Log board anti-deformation treatment device and treatment method thereof
By combining the moisture content sensor, heating assembly and extrusion vibration assembly in the log sheet treatment device, the problems of plate deformation and uneven water vapor are solved, uniform heating and stress release of the plate are achieved, and treatment efficiency and quality are improved.
Patent Information
- Application Number
- CN202411657858.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-11-20
- Publication Date
- 2024-12-17
- Estimated Expiration
- 2044-11-20
AI Technical Summary
During the processing process, log sheets are prone to deformation due to stress changes, which are difficult to effectively solve in traditional treatment methods, and the deformation problem caused by uneven water vapor during heating still exists.
A device including a treatment box, heating assembly, extrusion vibration assembly and pretreatment assembly is designed. The moisture content of the plate is detected through a moisture content sensor, the power of the heating plate is controlled, and the internal stress of the wood is released by the extrusion vibration assembly, and the air pump is pumped out. Water vapor and jet plate preheat and wet the sheet to ensure uniform heating and stress release.
The partition heating and stress adjustment of the plate are realized, which effectively prevents deformation, improves the processing efficiency and quality, and ensures that the plates of different thicknesses can be effectively processed.
Smart Images

Figure CN119141655A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of log board anti-deformation, and in particular to a log board anti-deformation processing device and a processing method thereof. Background Art
[0002] In the wood processing industry, the deformation problem of log boards has always been a key problem that has troubled producers. Log boards are very likely to deform during processing or use due to the influence of various factors. This not only affects the appearance quality of the boards, but more seriously reduces their performance and brings economic losses to related industries.
[0003] Wood itself is a natural material with a complex stress structure. After logging, the moisture distribution inside the wood is uneven, and during the processing, operations such as cutting and drying will further change the stress balance inside the wood. When the stress exceeds the bearing capacity of the wood fiber, the board will deform. Traditional treatment methods are often unable to effectively solve this problem, or the treatment process is not perfect, resulting in deformation problems still occurring frequently.
[0004] In addition, the moisture content of wood has a crucial impact on its stability. If the moisture content cannot be accurately controlled during the processing, or targeted treatment cannot be carried out according to the moisture content of different parts of the board, it is easy to cause the local moisture content to be too high or too low, which in turn causes deformation. Moreover, in treatment processes such as heating, simple heating alone is often unable to fully release the internal stress of the wood, and may also cause new stress problems due to local uneven heating. At the same time, excessive water vapor generated during the heating process or failure to be discharged in time may cause deformation of the wood. In local areas, excessive water vapor accumulation may cause the wood fibers to expand excessively, exceeding their elastic limit. When the water vapor cools or escapes, the wood will leave permanent deformation.
[0005] To this end, the present invention provides a log board anti-deformation processing device and a processing method thereof to solve the above-mentioned problem. Summary of the invention
[0006] In view of the deficiencies in the prior art, the present invention provides a log board anti-deformation processing device and a processing method thereof, which solve the above-mentioned problems.
[0007] To achieve the above objectives, the present invention is implemented through the following technical solutions: a device for anti-deformation processing of log boards, comprising a processing box, a first conveyor belt and a second conveyor belt, automatic sealing doors are provided on both sides of the processing box, an extrusion vibration component is provided inside the processing box, a pretreatment component is provided on the top of the first conveyor belt, a heating component is provided between the processing box and the first conveyor belt, the heating component comprises a bracket, the bracket is fixedly installed on the top of the first conveyor belt, a moisture content sensor is fixedly installed on the bottom of the bracket, a third conveyor belt is fixedly installed on the inner bottom of the processing box, a pressing plate is provided above the third conveyor belt, a heating plate is fixedly installed on the bottom of the pressing plate, a controller is fixedly installed on the top of the processing box, the controller is electrically connected to the heating plate, and the controller is electrically connected to the moisture content sensor.
[0008] Preferably: the pretreatment component includes a jet plate, support plates are fixedly installed on both sides of the jet plate, a rotary joint is fixedly installed inside the support plate, a roller is fixedly installed between the two rotary joints, the outer section of the rotary joint is fixedly installed inside the support plate, the inner section of the rotary joint is located on the inner side of the support plate, the roller is hollow, and the roller is connected to the rotary joint.
[0009] Preferably: a second connecting pipe is fixedly installed between the rotary joint and the jet plate, the second connecting pipe is connected to the rotary joint, the second connecting pipe is connected to the inside of the jet plate, a spray hole is opened at the bottom of the jet plate, and the second connecting pipe is connected to the spray hole.
