Welding equipment
By using a negative ion atmosphere device and inert gas to remove the oxide layer in wave soldering equipment, combined with infrared and hot air assisted preheating, the problems of high welding defective rate and energy consumption in traditional wave soldering are solved, and an efficient and environmentally friendly welding process is achieved.
Patent Information
- Application Number
- CN202322905761.9
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-10-27
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2033-10-27
AI Technical Summary
Traditional wave soldering has problems such as high welding defect rate, pollution and energy consumption caused by flux residue, and low welding efficiency.
A welding equipment is designed that uses a negative ion atmosphere device and an inert gas mixture for preheating and deoxidation, replacing flux, and combines infrared and hot air reflow systems to improve energy utilization.
It significantly reduces the welding defect rate and energy consumption, reduces the use of flux, improves welding efficiency and product quality, avoids the board washing process, and improves the wettability of the welding surface.
Smart Images

Figure CN221870591U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to a welding process, in particular to a welding device. Background Art
[0002] Wave soldering originated in the mid-1950s and has undergone more than 60 years of improvement. Although the design of electronic products is increasingly inclined to use SMD components instead of plug-ins, due to the low reliability and poor heat dissipation of common SMD soldering joints, wave soldering has the advantages of firm solder joints, good heat dissipation, high welding efficiency and low cost. In addition, many devices such as high-power components are currently only plug-ins, so wave soldering is still the welding process that most electronic products need to adopt, and it has a very broad prospect of use.
[0003] At present, traditional wave soldering has many defects during use: 1. The welding defect rate is high, and defects such as short circuit, bridging, solder balls and leaks occur frequently. The amount of tin slag generated by welding is relatively large, and a large number of tests are required in the later stage, and manual soldering is required, which requires a large amount of manpower; 2. A large amount of flux is used in the welding process, and the residual flux will lead to reduced product quality. It is necessary to add a board washing process, which is complicated and pollutes the environment. At the same time, the flux evaporates into the equipment and condenses, resulting in a short equipment maintenance cycle; 3. The energy consumption is large. During the wave soldering preheating and welding process, the cavity is open, and most of the energy is dissipated into the outside air, and the energy utilization rate is very low. Utility Model Content
[0004] The technical problem solved by the utility model is to provide a welding device to significantly reduce or even completely replace soldering flux, reduce welding defects and reduce energy consumption.
[0005] In order to solve the above problems, the utility model adopts the following technical solutions:
[0006] A welding device, comprising a preheating zone, a welding zone and a conveying system arranged in the preheating zone and the welding zone, wherein the preheating zone is used to preheat a PCB board to be welded, and further comprising:
[0007] A negative ion atmosphere device is arranged in a preheating zone, and comprises: a mounting seat, a negative ion emitting component and an air outlet pipe; the negative ion emitting component is mounted on the mounting seat, and the negative ion emitting component is used to generate negative ions; the air outlet pipe is mounted on the mounting seat and adjacent to the negative ion emitting component, and the air outlet pipe is provided with a plurality of air outlet holes arranged at intervals;
[0008] An atmosphere supply system, providing an initial mixed gas containing an inert gas and a reducing gas which has been heated to an exhaust pipe;
[0009] When the gas supply system provides an initial mixed gas to the gas outlet pipe and the negative ion emitting component is energized, the initial mixed gas is ejected from the gas outlet hole of the gas outlet pipe and blown toward the negative ion emitting component to form a gas mixture containing an inert gas and a negatively charged reducing gas. The gas mixture removes the oxide layer on the surface of the PCB board and preheats the PCB board.
[0010] Furthermore, the mounting seat includes a base, a left fixing part and a right fixing part, the left fixing part is installed on the left side of the base, the right fixing part is installed on the right side of the base, and an air outlet pipe is arranged between the left fixing part and the right fixing part; a plurality of spaced negative ion emitting components are respectively installed on the left fixing part and the right fixing part.
[0011] Furthermore, the base is provided with a groove, and the air outlet pipe is arranged in the groove.
[0012] Furthermore, each negative ion emitting component includes a negative ion emitting head and a carbon brush installed on the upper end of the negative ion emitting head, and the negative ion emitting head of each negative ion emitting component is respectively connected to the negative ion controller.
