Gating system of wind power bearing seat casting
By designing a semi-enclosed bottom pouring system with multiple transition runners and filter runners, the problems of turbulence and slag inclusion in the casting process of wind power bearing seat casting are solved, efficient iron flow and impurity filtration are achieved, and the Yield rate and performance.
Patent Information
- Application Number
- CN202420391944.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-02-29
- Publication Date
- 2024-11-12
- Estimated Expiration
- 2034-02-28
AI Technical Summary
Wind power bearing seat castings are prone to turbulence and slag inclusion during casting, resulting in a decrease in yield, and the prior art is difficult to meet the requirements of high strength and high performance.
A semi-enclosed bottom pouring system including straight runners, transverse runners, inner runners and transition runners is designed, using straight runners, trapezoidal filters and foam filters with a 90-degree right angle bent angle, through multiple The transition runner and filter runner achieve balanced flow of iron and impurity filtration, reducing the generation of oxidized slag inclusions.
It effectively reduces the generation of oxidized slag inclusions in molten iron, improves the yield of castings, ensures high strength and high performance of castings, and reduces the risks of impact and turbulence.
Smart Images

Figure CN221983843U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of casting technology for castings used in the wind energy field, and particularly to a gating system for a wind power bearing housing casting. Background Art
[0002] Wind energy is a renewable and pollution-free clean energy, and the vigorous development of wind energy is a reliable way to solve the energy for production and life.
[0003] With the rapid development of the wind power industry, the demand for ductile iron fittings for wind power has increased rapidly, and the ductile iron used for wind power has developed rapidly. Due to its low cost and high strength and toughness, ductile iron has been widely used. However, compared with ordinary ductile iron, higher quality and performance requirements are imposed on wind power castings because the working environment of wind turbines is harsh and maintenance is difficult. Therefore, higher quality and service performance requirements are imposed on wind power castings. As shown in the appendix Fig.10 is a large ductile iron wind power bearing housing (XB bearing housing). The casting product includes a wind power bearing housing casting a. The casting body a includes a quasi-cylindrical structure with a hollow central hole, and vertical parts are arranged on both radial sides of the quasi-cylindrical structure; there is a body nesting part a1 between the quasi-cylindrical structure and the vertical part; the overall blank weight of this casting is 4800 Kg, the pouring weight is 5700 Kg, the material is ductile iron EN-GJS-400-18LT, the external dimensions are 3585 mm × 2280 mm × 430 mm, the maximum wall thickness is 400 mm, the minimum wall thickness is 60 mm. For the casting product, key parts (vertical part a3) extending vertically are arranged on both sides, and there is a quasi-cylindrical structure with a central hole in the middle. No casting defects such as slag inclusions, shrinkage cavities, and shrinkage porosity are allowed in this key part (vertical part a3), and the requirements are extremely high. In addition, sampling rods are sleeved in the key part (vertical part a3) with a thickness of 320 mm to test mechanical properties (yield strength, tensile strength, elongation (elongation rate), impact performance, hardness) and metallography. The mechanical properties should meet the corresponding values in EN 1563 standard for 60 mm < t (wall thickness) ≤ 200 mm. Its casting technology is very difficult, and conventional casting processes cannot achieve it.
[0004] For this large ductile iron wind power bearing housing structure, due to its thick thickness, high height, and heavy weight, a large amount of molten iron is required to pour and fill the casting cavity. If the gating system is not designed reasonably, turbulent flow is likely to occur, resulting in the appearance of slag inclusions and gas holes, reducing the yield rate of the casting. Summary of the Utility Model
[0005] In view of the above-mentioned deficiencies in the prior art, the present application provides a casting system for wind turbine bearing seat castings that can effectively reduce turbulence during molten iron filling, enable slag inclusions to float on the surface of molten iron, effectively remove slag inclusions, and prevent iron slag from entering the casting, thereby achieving the purpose of reducing slag inclusions in the casting and greatly improving the casting yield rate.
[0006] In order to solve the above technical problems, the technical solution adopted in the present application is as follows: a casting system for a wind power bearing seat casting, the casting system includes a casting cavity, a casting structure connected to the casting cavity, the casting structure includes a straight runner, a cross runner and an ingrown runner connected to each other, the straight runner includes a first vertical portion, a second horizontal portion and a third vertical portion connected in sequence; the cross runner includes a horizontal extension portion and a vertical extension portion, a transition runner and a filter runner are arranged between the cross runner and the ingrown runner, the transition runner includes a first transition runner and a second transition runner connected to each other, the first transition runner is truncated, and the There are five second transition runners, which are circumferentially dispersed along the lower bottom surface of the truncated cone-shaped first transition runner; the vertical extension portion is interconnected with the first transition runner and the second transition runner; the five second transition runners are respectively connected to an entrail, and a filter runner consisting of a first filter part and a second filter part is arranged between each second transition runner and the entrail, the first filter part and the second filter part are connected vertically, and a foam filter is arranged between the two, and the tail end of the second transition runner is interconnected with the first filter part; one end of the entrail is connected with the second filter part, and the other end is connected with the bottom surface of the casting cavity.
