Prism structure, brightness enhancement film, POP type laminated brightness enhancement film applied to prism structure, and display device
By using the prism structure with the first prism and the second prism interlaced in the brightening film, combined with the high refractive index resin, the problem of easy damage to the brightening film during transportation and installation is solved, and high brightness and scratch resistance are achieved The improvement in performance simplifies the optical film structure and reduces costs.
Patent Information
- Application Number
- CN202420580313.8
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-03-25
- Publication Date
- 2024-11-15
- Estimated Expiration
- 2034-03-25
AI Technical Summary
The existing brightening films are easily damaged by scratches during transportation and installation, resulting in damage to the microstructure of the optical film, reducing utilization and yield. The existing protective measures such as residual glue left after the protective film is peeled off or high cost or high The refractive index of the resilience resin limits the luminance and cannot effectively protect the optical film microstructure.
The prism structure is adopted in which the first prism and the second prism are arranged intersected at preset angles. The height of the second prism is greater than that of the first prism, and the cross-section of the second prism is an isosceles triangle or flat top structure, combined with a high refractive index The photocuring hard resin forms an optimized transparent structural layer to improve scratch resistance and luminance.
It achieves high brightness and excellent scratch resistance, simplifies the optical film structure, reduces costs, avoids the appearance of the protective film after peeling off, and improves the optical benefits of the diaphragm.
Smart Images

Figure CN222014504U_ABST
Abstract
Description
Technical Field
[0001] The utility model relates to the technical field of optical films, in particular to a prism structure, a brightness enhancement film and applications thereof to a POP type laminating brightness enhancement film and a display device. Background Art
[0002] At present, brightness enhancement film (BEF) is usually used in backlight modules to gather light emitted by light sources. In particular, in display devices such as monitors, brightness enhancement film is often used to increase display brightness and thus reduce the energy consumption of the display. The brightness enhancement film is usually composed of a substrate and a focusing prism structure on the substrate, and both the substrate and the focusing prism structure are made of transparent resin material. Usually, the prism structure layer is composed of a plurality of identical prism strips for converging light, and these prism strips are arranged in parallel in the same direction to form a prism array. The prism array adjusts the light emitted outside the observer's field of view to within the observer's field of view through refraction and reflection of light, thereby improving the utilization rate of the light energy emitted by the light source.
[0003] However, the brightness enhancement film will be scratched to varying degrees during transportation and installation, causing damage to the optical film microstructure, thereby reducing utilization and yield, and thus increasing costs.
[0004] To solve the above problems, patent number CN206594325U proposes a high-transmittance, scratch-resistant, and brightening film, comprising a substrate, a brightening layer arranged on one side of the substrate, and an anti-sticking layer arranged on the other side of the substrate, the brightening layer comprising a first prism and a second prism, the cross-section of the second prism is an isosceles triangle, the cross-section of the first prism is a trapezoid, the top of the trapezoid is provided with diffusion particles, and the height of the first prism is greater than the height of the second prism.
[0005] Patent No. CN101216639A proposes an optical film, comprising a substrate and a microstructure layer located on a surface of the substrate, wherein the microstructure layer comprises one or more first regions, each of the first regions comprises at least one multi-peak columnar structure, the multi-peak columnar structure is a union structure formed by at least two columnar structures overlapping each other, and the maximum height of the multi-peak columnar structure is composed of an arc columnar structure; and the microstructure layer optionally comprises one or more second regions, each of the second regions comprises at least one single-peak prismatic columnar structure.
[0006] An optical film comprises a substrate, a microstructure layer located on one surface of the substrate and an anti-scratch layer located on the other surface of the substrate, wherein the microstructure layer comprises a repeating structure composed of a first region and a second region, wherein the first region comprises at least one multi-peak columnar structure, and the multi-peak columnar structure is composed of a union structure formed by at least two arc columnar structures overlapping each other, wherein adjacent side surfaces of two adjacent columnar structures are connected to form a valley line, and the height of the valley line is 45% to 80% of the height of the lower one of the two adjacent columnar structures; and the second region comprises at least one single-peak prismatic columnar structure; wherein the maximum height of the multi-peak columnar structure in the first region is greater than the maximum height of the single-peak prismatic columnar structure in the second region.
