A method for forming weakening lines in a planar wafer and a cutting machine thereof.
By using a method of irradiating with higher laser power near the intersection of wafers and lower laser power in the middle, orthogonal grid weakening lines are formed, solving the problem of chip strength reduction caused by subsurface cutting, and achieving improved chip strength and effective wafer separation.
Patent Information
- Application Number
- CN202610630695.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-05-09
- Publication Date
- 2026-11-17
AI Technical Summary
Existing subsurface dicing techniques may reduce chip strength when forming weakening lines, especially after internal modification of wafer materials.
By controlling the irradiation process of the laser beam, higher laser power is used near the intersection of the weakening lines and lower laser power is used in the middle part to form an orthogonal grid arrangement of weakening lines, thus ensuring the improvement of chip strength.
While maintaining effective wafer separation, it improves chip strength and reduces damage to materials inside the wafer.
Smart Images

Figure CN123124695A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to a method for forming weakening lines in a planar wafer, and a dicing machine for forming weakening lines in a planar wafer, wherein multiple weakening lines are arranged in an orthogonal grid. Background Technology
[0002] Slicing and dicing are known processes in the semiconductor industry, in which dicing machines are used to process workpieces or substrates, such as semiconductor wafers, which may contain, but are not limited to, silicon, or metal and / or ceramic wafers. In this specification, the term "wafer" is used to encompass all these products. In a dicing process (e.g., also called cutting, separating, dicing), the wafer is completely cut, thereby dividing the wafer into individual chips. In a dicing process (e.g., also called grooving, scoring, slotting, or trenching), channels or grooves are cut into the wafer. Any of these processes can be performed mechanically, for example using a diamond saw, or using laser cutting methods, both of which are now well-established technologies.
[0003] Other processes can then be applied, such as using a physical saw to completely bisect the diced wafer along the cut channels.
[0004] Another increasingly popular method is to use "subsurface dicing" (sometimes also called "stealth dicing"). This subsurface dicing technique divides the wafer into chips by internally altering the wafer substrate material to form weakening lines, and then applying mechanical force to induce cracks that cause the chips to separate along the weakening lines.
[0005] Depending on the substrate material and its thickness, one or more modification layers can be created along the weakening line to sufficiently weaken the material, thereby inducing cracks and separating the chip. Subsurface dicing uses a reflective spatial light modulator (SLM) to simultaneously create one or more modification layers in the substrate material.
[0006] Furthermore, the laser can be modulated by SLM to minimize laser aberrations at predetermined locations within the substrate material.
[0007] Figure 1 A basic planar wafer 1 is schematically shown above, which has been processed using a subsurface dicing process. (See diagram below.) Figure 1As shown, wafer 1 is provided with a plurality of electronic devices 2 arranged in a regular orthogonal array, such that straight channels 6 extend between the devices 2. Subsurface lines 3 are formed along these channels 6 using an incident laser, which is directed into the interior of the wafer, such that each device 2 is separated from its adjacent device 2 by the lines 3. In other words, the lines 3 define an orthogonal grid. The wafer material near each line 3 is relatively weaker than the other materials on the wafer; in other words, the lines 3 form weakening lines in the planar wafer 1. It should be noted that the lines 3 may actually be invisible and are shown here only for clarity. A subsequent mechanical fracture step (not shown) thereby physically separates the devices 2.
[0008] US10328521B2, EP2325689B1 and EP2186596B1 refer to exemplary prior art.
[0009] Subsurface dicing offers several advantages, including avoiding the cut loss or heat loss that can occur in laser cutting. Furthermore, it eliminates the need for wafer cooling, such as using liquid coolants, making the process completely dry. Additionally, subsurface dicing is suitable for very thin wafers, which is becoming increasingly important in industry.
[0010] However, there are also related drawbacks, particularly the possibility that subsurface dicing can lead to lower chip strength due to modifications to the interior of the wafer material. These modifications weaken the sidewalls and reduce chip strength. Summary of the Invention
[0011] The present invention aims to provide an improved method for forming weakening lines within a planar wafer, which enables the production of chips with improved chip strength.
[0012] According to the present invention, this objective is achieved by controlling the irradiation process to maximize irradiation near the "intersection" or intersection of the weakening lines.
[0013] This method can be used simultaneously for both subsurface and surface scribing methods. Furthermore, the method can be extended to use drilling, as further described below.
