Structures and methods for improving surface tension at wafer edges

By setting an extension in the wafer edge region and combining it with the wafer support stage to form a continuous surface, the problem of insufficient liquid film thickness of the wafer edge cleaning solution is solved, the surface tension of the wafer edge is improved, pattern bending defects are prevented, and the cleaning process window is increased.

CN123124701APending Publication Date: 2026-11-17SHANGHAI HUALI INTEGRATED CIRCUIT CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202611257826.5
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2026-08-18
Publication Date
2026-11-17

AI Technical Summary

Technical Problem

Insufficient liquid film thickness of the cleaning solution in the wafer edge region causes polysilicon pattern bending, affecting the cleaning process window and surface tension, which is difficult to improve effectively with existing technologies.

Method used

By combining wafer extensions with wafer support stages to form a continuous third top surface, the thickness of the cleaning fluid in the wafer edge area is consistent with that in the middle area, ensuring that the cleaning fluid covers the entire surface and preventing water residue in the polysilicon gaps.

Benefits of technology

By increasing the thickness of the cleaning solution in the wafer edge region, surface tension is improved, bending defects in the pattern structure are prevented, the cleaning process window is increased, and the cleaning effect is ensured.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN123124701A_ABST
    Figure CN123124701A_ABST
Patent Text Reader

Abstract

This invention discloses a structure for improving the surface tension of a wafer edge, comprising: a wafer extension. The wafer extension is placed on a wafer support stage. The wafer support stage is used to place the wafer. When the wafer is placed, the outer edge of the wafer and the inner edge of the wafer extension are in contact, so that the first top surface of the wafer and the second top surface of the wafer extension are connected together to form a continuous third top surface. During wafer cleaning, the cleaning fluid covers the entire third top surface. The first edge region of the cleaning fluid is located within the region of the second top surface and thus outside the edge region of the wafer, thereby increasing the thickness of the edge region of the wafer and improving the surface tension of the edge region. This invention also discloses a method for improving the surface tension of a wafer edge. This invention can ensure the liquid film thickness of the cleaning fluid in the wafer edge region, improve the surface tension of the wafer edge, prevent the occurrence of pattern bending defects at the wafer edge, and improve the cleaning process window.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] This invention relates to the field of semiconductor integrated circuit manufacturing, and particularly to a structure for improving the surface tension at wafer edges. This invention also relates to a method for improving the surface tension at wafer edges. Background Technology

[0002] In advanced nodes, as 3D architectures and channels become increasingly complex, the aspect ratio (AR) of the polysilicon gaps between polysilicon patterns increases due to the miniaturization of polysilicon patterning steps. This results in a smaller wet window margin in the poly process loop, especially at the wafer edge, increasing the risk of polysilicon pattern bending.

[0003] The main reason for polysilicon pattern bending in wet processes is that, due to surface tension, the cleaning fluid such as IPA in the wafer edge area has a thin liquid film, and the water replacement is incomplete, resulting in poly bending.

[0004] like Figure 1 The image shown is a schematic diagram of the cross-sectional structure of a wafer during existing wafer cleaning processes; as shown... Figure 2 The diagram shown is a top view of the wafer structure during existing wafer cleaning. Existing wafer cleaning methods include the following steps: Place wafer 101 on the wafer support stage.

[0005] A cleaning solution 102 is introduced to clean the wafer 101, wherein the cleaning solution 102 covers the entire top surface of the wafer 101 during cleaning. Figure 1 As shown, due to surface tension, the thickness d102 of the cleaning fluid 102 in the edge region 103 of the wafer 101 is less than the thickness d101 in the middle region of the wafer 101.

[0006] like Figure 3 As shown, polysilicon patterns 104 are formed on the wafer 101, and polysilicon gaps are present between the polysilicon patterns 104. In the edge region 103 of the wafer 101, due to the thinning of the cleaning fluid 102 (d102), incomplete water displacement occurs, that is, the water in the polysilicon gaps is not completely replaced by IPA, which leads to poly bending. Figure 3 The image shows a defect caused by two adjacent polysilicon patterns 104 bending and coming into contact. Summary of the Invention

[0007] The technical problem to be solved by this invention is to provide a structure that improves the surface tension of wafer edges, ensuring the thickness of the cleaning fluid film in the wafer edge region during wafer cleaning, thereby improving the surface tension of the wafer edges, preventing bending defects in the wafer edge pattern structure, and improving the cleaning process window. To this end, this invention also provides a method for improving the surface tension of wafer edges.