[0007] By adopting the above structure, the present application sets up a pouring system of this specific structure to constitute a semi-closed bottom pouring pouring system, in which the straight runner is partially set with a 90-degree right-angle bend, which can ensure that the straight runner is quickly filled with molten iron (molten iron for preparing castings), reducing the generation of oxidized slag inclusions in the molten iron and the filling flow rate; in addition, the present application can effectively filter impurities in the molten iron and prevent slag inclusions from entering the mold cavity by setting a first filter part and a second filter part and a foam filter therebetween; moreover, the present application sets up five second transition runners and extends them in a dispersed manner along the circumferential direction, which can realize five molten iron introduction channels with the casting mold cavity, improve the balance of the molten iron feeding in the mold cavity, and can achieve smooth entry into the mold cavity, reducing the generation of oxidized slag inclusions.
[0008] Furthermore, the first filter part and the second filter part described in the present application are a trapezoidal structure with one end narrow and the other end wide along the thickness direction, and one side of the wide bottom surface is close to the foam filter; the thickness of the first filter part and the second filter part is greater than the thickness of the second transition runner; with this structure, the molten iron enters the first filter part and the second filter part with large thickness and large pore size from the second transition runner with small thickness, and the flow rate is slowed down, which is more conducive to the smooth flow of the molten iron. When it enters the inner runner again, the flow rate is also slowed down, thereby reducing the impact on the casting cavity and making turbulence less likely to occur.
[0009] Furthermore, the periphery of the first filter part and the second filter part that are in contact with the foam filter is indented inward by 8mm to 12mm relative to the periphery of the foam filter; the above structure is set with an indentation specification, which can facilitate the filling of molding sand within this size range, thereby providing the filter with sufficient molding sand support and preventing the foam filter from being deformed or broken under the dual effects of high-temperature molten iron and hot air flow impact.
[0010] Furthermore, a third transition runner is arranged between the inner runner and the casting cavity, and the third transition runner is connected to the bottom of the casting cavity; the above structure, combined with a plurality of second transition runners respectively arranged and connected to the inner runners, is beneficial to the floating of molten iron slag, and is also beneficial to the molten iron entering the cavity more smoothly, reducing the generation of oxidized slag inclusions.
[0011] Furthermore, the end surface of the third transition runner communicating with the casting cavity is a rectangular structure, and the height of the third transition runner is 70 mm to 90 mm; adopting the above scheme can slow down the flow rate of molten iron entering the cavity.
[0012] Furthermore, the end face of the second transition runner close to the first transition runner is smaller than the end face close to the first filter portion, and the ratio of the end face areas of the two is 1:1.10-1.20; that is, the second transition runner is wide at one end and narrow at the other end. The above structure can effectively slow down the flow rate of molten iron, thereby reducing the generation of oxidized slag inclusions in molten iron and the filling flow rate.
[0013] Furthermore, the straight runner, cross runner, ingates and third transition runner are all made of refractory ceramic tubes. With this structure, it is not necessary to additionally use molding sand to mold the straight runner, ingates and third transition runner. Moreover, the refractory ceramic tubes are directly used to reduce sand blasting defects and avoid damage to the above-mentioned runners by high-temperature molten iron during the pouring process.
[0014] Furthermore, the total cross-sectional area ratio of the main casting units is: ΣA straight runner: ΣA second transition runner: ΣA endocastor: ΣA third transition runner outlet (i.e., the rectangular port connected to the casting cavity) = 1: 1.00~1.20: 1.20~1.30: 1.30~1.40; the present application sets the minimum cross-sectional area on the straight runner, and the straight runner partially adopts a 90-degree right-angle bend to ensure that the straight runner can be quickly filled, reducing the generation of oxidized slag inclusions in the molten iron and the filling flow rate.
[0015] Furthermore, the upper surface of the casting cavity is also provided with a safety riser and an air outlet; the safety riser is arranged on the end faces of the vertical parts on both sides of the casting cavity, and the air outlet is arranged on the end face of the cylindrical part in the middle of the casting cavity; with this structure, the air outlet can effectively discharge the high-temperature gas generated during the casting process, and the safety riser can also effectively supplement the molten iron, which can prevent the occurrence of shrinkage cavities and shrinkage in the casting, and has the functions of exhausting gas and collecting slag. BRIEF DESCRIPTION OF THE DRAWINGS
[0016] Figure 1 Structural schematic diagram of the first view of the casting structure of the wind turbine bearing seat of the present application.
