High-temperature-resistant and extrusion-resistant new energy battery sealing ring forming die and forming method

By designing a new energy battery sealing ring molding mold that is resistant to high temperature and extrusion, using servo motors and automated mechanical structures, the problem of low efficiency in the molding process of new energy battery sealing ring is solved, and rapid mold release and unloading are achieved, which improves the Forming efficiency and safety.

CN119319642APending Publication Date: 2025-01-17SUZHOU ORANGE ELECTRONIC PRECISION CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411784964.X
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-06
Publication Date
2025-01-17

AI Technical Summary

Technical Problem

New energy battery sealing rings are inefficient during processing, mold release and unloading require manual assistance, and the molding efficiency is not high, making safety and efficiency difficult to ensure.

Method used

Design high-temperature and extrusion-resistant new energy battery sealing ring molding mold, including lower mold and upper mold, drive the screw to rotate through a servo motor, combine contact blocks, deduplication components and guide rods to achieve automatic mold release and unloading, and improve molding efficiency.

Benefits of technology

It realizes rapid mold release and unloading of new energy battery sealing rings, improves overall working efficiency, simplifies the molding process, and ensures safety and efficiency.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119319642A_ABST
    Figure CN119319642A_ABST
Patent Text Reader

Abstract

The invention discloses a high-temperature-resistant and extrusion-resistant new energy battery sealing ring forming die and method, and relates to the field of battery sealing ring forming die, the high-temperature-resistant and extrusion-resistant new energy battery sealing ring forming die comprises a lower die, a die groove is formed in the center of the top of the lower die, and a first stripping assembly is movably connected into an inner cavity of the die groove; contact blocks are symmetrically and movably connected to the periphery of the top of the lower mold, injection molding openings are symmetrically formed in the two ends of the top of the upper mold, movable grooves are symmetrically formed in the two ends of the top of the lower mold, a second stripping assembly is installed on the left side of the lower mold, and a stripping rod is movably connected into an inner cavity of the upper mold; the two ends of the loading column are symmetrically and movably connected with supporting assemblies. According to the high-temperature-resistant and extrusion-resistant new energy battery sealing ring forming mold and the forming method, the mold can effectively improve the mold manufacturing efficiency through the two injection molding openings, a finished product can be rapidly discharged, and follow-up machining of the finished product is facilitated.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the field of battery sealing ring forming dies, and in particular to a high-temperature resistant and extrusion resistant new energy battery sealing ring forming die and a forming method. Background Art

[0002] A sealing ring is a device used to prevent liquid or gas leakage. It is usually made of elastic material and has a sealing function. The choice of material is of great significance to its sealing performance and service life. The performance of the material directly affects the performance of the sealing ring.

[0003] The sealing rings used in new energy batteries have low processing efficiency, and demoulding and unloading mostly require manual assistance. The efficiency is low and the safety cannot be guaranteed. In addition, manual stacking is required after unloading, which will further reduce the efficiency of the molding.

[0004] Therefore, it is necessary to propose a high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and forming method to solve the above problems. Summary of the invention

[0005] The main purpose of the present invention is to provide a high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and forming method, which can effectively solve the problems in the background technology.

[0006] To achieve the above object, the technical solution adopted by the present invention is: A high temperature resistant and extrusion resistant new energy battery sealing ring forming mold comprises a lower mold, a mold groove is opened in the middle of the top of the lower mold, a first stripping component is movably connected in the inner cavity of the mold groove, and contact blocks are symmetrically and movably connected around the top of the lower mold; The top of the lower mold is movably connected to the upper mold, injection ports are symmetrically provided at both ends of the top of the upper mold, movable grooves are symmetrically provided at both ends of the top of the lower mold, guide grooves are symmetrically provided at both ends of the lower mold, a second stripping assembly is installed on the left side of the lower mold, and a stripping rod is movably connected in the inner cavity of the upper mold; A material receiving box is installed on the right side of the lower mold, and a loading column is installed at the bottom of the inner cavity of the material receiving box. The two ends of the loading column are symmetrically and movably connected with support components, and the two ends of the top of the loading column are symmetrically and movably connected with operating handles, and the outer wall of the operating handle is provided with a C-shaped frame.

