Micropressure sensor chip
By combining beam-membrane and groove-membrane structural design with E-cup structure, the problem of insufficient sensitivity and linearity of MEMS piezoresistive pressure sensors in micro-pressure measurement is solved, realizing a micro-pressure sensor chip with high sensitivity and low nonlinearity, which is suitable for industrial, medical, petrochemical and defense fields.
Patent Information
- Application Number
- CN202420069195.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-01-11
- Publication Date
- 2024-11-19
- Estimated Expiration
- 2034-01-11
AI Technical Summary
Existing MEMS piezoresistive pressure sensors lack sufficient sensitivity and linearity in micro-pressure measurement and are difficult to mass-produce, especially for micro-pressure sensors below 1 kPa.
The structure adopts a combination of beam-membrane and groove-membrane design, combined with E-cup structure, and uses varistor to form Wheatstone bridge. Micro pressure sensor chip is fabricated through SOI process and RIE technology to increase stress concentration and overload resistance.
The sensitivity of the micro-pressure sensor chip has been increased by 5 times, the nonlinearity has been reduced to 0.3%FS, and it has good linearity and overload resistance, making it easy to mass-produce.
Smart Images

Figure CN222027817U_ABST
Abstract
Description
Technical Field
[0001] The present application relates to the field of sensors, and in particular to a micro-pressure sensor chip. Background Art
[0002] Micro Electro Mechanical System (MEMS) is an independent intelligent system that integrates micro-mechanisms, micro-sensors, micro-actuators and corresponding processing circuits. MEMS devices use micro-machining technology and can be mass-produced. MEMS devices are in the order of millimeters or even smaller micrometers, or even nanometers in size.
[0003] With the development of MEMS technology, MEMS pressure sensors are becoming more and more mature. With their advantages of high sensitivity, high precision, low power consumption and low cost, they have occupied most of the pressure sensor market. As the main branch of sensors, pressure sensors have been widely used in various fields such as industry, medical treatment, petrochemical industry and national defense. MEMS pressure sensors can be divided into capacitive, piezoresistive and resonant types according to the measurement principle. Among them, capacitive pressure sensors have high sensitivity and small temperature drift, but their input impedance is large, easily affected by parasitic capacitance, and are sensitive to interference from the surrounding environment; the manufacturing process of resonant pressure sensors is complex and the yield rate is low; although piezoresistive pressure sensors are easily affected by temperature, they can be compensated by circuits, etc., and piezoresistive pressure sensors are widely used because of their high sensitivity, low cost, fast response speed, good reliability and easy integration.
[0004] MEMS piezoresistive pressure sensors are based on the piezoresistive properties of silicon. Thin-film piezoresistors are formed on silicon substrates and connected into a Wheatstone bridge. When the sensor is subjected to pressure, the resistance changes, and an electrical signal proportional to the pressure change can be output through the detection circuit. Piezoresistors are often arranged in the stress concentration area at the edge of the stress film. As the sensor stress film becomes thinner, the sensor sensitivity increases. At the same time, the deflection of the sensor increases, and its nonlinearity gradually increases, which increases the difficulty of signal processing. In order to improve the sensitivity output of the sensor and improve nonlinearity, many new sensitive diaphragm structures have emerged, including double island structures, E-shaped cup structures, beam membrane structures, etc. These structures can solve the contradiction between output sensitivity and linearity to a certain extent. However, it still takes a long time from theoretical knowledge to mass production, and there is still no report on the mass production of silicon piezoresistive micro-pressure sensors below 1KPa. Utility Model Content
[0005] In order to solve the above technical problems or at least partially solve the above technical problems, the present application provides a micro-pressure sensor chip.