[0017] Figure 2 Structural schematic diagram of the second view of the casting structure of the wind turbine bearing seat of the present application.
[0018] Figure 3 The structural schematic diagram of the third view of the casting structure of the wind turbine bearing seat of the present application.
[0019] Figure 4 A structural schematic diagram of a bottom view of the casting structure of a wind turbine bearing seat in the present application.
[0020] Figure 5 Structural schematic diagram of a top view of the casting structure of a wind turbine bearing seat in the present application.
[0021] Figure 6 Structural schematic diagram of the front view of the casting structure of the wind turbine bearing seat of the present application.
[0022] Figure 7 This application Figure 6 Schematic diagram of the structure of a local enlarged view.
[0023] Figure 8 Structural schematic diagram of the first view of the casting system of the wind turbine bearing seat of the present application.
[0024] Fig. 9 The structural schematic diagram of the second view of the casting system of the wind turbine bearing seat of the present application.
[0025] Fig.10A schematic structural diagram of a wind turbine bearing seat casting (or called a casting cavity) of the present application.
[0026] As shown in the accompanying drawings: a. Casting cavity, 1. Straight runner, 101. First vertical portion, 102. Second lateral portion, 103. Third vertical portion, 2. Horizontal runner, 201. Horizontal extension portion, 202. Vertical extension portion, 3. Ingate, 4. Transition runner, 401. First transition runner, 402. Second transition runner, 403. Third transition runner, 5. Filter runner, 501. First filter portion, 502. Second filter portion, 6. Foam filter, 7. Safety riser, 8. Air outlet. DETAILED DESCRIPTION
[0027] The following will combine the embodiments and drawings to clearly and completely describe the technical solutions in the embodiments of the present application. Obviously, the described embodiments are only preferred embodiments, not all embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention;
[0028] It should also be noted that when a component is referred to as being "fixed to" another component, it may be directly on the other component or there may also be another intermediate component, fixed through the intermediate component. When a component is considered to be "connected" to another component, it may be directly connected to the other component or there may be another intermediate component at the same time. When a component is considered to be "set on" another component, it may be directly set on the other component or there may be another intermediate component at the same time. The terms "vertical", "horizontal", "left", "right" and similar expressions used herein are for illustrative purposes only. Unless otherwise defined, all technical and scientific terms used herein have the same meaning as those generally understood by technicians in the technical field of the present invention. The terms used in the specification of the present invention herein are only for the purpose of describing specific embodiments and are not intended to limit the present invention. The term "and / or" used herein includes any and all combinations of one or more related listed items.
[0029] The casting cavity of the present application can be the structure of the casting cavity for pouring, or the final casting structure, because the casting is obtained by first forming a cavity consistent with the casting structure, pouring molten iron in the cavity and cooling it. Therefore, the casting cavity (body) of the present application and the structure of the casting can be referred to as the same, and the structural relationship between each structure and the casting cavity body can also be seen as the structural relationship between the casting.
[0030] As attached Figure 1-9As shown, a pouring system of a wind turbine bearing seat casting of the present application is shown, the pouring system includes a casting cavity a, a pouring structure connected to the casting cavity a, the pouring structure includes a straight runner 1, a horizontal runner 2 and an inner runner 3 connected to each other, the straight runner 1 includes a first vertical portion 101, a second horizontal portion 102 and a third vertical portion 103 connected in sequence (that is, the tail end of the first vertical portion is connected to the second horizontal portion, and the second horizontal portion extends horizontally for a distance so that the subsequent third vertical portion is laterally offset by a certain distance); the horizontal runner 2 It includes a lateral extension portion 201 and a vertical extension portion 202. A transition runner 4 and a filter runner 5 are arranged between the cross runner 2 and the inner runner 3. The transition runner 4 includes a first transition runner 401 and a second transition runner 402 that are interconnected. The first transition runner 401 is truncated cone-shaped. The second transition runner 402 is provided with five circumferentially dispersed arrangements along the lower bottom surface of the truncated cone-shaped first transition runner 401 (that is, the five second transition runners are evenly distributed along the circumference of the large bottom surface of the first transition runner); the vertical The vertical extension portion 202 is connected to the first transition runner 401 and the second transition runner 402 (specifically, the five second transition runners have a disk connected to the bottom surface of the first transition runner, and the five second transition runners are arranged on the circumference of the disk. The molten iron enters the disk from the vertical extension portion and then hits the first transition runner upward, falls back into the disk and then disperses into the five second transition runners, so as to achieve the buffering of the molten iron and reduce its flow rate); each of the five second transition runners 402 is connected to an inner runner 3, and each second transition runner 4 A filter runner 5 consisting of a first filter part 501 and a second filter part 502 is arranged between 02 and the ingrowth 3. The first filter part 501 and the second filter part 502 are connected to each other up and down (the first filter part 501 and the second filter part 502 are both trapezoidal structures with the same size), and a foam filter 6 is arranged between the two, and the tail end of the first filter part 501 is connected to the foam filter 6; one end of the ingrowth 3 is connected to the second filter part 502, and the other end is connected to the bottom surface of the casting cavity a.
