A device and method for rapid repair and oxidation prevention of irregularly shaped sealed components.
By combining the rotation of the guide pulley driven by the handle slider with back air jet protection, the problems of insufficient repair accuracy and weld oxidation in the repair of titanium alloy irregular-shaped closed components are solved. This enables non-destructive unloading of closed components and improvement of weld quality, and is applicable to the field of sheet metal clamp welding.
Patent Information
- Application Number
- CN202611466811.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-09-20
- Publication Date
- 2026-11-17
AI Technical Summary
The existing repair and positioning welding process for irregularly shaped titanium alloy closed components has problems such as insufficient repair accuracy, high oxidation defects at weld points, and inability to safely unload the rigid support of the closed cavity.
The guide pulley is driven by a handle slider, and conformal support and non-destructive unloading are achieved through radial synchronous extension and retraction of the four-lobed unit. Combined with the back air jet of the vent pipe to form micro-positive pressure inertial protection, and the radial clamping component provides three-dimensional rigid constraint, thereby improving the repair accuracy and weld quality.
It achieves non-destructive unloading of enclosed components, anti-oxidation protection of weld joints, and improved repair precision, meeting the long-term use requirements of mass production.
Smart Images

Figure CN123103261A_ABST
Abstract
Description
Technical Field
[0001] This application belongs to the field of sheet metal welding technology, specifically relating to a device and method for rapid repair and anti-oxidation of irregularly shaped closed components. Background Technology
[0002] In the field of manufacturing titanium alloy welded components for aero-engines and fuselages, irregularly shaped enclosed components are typically formed by welding together multiple titanium alloy sub-components. For example... Figure 1 As shown, a typical irregularly shaped enclosed component, represented by the air radiator cover, consists of air radiator cover part A, air radiator cover part B, air radiator cover part C, and air radiator cover part D. Its outline is an irregular cylindrical shape with an internal cavity structure, and the surrounding welds are distributed in a spatial curve. Due to the inherent precision limitations of sheet metal forming processes, the forming tolerance of each sub-component is typically ±0.5mm, while the required gap for subsequent argon arc welding and tack welding processes must be controlled within 0.1mm. The sub-components in their free state cannot be directly joined to meet the welding tolerance requirements.
[0003] Current repair processes typically rely on the combined operation of fitters and welders. Operators apply directional pressure to the mating edges for temporary positioning, and then complete the placement of positioning welds under pressure. This method has two problems: First, manual pressure application is random, and the concentrated force applied to the outer wall of the component can easily introduce residual stress during the repair stage. This stress is released under the subsequent TIG welding thermal cycle, leading to warping or localized burn-through of the component. Second, the number of positioning welds increases significantly with insufficient repair precision, requiring multiple welds per weld pass to maintain the assembly posture, further exacerbating the heat input concentration effect.
[0004] Titanium alloys exhibit high chemical reactivity at high temperatures. During tack welding, if the molten area is exposed to air, oxidation discoloration and porosity defects easily occur on the weld surface and near the weld. Actual production statistics show that the oxidation defect rate of welds using open-type tooling is close to 100%. To improve this situation, some tooling uses flexible copper tubing attached to the outer wall of the component and inert gas is introduced for local protection. While this method has some conformal capability, the flexible connection results in insufficient sealing of the protective cavity, making it difficult to maintain the ventilation pressure. Furthermore, the copper tubing is prone to plastic deformation after repeated insertion and removal, and the protective effect continuously diminishes with increasing usage frequency. If an integral rigid filling structure is used to internally support the enclosed component, a mechanical interference problem arises where the support cannot be safely unloaded from the enclosed cavity; forcibly removing it will cause damage to the component surface or jamming of the tooling.
