Pixel doping diffusion test structure
By setting trench isolation and light blocking structures on the test wafer to simulate the actual structure of the CMOS image sensor, the problem of inaccurate pixel doping diffusion testing is solved and the accuracy of doping calibration is improved, especially at small pixel sizes.
Patent Information
- Application Number
- CN202323376147.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-12-11
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2033-12-11
AI Technical Summary
The pixel doping diffusion test in the existing technology is inaccurate, especially in small pixel sizes, resulting in insufficient calibration accuracy of doping concentration, and the impact of the actual manufacturing structure on the doping concentration cannot be accurately reflected.
A test structure for pixel doping diffusion was designed. By setting up a trench isolation structure and a light blocking structure on the test wafer, it simulated the structure in the actual CMOS image sensor, thereby modulating the doping distribution during the test stage and improving the test accuracy.
By simulating the actual structure, the test results are closer to the actual doping effect, reducing the deviation between the test and the actual doping effect, and improving the accuracy of doping calibration, especially at small pixel sizes.
Smart Images

Figure CN221928075U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of pixel doping diffusion testing, in particular to a pixel doping diffusion testing structure. Background Art
[0002] An image sensor is a device that converts light signals into electrical signals. Generally, large-scale commercial image sensor chips include two categories: charge coupled device (CCD) and complementary metal oxide semiconductor (CMOS) image sensor chips.
[0003] Compared with traditional CCD sensors, CMOS image sensors have the characteristics of low power consumption, low cost and compatibility with CMOS technology, so they are increasingly widely used. Now CMOS image sensors are not only used in consumer electronics, such as miniature digital cameras (DSC), mobile phone cameras, camcorders and digital single-lens reflex cameras (DSLR), but also in automotive electronics, monitoring, biotechnology and medicine.
[0004] CMOS image sensors can be divided into two types of image sensors, front-illuminated and back-illuminated, according to the different paths of incident light entering the photodiode. Front-illuminated refers to an image sensor in which incident light enters the photodiode from the side close to the circuit connection layer, while back-illuminated refers to an image sensor in which incident light enters the photodiode from the side away from the circuit connection layer. Among them, the photodiode is mainly formed by N-type doping of a P-type doped silicon substrate to form a PN junction. In addition, the preparation of transistors in pixel units, the preparation of isolation between pixel units, and the preparation of isolation between transistors in pixel units are mostly based on N-type doping and P-type doping. The concentration of N-type doping and P-type doping needs to be accurately controlled to ensure that the CMOS image sensor has good performance.
[0005] In order to accurately control the concentration of N-type doping and the concentration of P-type doping, it is usually necessary to test the distribution of N-type doping and P-type doping diffusion in advance. The doping calibration of large pixels is generally performed on the optical sheet, that is, N-type doping or P-type doping is performed on a clean wafer by IMP (ion implantation), and then the longitudinal distribution of doping diffusion is calibrated by SIMS (secondary ion mass spectrometry) testing. The doping diffusion is usually set to be isotropic in the simulation. However, as the pixel size gradually decreases, the challenge of pixel doping simulation gradually increases. The doping concentration increases, and even the diffusion temperature is high. The accuracy of simulation using the calibration parameters of large pixels can no longer meet the requirements. Moreover, in the actual production of CMOS image sensors, there are other structures that affect the doping concentration. The test results and calibration results of doping tests on clean wafers are inaccurate and deviate from the actual doping effect. Utility Model Content
[0006] In order to overcome the shortcomings and deficiencies in the prior art, the purpose of the present invention is to provide a pixel doping diffusion test structure to solve the problem of inaccurate pixel doping diffusion test in the prior art.
[0007] The purpose of the utility model is achieved through the following technical solutions:
[0008] The utility model provides a pixel doping diffusion test structure, which is suitable for the pixel doping diffusion test method as described above, and the test structure comprises:
[0009] A test wafer, wherein a doped region is provided in the test wafer;
[0010] A test modulation structure is provided on the front side of the test wafer to modulate the doping of the test wafer.
[0011] In one embodiment, the test modulation structure includes at least one of a trench isolation structure and a light blocking structure.
[0012] In one embodiment, the trench isolation structure extends into the test wafer to modulate the doping process based on the trench isolation structure located inside the test wafer; and / or, the light blocking structure is at least located on the test wafer to modulate the doping process based on the light blocking structure located on the test wafer.
[0013] In one embodiment, the arrangement of the trench isolation structure and the doped region and the arrangement of the light blocking structure and the doped region includes at least one of the following: the projections of the trench isolation structure and the doped region on the surface of the test wafer at least partially overlap; and the projections of the doped region on the surface of the test wafer cover the projections of the openings between adjacent trench isolation structures on the surface of the test wafer; and the projections of the light blocking structure and the doped region on the surface of the test wafer are staggered.
[0014] In one embodiment, the projection of the trench isolation structure and the doped region on the surface of the test wafer partially overlap, the projection of the doped region on the surface of the test wafer covers the projection of the opening between adjacent trench isolation structures on the surface of the test wafer, and the projection of the light blocking structure on the surface of the test wafer is located outside the doped region.
[0015] In one embodiment, the trench isolation structure includes at least one of a first trench isolation structure completely offset from the light blocking structure, a second trench isolation structure partially overlapping the light blocking structure, and a third trench isolation structure completely overlapping the light blocking structure.
[0016] In one embodiment, the light blocking structure includes at least one of a first light blocking structure completely offset from the trench isolation structure, a second light blocking structure partially overlapping with the trench isolation structure, and a third light blocking structure completely overlapping with the trench isolation structure, and / or the trench isolation structure adopts a shallow trench isolation structure, and the light blocking structure adopts photoresist.
[0017] In one embodiment, the image sensor includes a plurality of pixel units arranged in an array and having a size less than 3 μm×3 μm; and / or, the test structure prepared by the test wafer includes a plurality of test units, and the test units correspond to the pixel units of the image sensor; and / or, the arrangement of the test modulation structure includes a proportion of the test modulation structure to the test unit that increases as the size of the test unit decreases.