[0031] By adopting the above structure, the present application sets up a pouring system of this specific structure to constitute a semi-closed bottom pouring pouring system, in which the straight runner is partially set with a 90-degree right-angle bend, which can ensure that the straight runner is quickly filled with molten iron (molten iron for preparing castings), reducing the generation of oxidized slag inclusions in the molten iron and the filling flow rate; in addition, the present application can effectively filter impurities in the molten iron and prevent slag inclusions from entering the mold cavity by setting a first filter part and a second filter part and a foam filter therebetween; moreover, the present application sets up five second transition runners and extends them in a dispersed manner along the circumferential direction, which can realize five molten iron introduction channels with the casting mold cavity, improve the balance of the molten iron feeding in the mold cavity, and can achieve smooth entry into the mold cavity, reducing the generation of oxidized slag inclusions.
[0032] As attached Figure 1-6 As shown in 8-9, the first filter part 501 and the second filter part 502 described in the present application are a trapezoidal structure with one end narrow and the other end wide along the thickness direction, and one side of the wide bottom surface is close to the foam filter 6; the thickness of the first filter part 501 and the second filter part 502 is greater than the thickness of the second transition runner 402; with this structure, the molten iron enters the first filter part 501 and the second filter part 502 with large thickness and large pore size from the second transition runner with small thickness, and the flow rate is slowed down, which is more conducive to the smooth flow of the molten iron. When it enters the inner runner again, the flow rate is also slowed down, thereby reducing the impact on the casting cavity and making turbulence less likely to occur.
[0033] As an example, the attached Figure 1-5 As shown, the periphery of the first filter portion 501 and the second filter portion 502 described in the present application that are in contact with the foam filter 6 is indented inward by 8mm to 12mm relative to the periphery of the foam filter 6; that is, the edges of the large bottom surfaces of the first filter portion 501 and the second filter portion 502 are indented inward by a certain size relative to the circumferential edges of the foam filter 6. The above structure sets an indentation specification, which can facilitate the filling of molding sand within this size range, thereby providing the filter with sufficient molding sand support, preventing the foam filter from being deformed or broken under the dual effects of the impact of high-temperature molten iron and hot air flow.
[0034] As attached Figure 1-10 As shown, a third transition runner 403 is also arranged between the inner runner 3 described in the present application and the casting cavity a, and the third transition runner 403 is connected to the bottom of the casting cavity a; the above-mentioned structure, combined with a plurality of second transition runners respectively arranged and connected to the inner runners, is beneficial to the floating of molten iron slag, and is also beneficial to the molten iron entering the cavity more smoothly, reducing the generation of oxidized slag inclusions.
[0035] As attached Figure 1 As shown, the end face of the third transition runner 403 described in the present application that is connected to the casting cavity a is a rectangular structure, and the height of the third transition runner 403 is 70mm to 90mm; adopting the above scheme can slow down the flow rate of molten iron entering the cavity.
[0036] As attached Figure 4-5 As shown, the end face of the second transition runner 402 described in the present application, which is close to the first transition runner 401, is smaller than the end face of the second transition runner, which is close to the first filter portion 501, and the ratio of the end face areas of the two is 1:1.10-1.20; that is, the second transition runner is a structure of unequal diameters with one end narrow and the other end wide. The above structure can effectively slow down the flow rate of molten iron, thereby reducing the generation of oxidized slag inclusions in molten iron and the filling flow rate.
[0037] As an example, the straight runner 1, cross runner 2, ingente 3 and third transition runner 403 described in the present application are all composed of refractory ceramic tubes (commercially available hollow refractory ceramic tubes can be used, which can meet the casting requirements of the present application); with this structure, there is no need to additionally use sand casting to mold the above-mentioned straight runner, ingente and third transition runner, and refractory ceramic tubes are directly used to reduce sand blasting defects and avoid damage to the above-mentioned runners by high-temperature molten iron during the casting process.