[0005] Therefore, the existing titanium alloy irregular-shaped closed component repair and positioning welding process and supporting tooling are significantly insufficient in simultaneously solving three aspects: repair accuracy control, weld point oxidation protection, and safe unloading of the closed cavity rigid support. Summary of the Invention
[0006] To address the issues of positioning gap differences, residual stress introduced by manual pressure, and oxidation defects caused by lack of gas protection during the repair of irregularly shaped titanium alloy enclosed components, this application provides a device and method for rapid repair and oxidation prevention of irregularly shaped enclosed components. The device uses a handle slider to drive the guide pulley to rotate, forcing the segmented units to expand and contract radially synchronously, achieving conformal support and non-destructive unloading. This is combined with the air vent pipe to create a micro-positive pressure inertial protection, while an independent radial clamping assembly provides three-dimensional rigid constraint, thereby simultaneously improving repair accuracy and weld quality.
[0007] To achieve the above technical objectives, this application specifically employs the following technical solution: In one aspect of this application, a device for rapid repair and oxidation prevention of irregularly shaped sealing components is provided, comprising the following steps: Base; The four-lobed collaborative scaling mechanism includes a guide pulley, a handle slider, an extension arm, and four lobe units. The guide pulley is coaxially fixed to the center of the back of the base. Four second arc-shaped grooves are evenly distributed on the circumferential surface of the guide pulley facing away from the base. A first arc-shaped groove is formed along the circumferential direction in the non-shaped area on the back of the base. The handle slider slides through the first arc-shaped groove, and the end of the handle slider is rigidly connected to the guide pulley through the extension arm. The four segmented units are arranged one-to-one with the four second arc-shaped grooves. Each segmented unit includes a slider, a positioning block, a conformal copper body, a vent pipe, and a vent hole. The slider is slidably embedded in the corresponding second arc-shaped groove. The positioning block is rigidly fixed to the upper end of the slider. The conformal copper body is fixed on the positioning block and conforms to the weld bead direction of the part. A groove is provided on the inner side of the conformal copper body. The vent pipe is built into the groove. The vent hole is opened on the wall of the vent pipe. The spray direction of the vent hole is opposite to the weld bead of the workpiece and faces the inside of the groove. The inner wall of the conformal copper body and the butt weld bead of the sub-part form a micro-closed cavity. A part positioning and clamping mechanism, comprising a radial clamping assembly and a top positioning assembly, wherein the radial clamping assembly is used to press and lock the lower edge of the sub-part, and the top positioning assembly is used to constrain the upper edge of the sub-part; When the handle slider slides along the first arc-shaped groove, the handle slider drives the guide pulley to rotate through the extension arm, and the four second arc-shaped grooves generate radial force through the mating surface between the groove wall and the slider, forcing the four sliders to expand or contract synchronously in the radial direction.
[0008] In one embodiment, each of the segmented units further includes a support frame, one end of which is fixed to the slider, and the other end of which is connected to the curve inflection point of the conformal copper body in a combined tension and compression configuration.
[0009] In one embodiment, the support frame is a steel component. One end of the support frame is fixed to the slider by bolts, and the other end of the support frame is connected to the bottom curve inflection point and stress concentration point of the conformal copper body in a combined tension and compression force form. The support frame provides multi-point rigid support for the conformal copper body.
[0010] In one embodiment, the radial clamping assembly includes a push plate, a pressure claw, a fastening element, and a guide fixing shaft. The guide fixing shaft is fixedly connected to the base. The push plate and the pressure claw are slidably disposed along the guide fixing shaft. The inner working surface of the push plate directly abuts the lower edge of the pressing component. The pressure claw locks the side wall of the push plate through the fastening element to restrict the push plate from retracting.
[0011] In one embodiment, the radial clamping assembly is provided at the lower part of the base, and the push plate and the pressure claw are both slidably sleeved on the guide fixing shaft fixed to the base in a radial direction, and the push plate and the pressure claw are arranged opposite to each other; the upper thread of the pressure claw is connected to the fastening element, and the end of the fastening element passes through the pressure claw; When the push plate moves along the guide fixing shaft to a predetermined position at the lower edge of the pressing component, the fastening element is tightened or pressed down so that the pressure claw is tightly abutted and locked with the guide fixing shaft. The pressure claw acts as a radial stop to restrict the push plate from retracting outward.
