Brown oxidation auxiliary clamp
By designing the browning auxiliary fixture of the inclined cavity wall and the drainage groove, the problem of the clamp mark on the bottom of the copper block in the existing technology is solved, the bonding force between the copper block and the PCB is improved, and it is suitable for copper blocks of different sizes and structures. Achieved better browning effect and versatility.
Patent Information
- Application Number
- CN202420359767.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-26
- Publication Date
- 2024-10-22
- Estimated Expiration
- 2034-02-26
AI Technical Summary
Existing browning fixtures easily form fixture marks when the bottom surface of the copper block contacts, resulting in insufficient bonding force between the copper block and the PCB. It is especially suitable for through-buried structures, but not for internally buried structures.
An auxiliary browning fixture is designed. The accommodation cavity adopts a sloped cavity wall design. The top through-hole and the bottom through-hole have no mesh, ensuring that the top, bottom and sides of the copper block are exposed and can fully contact with the browning potion. , and promote the flow of liquid medicine through the drainage slot, suitable for copper blocks of different sizes.
It achieves a good browning effect of the copper block, improves the bonding force between the copper block and the PCB, is suitable for embedded structures, has strong versatility and low cost.
Smart Images

Figure CN221886815U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of PCB (Printed Circuit Board), in particular to a browning auxiliary clamp. Background Art
[0002] To improve the heat dissipation effect of electronic components, designers usually choose to embed copper blocks in the PCB at the corresponding position of the electronic components. In order to ensure the reliability of the copper block embedded PCB product, the copper block will be browned to improve its bonding strength. However, due to the small size of the copper block, it cannot be directly passed through the browning line, and a pad fixture is required to assist in production. Most of the browning pad fixtures currently used in the industry are designed as Figure 1 and Figure 2 The hollow grid-shaped stepped groove shown in the figure has a size adapted to the size of the copper block 7. It is appropriately enlarged to ensure that the copper block 7 can be normally placed in without affecting the browning of the side walls of the copper block 7. The hollow design of the bottom of the fixture ensures that the browning solution can be discharged normally without causing solution residue.
[0003] However, this browning fixture still has a big disadvantage: Figure 3 and Figure 4 As shown, a browning fixture mark will appear on the side of the copper block 7 that contacts the bottom of the hollow grid. For PCB products with embedded copper blocks, such poor browning will affect the reliability of the product, and problems such as delamination and bubbling are likely to occur between the copper block 7 and the PCB. Therefore, such browning fixtures are only suitable for PCB products with through-buried structures (the upper and lower surfaces of the copper block 7 are exposed to the outer layer), and are not suitable for PCB products with embedded structures (only the upper surface of the copper block 7 is exposed to the outer layer). Utility Model Content
[0004] The utility model aims to provide a browning auxiliary clamp to overcome the defect of the prior art that browning clamp marks are easily formed on the bottom surface of the copper block.
[0005] To achieve this purpose, the utility model adopts the following technical solutions:
[0006] A browning auxiliary fixture comprises a bearing structure body, wherein the bearing structure body is provided with a receiving cavity for placing a copper block to be browned;
[0007] The accommodating cavity includes: a top through-hole and a bottom through-hole respectively arranged on the opposite side surfaces of the bearing structure body, and a cavity wall surrounding the top through-hole and the bottom through-hole; the cavity wall is an inclined surface with an inclination angle relative to the bottom through-hole.
[0008] Optionally, a drainage groove is provided on the cavity wall.
[0009] Optionally, the drainage groove extends from the top end of the slope to the bottom end of the slope.
[0010] Optionally, there are multiple drainage grooves, which are evenly spaced on the cavity wall.
[0011] Optionally, the width of the drainage groove is 2 mm, and the distance between two adjacent drainage grooves is 4 mm.
[0012] Optionally, the top through-hole and the bottom through-hole have the same shape, and a center connecting line between the top through-hole and the bottom through-hole is perpendicular to the opposite side surfaces of the bearing structure body.
[0013] Optionally, the top through opening and the bottom through opening are circular or polygonal in shape.
[0014] Optionally, there are multiple accommodating cavities, which are arranged in a matrix on the bearing structure body.
[0015] Optionally, at least one of the area of the top through-hole, the area of the bottom through-hole, and the inclination angle of the cavity wall of at least two of the accommodating cavities is different.
[0016] Compared with the prior art, the beneficial effects of the utility model are:
[0017] Different from conventional browning auxiliary fixtures, the embodiment of the utility model has an unconventional inclined surface design for the cavity wall of the accommodating cavity of the browning auxiliary fixture. Based on the inclined cavity wall, the copper block to be browned will be suspended and stuck at a certain depth position in the accommodating cavity after being placed in the accommodating cavity; at this time, since the bottom through-hole of the accommodating cavity has no grid design, the top surface, bottom surface and side surface of the copper block to be browned are all exposed to the outside and can be fully in contact with the browning solution, so the copper block can achieve a good browning effect in the browning process, and improve the subsequent bonding strength between the copper block and the PCB.
