details described and it is deemed to be broadly construed without departing from the spirit and scope of the invention as set forth in the appended claims.
[0269] This application claims priority based on Japanese Patent Application No. 2022-074775 filed in Japan on April 28, 2022, which are hereby incorporated by reference and the contents thereof are incorporated into this specification as a part of what is described in this specification.
[0270] Explanation of symbols
[0271] 1-a manufacturing device for a battery electrode plate group, 2-a electrode plate conveying device, 2A, 2B-a conveyor belt, 2C-an opening and closing gate, 3-a electrode plate group accommodating frame, 31-a bottom, 32-a side wall, 33-an accommodating space, 34-a hole, 4-a positioning fixture, 41-a base, 42-a positioning pin, 42a-a pin body, 42b, 42c-a tip, 42d-a rod, 5-a limiting component, 51-a base, 51a-a limiting component, 51b-a limiting surface, 52-a pin receiving component, 6-a correcting component, 7A-a stacking electrode plate, 7B-a negative electrode plate with an electrolyte layer, 7C-a positive electrode plate, 8-a substrate, 8A-an active material layer forming region, 8B-a substrate extension setting portion, 8Ba-a positioning hole, 8C-a lead-out portion, 8D-an active material layer, 8E-an insulating portion, 8F-a solid electrolyte layer, 9-a battery electrode plate group.
Claims
1. A method for manufacturing a battery electrode plate group, which is a method for manufacturing a battery electrode plate group formed by alternately stacking a plurality of rectangular positive electrode plates and a plurality of rectangular negative electrode plates with a solid electrolyte layer interposed therebetween, comprising the following steps: A step of alternately placing rectangular positive electrode plates and rectangular negative electrode plates having positioning holes with a solid electrolyte layer interposed therebetween and temporarily positioning them to obtain a temporarily stacked electrode plate group in which the positioning holes communicate with each other; and For the connecting hole formed by connecting the positioning holes to each other, while limiting the change in the stacking direction of the opening side of one side of the connecting hole, the positioning pin is inserted from the opening side of the other side until it protrudes to the opening side of one side, thereby performing the main positioning process for the rectangular positive plate and the rectangular negative plate constituting the temporary stacked plate group.
2. The manufacturing method according to claim 1, wherein: In the main positioning step, the rectangular positive electrode plate and the rectangular negative electrode plate are moved in a direction perpendicular to the insertion direction by inserting the positioning pins to perform the main positioning.
3. The manufacturing method according to claim 1 or 2, wherein: The positioning pin includes a pin body portion having a diameter smaller than an inner diameter of the positioning hole, and a tip portion extending from one end of the pin body portion.
4. The manufacturing method according to claim 3, wherein: In the main positioning step, the pin body is inserted into the communication hole while being guided by the tip portion.
5. The manufacturing method according to any one of claims 1 to 4, wherein: At least one of the rectangular positive electrode plate and the rectangular negative electrode plate used in the step of obtaining the provisional laminated electrode plate group has a solid electrolyte layer on both main surfaces of the active material layer.
6. The manufacturing method according to any one of claims 1 to 5, wherein: In the step of obtaining the provisional laminated electrode plate group, the laminated rectangular positive electrode plates and the rectangular negative electrode plates are corrected to be flat.
7. The manufacturing method according to any one of claims 1 to 6, wherein: The rectangular positive electrode plate and / or the rectangular negative electrode plate used in the step of obtaining the provisional laminated electrode plate group includes a base extension portion having a positioning hole on at least one side of the short side of the active material layer.
8. The manufacturing method according to claim 7, wherein: The rectangular positive electrode plate and / or the rectangular negative electrode plate used in the step of obtaining the provisional laminated electrode plate group has two or more of the base extending portions.
9. The manufacturing method according to claim 7 or 8, wherein: The substrate extension portion is extended to both sides of the short side of the active material layer.
10. The manufacturing method according to any one of claims 1 to 9, wherein: In the step of obtaining the temporary stacked electrode plate group, the rectangular positive electrode plates and the rectangular negative electrode plates are alternately stacked and then shaken in a direction perpendicular to the stacking direction to assist the temporary positioning.
11. A device for manufacturing a battery electrode plate group, which is a device for manufacturing a battery electrode plate group formed by alternately stacking a plurality of rectangular positive electrode plates and a plurality of rectangular negative electrode plates with a solid electrolyte layer interposed therebetween, comprising: An electrode plate group accommodating frame having an accommodating space for accommodating rectangular positive electrode plates and rectangular negative electrode plates having positioning holes in a state of being alternately stacked with a solid electrolyte layer interposed therebetween, wherein the rectangular positive electrode plates and the rectangular negative electrode plates are accommodated in the accommodating space to form a temporarily stacked electrode plate group in which the rectangular positive electrode plates and the rectangular negative electrode plates are temporarily positioned and the positioning holes are connected to each other; a positioning fixture, which is arranged to be relatively movable toward the front or rear of the stacking direction of the temporary stacked electrode group and has a positioning pin vertically arranged thereon and inserted into the positioning hole; and A limiting component is configured to be relatively movable toward an opposing position of the positioning fixture via the electrode plate group containing frame, and to be relatively movable closer to or farther from the positioning fixture, the limiting component comprising a limiting portion for limiting changes in the stacking direction of an opening side of a connecting hole formed by connecting the positioning holes to each other, and a pin receiving portion provided on the limiting portion and receiving the positioning pin.
12. The manufacturing device according to claim 11, comprising: An electrode plate conveying device, which conveys the rectangular positive electrode plate and the rectangular negative electrode plate alternately into the accommodation space via a solid electrolyte layer; and A frame conveying device conveys the electrode plate group accommodating frame to between the positioning fixture and the limiting component.
13. The manufacturing device according to claim 11 or 12, wherein: The positioning pin includes a pin body portion having a diameter smaller than an inner diameter of the positioning hole, and a tip portion extending from one end of the pin body portion.
14. The manufacturing device according to any one of claims 11 to 13, wherein: At least one of the rectangular positive electrode plate and the rectangular negative electrode plate housed in the electrode plate group housing frame has a solid electrolyte layer on both main surfaces of its active material layer.
15. The manufacturing device according to any one of claims 11 to 14, comprising: A correction member corrects the stacked rectangular positive electrode plates and the rectangular negative electrode plates to be flat.
16. The manufacturing device according to any one of claims 11 to 15, wherein: The rectangular positive electrode plate and / or the rectangular negative electrode plate accommodated in the electrode plate group accommodating frame has a base extension portion having a positioning hole on at least one side of the short side of the active material layer.
17. The manufacturing device according to claim 16, wherein: The rectangular positive electrode plate and / or the rectangular negative electrode plate accommodated in the electrode plate group accommodating frame has two or more base material extension portions.
18. The manufacturing device according to claim 16 or 17, wherein: The substrate extension portion is extended to both sides of the short side of the active material layer.
19. The manufacturing device according to any one of claims 11 to 18, comprising: A shaking device shakes the electrode plate group housing frame in a direction perpendicular to the stacking direction of the rectangular positive electrode plates and the rectangular negative electrode plates.