[0012] In one embodiment, the top positioning assembly includes a support rod, a support bushing, a bracket, and a top positioning block. The top positioning block has an clearance opening for accommodating and constraining the upper extension of the conformal copper body. The support rod is vertically fixed to one side of the base, the support bushing is sleeved on the bottom of the support rod, the support bushing is fixedly connected to the base, the bracket is slidably engaged with the support rod and can slide up and down along the support rod, and the top positioning block is fixed to the top of the bracket.
[0013] In one embodiment, the top positioning assembly further includes a pressure block and a cylindrical pin with a fixed handle. The pressure block is circumferentially distributed on the outside of the top positioning block and is used to press the upper edge of the workpiece. The cylindrical pin with a fixed handle passes through the bracket and is used to lock the lifting position of the bracket.
[0014] In one embodiment, the clearance openings at the four corners of the top positioning block are L-shaped clearance openings, and the plurality of L-shaped clearance openings correspond one-to-one with the plurality of segmented units.
[0015] In one embodiment, the base is made of stainless steel, and the conformal copper body is made of copper, copper alloy, or high thermal conductivity aluminum bronze.
[0016] In another aspect of this application, a method for rapidly repairing and preventing oxidation of irregularly shaped sealing components is provided, and the apparatus for rapidly repairing and preventing oxidation of the irregularly shaped sealing components includes the following steps: S1: Tooling pre-adjustment and part placement: Release the locking state of the pressure claw, reverse the operation of the handle slider to make the four segmented units shrink synchronously, and leave an assembly allowance in the conformal copper body to place the sub-part into the tooling cavity. S2: Surface fitting and gap adjustment: The handle slider is operated in the forward direction to make the four segmented units extend outward synchronously. The conformal curved surface of the conformal copper body fits the outer edge of the sub-part to be welded area. The mating edge is filed under the support of the conformal copper body. S3: Gas path establishment and inertial protection: Connect the vent pipe to the argon gas source, and inject argon gas into the micro-enclosed cavity enclosed by the conformal copper body and the part through the vent hole to establish a micro-positive pressure inert protection layer. S4: Tack welding: Tack welds are arranged along the weld bead under inert atmosphere protection; S5: Tooling unloading and part removal: Cut off the air source, reverse the operation of the handle slider to make the four segmented units retract synchronously and detach from the mold surface, release the upper constraint, release the locking state of the pressure claw, and remove the workpiece.
[0017] In one embodiment, step S5, releasing the upper constraint includes: pulling out the cylindrical pin with the fixed handle, moving the bracket and the top positioning block upward, so that the clearance opening is disengaged from the upper end of the conformal copper body.
[0018] The beneficial effects of this application are as follows: 1. The scaling mechanism and clamping mechanism are decoupled to achieve non-destructive unloading of the enclosed component. The handle slider drives the guide pulley to rotate, and the radial component force between the second arc-shaped groove wall and the slider mating surface forces the four segmented units to expand or contract synchronously. This provides rigid conformal support for the conformal copper body during fitting and radially retracts and detaches from the mold surface during unloading. The radial clamping assembly slides and locks independently of the scaling mechanism along the guide fixed axis, and the two do not interfere with each other, solving the mechanical interference problem of rigid tooling being unable to safely withdraw from the enclosed cavity.
[0019] 2. Back-to-back ventilation, combined with a closed cavity, forms a slightly positive pressure inert protective layer. The ventilation pipe is built into the groove of the conformal copper body, with the ventilation hole spraying in the direction away from the weld bead and facing the inside of the groove. Argon gas slowly diffuses from the inside of the groove into the slightly closed cavity enclosed by the conformal copper body and the weld bead, forming a laminar flow displacement path from the inside to the outside. This avoids the gas flow directly blowing into the molten pool and causing disturbance. At the same time, the conformal copper body fits the workpiece to ensure the cavity is sealed, preventing the positioning weld points from oxidation.
