Large-area double-color injection molding product forming device

By setting multiple evenly distributed gates in the soft rubber cavity formed by the moving mold and the fixed mold, the problems of air trapping and material shortage in the soft rubber part during the molding process of large-area two-color products are solved, thereby improving the molding quality and yield.

CN221953746UActive Publication Date: 2024-11-05CHENGDU SHUANGYING AUTO SEAT CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420441227.9
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-03-07
Publication Date
2024-11-05
Estimated Expiration
2034-03-07

AI Technical Summary

Technical Problem

In the molding process of automotive parts, when molding large-area two-color products, the soft rubber part is prone to appearance defects such as air entrapment, cracking of the joint line and material shortage, resulting in low molding yield.

Method used

The moving mold and the fixed mold together form a soft rubber cavity. Several gates are set up to communicate with the soft rubber cavity. The number of gates is large and evenly distributed. The distance between adjacent gates is less than or equal to 100mm. The thickness of the soft rubber cavity is 1.8-2.5mm. The gates are arranged at equal intervals along the long side of the soft rubber cavity. The distance between the gates near the wide side and the wide side is 10-70mm less than the distance between adjacent gates to ensure rapid and full injection.

Benefits of technology

It improved the molding quality of the soft rubber part, reduced air trapping and material shortage problems, and improved the molding yield and injection efficiency of large-area two-color products.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221953746U_ABST
    Figure CN221953746U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of mold structures, and discloses a large-area double-color injection molding product forming device which comprises a movable mold and a fixed mold, the movable mold, the fixed mold and a hard rubber part jointly define a soft rubber cavity, a plurality of sprues communicated with the soft rubber cavity are arranged on the movable mold, and the distance between every two adjacent sprues is smaller than or equal to 100mm. According to the utility model, the plurality of sprues are arranged and the distance between the adjacent sprues is limited within the range of less than or equal to 100mm, so that the soft rubber cavity can be quickly and fully filled in the injection process, and the problem of low forming yield when the soft rubber part in a large-area double-color product is formed in the prior art is solved.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of mold structures, in particular to a large-area two-color injection molding product molding device. Background Art

[0002] In the process of automobile parts molding, large-area two-color products with large length and width will be formed, and the product injection molding process is divided into two steps. The first step is to inject hard rubber material to form the hard rubber part, and the second step is to rotate the movable mold 180° so that the hard rubber part, the fixed mold and the movable mold together form a soft rubber cavity for molding the soft rubber part, and then inject soft rubber material into the soft rubber cavity to form the soft rubber part. The soft rubber part covers the A surface of the hard rubber part injection molded in the first step, and after demolding, a two-color product is finally obtained.

[0003] Since the overall area of ​​the product is very large, for example Figure 1 and Figure 2 The length of the medium-sized product is close to 800mm and the width is close to 300mm. The material used for the soft rubber part is TPE and other highly elastic soft rubber materials. At the same time, the product is provided with openings (such as Figure 1 Therefore, in the second step of soft plastic injection molding, there are often defects in the appearance of parts such as air entrapment on the A side of the product, cracking of the joint line, and lack of material, resulting in a low yield rate of product molding. Therefore, it is necessary to improve the existing mold structure in order to improve the molding yield rate of large-area two-color injection products. Utility Model Content

[0004] The utility model aims to provide a large-area two-color injection molding product molding device to solve the problem of low molding yield when molding the soft rubber part of the large-area two-color product in the prior art.

[0005] To solve the above problems, the utility model adopts the following technical solution: a large-area two-color injection molding product molding device, including a movable mold and a fixed mold, the movable mold, the fixed mold and the hard rubber part together form a soft rubber cavity, and the movable mold is provided with a plurality of gates connected to the soft rubber cavity, and the distance between adjacent gates is less than or equal to 100mm.

[0006] The principle and beneficial effects of this scheme are as follows: in this application, a movable mold, a fixed mold and a hard rubber part that has been cast once are used to form a soft rubber cavity for molding the soft rubber part in the second step of the two-color product injection molding. Since the injection molding material corresponding to the soft rubber part has high elasticity, the number of gates connected to the soft rubber cavity is set to several in this application, and the glue is fed through multiple gates at the same time to improve the glue feeding capacity, so that the soft rubber cavity can complete the casting process quickly and efficiently, thereby reducing the quality defects such as air entrapment and cracking when the soft rubber part is injection molded, and improving the yield of two-color product injection molding; at the same time, in this application, the distance between adjacent gates is set to be less than or equal to 100mm, so as to further ensure the sufficiency and timeliness of the soft rubber cavity in the injection molding process during the large-area two-color injection molding product molding process, further reduce the appearance defects of parts during the molding process, and improve the yield of product molding.

[0007] Preferably, as an improvement, the shape of the soft-gel mold cavity is a long plate with two long sides and two short sides, and the thickness of the soft-gel mold cavity is 1.8-2.5 mm.

[0008] In this solution, the thickness of the soft rubber cavity is 1.8-2.5 mm, so that the injection process can be completed quickly and fully when the distance between adjacent gates is less than or equal to 100 mm, and a large-area two-color injection molded product that meets the requirements can be formed.

