Equipment and methods for fabricating contact vias on wafers
By integrating physical vapor deposition, atomic layer deposition, and chemical vapor deposition equipment into the same machine, the problems of high equipment cost, high process risk, and wafer oxidation in contact via fabrication are solved, achieving efficient and reliable via electrical performance.
Patent Information
- Application Number
- CN202611566097.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-10-10
- Publication Date
- 2026-11-17
AI Technical Summary
In existing technologies, the fabrication of contact vias requires deposition in a separate chamber, which results in high equipment costs, significant process risks, and easy oxidation during wafer transport, affecting electrical performance.
Physical vapor deposition (PVD) and atomic layer deposition (ALD) equipment are integrated within the same machine. By switching between different process zones via a movable stage, combined with chemical vapor deposition (CVD) equipment, wafers can be transferred within the machine, avoiding exposure of wafers to the atmosphere and reducing the use of chamber resources.
It reduced equipment costs, mitigated process risks, improved the electrical performance of vias, reduced wafer oxidation risks, and enhanced process efficiency and reliability.
Smart Images

Figure CN123108512A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of chip processing technology, and in particular to a device and method for preparing contact vias on a wafer. Background Technology
[0002] Contact vias are open structures obtained by etching the interlayer dielectric in semiconductor mid-stage processes (MEOL). The bottom of the via exposes the active silicon region of the transistor or polysilicon, and the via is filled with a conductive thin film to achieve a vertical ohmic conductive connection between the transistor device and the first metal interconnect.
[0003] In the current mid-stage manufacturing process of logic chips, contact vias are typically fabricated by using physical vapor deposition, atomic layer deposition, and chemical vapor deposition independently after metal silicide process.
[0004] However, existing deposition processes occupy a lot of equipment resources and increase process costs because they are carried out in separate chambers. Moreover, some processes are not completed in the same equipment, which requires wafer transfer. During the transfer, the wafer will come into contact with air and be oxidized, which will increase the resistance of the contact vias and reduce the electrical performance.
[0005] The fabrication of contact vias in related technologies requires deposition in separate chambers, and wafer transfer between chambers is prone to oxidation, resulting in high equipment costs and significant process risks. Currently, no effective solution has been proposed. Summary of the Invention
[0006] The present invention provides a wafer contact via fabrication equipment and method, which at least solves the problems in related technologies where the fabrication of contact vias requires deposition in an independent chamber, and wafer transfer between chambers is prone to oxidation, resulting in high equipment costs and high process risks.
[0007] One aspect of the present invention provides an apparatus for fabricating contact vias on a wafer, comprising: a first deposition chamber and a second deposition chamber disposed on the same machine platform; the first deposition chamber is provided with a movable stage, a physical vapor deposition (PVD) apparatus, and an atomic layer deposition (ALD) apparatus; the PVD apparatus is disposed at the top of the first deposition chamber and includes a magnetron, a cathode base, and a target material arranged sequentially, with a PVD deposition area below the target material; the ALD apparatus is disposed on the side of the first deposition chamber and includes an input gas pipe and a spray head; the input gas pipe connects a deposition gas source to the spray head; the spray head is rotatably mounted on a clearance cavity on the side, and when the spray head rotates out of the clearance cavity, the ALD area is below the spray head; the movable stage is used to support a wafer to be processed, the wafer to be processed including etched via structures, and the movable stage moves between the PVD area and the ALD area; the second deposition chamber is provided with a chemical vapor deposition (CVD) apparatus for performing CVD on the wafer to be processed.
[0008] As an optional solution, the target material of the physical vapor deposition equipment is titanium metal, and the cathode base is connected to the sputtering power supply; the movable stage has a built-in heating component for heating the wafer to be processed; the movable stage is also equipped with an electrostatic adsorption device for electrostatically adsorbing the wafer to be processed; the movable stage is connected to an RF bias power supply for applying an RF bias to the wafer to be processed during the physical vapor deposition process.
[0009] As an optional embodiment, the gas source of the atomic layer deposition equipment includes a TiCl4 gas source and an NH3 gas source; the spray head is connected to a rotating motor via a rotating shaft, the rotating motor is located outside the first deposition chamber, and the input gas pipe includes a first gas pipe and a second gas pipe respectively connected to the TiCl4 gas source and the NH3 gas source. Both the first gas pipe and the second gas pipe are located inside the rotating shaft, and the end of the rotating shaft near the rotating motor is provided with a gas passage interface for the first gas pipe and the second gas pipe. The gas passage interface is located outside the first deposition chamber and is connected to the corresponding gas source.
[0010] As an optional solution, the chemical vapor deposition equipment is installed at the top of the second deposition chamber, and a fixed stage is provided inside the second deposition chamber. The chemical vapor deposition equipment includes a gas spray head, which is connected to a tungsten deposition gas source. The tungsten deposition gas source includes an H2 gas source and a WF6 gas source.
[0011] As an alternative, a transfer device is provided between the first deposition chamber and the second deposition chamber. The transfer device includes a vacuum transfer chamber and a vacuum manipulator disposed in the vacuum transfer chamber. The vacuum transfer chamber is connected to the first deposition chamber and the second deposition chamber through a vacuum gate valve.
[0012] Another aspect of the present invention provides a method for fabricating contact vias on a wafer, comprising: fixing a wafer to be processed onto a movable stage of a first deposition chamber, and moving it to a physical vapor deposition area below a target of a physical vapor deposition apparatus, and depositing a metal adhesion layer on the etched via structure on the wafer to be processed; wherein the physical vapor deposition apparatus is disposed at the top of the first deposition chamber, and the physical vapor deposition apparatus includes a magnetron, a cathode base, and a target arranged sequentially; rotating the spray head of an atomic layer deposition apparatus out of the clearance cavity of the first deposition chamber, and moving the movable stage to the atomic layer deposition area below the spray head. In the deposition area, a diffusion barrier layer is deposited on the wafer to be processed that has already had a deposited metal adhesion layer. The atomic layer deposition equipment is located on the side of the first deposition chamber and includes an input gas pipe and a spray head. The input gas pipe connects the deposition gas source to the spray head, and the spray head is rotatably mounted on the side clearance cavity. The wafer to be processed with the deposited diffusion barrier layer is transferred to the second deposition chamber of the same machine, where a metal filling layer is deposited using a chemical vapor deposition (CVD) device to form contact vias. The second deposition chamber is equipped with a CVD device for performing CVD on the wafer to be processed.