[0018] In one embodiment, the doped region includes at least one of an N-type doped layer and a P-type doped layer.
[0019] In one embodiment, the doping region includes an N-type doping layer and two P-type doping layers, and the N-type doping layer is located between the two P-type doping layers; and / or, the doping region includes an N-type doping layer and a P-type doping layer, and the N-type doping layer is located below the P-type doping layer; and / or, the doping region includes a first doping layer doped with a first relative atomic mass and a second doping layer doped with a second relative atomic mass less than the first relative atomic mass, and the second doping layer is located above the first doping layer.
[0020] The beneficial effect of the utility model is that the doping of the test wafer is modulated by setting a test modulation structure on the front side of the test wafer, and then a doping diffusion test is performed on the test wafer provided with the test modulation structure, so that the influence of the test modulation structure on the doping distribution of the doping area in the test wafer can be tested, so that the test result is closer to the actual doping effect, so as to facilitate better calibration of the doping. BRIEF DESCRIPTION OF THE DRAWINGS
[0021] Figure 1 It is a schematic diagram of the structure of the test wafer in the first embodiment of the utility model;
[0022] Figure 2a-2c It is a schematic diagram of the flow structure of the testing method in the first embodiment of the present utility model;
[0023] Figure 3 It is the doping distribution condition tested by the test method in the first embodiment of the utility model;
[0024] Figure 4 It is a schematic diagram of the structure of the test wafer in the second embodiment of the utility model;
[0025] Figure 5a-5c It is a schematic diagram of the flow structure of the testing method in the second embodiment of the present utility model;
[0026] Figure 6 It is the doping distribution condition tested by the test method in the second embodiment of the present utility model;
[0027] Figure 7 This is one of the structural schematic diagrams of the test wafer of the third embodiment of the utility model;
[0028] Figure 8 This is the second structural schematic diagram of the test wafer of the third embodiment of the utility model;
[0029] Fig. 9 This is the third structural schematic diagram of the test wafer of the third embodiment of the utility model;
[0030] Fig.10 This is the fourth structural diagram of the test wafer of the third embodiment of the utility model;
[0031] Fig.11 This is the fifth structural diagram of the test wafer of the third embodiment of the utility model;
[0032] Fig.12 This is the sixth structural diagram of the test wafer of the third embodiment of the utility model;
[0033] Fig.13 This is the seventh structural diagram of the test wafer of the third embodiment of the utility model;
[0034] Figures 14a-14d The third embodiment of the present utility model corresponds to Fig.10 A schematic diagram of the flow structure of a test method for testing a wafer;
[0035] Fig.15 This is a schematic diagram of the structure of a test wafer according to a fourth embodiment of the utility model;
[0036] Figures 16a-16d It is a schematic diagram of the flow structure of the testing method in the fourth embodiment of the present utility model;
[0037] Fig.17 This is a schematic diagram of the structure of a test wafer according to a fifth embodiment of the present utility model;
[0038] Figures 18a-18d It is a schematic diagram of the flow structure of the testing method in the fifth embodiment of the present utility model.
[0039] Fig.19 It is a structural schematic diagram of another test chip in the fifth embodiment of the utility model. DETAILED DESCRIPTION
[0040] In order to further explain the technical means and effects adopted by the present invention to achieve the predetermined purpose of the present invention, the specific implementation method, structure, features and effects of the pixel doping diffusion test structure proposed by the present invention are described in detail below in conjunction with the accompanying drawings and preferred embodiments:
[0041] [Example 1]
[0042] Figure 1 Schematic diagram of the structure of the test structure in the first embodiment of the present utility model. Figure 1 As shown, a pixel doping diffusion test structure provided by the first embodiment of the utility model includes: a test wafer 10, in which a doping region 11 is provided. A test modulation structure is provided on the front of the test wafer 10 to modulate the doping of the test wafer 10. Since the structure on the wafer has an influence on the doping concentration in the actual production of the CMOS image sensor, the test modulation structure is used in the test stage to simulate the actual structure, so that the doping effect in the wafer test stage is closer to the actual doping effect, and the deviation between the test stage and the actual doping effect is reduced, so as to better calibrate the doping in practice.
[0043] The test modulation structure includes at least one of a trench isolation structure 12 and a light blocking structure 13, so that the doping effect in the wafer test stage is closer to the actual doping effect. In this embodiment, the test modulation structure is a trench isolation structure 12, so that the influence of the trench isolation structure 12 on the doping effect can be tested. It should be noted that other conditions of the test structure can be based on the existing design of the doping simulation in the preparation of the CMOS image sensor using a SIMS-based test method, for example, the injection energy and injection dose when the doping region is formed can correspond to the actual device.
[0044] Further, the trench isolation structure 12 extends into the test wafer 10, so as to modulate the doping process based on the trench isolation structure 12 located inside the test wafer 10. That is, in the subsequent step of forming the doping region 11, the doping process is performed in the presence of the trench isolation structure 12, which can modulate the distribution of doping ions during the ion implantation process of the doping region 11, and improve the test accuracy in the subsequent test process. In this embodiment, the trench isolation structure 12 adopts a shallow trench isolation structure.
[0045] In one example, the projection of the doped region 11 on the surface of the test wafer 10 covers the projection of the opening between adjacent trench isolation structures 12 on the surface of the test wafer 10; in a further example, there is a partial overlap between the projections of the trench isolation structure 12 and the doped region 11 on the surface of the test wafer 10; in another further example, there is a complete overlap between the projections of the trench isolation structure 12 and the doped region 11 on the surface of the test wafer 10.