[0009] Preferably, as an improvement, all gates are distributed along the extension direction of the two wide sides of the soft glue cavity.

[0010] Compared with setting gates around the entire soft-gel mold cavity, the complicated arrangement of the gates makes the entire mold structure complicated. Compared with setting gates on the wide side of the soft-gel mold cavity, after the rubber enters the soft-gel mold cavity from the wide side of the soft-gel mold cavity, it needs to flow a longer distance to completely fill the soft-gel mold cavity, resulting in low injection molding efficiency and easy appearance defects. In this solution, by setting the gates on the two long sides of the soft-gel mold cavity, not only the mold structure is simple, but also after the rubber enters the soft-gel mold cavity from the long side position of the soft-gel mold cavity, it can quickly fill the entire soft-gel mold cavity, the injection molding efficiency is high and the risk of appearance defects during the molding process is lower.

[0011] Preferably, as an improvement, in all gates along the long side of the soft glue cavity, the distances between adjacent gates are equal and are L.

[0012] In this solution, all gates along the long side of the soft rubber cavity are arranged at an equal distance of L, so that all gates can evenly inject rubber into the soft rubber cavity, so that the soft rubber cavity can quickly and evenly complete the pouring process, thereby improving the injection molding efficiency and product molding quality.

[0013] Preferably, as an improvement, the distance between the gate close to the wide side of the soft glue cavity and the wide side of the soft glue cavity is S, wherein S<L.

[0014] In this solution, the distance between the gate near the wide side of the soft glue cavity and the wide side is set smaller, so that the gate can fully pour the edge of the soft glue cavity near the wide side, reduce the problem of pouring material shortage near the wide side, and improve the injection molding quality of the product.

[0015] Preferably, as an improvement, S=L-(10-70) mm, and S is greater than or equal to 30 mm.

[0016] In this solution, the distance between the gate close to the wide side of the soft glue cavity and the wide side of the soft glue cavity is set to be greater than or equal to 30 mm, which can avoid the gate being too close to the wide side of the soft glue cavity and causing poor glue injection. At the same time, the distance between the gate and the wide side of the soft glue cavity is set to be less than the distance between adjacent gates by 10 to 70 mm, so that the glue injection at the wide side of the soft glue cavity is stronger, ensuring the adequacy of the glue injection at the wide side of the soft glue cavity.

[0017] Preferably, as an improvement, the thickness of the soft rubber cavity is 2 mm.

[0018] In this solution, the thickness of the soft rubber cavity is set to 2 mm. At this thickness value, a good-quality soft rubber part can be injection molded to obtain a large-area two-color injection molded product with a high yield.

[0019] Preferably, as an improvement, the wide side length of the soft rubber cavity is 200-300 mm.

[0020] Preferably, as an improvement, the long side length of the soft rubber cavity is 700-800 mm.

[0021] In this scheme, the wide side length of the soft rubber cavity is set at 200-300mm and the long side length is set at 700-800mm. Under the gate setting in this scheme, large-area two-color products with good surface quality and high yield can be molded. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 It is a schematic diagram of a large-area two-color injection molding product in the prior art.

[0023] Figure 2 for Figure 1 Exploded view of the hard and soft rubber parts of the product.

[0024] Figure 3 This is a schematic diagram of Embodiment 1 of the present utility model. DETAILED DESCRIPTION

[0025] The following is further described in detail through specific implementation methods:

[0026] The figure marks in the drawings of the specification include: product 1, hard rubber part 101, soft rubber part 102, soft rubber cavity 2, long side 201, wide side 202, gate 3, and diversion channel 4.

[0027] like Figure 1 and Figure 2 As shown, a schematic diagram of a large-area two-color injection molded product 1 currently used in automobiles is shown, wherein the product 1 includes a hard rubber part 101 and a soft rubber part 102, the material of the hard rubber part 101 is ABS, the material of the soft rubber part 102 is TPE, and the soft rubber part 102 is located on the A surface of the hard rubber part 101. During the injection molding process, the hard rubber part 101 is first cast and molded, and then the soft rubber part 102 of different colors is cast and molded on the A surface of the hard rubber part 101, and finally the two-color product 1 is obtained.

[0028] like Figure 1 As shown, the large-area two-color injection molded product 1 is in the shape of a long plate as a whole. The length of the product 1 is about 800 mm, the width is about 280 mm, and the thickness is about 2 mm. When the soft rubber part 102 is injection molded, since the soft rubber material is a highly elastic TPE and the area of ​​the product 1 is large and the thickness is small, when the soft rubber part 102 is injection molded, appearance quality defects such as air entrapment, material shortage, and cracking of the joint line often occur, resulting in a low molding yield of the product 1.

