Anti-splashing metal evaporation device
By configuring the material guide channel and purification area on the metal evaporation equipment, combined with the design of the cover to block splash, the problem of splash caused by impurities in the metal evaporation process in the existing technology is solved, and the coating quality and product cleanliness are significantly improved. .
Patent Information
- Application Number
- CN202420306083.6
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-19
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2034-02-19
AI Technical Summary
During the coating process of existing metal evaporation equipment, it is easy for particles to appear on the film surface due to the entry of impurities and splashing when the metal wire is melted, affecting product quality.
An anti-spatter metal evaporation device is designed, which includes a guide device above the molten pool of the evaporation boat. The guide device is equipped with a vertical guide channel and a purification area. The purification area removes metal through multiple buffer zones. Impurities on the wire are removed, and a cover is set above the material guide channel to block splashing molten metal.
It effectively reduces the particle rate of splashing during the coating process, improves the coating quality, and ensures the cleanliness and application performance of the product.
Smart Images

Figure CN221918199U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of coating equipment, in particular to a splash-proof metal evaporation device. Background Art
[0002] Lithium-ion batteries have been widely used in consumer electronics, electric vehicles and other fields. With the continuous development of the battery industry, current collectors with better performance are needed. Composite current collectors are a new type of current collector material, usually made of a polymer film substrate layer and a conductive metal layer plated on both sides of the polymer film substrate layer, forming a "sandwich structure". Compared with pure metal current collectors, the weight of composite current collectors can be reduced by 50% to 80%. At the same time, the thickness of the composite current collector is also reduced by 25%-40% compared to the thickness of the pure metal current collector, so that the space in the battery can be transferred to the electrode active material. The presence of the polymer substrate layer in the composite current collector can reduce the temperature rise of the battery and reduce the risk of thermal runaway of the battery.
[0003] The metal layer on the composite current collector can be formed by chemical plating, evaporation, magnetron sputtering, etc., but chemical plating is relatively polluting to the environment, and the thickness that can be plated by magnetron sputtering at one time is very thin, generally below 0.1 microns, which cannot meet the application requirements of the battery. Evaporation is not only pollution-free, but also has a fast coating speed and can achieve a greater thickness. The current process mainly places the metal wire directly into the evaporation boat and melts the metal wire through the heat on the surface of the evaporation boat. However, in this way, various impurities on and inside the metal wire will enter the evaporation boat, and because the evaporation material contains impurities, it is easy to splash during evaporation. The melting of the metal wire to form droplets is also easy to cause splashing, so that there will be many particles on the surface of the film during coating, affecting product application. Utility Model Content
[0004] The utility model discloses a splash-proof metal evaporation device, aiming to improve the problem that the existing evaporation equipment is prone to splashing due to impurities during evaporation.
[0005] The utility model adopts the following scheme:
[0006] The present application provides a splash-proof metal evaporation device, comprising an evaporation boat suitable for vaporizing a metal wire, a material guiding device is arranged above a molten pool of the evaporation boat, a material guiding channel suitable for the metal wire to enter and perpendicular to the molten pool surface of the evaporation boat is formed in the material guiding device, a cover opening whose opening is larger than that of the material guiding channel is formed at one end of the material guiding device close to the molten pool of the evaporation boat, the cover opening is suitable for shielding splashing metal liquid when the metal wire is liquefied and drips at a position close to the evaporation boat to generate splashing.
[0007] Furthermore, a purification zone is formed in the material guiding channel to remove impurities attached to the metal wire entering the material guiding channel.
[0008] Furthermore, the purification zone includes at least a first buffer zone, a second buffer zone, and a third buffer zone with successively increasing temperatures, and the first buffer zone, the second buffer zone, and the third buffer zone are suitable for respectively dewatering, degassing, and degreasing the metal wire when the metal wire passes through.
[0009] Furthermore, the material guiding channel is provided with a preheating functional zone at a position close to the evaporation boat, and the temperature of the preheating functional zone is 50-100° C. lower than the melting point of the metal wire.
[0010] Furthermore, the cover opening is detachably connected to the material guiding device to facilitate replacement of the cover opening.
[0011] Furthermore, the mask opening is formed in a cylindrical shape or a rectangular parallelepiped shape.
[0012] Furthermore, the bottom surface of the cover port is 3-6 mm above the surface of the molten pool in the evaporation boat.
[0013] Furthermore, the cover mouth is made of high temperature resistant ceramics or alloy.
[0014] Furthermore, the metal wire is aluminum and aluminum alloy wire or copper and copper alloy wire.