[0007] Preferably, connecting frames are symmetrically installed at the bottom of both ends of the first stripping component, fixed columns are symmetrically installed at both ends of the top of the connecting frame, limiting blocks are installed on the top of the fixed columns, and the outer wall of the fixed column is wrapped with a first spring.

[0008] Preferably, the bottom of the first spring is installed on the top of the connecting frame, the top of the first spring is installed on the bottom of the contact block, the limit block is movably connected in the inner cavity of the contact block, the contact block is sleeved on the outer wall of the fixed column, the left side of the contact block is inclined, and the top of the contact block is attached to the bottom of the upper mold.

[0009] Preferably, a first guide rod is installed in the inner cavity of the movable groove at one end, and a screw is rotatably connected in the inner cavity of the movable groove at the other end. A servo motor is installed on the right side of the lower mold, and the servo motor is installed on the right side of the screw through a first rotating shaft. Both ends of the bottom of the upper mold are movably connected in the inner cavities of the two movable grooves, the right side of one end of the bottom of the upper mold is threadedly connected to the outer wall of the screw, and the right side of the other end of the bottom of the upper mold is sleeved on the outer wall of the first guide rod.

[0010] Preferably, second guide rods are symmetrically installed in the inner cavities of the two guide grooves, and connecting rods are symmetrically installed on the right sides of both ends of the upper mold. The bottom of the connecting rod is movably connected in the inner cavity of the guide groove and sleeved on the outer wall of the second guide rod.

[0011] Preferably, the second stripping component is "C"-shaped, and an adaptation groove is provided on the left side of the upper mold. The adaptation groove and the second stripping component are adapted to each other in size. The top of the second stripping component is movably connected in the inner cavity of the adaptation groove, and reset blocks are symmetrically installed on the left sides of both ends of the stripping rod.

[0012] Preferably, reset grooves are symmetrically provided at both ends of the inner cavity of the adapter groove, a reset spring is installed in the inner cavity of the reset groove, one side of the reset spring is installed in the inner cavity of the reset groove, and the other side of the reset spring is installed on the side of the reset block, and the reset block is movably connected in the inner cavity of the reset groove.

[0013] Preferably, a through slot is opened in the middle of the top of the loading column, movable columns are symmetrically installed on the bottom of the two supporting components on opposite sides, connecting columns are symmetrically installed on the top of the two movable columns on opposite sides, the connecting columns are movably connected in the inner cavity of the through slot, and the operating handle is installed on the top of the connecting columns.

[0014] Preferably, a fixing rod is installed in the inner cavity of the through slot, and second springs are symmetrically wound around both ends of the outer wall of the fixing rod, one end of the second spring is installed in the inner cavity of the through slot, and the other end of the second spring is installed on the outer wall of the connecting column, and the left side of the C-shaped frame is rotatably connected to the top of the loading column.

[0015] A high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and a forming method, using the above-mentioned high temperature resistant and extrusion resistant new energy battery sealing ring forming mold, includes the following operating steps: S1: Inject the raw material for injection molding into the inner cavity of the mold groove through the injection port. After the injection molding is completed, start the servo motor to drive the screw to rotate so that the bottom of the upper mold can be connected with the screw thread. At this time, the upper mold can move to the left; S2: When the upper mold is separated from the top of the lower mold, the first spring can shrink the contact block toward the top, so that the first spring can drive the first stripping assembly to move toward the top of the inner cavity of the mold groove through the connecting frame. At this time, the new energy battery sealing ring after molding can be demolded from the mold groove; S3: The new energy battery sealing ring after demoulding is placed on the top of the first stripping component. After the upper mold continues to move to the left, it will be sleeved on the outer wall of the top of the second stripping component through the adapter groove. When the second stripping component contacts the stripping rod, the stripping rod will move to the right. At this time, the new energy battery sealing ring can be pushed into the inner cavity of the receiving box. At this time, the new energy battery sealing ring will be sleeved on the outer wall of the loading column; S4: Reset the upper mold. After the upper mold contacts the contact block, it will be moved to the bottom of the lower mold cavity. At the same time, the stripper rod will be separated from the second stripper assembly, so that the reset spring can reset the stripper rod through the reset block. When the upper mold is completely located on the top of the lower mold, the molding work of the new energy battery sealing ring can continue; S5: Flip the C-shaped frame to the left. At this time, the second spring will move the movable column outward through the connecting column, so that the movable column can drive the support assembly to separate from the inner cavity of the loading column. At this time, the two support assemblies can fit in the inner circle of the finished new energy battery sealing ring. After removing the loading column, the position of the finished new energy battery sealing ring can be transferred.