[0046] The doping region 11 includes at least one of an N-type doping layer 11n and a P-type doping layer 11p, and the doping distribution includes at least one of an N-type doping distribution and a P-type doping distribution corresponding to the doping region 11. In this embodiment, the doping region 11 is a P-type doping layer 11p. Of course, in other embodiments, the doping region 11 may also be an N-type doping layer 11n, or the doping region 11 may be a composite doping structure of an N-type doping layer 11n and a P-type doping layer 11p.
[0047] In one example, the doping region 11 includes an N-type doping layer and a P-type doping layer, and the N-type doping layer is located below the P-type doping layer. In one example, the doping region 11 includes a first doping layer doped with a first relative atomic mass and a second doping layer doped with a second relative atomic mass less than the first relative atomic mass, and the second doping layer is located above the first doping layer. For example, in some embodiments, the N-doping layer may be formed first, for example, by As doping. As has a large molecular weight and is more likely to cause amorphization of the silicon surface, resulting in an impact on subsequent doping; and then the P-doping layer may be formed, for example, by B doping. As may cause an impact on the doping distribution of B, resulting in calibration deviation. The above design of this example can effectively improve the test accuracy of the above-mentioned stacked structure device.
[0048] The CMOS image sensor includes a light sensing element (e.g., a photodiode) and a pixel support circuit. The photodiode may be a buried photodiode used in the current image sensor. In one application example, the pixel support circuit includes a reset transistor (RST), a source follower transistor (SF), a pixel selection transistor (RS), and a transfer transistor (TX) connected to the photodiode. During operation, the light sensing element generates photocharges in response to incident light during exposure. The transfer transistor is connected to a transfer signal that controls the transfer transistor to transfer the charge accumulated in the photodiode to a floating diffusion region (FD), the reset transistor is connected between VDD and the floating diffusion region, and responds to the reset signal to reset the sensor pixel circuit (e.g., discharge or charge the floating diffusion region and the photodiode to the current voltage). The gate of the source follower transistor is connected to the floating diffusion region. The source follower transistor is connected between VDD and the pixel selection transistor to respond to the potential of the floating diffusion region, and the pixel selection transistor connects the pixel circuit output from the source follower transistor to the bit line in response to the pixel selection control signal. In the above-mentioned pixel circuit, the photodiode and the floating diffusion region are reset by the temporarily valid reset signal and the transfer control signal. When the transmission control signal is released, the accumulation window (for example, the exposure phase) starts to work, and the incident light generates charge in the photodiode. The light-generated electrons in the photodiode gradually accumulate, and the charge of the photodiode represents the intensity of light incident on the photodiode during exposure.
[0049] In one example, the CMOS image sensor includes a plurality of pixel units arranged in an array and having a size of less than 3μm×3μm. The CMOS image sensor includes a plurality of pixel units arranged in an array and having a size of less than 3μm×3μm, which means that the pixel units are arranged in rows and columns as the minimum repeating units in the pixel array, and the maximum size of the pixel units in the row direction is less than 3μm and the maximum size of the pixel units in the column direction is less than 3μm. For example, the pixel units are square, and the square size is 2μm×2μm. For the CMOS image sensor of this example, a more accurate effect can be obtained by adopting the test structure of the utility model.
[0050] In one example, the arrangement of the test modulation structure includes that the proportion of the test modulation structure to the test unit increases as the size of the test unit decreases. Wherein, the test unit is a plurality of test units included in the test structure prepared by the test wafer. In some embodiments, the test unit corresponds to the pixel unit included in the pixel array of the image sensor. For example, the actual image sensor includes a pixel array composed of M rows and N columns of pixel units, and the test structure prepared by the test wafer includes an array composed of M rows and N columns of test units, and each test unit includes a test modulation structure. Of course, in other embodiments, it can also be proportional to the pixel array. In addition, the size of the test unit can be consistent with the size of the pixel unit, for example, the size and area of the two are equal or proportionally enlarged or reduced. In this example, the proportion of the test modulation structure to the test unit increases as the size of the test unit decreases. When the size of the test unit decreases, the degree of reduction of the size of the test modulation structure is smaller than the degree of reduction of the size of the test unit, and the size can be the corresponding projection area. For example, when the projection area of the test unit decreases from S1 to S2, the projection area of the test modulation structure decreases from S3 to S4, and S4 / S2 is greater than S3 / S1. This is beneficial for improving the test accuracy of small-sized devices based on the test modulation structure.
[0051] Figure 2a-2c Schematic diagram of the flow structure of the test method in the first embodiment of the present utility model. Figure 2a-2c As shown, this embodiment 1 also provides a pixel doping diffusion testing method, which is applicable to CMOS image sensors. The testing method includes:
[0052] like Figure 2aAs shown, a test wafer 10 is provided. The test wafer 10 is made of a semiconductor, such as silicon (Si). In one example, a silicon wafer is used, and other wafers used for SMIS testing may also be used. In this embodiment, a silicon wafer with P-type doping is used as the test wafer 10. Optionally, the P-type doping concentration of the test wafer 10 may be the same as the concentration of the P-type epitaxial layer of the actual CMOS image sensor, wherein the P-type doping may be obtained by performing P-type ion doping on a single crystal silicon wafer.
[0053] A test modulation structure is formed on the front side of the test wafer 10 to modulate the doping of the test wafer 10. In the present embodiment, the test modulation structure adopts a trench isolation structure 12, and the trench isolation structure 12 extends into the test wafer 10 to modulate the doping process based on the trench isolation structure 12 located inside the test wafer 10. The trench isolation structure 12 adopts a shallow trench isolation structure STI. Specifically, a photoresist layer is covered on the front side of the test wafer 10, and a mask is used to expose and develop the photoresist layer so that the photoresist layer forms a patterned structure; the test wafer 10 is etched using the patterned photoresist layer as a shield so that a groove is formed on the front side of the test wafer 10; and the trench isolation structure 12 is filled in the trench.