[0013] As an optional approach, the spray head of the atomic layer deposition (ALD) apparatus is rotated out of the clearance chamber of the first deposition chamber, and the movable stage is moved to the ALD region below the spray head to deposit a diffusion barrier layer on the wafer to be processed that has already had a deposited metal adhesion layer. This includes: if the spray head and the movable stage do not interfere with each other, first rotating the spray head out of the clearance chamber, and then moving the movable stage to the ALD region below the spray head; if the spray head and the movable stage interfere with each other, first moving the movable stage to the ALD region below the spray head, and then rotating the spray head out of the clearance chamber.
[0014] As an optional approach, a metal adhesion layer is first deposited on the etched via structure on the wafer to be processed, including: heating the movable stage to a preset temperature and moving it to the physical vapor deposition region; turning on the sputtering power supply to output power, inert gas ignition to form plasma, bombarding the target material to sputter out metallic titanium atoms; turning on the radio frequency bias power supply to apply radio frequency bias to the wafer to be processed, and at the preset temperature, the deposited metallic titanium atoms react with the silicon substrate of the wafer to be processed to generate metal silicide.
[0015] As an optional approach, a diffusion barrier layer is deposited on the wafer to be processed with a pre-deposited metal adhesion layer, comprising: spraying TiCl4 vapor through a spray head for a first preset pulse time, where it reacts and adsorbs with the surface of the pre-deposited metal adhesion layer, wherein the first preset pulse time is 0.5-3s; purging the chamber with an inert gas for a second preset pulse time, where the second preset pulse time is 0.5-10s and the gas flow rate is 100-50000sccm; spraying NH3 gas through a spray head for a first preset pulse time, where it reacts and adsorbs with the surface of the pre-deposited TiCl4 to generate a diffusion barrier layer, wherein the diffusion barrier layer is composed of TiN; and purging the chamber with an inert gas for a second preset pulse time to remove excess co-reacting gases and byproducts.
[0016] As an optional approach, the wafer to be processed, with a diffusion barrier layer already deposited, is transferred to a second deposition chamber on the same equipment. A metal-filling layer is deposited using a chemical vapor deposition (CVD) device to form contact vias. This includes: transferring the wafer to be processed to the second deposition chamber using a vacuum manipulator, placing it on a fixed stage within the second deposition chamber, and heating the wafer to a preset process temperature; introducing SiH4 gas and WF6 gas through a gas spray head to deposit a tungsten nucleation layer on the wafer; purging the chamber with inert gas according to a second preset pulse time to remove excess co-reacting gases and byproducts; and introducing H2 gas and WF6 gas through a gas spray head to grow a thick tungsten film on the tungsten nucleation layer to fill the via structure, thus forming contact vias.
[0017] The wafer contact via fabrication equipment provided in this invention integrates a top-mounted physical vapor deposition (PVD) device and a side-rotatable atomic layer deposition (ALD) device within the first deposition chamber of the same machine. A movable stage allows for switching between different process zones, and the spray head can be housed in an avoidance chamber to prevent interference with the PVD process. This integrates PVD and ALD processes into a single chamber, reducing chamber resource usage. Combined with a second deposition chamber on the same machine, the wafer can be transferred within the machine, reducing the risk of oxidation from exposure to the atmosphere. Simultaneously, the first deposition chamber enables high chemical vapor deposition and in-situ metal silicide generation, eliminating the need for a separate metal silicide step. This solves the problems of separate chambers, easy oxidation, and numerous process steps inherent in traditional processes, achieving the technical effects of saving equipment and process costs, reducing process risks, and improving the electrical performance of vias. Attached Figure Description
[0018] To more clearly illustrate the technical solutions in the embodiments of the present invention or the prior art, the accompanying drawings used in the description of the embodiments or the prior art will be briefly introduced below. Obviously, the drawings described below are merely some embodiments of the present invention. For those skilled in the art, other embodiments can be obtained based on these drawings without creative effort.
[0019] Figure 1 This is a schematic diagram of a wafer contact via fabrication apparatus according to an embodiment of the present invention.
[0020] Figure 2 This is a schematic diagram of the first deposition cavity structure according to an embodiment of the present invention.
[0021] Figure 3 This is a schematic diagram of physical vapor deposition performed in the first deposition chamber according to an embodiment of the present invention.
[0022] Figure 4 This is a schematic diagram of atomic layer deposition performed in the first deposition cavity according to an embodiment of the present invention.
[0023] Figures 5-8 This is a schematic diagram of the various steps in the fabrication process of a contact via according to an embodiment of the present invention.
[0024] Figure 9 This is a flowchart of a method for preparing contact vias on a wafer according to an embodiment of the present invention.
[0025] The reference numerals in the above figures are as follows: 1. First deposition chamber; 11. Clearance chamber; 2. Second deposition chamber; 3. Movable stage; 4. Physical vapor deposition equipment; 41. Magnetron; 42. Cathode base; 43. Target material; 44. Sputtering power supply; 5. Atomic layer deposition equipment; 51. Gas inlet pipe; 52. Spray head; 53. Rotating shaft; 54. Rotating motor; 6. Wafer to be processed; 61. Through-hole structure; 7. Chemical vapor deposition equipment; 8. Radio frequency bias power supply; 91. Metal adhesion layer; 92. Diffusion barrier layer; 93. Metal filler layer. Detailed Implementation
[0026] Embodiments of the present invention will now be described in more detail with reference to the accompanying drawings. While some embodiments of the invention are shown in the drawings, it should be understood that the invention can be implemented in various forms and should not be construed as limited to the embodiments set forth herein. Rather, these embodiments are provided to provide a more thorough and complete understanding of the invention. It should be understood that the accompanying drawings and embodiments are for illustrative purposes only and are not intended to limit the scope of protection of the invention.
[0027] like Figures 1 to 4As shown, an embodiment of the present invention provides a device for fabricating contact vias on a wafer, comprising: a first deposition chamber 1 and a second deposition chamber 2 disposed on the same machine platform, wherein a movable stage 3, a physical vapor deposition device 4 and an atomic layer deposition device 5 are disposed in the first deposition chamber 1.
[0028] The physical vapor deposition apparatus 4 is located at the top of the first deposition chamber 1. The physical vapor deposition apparatus 4 includes a magnetron 41, a cathode base 42 and a target 43 arranged in sequence. The area below the target 43 is the physical vapor deposition zone.
[0029] The atomic layer deposition apparatus 5 is located on the side of the first deposition chamber 1. The atomic layer deposition apparatus 5 includes an input gas pipe 51 and a spray head 52. The input gas pipe 51 connects the deposition gas source to the spray head 52. The spray head 52 is rotatably mounted on the side clearance chamber 11. When the spray head 52 rotates out of the clearance chamber 11, the area below the spray head 52 is the atomic layer deposition area.
[0030] The movable stage 3 is used to support the wafer 6 to be processed, which includes etched through-hole structures 61. The movable stage 3 moves between the physical vapor deposition region and the atomic layer deposition region.
