Compaction device for rapidly detecting iron-phosphorus ratio of lithium iron phosphate
By designing a compaction device for rapid detection of the iron-phosphorus ratio of lithium iron phosphate, using molds and X-ray fluorescence spectrometers, the problem of low detection efficiency in the existing technology is solved, rapid and accurate iron-phosphorus ratio detection is achieved, and shortened detection time and improves the stability of results.
Patent Information
- Application Number
- CN202322972377.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-02
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2033-11-02
AI Technical Summary
The existing methods for detecting the ratio of lithium iron phosphate to iron to phosphorus have low testing efficiency and require high professional skills of the testing personnel.
A compaction device for quickly detecting the ratio of lithium iron phosphate to iron phosphorus is designed. It includes a hollow-structured mold and a sealing ring. The air is discharged through the exhaust channel and the lithium iron phosphate material is pressed into a cylindrical powder under the applied pressure. film and use X-ray fluorescence spectrometer for rapid detection.
The detection time is greatly reduced from 5 hours with the traditional method to 10 minutes, and the difference between the detection results and the traditional method is small, improving the accuracy and stability of the detection.
Smart Images

Figure CN221926180U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of manufacturing lithium iron phosphate positive electrode materials, in particular to a compacting device for quickly detecting the iron-phosphorus ratio of lithium iron phosphate. Background Art
[0002] The current method for detecting the ratio of lithium iron phosphate to iron phosphorus is:
[0003] 1. The current method is the iron content test method in GB / T 33822-2017. Weigh 0.2±0.0002g in a 100ml beaker, add 10ml (1:1) hydrochloric acid, 10ml (1:1) nitric acid, and 5ml perchloric acid to the beaker in sequence; cover with a watch glass and place on a multi-purpose furnace to dissolve.
[0004] 2. Wait until a lot of white smoke appears and the inner wall of the beaker becomes smokeless and transparent (the sample is completely dissolved), remove the beaker and place it on a ceramic tray to cool to room temperature, and transfer it to a 250ml iodine volumetric flask.
[0005] 3. Add 10ml (1:1) hydrochloric acid to the iodine volumetric bottle and heat it on a stove until it boils (adjust to high heat).
[0006] Remove the bottle and add SnCl2 solution while it is hot until it turns light yellow (shake and drop), cover the bottle stopper and cool to 25±1℃, add 8 drops of sodium tungstate solution to the iodine volumetric flask, add TiCl3 solution until it turns tungsten blue, add 25% potassium dichromate until it is just colorless, add 10ml of sulfuric acid and phosphoric acid mixture (shake a few times to allow it to react fully), add 10 drops of sodium diphenylaminosulfonate indicator (shake a few times to allow it to react fully), titrate with potassium dichromate standard solution, and finally convert it to Fe%. The whole step takes 3h.
[0007] 4. Phosphorus content test method: dilute the sample after the first step digestion to a 250ml volumetric flask, transfer 25ml of the sample solution to a 250 beaker, add 10ml of nitric acid (1:1), add ultrapure water to 100ml, cover with a watch glass, slowly heat to boil, turn on the lowest heat, slowly pour in 50ml of quinolyl ketone to produce ammonium phosphomolybdate precipitate, turn off the heat and keep warm for 5min, take it down and cool, filter it with a G4 sand core filter device, dry it, calculate the weight of the ammonium phosphomolybdate precipitate, and then convert it to P%; the whole step takes 5h.
[0008] 5. Calculation formula: Fe / P=(Fe% / 55.845) / (P% / 30.97).
[0009] The above scheme takes a long time to test. The alternative scheme is the potentiometric titration of iron content in Appendix A of GB / T 33822-2017: in hydrochloric acid solution, stannous chloride is used to reduce trivalent iron to divalent iron, and then sulfuric acid / phosphoric acid mixed acid is added, potassium bisabolite standard solution is used as titrant, and titration test is performed using a potentiometric titrator. The phosphorus content is measured by the quinmolybdate gravimetric method in Appendix B: in an acidic medium, phosphate ions in the phosphorus-containing solution and the quinmolybdate reagent generate a yellow phosphoinositol precipitate, which is filtered, washed, dried and weighed, and the amount of the precipitate is converted to phosphorus content. This scheme also takes a long time and requires high professional skills of the test personnel. Utility Model Content
[0010] The utility model provides a compaction device for quickly detecting the ratio of lithium iron phosphate to iron and phosphorus, and one of the technical problems to be solved is: the technical problem of low test efficiency in the existing test method.