[0014] According to a first aspect of the present invention, a method is provided for forming weakening lines in a planar wafer, wherein a plurality of weakening lines are arranged in an orthogonal grid to prepare for a mechanical fracture step of breaking the planar wafer along the plurality of weakening lines, the method comprising the following steps: At least one laser beam is used to irradiate multiple portions of the planar wafer, each portion coinciding with a weakening line to be formed in the planar wafer, the multiple portions comprising: The intersecting portion, which is near the intersection of the orthogonal grids; and The middle section, which is located between adjacent intersecting sections; The intersecting portion is irradiated with a first average laser power, the middle portion is irradiated with a second average laser power, and the first average laser power is greater than the second average laser power.
[0015] According to a second aspect of the present invention, a method is provided for forming weakening lines in a planar wafer, wherein a plurality of devices are formed on the planar wafer in a regularly orthogonal array, the plurality of devices being spaced apart by channels, the method comprising: The channel is irradiated with at least one laser beam to weaken the planar wafer; The portion of the channel near the intersection of the channels is irradiated with a first average laser power, the portion of the channel between the intersections is irradiated with a second average laser power, and the first average laser power is greater than the second average laser power.
[0016] According to a third aspect of the present invention, a dicing machine for forming weakening lines in a planar wafer is provided, wherein a plurality of weakening lines are arranged in an orthogonal grid, the dicing machine comprising: Control device; A laser irradiation device adapted to focus a laser beam toward the planar wafer; and A conveying device for moving the planar wafer and the laser irradiation device relative to each other along a path parallel to the plane of the planar wafer; The control device is adapted to control the laser irradiation device and the transmission device to subject the intersection portion of the planar wafer to a first average laser power and the middle portion of the planar wafer to a second average laser power, wherein the intersection portion is close to the intersection point of the orthogonal grid, the middle portion is located between adjacent intersection portions, and the first average laser power is greater than the second average laser power. Attached Figure Description
[0017] The invention will now be described with reference to the accompanying drawings (not to scale), in which: Figure 1 The image above schematically illustrates a wafer using a known subsurface dicing process; Figure 2 An exemplary subsurface cutting apparatus for performing the method of the present invention is shown schematically from the side. Figure 3 A wafer processed according to an embodiment of the present invention is illustrated schematically; Figure 4A The diagram schematically illustrates the use of a single laser beam, according to... Figure 3 A portion of the wafer processed in the embodiment; Figure 4B The diagram schematically illustrates the use of multiple sub-beams, based on... Figure 3 A portion of the wafer processed in the embodiment; Figure 5 A wafer processed according to a second embodiment of the present invention is schematically shown from above; Figure 6A The diagram schematically illustrates the use of a single laser beam, according to... Figure 5 A portion of the wafer processed in the embodiment; Figure 6B The diagram schematically illustrates the use of multiple sub-beams, based on... Figure 5 A portion of the wafer processed in the embodiment; Figure 7 A wafer processed according to a fourth embodiment of the present invention is schematically shown from above; Figure 8 The diagram above, in an axonometric view, schematically illustrates the... Figure 7 A magnified portion of the wafer processed in the example; Figure 9 A wafer processed according to another embodiment of the present invention is schematically shown from above; Figure 10 This is shown schematically from the side according to Figure 9 A portion of the wafer processed in the embodiment; Figure 11 A wafer processed according to another embodiment of the present invention is schematically shown above; and Figure 12 This is shown schematically from the side according to Figure 11 A portion of the wafer processed in the example. Detailed Implementation
[0018] Figure 2 An exemplary subsurface cutting apparatus 10 for performing the method of the present invention is shown schematically from the side.
[0019] A laser source 11 is arranged to output a laser beam 12, which is guided along the optical path to wafer 1 via a first reflector 13 and a second reflector 14. A beam shaper 15, such as a diffractive optical element (DOE), a spatial light modulator, etc., is located in the optical path to generate an illumination pattern of incident laser light including various sub-beams 16. Each sub-beam 16 is focused by a respective focusing lens 17 to a focal point located within wafer 1. As shown, each sub-beam 16 is focused to a focal point at different depths of wafer 1. The laser source 11 is selected such that the laser beam 12 it generates can ablate the material of wafer 1. For example, a suitable laser source 11 can generate a laser beam with a wavelength in the range of about 1000 nm to 1500 nm, having: i) The pulse duration is in the range of approximately 1 ns to approximately 100 ns at approximately 5-50 kHz, and the output power is in the range of approximately 0.25 W to approximately 2.5 W; or ii) At approximately 5 to 50 kHz, the output power ranges from approximately 0.1 W to approximately 2 W, with a range of approximately 0.25 ps to approximately 25 ps.