[0031] The second deposition chamber 2 is equipped with a chemical vapor deposition device 7, which is used to perform chemical vapor deposition on the wafer 6 to be processed.
[0032] like Figure 2 As shown, the first deposition chamber 1 can be a composite vacuum process chamber within the machine, where both physical vapor deposition and atomic layer deposition (ALD) processes can be completed. Specifically, in the contact via of this embodiment, titanium is deposited as a metal adhesion layer using physical vapor deposition, and titanium nitride is deposited as a diffusion barrier layer using atomic layer deposition.
[0033] The avoidance cavity 11 is located in the storage position on the side of the first deposition cavity 1, and is used to house the spray head 52 when it is not in operation, so as to avoid interfering with the physical vapor deposition (PVD) sputtering process.
[0034] The aforementioned second deposition chamber 2 is an independent chemical vapor deposition process chamber within the same machine, mainly used for tungsten filling of contact vias as the final metal filling layer to complete the preparation of contact vias.
[0035] The movable stage 3 can change the vertical position of the high-temperature electrostatic chuck used to support, fix and heat the wafer, and can be switched between different process positions.
[0036] The physical vapor deposition (PVD) equipment 4 is a magnetron sputtering assembly that uses ion bombardment of the target to achieve physical sputtering of titanium films. The atomic layer deposition (ALD) equipment 5 includes an input gas pipe 51 and a rotatable spray head 52, and is an assembly that uses pulsed gas supply to achieve atomic-level thin film growth.
[0037] The physical vapor deposition zone and the atomic layer deposition zone are two working positions within the same cavity space inside the first deposition chamber 1, respectively adapted to the physical vapor deposition equipment 4 and the atomic layer deposition equipment 5, and are defined by the stage position and the working status of the spray head.
[0038] In this embodiment, the first deposition chamber 1 and the second deposition chamber 2 are set on the same machine. The two chambers belong to the same cluster equipment and can be transferred by relying on the vacuum transmission path inside the machine without having to be transferred out of the machine to come into contact with the atmosphere.
[0039] The physical vapor deposition apparatus 4 is located at the top of the first deposition chamber and consists of a magnetron 41, a cathode base 42, and a target 43. The magnetron 41 provides the sputtering magnetic field, and the cathode base 42 serves as the cathode electrode to support the target. The target 43 faces the downward-facing movable stage 3, enabling vertical downward sputtering and ensuring film coverage at the via steps.
[0040] like Figure 3 and Figure 4 As shown, the atomic layer deposition equipment 5 is located on the side of the first deposition chamber 1, and the spray head 52 is rotatably mounted in the clearance chamber 11. When not in operation, the spray head 52 retracts into the clearance chamber 11, without obstructing the transmission of sputtered particles; when performing the atomic layer deposition (ALD) process, it rotates out to the top of the wafer on the movable stage 3 to supply the ALD reaction gas source; the input gas pipe 51 is responsible for delivering the precursor gas source to the spray head 52.
[0041] The movable stage 3 carries the wafer with through-hole structure and can move between the physical vapor deposition region and the atomic layer deposition region. The movable stage 3 changes the height of the wafer by displacement, and the wafer is raised to the ground below the target and enters the physical vapor deposition region. After the wafer is lowered, it enters the atomic layer deposition region in conjunction with the rotating spray head 52.
[0042] Under the same machine, the wafer is placed on the movable stage 3. The stage is raised and the spray head 52 is stored in the clearance cavity 11. Titanium is deposited by sputtering using the top PVD equipment. Under high temperature conditions, titanium can react with the silicon substrate in situ to form metal silicide. The stage is lowered and the spray head 52 rotates out from the clearance cavity 11 to above the wafer to perform atomic layer deposition to prepare titanium nitride. After the above thin film is completed, the wafer is transferred to the second deposition cavity 2 in the vacuum environment inside the machine to perform chemical vapor deposition to fill the vias.
[0043] This embodiment integrates Physical Vapor Deposition (PVD) and Atomic Layer Deposition (ALD) processes into a single first deposition chamber, reducing the number of process chambers and saving equipment hardware resources. By placing the second deposition chamber 2 and the first deposition chamber 1 on the same equipment configuration, vacuum transfer within the wafer equipment avoids atmospheric contact, suppresses wafer surface oxidation, and improves the electrical performance of vias, further saving equipment resources. Furthermore, the high-temperature PVD process within the chamber allows for in-situ formation of metal silicides, eliminating the need for a separate metal silicide step, shortening the process flow, and reducing yield risks associated with process fluctuations.
[0044] This overcomes the limitations of traditional PVD solutions. Ti and ALD TiN uses separate process cavities, resulting in high equipment resource consumption; wafers transported across cavities / machines are susceptible to atmospheric oxidation; and a separate metallization process is required, leading to high process costs and significant process risks.
[0045] As an optional embodiment, the target material 43 of the physical vapor deposition equipment 4 is titanium metal, and the cathode base 42 is connected to the sputtering power supply 44; the movable stage 3 has a built-in heating component for heating the wafer 6 to be processed; the movable stage 3 is also provided with an electrostatic adsorption device for electrostatic adsorption of the wafer 6 to be processed; the movable stage 3 is connected to an RF bias power supply 8 for applying an RF bias to the wafer 6 to be processed during the physical vapor deposition process.
[0046] The aforementioned sputtering power supply 44 can be a DC power supply for magnetron sputtering, providing sputtering power to the cathode base 42 and the target material 43, enabling argon gas Ar ignition and titanium target sputtering.
[0047] In the physical vapor deposition equipment 4, the target material 43 is made of metallic titanium, which serves as the sputtering source to provide titanium deposition atoms. The sputtering power supply 44 outputs electrical energy to the cathode base 42, causing the target material 43 to form a negative cathode. The inert gas in the chamber is ionized to generate plasma, and the ions bombard the metallic titanium target material 43, sputtering out titanium atoms for film formation.
[0048] The heating component mentioned above can be a heating and temperature measurement unit integrated inside the movable stage 3, used to heat the wafer 6 to be processed to the high temperature required by the process, support the in-situ silicide reaction between titanium and silicon substrate, and automatically form metal silicides during physical vapor deposition, eliminating the need for a separate metal silicide process.
[0049] The heating element is embedded in the movable stage 3, which can lift and maintain the wafer 6 to be processed at the target process temperature, for PVD. Ti deposition simultaneously generates metal silicides in situ, providing the necessary temperature conditions.
[0050] The electrostatic adsorption device is an electrostatic chuck electrode structure set on the movable stage 3, which fixes the wafer 6 to be processed by electrostatic force to achieve stable clamping of the wafer.
[0051] The wafer 6 to be processed is firmly fixed to the surface of the stage by electrostatic adsorption, which avoids the wafer from shifting under the action of plasma and reduces particle generation.