[0020] 3. The rigid-flexible coupling support structure balances conformal fitting accuracy with rigidity retention. The conformal copper body provides conformal curved surface support consistent with the weld bead direction. The steel support frame is connected to the bottom curve inflection point of the conformal copper body in a combined tension and compression stress form, compensating for the flexibility of the copper material itself. This allows the tooling to maintain surface accuracy under the action of fitting, grinding, and welding heat input. The fitting gap and misalignment are reduced to within 0.1mm, the number of positioning welds is reduced, and the residual stress introduced by manual directional pressure is eliminated.
[0021] 4. The top L-shaped clearance opening and the bottom pressure claw-push plate locking mechanism form a three-dimensional spatial constraint. The tooling surface has no reduction in accuracy after multiple loading and unloading cycles, which meets the long-term use requirements of mass production lines. Attached Figure Description
[0022] Figure 1 This is a schematic diagram of the external shape of the air radiator cover assembly of this application; Figure 2 This is a schematic diagram of the structure of the device according to an embodiment of this application; Figure 3 This is a schematic diagram of the front structure of the device base according to an embodiment of this application; Figure 4 This is a schematic diagram of the back structure of the device base in an embodiment of this application; Figure 5 This is a schematic diagram of the main support mechanism of the device according to an embodiment of this application; Figure 6 This is a schematic diagram of the segmented unit structure in an embodiment of this application; Figure 7 This is a schematic diagram of the ventilation pipe structure in the ventilation protection structure of this application embodiment; In the diagram: 1-Air radiator top cover A; 2-Air radiator top cover B; 3-Air radiator top cover C; 4-Air radiator top cover D; 5-Ventilation pipe; 6-Irregular copper body; 7-Support frame; 8-Positioning block; 9-Slider; 10-Ventilation hole; 11-Base; 12-Pressure claw; 13-Push plate; 14-Handle slider; 15-First arc groove; 16-Support bushing; 17-Bracket; 18-Top positioning block; 19-Connecting shaft; 20-Guide pulley; 21-Extension arm; 22-Second arc groove; 23-Pressure block; 24-Support rod; 25-Cylindrical pin with fixed handle; 26-Fastening element. Detailed Implementation
[0023] The technical solution of this application will be clearly and completely described below with reference to specific embodiments. However, those skilled in the art will understand that the embodiments described below are only some embodiments of this application, not all embodiments, and are only used to illustrate this application, and should not be regarded as limiting the scope of this application. Based on the embodiments in this application, all other embodiments obtained by those skilled in the art without creative effort are within the scope of protection of this application.
[0024] In one specific embodiment, refer to Figure 2-7 As shown, a device for rapid repair and oxidation prevention of irregularly shaped enclosed components includes a base 11, a four-lobed collaborative scaling mechanism, a conformal gas protection mechanism, and a part positioning and clamping mechanism.
[0025] The base 11 serves as the main body of the tooling, providing rigid support and installation reference for the entire machine. A guide pulley 20 is coaxially fixed at the center of the back of the base 11, and four second arc-shaped grooves 22 are evenly distributed on the circumferential surface of the guide pulley 20 facing away from the base 11. A first arc-shaped groove 15 is formed circumferentially in the non-shaped area on the back of the base 11. The handle slider 14 slides through the first arc-shaped groove 15, and the end of the handle slider 14 is rigidly connected to the guide pulley 20 through an extension arm 21.
[0026] The base 11 has a radial clamping assembly at its lower part, including a push plate 13, a pressure claw 12, and a guide fixing shaft. Both the push plate 13 and the pressure claw 12 are radially slidably mounted on the guide fixing shaft fixed to the base 11, with the push plate 13 and pressure claw 12 positioned opposite each other. The inner working surface of the push plate 13 directly abuts against the lower edge of the pressing component. A fastening element 26 is threaded onto the pressure claw 12, with its end passing through the pressure claw 12 and facing the guide fixing shaft. When the push plate 13 moves along the guide fixing shaft to a predetermined position abutting against the lower edge of the pressing component, it simultaneously tightens or presses down the fastening element 26, with the end of the fastening element 26 pressing against the guide fixing shaft, causing the pressure claw 12 to tightly abut and lock against the guide fixing shaft. The pressure claw 12 acts as a radial stop, restricting the push plate 13 from retracting outwards and rigidly fixing the pressing position of the push plate 13.