[0010] Preferably: an air pump is fixedly installed on the top of the processing box, a first connecting pipe is fixedly installed between the outlet of the air pump and the rotary joint, the first connecting pipe is connected to the inside of the rotary joint, and the inlet of the air pump is connected to the inside of the processing box.
[0011] Preferably: side blocks are fixedly installed on both sides of the first conveyor belt, a side frame is fixedly installed on the top of the side block, a slider is slidably connected inside the side frame, and the slider is fixedly installed on the front and rear sides of the jet plate.
[0012] Preferably, a slide bar is fixedly installed inside the side frame, the slide bar movably passes through the inside of the slider, a first spring is fixedly installed between the bottom of the slider and the top of the side block, and the first spring is sleeved on the outside of the slide bar.
[0013] Preferably: a cooling mechanism is fixedly installed on the top of the second conveyor belt, and the cooling mechanism consists of an internal cooling fan and an external shell.
[0014] Preferably: the extrusion vibration assembly includes a vibration plate, second springs are fixedly installed at the four corners of the bottom of the vibration plate, the second spring is fixedly installed on the top of the pressure plate, a first motor is fixedly installed on the top of the pressure plate, and a cam is fixedly installed on the output end of the first motor.
[0015] Preferably: a second motor is fixedly installed on the inner bottom of the processing box, a screw is rotatably connected between the output end of the second motor and the side wall of the processing box, the screw is rotatably connected to the processing box, the screw is fixedly connected to the output end of the second motor, a moving block is threaded on the outer side of the screw, the moving block is slidably connected to the inner bottom of the processing box, and a connecting rod is hinged between the moving block and the pressure plate.
[0016] The processing method of the log board anti-deformation processing device comprises the following steps: Step 1: convey the plate into the processing box through the first conveyor belt and the third conveyor belt, detect the moisture content of the plate through the moisture content sensor, and control multiple heating plates to enable different powers; Step 2: By placing the pressing plate and the heating plate close to the wooden board, the wooden board is heated and squeezed, thereby eliminating the stress inside the board and preventing the board from deforming.
[0017] Step 3: The high-temperature water vapor generated by heating is extracted through a vacuum pump and passed into the roller and the jet plate. The stress elimination effect is further improved by preheating the plate and moistening the surface. Beneficial Effects
[0018] The present invention provides a log board anti-deformation processing device and a processing method thereof. Compared with the prior art, it has the following beneficial effects: 1. The anti-deformation treatment device and treatment method for log boards use moisture sensors to continuously detect the moisture content of various parts of the board. The controller accurately adjusts the power of the heating plate according to the detection results to achieve zoned heating. This method can avoid insufficient or excessive heating of certain parts of the board, making the internal fibers of the wood more flexible under moderate heating, which is conducive to stress adjustment, thereby effectively preventing deformation of the board due to stress problems.
[0019] 2. The device and method for preventing deformation of log boards work by squeezing the vibration component during the heating process. The first motor drives the cam to rotate and generate vibration. The cam hits the vibration plate and cooperates with the second spring to greatly increase the vibration of the pressure plate. Vibration is applied to the board during heating, so that the internal stress of the board is partially released, preventing the board from being deformed due to local stress concentration.
[0020] 3. The anti-deformation treatment device and treatment method of the log board, the pretreatment component uses an exhaust pump to extract the water vapor generated by heating, so that it enters the drum and the jet plate in sequence through the first connecting pipe and the rotary joint. On the one hand, the water vapor can heat the drum, and on the other hand, the jet plate can preheat and pre-moisten the surface of the next board to be processed. This method can not only utilize the waste water vapor resources, but also balance the moisture content inside and outside the wood, further ensure stress release, and improve the processing efficiency and quality. The drum can automatically adjust its position according to the thickness of the board to ensure that boards of different thicknesses can be effectively processed. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] In order to more clearly illustrate the embodiments of the present invention or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the present invention. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.
[0022] Figure 1 It is a three-dimensional diagram of the external structure of the present invention; Figure 2 It is a side structural stereogram of the present invention; Figure 3 is a three-dimensional diagram of the structure of the pretreatment component of the present invention; Figure 4 It is a stereoscopic diagram of the overall structure of the pretreatment component of the present invention; Figure 5 The present invention Figure 4 A magnified view of the structure at center; Figure 6 It is a three-dimensional diagram of the internal structure of the processing box of the present invention; Figure 7 It is a three-dimensional diagram of the top structure inside the processing box of the present invention.