[0054] like Figure 2b As shown, the test wafer 10 is doped by IMP (ion implantation) from the front side of the test wafer 10 to form a doped region 11 in the test wafer 10. In this embodiment, the projection of the doped region 11 on the surface of the test wafer 10 covers the projection of the opening between adjacent trench isolation structures 12 on the surface of the test wafer 10. At the same time, there is at least one trench isolation structure 12 that completely overlaps with the projection of the doped region 11 on the surface of the test wafer 10, and two are designed in this embodiment. Among them, the doped region 11 is a P-type doped layer 11p.
[0055] like Figure 2c As shown, a doping diffusion test is performed on the test wafer 10 from the front side of the test wafer 10 using SIMS (secondary ion mass spectrometry) to obtain the doping distribution of the doping region 11, so that in the case of a test wafer 10 with a trench isolation structure 12, a more accurate doping distribution of the doping region 11 suitable for a CMOS image sensor can be obtained, such as a more accurate P-type doping diffusion condition.
[0056] Figure 3 This is the doping distribution condition tested by the testing method in the first embodiment of the present utility model. Figure 3 The dashed curve is the doping distribution test curve A2 without the trench isolation structure 12, and the solid curve is the doping distribution test curve A1 with the trench isolation structure 12 in this embodiment. The horizontal axis is the depth of the test structure (nm), and the vertical axis is the concentration of P-type ions after doping. Figure 3 It can be seen that there is an obvious difference in the longitudinal distribution with or without the trench isolation structure 12. For large pixels, the doping concentration without the trench isolation structure 12 is weak, the doping CD is larger, and the impact caused by the error is not too significant; but for small pixels, the impact is very obvious. The accuracy of the doping distribution of P-type doping with or without the trench isolation structure 12 will directly affect the isolation performance, and the accuracy of the doping distribution of N-type doping with or without the trench isolation structure 12 will directly affect the lateral diffusion of the PD (photodiode) and affect the PD morphology profile.
[0057] [Example 2]
[0058] Figure 4 Schematic diagram of the structure of the test structure in the second embodiment of the present utility model. Figure 4 As shown, the second embodiment of the utility model provides a test structure for pixel doping diffusion, including: a test chip 10, in which a doping region 11 is provided. A test modulation structure is provided on the front of the test chip 10 to modulate the doping of the test chip 10. Since in the actual production of CMOS image sensors, objects on the chip have an impact on the doping concentration, by using a test modulation structure to model the actual objects in the test stage, the doping effect in the chip test stage is closer to the actual doping effect, and the deviation between the test stage and the actual doping effect is reduced, so as to better calibrate the doping in practice. The main differences between this embodiment and the first embodiment are described in detail below, and similar designs are not repeated.
[0059] The test modulation structure includes at least one of the trench isolation structure 12 and the light blocking structure 13, so that the doping effect in the wafer test stage is closer to the actual doping effect. In this embodiment, the test modulation structure is the light blocking structure 13, so that the influence of the light blocking structure 13 on the doping effect can be tested.
[0060] Further, the light blocking structure 13 is at least located on the test wafer 10, so as to modulate the doping process based on the light blocking structure 13 located on the test wafer 10. That is, in the subsequent step of forming the doping region 11, the doping process is performed in the presence of the light blocking structure 13, which can improve the test accuracy in the subsequent test process. In this embodiment, the projections of the light blocking structure 13 and the doping region 11 on the surface of the test wafer 10 are staggered, and the light blocking structure 13 uses photoresist.
[0061] The doping region 11 includes at least one of an N-type doping layer 11n and a P-type doping layer 11p, and the doping distribution includes at least one of an N-type doping distribution and a P-type doping distribution corresponding to the doping region 11. In this embodiment, the doping region 11 is a P-type doping layer 11p. Of course, in other embodiments, the doping region 11 may also be an N-type doping layer 11n, or the doping region 11 may be a composite doping structure of an N-type doping layer 11n and a P-type doping layer 11p.
[0062] Figure 5a-5c Schematic diagram of the flow structure of the test method in the first embodiment of the present utility model. Figure 5a-5c As shown, the second embodiment also provides a method for testing pixel doping diffusion, which is applicable to CMOS image sensors. The same points between the second embodiment and the first embodiment are not repeated here. The testing method includes:
[0063] like Figure 5a As shown, a test wafer 10 is provided. The test wafer 10 is made of semiconductor, such as silicon (Si). In this embodiment, a silicon wafer with P-type doping is used as the test wafer 10.
[0064] A test modulation structure is formed on the front side of the test wafer 10 to modulate the doping of the test wafer 10. In this embodiment, the test modulation structure uses a light blocking structure 13, and the light blocking structure 13 is at least located on the test wafer 10, so as to modulate the doping process based on the light blocking structure 13 located on the test wafer 10. The light blocking structure 13 uses a photoresist PR. Specifically, a photoresist layer is covered on the front side of the test wafer 10, and a mask is used to expose and develop the photoresist layer, so that the photoresist layer forms a patterned structure.
[0065] like Figure 5b As shown, the test wafer 10 is doped by IMP (ion implantation) from the front side of the test wafer 10 to form a doped region 11 in the test wafer 10. The projections of the light blocking structure 13 and the doped region 11 on the surface of the test wafer 10 are staggered. The doped region 11 is a P-type doped layer 11p.
[0066] like Figure 5c As shown, a doping diffusion test is performed on the test wafer 10 from the front side of the test wafer 10 using SIMS (secondary ion mass spectrometry) to obtain the doping distribution of the doping region 11, so that in the case of the test wafer 10 with a light blocking structure 13, a more accurate doping distribution of the doping region 11 suitable for the CMOS image sensor can be obtained, such as a more accurate P-type doping diffusion condition.
