Device for continuously producing sodium fluoride
By using a high shear reactor and centrifugal separator in the production of sodium fluoride, combined with acrylamide precipitation additives, the purity and impurities of fluorine resource recovery in phosphoric acid are solved, the yield and purity of sodium fluoride are improved, and the purity of sodium fluoride is reduced. Wastewater discharge achieves efficient and environmentally friendly sodium fluoride production.
Patent Information
- Application Number
- CN202420668977.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Utility models(China)
- Current Assignee / Owner
- Filing Date
- 2024-04-02
- Publication Date
- 2024-11-22
- Estimated Expiration
- 2034-04-02
AI Technical Summary
When the prior art uses phosphoric acid to recover fluorine resources, sodium fluoride has low purity, high impurity content, long reaction time, and wastewater discharge problems have not been effectively solved, resulting in low resource utilization efficiency and great environmental impact.
The technology of high shear reactor and centrifugal separator combined with acrylamide as a precipitation additive is used to improve the purity and yield of sodium fluoride through efficient mixing and separation processes, and reduce wastewater discharge through clean liquid reuse.
It significantly improves the production efficiency and purity of sodium fluoride, shortens the reaction time, reduces production costs, and achieves efficient utilization of resources and environmental protection.
Smart Images

Figure CN222034749U_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of chemical sodium fluoride manufacturing, and in particular to a device for continuously producing sodium fluoride. Background Art
[0002] In the chemical industry, sodium fluoride is widely used. It is not only the main source of fluoride ions in many fluorine compounds, but also used to manufacture other fluorides, as a hydrogen fluoride absorbent in fluorine chemical industry, fungicide, insecticide, wood preservative, water treatment agent, light metal fluoride salt treatment agent, smelting metal protective agent, as well as in the nuclear industry, metal cleaning, flux, welding agent and adhesive corrosion protection and other fields. With the rapid development of the domestic sodium fluoride industry, the demand for sodium fluoride is also growing, especially in the fields of smelting and refining, wear-resistant materials and ferrous metal surface treatment.
[0003] At present, the main source of fluorine in my country's fluorine chemical industry is fluorite, but with the rapid development of the fluorine chemical industry and the over-exploitation of fluorite resources, serious damage has been caused to environmental resources. In response to resource depletion and environmental protection requirements, the mining of fluorite and the process of producing anhydrous hydrogen fluoride using fluorite as raw material have been strictly restricted, forcing the fluorine chemical industry to seek new fluorine sources.
[0004] With the depletion of traditional fluorite resources, fluorine in phosphate rock has become an important fluorine resource. Phosphate rock is mainly used to produce phosphoric acid, and the phosphoric acid with too high fluorine content produced during the production of wet-process phosphoric acid needs to be defluorinated to meet further production and application needs. The fluorine in wet-process phosphoric acid mainly exists in the form of fluorosilicic acid, which is currently mainly recycled in the form of sodium fluorosilicate and potassium fluorosilicate products, but the market demand for these products is limited, resulting in low efficiency in the utilization of fluorine resources in phosphorus chemical industry and waste of resources. Therefore, how to efficiently use fluorosilicic acid in wet-process phosphoric acid to prepare sodium fluoride with market prospects has become the focus of research in phosphorus chemical industry and fluorine chemical industry.
[0005] Although various methods for producing sodium fluoride using sodium fluorosilicate have been proposed in the prior art, such as the method for preparing sodium fluoride using wet phosphoric acid defluorination residue disclosed in CN104386711A, the method for efficiently producing silicon tetrafluoride and sodium fluoride using sodium fluorosilicate disclosed in CN110683548A, and the production method for co-producing sodium fluoride with sodium silicate disclosed in CN105858676A. Although these methods have achieved the recycling of fluorine resources to a certain extent, there are still many shortcomings, such as the impurities that may be contained in the reaction affect the purity of the final sodium fluoride product, as well as the efficiency and cost issues in the separation process.
[0006] Therefore, developing a new technology for producing high-purity, low-impurity sodium fluoride, recycling fluorine resources in an efficient and environmentally friendly way, and meeting the demand for high-quality sodium fluoride in the fluorine chemical industry are crucial to promoting sustainable resource utilization and supporting the development of the fluorine chemical industry. The current challenge is to find a method that can maximize the recovery of fluorine from phosphoric acid and produce sodium fluoride with high purity and low impurity content. This requires an innovative method for separating fluorine from phosphoric acid that can overcome the limitations of existing technologies.