[0020] In this embodiment, wafer 1 and the flexible sheet 4 supporting it are located on chuck 18, which is drivable in a horizontal (XY) plane (as indicated by the large arrow), thus constituting a transport device for moving the planar wafer and the laser irradiation device relative to each other along a path parallel to the plane of wafer 1. The laser irradiation device or laser assembly, namely laser source 11, first mirror 13, second mirror 14, beam shaper 15, and focusing lens 17, remains stationary, while chuck 18 moves wafer 1 relative to the incident laser along a path parallel to the plane of wafer 1. While wafer 1 is irradiated by the incident laser, the relative movement along the translational direction of the path is used to form a line in wafer 1 along which the wafer material is photomodified by the irradiation. Each such irradiation line corresponds to a weakening line formed in wafer 1.
[0021] In other embodiments (not shown), wafer 1 may remain stationary while laser beam 12 is translated, or both wafer 1 and laser beam 12 may be translated. Furthermore, although the illustrated dicing apparatus 10 divides laser beam 12 into three independent sub-beams 16, this is not essential to the invention; in practice, only a single laser beam with a single corresponding focal point in wafer 1 is needed. However, in some cases, using multiple (e.g., at least two) such sub-beams may be advantageous.
[0022] The device includes a control unit 5, which may include, for example, a processor, a computer, etc., and may be located at the machine or remotely but in communication with it (e.g., cloud-based software), which controls the operation of the machine.
[0023] According to the present invention, this device can be used in the following ways: First, it is necessary to determine the locations where weakening lines will be formed on planar wafer 1, and to determine the start and end positions for each weakening line. For this type of application, the weakening lines will typically be formed at... Figure 1 The orthogonal grid pattern shown is formed, in which each weakening line will be located at an equidistant point between adjacent devices 2. The start and end points of each weakening line are typically located at opposite edges of wafer 1, which means that weakening lines are formed on the entire surface of wafer 1.
[0024] Then, using the aforementioned device, the planar wafer 1 and the laser assembly are moved relative to each other along a path parallel to the plane of wafer 1 from a position near the start position of each weakening line to a position near the end position of each weakening line.
[0025] The above steps are standard procedures in the art. However, according to the present invention, while the planar wafer 1 and the laser device are moving relative to each other, a first average laser power is applied to the planar wafer 1 along a first portion of the path, and a second average laser power is applied along a second portion (non-overlapping portion) of the path, wherein the first average laser power is greater than the second average laser power, so as to weaken the wafer 1 along the path between the starting position and the ending position.
[0026] Here, the term "average laser power" is used to refer to the time-averaged laser power that is substantially independent of the pulse time and / or wavelength of the laser used. Typically, average laser power can be expressed as the RMS or "root mean square" power of the laser beam.
[0027] Therefore, in the case where the laser beam includes a pulsed laser beam with a pulse period, the first part is irradiated for a first time period, the second part is irradiated for a second time period, and both the first time period and the second time period are longer than the pulse period.
[0028] Within the scope of this method, various types of weakening lines can be formed. Now, refer to... Figures 3 to 8 Describe some basic examples.
[0029] For clarity, the following discussion will be conducted: The term "path" refers to the relative travel path between wafer 1 and the laser device; The term "channel" refers to the narrow gap between rows and columns of devices in an orthogonal array; The term "weakening line" refers to the entire line along the path of wafer 1. Importantly, the weakening line does not necessarily include the region of wafer 1 modified by irradiating the entire weakening line with laser light; and The term "irradiation line" refers to a portion of the weakening line where laser light is irradiated onto wafer 1.
[0030] Therefore, in this context, a weakening line can include multiple non-overlapping single illumination lines.