[0011] In view of the above problems in the prior art, according to one aspect disclosed by the present utility model, the present utility model adopts the following technical solution:
[0012] A compaction device for quickly detecting the ratio of lithium iron phosphate to iron phosphorus, comprising:
[0013] A sixth mold, which is a hollow structure;
[0014] a fifth mold, the upper part of which is provided with a first boss extending into the lower part of the hollow structure of the sixth mold, and an exhaust channel is provided in the fifth mold, and the exhaust channel passes through the top of the first boss;
[0015] Two fourth molds are provided in the hollow structure of the sixth mold, and the lithium iron phosphate material to be compacted is placed between the two fourth molds;
[0016] The third mold has a lower portion inserted into the hollow structure of the sixth mold.
[0017] In order to better realize the utility model, a further technical solution is:
[0018] Furthermore, it also includes:
[0019] The first mold is arranged above the third mold.
[0020] Furthermore, the first mold is provided with a first cavity to cooperate with the upper end of the third mold.
[0021] Furthermore, it also includes:
[0022] The second mold is arranged above the first mold.
[0023] Furthermore, an original arc-shaped protrusion is arranged on the upper part of the first mold, and an arc-shaped cavity matching with the original arc-shaped protrusion is arranged on the second mold.
[0024] Furthermore, a sealing ring is arranged between the first boss of the fifth mold and the inner wall of the hollow structure of the sixth mold.
[0025] Furthermore, it also includes:
[0026] A pipe joint is arranged on the fifth mold and communicated with the exhaust channel.
[0027] Furthermore, the fifth mold is replaced by a seventh mold, a second boss is disposed on the upper portion of the seventh mold and can be inserted into the lower portion of the hollow structure of the sixth mold, and a second cavity is also disposed on the seventh mold for accommodating the compacted lithium iron phosphate material.
[0028] Furthermore, a vent hole is provided on the seventh mold, and the vent hole is communicated with the second cavity.
[0029] Compared with the prior art, one of the beneficial effects of the utility model is:
[0030] The utility model discloses a compaction device for quickly detecting the iron-phosphorus ratio of lithium iron phosphate. The data calibration results tested by the device are compared with the traditional results, and the data difference is small. The traditional test method takes 5 hours to output the iron-phosphorus ratio, while the device of the utility model and the corresponding method only take 10 minutes to obtain the iron-phosphorus ratio, greatly reducing the detection time. BRIEF DESCRIPTION OF THE DRAWINGS
[0031] In order to more clearly illustrate the embodiments of the present application document or the technical solutions in the prior art, the drawings required for use in the description of the embodiments or the prior art are briefly introduced below. Obviously, the drawings described below are only references to some embodiments in the present application document. For those skilled in the art, other drawings can be obtained based on these drawings without creative work.
[0032] Figure 1 It is a schematic diagram according to an embodiment of the utility model.
[0033] Figure 2 The structure of the first mold according to one embodiment of the utility model is shown.
[0034] Figure 3 The structure of the second mold according to one embodiment of the utility model is shown.
[0035] Figure 4 It is a front view of a fifth mold according to an embodiment of the utility model.
[0036] Figure 5 It is a top view of a fifth mold according to an embodiment of the utility model.
[0037] Figure 6 It is a structural schematic diagram of a seventh mold according to another embodiment of the utility model.
[0038] Figure 7 It is a schematic structural diagram of a compaction device for rapidly detecting the ratio of lithium iron phosphate to iron phosphorus according to another embodiment of the utility model during material taking.
[0039] The names of the drawings corresponding to the reference numerals are:
[0040] 1-first mold, 2-second mold, 3-third mold, 4-fourth mold, 5-fifth mold, 6-sixth mold, 7-seventh mold, 8-lithium iron phosphate material, 9-first boss, 10-exhaust channel, 11-first cavity, 12-original arc-shaped protrusion, 13-arc-shaped cavity, 14-sealing ring, 15-pipe joint, 16-second boss, 17-second cavity, 18-vent. DETAILED DESCRIPTION
[0041] The present invention is further described in detail below in conjunction with the embodiments, but the implementation manner of the present invention is not limited thereto.