[0023] In the figure: 1. treatment box; 2. pretreatment component; 21. vacuum pump; 22. first connecting pipe; 23. side block; 24. side frame; 25. jet plate; 26. roller; 27. second connecting pipe; 28. support plate; 29. rotary joint; 210. first spring; 211. slider; 212. slide bar; 3. heating component; 31. bracket; 32. moisture sensor; 33. controller; 34. pressure plate; 35. heating plate; 4. extrusion vibration component; 41. connecting rod; 42. vibration plate; 43. second spring; 44. first motor; 45. cam; 46. moving block; 47. screw; 48. second motor; 5. automatic sealing door; 6. first conveyor belt; 7. second conveyor belt; 8. cooling mechanism; 9. third conveyor belt. DETAILED DESCRIPTION
[0024] It should be noted that in the description of the embodiments of the present application, the terms "front, rear", "left, right", "up, down", etc. indicating directions or positional relationships are based on the directions or positional relationships shown in the accompanying drawings, and are only for the convenience of describing the present application and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific direction, be constructed and operated in a specific direction, and therefore cannot be understood as a limitation on the present application. The terms "install", "connect", and "connected" should be understood in a broad sense, for example, it can be a fixed connection, a detachable connection, or an integral connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be a connection between the two elements. For those of ordinary skill in the art, the specific meanings of the above terms in the present application can be understood according to specific circumstances.
[0025] The present application is further described in detail below through drawings and examples.
[0026] Reference Figures 1 to 7 The embodiment of the present application provides an anti-deformation processing device for log boards, including a processing box 1, a first conveyor belt 6 and a second conveyor belt 7. Automatic sealing doors 5 are provided on both sides of the processing box 1. An extrusion vibration component 4 is provided inside the processing box 1. A pretreatment component 2 is provided on the top of the first conveyor belt 6. A heating component 3 is provided between the processing box 1 and the first conveyor belt 6. The heating component 3 includes a bracket 31. The bracket 31 is fixedly installed on the top of the first conveyor belt 6. A moisture content sensor 32 is fixedly installed on the bottom of the bracket 31. A third conveyor belt 9 is fixedly installed on the inner bottom of the processing box 1. A pressing plate 34 is provided above the third conveyor belt 9. A heating plate 35 is fixedly installed on the bottom of the pressing plate 34. A controller 33 is fixedly installed on the top of the processing box 1. The controller 33 is electrically connected to the heating plate 35, and the controller 33 is electrically connected to the moisture content sensor 32. A second motor 48 is fixedly installed on the inner bottom of the processing box 1, and a screw 47 is rotatably connected between the output end of the second motor 48 and the side wall of the processing box 1. The screw 47 is rotatably connected to the processing box 1, and the screw 47 is fixedly connected to the output end of the second motor 48. A moving block 46 is screwed on the outer side of the screw 47, and the moving block 46 is slidably connected to the inner bottom of the processing box 1. A connecting rod 41 is hinged between the moving block 46 and the pressure plate 34.
[0027] In this embodiment, when the stress of the plate is eliminated, the plate is transported by the first conveyor belt 6, and the plate is transported to the inside of the processing box 1 in cooperation with the third conveyor belt 9. When the plate is transported, the moisture content inside the plate can be detected by the moisture content sensor 32 above, and the moisture content of each part of the plate can be detected separately by continuously detecting the plate, and when the heating plate 35 is started by the controller 33, the heating power of the heating plate 35 can be adjusted according to the moisture content of different positions of the plate. The heating plate 35 can ensure that some parts will not be insufficiently heated or overheated during heating by zoning the plates at different moisture content positions. After the plate moves to the position, the screw 47 is driven to rotate by starting the second motor 48. The rotation of the screw 47 can drive the moving block 46 thereon to move in the opposite direction synchronously. The synchronous reverse movement of the moving block 46 can cooperate with the connecting rod 41 to realize the downward movement of the pressing plate 34. The downward movement of the pressing plate 34 drives the heating plate 35 to fit above the plate. By squeezing and heating the plate, the plate is moderately heated, making the fibers inside the wood more flexible and convenient for stress adjustment.