[0067] Figure 6 This is the doping distribution condition tested by the testing method in the second embodiment of the present utility model. Figure 6The dashed curve is the doping distribution test curve B2 without the light blocking structure 13, and the solid curve is the doping distribution test curve B1 with the light blocking structure 13 in this embodiment. The horizontal axis is the depth of the test structure (nm), and the vertical axis is the concentration of P-type ions after doping. Figure 6 It can be seen that the surface of the test wafer 10 with the light blocking structure 13 has more doping, that is, the area between the doping region 11 and the front of the test structure has more doping distribution, which is also the effect caused by the smaller distance of the light blocking structure 13 in the small pixel.
[0068] [Example 3]
[0069] Figure 7 This is one of the structural schematic diagrams of the test wafer in the third embodiment of the utility model. Figure 8 This is the second structural schematic diagram of the test wafer in the third embodiment of the utility model. Fig. 9 This is the third structural schematic diagram of the test wafer in the third embodiment of the utility model. Fig.10 This is the fourth structural schematic diagram of the test wafer in the third embodiment of the utility model. Fig.11 This is the fifth structural diagram of the test wafer in the third embodiment of the utility model. Fig.12 This is the sixth structural schematic diagram of the test wafer in the third embodiment of the present utility model. Fig.13 This is the seventh structural diagram of the test wafer of the third embodiment of the utility model. The main differences between this embodiment and the first and second embodiments are described in detail below, and similar designs will not be repeated.
[0070] like Figures 7 to 13 As shown, a pixel doping diffusion test structure provided by the third embodiment of the utility model includes: a test wafer 10, in which a doping region 11 is provided. A test modulation structure is provided on the front of the test wafer 10 to modulate the doping of the test wafer 10. Since the structure on the wafer has an influence on the doping concentration in the actual production of the CMOS image sensor, the test modulation structure is used to model the structure in the actual CMOS image sensor in the test stage, so that the doping effect in the wafer test stage is closer to the actual doping effect, and the deviation between the test stage and the actual doping effect is reduced, so as to better calibrate the doping in practice.
[0071] The test modulation structure includes at least one of a trench isolation structure 12 and a light blocking structure 13, so that the doping effect in the wafer test stage is closer to the actual doping effect. In the present embodiment, the test modulation structure includes a trench isolation structure 12 and a light blocking structure 13, so that a more accurate doping distribution can be obtained based on the influence of the trench isolation structure 12 and the light blocking structure 13 on the doping effect. The trench isolation structure 12 extends into the test wafer 10 to modulate the doping process based on the trench isolation structure 12 located inside the test wafer 10. The light blocking structure 13 is located on the test wafer 10 to modulate the doping process based on the light blocking structure 13 located on the test wafer 10. Further, in the present embodiment, the trench isolation structure 12 adopts a shallow trench isolation structure, and the light blocking structure 13 adopts photoresist.
[0072] Furthermore, the trench isolation structure 12 and the doped region 11 at least partially overlap on the surface of the test wafer 10. The projections of the light blocking structure 13 and the doped region 11 on the surface of the test wafer 10 are staggered.
[0073] The trench isolation structure 12 includes at least one of a first trench isolation structure 12 a completely offset from the light blocking structure 13 , a second trench isolation structure 12 b partially overlapping the light blocking structure 13 , and a third trench isolation structure 12 c completely overlapping the light blocking structure 13 .
[0074] The light blocking structure 13 includes at least one of a first light blocking structure 13 a completely offset from the trench isolation structure 12 , a second light blocking structure 13 b partially overlapping the trench isolation structure 12 , and a third light blocking structure 13 c completely overlapping the trench isolation structure 12 .
[0075] In one embodiment, if Figure 7 As shown, the trench isolation structure 12 and the doped region 11 completely overlap on the surface of the test wafer 10 , the trench isolation structure 12 adopts a first trench isolation structure 12 a completely staggered with the light blocking structure 13 , and the light blocking structure 13 adopts a first light blocking structure 13 a completely staggered with the trench isolation structure 12 .
[0076] In one embodiment, if Figure 8 As shown, the trench isolation structure 12 partially overlaps with the doped region 11 on the surface of the test wafer 10 , the trench isolation structure 12 adopts a second trench isolation structure 12 b that partially overlaps with the light blocking structure 13 , and the light blocking structure 13 adopts a second light blocking structure 13 b that partially overlaps with the trench isolation structure 12 .
[0077] In one embodiment, if Fig. 9As shown, the trench isolation structure 12 adopts a third trench isolation structure 12c that completely overlaps with the light blocking structure 13, and the light blocking structure 13 adopts a third light blocking structure 13c that completely overlaps with the trench isolation structure 12. The third trench isolation structure 12c and the projection of the doped region 11 on the surface of the test wafer 10 are staggered.
[0078] In one embodiment, if Fig.10 As shown, the trench isolation structure 12 partially overlaps with the doped region 11 on the surface of the test wafer 10, the trench isolation structure 12 adopts a second trench isolation structure 12b that partially overlaps with the light blocking structure 13, and the light blocking structure 13 includes a first light blocking structure 13a that is completely staggered with the trench isolation structure 12 and a second light blocking structure 13b that partially overlaps with the trench isolation structure 12.
[0079] In one embodiment, if Fig.11 As shown, the trench isolation structure 12 includes a first trench isolation structure 12a that is completely staggered with the light blocking structure 13 and a third trench isolation structure 12c that is completely overlapped with the light blocking structure 13, the light blocking structure 13 includes a first light blocking structure 13a that is completely staggered with the trench isolation structure 12 and a third light blocking structure 13c that is completely overlapped with the trench isolation structure 12, and the projection of the doped region 11 on the surface of the test wafer 10 covers the projection of the opening between adjacent trench isolation structures 12 on the surface of the test wafer 10.
