Safety memory circuit with temperature protection for automobile traveling data recorder
By spraying a polymer nano-waterproof coating layer on the car driving recorder and using RTC silicone rubber for potting, combined with heat-absorbing medium particles, the waterproof problem under high temperature water vapor and water pressure is solved, achieving temperature regulation and cost savings, and improving High temperature resistance of secure memory chips.
Patent Information
- Application Number
- CN202323030349.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2023-11-09
- Publication Date
- 2024-10-29
- Estimated Expiration
- 2033-11-09
AI Technical Summary
The safety storage circuit of the existing car driving recorder is easily damaged by water vapor under high temperature water vapor and 1.0MPa water pressure, causing the chip surface test paper to change color and cannot meet certification requirements. Moreover, the traditional epoxy resin coating and sealing structure increases the cost and Difficulty of repair.
The method of combining the polymer nano-waterproof coating layer and RTC silicone rubber potting is used to form a continuous waterproof protective layer, and heat-absorbing medium particles are mixed in the silicone rubber to adjust the temperature field and buffer the water pressure.
It achieves waterproof performance under high-temperature water vapor and 1.0MPa water pressure, reduces chip temperature, simplifies operation, reduces costs, and improves maintenance convenience and temperature adjustment capabilities.
Smart Images

Figure CN221930441U_ABST
Abstract
Description
Technical Field
[0001] The utility model belongs to the technical field of vehicle information storage equipment and relates to a safety memory circuit of a vehicle driving recorder with temperature protection. Background Art
[0002] According to the requirements of Appendix E of GB / T 19056-2021 "Automobile Driving Recorder" national standard newly released on December 30, 2021, the data of the vehicle driving recorder installed in various passenger cars, dangerous goods transport vehicles, semi-trailer tractors and other trucks with a mass greater than or equal to 12,000 kg can still be read after the safety memory of the vehicle driving recorder is burned at 1100°C for 15 minutes, roasted at 260°C for 2 hours, subjected to 10KN static pressure and immersed in 100m water depth. At the same time, according to the provisions of "CTS-CSP-J005-2020 Certification Method for Protective Memory for Automobile Driving Recorders", in the above temperature field, the temperature of the safety storage chip of the vehicle driving recorder shall not exceed 125°C. After immersion in 100m water depth for 48 hours (1.0MPa water pressure for 48h), the water-discoloration test paper on the surface of the chip shall not change color due to water vapor, etc.
[0003] At present, most of the car driving recorders that meet the standards in the market use a heat-absorbing medium with a high water content to adjust the temperature field around the chip, and the heat is taken away by evaporation of water vapor. Water vapor will also cause water vapor damage to the safe storage circuit of the car driving recorder. At the same time, the superposition of 48 hours of 1.0MPa water pressure may cause the test paper on the surface of the chip to change color, which does not meet the requirements of the certification method. How to ensure the waterproofness of the safe storage circuit of the car driving recorder has become an urgent problem to be solved. The most common method is to use epoxy resin to cover and isolate water vapor. The problem is poor maintainability. The thermal shrinkage of the selected resin needs to match the circuit to prevent shrinkage from causing extrusion damage to the circuit components; another method is to seal the safe storage circuit of the car driving recorder through a structure to completely isolate it from water vapor. The disadvantage is that an additional sealing structure is added, resulting in increased costs. Utility Model Content
[0004] The utility model aims to provide a safety memory circuit of a car driving recorder with temperature protection, which ensures that the safety memory chip is not damaged by water vapor under high temperature water vapor and 1.0MPa water pressure for 48 hours, and can adjust the chip temperature at the same time.
[0005] The technical solution for realizing the purpose of using the novel device is as follows: In order to achieve the above-mentioned purpose, a temperature-protected automobile driving recorder safety memory circuit is proposed, and the surface of the automobile driving recorder safety memory circuit board is sprayed with a polymer nano waterproof coating layer, so that a continuous waterproof protective coating is formed on the surface of the circuit board; the circuit board with the high-density nano waterproof coating is potted and evenly wrapped by RTC silicone rubber.
[0006] In a possible embodiment, the thickness of the RTC (room temperature curing) silicone rubber is not less than 1 mm.
[0007] Preferably, the RTC silicone rubber has an operating temperature range of -50°C to 200°C.
[0008] In a possible embodiment, the RTC silicone rubber has an elongation at break greater than 300%, a tensile strength greater than 2 MPa, a tear strength greater than 2.5 MPa, and a viscosity no greater than 3000 mPS.
[0009] Furthermore, the RTC silicone rubber is evenly mixed with heat absorbing medium particles before potting.
[0010] In a possible embodiment, the mass fraction of the heat absorbing medium particles does not exceed 8%.