[0031] Figure 3 A planar wafer 1 processed by the subsurface dicing method according to a first embodiment of the present invention is shown. For consistency, the wafer 1 shown is similar to... Figure 1A wafer 1 has devices 2 arranged in an identical orthogonal array thereon, separated by channels 6. In this embodiment, a subsurface dicing process is used to generate multiple weakening lines coinciding with channels 6, as described in more detail below, and these are repeated at different locations on wafer 1 as needed to re-form an orthogonal grid. However, in this embodiment, in the central region of wafer 1, laser energy is applied only to the first portion of channels 6 / weakening lines of wafer 1, i.e., at irradiation line 23, at the intersection 33 of the orthogonal grid, i.e., the area where weakening lines extending parallel to the Y-axis and extending parallel to the X-axis intersect in the orthogonal grid, the X and Y axes being orthogonal to each other and extending parallel to the plane of wafer 1, thus forming a cross shape. Therefore, each intersection 33 is close to the corner of at least one adjacent device 2, but far away from the weakening line portion located between adjacent devices 2 in a row or column (hereinafter referred to as the "middle portion"). It should be noted that the irradiation line 23 and the intersection 33 may actually be invisible, and are shown here only for clarity. By limiting the extension of the irradiation line 23 in this way, little or no damage is caused to the wafer 1 in the region between adjacent devices 2 (i.e., the middle portion). However, it has been found that satisfactory chip separation can still be achieved even with such a reduced total length of the irradiation line 23 along the weakening line. In this central region, the irradiated portion can be approximately 20% to 50% of the expected chip size.
[0032] exist Figure 3 In the outer region of wafer 1, namely near its outer edge and between the outer edge and the radially outermost device 2, the irradiation line 23 remains fully formed because this facilitates separation without affecting the chip intensity near any device 2. However, this configuration is entirely optional, and in other embodiments, this outer region may not be treated in this way.
[0033] Figure 4A The diagram schematically illustrates the use of a single laser beam, according to... Figure 3 A portion of wafer 1 processed in the embodiment. More specifically, Figure 4A The portion of wafer 1 shown is along Figure 3The line AA shown is taken from the central region of wafer 1, which includes a portion of the nearest weakening line. It can be seen that the irradiation line 23 is entirely within the body of wafer 1, i.e., completely internal and spaced apart from the top and bottom surfaces of wafer 1. Furthermore, the irradiation line 23 is primarily located away from the individual devices 2, resulting in minimal lateral overlap between the irradiation line 23 and the devices 2. In some embodiments (not shown), overlap may not be necessary at all, depending on factors such as the thickness and material of wafer 1. Additionally, in this embodiment, the wafer is not irradiated (i.e., zero) at portions of the path or weakening line between adjacent irradiation lines 23 (i.e., the middle portion). For clarity, each irradiation line 23 includes a first portion of the path / weakening line / channel 6, i.e., an intersection portion, where wafer 1 experiences a relatively high average laser power, while at portions of the path between each irradiation line 23 (i.e., the middle portion), wafer 1 experiences a relatively low average laser power, which is zero. Furthermore, the path includes multiple first portions (intersection portions, i.e., irradiation lines 23) intersecting with multiple second portions (middle portions).
[0034] Figure 4B The diagram schematically illustrates the use of multiple sub-beams 16, according to... Figure 3 A portion of wafer 1 processed in the embodiment, viewed similarly Figure 4A In this case, something like... Figure 2 The cutting apparatus 10 shown splits the laser beam 12 output from the laser source 11 into three sub-beams 16, each focused at a different depth on the wafer 1, thereby producing vertically spaced irradiation lines 23A, 23B, and 23C. The irradiation arrangement is consistent with... Figure 4A Similar to that. Different numbers of sub-beams can be used as needed.
[0035] In this embodiment, the average laser energy applied to the wafer in the middle section is zero, which can be achieved in several ways. For example, one possibility is to directly adjust the output power of the laser source 11 to change the average laser power output by the laser source 11. In this case, the average laser power in the middle section is zero, which is similar to turning off the laser source 11 in these sections of the path. Another possibility is to provide a beam modulator disposed in the optical path of the generated laser beam 12, located between the laser source 11 and the internal focal point of the wafer 1. The average laser power of the generated laser beam 12 can then be changed by controlling the beam modulator. A suitable beam modulator can be used for this purpose. A simple mechanical example may include a so-called "optical chopper," which may include a rotating opaque disk having a light-transmitting window in a sector of the disk, the disk being placed in the optical path and rotated such that the light-transmitting sector periodically moves in and out of the optical path. When the laser beam 12 is incident on the transparent sector, virtually all laser energy is transmitted through; however, when the laser beam 12 is incident on a portion of the disk away from the sector, the laser beam 12 is blocked, and no laser energy is transmitted through. Other forms of movable optical barriers can also be used. The laser beam 12 can also be modulated equivalently using other tools, such as switchable optics, beam shapers, beam deflectors, etc.