[0080] In one embodiment, if Fig.12 As shown, the trench isolation structure 12 includes a first trench isolation structure 12a that is completely offset from the light blocking structure 13, and a second trench isolation structure 12b that partially overlaps with the light blocking structure 13; the light blocking structure 13 includes a first light blocking structure 13a that is completely offset from the trench isolation structure 12, and a second light blocking structure 13b that partially overlaps with the trench isolation structure 12; the projection of the doped region 11 on the surface of the test wafer 10 covers the projection of the opening between adjacent trench isolation structures 12 on the surface of the test wafer 10; in this example, the opening between adjacent trench isolation structures 12 refers to the opening formed between the first trench isolation structure 12a that is completely offset from the light blocking structure 13 and the second trench isolation structure 12b that partially overlaps with the light blocking structure 13.
[0081] In one embodiment, if Fig.13As shown, the trench isolation structure 12 includes a first trench isolation structure 12a completely staggered with the light blocking structure 13, a second trench isolation structure 12b partially overlapping with the light blocking structure 13, and a third trench isolation structure 12c completely overlapping with the light blocking structure 13. The light blocking structure 13 includes a first light blocking structure 13a completely staggered with the trench isolation structure 12, a second light blocking structure 13b partially overlapping with the trench isolation structure 12, and a third light blocking structure 13c completely overlapping with the trench isolation structure 12. The projection of the doped region 11 on the surface of the test wafer 10 covers the projection of the opening between adjacent trench isolation structures 12 on the surface of the test wafer 10.
[0082] The specific patterns of the trench isolation structure 12 and the light blocking structure 13 can be set according to actual test requirements. In the present invention, the test modulation structure can make the test structure closer to the actual structure of the CMOS image sensor, thereby improving the accuracy of the doping diffusion test.
[0083] The doping region 11 includes at least one of an N-type doping layer 11n and a P-type doping layer 11p, and the doping distribution includes at least one of an N-type doping distribution and a P-type doping distribution corresponding to the doping region 11. In this embodiment, the doping region 11 is an N-type doping layer 11n.
[0084] Figures 14a-14d The third embodiment of the present utility model corresponds to Fig.10 Schematic diagram of the process structure of the test method for testing a wafer. Figures 14a-14c As shown, this third embodiment also provides a pixel doping diffusion testing method, which is applicable to CMOS image sensors. The testing method includes:
[0085] like Fig.14a As shown, a test wafer 10 is provided. The test wafer 10 is made of semiconductor, such as silicon (Si). In this embodiment, a silicon wafer with P-type doping is used as the test wafer 10.
[0086] A test modulation structure is formed on the front side of the test wafer 10 to modulate the doping of the test wafer 10. In this embodiment, the test modulation structure includes a trench isolation structure 12 and a light blocking structure 13, wherein the trench isolation structure 12 extends into the test wafer 10 to modulate the doping process based on the trench isolation structure 12 located inside the test wafer 10. The light blocking structure 13 is at least located on the test wafer 10 to modulate the doping process based on the light blocking structure 13 located on the test wafer 10.
[0087] The trench isolation structure 12 adopts a shallow trench isolation structure STI. Specifically, a first photoresist layer is covered on the front side of the test wafer 10, and the first photoresist layer is exposed and developed using a mask, so that the first photoresist layer forms a patterned structure; the test wafer 10 is etched using the patterned first photoresist layer as a shield, so that a trench is formed on the front side of the test wafer 10; the trench is filled in the trench to form the trench isolation structure 12, and the filling material is selected as silicon oxide in this embodiment.
[0088] like Fig.14b As shown, the light blocking structure 13 is made of photoresist PR. Specifically, a second photoresist layer is covered on the front side of the test wafer 10, and a mask is used to expose and develop the second photoresist layer, so that the second photoresist layer forms a patterned structure to form the light blocking structure 13.
[0089] like Fig.14c As shown, the test wafer 10 is doped by IMP (ion implantation) from the front side of the test wafer 10 to form a doped region 11 in the test wafer 10. In this embodiment, the doped region 11 is an N-type doped layer 11n. The trench isolation structure 12 overlaps with the doped region 11 on the surface of the test wafer 10. The trench isolation structure 12 adopts a second trench isolation structure 12b that partially overlaps with the light blocking structure 13. The light blocking structure 13 includes a first light blocking structure 13a that is completely staggered with the trench isolation structure 12 and a second light blocking structure 13b that partially overlaps with the trench isolation structure 12.
[0090] like Fig.14d As shown, a doping diffusion test is performed on the test wafer 10 from the front side of the test wafer 10 using SIMS (secondary ion mass spectrometry) to obtain the doping distribution of the doping region 11, so that in the case of the test wafer 10 having both the trench isolation structure 12 and the light blocking structure 13, a more accurate doping distribution of the doping region 11 suitable for the CMOS image sensor can be obtained, such as a more accurate N-type doping diffusion condition.
[0091] [Example 4]
[0092] Fig.15 Schematic diagram of the structure of the test wafer in the fourth embodiment of the utility model. Fig.15 As shown, the pixel doping diffusion test structure and test method provided in the fourth embodiment of the present invention are similar to those in the third embodiment ( Figures 7 to 13) are basically the same as the test structure and test method of pixel doping diffusion in the embodiment, except that, in the present embodiment: the doping region 11 is a P-type doping layer 11p, so that in the case of a test wafer 10 having both a trench isolation structure 12 and a light blocking structure 13, a more accurate doping distribution of the doping region 11 suitable for the CMOS image sensor is obtained, such as a more accurate P-type doping diffusion condition.
[0093] Figures 16a-16d This is the fourth embodiment of the utility model corresponding to Fig.10 Schematic diagram of the process structure of the test method for testing a wafer. Figures 16a-16d As shown, this fourth embodiment also provides a method for testing pixel doping diffusion, which is applicable to CMOS image sensors. The testing method includes:
[0094] like Fig.16a As shown, a test wafer 10 is provided. The test wafer 10 is made of semiconductor, such as silicon (Si). In this embodiment, a silicon wafer with P-type doping is used as the test wafer 10.