[0008] To solve the above-mentioned technical problems, the structure for improving the surface tension of wafer edges provided by the present invention includes: a wafer extension.

[0009] The wafer extension is placed on the wafer support platform.

[0010] The wafer support stage is used to place the wafer. When the wafer is placed, the outer edge of the wafer and the inner edge of the wafer extension come into contact, so that the first top surface of the wafer and the second top surface of the wafer extension are connected together to form a continuous third top surface.

[0011] During wafer cleaning, the cleaning solution is spread across the entire third top surface, with the first edge region of the cleaning solution located within the area of ​​the second top surface and thus outside the edge region of the wafer, to increase the thickness of the edge region of the wafer and thereby improve the surface tension of the edge region of the wafer.

[0012] A further improvement is that the thickness of the wafer extension is the same as the thickness of the wafer.

[0013] A further improvement is that the thickness of the cleaning solution in the edge region of the wafer is equal to the thickness in the middle region of the wafer.

[0014] A further improvement is that the cleaning fluid includes IPA.

[0015] A further improvement is that polysilicon patterns are formed on the wafer, and polysilicon gaps are present between the polysilicon patterns; the thickness of the cleaning solution in the edge region of the wafer is sufficient to allow the IPA to completely replace the water in the polysilicon gaps in the edge region of the wafer during wafer cleaning.

[0016] A further improvement is that the wafer support stage is located in the cleaning chamber.

[0017] To solve the above-mentioned technical problems, the method for improving the surface tension of wafer edges provided by the present invention includes the following steps: Set up wafer extensions.

[0018] The wafer and the wafer extension are placed sequentially on the wafer support stage. After the wafer and the wafer extension are placed, the outer edge of the wafer and the inner edge of the wafer extension come into contact, so that the first top surface of the wafer and the second top surface of the wafer extension are connected together to form a continuous third top surface.

[0019] A cleaning solution is introduced to clean the wafer. During the wafer cleaning process, the cleaning solution covers the entire third top surface. The first edge region of the cleaning solution is located within the region of the second top surface and thus outside the edge region of the wafer, in order to increase the thickness of the edge region of the wafer and thereby improve the surface tension of the edge region of the wafer.

[0020] A further improvement is that the thickness of the wafer extension is the same as the thickness of the wafer.

[0021] A further improvement is that the thickness of the cleaning solution in the edge region of the wafer is equal to the thickness in the middle region of the wafer.

[0022] A further improvement is that the cleaning fluid includes IPA.

[0023] A further improvement is that polysilicon patterns are formed on the wafer, and polysilicon gaps are present between the polysilicon patterns; the thickness of the cleaning solution in the edge region of the wafer is sufficient to allow the IPA to completely replace the water in the polysilicon gaps in the edge region of the wafer during wafer cleaning.

[0024] A further improvement is that the wafer support stage is located in the cleaning chamber.

[0025] This invention, by setting a wafer extension, can extend the top surface of the wafer, i.e., the first top surface. In this way, during cleaning, the surface that actually contacts the cleaning fluid is the extended third top surface. Thus, the edge region of the cleaning fluid, i.e., the first edge region, will be located on the top surface of the wafer extension, i.e., the second top surface. This can prevent the adverse effects of the first edge region of the cleaning fluid on the edge region of the wafer when it is located on the edge region of the wafer. This includes: ensuring the liquid film thickness of the cleaning fluid in the edge region of the wafer during wafer cleaning, thereby improving the surface tension of the wafer edge, preventing bending defects in the pattern structure of the wafer edge, and improving the cleaning process window. Attached Figure Description

[0026] The present invention will be further described in detail below with reference to the accompanying drawings and specific embodiments: Figure 1 This is a schematic diagram of the cross-sectional structure of a wafer during existing wafer cleaning. Figure 2 This is a schematic diagram of the wafer top view structure during existing wafer cleaning; Figure 3 This is a schematic diagram of the polysilicon bending structure that occurs in the wafer edge region during existing wafer cleaning processes. Figure 4 This is a cross-sectional schematic diagram of the structure for improving the surface tension at the edge of a wafer according to an embodiment of the present invention; Figure 5 This is a top view schematic diagram of the structure for improving the surface tension at the edge of a wafer according to an embodiment of the present invention; Figure 6 This is a schematic diagram of the polycrystalline silicon structure in the wafer edge region after wafer cleaning using the structure for improving the surface tension of the wafer edge according to an embodiment of the present invention. Detailed Implementation

