Cutting methods for gold-backed wafers
By slotting the front side of the wafer and using laser cutting to cut the metal layer, the problems of edge chipping and burrs caused by the metal layer in the cutting of back-gold wafers are solved, improving cutting efficiency and reliability.
Patent Information
- Application Number
- CN202611137876.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2026-07-29
- Publication Date
- 2026-11-17
AI Technical Summary
Existing technologies suffer from problems such as metal sticking to the cutting tool, reduced cutting force, back edge chipping, burrs, and peeling of the metal layer due to the thickening of the metal layer on the back side of the wafer.
A pre-cut groove is formed on the front side of the wafer using a dicing machine, controlling the substrate allowance between the bottom of the groove and the lower surface of the metal layer. Then, a laser dicing machine is used to cut the metal layer along the groove, achieving non-contact processing.
It improves cutting efficiency, reduces the mechanical stress on the metal layer, effectively solves the problems of chipping and burrs in metal layer cutting, and ensures the stability and reliability of cutting.
Smart Images

Figure CN123124696A_ABST
Abstract
Description
Technical Field
[0001] This invention relates to the field of wafer processing technology, and more specifically, to a method for cutting gold-backed wafers. Background Technology
[0002] Driven by factors such as high voltage and high current, ultra-thin wafers, high-reliability packaging, heat dissipation, and thermal stress, the metal layer on the back of power semiconductors like IGBTs (Insulated Gate Bipolar Transistors) and CSP (Chip Scale Package) wafers is becoming increasingly thicker. This is to accommodate higher current densities, lower conduction losses, stronger heat dissipation, and greater power cycling resistance, while also matching wafer thinning, back-side process upgrades, and copper plating. Thicker back-side metal is far more ductile than brittle silicon substrates. During abrasive wheel cutting, the metal layer is less prone to brittle fracture and more easily torn, leading to large chipping, corner breakage, and delamination (metal-wafer interface separation) on the back-side metal side. Stress is transferred to the front-side device area, causing chipping and microcracks in the front-side silicon. The thicker the metal, the harder / stickier it is, resulting in poorer chipping control, especially during narrow-groove / small-pitch cutting. Severe metal burrs are difficult to clean in the later stages. Tough metals are squeezed, stretched, and drawn under high-speed cutting by the grinding wheel, forming metal burrs / flashes on both sides of the cut. Burrs can easily short-circuit adjacent pads / electrodes, causing poor electrical properties. The hardness of the burrs can easily scratch the device, and wet / plasma deburring is much more difficult. Cu and Au thick metals have more stubborn burrs than Al. Metal adhesion and tool blockage occur when, under high-temperature cutting, molten / plastically deformed thick metals adhere to the gaps between the abrasive grains of the grinding wheel, causing the tool to block the hole. The cutting ability of the tool drops sharply, resulting in excessive edge chipping. The risk of microcracks and delamination increases. The thermal expansion coefficient of thick metals differs greatly from that of the wafer substrate (Si / SiC). The heat generated during cutting and the mechanical stress are superimposed, resulting in internal stress delamination at the metal-wafer interface. Transverse / longitudinal microcracks are induced inside the substrate, leading to reliability failure (temperature cycling, thrust).
[0003] Therefore, there is an urgent need for a cutting method for gold-backed wafers that can solve problems such as metal sticking to the cutter, reduced cutting force, back edge chipping, burrs on the metal layer, and peeling caused by the thickening of the metal layer on the back of the wafer. Summary of the Invention
[0004] This application proposes a cutting method for gold-backed wafers that can solve problems such as metal sticking to the cutter, reduced cutting force, back edge chipping, burrs on the metal layer, and peeling caused by the thickening of the metal layer on the back of the wafer.
[0005] Therefore, the first objective of this application is to provide a method for dicing gold-backed wafers.
[0006] In view of the above, the embodiments of the first aspect of this application provide a method for cutting a gold-backed wafer, which includes a wafer body and a metal layer, the metal layer being disposed on the back side of the wafer body. The method for cutting the gold-backed wafer includes: using a scribing device to cut a groove on the front side of the wafer body to form a cutting groove, the distance from the bottom of the cutting groove to the side of the metal layer away from the wafer body being a first distance, the first distance being greater than the thickness of the metal layer; and using a laser scribing device to cut along the cutting groove to cut through the metal layer, thereby completing the cutting of the gold-backed wafer.