[0007] In the prior art, in order to protect the microstructure of the brightness enhancement film, a protective film is usually applied on the brightness enhancement film. The protective film is adhered to the prism structure layer of the brightness enhancement film through an adhesive layer to protect the prism structure layer. However, there will be residual adhesive left after the protective film is peeled off and other risks of poor appearance, which will also lead to increased costs. This method can only prevent the damage to the surface microstructure of the optical film product during the transportation stage, but cannot protect the optical film microstructure during the backlight module assembly stage and the transportation stage of the finished display. Alternatively, a resilient self-repairing resin is used as the UV resin coating of the microstructure layer to improve the scratch resistance of the brightness enhancement film. However, the refractive index of the resin with excellent high resilience and scratch resistance is usually not more than 1.56, which limits the brightness of the brightness enhancement film.
[0008] On the other hand, there are also methods proposed to improve the scratch resistance of the brightness enhancement film by microstructure design, such as a fully rounded prism structure, or a high (rounded prism) and low (pointed prism) structure. The former has low brightness due to the destruction of the prism tip, and too many rounded corners are prone to film adsorption problems. Although the latter retains some prism tips and provides brightness guarantee, the mold processing time is long, and the same direction of large and small prisms is prone to optical interference problems. No effective solution has been proposed for the above problems. Utility Model Content
[0009] Purpose of the utility model: To provide a prism structure, a brightness enhancement film and its application in a POP type laminated brightness enhancement film and a display device, so as to solve the above-mentioned problems existing in the prior art.
[0010] Technical solution: A prism structure, comprising: a plurality of first prisms and a plurality of second prisms arranged in an array, and the height of the second prisms is greater than the height of the first prisms; wherein the first prisms and the second prisms are arranged alternately with each other according to a preset angle.
[0011] Preferably, the first extension axis of the first prism and the second extension axis of the second prism are in different extension directions and are arranged in a staggered manner.
[0012] Preferably, the angle a between the extension direction of the first prism and the extension direction of the second prism is 10°~170°.
[0013] Preferably, the height h of the first prism is 10-40 um.
[0014] Preferably, the distance d between adjacent second prisms is 0-20h.
[0015] Preferably, a height H of the second prism is greater than a height h of the first prism, and H ≧ h+1 um.
[0016] Preferably, the cross section of the second prism is an isosceles triangle, and the top angle thereof is a rounded or flat-top structure.
[0017] Preferably, when the vertex angle of the second prism is rounded, the center of the arc is located on the perpendicular line of the second prism, and the fillet radius r is 0.25-5 um.
[0018] Preferably, when the vertex angle of the second prism is a flat-top structure, its vertex angle width W is 0.5-7 um.
[0019] Preferably, the cross section of the first prism is an isosceles right triangle.
[0020] Preferably, the first prism and the second prism are photocurable hard resins, and the refractive index range of the resins is 1.5-1.7.
[0021] Preferably, the second prism is configured as a non-pointed prism structure.
[0022] In order to achieve the above objective, according to another aspect of the present application, a brightness enhancement film is also provided.
[0023] The brightness enhancement film according to the present application is characterized by comprising the prism structure as described above;
[0024] It also includes: the first prism and the second prism are arranged alternately with each other at a preset angle to form a transparent structure layer; and a substrate layer is arranged on the side of the transparent structure layer away from the extension axis.
[0025] In order to achieve the above-mentioned purpose, according to another aspect of the present application, a POP-type laminating brightness enhancement film is also provided.
[0026] According to the POP type laminated brightness enhancement film of the present application, the upper prism layer includes the brightness enhancement film as described above.
[0027] In order to achieve the above objective, according to another aspect of the present application, a display device is also provided.
[0028] The display device according to the present application includes the brightness enhancement film as described above.