[0006] In the first aspect, the present application provides a micro-pressure sensor chip, comprising: a varistor, an aluminum electrode, an intermediate silicon layer, a silicon boss, a buried oxide layer and glass, wherein the varistor is arranged on the top surface of the intermediate silicon layer, the aluminum electrode is connected to the varistor, the buried oxide layer is arranged on the bottom surface of the intermediate silicon layer, the silicon boss is arranged on the bottom surface of the buried oxide layer, and the glass is connected to the intermediate silicon layer.
[0007] Preferably, four varistors are arranged on the middle silicon layer.
[0008] Preferably, each of the varistor is connected to a corresponding aluminum electrode.
[0009] Preferably, the varistor is led to the aluminum electrode through a conduction tape.
[0010] Preferably, a groove is provided on the middle silicon layer.
[0011] Preferably, the groove is adjacent to the varistor.
[0012] Preferably, the groove is located between four varistors.
[0013] Preferably, a cavity is formed between the buried oxide layer and the glass.
[0014] Preferably, the four varistors are connected to form a Wheatstone bridge.
[0015] Preferably, the groove is L-shaped.
[0016] The above technical solution provided by the embodiment of the present application has the following advantages compared with the prior art:
[0017] The structure of a micro-pressure sensor chip provided in an embodiment of the present application, which combines a beam membrane and a groove membrane, is more conducive to stress concentration. Compared with a flat membrane structure of the same size, its full-scale output is increased by about 5 times; the addition of a back boss can play a limiting role under high pressure conditions, has good overload resistance, and at the same time reduces the chip nonlinearity from 4.9% FS to 0.3% FS; it can realize the measurement of tiny pressures and ensure a certain sensitivity output, and has the advantages of high sensitivity, good linearity, strong overload capacity, and ease of mass production. BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The accompanying drawings herein are incorporated in and constitute a part of the specification, illustrate embodiments consistent with the present utility model, and together with the description, are used to explain the principles of the present utility model.
[0019] In order to more clearly illustrate the technical solutions in the embodiments of the utility model or the prior art, the drawings required for use in the embodiments or the description of the prior art will be briefly introduced below. Obviously, for ordinary technicians in this field, other drawings can be obtained based on these drawings without paying any creative labor.
[0020] Figure 1 is a schematic diagram of a Wheatstone bridge;
[0021] Figure 2 This is a double buried oxide layer SOI process flow chart;
[0022] Figure 3 This is the chip process flow chart;
[0023] Figure 4 This is the front view of the micro-pressure chip;
[0024] Figure 5 A rear view of a micro-pressure sensor chip provided in an embodiment of the present application;
[0025] Figure 6 A cross-sectional view of a micro-pressure sensor chip provided in an embodiment of the present application. DETAILED DESCRIPTION
[0026] In order to make the purpose, technical solution and advantages of the embodiments of the present application clearer, the technical solution in the embodiments of the present application will be clearly and completely described below in conjunction with the drawings in the embodiments of the present application. Obviously, the described embodiments are part of the embodiments of the present application, not all of the embodiments. Based on the embodiments in the present application, all other embodiments obtained by ordinary technicians in this field without making creative work are within the scope of protection of this application.
[0027] like Figure 1-6 The present application provides a micro-pressure sensor chip, comprising: a varistor 1, an aluminum electrode 4, an intermediate silicon layer 5, a silicon boss 7, a buried oxide layer 8 and a glass 9, wherein the varistor 1 is arranged on the top surface of the intermediate silicon layer 5, the aluminum electrode 4 is connected to the varistor 1, the buried oxide layer 8 is arranged on the bottom surface of the intermediate silicon layer 5, the silicon boss 7 is arranged on the bottom surface of the buried oxide layer 8, and the glass 9 is connected to the intermediate silicon layer 5.
[0028] In the embodiment of the present application, four varistors 1 are arranged on the intermediate silicon layer 5 , and each of the varistors 1 is correspondingly connected to an aluminum electrode 4 .
[0029] In the embodiment of the present application, a groove 3 is provided on the intermediate silicon layer 5, and the groove 3 is adjacent to the varistor 1. The groove 3 is adjacent to the varistor 1 so that the stress is more concentrated on the varistor, which can improve the sensitivity of the chip.