[0007] In this technical solution, the dicing method for gold-backed wafers is used for wafers with a metal layer already prepared on the back side. First, a dicing machine is used to create a groove on the front side of the wafer (the side without the metal layer). The purpose of this step is not to cut through the entire wafer, but to pre-form a "pre-dicing groove." The depth of this "groove" is precisely controlled, leaving a "substrate allowance" between the bottom of the groove and the lower surface of the metal layer on the back side. A laser dicing machine is then used to cut along the groove, separating the metal layer. The energy of the laser beam is precisely focused, its function being to ablate and penetrate the pre-reserved layer of wafer thickness, thus ultimately separating the entire gold-backed wafer unit. The entire process, starting from the front side of the wafer and ending on the metal layer side, achieves indirect, non-contact (at the critical first step) processing of the fragile metal layer. Compared to the traditional one-time cut-through method, this solution first uses a grinding wheel to mechanically cut most of the thickness of the wafer body, which is highly efficient and has a small heat-affected zone; the second step uses a laser to precisely remove the thin layer and metal, avoiding the mechanical stress pulling on the metal layer, and effectively solving the problems of cutting edge chipping and metal burrs caused by the metal layer in the cutting of back-gold wafers.
[0008] In any of the above technical solutions, optionally, the dicing equipment includes a dicing wheel. Before the step of using the dicing equipment to cut grooves on the front side of the wafer body to form dicing grooves, the cutting method further includes obtaining the diameter of the dicing wheel; and adjusting the height of the dicing wheel based on the diameter of the dicing wheel to adjust the distance between the dicing wheel and the side of the metal layer away from the wafer body.
[0009] In this technical solution, before initiating the grinding wheel grooving step, the method includes a precise tool setting and height setting process for the grinding wheel dicing equipment. Specifically, the operator needs to obtain the precise physical diameter of the grinding wheel to be used. Because of tolerances in the manufacturing and installation of the grinding wheel, and because the diameter decreases due to wear during use, this diameter is a critical initial parameter that needs to be measured or calibrated. Based on the measured actual diameter of the grinding wheel, the system dynamically adjusts the height position of the grinding wheel spindle. The principle of adjustment is that the cutting depth of the grinding wheel (i.e., the grooving depth) is determined by the position of its lowest point of the cutting edge relative to the wafer surface. By raising and lowering the spindle, the cutting reference plane of the grinding wheel cutting edge can be changed. The direct purpose of the adjustment is to precisely control the preset distance between the "lowest point of the grinding wheel cutting edge" and the "lower surface of the wafer's bottom metal layer," thereby ensuring that the "substrate allowance" plus the thickness of the metal layer between the bottom of the final grooving and the metal layer falls precisely within the target range of 25-30 micrometers. For example, if measurements show that the grinding wheel diameter has decreased by 10 micrometers due to wear, the system will automatically adjust the grinding wheel spindle downwards by an additional 10 micrometers to ensure that the cutting depth of the blade remains constant, maintaining a constant substrate allowance. This height adjustment step is essentially a dynamic "blade compensation" or "zero-point setting" process based on the actual geometry of the grinding wheel. Its beneficial effect is that it can compensate for the dimensional fluctuations of the grinding wheel itself, ensuring the repeatability and consistency of the first-step pre-cutting depth from the source. This is the foundation for the subsequent laser steps to stably and reliably complete the final cut. Without this step, the difference in grinding wheel diameter will directly translate into a difference in pre-cutting depth, potentially leading to an excessively thick substrate allowance (making it difficult for the laser to cut through) or an excessively thin or even zero substrate allowance (damaging the metal layer with the grinding wheel), causing the entire process to fail.
[0010] In any of the above technical solutions, optionally, the particle size of the grinding wheel is greater than or equal to 3500 mesh and less than or equal to 4000 mesh.
[0011] In any of the above technical solutions, optionally, the particle size of the grinding wheel is greater than or equal to 3500 mesh and less than or equal to 3600 mesh.
[0012] In any of the above technical solutions, the metal layer may optionally include one of a NiTiAg alloy layer, an AlTiNiVCuAg alloy layer, or an AlTiNiVCuAgAu alloy layer.
[0013] In any of the above technical solutions, optionally, the cutting speed of the grinding wheel is greater than 15 mm / s and less than or equal to 35 mm / s.
[0014] In any of the above technical solutions, optionally, the cutting speed of the grinding wheel is greater than 25 mm / s and less than or equal to 30 mm / s.