[0029] Beneficial effect: In the embodiment of the present application, the micro-prism structure is optimized, and the first prism and the second prism are staggered at a preset angle to achieve the purpose of high brightness and excellent scratch resistance, thereby achieving the technical effect of simplifying the optical film structure and improving the optical benefit of the film, thereby solving the problem in the prior art that a layer of protective film is usually applied to the brightness enhancement film, and the protective film is adhered to the prism structure layer of the brightness enhancement film by glue to protect the prism structure layer, but there will be residual glue left after the protective film is peeled off and other risks of poor appearance, which will also lead to an increase in cost; or a resin with good self-rebound and scratch resistance is used as The UV resin coating on the upper layer is used to improve the scratch resistance of the brightness enhancing film. However, the refractive index of the resin with excellent high rebound scratch resistance is usually not more than 1.56, which limits the brightness of the brightness enhancing film. On the other hand, there are also methods proposed to improve the scratch resistance of the brightness enhancing film by microstructure design, such as a full rounded prism structure, or a high (rounded prism) and low (pointed prism) structure. The former has low brightness due to the destruction of the prism tip, and too many dome angles are prone to film adsorption problems. Although the latter retains some prism tips and provides brightness guarantee, the mold processing time is long, and the same direction of large and small prisms is prone to optical interference. Technical problems. BRIEF DESCRIPTION OF THE DRAWINGS
[0030] Figure 1 It is a schematic diagram of the prism structure of the utility model;
[0031] Figure 2 It is a schematic diagram of a first prism of the utility model;
[0032] Figure 3 is a cross-sectional schematic diagram of a first prism structure of the utility model;
[0033] Figure 4 is a schematic diagram of a second prism of the utility model;
[0034] Figure 5 is a cross-sectional schematic diagram of the second prism structure of the present utility model; and
[0035] Figure 6 It is a cross-sectional schematic diagram of another second prism structure of the utility model.
[0036] The accompanying drawings are marked as follows:
[0037] 1. First prism; 1', first extension axis; 2. Second prism; 2', second extension axis; 3. Base material layer. DETAILED DESCRIPTION
[0038] In order to enable those skilled in the art to better understand the solution of the present application, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are only part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without creative work should fall within the scope of protection of the present application.
[0039] It should be noted that the terms "first", "second", etc. in the specification and claims of the present application and the above-mentioned drawings are used to distinguish similar objects, and are not necessarily used to describe a specific order or sequential order. It should be understood that the data used in this way can be interchanged where appropriate, so that the embodiments of the present application described here. In addition, the terms "including" and "having" and any of their variations are intended to cover non-exclusive inclusions, for example, a process, method, system, product or device comprising a series of steps or units is not necessarily limited to those steps or units clearly listed, but may include other steps or units that are not clearly listed or inherent to these processes, methods, products or devices.
[0040] In addition, the terms "installed", "set", "provided with", "connected", "connected", and "socketed" should be understood in a broad sense. For example, it can be a fixed connection, a detachable connection, or an integral structure; it can be a mechanical connection, or an electrical connection; it can be a direct connection, or an indirect connection through an intermediate medium, or it can be an internal connection between two devices, elements, or components. For those of ordinary skill in the art, the specific meanings of the above terms in this utility model can be understood according to specific circumstances.
[0041] It should be noted that, in the absence of conflict, the embodiments and features in the embodiments of the present application can be combined with each other. The present application will be described in detail below with reference to the accompanying drawings and in combination with the embodiments.
[0042] like Figure 1 As shown, the present application relates to a prism structure, a brightness enhancement film and its application in a POP type laminated brightness enhancement film and a display device. The prism structure comprises: a plurality of first prisms 1 and a plurality of second prisms 2 arranged in an array, respectively, and the height of the second prism 2 is greater than the height of the first prism 1; the first prism 1 and the second prism 2 are formed by adopting methods including but not limited to: sputtering, evaporation, spraying, coating or mold imprinting, so as to obtain the desired prism structure. The prism structure can be a conventional prism structure in the field of optical films, which can be used for various optical applications such as light splitting, focusing, and beam splitting; at the same time, these prisms can be arranged into various geometric shapes to achieve different optical functions.
[0043] Among them, Figure 2-3As shown, the first prism 1 is the same as a conventional brightness enhancement film, and is an isosceles triangle structure with equal heights and right angles arranged in close proximity.
[0044] By making the height of the second prism 2 greater than the height of the first prism 1 , scratch resistance can be achieved, and at the same time, the first prism 1 can be protected.
[0045] The first prism 1 and the second prism 2 are arranged in an interlaced manner at a preset angle, so that the prism structure has high brightness and scratch resistance. The structure is optimized by arranging the first prism 1 and the second prism 2 on the same plane and in an interlaced manner at a preset angle, thereby obtaining the desired scratch-resistant brightness enhancement film, and finally making the brightness enhancement film have high brightness and excellent scratch resistance.
[0046] The brightness enhancement film of the present application can improve the scratch resistance of the brightness enhancement film while ensuring high brightness due to the special design of the compound prism.