[0016] Compared with the prior art, the present invention provides a high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and forming method, which has the following beneficial effects: The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and forming method, through the contact block set, will be squeezed by the upper mold in normal state, so as to drive the first stripping component to be located at the bottom of the inner cavity of the mold groove through the connecting frame. When the upper mold is separated from the top of the lower mold, the first stripping component can be lifted up by the set first spring, so that the finished new energy battery sealing ring located in the inner cavity of the mold groove can be demolded. After the molding of the new energy battery sealing ring is completed, this structure can quickly demold it, which can effectively improve the overall work efficiency, and the structure is simple and fast. The left side of the contact block is inclined, and it can also be squeezed into the inner cavity of the lower mold after the upper mold is reset.

[0017] The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and forming method start the set servo motor to drive the screw to rotate, so that the bottom of the upper mold can be threadedly connected with the screw. At this time, the upper mold can be moved left and right. When it is located at the top of the lower mold, the molding work can be carried out through the opened injection port. After it is separated from the lower mold, the new energy battery sealing ring can be demolded and unloaded. The first guide rod, the guide groove and the second guide rod are set to ensure the stability of the movement of the lower mold.

[0018] The high-temperature and extrusion-resistant new energy battery sealing ring forming mold and forming method, after the upper mold moves to the left, it will be mounted on the outer wall of the second stripping component through an adapter groove. When the second stripping component contacts the stripping rod, it will push the stripping rod to the right, so that the stripping rod can push the new energy battery sealing ring and allow it to fall into the inner cavity of the receiving box, thereby facilitating the unloading of the new energy battery sealing ring. When the upper mold is reset, the reset spring can be used to drive the stripping rod to reset through the reset block.

[0019] The high temperature and extrusion resistant new energy battery sealing ring forming mold and forming method, through the set C-shaped frame, can limit the support component through the operating handle in normal state, after the C-shaped frame is rotated to the left, the support component can be bounced outward by the set second spring, so that the new energy battery sealing ring set on the outer wall of the loading column can be positioned, so as to facilitate its subsequent position transfer. BRIEF DESCRIPTION OF THE DRAWINGS

[0020] Figure 1 It is a schematic diagram of the overall structure of the present invention; Figure 2 It is a structural schematic diagram of the lower mold of the present invention; Figure 3 It is a schematic structural diagram of the first stripping assembly of the present invention; Figure 4 It is a structural schematic diagram of the upper mold of the present invention; Figure 5 It is a schematic structural diagram of a loading column of the present invention; Figure 6 It is a structural schematic diagram of the support assembly of the present invention.

[0021] In the figure: 1. lower mold; 2. upper mold; 3. injection port; 4. movable groove; 5. screw; 6. servo motor; 7. first guide rod; 8. guide groove; 9. second guide rod; 10. connecting rod; 11. mold groove; 12. first stripping assembly; 13. contact block; 14. connecting frame; 15. fixed column; 16. limit block; 17. first spring; 18. second stripping assembly; 19. adapter groove; 20. reset spring; 21. stripping rod; 22. reset block; 23. material receiving box; 24. loading column; 25. support assembly; 26. through groove; 27. operating handle; 28. C-shaped frame; 29. ​​movable column; 30. connecting column; 31. fixed rod; 32. second spring. DETAILED DESCRIPTION