[0015] Optionally, in any of the above technical solutions, the grinding wheel dicing device includes a grinding wheel dicing disc, the thickness of which is greater than or equal to 30 μm and less than or equal to 40 μm.
[0016] In any of the above technical solutions, optionally, the step of using a dicing wheel device to cut grooves on the front side of the wafer body to form a dicing groove includes: obtaining a dicing path on the front side of the wafer body; controlling the dicing wheel device to cut grooves along the dicing path on the front side of the wafer body to form a dicing groove; wherein the width of the dicing path is greater than or equal to 60 μm and less than or equal to 80 μm.
[0017] Optionally, in any of the above technical solutions, the gold-backed wafer includes either an 8-inch gold-backed wafer or a 12-inch gold-backed wafer.
[0018] In any of the above technical solutions, optionally, the spindle speed of the grinding wheel is greater than or equal to 30,000 revolutions per minute and less than or equal to 55,000 revolutions per minute.
[0019] In any of the above technical solutions, optionally, the spindle speed of the grinding wheel is greater than or equal to 40,000 revolutions per minute and less than or equal to 45,000 revolutions per minute.
[0020] In any of the above technical solutions, optionally, the thickness of the wafer body is greater than or equal to 80 μm and less than or equal to 120 μm, and the thickness of the metal layer is greater than or equal to 5 μm and less than 25 μm.
[0021] In any of the above technical solutions, optionally, the first distance is greater than or equal to 25 μm and less than or equal to 30 μm.
[0022] In any of the above technical solutions, optionally, the first distance is greater than or equal to 25 μm and less than or equal to 27 μm.
[0023] Additional aspects and advantages of this application will become apparent in the following description or may be learned by practice of this application. Attached Figure Description
[0024] To more clearly illustrate the embodiments of this application or related technologies, the accompanying drawings used in the description of the embodiments or related technologies will be briefly introduced below. Obviously, the accompanying drawings described below are only some embodiments of this application. For those skilled in the art, other drawings can be obtained based on the structures shown in these drawings without creative effort.
[0025] Figure 1 This is a schematic flowchart of a method for dicing a gold-backed wafer according to an embodiment of this application. Detailed Implementation
[0026] To better understand the above-mentioned objectives, features, and advantages of this application, the application will be further described in detail below with reference to the accompanying drawings and specific embodiments. It should be noted that, unless otherwise specified, the embodiments and features described in these embodiments can be combined with each other.
[0027] Many specific details are set forth in the following description in order to provide a full understanding of this application. However, this application may also be implemented in other ways different from those described herein. Therefore, the scope of protection of this application is not limited to the specific embodiments disclosed below.
[0028] The present invention provides a method for dicing gold-backed wafers, which includes a wafer body and a metal layer disposed on the back side of the wafer body, such as... Figure 1 As shown, the dicing methods for gold-backed wafers include:
[0029] S101: A dicing machine is used to cut grooves on the front side of the wafer body to form a dicing groove. The distance from the bottom of the dicing groove to the side of the metal layer away from the wafer body is the first distance. The first distance is greater than the thickness of the metal layer.
[0030] S103: A laser scribing device is used to cut along the dicing groove to cut through the metal layer and complete the cutting of the back gold wafer.
[0031] In this embodiment, the dicing method for gold-backed wafers is used for wafers with a metal layer already prepared on the back side. First, a dicing machine is used to create a groove on the front side of the wafer (i.e., the side without the metal layer). The purpose of this step is not to cut through the entire wafer, but to pre-form a "pre-dicing groove." The depth of this "dicing groove" is precisely controlled, leaving a "substrate allowance" between the bottom of the groove and the lower surface of the metal layer on the back side. This "substrate allowance" plus the thickness of the metal layer is designed to be greater than or equal to 25 micrometers and less than or equal to 30 micrometers. A laser dicing machine is then used to completely cut the metal layer along the dicing groove. The energy of the laser beam is precisely focused, its function being to ablate and penetrate the 25-30 micrometer layer reserved in the first step, thereby ultimately separating the entire gold-backed wafer unit. The entire process, starting from the front side of the wafer and ending on the metal layer side, achieves indirect, non-contact (at the critical first step) processing of the fragile metal layer. Compared to the traditional one-time cut-through method, this solution first uses a grinding wheel to mechanically cut most of the thickness of the wafer body, which is highly efficient and has a small heat-affected zone; the second step uses a laser to precisely remove the thin layer and metal, avoiding the mechanical stress pulling on the metal layer, and effectively solving the problems of cutting edge chipping and metal burrs caused by the metal layer in the cutting of back-gold wafers.