[0027] The radial clamping assembly and the four-segment collaborative scaling mechanism are structurally independent and completely decoupled in motion. The handle slider 14 reciprocates along the first arc-shaped groove 15, driving the guide pulley 20 to rotate around the fixed central axis via the extension arm 21. When the guide pulley 20 rotates, the four second arc-shaped grooves 22 generate radial force through the groove walls and the lateral mating surfaces of the sliders 9, forcing the four sliders 9 to expand outward or contract inward synchronously in the radial direction. During clamping, the push plate 13 slides independently of the handle slider 14 along the guide fixed axis to press against the workpiece. After locking, it works in conjunction with the segmented unit to provide three-dimensional rigid constraint. The sliding operation of the push plate 13 and the reciprocating motion of the handle slider 14 do not interfere with each other.
[0028] Four segmented units are arranged in a one-to-one correspondence with four second arc-shaped grooves 22. Each segmented unit includes a slider 9, a positioning block 8, a conformal copper body 6, a vent pipe 5, a support frame 7, and a vent hole 10. The slider 9 is slidably embedded in the corresponding second arc-shaped groove 22, and the positioning block 8 is rigidly fixed to the upper end of the slider 9. The conformal copper body 6 is fixed on the positioning block 8, and the contour of the conformal copper body 6 is a conformal curve to conform to the weld bead direction of the part.
[0029] Specifically, the conformal copper body 6 has a stepped groove milled on its inner side, with a width of 10mm and a depth of 10mm. The overall cross-sectional dimensions of the conformal copper body 6 are 20mm × 20mm. The vent pipe 5 is a φ8 copper pipe, which is built into the stepped groove. Ventilation holes 10 are evenly spaced along the axial direction on the wall of the vent pipe 5, with a spacing of 10mm between adjacent ventilation holes 10. The diameter of the ventilation holes 10 is φ1.2mm. The spray direction of the ventilation holes 10 is opposite to the workpiece weld bead and faces the inside of the stepped groove. The inner wall of the conformal copper body 6 and the butt weld bead of the sub-part form a micro-closed cavity.
[0030] The support frame 7 is a steel component. One end of the support frame 7 is fixed to the slider 9 by bolts, and the other end of the support frame 7 is connected to the bottom curve inflection point and stress concentration point of the conformal copper body 6 in a combined tension and compression stress manner. The support frame 7 provides multi-point rigid support for the conformal copper body 6 to compensate for the flexible deformation of the conformal copper body 6 and prevent the loss of surface accuracy of the conformal copper body 6 caused by the heat input of repair grinding and positioning welding.
[0031] The part positioning and clamping mechanism includes a radial clamping assembly and a top positioning assembly. The radial clamping assembly is used to press and lock the lower edge of the part, and the top positioning assembly is used to constrain the upper edge of the part.
[0032] The radial clamping assembly includes a push plate 13, a pressure claw 12, a fastening element 26, and a guide fixing shaft. The guide fixing shaft is fixedly connected to the base 11. The push plate 13 and the pressure claw 12 are slidably arranged along the guide fixing shaft, with the push plate 13 and the pressure claw 12 arranged opposite to each other. The inner working surface of the push plate 13 is used to directly press against the lower edge of the component. The pressure claw 12 is threaded with a fastening element 26, the end of which passes through the pressure claw 12 and is aligned with the guide fixing shaft. When the push plate 13 moves along the guide fixing shaft to a predetermined position against the lower edge of the component, the fastening element 26 is tightened or pressed down, and the end of the fastening element 26 presses against the guide fixing shaft, so that the pressure claw 12 and the guide fixing shaft are tightly abutted and locked. The pressure claw 12 acts as a radial stop to restrict the push plate 13 from retracting outward, rigidly fixing the pressing position of the push plate 13.