[0042] See also Figure 1 As shown, Figure 1 The structure of a compaction device for quickly detecting the ratio of lithium iron phosphate to iron phosphorus according to an embodiment of the utility model is shown. A compaction device for quickly detecting the ratio of lithium iron phosphate to iron phosphorus comprises:
[0043] The sixth mold 6 is a hollow structure;
[0044] A fifth mold 5, the upper part of which is provided with a first boss 9 extending into the lower part of the hollow structure of the sixth mold 6, and an exhaust channel 10 is provided in the fifth mold 5, and the exhaust channel 10 passes through the top of the first boss 9;
[0045] Two fourth molds 4 are provided in the hollow structure of the sixth mold 6, and the lithium iron phosphate material 8 to be compacted is placed between the two fourth molds 4;
[0046] The third mold 3 , the lower part of which is inserted into the hollow structure of the sixth mold 6 .
[0047] In the above embodiment, by applying pressure to the third mold 3, the third mold 3 moves downward to squeeze the fourth mold 4, and the two fourth molds 4 press the lithium iron phosphate material 8 into a shape that can be quickly tested for the iron-phosphorus ratio. During the compression process, the air in the hollow structure of the sixth mold 6 is discharged through the exhaust channel 10.
[0048] Combination Figure 2 and Figure 3 As shown, Figure 2 The structure of the first mold according to one embodiment of the utility model is shown. Figure 3 The structure of the second mold according to an embodiment of the utility model is shown, and the first mold 1 is arranged above the third mold 3. The first mold 1 can cooperate with the upper end of the third mold 3 by setting a first cavity 11. The second mold 2 is arranged above the first mold 1. An original arc-shaped protrusion 12 is arranged on the upper part of the first mold 1, and an arc-shaped cavity 13 cooperating with the original arc-shaped protrusion 12 is arranged on the second mold 2. Through the technical solution of this embodiment, the first mold 1 and the second mold 2 increase the force-bearing area, so that the third mold 3 is more evenly stressed.
[0049] Recombination Figure 4 and Figure 5 As shown, Figure 4 This is a front view of a fifth mold according to an embodiment of the utility model. Figure 5 This is a top view of the fifth mold according to an embodiment of the present utility model. A sealing ring 14 is arranged between the first boss 9 of the fifth mold 5 and the inner wall of the hollow structure of the sixth mold 6 .
[0050] The pipe joint 15 is arranged on the fifth mold 5 and communicated with the exhaust channel 10. A hose can be connected to the pipe joint 15.
[0051] After the lithium iron phosphate material 8 is pressed, the lithium iron phosphate material 8 needs to be taken out. In order to facilitate the removal of the lithium iron phosphate material 8, the fifth mold 5 is replaced by the seventh mold 7. Figure 6 and Figure 7 As shown, Figure 6 is a structural schematic diagram of a seventh mold according to another embodiment of the utility model, Figure 7 This is a schematic diagram of the structure of a compaction device for rapid detection of the iron-phosphorus ratio of lithium iron phosphate according to another embodiment of the utility model when taking materials. The upper part of the seventh mold 7 is provided with a second boss 16 capable of being inserted into the lower part of the hollow structure of the sixth mold 6. The seventh mold 7 is also provided with a second cavity 17 for accommodating the compacted lithium iron phosphate material 8. The seventh mold 7 is provided with a vent hole 18, and the vent hole 18 is connected to the second cavity 17.
[0052] The seventh mold 7 has a splicing function, and after applying a certain pressure to the lithium iron powder material, a complete and undamaged cylindrical powder tablet with a thickness of about 3 mm and a diameter of 3 cm is obtained, which is conducive to test stability and accuracy. The calibrated XRF is then used to quickly detect the iron-phosphorus ratio of lithium iron phosphate.
[0053] When testing with the above device, first place the lithium iron phosphate powder in the above mold, press the powder into a sheet under a certain pressure, and the powder density reaches 2.5g / cm 3 Close to the metal density, then take out the powder tablet, the powder tablet must be intact, the contact surface is smooth and flat, the equipment can be a handheld X-ray fluorescence spectrometer, the brand can be Olympus VANTA (XRF), select the geochemical mode (qualitative and semi-quantitative analysis of non-metallic compounds), measure the powder tablet, place the powder tablet in an environment without magnetic field interference, place the XRF measurement window directly at the center of the tablet, select the element to be tested, click measurement, and the Fe% and P% content will be obtained in 20S.
[0054] Tablet production: A custom mold is used to apply pressure to the top of the second mold 2. The tablets pressed under 1T pressure for 20s and 2T pressure for 20s are easy to break or fall off. The tablets pressed under 3T pressure for 20s are complete and not easy to damage. Therefore, 3T pressure is used, and the tablets are formed into a cylindrical shape in the sixth mold 6. After holding the pressure for 20s, the fifth mold 5 is removed, and then the seventh mold 7 is spliced and placed under the sixth mold 6. Then pressure is applied to the top of the second mold 2. When the fourth mold 4 and the material fall into the internal groove of the seventh mold 7, the fourth mold 4 is removed, and the seventh mold 7 is disassembled to take out the complete material tablet.