[0022] In order to make the technical means, creative features, objectives and effects achieved by the present invention easy to understand, the present invention is further explained below in conjunction with specific implementation methods. Example

[0023] like Figure 1-Figure 3 As shown, a high temperature resistant and extrusion resistant new energy battery sealing ring forming mold comprises a lower mold 1, a mold groove 11 is opened in the middle of the top of the lower mold 1, a first stripping component 12 is movably connected in the inner cavity of the mold groove 11, and a contact block 13 is symmetrically and movably connected around the top of the lower mold 1, and a connecting frame 14 is symmetrically installed at the bottom of both ends of the first stripping component 12, and a fixed column 15 is symmetrically installed at both ends of the top of the connecting frame 14. A limiting block 16 is installed on the top of the fixed column 15, and a first spring 17 is wound around the outer wall of the fixed column 15. The bottom of the first spring 17 is installed on the top of the connecting frame 14, and the top of the first spring 17 is installed on the bottom of the contact block 13. The limiting block 16 is movably connected in the inner cavity of the contact block 13, and the contact block 13 is sleeved on the outer wall of the fixed column 15. The left side of the contact block 13 is inclined, and the top of the contact block 13 fits the bottom of the upper mold 2; The contact block 13 is arranged, which will be squeezed by the upper mold 2 in normal state, so that the first stripping component 12 is driven to be located at the bottom of the inner cavity of the mold groove 11 through the connecting frame 14. When the upper mold 2 is separated from the top of the lower mold 1, the first stripping component 12 can be lifted up by the arranged first spring 17, so that the finished new energy battery sealing ring located in the inner cavity of the mold groove 11 can be demolded. After the molding of the new energy battery sealing ring is completed, this structure can quickly demold it, which can effectively improve the overall work efficiency, and the structure is simple and fast. The left side of the contact block 13 is inclined, and it can also be squeezed into the inner cavity of the lower mold 1 after the upper mold 2 is reset. Example

[0024] like Figure 1 , Figure 2 , Figure 4As shown, a high temperature and extrusion resistant new energy battery sealing ring forming mold, the top of the lower mold 1 is movably connected to the upper mold 2, the two ends of the top of the upper mold 2 are symmetrically provided with injection ports 3, the two ends of the top of the lower mold 1 are symmetrically provided with movable grooves 4, the two ends of the lower mold 1 are symmetrically provided with guide grooves 8, and a second stripping component 18 is installed on the left side of the lower mold 1, and a stripping rod 21 is movably connected to the inner cavity of the upper mold 2, a first guide rod 7 is installed in the inner cavity of the movable groove 4 at one end, and a screw rod 5 is rotatably connected to the inner cavity of the movable groove 4 at the other end, a servo motor 6 is installed on the right side of the lower mold 1, and the servo motor 6 is installed on the right side of the screw rod 5 through the first rotating shaft, both ends of the bottom of the upper mold 2 are movably connected in the inner cavities of the two movable grooves 4, the right side of one end of the bottom of the upper mold 2 is threadedly connected to the outer wall of the screw rod 5, and the right side of the other end of the bottom of the upper mold 2 is sleeved on the first guide rod The outer wall of the rod 7, the second guide rod 9 is symmetrically installed in the inner cavity of the two guide grooves 8, the connecting rod 10 is symmetrically installed on the right side of the two ends of the upper mold 2, the bottom of the connecting rod 10 is movably connected in the inner cavity of the guide groove 8 and is sleeved on the outer wall of the second guide rod 9, the second stripping component 18 is "C" shaped, an adaptation groove 19 is opened on the left side of the upper mold 2, the adaptation groove 19 and the second stripping component 18 are adapted in size, the top of the second stripping component 18 is movably connected in the inner cavity of the adaptation groove 19, and reset blocks 22 are symmetrically installed on the left sides of the two ends of the stripping rod 21, and reset grooves are symmetrically opened at both ends of the inner cavity of the adaptation groove 19. A reset spring 20 is installed in the inner cavity of the reset groove, one side of the reset spring 20 is installed in the inner cavity of the reset groove, and the other side of the reset spring 20 is installed on the side of the reset block 22, and the reset block 22 is movably connected in the inner cavity of the reset groove; By starting the servo motor 6, the screw rod 5 is driven to rotate, so that the bottom of the upper mold 2 can be threadedly connected with the screw rod 5. At this time, the upper mold 2 can be moved left and right. When it is located at the top of the lower mold 1, the molding work can be carried out through the opened injection port 3. When it is separated from the lower mold 1, the new energy battery sealing ring can be demolded and unloaded. The first guide rod 7, the guide groove 8 and the second guide rod 9 can ensure the stability of the movement of the lower mold 1. After the upper mold 2 moves to the left, it will be sleeved on the outer wall of the second stripping component 18 through the adapter groove 19. When the second stripping component 18 contacts the stripping rod 21, the stripping rod 21 will be pushed to the right, so that the stripping rod 21 can push the new energy battery sealing ring so that it can fall into the inner cavity of the receiving box 23, thereby facilitating the unloading of the new energy battery sealing ring. When the upper mold 2 is reset, the reset spring 20 can be used to drive the stripping rod 21 to reset through the reset block 22. Example