[0033] The top positioning assembly includes a support rod 24, a support bushing 16, a bracket 17, and a top positioning block 18. The support rod 24 is vertically fixed to one side of the base 11. The support bushing 16 is fitted onto the bottom of the support rod 24 and is fixedly connected to the base 11. The bracket 17 slides along the support rod 24, allowing it to slide up and down. The top positioning block 18 is fixed to the top of the bracket 17 via a connecting shaft 19. The top positioning block 18 has an clearance opening to accommodate and constrain the upper extension of the conformal copper body 6. The top positioning assembly also includes a pressure block 23 and a cylindrical pin 25 with a fixed handle. The pressure block 23 is circumferentially distributed on the outside of the top positioning block 18 and is used to press the upper edge of the workpiece. The cylindrical pin 25 with a fixed handle passes through the bracket 17 and is used to lock the lifting position of the bracket 17.
[0034] The four corner openings of the top positioning block 18 are L-shaped clearance openings, and there are four L-shaped clearance openings in total. Each of the four L-shaped clearance openings corresponds to one of the four segmented units. After the segmented unit extends outward to fit the part, the upper extension of the conformal copper body 6 is positioned into the L-shaped clearance opening. The L-shaped clearance opening forms an upper anti-deformation constraint on the upper extension of the conformal copper body 6.
[0035] As the conformal copper body 6 expands and moves with the four segmented units to fit the inner wall of the workpiece, the inner wall of the conformal copper body 6 and the butt welds of the multiple pieces together form multiple independent micro-enclosed cavities. The upper end of the vent pipe 5 is connected to an external argon gas supply line, and argon gas is injected into the groove of the conformal copper body 6 in a back-facing manner through the vent hole 10. The argon gas slowly diffuses from the inside of the groove to the outside, gradually replacing the air in the micro-enclosed cavities and establishing a stable micro-positive pressure inert protective atmosphere within the micro-enclosed cavities. The injection direction of the vent hole 10 is opposite to the workpiece weld and facing the inside of the groove, so that the argon gas does not blow directly onto the molten pool area, avoiding disturbance to the molten pool caused by direct airflow. The tight fit between the inner wall of the conformal copper body 6 and the outer wall of the workpiece ensures the airtightness of the micro-enclosed cavities.
[0036] Based on the above-described device, this embodiment provides a method for rapidly repairing and preventing oxidation of irregularly shaped sealed components, specifically including the following steps: S1: Tooling pre-adjustment and parts placement Loosen the fastening element 26 to release the locking state of the pressure claw 12 on the push plate 13. Push and pull the handle slider 14 in the opposite direction. The handle slider 14 slides in the opposite direction along the first arc groove 15, driving the guide pulley 20 to rotate around the fixed central axis through the extension arm 21. When the guide pulley 20 rotates in the opposite direction, the four second arc grooves 22 generate radial force through the mating surface between the groove wall and the slider 9, forcing the four sliders 9 to slide synchronously inward in the radial direction, driving the four segmented units to retract synchronously. The conformal copper body 6 and the positioning block 8 retract inward with the slider 9, leaving assembly allowance for the insertion of the sub-parts. Place the four TC1M titanium alloy sub-parts into the tooling cavity in the assembly sequence, so that the mating edges of each sub-part are in the position to be repaired.
[0037] S2: Surface fitting and gap adjustment The handle slider 14 is pushed and pulled forward, sliding along the first arc-shaped groove 15. The extension arm 21 drives the guide pulley 20 to rotate forward around the fixed central axis. When the guide pulley 20 rotates forward, the four second arc-shaped grooves 22 generate radial force through the mating surfaces of the groove walls and sliders 9, forcing the four sliders 9 to slide outwards radially and synchronously, causing the four segmented units to extend outwards synchronously. The conformal curved surface of the conformal copper body 6 moves outwards with the segmented units, closely fitting the outer edge of the sub-part's welding area. Under the rigid support of the conformal copper body 6, the fitter files the butt joint edges of the sub-part to control the fitting gap and misalignment within 0.1mm.