[0013] Furthermore, the air outlet pipe is in the shape of an elongated strip, the air outlet holes are arranged at intervals along the length direction of the air outlet pipe, an air inlet is arranged at one end of the air outlet pipe, and the total cross-sectional area of the air outlet holes is smaller than the cross-sectional area of the air inlet.
[0014] Furthermore, the preheating zone is sealed by a shell cover, a plate inlet is provided at one end of the preheating zone, a first flexible windshield curtain is provided at the plate inlet, the other end of the preheating zone is connected to the welding zone, and a second flexible windshield curtain is provided at the connection between the preheating zone and the welding zone.
[0015] Furthermore, the welding equipment is also provided with an atmosphere concentration detection device for detecting the concentration of the inert gas and the reducing gas. By providing the atmosphere concentration detection device, the supply amount of the inert gas and the reducing gas is controlled respectively, thereby achieving the set atmosphere concentration.
[0016] Furthermore, there are multiple negative ion atmosphere devices, each of which is arranged at intervals, and each of which is installed below the conveying system. The negative ion atmosphere device is 5-10 mm away from the bottom surface of the PCB board. In this way, a good reduction effect can be achieved.
[0017] Furthermore, the negative ion atmosphere device is installed in the preheating zone through a bottom plate, and the bottom plate is a non-conductive bottom plate.
[0018] Furthermore, the conveying system is inclined upward at an angle of 3-7° to the horizontal direction, which is beneficial to improving the tinning quality of the PCB board when passing through the tin furnace.
[0019] Furthermore, the welding equipment is also provided with a hot air reflow system, which is arranged at one end of the preheating zone to provide the energy required for preheating the PCB board. In terms of preheating energy, the PCB board needs to be preheated to 95-120°C, and the power of the heating device needs to be at least greater than 3KW to provide most of the energy required for preheating.
[0020] Furthermore, the reducing gas can be produced by directly purchasing a mixed gas of an inert gas and a reducing gas in a certain concentration ratio, or it can be produced by using chemicals, such as formic acid cracking to produce hydrogen, and oxalic acid cracking to produce carbon monoxide.
[0021] Furthermore, reducing gases generally have a safe concentration range for use, such as the explosion limit of hydrogen is 4%-75%, and the explosion limit of carbon monoxide is 12.5%-74.2%. Carbon monoxide is a toxic gas, and these reducing gases must be controlled within a safe concentration range during use.
[0022] The beneficial effects of the utility model are:
[0023] 1. Negative ions are introduced into the reducing atmosphere, which greatly improves the effect of the reducing atmosphere in reducing oxides, and can replace the effect of flux in removing oxides. The protective atmosphere can reduce the surface tension of the material being welded. Therefore, the welding equipment of this utility model can greatly reduce the use of flux, or even completely replace flux, eliminate flux pollution, and reduce the board washing process;
[0024] 2. The negative ion atmosphere device is assembled by a mounting base, a negative ion emitting component and an air outlet pipe. It is not only simple in structure, but also conducive to forming a high concentration of negatively charged reducing gas, which is conducive to quickly removing the oxide layer on the surface of the PCB board;
[0025] 3. The use of inert gas as the protective atmosphere can ensure that the oxygen concentration in the cavity space is less than 5000PPM, and the negative ion plus reducing atmosphere can reduce some of the residual oxygen in the cavity, so that the effect of atmosphere protection and oxidation reduction is further improved, effectively reducing the formation of metal oxides, increasing the wettability of the welding surface, and reducing the welding defect rate;
[0026] 4. The heat carried by the protective atmosphere is mainly used to preheat the PCB board, and infrared and hot air reflow are used to assist in preheating, which improves energy utilization and reduces the overall energy consumption of the equipment. BRIEF DESCRIPTION OF THE DRAWINGS
[0027] Figure 1 This is the overall diagram of the wave soldering structure of Example 1 of the utility model;
[0028] Figure 2 This is a structural diagram of a negative ion atmosphere device according to Embodiment 1 of the present utility model;
[0029] Figure 3 This is a pipeline diagram of the atmosphere supply system for the protective atmosphere and the reducing atmosphere in Example 1 of the utility model;