[0011] Preferably, the particle size of the heat absorbing medium is not greater than 20 μm; the particle size is below 20 microns (without affecting fluidity and perspective), does not chemically react or physically change with the RTC silicone rubber, absorbs heat at 80°C to 180°C, begins to decompose, and releases gas to take away the heat.
[0012] Compared with the prior art, the beneficial effects of this new method are:
[0013] 1. Use polymer waterproof coating to replace vacuum atmospheric deposition. The operation is simple. Only general spraying equipment or immersion method is needed to achieve surface film coating. The operation time is short. It only takes 15 minutes to complete the curing. The film layer is continuous and the film defects can be checked by ultraviolet light. Vacuum atmospheric deposition requires professional equipment to operate. The operation time is more than 24 hours. The film layer cannot be detected and the cost is high.
[0014] 2Compared with epoxy resin potting, RTC silicone rubber potting can form a softer protective layer on the surface of the car driving recorder security memory circuit. The higher elasticity can buffer the squeeze damage of water pressure or static pressure and protect the chip; the lower tensile strength and tear strength can protect the protective layer from being damaged under 1.0MPa water pressure, making it convenient to remove the protective layer without damaging the electronic devices when a fault occurs, which are all features that epoxy resin does not have. Compared with the waterproof sealing structure for the security storage chip, the cured RTC potting glue replaces the more complex sealing structure, saving costs and process equipment.
[0015] 3 Compared with general epoxy resin and silicone rubber potting, mixing and dispersing a certain mass fraction of powdered heat-absorbing medium in the potting protective layer can adjust the temperature field around the car driving recorder's security memory to a certain extent. When the chip operating temperature or the temperature in the fire exceeds 80°C, the heat-absorbing medium dispersed in the potting protective layer begins to absorb heat and convert into gas for discharge, reducing the temperature rise rate around the chip and ensuring that the chip can maintain a temperature of no more than 125°C for a longer period of time. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] In order to more clearly illustrate the technical solution of the present invention, the following briefly introduces the drawings required for describing the embodiments.
[0017] Figure 1 It is a schematic diagram of the appearance of a safety memory circuit of a vehicle driving recorder with temperature protection according to a preferred embodiment of the utility model;
[0018] Figure 2 The present invention is a schematic cross-sectional view of a safety memory circuit of a vehicle driving recorder with temperature protection according to a preferred embodiment of the present invention. DETAILED DESCRIPTION
[0019] The present invention is further described below in conjunction with specific embodiments, so that the advantages and features of the present invention will become clearer as the description progresses, but these embodiments are only exemplary and do not constitute any limitation on the scope of the present invention. It should be understood by those skilled in the art that the details and forms of the technical solution of the present invention may be modified and replaced without departing from the spirit and scope of the present invention, but these modifications and replacements all fall within the protection scope of the present invention.
[0020] like Figure 1-Figure 2 As shown, a temperature-protected automobile driving recorder safety memory circuit 1 is provided, wherein a polymer nano waterproof coating layer is sprayed on the surface of the automobile driving recorder safety memory circuit board, so that a continuous waterproof protective coating is formed on the surface of the circuit board; the circuit board with the polymer nano waterproof coating is potted and evenly wrapped by RTC silicone rubber 2.
[0021] In a possible embodiment, the thickness of the RTC (room temperature curing) silicone rubber 2 is not less than 1 mm.
[0022] Preferably, the RTC silicone rubber 2 has an operating temperature range of -50°C to 200°C.
[0023] In a possible embodiment, the RTC silicone rubber 2 has an elongation at break greater than 300%, a tensile strength greater than 2 MPa, a tear strength greater than 2.5 MPa, and a viscosity no greater than 3000 mPS.
[0024] Furthermore, the RTC silicone rubber 2 is uniformly mixed with heat absorbing medium particles 3 before potting.
[0025] In a possible embodiment, the mass fraction of the heat absorbing medium particles does not exceed 8%.
[0026] Preferably, the particle size of the heat absorbing medium is not greater than 20 μm; the particle size is below 20 microns (without affecting fluidity and perspective), does not chemically react or physically change with the RTC silicone rubber, absorbs heat at 80°C to 180°C, begins to decompose, and releases gas to take away the heat.
[0027] This specific implementation scheme provides a method for three-proof protection of the safety storage circuit of the automobile driving recorder, and at the same time, this method has a certain temperature protection effect on the circuit.
[0028] After the automobile driving recorder safety memory circuit board is degreased, degreased, cleaned and dried, the polymer nano waterproof agent 1 containing fluorine polymerization is evenly sprayed on the circuit surface, or the automobile driving recorder safety storage circuit is immersed in the waterproof agent for 5 to 10 seconds, taken out and cured in the air for 5 to 10 minutes, and the continuity of the film layer is detected by ultraviolet light, and the uncontinuous film is supplemented by a brushing process to ensure that all devices and cables of the entire circuit board are wrapped by the tough film formed by the waterproof agent. After complete curing for 15 minutes, the subsequent potting protection process can be carried out.