[0018] At the same time, the accommodating cavity of the browning auxiliary clamp has a certain depth, and the cross-sectional areas at different depths are different, so that copper blocks of different sizes to be browned, when placed in accommodating cavities of the same specifications, will be suspended and stuck at different depths of the accommodating cavities, and good browning effects can be obtained. Therefore, the browning auxiliary clamp of the embodiment of the utility model can be suitable for copper blocks of different thicknesses and widths, realizing multiple uses of one clamp, strong versatility, and cost reduction. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative work.
[0020] Figure 1 It is a top view of the existing browning auxiliary fixture.
[0021] Figure 2 It is a side view of the existing browning auxiliary fixture.
[0022] Figure 3 This is a diagram showing the browning effect of the top surface of the copper block after browning using the existing browning auxiliary fixture.
[0023] Figure 4 This is a diagram showing the browning effect of the bottom surface of the copper block after browning is completed using the existing browning auxiliary fixture.
[0024] Figure 5 A top view of the browning auxiliary clamp provided in an embodiment of the utility model.
[0025] Figure 6 A side view of the browning auxiliary clamp provided in an embodiment of the utility model.
[0026] Figure 7 A three-dimensional diagram of the browning auxiliary fixture after carrying the copper block provided by an embodiment of the utility model.
[0027] Figure 8 A side view of the browning auxiliary fixture after carrying the copper block provided by an embodiment of the utility model.
[0028] Description of reference numerals:
[0029] The bearing structure body 1, the accommodating cavity 2, the top through-hole 3, the bottom through-hole 4, the cavity wall 5, the drainage groove 6, and the copper block 7. DETAILED DESCRIPTION
[0030] In order to make the utility model's purpose, features, and advantages more obvious and easy to understand, the following will be combined with the drawings in the utility model embodiments to clearly and completely describe the technical solutions in the utility model embodiments. Obviously, the embodiments described below are only part of the utility model embodiments, not all of the embodiments. Based on the embodiments in the utility model, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the utility model.
[0031] In the prior art, the bottom of the receiving cavity 2 of the browning auxiliary fixture is designed to Figure 1 and Figure 2 The hollow grid shape shown causes part of the bottom surface of the copper block 7 to be in close contact with the grid during use, resulting in that part of the bottom surface of the copper block 7 cannot be well browned, ultimately affecting the bonding reliability between the copper block 7 and the PCB.
[0032] To this end, an embodiment of the utility model provides a browning auxiliary clamp to improve the problem of clamp marks on the bottom surface of the copper block 7 after browning, enhance the bonding strength of the embedded structure PCB, and can be used to place copper blocks 7 of various sizes to enhance versatility.
[0033] For details, please refer to Figure 5 and Figure 6 The browning auxiliary fixture provided by the embodiment of the utility model comprises a bearing structure body 1, and the bearing structure body 1 is provided with a receiving cavity 2 for placing a copper block 7 to be browned;
[0034] The accommodating cavity 2 includes: a top through-hole 3 and a bottom through-hole 4 which are respectively arranged on the opposite side surfaces of the supporting structure body 1, and a cavity wall 5 which is surrounded between the top through-hole 3 and the bottom through-hole 4; the cavity wall 5 is an inclined surface with an inclination angle relative to the bottom through-hole 4, and the size of the inclination angle is not limited.
[0035] It can be understood that the accommodating cavity 2 needs to be adapted to the size of the copper block 7 to be browned, that is, the top through-hole 3 of the accommodating cavity 2 is larger than the cross-sectional size of the copper block 7 to be browned, and the bottom through-hole 4 of the accommodating cavity 2 is smaller than the cross-sectional size of the accommodating cavity 2, so as to ensure that the copper block 7 to be browned can be placed into the accommodating cavity 2 from the top and will not fall out from the bottom of the accommodating cavity 2.
[0036] Different from the conventional browning auxiliary clamp, the embodiment of the utility model has an unconventional structural design for the accommodating cavity 2 of the browning auxiliary clamp: the cavity wall 5 adopts an inclined surface design. Figure 7 and Figure 8 As shown, based on the inclined cavity wall 5, the copper block 7 to be browned will be suspended and stuck at a certain depth position in the accommodating cavity 2 after being placed in the accommodating cavity 2; at this time, the bottom through-hole 4 of the accommodating cavity 2 does not need a grid design, and the top surface, bottom surface and side surface of the copper block 7 to be browned are exposed to the outside and can fully contact with the browning solution. Therefore, the copper block 7 can achieve a good browning effect in the browning process, thereby improving the subsequent bonding strength between the copper block 7 and the PCB.
[0037] At the same time, the accommodating cavity 2 of the browning auxiliary fixture has a certain depth, and the cross-sectional areas at different depth positions are different, so that when copper blocks 7 to be browned of different sizes are placed in the accommodating cavity 2 of the same specification, they will be suspended and stuck at different depth positions of the accommodating cavity 2, such as Figure 8 As shown, these copper blocks 7 can all achieve good browning effects, so the browning auxiliary fixture of the embodiment of the utility model can be used for browning copper blocks 7 of different thicknesses and widths, achieving multiple uses of one fixture, strong versatility, and cost reduction.