[0030] In the embodiment of the present application, the groove 3 is located between the four varistors 1. The groove 3 is located between the four varistors 1. When pressure is applied, stress is concentrated on the varistors, the resistors respond more sensitively, the variation range increases, and the chip output increases accordingly.
[0031] In the embodiment of the present application, a cavity 6 is formed between the buried oxide layer 8 and the glass 9. The cavity 6 and the upper diaphragm together constitute a pressure-sensing structure. Because of the presence of the cavity 6, when the diaphragm is subjected to uniform stress, the deflection generated at the center of the diaphragm will be greater, and the change of the piezoresistive part will increase accordingly, thereby increasing its sensitivity.
[0032] The pressure sensitive unit of the sensor is prepared by combining a beam membrane and a slot membrane. The piezoresistors 1 are placed at the stress concentration point above the beam membrane structure. Four piezoresistors 1 are connected to form a Wheatstone bridge, such as Figure 1 As shown in the figure, when the sensor chip is in working state, the diaphragm will be slightly deformed under the action of micro pressure, and the resistance value of the varistor 1 will change with the pressure change. The detection of micro pressure can be realized by using the Wheatstone bridge. Another feature of the sensor is that the back side adopts the E-cup structure. The sensitive film is relatively thin. The E-cup structure can play a limiting role when the external pressure is too large, improve the overload resistance of the sensor, and reduce the nonlinearity of the chip.
[0033] The production process of this micro-pressure sensor chip is as follows:
[0034] 1. Prepare three silicon wafers and clean them;
[0035] 2. Take two of the wafers, perform thermal oxidation treatment, form a SiO2 layer on them, and then use ion implantation to implant hydrogen ions into the wafer substrate;
[0036] 3. Bond one of the processed wafers to the unprocessed wafer;
[0037] 4. Two-step heat treatment: the first step is heat treatment at 400-600℃. The wafer implanted with hydrogen ions will break at the hydrogen ion enrichment point, and the silicon layer can still be used after peeling off; the second step is high-temperature heat treatment at 1100℃ to form Si-O-Si bonds at the bonding interface, improve the strength of the bonding interface, and eliminate the implantation damage in the SOI layer;
[0038] 5. Perform chemical mechanical polishing (CMP) on the surface to obtain an SOI wafer having a buried oxide layer 8;
[0039] 6. Bonding the SOI wafer having a buried oxide layer 8 to the wafer formed by thermal oxidation in step 2;
[0040] 7. After bonding, a two-step heat treatment is performed, which is consistent with step 4, to form a silicon wafer and a wafer with a double buried oxide layer 8;
[0041] 8. Obtaining an SOI wafer having a double buried oxide layer 8 by chemical mechanical polishing;
[0042] 9. Perform ion implantation on the top silicon layer of the SOI wafer of the double buried oxide layer 8 to form a doped layer;
[0043] 10. Spin the upper layer of the SOI wafer with the double buried oxide layer 8 to photoetch four "L"-shaped grooves 3, then use the photoresist as a mask to etch the doped silicon layer, the first buried oxide layer 8, and a part of the middle silicon layer 5 using RIE (Reactive Ion Etching) technology, remove the photoresist, and obtain four "L"-shaped grooves 3 to form a ladder beam film and groove film structure. This structure can concentrate stress on the ladder beam film, which can greatly improve the chip sensitivity;
[0044] 11. Photolithography a varistor 1 pattern on the beam membrane structure, then use photoresist as a mask, use RIE technology to etch silicon to the silicon dioxide layer, remove the photoresist, and obtain four varistors 1;
[0045] 12. Depositing a silicon nitride passivation layer on the upper and lower surfaces;
[0046] 13. Dry etching is performed on the back cavity. First, the cavity 6 is photoetched, and then a certain thickness of silicon material is removed using a photoresist as a mask and the second buried oxide layer 8 as an etching stop layer. At the same time, a silicon boss 7 is formed on the back. When pressure is applied, the silicon boss 7 can play a limiting role;
[0047] 14. Etch away the silicon nitride on the back side using RIE technology, and then bond with glass 9;
[0048] 15. Sprinkle glue on the front side and etch the lead holes by photolithography;
[0049] 16. Metal aluminum is sputtered on the front surface, and photolithography is performed using the electrode plate to form a pad after photolithography. Finally, the remaining passivation layer is etched away using RIE technology.