[0029] The circuit board with the waterproofing agent is placed in a specific mold, and the RTC potting glue 2 containing the powdered heat-absorbing medium 3 is poured into the mold and left to cure. In this embodiment, it is recommended to use two-component RTC silicone rubber 9086 as the main potting material, and the 9086 silicone rubber is fully stirred for 1 to 2 minutes at a mass ratio of 10:1, and the heat-absorbing medium is mixed into the mixture at a content not exceeding 8% (5% is recommended). After fully stirring, the mixture is placed in a vacuum machine and maintained at a negative pressure of less than 1000 Pa for 5 minutes until the bubbles in the mixture completely disappear; the vacuumed mixture is slowly injected into the mold containing the automobile driving recorder safety memory circuit board 1 in batches, and exposed to the air and left to cure.
[0030] The three-proof protection method of the automobile driving recorder safety memory with temperature protection designed in this specific embodiment, on the one hand, a continuous protective film is formed on the surface of the automobile driving recorder safety memory circuit through a fluoride polymer nano waterproof agent 1, and the three-proof protection is achieved by using the hydrophobicity and material properties of the film layer itself, and the film layer is ensured to be continuous and prevent water immersion in 48 hours of 1.0MPa water pressure through the flexibility and tensile and tearing strength of the film layer; on the other hand, the entire automobile driving recorder safety storage circuit is wrapped by RTC silicone rubber potting 2, and the film layer thickness is not less than 1mm. The cured silicone rubber is sealed, non-absorbent, flexible, and easy to peel, etc., to meet the basic requirements of waterproofing and 1.0MPa water pressure for 48 hours. At the same time, the heat-absorbing medium particles 3 are evenly mixed and dispersed in the silicone rubber, so that the automobile driving recorder safety memory circuit after potting and curing contains a certain amount of heat-absorbing medium around it, which can absorb heat and convert into gas and release it when the external temperature exceeds 80°C, taking away heat to reduce the heating rate around the circuit board, and can also absorb chip heat when the chip temperature is higher than 80°C to reduce the chip temperature.
[0031] The above measures can meet the basic requirements of the three-proof of the automobile driving recorder's safety memory circuit and no discoloration under 1.0MPa water pressure for 48 hours. At the same time, the internal and external temperature changes exceeding 80°C can be adjusted to increase the high temperature resistance time of the automobile driving recorder's safety storage chip.
[0032] The above description is only a preferred embodiment of the present invention and is not intended to limit the present invention. Any modifications, equivalent substitutions, improvements, etc. made within the spirit and principles of the present invention should be included in the protection scope of the present invention.
[0033] In addition, it should be understood that although the present specification is described in accordance with implementation methods, not every implementation method contains only one independent technical solution. This narrative method of the specification is only for the sake of clarity. Those skilled in the art should regard the specification as a whole. The technical solutions in each embodiment can also be appropriately combined to form other implementation methods that can be understood by those skilled in the art.
Claims
1. A temperature-protected automobile driving recorder safety memory circuit, characterized in that: The surface of the circuit board of the automobile driving recorder safety memory is sprayed with a polymer nano waterproof coating layer, so that a continuous waterproof protective coating is formed on the surface of the circuit board; the circuit board with the polymer nano waterproof coating layer is potted and evenly wrapped by room temperature curing silicone rubber.
2. A temperature-protected automobile driving recorder safety memory circuit according to claim 1, characterized in that: The thickness of the room temperature curing silicone rubber is not less than 1 mm.
3. The temperature-protected automobile driving recorder safety memory circuit according to claim 1, characterized in that: The room temperature curing silicone rubber has an operating temperature range of -50°C to 200°C.
4. The temperature-protected automobile driving recorder safety memory circuit according to claim 1, characterized in that: The room temperature curing silicone rubber has an elongation at break greater than 300%, a tensile strength greater than 2MPa, a tear strength greater than 2.5MPa, and a viscosity no greater than 3000mPS.
5. The temperature-protected automobile driving recorder safety memory circuit according to claim 1, characterized in that: The room temperature curing silicone rubber is uniformly mixed with heat absorbing medium particles before potting.
6. The temperature-protected automobile driving recorder safety memory circuit according to claim 5, characterized in that: The mass fraction of the heat absorbing medium particles does not exceed 8%.
7. The temperature-protected automobile driving recorder safety memory circuit according to claim 5, characterized in that: The particle size of the heat absorbing medium is not greater than 20 μm.