[0036] These two modulation techniques can also be used to provide a non-zero average laser power to wafer 1 in the middle section, which is lower than the average laser power received by wafer 1 at the intersection. For example, a disk similar to the one described above can be used, in which a partially transparent fan-shaped area is provided so that some (but not all) of the incident laser energy is scattered. Similarly, other modulation devices can also be used to provide the desired non-zero average laser power, which is well known in the art.
[0037] Figure 5 A planar wafer 1 processed according to a method of a second embodiment of the present invention is shown. For consistency, the wafer 1 shown is similar to... Figure 1 A wafer 1 has devices 2 arranged in an identical orthogonal array thereon, separated by channels 6. In this embodiment, a subsurface dicing process is used to generate multiple weakening lines coinciding with channels 6, as described in more detail below, and these lines are repeated at different locations on wafer 1 as needed to re-form an orthogonal grid. In this embodiment, a relatively high average laser power is applied to wafer 1 at the first portion of the weakening lines (i.e., the intersection 43 of the orthogonal grid) in the central region of wafer 1. The intersection 43 is the region where weakening lines extending parallel to the Y-axis and extending parallel to the X-axis intersect in the orthogonal grid. The X-axis and Y-axis are orthogonal to each other and extend parallel to the plane of wafer 1 (i.e., similar to...). Figure 3The intersection 33). In the second part 44 of the path, located between adjacent intersections 43 in the weakening line, a relatively low average laser power is applied to wafer 1. By limiting the extension range of the relatively high power irradiation in this way, little or no damage is caused to wafer 1 in the region between adjacent devices 2. However, with Figure 3 Compared to the embodiment shown, applying non-zero average laser power to the middle portion 44 facilitates the fracture of wafer 1.
[0038] It should be noted that the weakening lines may actually be invisible; they are shown here only for clarity.
[0039] exist Figure 5 In the outer region of wafer 1, i.e., near its outer edge, between the outer edge and the radially outermost device 2, an irradiation line 45 formed using a relatively high average laser power is created, as this facilitates separation without affecting the chip intensity near any device 2. However, this configuration is entirely optional, and in other embodiments, this outer region may not be treated in this way.
[0040] Figure 6A The diagram schematically illustrates, from the side, the use of a single laser beam or alternatively, multiple laser beams, and alternative laser power modulation methods using the methods described above, based on... Figure 5 A portion of wafer 1 processed in the embodiment. More specifically, Figure 6A The portion of wafer 1 shown is along Figure 5 The line AA shown is taken from the central region of wafer 1, which includes a portion of the nearest weakening line. It can be seen that the weakening line is entirely within the body of wafer 1, i.e., completely internal and spaced apart from the top and bottom surfaces of wafer 1. Furthermore, the first portion with relatively high average power, i.e., at the intersection 43, is primarily located away from the corresponding device 2, resulting in minimal lateral overlap between the intersection 43 and device 2. In some embodiments (not shown), overlap may not be necessary at all, depending on, for example, the thickness and material of wafer 1. In this embodiment, some relatively low power irradiation exists in the intermediate portion 44 between adjacent intersections 43.
[0041] In this embodiment, this power modulation between the intersection and the middle portion can be achieved not by modulating the power of the laser beam 12 or the laser source 11 (both of which can remain constant throughout the process), but by adjusting the relative moving speed between the wafer 1 and the laser irradiation device, i.e., for Figure 6A The weakening line shown is parallel to Figure 5The X-axis direction is shown. More specifically, by appropriately controlling the conveying device, the relative movement speed of the intersections along the path can be made lower than the speed along the middle section of the path. In this way, the laser energy received per unit length in the intersection 43 will be greater than the laser energy received per unit length in the middle section 44.