[0038] S3: Gas path establishment and inertia protection Connect the upper end of the vent pipe 5 to an external argon gas supply line and adjust the argon gas flow rate to 5L / min~15L / min. Argon gas is injected through the vent hole 10 on the wall of the vent pipe 5 into the micro-enclosed cavity enclosed by the conformal copper body 6 and the sub-component. The injection direction of the vent hole 10 is opposite to the weld bead on the workpiece and faces the inside of the groove on the conformal copper body 6, allowing the argon gas to slowly diffuse from the inside of the groove to the outside, forming a slow-displacement laminar flow within the micro-enclosed cavity. This gradually replaces the air within the micro-enclosed cavity, establishing a stable micro-positive pressure inert gas protective layer on the back of the weld bead and in the tack weld area.
[0039] S4: Positioning Welding Under an inert atmosphere, tack welds are arranged along the weld bead. Welding heat is applied to the conformal copper body 6 and the support frame 7. The conformal copper body 6 and the support frame 7 jointly bear the welding heat cycle, suppressing thermal deformation and residual stress concentration in the sub-component. The surface of the tack welds is silvery-white, without oxidation discoloration or porosity defects.
[0040] S5: Tooling unloading and parts removal After welding, the argon gas supply is cut off. Pushing and pulling the handle slider 14 in the opposite direction causes the guide pulley 20 to reverse, and the four segmented units retract inwards synchronously, disengaging the conformal curved surface of the conformal copper body 6 from the part's profile. Pulling out the cylindrical pin 25 with the fixed handle releases the lock between the bracket 17 and the support rod 24. Moving the bracket 17 upward causes the top positioning block 18 to slide upwards along the support rod 24, disengaging the L-shaped clearance openings at the four corners of the top positioning block 18 from the upper extension of the conformal copper body 6. Loosening the fastening element 26 releases the locking of the pressure claw 12 onto the push plate 13, allowing the workpiece to be removed vertically upwards along the axial direction.
[0041] Although the embodiments of this application have been described above in conjunction with the accompanying drawings, this application is not limited to the specific embodiments and application fields described above. The specific embodiments described above are merely illustrative and instructive, not restrictive. Those skilled in the art can make many other forms based on the guidance of this specification and without departing from the scope of protection of the claims of this application, and these are all within the scope of protection of this application.
Claims
1. A device for rapid repair and oxidation prevention of irregularly shaped sealed components, characterized in that, include: Base; The four-lobed collaborative scaling mechanism includes a guide pulley, a handle slider, an extension arm, and four lobe units. The guide pulley is coaxially fixed to the center of the back of the base. Four second arc-shaped grooves are evenly distributed on the circumferential surface of the guide pulley facing away from the base. A first arc-shaped groove is formed along the circumferential direction in the non-shaped area on the back of the base. The handle slider slides through the first arc-shaped groove, and the end of the handle slider is rigidly connected to the guide pulley through the extension arm. The four segmented units are arranged one-to-one with the four second arc-shaped grooves. Each segmented unit includes a slider, a positioning block, a conformal copper body, a vent pipe, and a vent hole. The slider is slidably embedded in the corresponding second arc-shaped groove. The positioning block is rigidly fixed to the upper end of the slider. The conformal copper body is fixed on the positioning block and conforms to the weld bead direction of the part. A groove is provided on the inner side of the conformal copper body. The vent pipe is built into the groove. The vent hole is opened on the wall of the vent pipe. The spray direction of the vent hole is opposite to the weld bead of the workpiece and faces the inside of the groove. The inner wall of the conformal copper body and the butt weld bead of the sub-part form a micro-closed cavity. A part positioning and clamping mechanism, comprising a radial clamping assembly and a top positioning assembly, wherein the radial clamping assembly is used to press and lock the lower edge of the sub-part, and the top positioning assembly is used to constrain the upper edge of the sub-part; When the handle slider slides along the first arc-shaped groove, the handle slider drives the guide pulley to rotate through the extension arm, and the four second arc-shaped grooves generate radial force through the mating surface between the groove wall and the slider, forcing the four sliders to expand or contract synchronously in the radial direction.
2. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 1, characterized in that, Each of the segmented units also includes a support frame, one end of which is fixed to the slider, and the other end of which is connected to the curve inflection point of the conformal copper body in a combined tension and compression force manner.
3. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 2, characterized in that, The support frame is a steel component. One end of the support frame is fixed to the slider by bolts, and the other end of the support frame is connected to the bottom curve inflection point and stress concentration point of the conformal copper body in a combined tension and compression force form. The support frame provides multi-point rigid support for the conformal copper body.
4. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 1, characterized in that, The radial clamping assembly includes a push plate, a pressure claw, a fastening element, and a guide fixing shaft. The guide fixing shaft is fixedly connected to the base. The push plate and the pressure claw are slidably arranged along the guide fixing shaft. The inner working surface of the push plate directly abuts the lower edge of the pressing part. The pressure claw locks the side wall of the push plate through the fastening element to restrict the push plate from retracting.
5. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 4, characterized in that, The base is provided with the radial clamping assembly at its lower part. The push plate and the pressure claw are both slidably sleeved on the guide fixing shaft fixed to the base in a radial direction, and the push plate and the pressure claw are arranged opposite to each other. The upper thread of the pressure claw is connected to the fastening element, and the end of the fastening element passes through the pressure claw. When the push plate moves along the guide fixing shaft to a predetermined position at the lower edge of the pressing component, the fastening element is tightened or pressed down so that the pressure claw is tightly abutted and locked with the guide fixing shaft. The pressure claw acts as a radial stop to restrict the push plate from retracting outward.
6. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 1, characterized in that, The top positioning assembly includes a support rod, a support bushing, a bracket, and a top positioning block. The top positioning block has an clearance opening, which is used to accommodate and constrain the upper extension of the conformal copper body. The support rod is vertically fixed to one side of the base, the support bushing is sleeved on the bottom of the support rod, the support bushing is fixedly connected to the base, the bracket is slidably engaged with the support rod and can slide up and down along the support rod, and the top positioning block is fixed to the top of the bracket.
7. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 6, characterized in that, The top positioning component also includes a pressure block and a cylindrical pin with a fixed handle. The pressure block is circumferentially distributed on the outside of the top positioning block and is used to press the upper edge of the workpiece. The cylindrical pin with a fixed handle passes through the bracket and is used to lock the lifting position of the bracket.
8. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 6, characterized in that, The clearance openings at the four corners of the top positioning block are L-shaped clearance openings, and each of the L-shaped clearance openings corresponds to one of the multiple segmented units.
9. The device for rapid repair and oxidation prevention of irregularly shaped sealed components according to claim 1, characterized in that, The base is made of stainless steel, and the conformal copper body is made of copper, copper alloy or high thermal conductivity aluminum bronze.
10. A method for rapid repair and oxidation prevention of irregularly shaped sealing components, based on the device according to any one of claims 1-9, characterized in that, Includes the following steps: S1: Tooling pre-adjustment and part placement: Release the locking state of the pressure claw, reverse the operation of the handle slider to make the four segmented units shrink synchronously, and leave an assembly allowance in the conformal copper body to place the sub-part into the tooling cavity. S2: Surface fitting and gap adjustment: The handle slider is operated in the forward direction to make the four segmented units extend outward synchronously. The conformal curved surface of the conformal copper body fits the outer edge of the sub-part to be welded area. The mating edge is filed under the support of the conformal copper body. S3: Gas path establishment and inertial protection: Connect the vent pipe to the argon gas source, and inject argon gas into the micro-enclosed cavity enclosed by the conformal copper body and the part through the vent hole to establish a micro-positive pressure inert protection layer. S4: Tack welding: Tack welds are arranged along the weld bead under inert atmosphere protection; S5: Tooling unloading and part removal: Cut off the air source, reverse the operation of the handle slider to make the four segmented units retract synchronously and detach from the mold surface, release the upper constraint, release the locking state of the pressure claw, and remove the workpiece.