[0027] like Figure 4 The diagram shown is a cross-sectional view of a structure for improving surface tension at the wafer edge according to an embodiment of the present invention; as shown... Figure 5 The diagram shown is a top view of the structure for improving the surface tension at the wafer edge according to an embodiment of the present invention; as shown... Figure 6 The diagram shown is a schematic representation of the polysilicon structure in the wafer edge region after wafer cleaning using the structure for improving wafer edge surface tension according to an embodiment of the present invention. The structure for improving wafer edge surface tension according to an embodiment of the present invention includes: Wafer extension 202.

[0028] The wafer extension 202 is placed on a wafer support stage (not shown).

[0029] In this embodiment of the invention, the wafer support stage can adopt any structure that can support and fix the wafer 201 from the reverse side of the cleaning surface of the wafer 201.

[0030] The wafer support stage is located in the cleaning chamber. The wafer support stage is used to place the wafer 201. When the wafer 201 is placed, the outer edge of the wafer 201 contacts the inner edge of the wafer extension 202, so that the first top surface of the wafer 201 and the second top surface of the wafer extension 202 are connected together to form a continuous third top surface.

[0031] During the cleaning of the wafer 201, the cleaning fluid 203 is spread over the entire third top surface. The first edge region 204 of the cleaning fluid 203 is located within the region of the second top surface and thus outside the edge region 205 of the wafer 201, so as to increase the thickness d202 of the edge region 205 of the wafer 201 and thereby improve the surface tension of the edge region 205 of the wafer 201.

[0032] In this embodiment of the invention, the thickness of the wafer extension 202 is the same as the thickness of the wafer 201.

[0033] In this embodiment of the invention, the thickness d202 of the cleaning fluid 203 in the edge region 205 of the wafer 201 is equal to the thickness d201 in the middle region of the wafer 201. For example... Figure 4 As shown, in some embodiments, d202 can also be less than d201, but d202 and... Figure 1 Compared to the existing methods, d201 is larger, and d202 only needs to satisfy the condition that no surface tension-related defects will appear at the wafer edge.

[0034] In some embodiments, the cleaning fluid 203 includes IPA.

[0035] like Figure 6 As shown, polysilicon patterns 206 are formed on the wafer 201, and polysilicon gaps are present between the polysilicon patterns 206; the thickness d202 of the cleaning fluid 203 in the edge region 205 of the wafer 201 is such that when the wafer 201 is cleaned, the IPA can completely replace the water in the polysilicon gaps in the edge region 205 of the wafer 201.

[0036] In this embodiment of the invention, by setting a wafer extension 202, the top surface of the wafer 201, i.e., the first top surface, can be extended. Thus, during cleaning, the surface that actually contacts the cleaning fluid 203 is the extended third top surface. In this way, the edge region of the cleaning fluid 203, i.e., the first edge region 204, will be located on the top surface of the wafer extension 202, i.e., the second top surface. This can prevent the first edge region 204 of the cleaning fluid 203 from having an adverse effect on the edge region 205 of the wafer 201 when it is located. This includes ensuring the liquid film thickness of the cleaning fluid 203 in the edge region of the wafer 201 during cleaning, thereby improving the surface tension of the edge of the wafer 201, preventing bending defects in the pattern structure of the edge of the wafer 201, and improving the cleaning process window.

[0037] The method for improving the surface tension at the edge of a wafer according to embodiments of the present invention includes the following steps: Set wafer extension 202.

[0038] The wafer 201 and the wafer extension 202 are placed sequentially on a wafer support stage. After placement, the outer edge of the wafer 201 and the inner edge of the wafer extension 202 come into contact, connecting the first top surface of the wafer 201 and the second top surface of the wafer extension 202 to form a continuous third top surface. In this embodiment of the invention, the wafer support stage is located in a cleaning chamber. The thickness of the wafer extension 202 is the same as the thickness of the wafer 201.

[0039] The wafer 201 is cleaned by introducing cleaning solution 203. During the cleaning of the wafer 201, the cleaning solution 203 covers the entire third top surface. The first edge region 204 of the cleaning solution 203 is located in the region of the second top surface and thus outside the edge region 205 of the wafer 201, so as to increase the thickness d202 of the edge region 205 of the wafer 201 and thereby improve the surface tension of the edge region 205 of the wafer 201.