[0047] From the above description, it can be seen that the present application achieves the following technical effects:
[0048] In the embodiment of the present application, the micro-prism structure is optimized, and the first prism 1 and the second prism 2 are staggered with each other according to a preset angle, so as to achieve the purpose of high brightness and excellent scratch resistance, thereby achieving the technical effect of simplifying the optical film structure and improving the optical benefit of the film, thereby solving the problem that in the prior art, a protective film is usually applied to the brightness enhancement film, and the protective film is adhered to the prism structure layer of the brightness enhancement film by glue to protect the prism structure layer, but there will be residual glue left after the protective film is peeled off and other risks of poor appearance, which will also lead to an increase in cost; or a resin with good self-rebounding scratch resistance is used as the upper A layer of UV resin coating is applied to improve the scratch resistance of the brightness enhancing film, but the refractive index of the resin with excellent high resilience and scratch resistance is usually not more than 1.56, which limits the brightness of the brightness enhancing film. On the other hand, methods have been proposed to improve the scratch resistance of the brightness enhancing film by microstructure design, such as a full rounded prism structure, or a high (rounded prism) and low (pointed prism) structure. The former has low brightness due to the destruction of the prism tip, and too many dome angles are prone to film adsorption problems. Although the latter retains some prism tips and provides brightness guarantee, the mold processing time is long, and the same direction of large and small prisms is prone to optical interference.
[0049] Furthermore, the first extension axis 1' of the first prism 1 and the second extension axis 2' of the second prism 2 are in different extension directions and are arranged in a staggered manner. It can be understood that by extending along the extension directions of the first extension axis 1' and the second extension axis 2' respectively and making the extension directions of the two extension axes in different extension directions, it is ensured that an angle is formed between the first extension axis 1' and the second extension axis 2'; at the same time, the staggered prism microstructure is adopted, which can have high brightness and good scratch resistance; thus having good optical performance.
[0050] It should be noted that 1' is also the extending direction of the vertex angle of the first prism, 2' is also the extending direction of the vertex angle of the second prism, and a is the included angle between 1' and 2'.
[0051] Furthermore, the angle a between the extension direction of the first prism 1 and the extension direction of the second prism 2 is 10° to 170°. It is understandable that by setting the angle a between the extension directions of the first prism 1 and the second prism 2 in the range of 10° to 170°, it is possible to ensure that the prism structure has good optical performance, thereby avoiding the situation where the angle is too large or too small to cause poor effect.
[0052] Furthermore, the height h of the first prism 1 is 10-40 um. It is understandable that by setting the height range of the first prism 1 to 10-40 um, a variety of sizes can be selected, thereby meeting diverse usage requirements; at the same time, setting the height of the first prism 1 within the above range can ensure that the first prism 1 has good optical performance.
[0053] Furthermore, the spacing d between adjacent second prisms 2 is 0-20h. It is understandable that by setting the spacing between two adjacent second prisms 2 to 0-20h, a good brightness effect can be ensured, while avoiding the situation where the protection effect is poor and the scratch resistance strength is reduced due to too large a spacing.
[0054] Furthermore, the height H of the second prism 2 is greater than the height h of the first prism 1, and H ≧h+1um. It is understandable that, because the height of the second prism 2 is greater than the height of the first prism 1, the first prism 1 is well protected and scratch-resistant, thereby improving the optical performance; and the first prism 1 can be made of a variety of materials to choose from.
[0055] like Figure 4As shown, the cross section of the second prism 2 is an isosceles triangle, and its vertex angle is a rounded or flat-top structure. It can be understood that by setting the cross section of the second prism 2 to an isosceles right triangle, the effect of improving the structural stability can be achieved; at the same time, setting its vertex angle to a rounded or flat-top structure can improve the brightness gain effect of the brightness enhancement film and also have good scratch resistance. Preferably, the cross section of the second prism 2 is an isosceles right triangle.
[0056] like Figure 5 As shown, when the vertex of the second prism 2 is rounded, the center of the arc is located on the perpendicular bisector of the second prism 2, and the fillet radius r is 0.25-5 um. It can be understood that by setting the fillet radius r to 0.25-5 um, a variety of sizes can be selected, thereby meeting a variety of usage requirements.
[0057] It should be noted that when the r angle of the tip of the second prism 2 is too small, sufficient scratch resistance cannot be provided. When the r angle of the tip of the second prism 2 is too large, the contact area is too large to cause inter-film adsorption. Therefore, setting the fillet radius within the above range can ensure good optical performance.