[0028] Reference Figures 1 to 7 In one aspect of the present embodiment, the pretreatment assembly 2 includes an air jet plate 25, a support plate 28 is fixedly installed on both sides of the air jet plate 25, a rotary joint 29 is fixedly installed inside the support plate 28, a roller 26 is fixedly installed between the two rotary joints 29, the outer section of the rotary joint 29 is fixedly installed inside the support plate 28, the inner section of the rotary joint 29 is located inside the support plate 28, the roller 26 is hollow, and the roller 26 is connected to the rotary joint 29. A second connecting pipe 27 is fixedly installed between the rotary joint 29 and the air jet plate 25, the second connecting pipe 27 is connected to the rotary joint 29, the second connecting pipe 27 is connected to the inside of the air jet plate 25, a spray hole is opened at the bottom of the air jet plate 25, and the second connecting pipe 27 is connected to the spray hole to the treatment box 1. A vacuum pump 21 is fixedly installed on the top of the treatment box 1, a first connecting pipe 22 is fixedly installed between the outlet of the vacuum pump 21 and the rotary joint 29, the first connecting pipe 22 is connected to the inside of the rotary joint 29, and the inlet of the vacuum pump 21 is connected to the inside of the treatment box 1.
[0029] Side blocks 23 are fixedly installed on both sides of the first conveyor belt 6, and a side frame 24 is fixedly installed on the top of the side block 23. A slider 211 is slidably connected inside the side frame 24, and the slider 211 is fixedly installed on the front and rear sides of the jet plate 25. A slide bar 212 is fixedly installed inside the side frame 24, and the slide bar 212 movably passes through the inside of the slider 211. A first spring 210 is fixedly installed between the bottom of the slider 211 and the top of the side block 23, and the first spring 210 is sleeved on the outside of the slide bar 212.
[0030] The extrusion vibration assembly 4 includes a vibration plate 42, and second springs 43 are fixedly installed at the four corners of the bottom of the vibration plate 42. The second spring 43 is fixedly installed on the top of the pressure plate 34. A first motor 44 is fixedly installed on the top of the pressure plate 34, and a cam 45 is fixedly installed at the output end of the first motor 44.
[0031] In this embodiment, when the plate is heated, the first motor 44 is started, and the first motor 44 drives the cam 45 to rotate, and the rotation of the cam 45 generates vibration, and the cam 45 knocks the upper vibration plate 42 and cooperates with the second spring 43 to greatly increase the vibration generated by the pressing plate 34. In the process of heating the plate, the vibration applied to the plate by the pressing plate 34 is cooperated, so that the internal stress of the wood is partially released, and the plate is prevented from being deformed due to local stress concentration; When heated, more water vapor will be generated, and the generated water vapor will be extracted by the vacuum pump 21. The extracted water vapor will enter the inside of the roller 26 through the first connecting pipe 22 and the rotating joint 29, and heat the roller. The water vapor will then enter the inside of the jet plate 25 through the second connecting pipe 27, and will be ejected through the jet plate 25 to the top of the next plate to be processed above the first conveyor belt 6. When the plate is transported on the first conveyor belt 6, when the plate passes through the roller 26, the roller 26 can be squeezed upward according to the thickness of the wood board, and the jet plate 25 and the slider 211 move up along the side frame 24, and the roller 26 can move along the plate. The top of the wood is rotated, in this way, it is ensured that the roller 26 of plates of different thicknesses can roll thereon, and the jet plate 25 can be attached to the top of the plate, the plate can be preheated by the roller 26 and the jet plate 25, and the gas ejected by the jet plate 25 can pre-wet the surface of the plate to a certain extent. A certain amount of moisture on the surface of the wood can balance the moisture content inside and outside the wood, ensuring that there is no large difference in moisture content when the inside and outside are heated, and further ensuring the release of stress; after the processing is completed, the plate is discharged through the second conveyor belt 7, and the plate is cooled by the cooling mechanism 8.
[0032] This embodiment also discloses a processing method of the log board anti-deformation processing device, comprising the following steps: Step 1: convey the plate to the inside of the processing box 1 through the first conveyor belt 6 and the third conveyor belt 9, detect the moisture content of the plate through the moisture content sensor 32, and control the multiple heating plates 35 to enable different powers; Step 2: The pressing plate 34 and the heating plate 35 are placed close to the wooden board to heat and squeeze the wooden board, thereby eliminating the stress inside the board and preventing the board from deforming; Step 3: The high-temperature water vapor generated by heating is extracted by the vacuum pump 21 and passed into the roller 26 and the jet plate 25. By preheating the plate and wetting the surface, the stress elimination effect is further improved.