[0042] Figure 6B The diagram schematically illustrates the use of multiple sub-beams 16, according to... Figure 5 A portion of wafer 1 processed in the embodiment, viewed similarly Figure 6A In this case, something like... Figure 2 The dicing apparatus 10 shown splits a laser beam 12 output from a laser source 11 into three sub-beams 16, each focused to a different depth on the wafer 1, thereby producing vertically spaced illumination lines 46A, 46B, and 46C. In this embodiment, one of the sub-beams 16 forming illumination line 46B remains continuously on with a constant average laser power throughout the path. However, the other sub-beams 16 forming illumination lines 46A and 46C are modulated so that a non-zero average laser power is applied only in the first portion and a zero average laser power is applied in the second portion 44. This modulation can be achieved, for example, using a modulation device in the optical path of the respective sub-beam 16, as generally described above. This arrangement will again produce a weakening line having intersecting intersections and intermediate portions in the path, wherein the total average laser power applied to the wafer 1 at the intersections is greater than the total average laser power applied to the wafer 1 at the intermediate portions 44.
[0043] The embodiments described so far relate to subsurface dicing methods in which an irradiating laser beam is focused inside the wafer. However, the invention is not limited thereto, and the two embodiments described below use alternative methods.
[0044] Figure 7 The wafer 1, processed according to the fourth embodiment of the present invention, is schematically shown from above. Figure 8 A magnified portion of wafer 1 is schematically shown from above in an isometric view. In this embodiment, a surface scribing technique is used. Surface scribing using a laser is well known, and in this technique, an irradiating laser beam (or multiple laser beams) is directed to the upper surface of the wafer, resulting in the formation of grooves that extend into the wafer body but do not extend through the entire thickness of the wafer. For this type of scribing process, an ultraviolet laser source can be used, which is well known in the art. Except that the grooves are formed near the upper surface of wafer 1 rather than inside it, this embodiment is similar to... Figure 3 In one embodiment, an illumination line 55 coinciding with channel 6 is formed using a laser beam (or multiple laser beams), and these illumination lines 55 form an intersection 53 in the central region of wafer 1. Figure 3Similar to the embodiment, the intersection 53 is the region in the orthogonal grid where a weakening line extending parallel to the Y-axis and a weakening line extending parallel to the X-axis intersect. The X-axis and Y-axis are orthogonal to each other and extend parallel to the plane of wafer 1, thus forming a cross shape. The intersection 53 is located near the corner of at least one adjacent device 2, but away from the middle portion of the weakening line located between adjacent devices 2 in a row or column.
[0045] exist Figure 7 In the outer region of wafer 1, namely near its outer edge and between the outer edge and the radially outermost device 2, the irradiation line 55 remains fully formed because this facilitates separation without affecting the chip intensity near any device 2. However, this configuration is entirely optional, and in other embodiments, this outer region may not be treated in this way.
[0046] In related embodiments (not shown), similar methods as described above can be used. Figure 5 The method described. In other words, the cross portion 53 can be formed using one or more irradiating laser beams with relatively high average power, while the remaining middle portion of the weakened line can be formed using one or more irradiating laser beams with relatively low average laser power. This can be achieved in several ways. For example, if multiple irradiating laser beams are used to generate the cross portion 53, one or more of these multiple laser beams can be "turned off" (similar to...) when dicing the middle region of the weakened line. Figure 6B (as in the embodiments), or the laser can be modulated to reduce the irradiation power in these intermediate regions (similar to...). Figure 6A (Example).
[0047] Figure 9 The wafer 1, processed according to another embodiment of the present invention, is schematically shown from above. Figure 10 A portion of wafer 1 is schematically shown from the side.
[0048] In this embodiment, each intersection 63 is formed by a plurality of discrete, closely spaced individual boreholes 66. For example... Figure 10 As shown, each drill hole 66 can extend through the entire thickness of wafer 1. The drill holes 66 are formed by laser drilling. As is known per se, laser drilling can be achieved by directing the laser beam to irradiate a point on wafer 1 without relative movement between wafer 1 and the laser beam. As is known per se, this drilling process can be performed using an ultraviolet laser source. In practice, the sidewalls of the drill holes 66 thus produced may be less... Figure 10 As shown, they are parallel. Figure 10Wafer 1 with ideal drilling is shown. After drilling a first hole at a first point in the intersection 63, the planar wafer 1 is repositioned relative to the laser irradiation device such that the laser beam is directed to a second point within the intersection 63. A second hole is then formed at the intersection 63 of the planar wafer. This process can be repeated as needed to form as many additional holes as possible in the intersection 63. Although drilling creates discrete weakened regions in wafer 1, by limiting the formation of the holes to the intersection 63, or by providing a higher line density of holes 66 in the intersection 63 than in the intermediate portion 64 between the intersections 63, the average laser power applied per unit length will be greater in the intersection 63 than in the intermediate portion 64, as in the previously described embodiment.