[0052] The aforementioned radio frequency bias power supply 8 is electrically connected to the movable stage 3. During the physical vapor deposition (PVD) process, radio frequency bias is applied to the wafer 6 to be processed to control the bombardment effect of ions in the plasma sputtered by the titanium target.
[0053] The radio frequency bias power supply 8 is enabled only in the physical vapor deposition process. Radio frequency bias is applied to the wafer 6 to be processed to adjust the ion energy and improve the step coverage and film adhesion of the titanium layer.
[0054] The sputtering power supply 44 supplies power to the cathode base 42 and the titanium target 43 to achieve titanium atom sputtering; the movable stage 3 uses an electrostatic adsorption device to firmly hold the wafer 6 to be processed, and the built-in heating component heats the wafer to the temperature required for the siliconization reaction; in the PVD deposition stage, the radio frequency bias power supply 8 applies radio frequency bias to the wafer 6 to be processed through the movable stage 3. Under the combined effect of temperature, sputtering power and radio frequency bias, the titanium layer is deposited and the in-situ reaction between titanium and silicon substrate is achieved to generate metal silicide.
[0055] This solves the problems of existing technologies that require an additional independent metal silicide process, resulting in numerous process steps, high costs, and significant process risks; at the same time, it improves the quality of sputtered film formation and ensures the film formation effect of titanium layers inside high aspect ratio contact vias.
[0056] As an optional embodiment, the gas source of the atomic layer deposition apparatus 5 includes a TiCl4 gas source and an NH3 gas source; the spray head 52 is connected to the rotating motor 54 via a rotating shaft 53. The rotating motor 54 is located outside the first deposition chamber 1. The input gas pipe 51 includes a first gas pipe and a second gas pipe that are respectively connected to the TiCl4 gas source and the NH3 gas source. Both the first gas pipe and the second gas pipe are located inside the rotating shaft 53. The end of the rotating shaft 53 near the rotating motor 54 is provided with a gas passage interface for the first gas pipe and the second gas pipe. The gas passage interface is located outside the first deposition chamber 1 and is connected to the corresponding gas source.
[0057] The TiCl4 gas source and NH3 gas source mentioned above are both precursor gas sources for the atomic layer deposition preparation of titanium nitride. TiCl4 is the titanium source and NH3 is the nitrogen source. The two are alternately pulsed into the cavity to generate a titanium nitride thin film through a surface self-limiting reaction.
[0058] The rotating shaft 53 is a transmission component used to transmit the torque of the rotating motor 54 to drive the spray head 52 to rotate. It also serves as a gas passage carrier and integrates two independent air pipes inside.
[0059] The rotary motor 54 provides rotational driving force to drive the rotary shaft 53 to rotate the spray head 52, thereby enabling the spray head 52 to switch between the avoidance position and the process working position.
[0060] The first and second air pipes are two independent pipelines obtained by splitting the input air pipe 51, which respectively transport TiCl4 and NH3 precursors; the air pipe interface is an external connector that connects the air source and the air pipe.
[0061] Titanium tetrachloride is used as the titanium precursor and ammonia is used as the nitrogen reaction gas. The two gas sources are alternately pulsed to meet the material requirements of ALD titanium nitride self-limited growth.
[0062] TiCl4 and NH3 gas source matched atomic layer deposition (ALD) process can grow dense titanium nitride diffusion barrier layer with good shape preservation, which is suitable for the film formation requirements of high aspect ratio contact via sidewall. The rotating motor 54 is arranged outside the cavity of the avoidance cavity 11 to prevent the motor from being corrosive precursors and plasma environment inside the cavity; thus improving the equipment life and operational reliability.
[0063] The motor output torque is transmitted through the rotating shaft 53, which drives the spray head 52 to rotate, completing the position switching between storage avoidance and process positioning.
[0064] The first and second process gas pipes, used for separately transporting TiCl4 and NH3, are embedded inside the rotating shaft 53 and rotate together with it. This eliminates the need for an exposed flexible hose in the clearance cavity 11 of the first deposition chamber 1, allowing the two precursor gases to be supplied to the spray head 52 separately.
[0065] The two gas lines are integrated inside the rotating shaft 53 and rotate synchronously with the shaft, eliminating the need for the easily aging flexible gas lines in the chamber and reducing the risk of line bending failure. The air passage interface on the rotating shaft 53 is located on the outside of the cavity, and the precursor air source is connected outside the cavity, which reduces the number of joints inside the cavity and reduces the risk of leakage and particle precipitation from the joints inside the cavity.
[0066] The gas interface is located outside the cavity, reducing the number of sealing joints inside the cavity, lowering the probability of gas leakage and particle generation from internal components, and improving wafer process yield.
[0067] The rotating motor 54 drives the rotating shaft 53 to rotate, causing the spray head 52 to rotate to the atomic layer deposition area above the wafer. TiCl4 and NH3 are respectively delivered to the spray head 52 through the gas interface outside the cavity and through the independent first gas pipe and second gas pipe inside the rotating shaft 53. They are released onto the wafer surface in alternating pulses according to the atomic layer deposition (ALD) process sequence, and a titanium nitride diffusion barrier layer is generated by self-limiting surface reaction. After the process is completed, the rotating motor 54 drives the rotating shaft 53 in the opposite direction to rotate the spray head 52 back to the storage position without interfering with the PVD sputtering process.
[0068] This solves the technical problems in the air supply structure of the rotatable spray head, such as the easy aging and leakage of the hoses arranged in the chamber, the easy generation of particulate pollution from the many internal joints, and the damage to the motor caused by the corrosive environment of the chamber, thus ensuring the stable and reliable implementation of the atomic layer deposition titanium nitride process.
[0069] As an optional embodiment, the chemical vapor deposition apparatus 7 is disposed at the top of the second deposition chamber 2, and a fixed stage is disposed inside the second deposition chamber 2. The chemical vapor deposition apparatus 7 includes a gas spray head, which is connected to a tungsten deposition gas source; the tungsten deposition gas source includes an H2 gas source and a WF6 gas source.
[0070] The aforementioned fixed stage is a heating base inside the second deposition chamber 2 used to support the wafer. Its position is fixed, and it can heat the wafer to provide the reaction temperature for the chemical vapor deposition of tungsten.
[0071] The aforementioned gas spray head is a porous gas supply component fixedly installed at the top of the chamber, which evenly distributes and sprays the tungsten deposition gas onto the wafer surface. This tungsten deposition gas source is used to achieve the process gas combination for tungsten film chemical vapor deposition.