[0032] In any of the above embodiments, optionally, the dicing device includes a dicing wheel, and before the step of using the dicing device to cut grooves on the front side of the wafer body to form dicing grooves, the cutting method further includes obtaining the diameter of the dicing wheel; and adjusting the height of the dicing wheel based on the diameter of the dicing wheel to adjust the distance between the dicing wheel and the side of the metal layer away from the wafer body.
[0033] In this embodiment, before initiating the grinding wheel grooving step, the method includes a precise tool setting and height setting process for the grinding wheel dicing equipment. Specifically, the operator needs to obtain the precise physical diameter of the grinding wheel to be used. Because of tolerances in the manufacturing and installation of grinding wheels, and because the diameter decreases due to wear during use, this diameter is a critical initial parameter that needs to be measured or calibrated. Based on the measured actual diameter of the grinding wheel, the system dynamically adjusts the height position of the grinding wheel spindle. The principle of adjustment is that the cutting depth of the grinding wheel (i.e., the grooving depth) is determined by the position of its lowest point of the cutting edge relative to the wafer surface. By raising and lowering the spindle, the cutting reference plane of the grinding wheel cutting edge can be changed. The direct purpose of the adjustment is to precisely control the preset distance between the "lowest point of the grinding wheel cutting edge" and the "lower surface of the wafer's bottom metal layer," thereby ensuring that the "substrate allowance" plus the thickness of the metal layer between the bottom of the final grooving and the metal layer falls precisely within the target range of 25-30 micrometers. For example, if measurements show that the grinding wheel diameter has decreased by 10 micrometers due to wear, the system will automatically adjust the grinding wheel spindle downwards by an additional 10 micrometers to ensure that the cutting depth of the blade remains constant, maintaining a constant substrate allowance. This height adjustment step is essentially a dynamic "blade compensation" or "zero-point setting" process based on the actual geometry of the grinding wheel. Its beneficial effect is that it can compensate for the dimensional fluctuations of the grinding wheel itself, ensuring the repeatability and consistency of the first-step pre-cutting depth from the source. This is the foundation for the subsequent laser steps to stably and reliably complete the final cut. Without this step, the difference in grinding wheel diameter will directly translate into a difference in pre-cutting depth, potentially leading to an excessively thick substrate allowance (making it difficult for the laser to cut through) or an excessively thin or even zero substrate allowance (damaging the metal layer with the grinding wheel), causing the entire process to fail.
[0034] In any of the above embodiments, optionally, the grinding wheel has a particle size greater than or equal to 3500 mesh and less than or equal to 4000 mesh.
[0035] In any of the above embodiments, optionally, the grinding wheel has a particle size greater than or equal to 3500 mesh and less than or equal to 3600 mesh.
[0036] In any of the above embodiments, the metal layer may optionally include one of a NiTiAg alloy layer, an AlTiNiVCuAg alloy layer, or an AlTiNiVCuAgAu alloy layer.
[0037] In any of the above embodiments, optionally, the cutting speed of the grinding wheel is greater than 15 mm / s and less than or equal to 35 mm / s.
[0038] In any of the above embodiments, optionally, the cutting speed of the grinding wheel is greater than 25 mm / s and less than or equal to 30 mm / s.
[0039] In any of the above embodiments, optionally, the grinding wheel dicing device includes a grinding wheel dicing blade with a thickness greater than or equal to 30 μm and less than or equal to 40 μm.
[0040] In any of the above embodiments, optionally, the step of using a dicing wheel device to cut grooves on the front side of the wafer body to form a dicing groove includes: obtaining a dicing path on the front side of the wafer body; controlling the dicing wheel device to cut grooves along the dicing path on the front side of the wafer body to form a dicing groove; wherein the width of the dicing path is greater than or equal to 60 μm and less than or equal to 80 μm.
[0041] In any of the above embodiments, the gold-backed wafer may optionally include one of an 8-inch gold-backed wafer and a 12-inch gold-backed wafer.
[0042] In any of the above embodiments, optionally, the spindle speed of the grinding wheel is greater than or equal to 30,000 revolutions per minute and less than or equal to 55,000 revolutions per minute.
[0043] In any of the above embodiments, optionally, the spindle speed of the grinding wheel is greater than or equal to 40,000 revolutions per minute and less than or equal to 45,000 revolutions per minute.