[0030] Figure 4 This is a pipeline diagram of the atmosphere supply system of the mixed gas in Example 1 of the utility model;
[0031] Figure 5 This is the overall diagram of the wave soldering structure of Embodiment 2 of the present utility model;
[0032] Figure markings: 1-preheating zone, 11-preheating chamber shell, 12-board inlet, 13-insulation layer, 141-first flexible windshield curtain, 142-second flexible windshield curtain, 15-synthetic stone bottom plate, 16-negative ion atmosphere device, 161-base, 162-left fixing part, 163-right fixing part, 1631-mounting hole, 165-air outlet pipe, 1651-air inlet, 1652-hollow pipe, 1653-air outlet, 164-negative ion emitting component, 1641-negative ion emitting head, 1642-carbon brush, 1643-cable, 1644-negative ion controller, 171-first atmosphere concentration detection point, 172-second atmosphere concentration detection point, 181-first temperature detection point; 182-second temperature detection point, 2-welding area, 21-welding chamber shell , 3-atmosphere supply system, 301-protective atmosphere generating device, 302-switching valve, 303-filter, 304-pressure control valve, 305-protective atmosphere tank, 306-switching valve, 307-pressure control valve, 308-flow control valve, 309-flow meter, 310-flow control valve, 311-flow meter, 312-chemical tank, 313-medium heater, 314-multi-pass piece, 4-conveyor system, 41-track width adjustment structure, 42-support frame, 43-chain claw structure, 44-PCB board, 51-infrared heating system, 511-infrared heating pipe, 512-reflector, 52-hot air reflux system, 521-hot air reflux chamber, 522-hot air motor, 523-axial flow fan, 524-volute, 525-heating pipe, 526-air outlet plate. DETAILED DESCRIPTION
[0033] The drawings of the present invention are only used for illustrative purposes and cannot be construed as limiting the present invention. In order to better illustrate the following embodiments, some parts of the drawings may be omitted, enlarged or reduced, and cannot represent the size of the actual product; for those skilled in the art, it is understandable that some well-known structures and their descriptions in the drawings may be omitted.
[0034] Example 1
[0035] refer to Figure 1 , Figure 2The utility model provides a welding device. In the present embodiment, the welding device is a wave soldering device, which includes a preheating zone 1, a welding zone 2 connected to the preheating zone 1, an atmosphere supply system 3 and a conveying system 4, wherein the preheating zone 1 is used to preheat a PCB board 44 to be welded; the conveying system 4 is arranged in the preheating zone 1 and the welding zone 2, and the conveying system 4 is inclined upward at an angle of 3-7° to the horizontal direction.
[0036] The preheating zone 1 is provided with a preheating chamber shell cover 11 for isolating the protective atmosphere and reducing atmosphere in the preheating zone 1 from the outside world. The preheating chamber shell cover 11 is composed of sheet metal or structural parts, and the components in contact with each other are sealed, which can be done by sealing tape, gasket or adhesive. The sealing treatment can reduce the escape of the protective atmosphere and reducing atmosphere in the preheating zone 1 to the outside atmosphere. The preheating chamber shell cover 11 is provided with a board inlet 12 at one end where the PCB board 44 enters (that is, a board inlet 12 is provided at one end of the preheating zone 1), and the other end is connected to the welding chamber shell cover 21. The outside of the preheating chamber shell cover 11 is wrapped with an insulation layer 13, and the material can be selected from quartz wool to slow down the heat energy loss of the preheating cavity. A first flexible windshield curtain 141 is provided inside the plate inlet 12; a second flexible windshield curtain 142 is provided at the joint of the preheating chamber shell 11 and the welding chamber shell 21; the materials of the first windshield curtain 141 and the second flexible windshield curtain 142 are anti-static, and need to be temperature-resistant above 250°C, and resistant to chemical corrosion by solder and solder fume. By providing the first flexible windshield curtain 141 and the second flexible windshield curtain 142, the loss of inert gas and reducing gas can be effectively reduced.
[0037] A non-conductive base plate is laid flat at the bottom of the preheating zone 1. In this embodiment, the non-conductive base plate is a synthetic stone base plate 15. Multiple rows of negative ion atmosphere devices 16 are installed on the upper surface of the synthetic stone base plate 15. The synthetic stone base plate 15 can prevent the negative ions generated by the negative ion atmosphere device 16 from being adsorbed by the conductor of the preheating zone.