[0058] like Figure 6 As shown, when the vertex angle of the second prism 2 is a flat-top structure, its vertex angle width W is 0.5-10 um. It is understandable that setting the vertex angle width W to 0.5-10 um can achieve the effect of multiple sizes being available, thereby being able to meet the effect of multiple usage requirements.
[0059] It should be noted that when the flat top width W at the tip of the second prism 2 is too small, it cannot provide sufficient scratch resistance. If it is too large, there will be adsorption between films due to excessive contact area, and obvious stripes will appear on the screen. Therefore, setting the W value within the above range can ensure good optical performance.
[0060] Furthermore, the cross section of the first prism 1 is an isosceles right triangle. It is understandable that by adopting an isosceles right triangle, good structural stability can be ensured; at the same time, an optical effect of improving brightness can be achieved, thereby having good optical performance.
[0061] Furthermore, the first prism 1 and the second prism 2 are light-cured hard resins with a refractive index range of 1.5 to 1.7. It is understandable that due to the difference in structural height, the second prism 2 protects the first prism 1, so that the product can choose a light-cured hard resin with a higher refractive index, thereby improving the brightness of the brightness enhancement film and taking into account the scratch resistance.
[0062] The specific examples are further described below:
[0063] The testing items of the brightness enhancement film provided by the utility model include but are not limited to: scratch resistance test and brightness test.
[0064] Scratch test: The brightness enhancement film of the following example is subjected to multiple scratch tests using a scratch test machine with a load of 200g and the back of the diffusion film; the scratch test may be performed using, but is not limited to, steel wool.
[0065] Brightness test: The brightness enhancement film of the following example was installed in the backlight module, and the brightness was measured using a BM-7AC brightness meter, and the picture condition was observed. Example
[0066] like Figure 1 As shown, the substrate layer 3 is PET, and a UV resin with a refractive index of 1.6 is selected; the height h of the first prism 1 is 20um; the height H of the second prism 2 is 24um, the spacing d between adjacent second prisms 2 is 20um, and the fillet radius r is 2.5um; the angle a between the extension direction of the first prism 1 and the extension direction of the second prism 2 is 90°.
[0067] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 7142cd / m², and the picture condition is normal. Example
[0068] The difference between Example 2 and Example 1 is that the included angle a between the extension direction of the first prism 1 and the extension direction of the second prism 2 is 50°.
[0069] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6857cd / m², and the picture condition is normal. Example
[0070] The difference between Example 3 and Example 1 is that the angle a between the extension direction of the first prism 1 and the extension direction of the second prism 2 is 10°.
[0071] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6503cd / m², and the picture condition is normal. Example
[0072] The difference between Example 4 and Example 1 is that the included angle a between the extension direction of the first prism 1 and the extension direction of the second prism 2 is 130°.
[0073] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6843cd / m², and the picture condition is normal. Example
[0074] The difference between Example 5 and Example 1 is that the distance d between adjacent second prisms 2 is 0.
[0075] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 7552cd / m², and the picture condition is normal. Example
[0076] The difference between Example 6 and Example 1 is that the distance d between adjacent second prisms 2 is 50 um.
[0077] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6941cd / m², and the picture condition is normal. Example
[0078] The difference between Example 7 and Example 1 is that the distance d between adjacent second prisms 2 is 100 um.
[0079] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6691cd / m², and the picture condition is normal. Example
[0080] The difference between Example 8 and Example 1 is that the distance d between adjacent second prisms 2 is 200 um.
[0081] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6435cd / m², and the picture condition is normal. Example
[0082] The difference between Example 9 and Example 1 is that the distance d between adjacent second prisms 2 is 400 um.
[0083] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6247cd / m², and the picture condition is normal. Example
[0084] The difference between Example 10 and Example 1 is that the fillet radius r is 0.25 um.
[0085] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 5 times ok, brightness is 7398cd / m², and the picture condition is normal. Example
[0086] The difference between Example 11 and Example 1 is that the fillet radius r is 5 um.
[0087] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6993cd / m², and the picture condition is normal. Example
[0088] The difference between Example 12 and Example 1 is that the second prism 2 is a flat-top structure, and its top angle width W is 0.5 um.
[0089] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 5 times ok, brightness is 7195cd / m², and the picture condition is normal. Example
[0090] The difference between Example 13 and Example 1 is that the second prism 2 is a flat-top structure, and its top angle width W is 5 um.