[0029] Embodiment 1

[0030] This embodiment is as shown in the attached Figure 3 As shown: a large-area two-color injection molding product molding device is used to mold the soft rubber part 102 in the above-mentioned large-area two-color injection molding product 1, so as to reduce the problems of more appearance quality defects and low molding yield rate during the molding process of the soft rubber part 102. Specifically, it includes a movable mold and a fixed mold, wherein the movable mold, the fixed mold and the already molded hard rubber part 101 together surround the soft rubber cavity 2 ( Figure 3 The movable mold, the fixed mold and the soft-gel mold cavity 2 are not shown in the figure. Since the shape and size of the soft-gel part 102 are exactly the same as those of the soft-gel mold cavity 2, Figure 3 The shape and size of the soft rubber part 102 shown in the figure is used as the soft rubber cavity 2), and the shape of the soft rubber cavity 2 is a long plate with two long sides 201 and two wide sides 202, and the thickness of the soft rubber cavity 2 in this embodiment is 1.8-2.5mm, preferably 2mm; the length of the wide side 202 of the soft rubber cavity 2 is 200-300mm, and the length of the long side 201 is 700-800mm. According to the structural shape of the product 1, the length of the wide side 202 and the length of the long side 201 can vary within the corresponding size range, and the soft rubber part 102 of the corresponding size can be formed using the soft rubber cavity 2.

[0031] like Figure 3 As shown, in this embodiment, a plurality of gates 3 connected to the soft rubber cavity 2 are provided on the movable mold, and each gate 3 is correspondingly provided with a runner 4. The soft rubber material in the injection process enters the soft rubber cavity 2 through the runner 4 to form the soft rubber product 1. In order to enable the gates 3 to stably and efficiently inject the soft rubber into the soft rubber cavity 2, in this embodiment, all the gates 3 are evenly distributed along the two long sides 201 of the soft rubber cavity 2 at equal distances, and the distance L between adjacent gates 3 on the same long side 201 is less than or equal to 100 mm. In this embodiment, L is 100 mm, so that all the gates 3 can quickly and fully evenly inject the soft rubber material into the soft rubber cavity 2.

[0032] Combination Figure 2 and Figure 3 Since the product 1 is provided with a long hole a and a round hole b, in order to reduce the problem of material shortage at the wide side 202 of the soft-gel cavity 2 during the injection molding process, in this embodiment, the distance between the gate 3 close to the wide side 202 of the soft-gel cavity 2 and the wide side 202 is set to S, where S<L, and S is greater than or equal to 30mm, to avoid the gate 3 being too close to the wide side 202 and affecting the uniformity of injection; at the same time, the relationship between S and L is: S=L-(10~70)mm, for example Figure 2 The distance between the gate 3 on the upper left side and the left wide side 202 is 89.9 mm, and the distance between the gate 3 on the lower left side and the left wide side 202 is 30.6 mm, so that the gate 3 close to the wide side 202 of the soft glue cavity 2 can fully inject filler into the wide side 202 of the soft glue cavity 2, effectively improving the molding quality.

[0033] In the present embodiment, since all the gates 3 are arranged at equal distances on the two long sides 201 of the soft rubber cavity 2, during injection, the soft rubber material flows from the two long sides 201 of the soft rubber cavity 2 into the soft rubber cavity 2, so that the soft rubber cavity 2 is quickly filled, and the distance between adjacent gates 3 is small, so that the soft rubber cavity 2 is fully filled, effectively reducing the problems of air entrapment, material shortage, etc. during the injection process, thereby improving the molding quality of the soft rubber part 102 during the injection molding process, and obtaining a large-area two-color injection molded product 1 with a higher yield.

[0034] The above is only an embodiment of the utility model, and the common knowledge such as the known specific technical solutions and / or characteristics in the solution is not described in detail here. It should be pointed out that for those skilled in the art, without departing from the technical solution of the utility model, several deformations and improvements can be made, which should also be regarded as the protection scope of the utility model, and these will not affect the effect of the implementation of the utility model and the practicality of the patent. The scope of protection required by this application shall be based on the content of its claims, and the specific implementation methods and other records in the specification can be used to interpret the content of the claims.

Claims

1. A large-area two-color injection molding device, comprising a movable mold and a fixed mold, characterized in that: The movable mold, the fixed mold and the hard rubber part together form a soft rubber cavity, and the movable mold is provided with a plurality of gates connected to the soft rubber cavity, and the distance between adjacent gates is less than or equal to 100 mm; the shape of the soft rubber cavity is a long plate with two long sides and two wide sides, and the thickness of the soft rubber cavity is 1.8-2.5 mm; all gates are distributed along the extension direction of the two long sides of the soft rubber cavity, and among all gates along the long sides of the soft rubber cavity, the distance between adjacent gates is equal and the distance is L.

2. A large-area two-color injection molding device according to claim 1, characterized in that: The distance between the gate close to the wide side of the soft plastic cavity and the wide side of the soft plastic cavity is S, where S<L.

3. A large-area two-color injection molding product molding device according to claim 2, characterized in that: Where S=L-(10~70)mm, and S is greater than or equal to 30mm.

4. A large-area two-color injection molding product molding device according to any one of claims 1 to 3, characterized in that: The thickness of the soft rubber cavity is 2 mm.

5. A large-area two-color injection molding device according to claim 4, characterized in that: The wide side length of the soft rubber cavity is 200-300 mm.

6. A large-area two-color injection molding device according to claim 5, characterized in that: The long side length of the soft rubber cavity is 700-800 mm.