[0072] Specifically, WF6 gas source can be selected as the tungsten precursor gas source, and H2 gas source as the reduction reaction gas source. The WF6 gas source provides tungsten element, and the H2 gas source acts as a reducing agent. The two are introduced according to the process sequence to undergo a reduction reaction to generate a tungsten film, thus completing the filling of the contact vias.
[0073] The chemical vapor deposition equipment 7 is arranged on top of the second deposition chamber 2. The fixed stage supports the wafer, and the wafer position is kept fixed to adapt to the deposition process of thermal chemical vapor deposition (CVD) tungsten.
[0074] The chemical vapor deposition equipment 7 includes a gas spray head, which is connected to a tungsten deposition gas source. The gas spray head receives the tungsten deposition gas source and distributes the process gas evenly downwards to the wafer surface, thereby achieving uniform film formation on the entire wafer surface.
[0075] The wafers with completed PVD-Ti and ALD-TiN thin film preparations are fed into the second deposition chamber 2 and placed on a fixed stage. WF6 and H2 tungsten deposition gases are delivered to the top gas spray head and uniformly sprayed onto the heated wafer surface. Tungsten hexafluoride is reduced by hydrogen gas, forming a tungsten nucleation layer and a main tungsten layer successively on the surface of the titanium nitride layer, completing the tungsten plug filling of the contact vias.
[0076] This embodiment also features a separate second deposition chamber specifically for tungsten chemical vapor deposition (CVD) filling, ensuring no interference with the process environment of the first deposition chamber 1 and avoiding cross-contamination. This achieves tungsten metal filling of the contact vias, resulting in low-resistance tungsten contact plugs that meet the conductivity requirements of the contact vias.
[0077] As an optional embodiment, a transfer device is provided between the first deposition chamber 1 and the second deposition chamber 2. The transfer device includes a vacuum transfer chamber and a vacuum manipulator disposed in the vacuum transfer chamber. The vacuum transfer chamber is connected to the first deposition chamber 1 and the second deposition chamber 2 through a vacuum gate valve.
[0078] The transfer device is responsible for transferring wafers between two process cavities, enabling wafers to move within the machine.
[0079] The aforementioned vacuum transfer cavity is a sealed vacuum chamber used solely for wafer transfer; it does not perform thin-film deposition processes and provides a vacuum environment for wafer transport. The vacuum robot is a multi-axis handling mechanism operating inside the vacuum transfer cavity. It relies on its end effector to lift the wafer edge to complete wafer pick-and-place operations, achieving wafer transfer in a vacuum environment.
[0080] The vacuum transfer chamber provides a vacuum environment for the transfer; the vacuum robot completes the wafer gripping and handling in a vacuum environment without contacting the atmosphere throughout the process.
[0081] The aforementioned vacuum gate valve, also known as a vacuum sealing valve, enables the connection or isolation between the vacuum transmission chamber and each deposition chamber, ensuring that the vacuum conditions of each chamber are independent.
[0082] When the vacuum gate valve is open, the vacuum robot can reach into the corresponding process chamber to pick up and place wafers; when the gate valve is closed, the vacuum transmission chamber is isolated from the process chamber, and each chamber can maintain its own process pressure without affecting each other.
[0083] When the process inside the first deposition chamber 1 is completed, the corresponding vacuum gate valve is opened; the vacuum robot extends into the first deposition chamber to pick up the wafer and withdraws from the vacuum transfer chamber; the vacuum gate valve on this side is closed, and then the vacuum gate valve leading to the second deposition chamber 2 is opened, and the robot sends the wafer into the second deposition chamber 2. After that, the robot retracts and the gate valve is closed; the wafer is in a vacuum environment from beginning to end and is not exposed to the atmosphere.
[0084] This solution addresses the technical problem of increased via resistance caused by vacuum oxidation during wafer transfer across cavities and equipment in traditional solutions. It also achieves isolation between different process cavities to prevent cross-contamination.
[0085] like Figures 5 to 9 As shown, this embodiment also provides a method for fabricating contact vias on a wafer, including: Step S1: Fix the wafer 6 to be processed onto the movable stage 3 of the first deposition chamber 1, and move it to the physical vapor deposition area below the target 43 of the physical vapor deposition equipment 4, and deposit a metal adhesion layer 91 on the etched via structure 61 on the wafer 6 to be processed; wherein, the physical vapor deposition equipment 4 is located at the top of the first deposition chamber 1, and the physical vapor deposition equipment 4 includes a magnetron 41, a cathode base 42 and a target 43 arranged in sequence.
[0086] Step S2: The spray head 52 of the atomic layer deposition equipment 5 is rotated out of the clearance cavity 11 of the first deposition chamber 1, and the movable stage 3 is moved to the atomic layer deposition area below the spray head 52 to deposit a diffusion barrier layer 92 on the wafer 6 to be processed with the deposited metal adhesion layer 91; wherein, the atomic layer deposition equipment 5 is located on the side of the first deposition chamber 1, and the atomic layer deposition equipment 5 includes an input gas pipe 51 and a spray head 52. The input gas pipe 51 connects the deposition gas source to the spray head 52, and the spray head 52 is rotatably mounted on the clearance cavity 11 on the side.
[0087] Step S3: The wafer 6 to be processed with the diffusion barrier layer 92 deposited is transferred to the second deposition chamber 2 of the same machine, and a metal filling layer 93 is deposited to form a contact via through the chemical vapor deposition equipment 7; wherein, the second deposition chamber 2 is equipped with the chemical vapor deposition equipment 7 for chemical vapor deposition of the wafer 6 to be processed.
[0088] like Figure 5 and Figure 6 As shown, in step S1 above, the wafer 6 to be processed is fixed on the movable stage 3 and raised to the physical vapor deposition area; the top magnetron 41, cathode base 42, and target 43 work together to complete magnetron sputtering, depositing a metal adhesion layer 91 on the wafer surface with through-hole structure 61; the stage can be heated, and the titanium can react with the silicon substrate to generate metal silicide in situ during deposition.
[0089] like Figure 7 As shown, in step S2 above, the spray head 52 is rotated out of the clearance cavity 11 and positioned, and the movable stage 3 is moved to the atomic layer deposition area; the atomic layer deposition equipment 5 supplies a reaction gas source, and relies on the ALD self-limiting surface reaction to deposit a diffusion barrier layer 92 on the metal adhesion layer 91.
[0090] like Figure 8As shown, in step S3, the wafer is vacuum transferred to the second deposition chamber 2 inside the same machine; a tungsten deposition gas source is introduced into the chemical vapor deposition equipment 7, a gas phase reduction reaction occurs, a metal filling layer 93 is deposited, and the contact via is prepared.