[0038] As an example, the total cross-sectional area ratio of the main casting units described in the present application is: ΣA straight runner: ΣA second transition runner: ΣA endocastor: ΣA third transition runner outlet (i.e., the rectangular port connected to the casting cavity) = 1: 1.00~1.20: 1.20~1.30: 1.30~1.40; the present application sets the minimum cross-sectional area on the straight runner, and the straight runner partially adopts a 90-degree right-angle bend to ensure that the straight runner can be quickly filled, reducing the generation of oxidized slag inclusions in the molten iron and the filling flow rate; the right-angle runner and the cross runner of the present application can adopt an integrated structure.
[0039] As attached Figure 8-10 As shown, the upper surface of the casting cavity a described in the present application is also provided with a safety riser 7 and an air outlet 8 (six safety risers and four air outlets); the safety riser 7 is arranged on the end faces of the vertical parts on both sides of the casting cavity a, and the air outlet 8 is arranged on the end face of the cylindrical part in the middle of the casting cavity a; with this structure, the air outlet can effectively discharge the high-temperature gas generated in the casting process, and the safety riser can also effectively supplement the molten iron, which can prevent the occurrence of shrinkage cavities and shrinkage in the casting, and has the functions of exhausting gas and collecting slag.
Claims
1. A pouring system for a wind turbine bearing seat casting, characterized in that: The pouring system includes a casting cavity and a pouring structure connected to the casting cavity. The pouring structure includes a straight runner, a cross runner and an ingode that are connected to each other. The straight runner includes a first vertical portion, a second horizontal portion and a third vertical portion that are connected in sequence. The cross runner includes a horizontal extension portion and a vertical extension portion. A transition runner and a filter runner are arranged between the cross runner and the ingode. The transition runner includes a first transition runner and a second transition runner that are connected to each other. The first transition runner is truncated cone-shaped. The second transition runner is provided with five lines that extend along the truncated cone-shaped first transition runner. The lower bottom surface of the transition runner is dispersed in the circumference; the vertical extension part is interconnected with the first transition runner and the second transition runner; the five second transition runners are respectively connected to an entrail, and a filter runner consisting of a first filter part and a second filter part is arranged between each second transition runner and the entrail, the first filter part and the second filter part are connected up and down, and a foam filter is arranged between the two, and the tail end of the second transition runner is interconnected with the first filter part; one end of the entrail is connected with the second filter part, and the other end is connected with the bottom surface of the casting cavity.
2. The pouring system for the wind turbine bearing seat casting according to claim 1 is characterized in that: The first filter part and the second filter part are a trapezoidal structure with one end narrower and the other end wider in the thickness direction, and one side of the wide bottom surface is close to the foam filter; the thickness of the first filter part and the second filter part is greater than the thickness of the second transition runner.
3. The pouring system for the wind turbine bearing seat casting according to claim 1 is characterized in that: The peripheries of the first filter part and the second filter part that are attached to the foam filter are indented inwardly by 8mm to 12mm relative to the periphery of the foam filter.
4. The pouring system for a wind turbine bearing seat casting according to claim 1 is characterized in that: A third transition runner is also provided between the inner runner and the casting cavity, and the third transition runner is connected to the bottom of the casting cavity.
5. The pouring system for the wind turbine bearing seat casting according to claim 4 is characterized in that: The end surface of the third transition runner communicating with the casting cavity is a rectangular structure, and the height of the third transition runner is 70 mm to 90 mm.
6. The pouring system for a wind turbine bearing seat casting according to claim 1, characterized in that: The end surface of the second transition runner close to the first transition runner is smaller than the end surface close to the first filter portion, and the ratio of the end surface areas of the two is 1:1.10-1.
20.
7. The pouring system for a wind turbine bearing seat casting according to claim 1, characterized in that: The straight runner, the cross runner, the inner runner and the third transition runner are all made of refractory ceramic tubes.
8. The pouring system for a wind turbine bearing seat casting according to claim 1, characterized in that: The total cross-sectional area ratio of the main pouring units of the straight runner, the second transition runner, the ingode and the third transition runner outlet is: ΣA straight runner: ΣA second transition runner: ΣA ingode: ΣA third transition runner outlet = 1: 1.00~1.20: 1.20~1.30: 1.30~1.
40.
9. The pouring system for a wind turbine bearing seat casting according to claim 1, characterized in that: The upper surface of the casting cavity is also provided with a safety riser and an air outlet; the safety riser is arranged on the end faces of the vertical parts on both sides of the casting cavity, and the air outlet is arranged on the end face of the cylindrical part in the middle of the casting cavity.