[0049] In an alternative embodiment, instead of drilling a single hole 66 and then moving the wafer 1 and the laser irradiation device relative to each other, the hole 66 can be generated by providing a diffractive optical element (DOE) to the laser irradiation device, such that the laser beam generated by the laser source passes through the DOE and is split into multiple discrete, separate sub-beams. Each sub-beam is directed to the wafer 1, and each sub-beam drills a separate hole. This allows multiple holes to be generated simultaneously at the intersections of the wafer 1 without relative movement of the wafer 1 and the laser irradiation device. However, to reproduce multiple holes at each intersection as needed, relative movement between the wafer 1 and the laser irradiation device is required. The DOE can be configured to generate various arrays of holes, such as those similar to... Figure 9 The cross-shaped arrangement, linear array, etc., are shown.
[0050] exist Figure 9 In the outer region of wafer 1, specifically near its outer edge and between the outermost radial device 2, the irradiation line 65 is fully formed, i.e., formed by dicing rather than drilling, through relative movement of wafer 1 and the laser source, as this facilitates separation without affecting chip strength near any device 2. However, this configuration is entirely optional, and in other embodiments, this outer region may not be treated in this way.
[0051] Figure 11 The wafer 1, processed according to yet another embodiment of the present invention, is schematically shown from above. Figure 12 This is shown schematically from the side according to Figure 11 A portion of the wafer processed in this embodiment. This embodiment can be considered as a reference to the above. Figure 9 and Figure 10 A simplified version of the described embodiment. Here, the laser irradiation device is again used to form drill holes 76 at the intersections 73 between the middle portions 74 of the channels 6 located between the devices 2. However, in this embodiment, only a single drill hole 76 is formed at each intersection 73. Since only a single drill hole 76 is formed at each intersection 73, compared with... Figure 9 and Figure 10 Compared to borehole 66, these boreholes are shown to have a relatively large diameter. However, the dimensions of borehole 76 can be determined and configured according to the wafer 1 under discussion.
[0052] exist Figure 11 In the outer region of wafer 1, specifically near its outer edge and between the outermost radial device 2, the irradiation line 75 is fully formed, i.e., formed by dicing rather than drilling, through relative movement of wafer 1 and the laser source, as this facilitates separation without affecting chip strength near any device 2. However, this configuration is entirely optional, and in other embodiments, this outer region may not be treated in this way.
[0053] The above embodiments are merely exemplary, and other possibilities and alternatives within the scope of this invention will be apparent to those skilled in the art.
Claims
1. A method for forming weakening lines in a planar wafer, wherein a plurality of weakening lines are arranged in an orthogonal grid to prepare for a mechanical fracture step of breaking the planar wafer along the plurality of weakening lines, characterized in that, The method includes the following steps: At least one laser beam is used to irradiate multiple portions of the planar wafer, each portion coinciding with a weakening line to be formed in the planar wafer, the multiple portions comprising: The intersecting portion, which is near the intersection of the orthogonal grids; and The middle section, which is located between adjacent intersecting sections; The intersecting portion is irradiated with a first average laser power, the middle portion is irradiated with a second average laser power, and the first average laser power is greater than the second average laser power.
2. The method according to claim 1, characterized in that, Includes the following steps: i) Determine the location where weakening lines will be formed in the planar wafer, and determine the start and end positions for each weakening line; ii) Provide a laser irradiation apparatus adapted to focus a laser beam onto a focal point on the planar wafer; iii) Move the planar wafer and the laser irradiation device relative to each other along a path parallel to the plane of the planar wafer from a position near the starting position to a position near the ending position; The path includes alternating intersections and intermediate sections.
3. The method according to claim 1, characterized in that, The laser beam comprises a pulsed laser beam with a pulse period, each intersection being irradiated for a first time period, each intermediate portion being irradiated for a second time period, and both the first time period and the second time period are longer than the pulse period.