[0007] To this end, researchers are exploring new technical paths, including improving the extraction and refining process of fluorine, and developing more efficient reaction catalytic systems. For example, by optimizing the reaction conditions of sodium fluorosilicate and sodium carbonate, controlling the reaction temperature and time, and adopting more efficient separation and purification technologies, the yield and purity of sodium fluoride can be significantly improved. In addition, the development of a low-cost, high-efficiency new process for the production of sodium fluoride will not only help reduce dependence on fluorite resources, but also promote the efficient use of fluorine resources and reduce the impact on the environment. Utility Model Content
[0008] The utility model aims to solve the problems of low purity and high impurity content of sodium fluoride in the process of preparing sodium fluoride, the problem of long reaction time of continuous production of sodium fluoride, and the problem of wastewater discharge in the process of preparing sodium fluoride.
[0009] The above technical objectives of the utility model are achieved through the following technical solutions:
[0010] A device for continuously producing sodium fluoride comprises a high shear reactor, wherein a sodium fluorosilicate slurry inlet pipe, a sodium carbonate solution inlet pipe and a high shear agitator motor are arranged on the top of the high shear reactor; the top of the high shear reactor is connected to the outlet of a clear liquid recovery pipe, the inlet of the clear liquid recovery pipe is connected to the clear liquid outlet of a centrifuge, the outlet of the high shear reactor is connected to the inlet of a reaction mixture outlet pipe, the outlet of the reaction mixture outlet pipe is connected to the reaction mixture inlet of the centrifuge, a silicon slag outlet pipe is arranged at the bottom of the centrifuge, and the centrifuge is connected to a drying system through a sodium fluoride crystallization outlet pipe.
[0011] The sodium carbonate solution inlet pipe delivers the sodium carbonate solution to the vicinity of the rotating shaft of the high shear agitator motor through the liquid delivery pipe.
[0012] The sodium fluorosilicate slurry inlet pipe and the sodium carbonate solution inlet pipe are connected to the high shear reactor through flanges.
[0013] The reaction mixture outlet pipe is provided with a flange.
[0014] The angle of the sodium fluoride crystallization outlet pipe is horizontally set downward at 15° to 45°.
[0015] Compared with the prior art, the utility model has the following beneficial effects:
[0016] 1. This device utilizes the efficient mixing of the high shear reactor to improve the reaction efficiency of sodium fluorosilicate and sodium carbonate, and significantly improves the production efficiency and product purity of sodium fluoride.
[0017] 2. Acrylamide is added as a precipitation aid during the reaction process. Acrylamide can promote the aggregation and precipitation of silicon slag. By promoting the precipitation of silicon slag with acrylamide, the subsequent separation process is simplified and the separation efficiency is improved.
[0018] 3. Reuse of clear liquid reduces wastewater discharge, reduces environmental impact, and achieves green production.
[0019] 4. The use of high shear reactor shortens the reaction time, improves production continuity and reduces production costs. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 This is a schematic diagram of a continuous production device for preparing sodium fluoride according to the utility model;
[0021] Figure numerals: 1. high shear reactor, 2. centrifuge, 3. drying system, 4. sodium fluorosilicate slurry inlet pipe, 5. sodium carbonate solution inlet pipe, 6. reaction mixture outlet pipe, 7. sodium fluoride crystallization outlet pipe, 8. silicon slag outlet pipe, 9. clear liquid recovery pipe, 10. liquid delivery pipe, 11. high shear agitator motor. DETAILED DESCRIPTION
[0022] The working principle of this device for preparing sodium fluoride from sodium fluorosilicate is: the efficient mixing of the high shear reactor is used to improve the reaction efficiency of sodium fluorosilicate and sodium carbonate, and it is also convenient for the subsequent product separation and purification. Acrylamide is added as a precipitation aid during the reaction process to optimize the separation effect of the reaction products. Acrylamide can promote the aggregation and precipitation of silicon slag, thus facilitating the subsequent separation process.
[0023] Example 1
[0024] The present invention provides a continuous production device for preparing sodium fluoride from sodium fluorosilicate, which adopts high shear reactor technology to realize a high-efficiency, low-cost continuous production process. In the device for continuously producing sodium fluoride, the high shear agitator motor 11, the centrifuge 2 and the drying system 3 are powered by an external power supply. By adding sodium fluorosilicate slurry and sodium carbonate solution to the high shear reactor, the reaction process is strengthened by using a high shear agitator at a reaction temperature of 80°C-100°C, and acrylamide is added to optimize the separation effect of the reaction product. After centrifugal separation, the obtained liquid is obtained to obtain sodium fluoride crystals and high-viscosity liquid silicon slag, and the clear liquid is reused to finally obtain first-grade sodium fluoride with a purity greater than 98%.