[0033] Meanwhile, the contents not described in detail in this specification belong to the prior art known to those skilled in the art.
[0034] Working principle: When the plate is undergoing stress elimination, the plate is transported by the first conveyor belt 6. When the plate is transported, the third conveyor belt 9 is used to transport the plate to the inside of the processing box 1. When the plate is transported, the moisture content inside the plate can be detected by the moisture content sensor 32 above, and the moisture content of each part of the plate can be detected separately by continuously detecting the plate. When the heating plate 35 is started by the controller 33, the heating power of the heating plate 35 can be adjusted according to the moisture content of different positions of the plate. The heating plate 35 can heat the plates at different moisture content positions in different zones to ensure that some parts are not heated insufficiently or overheated during heating. After the plate moves to the position, the second motor 48 is started to drive the screw 47 to rotate, and the rotation of the screw 47 can drive The moving block 46 on it moves synchronously in the opposite direction. The synchronous opposite movement of the moving block 46 can cooperate with the connecting rod 41 to realize the downward movement of the pressing plate 34. The downward movement of the pressing plate 34 drives the heating plate 35 to fit above the plate. By squeezing and heating the plate, the plate is moderately heated to make the fibers inside the wood more flexible and easy to adjust the stress. When the plate is heated, the first motor 44 is started, and the first motor 44 drives the cam 45 to rotate. The rotation of the cam 45 generates vibration, and the cam 45 knocks the upper vibration plate 42 and cooperates with the second spring 43 to greatly increase the vibration generated by the pressing plate 34. In the process of heating the plate, the vibration applied to the plate by the pressing plate 34 is cooperated to partially release the stress inside the wood, so as to prevent the plate from being deformed due to local stress concentration. When heated, more water vapor will be generated, and the generated water vapor will be extracted by the vacuum pump 21. The extracted water vapor will enter the inside of the roller 26 through the first connecting pipe 22 and the rotating joint 29, and heat the roller. The water vapor will then enter the inside of the jet plate 25 through the second connecting pipe 27, and will be ejected through the jet plate 25 to the top of the next plate to be processed above the first conveyor belt 6. When the plate is transported on the first conveyor belt 6, when the plate passes through the roller 26, the roller 26 can be squeezed upward according to the thickness of the wood board, and the jet plate 25 and the slider 211 move up along the side frame 24, and the roller 26 can move along the plate. The top of the wood is rotated, in this way, it is ensured that the roller 26 of plates of different thicknesses can roll thereon, and the jet plate 25 can be attached to the top of the plate, the plate can be preheated by the roller 26 and the jet plate 25, and the gas ejected by the jet plate 25 can pre-wet the surface of the plate to a certain extent. A certain amount of moisture on the surface of the wood can balance the moisture content inside and outside the wood, ensuring that there is no large difference in moisture content when the inside and outside are heated, and further ensuring the release of stress; after the processing is completed, the plate is discharged through the second conveyor belt 7, and the plate is cooled by the cooling mechanism 8.
[0035] It should be noted that, in this article, relational terms such as first and second, etc. are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device.
[0036] Although the embodiments of the present application have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present application, and that the scope of the present application is defined by the appended claims and their equivalents.
Claims
1. A log board anti-deformation processing device, comprising a processing box (1), a first conveyor belt (6) and a second conveyor belt (7), characterized in that: Automatic sealing doors (5) are provided on both sides of the processing box (1), an extrusion vibration component (4) is provided inside the processing box (1), a pre-processing component (2) is provided on the top of the first conveyor belt (6), a heating component (3) is provided between the processing box (1) and the first conveyor belt (6), the heating component (3) comprises a bracket (31), the bracket (31) is fixedly mounted on the top of the first conveyor belt (6), a moisture content sensor (32) is fixedly mounted on the bottom of the bracket (31), a third conveyor belt (9) is fixedly mounted on the inner bottom of the processing box (1), a pressing plate (34) is provided above the third conveyor belt (9), a heating plate (35) is fixedly mounted on the bottom of the pressing plate (34), and the processing box (1) is provided with a plurality of pre-processing components (2) on the top of the first conveyor belt (6). A controller (33) is fixedly mounted on the top of the sorting box (1), the controller (33) being electrically connected to the heating plate (35), and the controller (33) being electrically connected to the moisture content sensor (32). The pretreatment component (2) comprises an air jet plate (25), support plates (28) being fixedly mounted on both sides of the air jet plate (25), a rotary joint (29) being fixedly mounted inside the support plate (28), a roller (26) being fixedly mounted between the two rotary joints (29), an outer section of the rotary joint (29) being fixedly mounted inside the support plate (28), an inner section of the rotary joint (29) being located inside the support plate (28), the roller (26) being hollow, and the roller (26) being connected to the rotary joint (29).
