Zipper antiskid coating

By combining the elastic gel compressed layer and silicone anti-slip convex points in the zipper upper coating structure, the problem of zipper slippage under wet conditions is solved, and the pulling effect is enhanced and the force-saving pulling effect is achieved.

CN221963022UActive Publication Date: 2024-11-08FUJIAN AOLONG ENVIRONMENTAL PROTECTION NEW MATERIAL CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202420693750.0
Authority / Receiving Office
CN · China
Patent Type
Utility models(China)
Current Assignee / Owner
Filing Date
2024-04-07
Publication Date
2024-11-08
Estimated Expiration
2034-04-07

AI Technical Summary

Technical Problem

The existing zipper coating can easily cause slippage between the hands and the zipper puller under wet conditions, increasing the strength to pull the zipper, and not effectively preventing slippage.

Method used

Adopt a coating structure including a base layer, a compression layer, a friction layer and an anti-slip convex point. The compression layer is an elastic gel, the friction layer is silicone, and the anti-slip convex point is silicone coating. The compression layer sinks and the anti-slip convex point are enhanced by hand pressure. Friction, avoid sliding.

Benefits of technology

It effectively enhances the friction between the hands and the coating, prevents slipping, and makes pulling more labor-saving, and increases contact area and friction resistance through elastic sinking and anti-slip bumps.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN221963022U_ABST
    Figure CN221963022U_ABST
Patent Text Reader

Abstract

The utility model relates to the technical field of coatings, and provides an anti-skidding coating for a zipper, which is capable of avoiding skidding and enabling pulling to be more labor-saving, and comprises a base layer coated on a zipper head, a compression layer arranged on the base layer, a friction layer arranged on the compression layer, a plurality of anti-skidding salient points arranged on the friction layer, and when a hand touches the zipper head and pulls up the zipper head, the anti-skidding salient points are arranged on the friction layer. The compression layer deforms and sinks due to the pressure generated by the hand, and the friction force with the hand is greatly enhanced in cooperation with the anti-skid protruding points.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The utility model relates to the technical field of coatings, in particular to an anti-slip coating for zippers. Background Art

[0002] Coatings are widely used on the surfaces of various objects. Different effects are achieved by using different ingredients in the coating and by stacking different coatings in multiple layers. Some coatings can effectively prevent metal corrosion, while others can effectively prevent the surface of the workpiece from being scratched. Water-based coatings are coatings that use water as a solvent or as a dispersion medium. They have excellent non-stickiness and durability. Since no organic solvents are used, they are non-toxic, have no irritating odor, and will not pollute the environment. They are widely used in various fields.

[0003] In order to make the overall shape of the clothes more beautiful, manufacturers will spray coatings on the zippers of the clothes, so that the zippers and zipper pulls can produce different gloss and colors according to different coatings, and can make the metal zippers have better anti-rust and wear resistance.

[0004] Although the above-mentioned prior art can solve the corresponding technical problems, it still has certain defects: when the existing zipper coating is sprayed on a zipper puller without protrusions, the surface of the zipper puller is very smooth. When the sprayed zipper puller is pulled, if the hands are relatively wet, it is easy to cause the hands and the zipper puller to slip, and the coating cannot prevent the hands from slipping. The smooth surface of the coating may even aggravate the slipping phenomenon, so that a large force is required to pull the zipper puller. Utility Model Content

[0005] The utility model aims to provide a zipper anti-skid coating which can avoid slipping and make pulling more labor-saving in view of the defects and shortcomings of the prior art.

[0006] To achieve the above-mentioned purpose, the utility model adopts the following technical scheme: a zipper anti-slip coating, including a base layer applied to the zipper head, a compression layer is provided on the base layer, a friction layer is provided on the compression layer, and a plurality of anti-slip protrusions are provided on the friction layer. When the hand contacts the zipper head and pulls up the zipper head, the pressure generated by the hand causes the compression layer to deform and sink, and the friction with the hand is greatly enhanced in combination with the anti-slip protrusions.

[0007] A further improvement is that the compression layer is an elastic gel coating.

[0008] A further improvement is that a plurality of grooves are provided on the upper surface of the compression layer.

[0009] A further improvement is that the friction layer is a silicone coating layer.

[0010] A further improvement is that the anti-slip convex points are a silicone coating layer.

[0011] A further improvement is that a flattening layer is also provided on the anti-slip convex points.

[0012] A further improvement is that the flattening layer is a polyethylene coating.

[0013] A further improvement is that the compression layer has a thickness of 0.5 mm to 0.7 mm.

[0014] A further improvement is that the height of the anti-slip protrusions is 0.1mm-0.15mm.

[0015] After adopting the above technical scheme, the beneficial effect of the utility model is as follows: after spraying, the friction layer and the anti-slip bumps are used to effectively increase the friction between the hand and the coating when pulling the zipper head, and the elastic sinking effect produced by the compression layer after being pressed down allows the hand to effectively transmit the force to the coating, preventing sliding between the hand and the zipper head while making pulling more labor-saving. BRIEF DESCRIPTION OF THE DRAWINGS

[0016] In order to more clearly illustrate the embodiments of the utility model or the technical solutions in the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, the drawings described below are only some embodiments of the utility model. For ordinary technicians in this field, other drawings can be obtained based on these drawings without paying creative labor.

[0017] Figure 1 It is a structural schematic diagram of a front view cross section of the coating of the utility model. DETAILED DESCRIPTION

[0018] The utility model is now further described in conjunction with the accompanying drawings and specific embodiments.