[0091] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 10 times ok, brightness is 6841cd / m², and the picture condition is normal. Example
[0092] The difference between Example 14 and Example 1 is that the second prism 2 is a flat-top structure, and its top angle width W is 7 um.
[0093] At this time, after testing, the performance parameters of the brightness enhancement film are: scratch resistance is 12 times ok, brightness is 6528cd / m², and the picture condition is normal.
[0094] Comparative Example 1
[0095] The difference between Comparative Example 1 and Example 1 is that Comparative Example 1 does not have the second prism structure.
[0096] At this time, after testing, the performance parameters of the film are: scratch resistance is 1 NG, brightness is 5983cd / m², and the picture condition is normal.
[0097] Comparative Example 2
[0098] The difference between Comparative Example 2 and Example 1 is that the angle a between the extension direction of the first prism 1 and the extension direction of the second prism 2 is 175°.
[0099] At this time, after testing, the performance parameters of the film are: scratch resistance is 10 times ok, brightness is 6307cd / m², and the screen condition has interference fringes.
[0100] Comparative Example 3
[0101] The difference between Comparative Example 3 and Example 1 is that the distance d between adjacent second prisms 2 is 450 um.
[0102] At this time, after testing, the performance parameters of the film are: scratch resistance is 4 times NG, brightness is 6113cd / m², and the picture condition is normal.
[0103] Comparative Example 4
[0104] The difference between Comparative Example 4 and Example 1 is that the fillet radius r is 0.1 um.
[0105] At this time, after testing, the performance parameters of the film are: scratch resistance is 2 times NG, brightness is 7453cd / m², and the picture condition is normal.
[0106] Comparative Example 5
[0107] The difference between Comparative Example 5 and Example 1 is that the fillet radius r is 6 um.
[0108] At this time, after testing, the performance parameters of the film are: scratch resistance is 10 times ok, brightness is 6938cd / m², and the picture condition is adsorption.
[0109] Comparative Example 6
[0110] The difference between Comparative Example 6 and Example 1 is that the top angle width W is 0.4 um.
[0111] At this time, after testing, the performance parameters of the film are: scratch resistance is 4 times NG, brightness is 7208cd / m², and the picture condition is normal.
[0112] Comparative Example 7
[0113] The difference between Comparative Example 7 and Example 1 is that the vertex width W is 8 um.
[0114] At this time, after testing, the performance parameters of the film are: scratch resistance is 12 times ok, brightness is 6293cd / m², and the picture condition is adsorption.
[0115] The results of various embodiments and comparative examples are shown in Table 1:
[0116]
[0117] From the above test results we can see that:
[0118] 1. It can be seen from Examples 1 to 4 that the brightness enhancement film of the present invention adds a second prism 2, and the top angle of the second prism 2 is rounded, which can not only improve the brightness gain effect of the brightness enhancement film, but also have good scratch resistance.
[0119] 2. It can be seen from Example 1 and Comparative Example 1 that when the second prism structure 2 is not provided, the scratch resistance effect is very poor.
[0120] 3. It can be seen from Examples 1 to 4 and Comparative Example 2 that when the angle a between the second prism 2 and the first prism 1 is too small, interference fringes begin to appear on the screen.
[0121] 4. It can be seen from Examples 1 and 5-9 that the brightness enhancement film of the present invention adds a second prism 2, and the top angle of the second prism 2 is rounded, which can improve the brightness gain effect of the brightness enhancement film and provide good scratch resistance.
[0122] 5. It can be seen from Examples 1, 5-9 and Comparative Example 3 that when the spacing between the second prisms 2 increases, the brightness will gradually decrease. When the spacing between the second prisms 2 is too large, the protection effect will be poor and the scratch resistance will decrease.
[0123] 6. It can be seen from Examples 1 and 10-11 that, after adding the second prism 2, the brightness enhancement film of the utility model can improve the brightness gain effect of the brightness enhancement film and provide good scratch resistance.
[0124] 7. It can be seen from Examples 1, 10-11 and Comparative Examples 4-5 that when the r angle of the second prism tip 2 is too small, it cannot provide sufficient scratch resistance; when the r angle of the second prism tip is too large, inter-membrane adsorption will occur due to excessive contact area.
[0125] 8. It can be seen from Examples 1 and 12-14 that the brightness enhancement film of the utility model adds a second prism 2, and the top angle of the second prism 2 is a flat-top structure, which can improve the brightness gain effect of the brightness enhancement film and provide good scratch resistance. As the top angle size of the second prism 2 increases, the number of scratch resistance of the film tends to increase, and the brightness tends to decrease.