[0044] In any of the above embodiments, optionally, the thickness of the wafer body is greater than or equal to 80 μm and less than or equal to 120 μm, and the thickness of the metal layer is greater than or equal to 5 μm and less than 25 μm.
[0045] In any of the above embodiments, optionally, the first distance is greater than or equal to 25 μm and less than or equal to 30 μm.
[0046] In any of the above embodiments, optionally, the first distance is greater than or equal to 25 μm and less than or equal to 27 μm.
[0047] Step 1: Install the dicing blade on the equipment. Install the selected blade on the spindle of the dicing machine.
[0048] Step 2, sharpening: First, set the sharpening parameters on the dicing machine; after attaching the sharpening plate to the film, place it on the worktable, manually locate the starting position of the sharpening through the image, and the equipment will start sharpening. Confirm that the width of the sharpening marks is normal as above.
[0049] Step 3: After sharpening, remove the sharpening plate from the equipment. The sharpening blade will have some wear, so perform contact or non-contact height measurement to correct the blade wear.
[0050] Step 4: Set the cutting parameters in advance, such as spindle speed 45000RPM, cutting speed 30mm / s, leave 25um at the bottom of the grooved wafer (do not cut through the product), Y-axis step value, product size and thickness, intermediate blade height measurement frequency, etc.
[0051] Step 5, Fully Automatic Cutting: Attach the product to the UV film and place it in the material box (usually 25 products can be placed in one material box) → Place the material box on the equipment → Fully automatic operation begins, the equipment loads the product and places it on the worktable → According to the selected cutting parameters, align the image, find the graphic on the product and automatically align it, adjust the cutting angle and cutting path to confirm → Start cutting, cut each cutting path of the product in the 0° direction, turn 90° to cut the other side → Cutting ends → Cleaning → Unloading.
[0052] Step 6: The laser scribing machine cuts the remaining metal layer material in the product groove, and the steps are similar to those in step 5.
[0053] Cutting parameters: blade selection 3500-4000 mesh, cutting speed 15 mm / s - 30 mm / s, leave 25um - 30um at the bottom of the wafer, spindle speed 30000 RPM - 55000 RPM.
[0054] For example, the parameters that have been verified in practice are: select a 3500-grit dicing blade, spindle speed of 45000 RPM, cutting speed of 30 mm / s, and leave 25 μm at the bottom of the wafer.
[0055] First, a grinding wheel dicing machine is used to scribe the grooves, followed by laser dicing to cut through the wafer. This process is applied to wafers with a back metal layer thickness greater than 5µm in mid-to-high-end power semiconductor products. The combined grinding wheel dicing and laser dicing process uses a grinding wheel dicing machine to scribe the grooves, leaving a 25µm-30µm thickness at the bottom of the wafer without cutting through. Then, the wafer is transferred to the laser dicing process where a laser dicing machine cuts through the grooves to remove the remaining material (a small amount of silicon and metal layer). The overall (front, back, and side) cutting quality is good, resulting in high yield and high reliability for subsequent product packaging.
[0056] The laser scribing equipment uses a 355nm ultraviolet laser with an output power of 3W to 8W, a repetition frequency of 50kHz to 200kHz, and a pulse width on the order of nanoseconds or picoseconds. The cutting speed is 150mm / s to 300mm / s, and the depth of material removed with each cut is 1μm to 2μm. For the target cutting area of the metal layer, multiple repeated scans are performed using the same cutting trajectory. The number of scans is adaptively set according to the thickness of the metal layer to achieve complete cutting of the metal layer. For example, when the metal layer thickness is 10μm, the number of repeated scans is 5 to 10.
[0057] Specifically, the solution in this application uses a dicing machine to first scribe the wafer, allowing the front side of the wafer (i.e., the circuit layer on the wafer body) to be directly placed on top for dicing. Since the laser dicing machine requires image recognition, a metal layer can be placed within the dicing groove on the front side of the wafer, such as a LOW-K material (low dielectric constant dielectric material). Alternatively, a laser device with a downward-looking CCD (Charge-Coupled Device) can be used. In a laser dicing machine with the laser on top, where the wafer is very thin, a transparent film needs to be applied to the circuit layer with the metal side facing up. The circuit layer is adhered to the worktable, the metal layer is diced by the laser, and then a film-casting step is required during the dicing process with the metal side facing up for the dicing machine to recognize and cut. The solution in this application enables forward dicing without the need to re-fix the wafer or install additional equipment.
[0058] Additional aspects and advantages of this application will become apparent in the following description or may be learned by practice of this application.