[0050] Figure 4 It is a front view of the micro-voltage chip, where 1-1, 1-2, 1-3, and 1-4 are varistors; 2-1, 2-2, 2-3, and 2-4 are trapezoidal beams; 3-1, 3-2, 3-3, and 3-4 are four L-shaped grooves; 4-1, 4-2, 4-3, 4-4, and 4-5 are aluminum electrodes.
[0051] The structure of a micro-pressure sensor chip provided in an embodiment of the present application, which combines a beam membrane and a groove membrane, is more conducive to stress concentration. Compared with a flat membrane structure of the same size, its full-scale output is increased by about 5 times; the addition of a back boss can play a limiting role under high pressure conditions, has good overload resistance, and at the same time reduces the chip nonlinearity from 4.9% FS to 0.3% FS; it can realize the measurement of tiny pressures and ensure a certain sensitivity output, and has the advantages of high sensitivity, good linearity, strong overload capacity, and ease of mass production.
[0052] It should be noted that, in this article, relational terms such as "first" and "second" are only used to distinguish one entity or operation from another entity or operation, and do not necessarily require or imply any such actual relationship or order between these entities or operations. Moreover, the terms "include", "comprise" or any other variants thereof are intended to cover non-exclusive inclusion, so that a process, method, article or device including a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or device. In the absence of further restrictions, the elements defined by the sentence "comprise a ..." do not exclude the existence of other identical elements in the process, method, article or device including the elements.
[0053] The above description is only a specific embodiment of the present invention, so that those skilled in the art can understand or implement the present invention. Various modifications to these embodiments will be obvious to those skilled in the art, and the general principles defined herein can be implemented in other embodiments without departing from the spirit or scope of the present invention. Therefore, the present invention will not be limited to the embodiments shown herein, but should conform to the widest scope consistent with the principles and novel features applied herein.
Claims
1. A micro-pressure sensor chip, characterized in that: include: A varistor, an aluminum electrode, an intermediate silicon layer, a silicon boss, a buried oxide layer and glass, wherein the varistor is arranged on the top surface of the intermediate silicon layer, the aluminum electrode is connected to the varistor, the buried oxide layer is arranged on the bottom surface of the intermediate silicon layer, the silicon boss is arranged on the bottom surface of the buried oxide layer, and the glass is connected to the intermediate silicon layer.
2. The micro-pressure sensor chip according to claim 1, characterized in that: Four varistors are arranged on the middle silicon layer.
3. The micro-pressure sensor chip according to claim 2, characterized in that: Each of the varistor is correspondingly connected to an aluminum electrode.
4. The micro-pressure sensor chip according to claim 2, characterized in that: The varistor is led to the aluminum electrode through a conducting tape.
5. The micro-pressure sensor chip according to claim 2, characterized in that: The middle silicon layer is provided with a groove.
6. The micro-pressure sensor chip according to claim 5, characterized in that: The groove is adjacent to the varistor.
7. The micro-pressure sensor chip according to claim 6, characterized in that: The groove is located between the four varistors.
8. The micro-pressure sensor chip according to claim 1, characterized in that: A cavity is formed between the buried oxide layer and the glass.
9. The micro-pressure sensor chip according to claim 2, characterized in that: The four varistors are connected to form a Wheatstone bridge.
10. The micro-pressure sensor chip according to claim 5, characterized in that: The groove is L-shaped.