[0091] Steps S1 and S2 sequentially prepare the metal adhesion layer 91 and the diffusion barrier layer 92 in the same first deposition chamber 1, reducing the occupancy of the process chamber; metal silicides can be formed in situ, eliminating the need for a separate silicide process, reducing process costs and pollution risks. The spray head 52 can be retracted and avoided, so as not to interfere with the PVD and ALD processes, ensuring the quality of film formation.
[0092] The wafer transfer is completed within the same machine, ensuring the wafer remains completely protected from atmospheric exposure, thus preventing film oxidation and reducing contact via resistance. A second deposition chamber completes the metal filling, resulting in a high-performance contact via structure. This overcomes the technical challenges of separate chamber processing for PVD-Ti and ALD-TiN, which involves numerous process steps, high equipment costs, and increased contact resistance due to easy exposure to atmospheric oxidation during wafer transfer.
[0093] As an optional embodiment, the spray head 52 of the atomic layer deposition apparatus 5 is rotated out of the clearance cavity 11 of the first deposition chamber 1, and the movable stage 3 is moved to the atomic layer deposition area below the spray head 52 to deposit a diffusion barrier layer 92 on the wafer 6 to be processed with the deposited metal adhesion layer 91. This includes: if the spray head 52 and the movable stage 3 do not interfere with each other, first rotating the spray head 52 out of the clearance cavity 11, and then moving the movable stage 3 to the atomic layer deposition area below the spray head 52; if the spray head 52 and the movable stage 3 interfere with each other, first moving the movable stage 3 to the atomic layer deposition area below the spray head 52, and then rotating the spray head 52 out of the clearance cavity 11.
[0094] The spray head 52 and the movable platform 3 operate in different ways under different action sequence logics in order to avoid collision interference between moving parts.
[0095] In the non-interference operation, the spray head 52 is first rotated out of the avoidance cavity 11 to prepare for deposition. Then, the movable stage 3 is driven to move to the atomic layer deposition area. In this way, the movable stage 3 can carry out deposition as soon as possible after it is in place, thereby further improving the coordination efficiency of physical vapor deposition (PVD) and atomic layer deposition (ALD) in the first deposition cavity 1.
[0096] When interference occurs, the movable stage 3 can be moved to a lower position in the atomic layer deposition zone before the spray head 52 is rotated out, thus avoiding collisions between their movement paths. For example... Figure 3 and Figure 4 As shown, the movable stage 3 can move up and down in the first deposition chamber 1, which reduces the space requirement of the first deposition chamber 1, saves space for the processing equipment, and reduces the size of the processing equipment.
[0097] Based on the spatial relationship between the rotation trajectory of the spray head 52 and the lifting stroke of the movable platform 3, this embodiment distinguishes between two scenarios: interference and non-interference. The sequence of component actions is set differently to ensure that the spray head and the platform do not collide during their movement, thus completing the ALD process.
[0098] By taking into account different equipment structures and layouts, the timing of actions can be flexibly selected to prevent mechanical collisions between the spray head 52 and the movable platform 3, thus protecting the precision components inside the chamber and improving the safety and process compatibility of equipment operation.
[0099] This addresses the technical problem of spatial interference risk between the rotation of the spray head and the lifting and lowering of the platform, which can easily lead to component collision damage.
[0100] As an optional embodiment, a metal adhesion layer 91 is first deposited on the etched via structure 61 on the wafer 6 to be processed, including: heating the movable stage 3 to a preset temperature and moving it to the physical vapor deposition region; turning on the sputtering power supply 44 to output power, inert gas ignition to form plasma, bombarding the target material 43 to sputter out metal titanium atoms; turning on the radio frequency bias power supply 8 to apply radio frequency bias to the wafer 6 to be processed, and at the preset temperature, the deposited metal titanium atoms react with the silicon substrate of the wafer 6 to be processed to generate metal silicide.
[0101] The stage is heated to the high temperature required for the silane reaction, while the workstation is raised to the PVD process position below the target 43. The sputtering power supply 44 supplies Ar gas for ignition, and argon ions bombard the titanium target to generate titanium atoms, achieving the deposition of the metal adhesion layer 91. Radio frequency bias control of ion bombardment improves film quality; the high-temperature environment causes the titanium to react in situ with the silicon substrate to form metal silicides.
[0102] Metal silicides are generated in situ in the same process as the deposited titanium adhesion layer, eliminating the need for a separate metal silicide process, shortening the process flow, and reducing the risks of particle and process fluctuations caused by additional processes; radio frequency bias improves the coverage of titanium layer steps and film adhesion, ensuring low-ohmic contact performance of contact vias.
[0103] This technology solves the technical problems of traditional metal silicide processes, which require separate processing steps, involve many steps, have high costs, and pose significant process risks, while also improving the quality of titanium film formation.
[0104] As an optional embodiment, the deposition of a diffusion barrier layer 92 on the wafer 6 to be processed with the deposited metal adhesion layer 91 includes: spraying TiCl4 vapor through a spray head 52 for a first preset pulse time, which reacts and adsorbs with the surface of the deposited metal adhesion layer 91, wherein the first preset pulse time is 0.5-3s; purging the chamber with an inert gas for a second preset pulse time to remove excess co-reacting gases and byproducts, wherein the second preset pulse time is 0.5-10s and the gas flow rate is 100-50000sccm; spraying NH3 gas through a spray head 52 for a first preset pulse time, which reacts and adsorbs with the deposited TiCl4 surface to generate the diffusion barrier layer 92, wherein the composition of the diffusion barrier layer is TiN; and purging the chamber with an inert gas for a second preset pulse time to remove excess co-reacting gases and byproducts.
[0105] This embodiment defines the complete cycle sequence and process parameters for ALD preparation of the TiN diffusion barrier layer, including sequentially performing TiCl4 pulse adsorption, inert gas purging, NH3 pulse reaction, and another inert gas purging, repeating this cycle to obtain a TiN film of the target thickness. The TiCl4 and NH3 pulse duration is limited to 0.5 seconds. 3s, purging time 0.5 10s, purge gas flow rate 100 50000sccm.
[0106] Utilizing the self-confined surface reaction mechanism of atomic layer deposition: TiCl4 is briefly introduced to saturate the surface of the metal adhesion layer. Subsequently, an inert gas purging process removes unadsorbed precursors and byproducts from the chamber. NH3 is then introduced to react with the adsorbed titanium-containing species on the surface, generating TiN. This process is repeated to remove residual reaction gases; multiple cycles are performed to grow a dense titanium nitride diffusion barrier layer layer by layer.
[0107] Controlled pulse duration and purging parameters ensure that the reaction occurs only on the wafer surface, resulting in a TiN film with excellent step coverage and uniform thickness. This effectively removes residual precursors and byproducts, reduces film impurities, improves the density of the barrier layer, and inhibits the downward diffusion of subsequent tungsten and fluorine sources.