[0038] There are multiple negative ion atmosphere devices 16 , each of which is arranged at intervals in the preheating zone and installed below the conveying system 4 . Each of the negative ion atmosphere devices 16 is 5-10 mm away from the bottom surface of the PCB board 44 .
[0039] Each negative ion atmosphere device 16 includes: a mounting seat, an air outlet pipe 165 and a plurality of negative ion emitting components 164; each negative ion emitting component 164 is respectively mounted on the mounting seat, and each negative ion emitting component 164 is used to generate negative ions; the air outlet pipe 165 is mounted on the mounting seat and adjacent to the negative ion emitting component 164.
[0040] Specifically, the mounting base includes a base 161, a left fixing portion 162 and a right fixing portion 163. The base 161 is mounted on the surface of the synthetic stone bottom plate 15 and is provided with a groove. The right fixing portion 163 is mounted on the right side of the base 161 through a mounting hole 1631. The left fixing portion 162 is mounted on the left side of the base 161 in the same way. A plurality of negative ion emitting components 164 arranged at intervals are respectively mounted on the left fixing portion 162 and the right fixing portion 163.
[0041] The air outlet pipe 165 is arranged between the left fixing part 162 and the right fixing part 163 and installed in the groove of the base 161. The air outlet pipe 165 is in the shape of a long strip. The left and right sides of the air outlet pipe 165 are respectively provided with a plurality of air outlet holes 1653 arranged at intervals. The air outlet holes 1653 are arranged at intervals along the length direction of the air outlet pipe 165. A threaded air inlet 1651 is provided at one end of the air outlet pipe 165. The cross-sectional area of the air inlet 1651 is larger than the total cross-sectional area of the air outlet holes 1653. A hollow pipe 1652 is provided in the air outlet pipe 165. The protective atmosphere (inert gas) and reducing atmosphere (reducing gas) entering the air outlet pipe 165 from the air inlet 1651 are discharged from dozens of air outlet holes 1653 and blown toward the carbon brush 1642 of the negative ion emitting component 164. The cross-sectional area of the air inlet 1651 is larger than the total cross-sectional area of the air outlets 1653, which is conducive to forming a high pressure in the cavity of the hollow pipe 1652, so that the wind speeds of different air outlets 1653 are evenly pressurized. The structural connectors and the air outlet pipe 165 of the negative ion atmosphere device 16 are made of non-conductive and high temperature resistant materials above 300°C.
[0042] Each negative ion emitting component 164 is composed of a negative ion emitting head 1641, a carbon brush 1642, and a cable 1643 that is resistant to high temperatures above 300°C and connects the negative ion controller 1644 and the negative ion emitting head 1641. The negative ion emitting heads 1641 of each negative ion emitting component 164 are respectively connected to the negative ion controller 1644, and the negative ion controller 1644 provides a negative electrode signal of a certain power to the negative ion emitting head 1641. After the negative ion emitting head 1641 converts electrical energy, it discharges through the tip of the carbon brush 1642 to generate a large number of negative ions, which are attached to the reducing atmosphere to form a negatively charged reducing atmosphere. The generated negative ions are brought to the surface of the PCB board 44 by the protective atmosphere and reducing atmosphere blown out by the air outlet 1653, thereby removing the oxide layer on the surface of the PCB board 44. The concentration of negative ions in the preheating zone is greater than 10 million / cm3.