[0055] XRF calibration: First, select three gradients of iron-phosphorus content of lithium iron phosphate materials to make powder tablets, point the XRF window film (2cm in diameter) to the center of the tablet, select the geochemical mode, and perform linear calibration with the measured data and the known content, then perform blind testing and compare with traditional test data. The results are as follows:
[0056]
[0057] Retest results after calibration:
[0058]
[0059] Comparison with traditional detection methods:
[0060]
[0061]
[0062] Through the above experiments, it can be found that the iron-phosphorus ratio of lithium iron phosphate can be quickly and accurately detected by using the above device and the corresponding detection method.
[0063] The various embodiments in this specification are described in a progressive manner, and each embodiment focuses on the differences from other embodiments. The same or similar parts between the various embodiments can be referenced to each other.
[0064] The "one embodiment", "another embodiment", "embodiment", etc. mentioned in this specification refer to the specific features, structures or characteristics described in conjunction with the embodiment included in at least one embodiment generally described in this application. The same expression appearing in multiple places in the specification does not necessarily refer to the same embodiment. Further, when a specific feature, structure or characteristic is described in conjunction with any embodiment, it is claimed that the realization of such feature, structure or characteristic in conjunction with other embodiments also falls within the scope of the utility model.
[0065] Although the utility model is described herein with reference to a plurality of illustrative embodiments of the utility model, it should be understood that those skilled in the art may devise many other modifications and implementations that fall within the scope and spirit of the principles disclosed herein. More specifically, within the scope of the disclosure and claims of the present application, a variety of variations and improvements may be made to the components and / or layout of the subject combination layout. In addition to variations and improvements made to the components and / or layout, other uses will also be apparent to those skilled in the art.
Claims
1. A compaction device for rapid detection of lithium iron phosphate to iron phosphorus ratio, characterized in that include: a sixth mold (6) having a hollow structure; A fifth mold (5), the upper part of which is provided with a first boss (9) extending into the lower part of the hollow structure of the sixth mold (6), and an exhaust channel (10) is provided in the fifth mold (5), and the exhaust channel (10) passes through the top of the first boss (9); Two fourth molds (4) are arranged in the hollow structure of the sixth mold (6), and the lithium iron phosphate material (8) to be compacted is placed between the two fourth molds (4); The third mold (3), the lower part of which is inserted into the hollow structure of the sixth mold (6).
2. The compacting device for rapid detection of lithium iron phosphate to phosphorus ratio according to claim 1, characterized in that Also includes: The first mold (1) is arranged above the third mold (3).
3. The compacting device for rapid detection of lithium iron phosphate to phosphorus ratio according to claim 2, characterized in that The first mold (1) is provided with a first cavity (11) to cooperate with the upper end of the third mold (3).
4. The compaction device for rapid detection of lithium iron phosphate to phosphorus ratio according to claim 3, characterized in that Also includes: The second mold (2) is arranged above the first mold (1).
5. The compacting device for rapid detection of lithium iron phosphate to iron phosphorus ratio according to claim 4, characterized in that An original arc-shaped protrusion (12) is arranged on the upper part of the first mold (1), and an arc-shaped cavity (13) matching with the original arc-shaped protrusion (12) is arranged on the second mold (2).
6. The compaction device for rapid detection of lithium iron phosphate to phosphorus ratio according to claim 1, characterized in that A sealing ring (14) is provided between the first boss (9) of the fifth mold (5) and the inner wall of the hollow structure of the sixth mold (6).
7. The compaction device for rapid detection of lithium iron phosphate to phosphorus ratio according to claim 1, characterized in that Also includes: A pipe joint (15) is arranged on the fifth mold (5) and is connected to the exhaust channel (10).
8. The compacting device for rapid detection of the ratio of lithium iron phosphate to iron phosphorus according to any one of claims 1 to 7, characterized in that The fifth mold (5) is replaced by a seventh mold (7), the upper part of the seventh mold (7) is provided with a second boss (16) capable of being inserted into the lower part of the hollow structure of the sixth mold (6), and the seventh mold (7) is also provided with a second cavity (17) for accommodating the compacted lithium iron phosphate material (8).
9. The compacting device for rapid detection of lithium iron phosphate to phosphorus ratio according to claim 8, characterized in that The seventh mold (7) is provided with a vent hole (18), and the vent hole (18) is communicated with the second cavity (17).