[0019] See also Figure 1As shown, the technical solution adopted in this specific embodiment is: a zipper anti-skid coating, including a base layer 1 applied on the zipper head, a compression layer 2 is provided on the base layer 1, the compression layer 2 is an elastic gel coating, a friction layer 3 is provided on the compression layer 2, the friction layer 3 is a silicone coating layer, and a plurality of anti-skid convex points 4 are provided on the friction layer 3, the anti-skid convex points 4 are silicone coating layers, and this embodiment has eleven. When the hand contacts the zipper head and pulls up the zipper head, the pressure generated by the hand causes the compression layer 2 to deform and sink, and the friction with the hand is greatly enhanced in combination with the anti-skid convex points 4. When in use, first apply the base layer 1 on the smooth zipper head, and then Then, a compression layer 2 is applied on the base layer 1. After the compression layer 2 is dried, a friction layer 3 is applied on the compression layer 2, and anti-skid convex points 4 are arranged on the friction layer 3 by dotting. After the coating solidifies, when pulling, the hand contacts the friction layer 3 and the anti-skid convex points 4 of the coating, and applies pressure, so that the compression layer 2 is compressed and elastically deformed, thereby causing the friction layer 3 to sink at the same time, thereby greatly increasing the contact area between the hand and the friction layer 3. At this time, the friction resistance between the hand and the coating can be increased by cooperating with the friction layer 3 and the anti-skid convex points 4 to avoid slipping. At the same time, when pulling, the force transmission can be more sufficient by expanding the contact area, making the pulling more labor-saving;

[0020] The upper surface of the compression layer 2 is also provided with a plurality of grooves 6. In this embodiment, six grooves are provided, which is conducive to enabling the compression layer 2 to be compressed and deformed more quickly and with a larger deformation amplitude, thereby further enhancing the anti-slip effect.

[0021] The anti-slip convex point 4 is also provided with a flat layer 5, and the flat layer 5 is a polyethylene coating, which is conducive to making the surface look smoother and more beautiful;

[0022] The thickness of the compression layer 2 is 0.5 mm to 0.7 mm, which is conducive to increasing the upper limit of compression through thickness, thereby allowing the hand to press deeper and obtain a larger contact area;

[0023] The height of the anti-skid protrusions 4 is 0.1 mm-0.15 mm, which is conducive to making the coating thinner while maintaining the anti-skid effect.

[0024] Working principle of the utility model: when the utility model is used, firstly, a base layer 1 is applied on a smooth zipper head, and then a compression layer 2 is applied on the base layer 1. After the compression layer 2 is dried, a friction layer 3 is applied on top thereof, and anti-skid protrusions 4 are arranged on the friction layer 3 by dotting. After the coating is solidified, when pulling, the hand contacts the friction layer 3 and the anti-skid protrusions 4 of the coating, and applies pressure, so that the compression layer 2 is compressed and elastically deformed, thereby causing the friction layer 3 to sink at the same time, thereby greatly increasing the contact area between the hand and the friction layer 3. At this time, the friction layer 3 and the anti-skid protrusions 4 can be used to increase the friction resistance between the hand and the coating to avoid slipping. At the same time, when pulling, the force transmission can be more sufficient by expanding the contact area, making the pulling more labor-saving.

[0025] The utility model is intended to protect the structure of the product. The model of each component is not the content of the utility model, and it is also a known technology. Any component on the market that can achieve the above functions of the utility model can be used as a choice. Therefore, the model and other parameters of the component are not described in detail in this utility model. The contribution of this utility model lies in the scientific combination of various components.

[0026] The above shows and describes the basic principle and main features and advantages of the utility model. Those skilled in the art should understand that the utility model is not limited by the above embodiments. The above embodiments and descriptions are only for explaining the principle of the utility model. Without departing from the spirit and scope of the utility model, the utility model may have various changes and improvements, which fall within the scope of the utility model to be protected. The scope of protection of the utility model is defined by the attached claims and their equivalents. Anything not described in detail in the utility model is a well-known technology of those skilled in the art.

Claims

1. A zipper anti-slip coating, comprising a base layer (1) applied to a zipper head, characterized in that: A compression layer (2) is provided on the base layer (1), a friction layer (3) is provided on the compression layer (2), and a plurality of anti-slip convex points (4) are provided on the friction layer (3). When a hand contacts the zipper head and pulls up the zipper head, the pressure generated by the hand causes the compression layer (2) to deform and sink, and the friction force with the hand is greatly enhanced in combination with the anti-slip convex points (4).

2. The zipper anti-slip coating according to claim 1, characterized in that: The compression layer (2) is an elastic gel coating.

3. The anti-slip coating for zippers according to claim 1, characterized in that: The upper surface of the compression layer (2) is also provided with a plurality of grooves (6).

4. The anti-slip coating for zippers according to claim 1, characterized in that: The friction layer (3) is a silicone coating layer.

5. The zipper anti-slip coating according to claim 1, characterized in that: The anti-slip protrusions (4) are a silicone coating layer.

6. The anti-slip coating for zippers according to claim 1, characterized in that: A flattening layer (5) is also provided on the anti-slip protrusions (4).

7. The anti-slip coating for zippers according to claim 6, characterized in that: The flattening layer (5) is a polyethylene coating.

8. The anti-slip coating for zippers according to claim 1, characterized in that: The compression layer (2) has a thickness of 0.5 mm to 0.7 mm.

9. The anti-slip coating for zippers according to claim 1, characterized in that: The anti-slip protrusions (4) have a height of 0.1 mm to 0.15 mm.