[0025] like Figure 1 , Figure 5 , Figure 6As shown, a high temperature and extrusion resistant new energy battery sealing ring forming mold, a material receiving box 23 is installed on the right side of the lower mold 1, a loading column 24 is installed at the bottom of the inner cavity of the material receiving box 23, two ends of the loading column 24 are symmetrically and movably connected with support components 25, two ends of the top of the loading column 24 are symmetrically and movably connected with operating handles 27, the outer wall of the operating handle 27 is sleeved with a C-shaped frame 28, a through slot 26 is opened in the middle of the top of the loading column 24, and movable columns 29 are symmetrically installed at the bottom of the opposite side of the two support components 25, and connecting columns 30 are symmetrically installed on the opposite side of the top of the two movable columns 29. The connecting column 30 is movably connected in the inner cavity of the through slot 26, the operating handle 27 is installed on the top of the connecting column 30, and a fixing rod 31 is installed in the inner cavity of the through slot 26. The two ends of the outer wall of the fixing rod 31 are symmetrically wound with second springs 32, one end of the second spring 32 is installed in the inner cavity of the through slot 26, and the other end of the second spring 32 is installed on the outer wall of the connecting column 30, and the left side of the C-shaped frame 28 is rotatably connected to the top of the loading column 24; By means of the C-shaped frame 28, the support assembly 25 can be limited by the operating handle 27 in normal state. After the C-shaped frame 28 is rotated to the left, the support assembly 25 can be bounced outward by the second spring 32, so that the new energy battery sealing ring arranged on the outer wall of the loading column 24 can be positioned, so as to facilitate its subsequent position transfer.

[0026] A high temperature resistant and extrusion resistant new energy battery sealing ring forming mold and a forming method, using the above-mentioned high temperature resistant and extrusion resistant new energy battery sealing ring forming mold, includes the following operating steps: S1: Inject the raw material for injection molding into the inner cavity of the mold groove 11 through the injection port 3. After the injection molding is completed, start the servo motor 6 to drive the screw rod 5 to rotate, so that the bottom of the upper mold 2 can be threadedly connected with the screw rod 5, and the upper mold 2 can move to the left; S2: When the upper mold 2 is separated from the top of the lower mold 1, the first spring 17 can shrink the contact block 13 toward the top, so that the first spring 17 can drive the first stripping assembly 12 to move toward the top of the inner cavity of the mold groove 11 through the connecting frame 14. At this time, the new energy battery sealing ring after molding can be demolded from the mold groove 11; S3: The new energy battery sealing ring after demoulding is placed on the top of the first stripping component 12. After the upper mold 2 continues to move to the left, it will be sleeved on the outer wall of the top of the second stripping component 18 through the adapter groove 19. When the second stripping component 18 contacts the stripping rod 21, the stripping rod 21 will move to the right. At this time, the new energy battery sealing ring can be pushed into the inner cavity of the receiving box 23. At this time, the new energy battery sealing ring will be sleeved on the outer wall of the loading column 24; S4: Reset the upper mold 2. After the upper mold 2 contacts the contact block 13, it will be moved to the bottom of the inner cavity of the lower mold 1. At the same time, the stripping rod 21 will be separated from the second stripping assembly 18, so that the reset spring 20 can reset the stripping rod 21 through the reset block 22. When the upper mold 2 is completely located on the top of the lower mold 1, the molding work of the new energy battery sealing ring can continue; S5: Flip the C-shaped frame 28 to the left. At this time, the second spring 32 will move the movable column 29 outward through the connecting column 30, so that the movable column 29 can drive the support assembly 25 to separate from the inner cavity of the loading column 24. At this time, the two support assemblies 25 can be fitted in the inner circle of the finished new energy battery sealing ring. After removing the loading column 24, the position of the finished new energy battery sealing ring can be transferred.