[0043] The concentration detection point of the atmosphere concentration detection device is set in the welding area 2. The gas detection device is used to detect the concentration of the inert gas and the reducing gas in the preheating zone. If the oxygen concentration in the preheating zone is greater than the set concentration, such as exceeding 5000PPM, it is necessary to increase the protective atmosphere and reducing atmosphere to be added to the preheating zone 1. The reducing atmosphere is generally a flammable and explosive gas. For example, the explosion limit of hydrogen is 4%-75%, and the explosion limit of carbon monoxide is 12.5%-74.2%. Therefore, the concentration of the reducing atmosphere needs to be monitored in real time and controlled not to exceed the lower limit of the explosion limit. The length of the preheating zone 1 is relatively long, so the position of the concentration detection point is preferably greater than or equal to two, such as Figure 1 As shown, a first atmosphere concentration detection point 171 is set at the upper part of the front end of the preheating zone 1, and a second atmosphere concentration detection point 172 is set at the upper part of the rear end of the preheating zone 1. The preheating of the PCB board 44 needs to meet a certain temperature curve so that the PCB board 44 is heated evenly at all locations and the temperature is stably increased to a preset temperature. If a small amount of flux is used, the effective ingredients of the flux can also be activated according to a suitable temperature curve, thereby providing a guarantee for good product welding quality. The preheating zone 1 is relatively long. In order to better control the temperature at various locations in the preheating zone 1, the positions of the temperature detection points are preferably greater than or equal to two, such as Figure 1 As shown, a first temperature detection point 181 is set at the front end of the preheating zone 1 close to the negative ion atmosphere device 16, and a second temperature detection point 182 is set at the rear end of the preheating zone 1 close to the negative ion atmosphere device 16.
[0044] refer to Figure 3 , Figure 4 The supply of protective atmosphere and reducing atmosphere includes but is not limited to two methods: 1. Method A, the protective atmosphere and reducing atmosphere are controlled separately; 2. Method B, directly using the mixed atmosphere.
[0045] In the atmosphere supply system 3 of mode A, the protective atmosphere includes but is not limited to the following two supply modes:
[0046] 1. The protective atmosphere generator 301 generates the protective atmosphere, which is supplied to the filter 303 through the switch valve 302 for impurity removal, and the pressure is increased to a predetermined constant pressure by the pressure control valve 304; 2. The protective atmosphere is directly provided by the protective atmosphere tank 305 and pressurized through the switch valve 306 and the pressure control valve 307.
[0047] After the protective atmosphere is supplied to the system, it is divided into two paths. One path passes through the flow control valve 308 and the flow meter 309 and directly leads to the medium heater 313. The other path passes through the flow control valve 310 and the flow meter 311, and the protective atmosphere is passed into the chemical tank 312 containing chemicals that can produce reducing atmosphere (such as formic acid that can produce hydrogen, oxalic acid that can produce carbon monoxide), takes out the droplet vapor of the chemical, and then passes into the medium heater 313. The flow meter 309 and the flow meter 311 can respectively detect the flow of the protective atmosphere in the two paths, and the flow control valve 308 and the flow control valve 310 can respectively control the flow of the protective atmosphere directly passing to the medium heater 313 and passing into the chemical reagent tank 312. The medium heater 313 can heat the atmosphere to make the atmosphere temperature reach above 250°C, and can effectively preheat the PCB board 44 after entering the preheating zone 1, and the droplet vapor of the chemical can also be cracked under high temperature conditions to produce the reducing atmosphere required for the subsequent process. Therefore, the atmosphere coming out of the medium heater 313 is an initial mixed gas of the protective atmosphere and the reducing atmosphere, and the total amount and proportion of the mixture are respectively controlled by the flow control valve 308 and the flow control valve 310. The initial mixed gas finally passes through the multi-pass piece 314 and is distributed to each negative ion atmosphere device 16.
[0048] In the atmosphere supply system 3 of method B, a mixed atmosphere with a certain ratio is directly used, enters the system from the mixed atmosphere tank 315, passes through the switch valve 306, the pressure control valve 307, the flow control valve 308, the flow meter 309, the medium heater 313, and the multi-way piece 314 in sequence, and is distributed to each negative ion atmosphere device 16.
[0049] The conveying system 4 includes a track width adjustment structure 41, which adjusts the distance between a pair of support frames 42 installed below. The ball screw movement adjustment method can be selected. The track width adjustment range depends on the width of the PCB board 44 or the width of the carrier. A chain claw structure 43 is hung below the side of the support frame, and the chain claw clamps the PCB board 44 to move, completing the product conveying process in the preheating area.
[0050] Example 2
[0051] In order to realize the preheating and reduction process of the protective wave soldering of the utility model, the preheating system can use an infrared system or a hot air reflow system to assist preheating in addition to directly using atmosphere preheating. Infrared preheating and hot air preheating are auxiliary preheating methods, and only one of them can be selected, or both methods can be used at the same time.