[0126] 9. It can be seen from Examples 1, 12-14 and Comparative Examples 6-7 that when the W value of the second prism 2 is too small, the scratch resistance will be reduced. When the W value of the second prism 2 is too large, inter-film adsorption will occur.
[0127] It should be noted that 5 scratch resistance times is the bottom line for passing.
[0128] The present application also relates to a brightness enhancement film, comprising the prism structure as described above;
[0129] The first prism 1 and the second prism 2 are arranged alternately with each other at a preset angle to form a transparent structure layer; and
[0130] A substrate layer 3 is disposed on the side of the transparent structure layer away from the extension axis.
[0131] Specifically, the substrate layer 3 refers to the base material or substrate to which the optical film or coating is attached, which can achieve good fixing and supporting effects; at the same time, it can also cooperate with other film layer structures to achieve multiple functional effects. Preferably, the substrate layer is PET, PC, PMMA, PE, PVC or PS. It can achieve the effect of multiple materials to choose from, so that the effect can be easily achieved.
[0132] By staggering the first prism 1 and the second prism 2 on the substrate layer 3 at a preset angle, a single brightness enhancement film with a stable structure can be formed, while also having high brightness and scratch resistance.
[0133] The present application also relates to a POP-type laminated brightness enhancement film, wherein the upper prism layer includes the brightness enhancement film as described above.
[0134] The scratch-resistant compound staggered prism structure of the utility model can be applied to not only a single brightness enhancement film, but also a POP type laminated brightness enhancement film as an upper prism structure to improve the surface scratch resistance of the POP product.
[0135] The present application also relates to a display device, comprising the brightness enhancement film as described above.
[0136] The preferred embodiments of the present invention are described in detail above in conjunction with the accompanying drawings; however, the present invention is not limited to the specific details in the above embodiments. Within the technical concept of the present invention, various equivalent transformations can be made to the technical scheme of the present invention, and these equivalent transformations all belong to the protection scope of the present invention.
Claims
1. A prismatic structure, characterized in that: include: A plurality of first prisms (1) and a plurality of second prisms (2) are arranged in an array, and the height of the second prisms (2) is greater than the height of the first prisms (1); Wherein, the first prism (1) and the second prism (2) are arranged alternately with each other at a preset angle.
2. The prism structure according to claim 1, characterized in that: The first extension axis (1') of the first prism (1) and the second extension axis (2') of the second prism (2) are in different extension directions and are arranged in a staggered manner.
3. The prism structure according to claim 1, characterized in that: The included angle a between the extension direction of the first prism (1) and the extension direction of the second prism (2) is 10° to 170°.
4. The prism structure according to claim 1, characterized in that: The height h of the first prism (1) is 10-40 um.
5. The prism structure according to claim 1, characterized in that: The distance d between adjacent second prisms (2) is 0 to 20h.
6. The prism structure according to claim 1, characterized in that: The height H of the second prism (2) is greater than the height h of the first prism (1), and H≧h+1um.
7. The prism structure according to claim 1, characterized in that: The cross section of the second prism (2) is an isosceles triangle, and its top angle is a rounded or flat top structure.
8. The prism structure according to claim 7, characterized in that: When the vertex angle of the second prism (2) is rounded, the center of the arc is located on the perpendicular bisector of the second prism (2), and the rounded radius r is 0.25 to 5 um.
9. The prism structure according to claim 7, characterized in that: When the vertex of the second prism (2) is a flat-top structure, its vertex width W is 0.5-10 um.
10. The prism structure according to claim 1, characterized in that: The cross section of the first prism (1) is an isosceles right triangle.
11. The prism structure according to claim 1, characterized in that: The first prism (1) and the second prism (2) are photocurable hard resins, and the refractive index range is 1.5 to 1.
7.
12. The prism structure according to claim 1, characterized in that: The second prism (2) is configured as a non-pointed prism structure.
13. A brightness enhancement film, characterized in that: comprising a prismatic structure as claimed in any one of claims 1 to 12; It also includes: the first prism (1) and the second prism (2) are arranged alternately with each other at a preset angle to form a transparent structure layer; and The transparent structure layer is provided with a substrate layer (3) on the bottom side of the transparent prism structure layer.
14. Applied to POP type bonding brightening film, characterized in that: The upper prism layer includes the brightness enhancement film as claimed in claim 13.