[0095] A test modulation structure is formed on the front side of the test wafer 10 to modulate the doping of the test wafer 10. In this embodiment, the test modulation structure includes a trench isolation structure 12 and a light blocking structure 13, wherein the trench isolation structure 12 extends into the test wafer 10 to modulate the doping process based on the trench isolation structure 12 located inside the test wafer 10. The light blocking structure 13 is at least located on the test wafer 10 to modulate the doping process based on the light blocking structure 13 located on the test wafer 10.
[0096] The trench isolation structure 12 adopts a shallow trench isolation structure STI. Specifically, a first photoresist layer is covered on the front side of the test wafer 10, and the first photoresist layer is exposed and developed using a mask, so that the first photoresist layer forms a patterned structure; the test wafer 10 is etched using the patterned first photoresist layer as a shield, so that a trench is formed on the front side of the test wafer 10; the trench is filled in the trench to form the trench isolation structure 12, and the filling material is selected as silicon oxide in this embodiment.
[0097] like Fig.16b As shown, the light blocking structure 13 is made of photoresist PR. Specifically, a second photoresist layer is covered on the front side of the test wafer 10, and a mask is used to expose and develop the second photoresist layer, so that the second photoresist layer forms a patterned structure to form the light blocking structure 13.
[0098] like Fig.16cAs shown, the test wafer 10 is doped by IMP (ion implantation) from the front side of the test wafer 10 to form a doped region 11 in the test wafer 10. In this embodiment, the doped region 11 is a P-type doped layer 11p. The trench isolation structure 12 overlaps with the doped region 11 on the surface of the test wafer 10. The trench isolation structure 12 adopts a second trench isolation structure 12b that partially overlaps with the light blocking structure 13. The light blocking structure 13 includes a first light blocking structure 13a that is completely staggered with the trench isolation structure 12 and a second light blocking structure 13b that partially overlaps with the trench isolation structure 12.
[0099] like Fig.16d As shown, a doping diffusion test is performed on the test wafer 10 from the front side of the test wafer 10 using SIMS (secondary ion mass spectrometry) to obtain the doping distribution of the doping region 11, so that in the case of a test wafer 10 having both a trench isolation structure 12 and a light blocking structure 13, a more accurate doping distribution of the doping region 11 suitable for a CMOS image sensor can be obtained, such as a more accurate P-type doping diffusion condition.
[0100] It should be understood by those skilled in the art that the rest of the structure and working principle of this embodiment are the same as those of the third embodiment, and will not be described in detail here.
[0101] [Example 5]
[0102] Fig.17 This is a schematic diagram of the structure of the test wafer in the fifth embodiment of the utility model. Fig.17 As shown, the test wafer provided in the fifth embodiment of the present invention is the same as that in the third embodiment ( Figures 7 to 14d ) is basically the same as the test wafer in the embodiment, except that, in this embodiment: the doping region 11 includes a layer of N-type doping layer 11n and two layers of P-type doping layer 11p, and the layer of N-type doping layer 11n is located between the two layers of P-type doping layer 11p, so that the influence of the trench isolation structure 12 and the light blocking structure 13 on the composite doping diffusion of P-type doping and N-type doping of the test wafer 10 can be tested. Of course, in other embodiments, the doping region 11 may also include a layer of N-type doping layer 11n and a layer of P-type doping layer 11p, and the N-type doping layer 11n is located below the P-type doping layer 11p, such as Fig.19 As shown, the main differences between this embodiment and the aforementioned embodiments are described in detail below, and similar designs will not be repeated here.
[0103] Figures 18a-18d Schematic diagram of the flow structure of the test method in the fifth embodiment of the present utility model. Figures 18a-18d As shown, this fifth embodiment also provides a method for testing pixel doping diffusion, which is applicable to CMOS image sensors. The testing method includes:
[0104] like Fig.18a As shown, a test wafer 10 is provided. The test wafer 10 is made of semiconductor, such as silicon (Si). In this embodiment, a silicon wafer with P-type doping is used as the test wafer 10.
[0105] A test modulation structure is formed on the front side of the test wafer 10 to modulate the doping of the test wafer 10. In this embodiment, the test modulation structure includes a trench isolation structure 12 and a light blocking structure 13, wherein the trench isolation structure 12 extends into the test wafer 10 to modulate the doping process based on the trench isolation structure 12 located inside the test wafer 10. The light blocking structure 13 is at least located on the test wafer 10 to modulate the doping process based on the light blocking structure 13 located on the test wafer 10.
[0106] The trench isolation structure 12 adopts a shallow trench isolation structure STI. Specifically, a first photoresist layer is covered on the front side of the test wafer 10, and the first photoresist layer is exposed and developed using a mask, so that the first photoresist layer forms a patterned structure; the test wafer 10 is etched using the patterned first photoresist layer as a shield, so that a trench is formed on the front side of the test wafer 10; the trench is filled in the trench to form the trench isolation structure 12, and the filling material is selected as silicon oxide in this embodiment.
[0107] like Fig.18b As shown, the light blocking structure 13 is made of photoresist PR. Specifically, a second photoresist layer is covered on the front side of the test wafer 10, and a mask is used to expose and develop the second photoresist layer, so that the second photoresist layer forms a patterned structure to form the light blocking structure 13.
[0108] like Fig.18c As shown, the test wafer 10 is doped by IMP (ion implantation) from the front side of the test wafer 10, and a doping region 11 is formed in the test wafer 10. In this embodiment, the doping region 11 includes a layer of N-type doping layer 11n and two layers of P-type doping layer 11p, and the layer of N-type doping layer 11n is located between the two layers of P-type doping layer 11p. The trench isolation structure 12 overlaps with the doping region 11 on the surface of the test wafer 10, and the trench isolation structure 12 adopts a second trench isolation structure 12b that partially overlaps with the light blocking structure 13. The light blocking structure 13 includes a first light blocking structure 13a that is completely staggered with the trench isolation structure 12 and a second light blocking structure 13b that partially overlaps with the trench isolation structure 12.