[0027] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. It should be understood by those skilled in the art that the present invention is not limited to the above embodiments. The above embodiments and descriptions are only for explaining the principles of the present invention. Without departing from the spirit and scope of the present invention, the present invention may have various changes and improvements, which fall within the scope of the present invention to be protected. The scope of protection of the present invention is defined by the attached claims and their equivalents.

Claims

1. A high temperature resistant and extrusion resistant new energy battery sealing ring forming die, comprising a lower die (1), characterized in that: A mold groove (11) is provided in the middle of the top of the lower mold (1), a first stripping assembly (12) is movably connected in the inner cavity of the mold groove (11), and contact blocks (13) are symmetrically movably connected around the top of the lower mold (1); The top of the lower mold (1) is movably connected to the upper mold (2), injection ports (3) are symmetrically provided at two ends of the top of the upper mold (2), movable grooves (4) are symmetrically provided at two ends of the top of the lower mold (1), guide grooves (8) are symmetrically provided at two ends of the lower mold (1), a second stripping assembly (18) is installed on the left side of the lower mold (1), and a stripping rod (21) is movably connected in the inner cavity of the upper mold (2); A material receiving box (23) is installed on the right side of the lower mold (1), a loading column (24) is installed at the bottom of the inner cavity of the material receiving box (23), two ends of the loading column (24) are symmetrically and movably connected to support components (25), two ends of the top of the loading column (24) are symmetrically and movably connected to operating handles (27), and the outer wall of the operating handle (27) is sleeved with a C-shaped frame (28).

2. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 1 is characterized in that: Connecting frames (14) are symmetrically mounted at the bottom of both ends of the first stripping assembly (12), fixing columns (15) are symmetrically mounted at both ends of the top of the connecting frame (14), limiting blocks (16) are mounted on the top of the fixing columns (15), and a first spring (17) is wound around the outer wall of the fixing columns (15).

3. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 2 is characterized in that: The bottom of the first spring (17) is mounted on the top of the connecting frame (14), the top of the first spring (17) is mounted on the bottom of the contact block (13), the limit block (16) is movably connected in the inner cavity of the contact block (13), the contact block (13) is sleeved on the outer wall of the fixing column (15), the left side of the contact block (13) is inclined, and the top of the contact block (13) is in contact with the bottom of the upper mold (2).

4. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 1 is characterized in that: A first guide rod (7) is installed in the inner cavity of the movable groove (4) at one end, and a screw rod (5) is rotatably connected in the inner cavity of the movable groove (4) at the other end. A servo motor (6) is installed on the right side of the lower mold (1), and the servo motor (6) is installed on the right side of the screw rod (5) through a first rotating shaft. Both ends of the bottom of the upper mold (2) are movably connected in the inner cavities of the two movable grooves (4). The right side of one end of the bottom of the upper mold (2) is threadedly connected to the outer wall of the screw rod (5), and the right side of the other end of the bottom of the upper mold (2) is sleeved on the outer wall of the first guide rod (7).

5. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 1 is characterized in that: Second guide rods (9) are symmetrically installed in the inner cavities of the two guide grooves (8), and connecting rods (10) are symmetrically installed on the right sides of both ends of the upper mold (2), and the bottom of the connecting rod (10) is movably connected in the inner cavity of the guide groove (8) and sleeved on the outer wall of the second guide rod (9).

6. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 1, characterized in that: The second stripping component (18) is "C"-shaped, and an adapting groove (19) is provided on the left side of the upper mold (2). The adapting groove (19) is adapted to the size of the second stripping component (18). The top of the second stripping component (18) is movably connected in the inner cavity of the adapting groove (19), and reset blocks (22) are symmetrically installed on the left sides of both ends of the stripping rod (21).

7. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 6, characterized in that: Reset grooves are symmetrically provided at both ends of the inner cavity of the adapting groove (19), a reset spring (20) is installed in the inner cavity of the reset groove, one side of the reset spring (20) is installed in the inner cavity of the reset groove, and the other side of the reset spring (20) is installed on the side of a reset block (22), and the reset block (22) is movably connected in the inner cavity of the reset groove.

8. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 1, characterized in that: A through slot (26) is provided in the middle of the top of the loading column (24); movable columns (29) are symmetrically mounted on the bottom of opposite sides of the two support assemblies (25); connecting columns (30) are symmetrically mounted on opposite sides of the tops of the two movable columns (29); the connecting columns (30) are movably connected in the inner cavity of the through slot (26); and the operating handle (27) is mounted on the top of the connecting column (30).

9. The high temperature resistant and extrusion resistant new energy battery sealing ring forming mold according to claim 8, characterized in that: A fixing rod (31) is installed in the inner cavity of the through slot (26), and second springs (32) are symmetrically wound around the two ends of the outer wall of the fixing rod (31), one end of the second spring (32) is installed in the inner cavity of the through slot (26), and the other end of the second spring (32) is installed on the outer wall of the connecting column (30), and the left side of the C-shaped frame (28) is rotatably connected to the top of the loading column (24).

10. A molding method for a high temperature resistant and extrusion resistant new energy battery sealing ring molding die, using the above-mentioned high temperature resistant and extrusion resistant new energy battery sealing ring molding die, characterized in that: The steps include: S1: Injecting the raw material for injection molding into the inner cavity of the mold groove (11) through the injection port (3). After the injection molding is completed, the servo motor (6) is started to drive the screw rod (5) to rotate, so that the bottom of the upper mold (2) can be threadedly connected with the screw rod (5), and the upper mold (2) can move to the left side; S2: When the upper mold (2) is separated from the top of the lower mold (1), the first spring (17) can shrink the contact block (13) toward the top, so that the first spring (17) can drive the first stripping component (12) to move toward the top of the inner cavity of the mold groove (11) through the connecting frame (14). At this time, the new energy battery sealing ring after molding can be demoulded from the mold groove (11); S3: The new energy battery sealing ring after demoulding is placed on the top of the first stripping component (12). After the upper mold (2) continues to move to the left, it will be sleeved on the outer wall of the top of the second stripping component (18) through the adapter groove (19). When the second stripping component (18) contacts the stripping rod (21), the stripping rod (21) will move to the right. At this time, the new energy battery sealing ring can be pushed into the inner cavity of the receiving box (23). At this time, the new energy battery sealing ring will be sleeved on the outer wall of the loading column (24); S4: The upper mold (2) is reset. After the upper mold (2) contacts the contact block (13), it is moved toward the bottom of the inner cavity of the lower mold (1). At the same time, the stripping rod (21) is separated from the second stripping assembly (18), so that the reset spring (20) can reset the stripping rod (21) through the reset block (22). When the upper mold (2) is completely located on the top of the lower mold (1), the molding work of the new energy battery sealing ring can continue; S5: The C-shaped frame (28) is flipped to the left. At this time, the second spring (32) moves the movable column (29) outward through the connecting column (30), so that the movable column (29) can drive the support assembly (25) to leave the inner cavity of the loading column (24). At this time, the two support assemblies (25) can fit in the inner ring of the finished new energy battery sealing ring. After the loading column (24) is removed, the position of the finished new energy battery sealing ring can be transferred.