[0059] Furthermore, the use of terms such as "first," "second," etc., in this application is for descriptive purposes only and should not be construed as indicating or implying their relative importance or implicitly specifying the number of technical features indicated. Therefore, a feature defined as "first" or "second" may explicitly or implicitly include at least one of that feature. In the description of this application, "multiple" means at least two, such as two, three, etc., unless otherwise explicitly specified.
[0060] In this application, unless otherwise expressly specified and limited, the terms "connection," "fixed," etc., should be interpreted broadly. For example, "fixed" can mean a fixed connection, a detachable connection, or an integral part; it can mean a mechanical connection or an electrical connection; it can mean a direct connection or an indirect connection through an intermediate medium; it can mean the internal communication of two components or the interaction between two components, unless otherwise expressly limited. Those skilled in the art can understand the specific meaning of the above terms in this application according to the specific circumstances.
[0061] Furthermore, the embodiments of this application can be combined with each other, but only if they are based on what those skilled in the art can do. If the combination of embodiments is contradictory or cannot be implemented, it should be considered that such combination of embodiments does not exist and is not within the scope of protection claimed by this application.
[0062] The above are merely preferred embodiments of this application and are not intended to limit this application. Various modifications and variations can be made to this application by those skilled in the art. Any modifications, equivalent substitutions, improvements, etc., made within the spirit and principles of this application should be included within the protection scope of this application.
Claims
1. A method for dicing a gold-backed wafer, characterized in that, For dicing gold-backed wafers, the gold-backed wafer includes: a wafer body and a metal layer, the metal layer being disposed on the back side of the wafer body, and the dicing method of the gold-backed wafer includes: A dicing device is used to cut grooves on the front side of the wafer body to form dicing grooves. The distance from the bottom of the dicing groove to the side of the metal layer away from the wafer body is a first distance, and the first distance is greater than the thickness of the metal layer. The metal layer is cut through using a laser scribing device along the dicing groove to complete the cutting of the gold-backed wafer.
2. The method for dicing a gold-backed wafer according to claim 1, characterized in that, The dicing device includes a grinding wheel. Before the step of using the dicing device to cut grooves on the front side of the wafer body to form dicing grooves, the cutting method further includes obtaining the diameter of the grinding wheel. Based on the diameter of the grinding wheel, the height of the grinding wheel is adjusted to adjust the distance between the grinding wheel and the side of the metal layer away from the wafer body.
3. The method for dicing a gold-backed wafer according to claim 2, characterized in that, The grinding wheel has a particle size greater than or equal to 3500 mesh and less than or equal to 4000 mesh.
4. The method for dicing a gold-backed wafer according to claim 1, characterized in that, The metal layer includes one of a NiTiAg alloy layer, an AlTiNiVCuAg alloy layer, or an AlTiNiVCuAgAu alloy layer.
5. The method for dicing a gold-backed wafer according to claim 2, characterized in that, The cutting speed of the grinding wheel is greater than 15 mm / s and less than or equal to 35 mm / s; The grinding wheel dicing device includes a grinding wheel dicing blade, the thickness of which is greater than or equal to 30 μm and less than or equal to 40 μm.
6. The method for dicing a gold-backed wafer according to claim 1, characterized in that, The step of using a dicing wheel to cut grooves on the front side of the wafer body to form dicing grooves includes: Obtain the dicing marks on the front side of the wafer body; The grinding wheel dicing device is controlled to cut grooves along the dicing path on the front side of the wafer body to form the dicing grooves; The width of the cutting channel is greater than or equal to 60 μm and less than or equal to 80 μm.
7. The method for dicing a gold-backed wafer according to claim 2, characterized in that, The spindle speed of the grinding wheel is greater than or equal to 30,000 revolutions per minute and less than or equal to 55,000 revolutions per minute.
8. The method for dicing a gold-backed wafer according to claim 1, characterized in that, The gold-backed wafer includes one of an 8-inch gold-backed wafer and a 12-inch gold-backed wafer.
9. The method for dicing a gold-backed wafer according to any one of claims 1 to 8, characterized in that, The thickness of the wafer body is greater than or equal to 80 μm and less than or equal to 120 μm; The thickness of the metal layer is greater than or equal to 5 μm and less than 25 μm.
10. The method for dicing a gold-backed wafer according to any one of claims 1 to 8, characterized in that, The first distance is greater than or equal to 25 μm and less than or equal to 30 μm.