[0108] This addresses the issues of poor shape retention, high impurity content, and ineffective diffusion blocking in high aspect ratio contact vias.
[0109] As an optional embodiment, the wafer 6 to be processed, with the diffusion barrier layer 92 already deposited, is transferred to the second deposition chamber 2 of the same machine. A metal filling layer 93 is deposited using a chemical vapor deposition (CVD) device 7 to form a contact via. This includes: transferring the wafer 6 to be processed to the second deposition chamber 2 using a vacuum robot, placing it on the fixed stage of the second deposition chamber 2, and heating the wafer 6 to be processed to a preset process temperature; introducing SiH4 gas and WF6 gas through a gas spray head to deposit a tungsten nucleation layer on the wafer 6; purging the chamber with inert gas according to a second preset pulse time to remove excess co-reacting gas and byproducts; and introducing H2 gas and WF6 gas through a gas spray head to grow a thick tungsten film filling via structure 61 on the tungsten nucleation layer to form a contact via.
[0110] The wafer is transferred to the second deposition chamber 2 via a vacuum robot and heated to the process temperature. First, SiH4 and WF6 are introduced to deposit a tungsten nucleation layer. Then, inert gas is purged from the chamber. Next, H2 and WF6 are introduced to grow a thick tungsten film on the tungsten nucleation layer, completing the via filling.
[0111] The wafer is transferred and heated under vacuum; SiH4 reduces WF6 to form a continuous ultrathin tungsten nucleation layer on the TiN surface; residual SiH4 and fluorine-containing byproducts in the chamber are removed by purging; then WF6 is reduced by H2 to grow a thick tungsten film on the nucleation layer, filling the through-hole structure 61 and forming a tungsten metal filling layer for contacting the through-hole.
[0112] Vacuum transport avoids wafer oxidation; the formation of a tungsten nucleation layer first facilitates uniform nucleation of the tungsten film; after nucleation, purging removes residual silane to avoid interfering with subsequent bulk tungsten deposition, reducing film roughness and resistivity, and achieving good filling of contact vias.
[0113] This addresses the problems of poor tungsten nucleation, residual precursors interfering with the deposition of bulk tungsten, resulting in through-hole filling defects and high contact resistance.
[0114] This embodiment also provides an optional implementation method, which will be described in detail below. This implementation method involves physical vapor deposition of titanium (PVD Ti) + atomic layer deposition of titanium nitride (ALD TiN) + chemical vapor deposition of tungsten (CVD W) for contact vias. The above process steps are performed using the cooperation of a first deposition chamber 1 and a second deposition chamber 2 to fabricate the contact vias. Specifically, the wafer is placed into the process chamber, and deposition begins according to the following steps.
[0115] 1) The 400℃ high-temperature substrate is raised to the PVD process position, the inert gas Ar is used for ignition, the DC power supply power and the substrate RF bias voltage are increased, and physical vapor deposition of metallic titanium begins. At the same time as the metallic Ti is deposited, the metallic Ti reacts with the substrate Si at high temperature to form metal silicide.
[0116] 2) The base is lowered to the ALD process position, and the moving spray head 52 is moved to a height of about 10mm directly above the wafer 6 to be processed.
[0117] 3) Pulse TiCl4 vapor into the cavity with a pulse time of 0.5s-3s to allow it to react chemically and be adsorbed on the surface of the depositable substrate.
[0118] 4) Purge the chamber with inert gas for 0.5-10 seconds at a flow rate of 100-50000 sccm to remove excess co-reacting gases and byproducts.
[0119] 5) NH3 gas is pulsed into the cavity with a pulse duration of 0.5s-3s, so that it reacts chemically and is adsorbed on the surface of the depositable substrate.
[0120] 6) Purge the chamber with inert gas for 0.5-10 seconds at a flow rate of 100-50000 sccm to remove excess co-reaction gases and byproducts.
[0121] Repeat steps 3) to 6) to control the film growth thickness by controlling the number of ALD cycles.
[0122] It should be noted that the term "comprising" and its variations used in the embodiments of the present invention are open-ended, meaning "including but not limited to". The term "based on" means "at least partially based on". The term "one embodiment" means "at least one embodiment"; the term "another embodiment" means "at least one additional embodiment"; the term "some embodiments" means "at least some embodiments". The modifications of "one" and "a plurality" mentioned in the embodiments of the present invention are illustrative and not restrictive, and those skilled in the art should understand that unless explicitly indicated otherwise in the context, they should be understood as "one or more".
[0123] The steps described in the method embodiments provided by the present invention can be performed in different orders and / or in parallel. Furthermore, the method embodiments may include additional steps and / or omit the steps shown. The scope of protection of the present invention is not limited in this respect.
[0124] The term "embodiment" in this specification refers to a specific feature, structure, or characteristic described in connection with an embodiment that may be included in at least one embodiment of the invention. The appearance of this phrase in various places in the specification does not necessarily imply the same embodiment, nor does it imply independence or alternativeity from other embodiments. The various embodiments in this specification are described in a related manner, with reference to each other for similar or identical parts. In particular, for apparatus, device, and system embodiments, since they are substantially similar to method embodiments, the description is relatively simple, and relevant details are referred to in the description of the method embodiments.
[0125] The embodiments described above are merely illustrative of several implementations of the present invention, and while the descriptions are specific and detailed, they should not be construed as limiting the scope of protection. It should be noted that those skilled in the art can make various modifications and improvements without departing from the concept of the present invention, and these all fall within the scope of protection of the present invention. Therefore, the scope of protection of the present invention should be determined by the appended claims.
Claims
1. An apparatus for fabricating contact vias on a wafer, characterized in that, include: The first deposition chamber (1) and the second deposition chamber (2) are set on the same machine. The first deposition chamber (1) is equipped with a movable stage (3), a physical vapor deposition device (4) and an atomic layer deposition device (5). The physical vapor deposition apparatus (4) is located at the top of the first deposition chamber (1). The physical vapor deposition apparatus (4) includes a magnetron (41), a cathode base (42) and a target (43) arranged in sequence. The area below the target (43) is the physical vapor deposition zone. The atomic layer deposition apparatus (5) is located on the side of the first deposition chamber (1). The atomic layer deposition apparatus (5) includes an input gas pipe (51) and a spray head (52). The input gas pipe (51) connects the deposition gas source to the spray head (52). The spray head (52) is rotatably mounted on the side clearance chamber (11). When the spray head (52) rotates out of the clearance chamber (11), the area below the spray head (52) is the atomic layer deposition area. The movable stage (3) is used to support the wafer (6) to be processed, the wafer (6) to be processed includes etched through-hole structures (61), and the movable stage (3) moves between the physical vapor deposition region and the atomic layer deposition region; The second deposition chamber (2) is equipped with a chemical vapor deposition device (7) for performing chemical vapor deposition on the wafer (6) to be processed.