[0025] like Figure 1 As shown, sodium fluorosilicate slurry and sodium carbonate solution at 80°C-100°C are added through the sodium fluorosilicate slurry inlet pipe 4 and the sodium carbonate solution inlet pipe 5 on the top of the high shear reactor 1. The sodium fluorosilicate slurry is a mixed solution of sodium fluorosilicate and acrylamide, and the sodium carbonate solution inlet pipe 5 delivers the sodium carbonate solution to the vicinity of the rotating shaft of the high shear agitator motor 11 through the liquid delivery pipe 10. The speed of the high shear agitator motor is set at 600-800 rpm. Under the reaction temperature of 80°C-100°C and the high shear force provided by the high shear agitator motor 11, the two raw materials react rapidly under the strengthening effect of the high shear agitator, and acrylamide is added to promote the separation of the reaction products. The reaction mixture is sent to the centrifuge 2 through the reaction mixture outlet pipe 6. After centrifugal treatment, sodium fluoride crystals, silicon slag and clear liquid are separated. The silicon slag is discharged through the silicon slag outlet pipe 8, and the sodium fluoride crystals are sent to the drying system 3 for drying through the sodium fluoride crystal outlet pipe 7. The angle of the crystal outlet pipe 7 is set to be 15 to 45 degrees downward from the horizontal, which is convenient for the transmission of sodium fluoride crystal materials. Sodium fluoride with a purity greater than 98% is obtained. The clear liquid is recycled in the high shear reactor 1 through the clear liquid recovery pipe 9, realizing efficient utilization of raw materials and environmental protection.
[0026] By adopting a high shear reactor, this new type significantly improves the reaction rate and conversion efficiency of raw materials in the production process of sodium fluoride, shortens the production cycle, and reduces energy consumption. In addition, the addition of acrylamide as a precipitation aid effectively promotes the rapid precipitation and separation of silicon slag, further improving the purity of sodium fluoride. Through centrifugal separation technology, sodium fluoride crystals are effectively separated from silicon slag, ensuring the high purity and high quality of the product. The application of clear liquid recycling technology not only reduces wastewater discharge, but also realizes the recycling of raw materials, reduces production costs, and also plays a positive role in environmental protection.
[0027] The utility model patent uses a high shear reactor to accelerate the reaction process of sodium fluorosilicate and sodium carbonate, significantly improving the reaction rate and efficiency. Adding acrylamide as a precipitation aid effectively promotes the rapid precipitation and separation of silicon slag and improves the purity of the product.
[0028] Various modifications and variations can be made to the present invention without departing from the spirit and scope of the present invention. For example, the proportion of acrylamide used can be adjusted according to actual production needs to optimize the precipitation effect and production efficiency. In addition, the specific type and parameters of the high shear reactor, such as stirring rate, temperature control, etc., can also be optimized and adjusted according to actual production conditions to further improve production efficiency and product quality.
Claims
1. A device for continuously producing sodium fluoride, comprising a high shear reactor (1), characterized in that: The top of the high shear reactor (1) is provided with a sodium fluorosilicate slurry inlet pipe (4), a sodium carbonate solution inlet pipe (5) and a high shear agitator motor (11); the top of the high shear reactor (1) is connected to the outlet of a clear liquid recovery pipe (9), the inlet of the clear liquid recovery pipe (9) is connected to the clear liquid outlet of a centrifuge (2), the outlet of the high shear reactor (1) is connected to the inlet of a reaction mixture outlet pipe (6), the outlet of the reaction mixture outlet pipe (6) is connected to the reaction mixture inlet of the centrifuge (2), the bottom of the centrifuge (2) is provided with a silicon slag outlet pipe (8), and the centrifuge (2) is connected to a drying system (3) via a sodium fluoride crystallization outlet pipe (7).
2. The device for continuously producing sodium fluoride according to claim 1, characterized in that: The sodium carbonate solution inlet pipe (5) delivers the sodium carbonate solution to the vicinity of the rotating shaft of the high shear agitator motor (11) via the liquid delivery pipe (10).
3. The device for continuously producing sodium fluoride according to claim 1, characterized in that: The sodium fluorosilicate slurry inlet pipe (4) and the sodium carbonate solution inlet pipe (5) are connected to the high shear reactor (1) via flanges.
4. The device for continuously producing sodium fluoride according to claim 1, characterized in that: The reaction mixture outlet pipe (6) is provided with a flange.