[0040] In some embodiments, the cleaning fluid 203 includes IPA.

[0041] In the method of this embodiment of the invention, the thickness d202 of the cleaning fluid 203 in the edge region 205 of the wafer 201 is equal to the thickness d201 in the middle region of the wafer 201. For example... Figure 4 As shown, in some embodiments, d202 can also be less than d201, but d202 and... Figure 1 Compared to the existing methods, d201 is larger, and d202 only needs to satisfy the condition that no surface tension-related defects will appear at the wafer edge.

[0042] In some embodiments, a polysilicon pattern 206 is formed on the wafer 201, and polysilicon gaps are present between the polysilicon patterns 206; the thickness d202 of the cleaning fluid 203 in the edge region 205 of the wafer 201 is such that the IPA can completely replace the water in the polysilicon gaps in the edge region 205 of the wafer 201 during cleaning of the wafer 201.

[0043] The present invention has been described in detail above through specific embodiments, but these are not intended to limit the invention. Many modifications and improvements can be made by those skilled in the art without departing from the principles of the invention, and these should also be considered within the scope of protection of the present invention.

Claims

1. A structure for improving the surface tension at the edge of a wafer, characterized in that, include: Wafer extensions; The wafer extension is placed on the wafer support platform; The wafer support stage is used to place the wafer. When the wafer is placed, the outer edge of the wafer and the inner edge of the wafer extension come into contact, so that the first top surface of the wafer and the second top surface of the wafer extension are connected together to form a continuous third top surface. During wafer cleaning, the cleaning solution is spread across the entire third top surface, with the first edge region of the cleaning solution located within the area of ​​the second top surface and thus outside the edge region of the wafer, to increase the thickness of the edge region of the wafer and thereby improve the surface tension of the edge region of the wafer.

2. The structure for improving wafer edge surface tension as described in claim 1, characterized in that: The thickness of the wafer extension is the same as the thickness of the wafer.

3. The structure for improving wafer edge surface tension as described in claim 1, characterized in that: The thickness of the cleaning solution in the edge region of the wafer is equal to the thickness in the middle region of the wafer.

4. The structure for improving wafer edge surface tension as described in claim 1, characterized in that: The cleaning solution includes IPA.

5. The structure for improving wafer edge surface tension as described in claim 4, characterized in that: Polysilicon patterns are formed on the wafer, and polysilicon gaps are formed between the polysilicon patterns; the thickness of the cleaning solution in the edge region of the wafer is sufficient to allow the IPA to completely replace the water in the polysilicon gaps in the edge region of the wafer during wafer cleaning.

6. The structure for improving wafer edge surface tension as described in claim 1, characterized in that: The wafer support stage is located in the cleaning chamber.

7. A method for improving the surface tension at the edge of a wafer, characterized in that, Includes the following steps: Set up wafer extensions; The wafer and the wafer extension are placed on the wafer support stage in sequence. After the wafer and the wafer extension are placed, the outer edge of the wafer and the inner edge of the wafer extension come into contact, so that the first top surface of the wafer and the second top surface of the wafer extension are connected together to form a continuous third top surface. A cleaning solution is introduced to clean the wafer. During the wafer cleaning process, the cleaning solution covers the entire third top surface. The first edge region of the cleaning solution is located within the region of the second top surface and thus outside the edge region of the wafer, in order to increase the thickness of the edge region of the wafer and thereby improve the surface tension of the edge region of the wafer.

8. The method for improving wafer edge surface tension as described in claim 7, characterized in that: The thickness of the wafer extension is the same as the thickness of the wafer.

9. The method for improving the surface tension at the edge of a wafer as described in claim 7, characterized in that: The thickness of the cleaning solution in the edge region of the wafer is equal to the thickness in the middle region of the wafer.

10. The method for improving wafer edge surface tension as described in claim 7, characterized in that: The cleaning solution includes IPA.

11. The method for improving wafer edge surface tension as described in claim 10, characterized in that: Polysilicon patterns are formed on the wafer, and polysilicon gaps are formed between the polysilicon patterns; the thickness of the cleaning solution in the edge region of the wafer is sufficient to allow the IPA to completely replace the water in the polysilicon gaps in the edge region of the wafer during wafer cleaning.

12. The method for improving wafer edge surface tension as described in claim 7, characterized in that: The wafer support stage is located in the cleaning chamber.