[0052] Figure 5 This is the overall diagram of the wave soldering structure of the second embodiment of the utility model. Figure 1The structure is modified to increase the infrared heating system 51 and the hot air reflow system 52. The infrared heating system 51 includes an infrared heating tube 511 and a reflector 512. The reflector 512 is used to transfer more radiation energy generated by the infrared heating tube 511 to the PCB for preheating. The hot air reflow system 52 is arranged at one end of the preheating zone. The hot air reflow system 52 drives the axial flow fan 523 to rotate through the hot air motor 522, so that the gas in the hot air reflow chamber 521 is guided by the volute 524 and blown out from the air outlet plate 526 to preheat the PCB on the track.
Claims
1. A welding device, comprising a preheating zone, a welding zone, and a conveying system arranged in the preheating zone and the welding zone, wherein: The preheating zone is used to preheat the PCB board to be welded, and is characterized in that it also includes: A negative ion atmosphere device is arranged in the preheating zone, and comprises: a mounting seat, a negative ion emitting component and an air outlet pipe; the negative ion emitting component is mounted on the mounting seat, and the negative ion emitting component is used to generate negative ions; the air outlet pipe is mounted on the mounting seat and adjacent to the negative ion emitting component, and the air outlet pipe is provided with a plurality of air outlet holes arranged at intervals; An atmosphere supply system, providing a heated initial mixed gas containing an inert gas and a reducing gas to the gas outlet pipe; When the atmosphere supply system provides the initial mixed gas to the gas outlet pipe and the negative ion emitting component is energized, the initial mixed gas is ejected from the gas outlet hole of the gas outlet pipe and blown toward the negative ion emitting component to form a gas mixture containing the inert gas and the negatively charged reducing gas, and the gas mixture removes the oxide layer on the surface of the PCB board and preheats the PCB board.
2. The welding equipment according to claim 1, characterized in that: The mounting seat includes a base, a left fixing part and a right fixing part, the left fixing part is installed on the left side of the base, the right fixing part is installed on the right side of the base, and the air outlet pipe is arranged between the left fixing part and the right fixing part; a plurality of the negative ion emitting components arranged at intervals are respectively installed on the left fixing part and the right fixing part.
3. The welding equipment according to claim 2, characterized in that: The base is provided with a groove, and the air outlet pipe is arranged in the groove.
4. The welding equipment according to claim 2, characterized in that: Each of the negative ion emitting components comprises a negative ion emitting head and a carbon brush installed on the upper end of the negative ion emitting head. The negative ion emitting head of each of the negative ion emitting components is respectively connected to a negative ion controller.
5. The welding equipment according to claim 1, characterized in that: The air outlet pipe is in the shape of an elongated strip, and the air outlet holes are arranged at intervals along the length direction of the air outlet pipe. An air inlet is arranged at one end of the air outlet pipe, and the total cross-sectional area of the air outlet holes is smaller than the cross-sectional area of the air inlet.
6. The welding equipment according to claim 1, characterized in that: The preheating zone is sealed by a shell cover, a plate inlet is provided at one end of the preheating zone, a first flexible windshield curtain is provided at the plate inlet, the other end of the preheating zone is connected to the welding zone, and a second flexible windshield curtain is provided at the connection between the preheating zone and the welding zone.
7. The welding equipment according to claim 1, characterized in that: An atmosphere concentration detection device is also provided for detecting the concentrations of the inert gas and the reducing gas.
8. The welding equipment according to claim 1, characterized in that: There are multiple negative ion atmosphere devices, each of which is arranged at intervals. Each of the negative ion atmosphere devices is installed below the conveying system, and the negative ion atmosphere device is 5-10 mm away from the bottom surface of the PCB board.
9. The welding equipment according to claim 1, characterized in that: The negative ion atmosphere device is installed in the preheating zone through a bottom plate, and the bottom plate is a non-conductive bottom plate; the conveying system is inclined upward at an angle of 3-7° to the horizontal direction.
10. The welding equipment according to claim 1, characterized in that: A hot air reflow system is also provided, and the hot air reflow system is arranged at one end of the preheating zone to provide energy required for preheating the PCB board.