[0109] like Fig.18dAs shown, a doping diffusion test is performed on the test wafer 10 from the front side of the test wafer 10 using SIMS (secondary ion mass spectrometry) to obtain the doping distribution of the doping region 11, thereby being able to test the effects of the trench isolation structure 12 and the light blocking structure 13 on the composite doping diffusion of P-type doping and N-type doping in the test wafer 10.
[0110] It should be understood by those skilled in the art that the rest of the structure and working principle of this embodiment are the same as those of the third embodiment, and will not be described in detail here.
[0111] [Example 6]
[0112] The present application also provides a calibration method for pixel doping diffusion, which comprises: calibrating the doping distribution of the doping region 11 obtained by testing using the pixel doping diffusion test method as described above. Since the doping distribution of the doping region 11 obtained by the test method is closer to the actual doping effect, the deviation between the test stage and the actual doping effect is reduced, so as to better calibrate the doping in practice, and can be applicable to the lateral and longitudinal calibration of the doping of the image sensor.
[0113] In one embodiment, calibration using the doping distribution of the doping area includes: obtaining a test surface corresponding to the test wafer based on the test modulation structure, and performing lateral calibration based on the doping distribution of the test surface. The design of the test modulation structure can affect the doping distribution of the test surface (for example, the horizontal plane of the test structure corresponding to a certain depth position). For example, when the test modulation structure is a shallow trench isolation structure, its structure located in the test wafer may affect the reflection of the doped ions and the injection distribution at depth based on the material different from the test wafer. When the test modulation structure is a photoresist, it can block the injected ions and affect the ion distribution on the test surface. Of course, it can also affect the ion injection based on the reflection or refraction of the part located on the surface of the test wafer. In this embodiment, the influence based on the test modulation structure can be beneficial to improve the accuracy of lateral diffusion and facilitate the calibration of small-sized devices.
[0114] In this document, the directional words such as up, down, left, right, front, and back are defined by the positions of the structures in the drawings and the positions of the structures relative to each other, just for the sake of clarity and convenience in expressing the technical solution. It should be understood that the use of the directional words should not limit the scope of protection claimed in this application. It should also be understood that the terms "first" and "second" used in this document are only used to distinguish names and are not used to limit quantity and order.
[0115] The above description is only a preferred embodiment of the present invention, and does not limit the present invention in any form. Although the present invention has been disclosed as a preferred embodiment as above, it is not used to limit the present invention. Any technician familiar with the profession can make some changes or modifications to the technical contents disclosed above without departing from the scope of the technical solution of the present invention, which are equivalent embodiments of equivalent changes. However, any simple modification, equivalent changes and modifications made to the above embodiments based on the technical essence of the present invention without departing from the content of the technical solution of the present invention are still within the protection scope of the technical solution of the present invention.
Claims
1. A pixel doping diffusion test structure, characterized in that: The test structure includes: A test wafer, wherein the test wafer has a doped region; A test modulation structure is provided on the front side of the test wafer to modulate the doping of the test wafer.
2. The pixel doping diffusion test structure according to claim 1, characterized in that: The test modulation structure includes at least one of a trench isolation structure and a light blocking structure.
3. The pixel doping diffusion test structure according to claim 2, characterized in that: The trench isolation structure extends into the test wafer to modulate a doping process based on the trench isolation structure located inside the test wafer; And / or, the light blocking structure is at least located on the test wafer, so as to modulate the doping process based on the light blocking structure located on the test wafer.
4. The pixel doping diffusion test structure according to claim 2, characterized in that: The arrangement between the trench isolation structure and the doped region and between the light blocking structure and the doped region includes at least one of the following arrangements: The projections of the trench isolation structure and the doped region on the surface of the test wafer at least partially overlap; and the projections of the doped region on the surface of the test wafer cover the projections of the openings between adjacent trench isolation structures on the surface of the test wafer; and the projections of the light blocking structure and the doped region on the surface of the test wafer are staggered with each other.
5. The pixel doping diffusion test structure according to claim 4, characterized in that: The projection of the trench isolation structure and the doped region on the surface of the test wafer partially overlaps, the projection of the doped region on the surface of the test wafer covers the projection of the opening between adjacent trench isolation structures on the surface of the test wafer, and the projection of the light blocking structure on the surface of the test wafer is located at the periphery of the doped region.
6. The pixel doping diffusion test structure according to claim 2, characterized in that: The trench isolation structure includes at least one of a first trench isolation structure completely offset from the light blocking structure, a second trench isolation structure partially overlapping with the light blocking structure, and a third trench isolation structure completely overlapping with the light blocking structure.
7. The pixel doping diffusion test structure according to claim 2, characterized in that: The light blocking structure includes at least one of a first light blocking structure completely staggered with the trench isolation structure, a second light blocking structure partially overlapping with the trench isolation structure, and a third light blocking structure completely overlapping with the trench isolation structure, and / or the trench isolation structure adopts a shallow trench isolation structure and the light blocking structure adopts photoresist.
8. The pixel doping diffusion test structure according to claim 1, characterized in that: The test structure prepared by the test wafer includes a plurality of test units, and the test units correspond to pixel units of the image sensor; and / or, the arrangement of the test modulation structure includes that the proportion of the test modulation structure to the test unit increases as the size of the test unit decreases.
9. The pixel doping diffusion test structure according to any one of claims 1 to 8, characterized in that: The doping region includes at least one of an N-type doping layer and a P-type doping layer.
10. The pixel doping diffusion test structure according to claim 9, characterized in that: The doping region includes an N-type doping layer and two P-type doping layers, and the N-type doping layer is located between the two P-type doping layers; and / or, the doping region includes an N-type doping layer and a P-type doping layer, and the N-type doping layer is located below the P-type doping layer; and / or, the doping region includes a first doping layer doped with a first relative atomic mass and a second doping layer doped with a second relative atomic mass less than the first relative atomic mass, and the second doping layer is located above the first doping layer.