2. The preparation apparatus according to claim 1, characterized in that, The target material (43) of the physical vapor deposition equipment (4) is titanium metal, and the cathode base (42) is connected to the sputtering power supply (44); The movable stage (3) has a built-in heating component for heating the wafer (6) to be processed; the movable stage (3) is also provided with an electrostatic adsorption device for electrostatic adsorption of the wafer (6) to be processed; the movable stage (3) is connected to an RF bias power supply (8) for applying an RF bias to the wafer (6) to be processed during physical vapor deposition.
3. The preparation apparatus according to claim 1, characterized in that, The gas source of the atomic layer deposition equipment (5) includes a TiCl4 gas source and an NH3 gas source; The spray head (52) is connected to the rotating motor (54) via the rotating shaft (53). The rotating motor (54) is located outside the first deposition chamber (1). The input gas pipe (51) includes a first gas pipe and a second gas pipe that are respectively connected to the TiCl4 gas source and the NH3 gas source. The first gas pipe and the second gas pipe are both located inside the rotating shaft (53). The rotating shaft (53) is provided with a gas passage interface for the first gas pipe and the second gas pipe at one end near the rotating motor (54). The gas passage interface is located outside the first deposition chamber (1) and is connected to the corresponding gas source.
4. The preparation apparatus according to claim 1, characterized in that, The chemical vapor deposition device (7) is located at the top of the second deposition chamber (2). A fixed stage is provided inside the second deposition chamber (2). The chemical vapor deposition device (7) includes a gas spray head, which is connected to a tungsten deposition gas source. The tungsten deposition gas source includes an H2 gas source and a WF6 gas source.
5. The preparation apparatus according to claim 1, characterized in that, A transfer device is provided between the first deposition chamber (1) and the second deposition chamber (2). The transfer device includes a vacuum transfer chamber and a vacuum manipulator provided in the vacuum transfer chamber. The vacuum transfer chamber is connected to the first deposition chamber (1) and the second deposition chamber (2) through a vacuum gate valve.
6. A method for fabricating contact vias on a wafer, characterized in that, include: The wafer to be processed (6) is fixed on the movable stage (3) of the first deposition chamber (1) and moved to the physical vapor deposition area below the target (43) of the physical vapor deposition equipment (4). A metal adhesion layer (9) is deposited on the etched through-hole structure (61) on the wafer to be processed (6). The physical vapor deposition equipment (4) is located at the top of the first deposition chamber (1) and includes a magnetron (41), a cathode base (42) and a target (43) arranged in sequence. The spray head (52) of the atomic layer deposition apparatus (5) is rotated out of the clearance cavity (11) of the first deposition chamber (1), and the movable stage (3) is moved to the atomic layer deposition area below the spray head (52) to deposit a diffusion barrier layer (92) on the wafer (6) to be processed with the deposited metal adhesion layer (91); wherein, the atomic layer deposition apparatus (5) is located on the side of the first deposition chamber (1), the atomic layer deposition apparatus (5) includes an input gas pipe (51) and a spray head (52), the input gas pipe (51) connects the deposition gas source to the spray head (52), and the spray head (52) is rotatably mounted on the clearance cavity (11) on the side; The wafer (6) to be processed with the diffusion barrier layer (92) deposited is transferred to the second deposition chamber (2) of the same machine, and a metal filling layer (93) is deposited by the chemical vapor deposition equipment (7) to form contact vias; wherein, the second deposition chamber (2) is provided with the chemical vapor deposition equipment (7) for chemical vapor deposition on the wafer (6) to be processed.
7. The preparation method according to claim 6, characterized in that, Rotate the spray head (52) of the atomic layer deposition apparatus (5) out of the clearance cavity (11) of the first deposition chamber (1), and move the movable stage (3) to the atomic layer deposition area below the spray head (52) to deposit a diffusion barrier layer (92) on the wafer (6) to be processed that has been deposited with a metal adhesion layer (91), including: Without interference between the spray head (52) and the movable stage (3), the spray head (52) is first rotated out of the clearance cavity (11), and then the movable stage (3) is moved to the atomic layer deposition area below the spray head (52). In the event of interference between the spray head (52) and the movable stage (3), the movable stage (3) is first moved to the atomic layer deposition area below the spray head (52), and then the spray head (52) is rotated out of the clearance cavity (11).
8. The preparation method according to claim 7, characterized in that, A metal adhesion layer (91) is first deposited on the etched via structure (61) on the wafer to be processed (6), including: The movable stage (3) is heated to a preset temperature and moved to the physical vapor deposition zone; Turn on the sputtering power supply (44) to output power, the inert gas ignites to form plasma, and bombards the target material (43) to sputter out metallic titanium atoms; Turn on the radio frequency bias power supply (8) and apply radio frequency bias to the wafer to be processed (6). At the preset temperature, the deposited titanium atoms react with the silicon substrate of the wafer to be processed (6) to generate metal silicide.
9. The preparation method according to claim 7, characterized in that, Deposition of a diffusion barrier layer (92) on the wafer (6) to be processed with the deposited metal adhesion layer (91) includes: According to the first preset pulse time, TiCl4 vapor is sprayed out through the spray head (52) and reacts chemically with and adsorbs on the surface of the deposited metal adhesion layer (91). The first preset pulse time is 0.5-3s. According to the second preset pulse time, the chamber is purged with inert gas to remove excess co-reaction gas and byproducts. The second preset pulse time is 0.5-10s and the gas flow rate is 100-50000sccm. According to the first preset pulse time, NH3 gas is sprayed out through the spray head (52) and reacts chemically with and adsorbs on the surface of deposited TiCl4 to generate a diffusion barrier layer (92), the composition of which is TiN; According to the second preset pulse time, the chamber is purged with inert gas to remove excess co-reaction gases and byproducts.
10. The preparation method according to claim 7, characterized in that, The wafer (6) with the pre-deposited diffusion barrier layer (92) is transferred to the second deposition chamber (2) of the same machine, and a metal filling layer (93) is deposited through a chemical vapor deposition device (7) to form contact vias, including: The wafer (6) to be processed is transferred to the second deposition chamber (2) by a vacuum robot, placed on the fixed stage of the second deposition chamber (2), and the wafer (6) to be processed is heated to the preset process temperature; SiH4 gas and WF6 gas are introduced through a gas spray head to deposit a tungsten nucleation layer on the wafer to be processed (6); According to the second preset pulse time, the chamber is purged with inert gas to remove excess co-reaction gas and byproducts; H2 gas and WF6 gas are introduced through a gas spray head to grow a thick tungsten film filling through-hole structure (61) in the tungsten nucleation layer, forming contact through-holes.