[0038] In practical applications, the top through-hole 3 and the bottom through-hole 4 may have the same or different shapes (such as circular, polygonal, etc.), and the centers of the top through-hole 3 and the bottom through-hole 4 may be aligned or not, as long as the cavity wall 5 of the accommodating cavity 2 is ensured to be an inclined surface. In order to reduce the difficulty and cost of manufacturing, in an optional embodiment, the top through-hole 3 and the bottom through-hole 4 have the same shape, and the center connecting line of the top through-hole 3 and the bottom through-hole 4 is perpendicular to the opposite side surfaces of the supporting structure body 1.
[0039] For example, a 4 mm thick hard substrate is selected and milled into Figure 5 The structure shown has beveled edges on all sides and a hollowed-out middle, and the width of the slopes on all sides is 10 mm, and the length and width of the bottom through-hole 4 are 10 mm and 5 mm respectively. It should be noted that the above thickness, length and width are not fixed, and are only suitable for the fixture design of most copper blocks 7. If the size of the copper block 7 is too large or too small, the width and thickness can be appropriately increased or decreased according to the actual size of the copper block 7. In short, it is necessary to ensure that the diagonal width of the bottom through-hole 4 is smaller than the minimum width of the copper block 7 to prevent the copper block 7 from falling out of the bottom through-hole 4.
[0040] In order to improve the effect of the fixture in draining the solution and promote the uniformity of the flow of the browning solution around the copper block 7, in the embodiment of the utility model, a drainage groove 6 is further provided on the cavity wall 5 of the accommodating cavity 2. Through the drainage groove 6, the browning solution can flow on the cavity wall 5 to ensure the browning effect of the side wall of the copper block 7.
[0041] Furthermore, the drainage groove 6 can be made by milling, extending from the top of the inclined surface to the bottom of the inclined surface. The number of the drainage grooves 6 is determined by the width of the four sides, and can be multiple, and evenly spaced on the cavity wall 5. For example, Figure 7 As shown, the width of the drainage groove 6 is 2 mm, and the distance between two adjacent drainage grooves 6 is 4 mm.
[0042] In addition, if Figure 7 As shown, the number of the accommodating cavities 2 can be multiple, and they are arranged in a matrix on the bearing structure body 1. It can be understood that the specifications of each accommodating cavity 2, such as the area and shape of the top through-hole 3, the area and shape of the bottom through-hole 4, the inclination angle of the cavity wall 5, etc., can be the same or different, and can be flexibly designed according to application requirements, and this embodiment does not limit this.
[0043] As described above, the above embodiments are only used to illustrate the technical solutions of the utility model, rather than to limit it. Although the utility model has been described in detail with reference to the aforementioned embodiments, those skilled in the art should understand that the technical solutions described in the aforementioned embodiments can still be modified, or some of the technical features can be replaced by equivalents. However, these modifications or replacements do not deviate the essence of the corresponding technical solutions from the spirit and scope of the technical solutions of the various embodiments of the utility model.
Claims
1. A browning auxiliary fixture, comprising a bearing structure body (1), characterized in that: The supporting structure body (1) is provided with a receiving cavity (2) for placing the copper block (7) to be browned; The accommodating cavity (2) comprises: a top through-hole (3) and a bottom through-hole (4) respectively arranged on two opposite side surfaces of the bearing structure body (1), and a cavity wall (5) arranged between the top through-hole (3) and the bottom through-hole (4); the cavity wall (5) is an inclined surface having an inclination angle relative to the bottom through-hole (4).
2. The browning auxiliary fixture according to claim 1, characterized in that: The cavity wall (5) is provided with a drainage groove (6).
3. The browning auxiliary fixture according to claim 2, characterized in that: The drainage groove (6) extends from the top end of the inclined surface to the bottom end of the inclined surface.
4. The browning auxiliary fixture according to claim 2, characterized in that: The drainage grooves (6) are multiple in number and are evenly spaced and arranged on the cavity wall (5).
5. The browning auxiliary fixture according to claim 4, characterized in that: The width of the drainage groove (6) is 2 mm, and the distance between two adjacent drainage grooves (6) is 4 mm.
6. The browning auxiliary fixture according to claim 1, characterized in that: The top through-hole (3) and the bottom through-hole (4) have the same shape, and a central connecting line between the top through-hole (3) and the bottom through-hole (4) is perpendicular to the opposite side surfaces of the bearing structure body (1).
7. The browning auxiliary fixture according to claim 1, characterized in that: The top through-hole (3) and the bottom through-hole (4) are circular or polygonal in shape.
8. The browning auxiliary fixture according to claim 1, characterized in that: The number of the accommodating cavities (2) is multiple and they are arranged in a matrix on the bearing structure body (1).
9. The browning auxiliary fixture according to claim 8, characterized in that: At least one of the area of the top through-hole (3), the area of the bottom through-hole (4), and the inclination angle of the cavity wall (5) of at least two of the accommodating cavities (2) is different.