[0015] Beneficial effects:
[0016] The utility model provides a material guide channel above the molten pool of the evaporation boat, so that the metal wire can drip into the molten pool of the evaporation boat after melting in the area near the evaporation boat. A cover with an opening larger than the material guide channel is provided at the bottom of the material guide channel to shield the metal liquid from splashing when the metal wire is liquefied and dripping when it is close to the evaporation boat, thereby preventing particles from being generated on the film surface during film coating and affecting product application. Furthermore, a purification zone is provided on the material guide channel, which can greatly reduce the probability of large metal particles splashing out during evaporation and improve the quality of evaporation. Specifically, the purification zone includes a first buffer zone, a second buffer zone, and a third buffer zone, which are respectively used to remove impurities such as moisture, gas, and grease, thereby improving the cleanliness of the metal liquid entering the evaporation boat, greatly reducing the problem of material splashing during evaporation, and helping to improve the quality of evaporation. BRIEF DESCRIPTION OF THE DRAWINGS
[0017] Figure 1 It is a schematic structural diagram of a splash-proof metal evaporation device according to an embodiment of the utility model;
[0018] Icons: material guiding device 1, material guiding channel 11, hood 12, evaporation boat 2, molten pool 21, purification area 3, metal wire 4. DETAILED DESCRIPTION
[0019] Example 1
[0020] Combination Figure 1 The present embodiment provides a splash-proof metal evaporation device, comprising an evaporation boat 2 suitable for vaporizing a metal wire 4, a material guiding device 1 is arranged above a molten pool 21 of the evaporation boat 2, a material guiding channel 11 suitable for the metal wire 4 to enter and vertical to the surface of the molten pool 21 of the evaporation boat 2 is formed in the material guiding device 1, a cover opening 12 whose opening is larger than that of the material guiding channel 11 is formed at one end of the material guiding device 1 close to the molten pool 21 of the evaporation boat 2, and the cover opening 12 is suitable for shielding splashing metal liquid when the metal wire 4 liquefies and drips at a position close to the evaporation boat 2 to generate splashing.
[0021] In this embodiment, the material guide device 1 is a material guide tube, and a material guide channel 11 is formed in the material guide tube. The metal wire 4 can pass through the material guide device 1 to enter the molten pool 21 of the evaporation boat 2 and realize vaporization on the evaporation boat 2. A cover 12 is provided at one end of the material guide device 1 close to the evaporation boat 2. Here, the opening of the cover 12 is larger than the size of the material guide channel 11, so as to form a shield to prevent the metal splashing liquid from flying out and affecting the evaporation effect, and at the same time prevent the metal splashing liquid from splashing onto other parts of the evaporation device. Here, the cover 12 can be made of high-temperature resistant ceramics or other alloy materials, which can be detachably installed on the material guide device 1, so as to facilitate replacement as needed. Of course, in other embodiments, the cover 12 can also be integrally formed on the material guide device 1.
[0022] In this embodiment, the shield opening 12 is formed in a cylindrical or rectangular shape, and its internal hollowness is connected to the material guide channel 11, thereby forming a protective shield with an area larger than the material guide channel 11 to shield the splash caused by the metal liquid of the metal wire 4 when it drips at the dripping position. Preferably, the bottom surface of the shield opening 12 is 3-6 mm above the surface of the molten pool 21 in the evaporation boat 2, so that the splash of the metal liquid can be shielded to the maximum extent, and the material guide channel 11 will not be completely closed at the bottom. Of course, the shape of the shield opening 12 is not limited to a cylindrical or rectangular shape, and other shapes that can be formed to shield the splashing liquid are also within the protection scope of this application.
[0023] In one embodiment, the purification zone 3 is arranged on the material guide device 1, which can act on the material guide channel 11 to remove impurities from the metal wire 4 in the material guide channel 11. Specifically, the purification zone 3 includes at least a first buffer zone, a second buffer zone, and a third buffer zone, which are relatively closed to prevent new impurities from entering during impurity treatment. Here, the first buffer zone, the second buffer zone, and the third buffer zone can be integrated in the same structure in sequence, or they can be arranged in sections. The first buffer zone, the second buffer zone, the third buffer zone, and the entire evaporation boat 2 device are generally in the vacuum chamber of the coating equipment, and the vacuum environment can be used to extract water vapor or impurity gas to improve the impurity removal efficiency. Specifically, the first buffer zone, the second buffer zone, and the third buffer zone are heated at high temperature to evaporate water, gas, and grease and remove them by vacuuming to improve the cleanliness of the metal wire 4. In this embodiment, the first buffer zone, the second buffer zone, and the third buffer zone are all provided with heating devices, and the temperature can be controlled as needed. Specifically, in this embodiment, the temperature of the first buffer zone, the second buffer zone, and the third buffer zone increases in sequence during operation, so as to be used for water removal, adsorbed gas removal, and grease removal, respectively. It should be noted that the temperatures in the first buffer zone, the second buffer zone and the third buffer zone are all lower than the melting point of the metal wire 4 .
[0024] In another embodiment, a preheating functional area is further provided at one end of the material guiding device 1 close to the evaporation boat 2, and the temperature of the preheating functional area is 50-100°C lower than the melting point of the entering metal wire 4, so that the metal wire 4 can be preheated in advance during the entry process, so that the temperature can be quickly increased to achieve rapid melting when it is close to the molten pool 21 of the evaporation boat 2, thereby reducing the problem of increased melting time and increased splashing due to the inability to quickly liquefy near the evaporation boat 2 due to the low temperature.
[0025] In this embodiment, the metal wire 4 is aluminum and aluminum alloy wire or copper and copper alloy wire, or other metal materials suitable for evaporation.