4. The method according to claim 2, characterized in that, This includes repeating step iii) to form a plurality of weakening lines in the planar wafer, the plurality of weakening lines defining the orthogonal grid.
5. The method according to claim 1, characterized in that, The second average laser power is zero, so that the planar wafer is essentially unaffected by laser power at the middle portion.
6. The method according to claim 2, characterized in that, The laser irradiation device includes a laser source for generating a laser beam, and step iii) includes adjusting the output power of the laser source to change the average laser power.
7. The method according to claim 2, characterized in that, The laser irradiation apparatus includes a laser source for generating a laser beam and a beam modulator disposed in the optical path of the generated laser beam between the laser source and the focal point, and step iii) includes changing the average laser power of the generated laser beam by controlling the beam modulator.
8. The method according to claim 2, characterized in that, Step iii) includes adjusting the relative movement speed between the planar wafer and the laser irradiation device, wherein the relative movement speed along a first portion of the path is less than the relative movement speed along a second portion of the path.
9. The method according to claim 2, characterized in that, Step ii) includes providing a laser irradiation apparatus suitable for focusing a laser beam into the interior of the planar wafer to generate a subsurface weakening line in step iii).
10. The method according to claim 2, characterized in that, Step ii) includes providing a laser irradiation device suitable for focusing a laser beam onto a focal point near the upper surface of the planar wafer to form a groove in the upper surface in step iii).
11. The method according to claim 1, characterized in that, Includes the following steps: i) Provide a laser irradiation device adapted to guide a laser beam to the planar wafer; ii) Positioning the planar wafer relative to the laser irradiation device such that the laser beam is directed to a first point within the intersection portion; and iii) Drill holes at the intersection of the planar wafer using the laser beam.
12. The method according to claim 11, characterized in that, Further steps include: iv) Reposition the planar wafer relative to the laser irradiation device such that the laser beam is directed to a second point within the intersection portion; and v) Drill a second hole at the intersection of the planar wafer using the laser beam.
13. The method according to claim 12, characterized in that, Includes the following steps: The planar wafer is repositioned relative to the laser irradiation device such that the laser beam is directed to an additional point within the intersection, and the laser beam is used to drill additional holes at the intersection of the planar wafer.
14. The method according to claim 11, characterized in that, Step i) includes providing a diffractive optical element for the laser irradiation device, and the hole drilled in step iii) is one of a plurality of holes drilled simultaneously by guiding the laser beam through the diffractive optical element to the planar wafer.
15. A method for forming weakening lines in a planar wafer, wherein a plurality of devices are formed on the planar wafer in a regularly orthogonal array, the plurality of devices being separated by channels, characterized in that, The method includes: The channel is irradiated with at least one laser beam to weaken the planar wafer; The portion of the channel near the intersection of the channels is irradiated with a first average laser power, the portion of the channel between the intersections is irradiated with a second average laser power, and the first average laser power is greater than the second average laser power.
16. A dicing machine for forming weakening lines in a planar wafer, wherein multiple weakening lines are arranged in an orthogonal grid, characterized in that, The cutting machine includes: Control device; A laser irradiation device adapted to focus a laser beam toward the planar wafer; and A conveying device for moving the planar wafer and the laser irradiation device relative to each other along a path parallel to the plane of the planar wafer; The control device is adapted to control the laser irradiation device and the transmission device to subject the intersection portion of the planar wafer to a first average laser power and the middle portion of the planar wafer to a second average laser power, wherein the intersection portion is close to the intersection point of the orthogonal grid, the middle portion is located between adjacent intersection portions, and the first average laser power is greater than the second average laser power.
17. The cutting machine according to claim 16, characterized in that, The laser irradiation device includes a laser source for generating a laser beam and a beam modulator disposed in the optical path of the generated laser beam between the laser source and the planar wafer, wherein the beam modulator is controlled by a control device.
18. The cutting machine according to claim 17, characterized in that, The beam modulator includes a switchable beam shaper.
19. The cutting machine according to claim 17, characterized in that, The beam modulator includes a movable optical barrier.
Citation Information
Patent Citations
Laser working method and laser working apparatus
EP2186596B1
Aberration-correcting method
EP2325689B1
Laser machining device and laser machining method
US10328521B2