2. The device for preventing deformation of log board according to claim 1, characterized in that: A second connecting pipe (27) is fixedly installed between the rotating joint (29) and the jet plate (25); the second connecting pipe (27) is in communication with the rotating joint (29); the second connecting pipe (27) is in communication with the interior of the jet plate (25); a jet hole is provided at the bottom of the jet plate (25); the second connecting pipe (27) is in communication with the jet hole.
3. The device for preventing deformation of log board according to claim 1, characterized in that: An air extraction pump (21) is fixedly installed on the top of the processing box (1), and a first connecting pipe (22) is fixedly installed between the outlet of the air extraction pump (21) and the rotary joint (29), the first connecting pipe (22) is connected to the inside of the rotary joint (29), and the inlet of the air extraction pump (21) is connected to the inside of the processing box (1).
4. The device for preventing deformation of log board according to claim 1, characterized in that: Side blocks (23) are fixedly mounted on both sides of the first conveyor belt (6), a side frame (24) is fixedly mounted on the top of the side block (23), a slider (211) is slidably connected inside the side frame (24), and the slider (211) is fixedly mounted on the front and rear sides of the jet plate (25).
5. The device for preventing deformation of log board according to claim 4, characterized in that: A sliding rod (212) is fixedly installed inside the side frame (24), and the sliding rod (212) movably passes through the inside of the slider (211). A first spring (210) is fixedly installed between the bottom of the slider (211) and the top of the side block (23), and the first spring (210) is sleeved on the outside of the sliding rod (212).
6. The device for preventing deformation of log board according to claim 1, characterized in that: A cooling mechanism (8) is fixedly mounted on the top of the second conveyor belt (7), and the cooling mechanism (8) is composed of an internal cooling fan and an external casing.
7. The device for preventing deformation of log board according to claim 1, characterized in that: The extrusion vibration assembly (4) comprises a vibration plate (42), second springs (43) are fixedly mounted at the four corners of the bottom of the vibration plate (42), the second spring (43) is fixedly mounted on the top of the pressure plate (34), a first motor (44) is fixedly mounted on the top of the pressure plate (34), and a cam (45) is fixedly mounted on the output end of the first motor (44).
8. The device for preventing deformation of log board according to claim 1, characterized in that: A second motor (48) is fixedly mounted on the inner bottom of the processing box (1); a screw rod (47) is rotatably connected between the output end of the second motor (48) and the side wall of the processing box (1); the screw rod (47) is rotatably connected to the processing box (1); the screw rod (47) is fixedly connected to the output end of the second motor (48); a moving block (46) is screwed on the outer side of the screw rod (47); the moving block (46) is slidably connected to the inner bottom of the processing box (1); and a connecting rod (41) is hinged between the moving block (46) and the pressure plate (34).
9. A method for treating a log board with an anti-deformation treatment device, for using the log board with an anti-deformation treatment device as claimed in any one of claims 1 to 4, characterized in that: The steps include: Step 1: conveying the plate into the processing box (1) via a first conveyor belt (6) and a third conveyor belt (9), detecting the moisture content of the plate via a moisture content sensor (32), and controlling a plurality of heating plates (35) to enable different powers; Step 2: by placing the pressing plate (34) and the heating plate (35) in close contact with the wooden board, the wooden board is heated and pressed so as to eliminate the stress inside the board, thereby preventing the board from deforming; Step 3: The high-temperature water vapor generated by heating is extracted by the vacuum pump (21) and passed into the roller (26) and the jet plate (25), thereby preheating the plate and moistening the surface, thereby further improving the stress elimination effect.
Citation Information
Patent Citations
Drying device with intelligent temperature control function
CN104534837A
Plate drying device and solid wood plate anti-deformation drying treatment method
CN118816506A
Film laminating device for bottom mat in household appliance industry
CN213798105U
Bamboo furniture board stress quick release treatment device
CN214925278U
Automatic humidity adjusting device of diaphragm coating machine and coating machine
CN221832676U
Cited By
Heat sealing device for inflatable paddle board production
CN120588503A
A hot sealing device for inflatable paddleboard production
CN120588503B