[0026] The evaporation boat 2 device and the evaporation process are prior art and will not be described in detail here.
[0027] The utility model also provides a working process of the anti-splashing metal evaporation device, comprising the following steps:
[0028] S1, the metal wire 4 is introduced into the first buffer zone of the material guiding device 1 to evaporate water, the temperature of the first buffer zone is set to 150-250° C., and the evaporation time is 0.01-3 min;
[0029] S2, continue to guide the metal wire 4 into the second buffer zone to remove the adsorbed gas, the temperature of the second buffer zone is set to 300-400° C., and the adsorbed gas removal time is 0.01-4 min;
[0030] S3, continue to guide the metal wire 4 into the third buffer zone to remove grease, the temperature of the second buffer zone is set to 450-550° C., and the grease removal time is 0.01-5 min;
[0031] S4, continue to introduce the metal wire 4 into the preheating functional area for preheating;
[0032] S5 , the metal wire 4 continues to move until it is evaporated in the evaporation boat 2 .
[0033] In this embodiment, the metal wire 4 is aluminum and aluminum alloy wire or copper and copper alloy wire or other metal materials suitable for evaporation. In this embodiment, the metal liquid is subjected to an evaporation process in the evaporation boat 2 to form the final evaporation product, and the process is prior art and will not be repeated here. For example, the product structure manufactured by the above method is generally a three-layer structure, evaporation metal layer + polymer layer + evaporation metal layer, wherein the evaporation metal is generally aluminum and copper; the polymer layer can be a polymer such as PET, PP, PI, PE, etc. For example, in one embodiment, the metal wire 4 is aluminum wire, the temperature of the first buffer zone is set to 200°C, the dewatering time is 0.05min, the temperature of the second buffer zone is set to 350°C, the time for removing adsorbed gas is 0.05min, the temperature of the third buffer zone is set to 500°C, the time for removing grease is 0.05min, the temperature of the preheating function zone is set to 560°, and the preheating time is 0.05min, so as to achieve a 1μm aluminum layer on both sides of the 6μmPET film. In this embodiment, the occurrence of splashing during the evaporation process is greatly reduced.
[0034] Through the embodiments of the utility model, the probability of splashing out large particles of aluminum during vapor deposition can be greatly reduced, thereby improving the vapor deposition quality.
[0035] It should be understood that the above are only preferred implementations of the present invention, and the protection scope of the present invention is not limited to the above embodiments. All technical solutions under the concept of the present invention belong to the protection scope of the present invention.
[0036] The above description of the drawings used in the implementation manner only shows certain embodiments of the utility model and should not be regarded as limiting the scope. For ordinary technicians in this field, other relevant drawings can be obtained based on these drawings without paying creative work.
Claims
1. A splash-proof metal evaporation device, comprising an evaporation boat suitable for vaporizing a metal wire, characterized in that: A material guiding device is arranged above the molten pool of the evaporation boat, and a material guiding channel suitable for the metal wire to enter and perpendicular to the molten pool surface of the evaporation boat is formed in the material guiding device. A shield opening whose opening is larger than the material guiding channel is formed at one end of the material guiding device close to the molten pool of the evaporation boat, and the shield opening is suitable for shielding splashing molten metal when the metal wire liquefies and drips at a position close to the evaporation boat to generate splashing.
2. The splash-proof metal vapor deposition device according to claim 1, characterized in that: A purification zone is formed in the material guiding channel to remove impurities attached to the metal wire entering the material guiding channel.
3. The splash-proof metal vapor deposition device according to claim 2, characterized in that: The purification zone at least includes a first buffer zone, a second buffer zone, and a third buffer zone, the temperatures of which increase in sequence. The first buffer zone, the second buffer zone, and the third buffer zone are suitable for respectively removing water, air, and grease from the metal wire when the metal wire passes through.
4. The splash-proof metal vapor deposition device according to claim 3, characterized in that: The material guiding channel is provided with a preheating functional zone at a position close to the evaporation boat, and the temperature of the preheating functional zone is 50-100° C. lower than the melting point of the metal wire.
5. The splash-proof metal vapor deposition device according to claim 3, characterized in that: The cover opening is detachably connected to the material guiding device to facilitate replacement of the cover opening.
6. The splash-proof metal vapor deposition device according to claim 1, characterized in that: The cover opening is formed in a cylindrical shape or a rectangular parallelepiped shape.
7. The splash-proof metal vapor deposition device according to claim 6, characterized in that: The bottom surface of the cover port is 3-6 mm above the molten pool surface in the evaporation boat.
8. The splash-proof metal vapor deposition device according to claim 7, characterized in that: The cover opening is made of high temperature resistant ceramics or alloy.
9. The splash-proof metal vapor deposition device according to claim 8, characterized in that: The metal wire is aluminum and aluminum alloy wire or copper and copper alloy wire.
Citation Information
Cited By
Anti-splashing metal evaporation device and metal evaporation process
CN117904582A
Anti-splashing metal evaporation device and metal evaporation process
CN117904582B